50% natural, renewable and impermeable compound that is resistant to high temperatures and is widely used in industry, combining natural, physical, mechanical and thermal properties

A composite material combining coconut shell, expanded perlite, and epoxy resin, with carbon fiber reinforcement, addresses the need for high-temperature resistance and efficient production, offering improved industrial performance and ease of manufacturing.

WO2024243712A1PCT designated stage expired Publication Date: 2024-12-05MELOSSI JIMENEZ ANDRES +1
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
PCT/CL2024/050079
Authority / Receiving Office
WO · WO
Patent Type
Applications
Current Assignee / Owner
Priority Date
2023-06-01
Filing Date
2024-07-31
Publication Date
2024-12-05

AI Technical Summary

Technical Problem

Current materials fail to combine natural, physical, mechanical, and thermal properties effectively for wide industrial use, particularly lacking in high temperature resistance and ease of production.

Method used

A composite material is created by mixing coconut shell powder with expanded perlite and epoxy resin, incorporating carbon fiber fabric, and using a molding process with controlled temperature and pressure to produce a waterproof, high-temperature-resistant product.

Benefits of technology

The resulting material exhibits enhanced resistance to high temperatures and fire, with improved production efficiency and uniformity, suitable for diverse industrial applications.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 000006
    Figure 000006
  • Figure 00000005_0000
    Figure 00000005_0000
  • Figure 00000005_0001
    Figure 00000005_0001
Patent Text Reader

Abstract

The invention relates to a 50% natural, renewable and impermeable compound that is widely used in industry and combines natural, physical, mechanical and thermal properties. Said compound is characterised in that when it solidifies, it withstands temperatures between 300°C and 405°C, becoming water-resistant. The compound is obtained by combining the blend of 8 parts of powdered coconut shell (endocarp) with 2 parts of expanded perlite (of rhyolite mineral) that is also powered and 80% epoxy resin in relation to the amount of coconut shell powder to be used, until achieving a lump-free moistened powder. This powder is then poured into the desired matrix and a carbon fibre fabric layer is added in the lower portion and another layer is added in the upper portion of the compound. It is pressed at a maximum of 1000 kg of pressure with levelling sensors and at a temperature of 110°C, to then cool and obtain the desired part by means of chiller equipment. When this compound solidifies by means of compression and moulding, it enables the manufacture, via thermal action and according to its intended use, of cabinets for electrical devices or, for example, boards for interiors, mirror frames, etc., in the automotive industry.
Need to check novelty before this filing date? Find Prior Art

Description

[0001] 50% NATURAL AND RENEWABLE COMPOUND. WATERPROOF, HIGH TEMPERATURE RESISTANT, WIDELY USED INDUSTRIALLY, COMBINING NATURAL, PHYSICAL, MECHANICAL, AND THERMAL PROPERTIES

[0002] DESCRIPTIVE MEMORY

[0003] DETAILED DESCRIPTION OF THE INVENTION

[0004] Starting from the coconut shell:

[0005] • The coconut shell is crushed into a powder state at a density of 0.50 gr / ml.

[0006] • Coconut shell powder is mixed with expanded perlite (a natural mineral obtained from the piolite plant). The expanded perlite is ground into a powder state at a density of 0.30 g / ml, with the mixing percentages being 8 parts coconut shell and 2 parts expanded perlite. The addition of expanded perlite provides greater strength when the final product is exposed to high temperatures.

[0007] • Epoxy resin is incorporated, the quantity to be incorporated is 80% in relation to the coconut shell to be used, since when the resin is introduced into the mixture through an aluminum paddle, it is absorbed by the coconut powder, leaving a moistened powder without lumps, and mixing must be carried out by mechanical action until the powder is uniform without lumps.

[0008] • In the molding and pressing process by means of a die: a)- the lower part of the die is incorporated into the pneumatic press, which will form the visible part of the product to be molded, b)- the powder mixture is incorporated into it, c)- the pressing action is exerted by the upper plate with leveling and temperature sensors of 110 ° C, which is subject to the pneumatic piston, the leveling sensor system is important to obtain a uniform mixture in the entire molded product, when pressure is exerted this causes the resin to be released and mixed in total proportion and uniformity, the minimum pressure exerted is 300 kg, maximum 1000 kg.d)- the matrix is ​​cooled by means of a chiller equipment which has the water circuit inside, this cold blast causes the material to solidify forming a compact compound and can be unmolded without problem, providing speed to the online production process, e)- Within the making of the invented material, carbon fiber cloth was incorporated in the pressing stage, this is applied on both sides of the compound covering it, that is, the carbon fiber cloth is placed on the lower matrix, then the coconut powder moistened with the resin is applied and then the other layer of carbon fiber cloth is incorporated with the holes for the metal fastening fitting. This carbon fiber cloth compound increases the resistance by 105 ° C in case of a fire accident and gives one more minute of time to the compound in which it catches fire.

[0009] FORMULATION

[0010] Molded compound 2.5 mm thick, formula per cm2

[0011] Octopus coconut shell (endocarp) d=0.50 gr / ml 0.28 gr.

[0012] Expanded pearls of polvo piolite d=0.30 gr / ml 0.056 gr.

[0013] Epoxy resin 0.224 gr.

Claims

CLAIMS Having thus specially described and determined the nature of the present invention and the manner in which it is to be put into practice, it is declared to be claimed as property and exclusive right:

1. A 50% natural and renewable compound, waterproof, resistant to high temperatures, widely used in industry, combining natural, physical, mechanical and thermal properties, CHARACTERIZED because when solidified it withstands temperatures between 300° C and 405° C and is comprised of coconut shell, expanded pearls, epoxy resin, carbon fiber cloth, where taken to the desired matrix at a temperature of 110° C it is molded and pressed and then cooled to obtain the required piece; 2. The composition of claim No. 1 CHARACTERIZED in that it comprises coconut shell (endocarp) brought to a powder state at a density of 0.50 gr / ml, expanded pearlite (piolite mineral) brought to a powder state at a density of 0.30 gr / ml, epoxy resin (80% in relation to the amount of coconut shell powder to be used), carbon fiber fabric on both sides of the matrix to be used; 3. The process for manufacturing the compound of claim 1, CHARACTERIZED in that it comprises the following steps: mixing the coconut shell in powder state (8 parts) with the expanded pearls also in powder state (2 parts) and the epoxy resin (80% in relation to the amount of coconut shell powder to be used) until a moistened powder without lumps remains, where in the desired matrix a layer of carbon fiber cloth is added in the lower part and another layer in the upper part of the material and it is pressed at a maximum of 1000 kg of pressure with leveling sensors and at a temperature of 110 ° C, and then cooled by means of chiller equipment and the desired piece is obtained.

Citation Information

Patent Citations

  • Heat-insulation bamboo-plastic foamed composite door and window material capable of removing formaldehyde and preparation method thereof

    CN106117801A

  • Ceramic-polymer composite capacitors and manufacturing method

    CN110945612A