Semiconductor device
The semiconductor device addresses internal destruction of the main electrode by using a buffer plate and bonding material to manage thermal deformation, improving durability and reducing series resistance.
Patent Information
- Application Number
- PCT/JP2024/018982
- Authority / Receiving Office
- WO · WO
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2023-05-30
- Filing Date
- 2024-05-23
- Publication Date
- 2024-12-05
AI Technical Summary
Conventional semiconductor devices experience internal destruction of the main electrode due to thermal deformation, leading to increased electrical or thermal series resistance and potential disconnection, especially during power cycle tests.
A semiconductor device design that includes a buffer plate bonded to the main electrode using a buffer bonding material, where the buffer plate's outer edge overlaps or lies outside a virtual annular curve defined by the main electrode's edge, effectively restraining thermal deformation and reducing thermal stress on the main electrode.
This design suppresses internal destruction of the main electrode, enhancing its durability and lifespan by mitigating thermal deformation and stress, thereby maintaining effective bonding and reducing electrical or thermal series resistance.
Smart Images

Figure JP2024018982_05122024_PF_FP_ABST
Abstract
Description
Semiconductor Devices
[0001] The present disclosure relates to semiconductor devices.
[0002] This application claims priority based on Japanese Application No. 2023-089064, filed on May 30, 2023, and incorporates by reference all of the contents of the aforementioned Japanese application.
[0003] As an example of a semiconductor device suitable for a power module, a semiconductor device has been proposed in which a buffer plate is bonded to a main electrode of a semiconductor chip and bonding wires are bonded to the buffer plate.
[0004] Japanese Patent Publication No. 2018-186220 Japanese Patent Publication No. 2017-005037 Japanese Patent Publication No. 2019-057663
[0005] The semiconductor device disclosed herein comprises a semiconductor chip having a semiconductor substrate and a main electrode provided on the semiconductor substrate, a buffer plate having a first thickness, and a buffer bonding material having a second thickness provided between the main electrode and the buffer plate, wherein the main electrode has a first main surface, and when viewed in a plan view from a direction perpendicular to the first main surface, the outer edge of the buffer plate overlaps with a virtual annular first curve that is located inward from the outer edge of the main electrode by the sum of the first thickness and the second thickness, or is outside the first curve.
[0006] FIG. 1 is a top view showing a semiconductor device according to a first embodiment. FIG. 2 is a cross-sectional view showing the semiconductor device according to the first embodiment. FIG. 3 is a top view showing an enlarged view of a silicon carbide substrate and a buffer plate according to the first embodiment. FIG. 4 is a cross-sectional view showing an enlarged view of a silicon carbide substrate, an anode electrode, a buffer bonding material, and a buffer plate according to the first embodiment. FIG. 5 is a top view showing an enlarged view of a silicon carbide substrate, an anode electrode, and a buffer plate according to a modified example of the first embodiment. FIG. 6 is a cross-sectional view showing an enlarged view of a silicon carbide substrate, an anode electrode, a buffer bonding material, and a buffer plate according to a modified example of the first embodiment. FIG. 7 is a top view showing a first example of a planar shape of a buffer plate. FIG. 8 is a top view showing a second example of a planar shape of a buffer plate. FIG. 9 is a top view showing a third example of a planar shape of a buffer plate. FIG. 10 is a top view showing a semiconductor device according to a second embodiment. FIG. 11 is a cross-sectional view showing a semiconductor device according to the second embodiment. FIG. 12 is a cross-sectional view showing a guard ring region of an example of a transistor.
[0007] [Problem to be Solved by the Present Disclosure] In conventional semiconductor devices, failures such as peeling due to internal destruction of the main electrode may occur.
[0008] An object of the present disclosure is to provide a semiconductor device that can suppress internal breakdown of a main electrode.
[0009] [Advantages of the Present Disclosure] According to the present disclosure, internal destruction of the main electrode can be suppressed.
[0010] The embodiments for carrying out the invention are described below.
[0011] [Description of the embodiments of the present disclosure] First, the embodiments of the present disclosure will be listed and described. In the following description, the same or corresponding elements will be denoted by the same reference numerals, and the same description will not be repeated.
[0012] [1] A semiconductor device according to one aspect of the present disclosure includes a semiconductor chip including a semiconductor substrate and a main electrode provided on the semiconductor substrate, a buffer plate having a first thickness, and a buffer bonding material having a second thickness provided between the main electrode and the buffer plate, wherein the main electrode has a first main surface, and in a plan view perpendicular to the first main surface, an outer edge of the buffer plate overlaps with a virtual annular first curve that is located inward from the outer edge of the main electrode by a distance equal to the sum of the first thickness and the second thickness, or is outside the first curve.
[0013] Because the buffer plate is bonded to the main electrode by the buffer bonding material, the thermal deformation of the main electrode can be restrained by the buffer plate. In this case, as described below, in a plan view, the outer edge of the buffer plate overlaps with a virtual annular first curve located inward by the sum of the first thickness and the second thickness from the outer edge of the main electrode, or is outside the first curve, so that the thermal deformation of the main electrode can be more effectively suppressed by the buffer bonding material. Therefore, thermal stress generated in the main electrode due to thermal deformation can be suppressed, and internal destruction of the main electrode can be suppressed.
[0014] Internal breakdown of the main electrode occurs when grain boundary sliding and cracks occurring at the grain boundaries of the crystals that make up the main electrode accumulate due to repeated thermal deformation. Internal breakdown of the main electrode is confirmed, for example, as a decrease in the density of the main electrode or an increase in the thickness of the main electrode. Furthermore, when internal breakdown occurs in the main electrode, the effective bonding area between the main electrode and the components sandwiching it decreases. Therefore, internal breakdown can also be confirmed as an increase in electrical or thermal series resistance.
[0015] Internal breakdown of the main electrode can also occur during a power cycle test. In other words, during a power cycle test, repeated temperature increases and decreases can cause grain boundary sliding, resulting in internal breakdown. For example, in the later stages of a power cycle test, internal breakdown of the main electrode can be observed as breakage or peeling of the main electrode, a sudden increase in electrical resistance or disconnection, or a sudden increase in thermal resistance or thermal runaway. These phenomena become particularly noticeable just before the end of life.
[0016] [2] In [1], in a plan view perpendicular to the first principal surface, an outer edge of the buffer plate may overlap with a virtual annular second curve located inward from the outer edge of the main electrode by half the sum of the first thickness and the second thickness, or may be located outside the second curve. In this case, thermal deformation of the main electrode can be further suppressed by the buffer bonding material.
[0017] [3] In [1] or [2], the semiconductor substrate may have an element region where a semiconductor element is provided and a guard ring region surrounding the element region in a plan view perpendicular to the first main surface, and an outer edge of the buffer plate may be located inside the guard ring region in a plan view perpendicular to the first main surface. In this case, discharge between the buffer plate and the guard ring is suppressed, and a good breakdown voltage is obtained.
[0018] [4] In any of [1] to [3], the outer edge of the buffer plate may have a linear region and a curved region connected to the linear region, the semiconductor substrate may have a single crystal substrate and an epitaxial layer provided on the single crystal substrate and having a third thickness, and the value obtained by dividing the radius of curvature of the curved region by the third thickness may be equal to or greater than 5 and equal to or less than 10. In this case, good withstand voltage and life may be obtained.
[0019] [5] In any one of [1] to [4], an outer edge of the buffer bonding material may overlap the first curved line or be outside the first curved line in a plan view perpendicular to the first main surface. In this case, the main electrode and the buffer plate can be easily bonded firmly.
[0020] [6] In any one of [1] to [5], the main electrode may include an aluminum layer or an aluminum alloy layer, which makes it easier to obtain good electrical conductivity in the main electrode.
[0021] [7] In [6], the first linear expansion coefficient of the semiconductor substrate and the second linear expansion coefficient of the buffer plate may be smaller than the third linear expansion coefficient of the main electrode, and the second linear expansion coefficient may be smaller than the first linear expansion coefficient. In this case, because the third linear expansion coefficient is larger than the first linear expansion coefficient, the main electrode tends to thermally deform more than the semiconductor substrate. However, because the second linear expansion coefficient is smaller than the first linear expansion coefficient, the thermal deformation of the main electrode can be effectively suppressed by the buffer bonding material. Therefore, thermal stress generated in the main electrode due to thermal deformation can be suppressed, and internal destruction of the aluminum layer or aluminum alloy layer included in the main electrode can be suppressed.
[0022] Generally, aluminum or aluminum alloy layers are weaker than other metal components of semiconductor devices in terms of strength and heat resistance. The grain boundary sliding that causes internal destruction of the main electrode is called creep, and the creep onset temperature can be determined by using a temperature 0.4 times the melting point (Tm). This index indicates that creep begins at a lower temperature in aluminum or aluminum alloy layers than in other components. For example, the values of "Tm x 0.4" for aluminum, copper, and nickel are 100°C, 270°C, and 418°C, respectively.
[0023] In particular, when the aluminum or aluminum alloy layer included in the main electrode is formed by sputtering, the grain size of the crystals constituting the aluminum or aluminum alloy layer is small, on the order of a few micrometers, and therefore, grain boundaries exist at high density in the aluminum or aluminum alloy layer.When thermal strain occurs between the layers sandwiching the main electrode due to temperature rise and fall cycles during a power cycle test, grain boundary sliding is likely to occur.
[0024] In contrast, when the second linear expansion coefficient is smaller than the first linear expansion coefficient, the buffer bonding material can effectively suppress thermal deformation of the main electrode, thereby suppressing internal destruction of the aluminum layer or aluminum alloy layer contained in the main electrode.
[0025] [8] In any one of [1] to [7], the buffer bonding material may include a copper sintered body or a silver sintered body. In this case, the main electrode and the buffer plate can be easily bonded firmly.
[0026] [9] A semiconductor device according to another aspect of the present disclosure includes a semiconductor chip including a semiconductor substrate and a main electrode provided on the semiconductor substrate, a buffer plate having a first thickness, and a buffer bonding material provided between the main electrode and the buffer plate and having a second thickness, wherein the main electrode has a first main surface, and in a plan view from a direction perpendicular to the first main surface, an outer edge of the buffer plate overlaps with a virtual annular first curved line that is located inward from the outer edge of the main electrode by a sum of the first thickness and the second thickness, or is located outside the first curved line, and the outer edge of the buffer plate is separated by a linear region and a linear region that is located outside the linear region. a curvature region adjacent to the buffer region, the semiconductor substrate having a single crystal substrate and an epitaxial layer provided on the single crystal substrate and having a third thickness, the radius of curvature of the curvature region divided by the third thickness being 5 to 10, the main electrode including an aluminum layer or an aluminum alloy layer, a first linear expansion coefficient of the semiconductor substrate and a second linear expansion coefficient of the buffer plate being smaller than a third linear expansion coefficient of the main electrode, the second linear expansion coefficient being smaller than the first linear expansion coefficient, and the buffer bonding material including a copper sintered body or a silver sintered body. In this case, thermal stress generated in the main electrode due to thermal deformation is particularly easily suppressed, and internal destruction of the main electrode is particularly easily suppressed.
[0027] [Details of Embodiments of the Present Disclosure] Embodiments of the present disclosure will be described in detail below, but the present embodiments are not limited thereto. Note that, in this specification and drawings, components having substantially the same functional configurations may be denoted by the same reference numerals to avoid redundant description. In this specification and drawings, the X1-X2 direction, the Y1-Y2 direction, and the Z1-Z2 direction are defined as mutually orthogonal directions. The plane including the X1-X2 direction and the Y1-Y2 direction is defined as the XY plane, the plane including the Y1-Y2 direction and the Z1-Z2 direction is defined as the YZ plane, and the plane including the Z1-Z2 direction and the X1-X2 direction is defined as the ZX plane. For convenience, the Z1 direction is defined as the upward direction, and the Z2 direction is defined as the downward direction. Furthermore, in this disclosure, planar view refers to viewing an object from the Z1 side.
[0028] (First Embodiment) A first embodiment will be described. The first embodiment relates to a semiconductor device. FIG. 1 is a top view showing the semiconductor device according to the first embodiment. FIG. 2 is a cross-sectional view showing the semiconductor device according to the first embodiment. FIG. 2 corresponds to a cross-sectional view taken along line II-II in FIG. 1.
[0029] As shown in Figures 1 and 2, the semiconductor device 1 according to the first embodiment mainly includes a heat sink 120, a substrate 110, a terminal 102, a terminal 103, a case 190, a diode 300, and a buffer plate 500.
[0030] The heat sink 120 is, for example, a rectangular plate-like body with a uniform thickness in a plan view. The material of the heat sink 120 is a metal with high thermal conductivity, such as copper (Cu), a copper alloy, aluminum (Al), or an aluminum-silicon-carbon alloy (Al-Si-C alloy). The heat sink 120 is fixed to a cooler or the like using a thermal interface material (TIM) or the like.
[0031] The case 190 is formed, for example, in a frame shape in a plan view, and the outer shape of the case 190 is the same as the outer shape of the heat sink 120. The case 190 is made of an insulating material such as resin. The case 190 has a pair of side walls 191 and 192 facing each other and a pair of end walls 193 and 194 connecting both ends of the side walls 191 and 192. The side walls 191 and 192 are arranged parallel to the ZX plane, and the end walls 193 and 194 are arranged parallel to the YZ plane. The side wall 191 is arranged on the Y1 side of the side wall 192, and the end wall 193 is arranged on the X2 side of the end wall 194.
[0032] Terminal 102 is disposed on the upper surface (surface on the Z1 side) of end wall portion 193, and terminal 103 is disposed on the upper surface (surface on the Z1 side) of end wall portion 194. Terminal 102 and terminal 103 are each made of a metal plate.
[0033] Inside the case 190, the substrate 110 is disposed on the Z1 side of the heat sink 120. The substrate 110 has an insulating substrate 119, a second conductive pattern 112, a third conductive pattern 113, and a conductive layer 115. The first conductive pattern 111, the second conductive pattern 112, the third conductive pattern 113, the fourth conductive pattern 114, and the conductive layer 115 are made of Cu.
[0034] The second conductive pattern 112 and the third conductive pattern 113 are provided on the Z1 side surface of the insulating substrate 119. The conductive layer 115 is provided on the Z2 side surface of the insulating substrate 119. The conductive layer 115 is bonded to the heat sink 120 by a bonding material 131. The bonding material 131 may be a solder material or a sintered bonding material. When the bonding material 131 is a sintered bonding material, operation at a higher temperature, near the melting point of the solder or higher, is possible.
[0035] As shown in FIG. 2 , the diode 300 mainly includes a silicon carbide substrate 310 , an anode electrode 332 , and a cathode electrode 333 .
[0036] Silicon carbide substrate 310 has main surface 310A and main surface 310B opposite main surface 310A. Main surface 310A is on the Z1 side of main surface 310B. Silicon carbide substrate 310 has, for example, a rectangular parallelepiped shape. Main surfaces 310A and 310B are surfaces parallel to the XY plane. Silicon carbide substrate 310 has a silicon carbide single crystal substrate 311 and a silicon carbide epitaxial layer 312 provided on silicon carbide single crystal substrate 311. Main surface 310A is on silicon carbide epitaxial layer 312, and main surface 310B is on silicon carbide single crystal substrate 311.
[0037] The anode electrode 332 is provided on the main surface 310A, and the cathode electrode 333 is provided on the main surface 310B. The anode electrode 332 has a main surface 332B facing the main surface 310A and a main surface 332A opposite the main surface 332B. The main surface 332A is on the Z1 side of the main surface 332B. The diode 300 is provided on the third conductive pattern 113. The anode electrode 332 includes, for example, an aluminum layer. Instead of the aluminum layer, the anode electrode 332 may include an aluminum alloy layer such as an aluminum-silicon alloy (Al-Si alloy) or an Al-Si-Cu alloy. The cathode electrode 333 includes an ohmic layer and a bonding layer provided on the ohmic layer. The ohmic layer includes, for example, nickel or a nickel alloy. Nickel or a nickel alloy has good contact resistance with silicon carbide. The bonding layer includes a nickel layer. The bonding layer may further include a gold layer or a silver layer provided on the nickel layer. When the cathode electrode 333 includes a bonding layer, good bonding properties are obtained between the cathode electrode 333 and the third conductive pattern 113. The cathode electrode 333 is bonded to the third conductive pattern 113 using a bonding material 133 such as a silver sintered body or a copper sintered body. The diode 300 is an example of a semiconductor chip. The silicon carbide substrate 310 is an example of a semiconductor substrate. The anode electrode 332 is an example of a main electrode. The main surface 332A is an example of a first main surface.
[0038] The buffer plate 500 is, for example, a laminated material having a first copper layer 510, an iron-nickel alloy layer 520, and a second copper layer 530. The iron-nickel alloy layer 520 is provided on the Z1 side of the first copper layer 510, and the second copper layer 530 is provided on the Z1 side of the iron-nickel alloy layer 520. That is, the iron-nickel alloy layer 520 is provided on the first copper layer 510, and the second copper layer 530 is provided on the iron-nickel alloy layer 520. The iron-nickel alloy layer 520 is, for example, a layer of an iron-nickel alloy containing 36% by mass of nickel. The iron-nickel alloy layer 520 may contain approximately 0.7% by mass of manganese. The iron-nickel alloy layer 520 may contain approximately 17% by mass of cobalt. The material of the iron-nickel alloy layer 520 may be Invar (registered trademark). The buffer plate 500 has a thickness T1. The thickness T1 is, for example, not less than 0.05 mm and not more than 0.25 mm. For example, the thickness T1 of the buffer plate 500 is smaller than the thickness of the diode 300. The buffer plate 500 is provided on the anode electrode 332. The first copper layer 510 is bonded to the anode electrode 332 using a buffer bonding material 135 such as a silver sintered body or a copper sintered body. The buffer bonding material 135 has a thickness T2. The thickness T2 is, for example, not less than 0.02 mm and not more than 0.10 mm. The thickness T1 is an example of a first thickness. The thickness T2 is an example of a second thickness.
[0039] The silicon carbide substrate 310 has a first linear expansion coefficient ρ1, the buffer plate 500 has a second linear expansion coefficient ρ2, and the anode electrode 332 has a third linear expansion coefficient ρ3. Unless otherwise specified, the linear expansion coefficient in this disclosure refers to the linear expansion coefficient in a direction parallel to the main surface 310A at 25°C. Furthermore, unless otherwise specified, the linear expansion coefficient in this disclosure refers to the linear expansion coefficient when the silicon carbide substrate 310, the buffer plate 500, and the anode electrode 332 are unbonded and the silicon carbide substrate 310, the buffer plate 500, and the anode electrode 332 are separated into a single body. The first linear expansion coefficient ρ1 and the second linear expansion coefficient ρ2 are smaller than the third linear expansion coefficient ρ3. The second linear expansion coefficient ρ2 may be larger or smaller than the first linear expansion coefficient ρ1, but when the difference between the first linear expansion coefficient ρ1 and the second linear expansion coefficient ρ2 is small, thermal stress acting on the anode electrode 332 is easily suppressed. When the second linear expansion coefficient ρ2 is smaller than the first linear expansion coefficient ρ1, the life is more likely to be extended than when the second linear expansion coefficient ρ2 is larger than the first linear expansion coefficient ρ1. For example, when the first linear expansion coefficient ρ1 is 4.0×10-6 / °C, whereas the second linear expansion coefficient ρ2 is 1.2 × 10 -6 / ℃ or more 3.9 x 10 -6 / °C or less. In this case, the value of "ρ2 - ρ1" is -2.8 × 10 -6 / ℃ or more -0.1 x 10 -6 / °C or less, and a longer life is likely to be obtained than when the value of "ρ2 - ρ1" is positive. The linear expansion coefficient of iron-nickel alloy is 1.2 × 10 -6 / °C, and the linear expansion coefficient of copper is 16.5 × 10 -6 / °C, and the linear expansion coefficient of aluminum is 23.1 × 10 -6 / °C. When the anode electrode 332 is made of aluminum, the third linear expansion coefficient ρ3 is about 23.1×10 -6 / ℃.
[0040] The semiconductor device 1 further includes wires 162, 165, and 166. The number of each of the wires 162, 165, and 166 is not limited, and may be one, or two or more.
[0041] Wire 162 connects second copper layer 530 of buffer plate 500 to second conductive pattern 112. Wire 165 connects second conductive pattern 112 to terminal 102. Wire 166 connects third conductive pattern 113 to terminal 103. Wires 162, 165, and 166 are, for example, copper wires. Each of wires 162, 165, and 166 has a diameter of, for example, 100 μm or more and 400 μm or less. Wires 162, 165, and 166 are bonded by, for example, ultrasonic bonding.
[0042] Here, the positional relationship between silicon carbide substrate 310, anode electrode 332, buffer bonding material 135, and buffer plate 500 will be described. Fig. 3 is an enlarged top view of silicon carbide substrate 310 and buffer plate 500 in the first embodiment. Fig. 4 is an enlarged cross-sectional view of silicon carbide substrate 310, anode electrode 332, buffer bonding material 135, and buffer plate 500 in the first embodiment. Fig. 4 corresponds to a cross-sectional view taken along line IV-IV in Fig. 3 .
[0043] In plan view, silicon carbide substrate 310 has element region 21 and termination region (ineffective region) 22 surrounding element region 21. For example, silicon carbide single crystal substrate 311 has n-type conductivity, and silicon carbide epitaxial layer 312 has n-type layer 313 and multiple annular p-type layers 314 formed on the surface layer portion of n-type layer 313. The multiple p-type layers 314 are arranged in multiple layers, with parts of n-type layer 313 between adjacent p-type layers 314.
[0044] The element region 21 includes a portion of the n-type layer 313 that is surrounded by a plurality of p-type layers 314, and an anode electrode 332 is provided on the n-type layer 313 within the element region 21. The element region 21 includes a Schottky barrier diode 30 as a semiconductor element.
[0045] Termination region 22 includes guard ring region 31, and guard ring region 31 includes a plurality of p-type layers 314. Each of the plurality of p-type layers 314 is a conductive region that acts as a guard ring.
[0046] The guard ring, also known as a breakdown voltage termination structure, is used to obtain "breakdown voltage," which is one of the important operating characteristics of a power device. By providing the guard ring on the outer periphery of the active region on the upper surface of silicon carbide substrate 310, it becomes possible to stably maintain high breakdown voltage.
[0047] The guard ring region 31 has linear regions 32 and curvature regions 33 connected to the linear regions 32. Specifically, four linear regions 32 and four curvature regions 33 are alternately arranged to form the annular guard ring region 31. The curvature regions 33 are formed along the arc of a circle with a center C1. The curvature regions 33 have a radius of curvature R1. The radius of curvature R1 is, for example, not less than 50 μm and not more than 1260 μm.
[0048] When the guard ring region 31 includes multiple p-type layers 314, the multiple p-type layers 314 are arranged with a gap between them. Specifically, each of the multiple p-type layers 314 has a linear region 32 and a curved region 33. The linear regions 32 of the multiple p-type layers 314 are arranged parallel to each other in a planar view. The curved regions 33 of the multiple p-type layers 314 are arranged along arcs of concentric circles having a center C1 and different radii. The p-type impurity concentrations of the multiple p-type layers 314 may be the same or different. For example, the impurity concentration of the p-type layer 314 on the outer periphery of the multiple p-type layers 314 may be lower than the impurity concentration of the p-type layer 314 on the inner periphery.
[0049] The anode electrode 332 is provided inside the innermost p-type layer 314 in a plan view. In a plan view, the anode electrode 332 is separated from all of the p-type layers 314. For example, the shape of the outer edge 332E of the anode electrode 332 is similar to the shape of the inner edge 314F of the innermost p-type layer 314. The distance between the outer edge 332E of the anode electrode 332 and the inner edge 314F of the innermost p-type layer 314 is, for example, 15 μm or more and 50 μm or less. The distance between adjacent p-type layers 314 is, for example, 5 μm or more and 10 μm or less.
[0050] In a plan view, an outer edge 135E of the buffer bonding material 135 coincides with an outer edge 332E of the anode electrode 332. The entire lower surface of the buffer bonding material 135 and the entire upper surface of the anode electrode 332 are in contact with each other. In addition, in a plan view, an outer edge 500E of the buffer plate 500 coincides with the outer edge 332E of the anode electrode 332 and the outer edge 135E of the buffer bonding material 135. The entire lower surface of the buffer plate 500 and the entire upper surface of the buffer bonding material 135 are in contact with each other.
[0051] Focusing on thermal deformation of silicon carbide substrate 310 and anode electrode 332, because first linear expansion coefficient ρ1 is smaller than third linear expansion coefficient ρ3, anode electrode 332 may thermally deform to a greater extent than silicon carbide substrate 310. Because silicon carbide substrate 310 and anode electrode 332 are firmly bonded to each other, the greater the difference between first linear expansion coefficient ρ1 and third linear expansion coefficient ρ3, the greater the thermal stress acting on anode electrode 332, making it more likely that internal destruction will occur in anode electrode 332.
[0052] Meanwhile, the buffer plate 500 is joined to the anode electrode 332 by the buffer bonding material 135, and thermal deformation of the anode electrode 332 is restricted by the buffer plate 500. In this embodiment, an outer edge 500E of the buffer plate 500 coincides with an outer edge 332E of the anode electrode 332 in a plan view. Therefore, thermal deformation of the anode electrode 332 can be significantly suppressed by the buffer plate 500 and the silicon carbide substrate 310. Therefore, according to this embodiment, thermal stress occurring in the anode electrode 332 due to thermal deformation can be suppressed, and internal destruction of the anode electrode 332 can be suppressed.
[0053] Because the anode electrode 332 includes an aluminum layer or an aluminum alloy layer, good electrical conductivity is easily achieved in the anode electrode 332. Meanwhile, the first linear expansion coefficient ρ1 of the silicon carbide substrate 310 and the second linear expansion coefficient ρ2 of the buffer plate 500 are smaller than the third linear expansion coefficient ρ3 of the anode electrode 332, and the second linear expansion coefficient ρ2 is smaller than the first linear expansion coefficient ρ1. In this case, the anode electrode 332 tends to thermally deform to a greater extent than the silicon carbide substrate 310. However, because the second linear expansion coefficient ρ2 is smaller than the first linear expansion coefficient ρ1, the thermal deformation of the anode electrode 332 can be effectively suppressed by the buffer bonding material 135. Therefore, thermal stress generated in the anode electrode 332 due to thermal deformation can be suppressed, and internal destruction of the anode electrode 332 can be suppressed.
[0054] When the buffer bonding material 135 contains a copper sintered body or a silver sintered body, the anode electrode 332 and the buffer plate 500 can be easily bonded firmly to each other.
[0055] In this embodiment, by bonding the wire 162 to the buffer plate 500, the wire 162 can be electrically connected to the anode electrode 332 via the buffer plate 500. Therefore, even if ultrasonic bonding is used to bond the wire 162, damage to the diode 300 can be suppressed. If the wire 162 is a copper wire, it is easy to bond the wire 162 to the second copper layer 530 of the buffer plate 500, and it is also easy to obtain low electrical resistance for the wire 162.
[0056] The buffer plate 500 may not include the first copper layer 510 and the second copper layer 530. In other words, the buffer plate 500 may be made of an iron-nickel alloy layer 520 such as Invar.
[0057] A plurality of diodes 300 may be provided on the third conductive pattern 113. In this case, the plurality of diodes 300 are electrically connected in parallel to one another.
[0058] (Modification of First Embodiment) A modification of the first embodiment will be described. The modification differs from the first embodiment mainly in the arrangement of the buffer bonding material 135 and the buffer plate 500. Fig. 5 is an enlarged top view of the silicon carbide substrate 310, the anode electrode 332, and the buffer plate 500 in the modification of the first embodiment. Fig. 6 is an enlarged cross-sectional view of the silicon carbide substrate 310, the anode electrode 332, the buffer bonding material 135, and the buffer plate 500 in the modification of the first embodiment. Fig. 6 corresponds to a cross-sectional view taken along line VI-VI in Fig. 5.
[0059] In the modification of the first embodiment, in a plan view, an outer edge 500E of the buffer plate 500 overlaps with a virtual annular first curve 41 that is located inward by the sum of thicknesses T1 and T2 from an outer edge 332E of the anode electrode 332. The configuration of the modification is the same as that of the first embodiment.
[0060] As in the first embodiment, this modification also makes it possible to suppress the thermal stress that occurs in the anode electrode 332 due to thermal deformation, and to suppress internal destruction of the anode electrode 332 .
[0061] Even if the outer edge 500E is outside the first curve 41 in plan view, it is possible to suppress thermal stress occurring in the anode electrode 332 due to thermal deformation and suppress internal destruction of the anode electrode 332. In plan view, the outer edge 500E may overlap with the imaginary annular second curve 42 located inward from the outer edge 332E by half the sum of the thickness T1 and the thickness T2, or may be located outside the second curve 42. In plan view, the outer edge 500E may overlap with the imaginary annular third curve 43 located inward from the outer edge 332E by one-fifth the sum of the thickness T1 and the thickness T2, or may be located outside the third curve 43.
[0062] On the other hand, when the outer edge 500E is located inside the first curve 41, a large portion of the anode electrode 332 is not restrained from thermal deformation by the buffer plate 500. This causes large thermal stress to act locally on the anode electrode 332, making it more likely to suffer internal damage. Note that although the thicknesses of the buffer plate 500 and the buffer bonding material 135 can be determined independently, internal damage to the anode electrode 332 is more likely to be prevented when the thickness of the buffer bonding material 135 is smaller than the thickness of the buffer plate 500.
[0063] Even if the outer edge 500E is outside the outer edge 332E in plan view, thermal stress generated in the anode electrode 332 due to thermal deformation can be suppressed, and internal destruction of the anode electrode 332 can be suppressed. However, if the outer edge 500E overlaps the p-type layer 314 in plan view, a large voltage, for example, several hundred to several thousand volts, can be generated between the buffer plate 500 and the p-type layer 314, which may result in discharge. The occurrence of discharge leads to a decrease in the breakdown voltage. If the outer edge 500E is inside the inner edge 314F of the innermost p-type layer 314 in plan view, such a decrease in the breakdown voltage can be suppressed.
[0064] In the first embodiment and its modified examples, the inventors of the present application have confirmed through an internal stress analysis of the semiconductor device 1 using the finite element method that thermal deformation of the anode electrode 332 can be suppressed and internal destruction of the anode electrode 332 can be suppressed. Furthermore, in a power cycle test using an actually fabricated sample, internal destruction occurred in the anode electrode 332 when the outer edge 500E of the buffer plate 500 was inside the first curve 41 in a plan view.
[0065] In addition, when viewed from above, the outer edge 135E of the buffer bonding material 135 overlaps the first curve 41 or is located outside the first curve 41, which makes it easier to firmly bond the anode electrode 332 and the buffer plate 500 together.
[0066] Next, the planar shape of the buffer plate 500 will be described. Fig. 7 is a top view showing a first example of the planar shape of the buffer plate 500. Fig. 8 is a top view showing a second example of the planar shape of the buffer plate 500. Fig. 9 is a top view showing a third example of the planar shape of the buffer plate 500.
[0067] The outer edge 332E of the anode electrode 332 has straight line regions 52 and curved regions 53 that connect to the straight line regions 52. Specifically, four straight line regions 52 and four curved regions 53 are arranged alternately. The curvature regions 53 are formed along the arcs of a circle with a center C2. The curvature regions 53 have a radius of curvature R2.
[0068] The outer edge 500E of the buffer plate 500 has straight regions 62 and curvature regions 63 that connect to the straight regions 62. Specifically, four straight regions 62 and four curvature regions 63 are arranged alternately. The curvature regions 63 are formed along the arcs of a circle with a center C3. The curvature regions 63 have a radius of curvature R3.
[0069] 7, the linear region 52 and the linear region 62 overlap in a plan view, and the radius of curvature R3 is greater than the radius of curvature R2. In this case, depending on the difference between the radius of curvature R3 and the radius of curvature R2, the outer edge 500E may be located inside the first curved line 41.
[0070] 8 , linear region 52 and linear region 62 overlap in plan view, and radius of curvature R3 is smaller than radius of curvature R2. In this case, depending on the difference between radius of curvature R3 and radius of curvature R2, outer edge 500E may overlap p-type layer 314 in plan view.
[0071] 9 , in a plan view, the point of curvature region 53 that is farthest from linear region 52 and the point of curvature region 63 that is farthest from linear region 62 overlap, and radius of curvature R3 is smaller than radius of curvature R2. In this case, depending on the difference between radius of curvature R3 and radius of curvature R2, outer edge 500E may be located inside first curve 41.
[0072] In any of the first, second, and third examples, if the conditions of the first embodiment or its modified examples are satisfied in all of the four straight regions 52 and four curvature regions 63, internal breakdown of the anode electrode 332 is particularly likely to be suppressed. However, the above conditions do not need to be satisfied in areas where there is a loose thermal design margin due to factors such as the in-plane temperature distribution of the diode 300 during operation of the semiconductor device 1. If the above conditions are satisfied even partially, internal breakdown of the anode electrode 332 can be suppressed in those areas.
[0073] As described above, for example, the shape of the outer edge 332E of the anode electrode 332 is similar to the shape of the inner edge 314F of the innermost p-type layer 314. Therefore, the radius of curvature R2 depends on the radius of curvature R1 of the curvature region 33. The larger the radius of curvature R1, the more the electric field concentration is alleviated, resulting in a higher breakdown voltage. On the other hand, the larger the radius of curvature R1, the smaller the area of the element region 21, resulting in a lower on-current. For this reason, the radius of curvature R1 is determined depending on the required breakdown voltage and on-current. The thickness of the silicon carbide epitaxial layer 312 is also determined depending on the required breakdown voltage.
[0074] Taking these factors into consideration, the inventors of the present application investigated the occurrence of discharge and the lifetime when the radius of curvature R3 of the buffer plate 500 was changed for various thicknesses T3 of the silicon carbide epitaxial layer 312. As a result, in samples in which the thickness T3 of the silicon carbide epitaxial layer 312 was set to 10 μm in order to obtain a withstand voltage of 1200 V, discharge occurrence was suppressed and an excellent lifetime was obtained when the radius of curvature R3 was 50 μm or more and 175 μm or less. Furthermore, in samples in which the thickness T3 of the silicon carbide epitaxial layer 312 was set to 15 μm in order to obtain a withstand voltage of 1700 V, discharge occurrence was suppressed and an excellent lifetime was obtained when the radius of curvature R3 was 75 μm or more and 150 μm or less. In samples in which the thickness T3 of the silicon carbide epitaxial layer 312 was set to 30 μm in order to obtain a breakdown voltage of 3300 V, when the radius of curvature R3 was 150 μm or more and 325 μm or less, discharge was suppressed and an excellent life was obtained.
[0075] From these results, the inventors of the present application focused on the ratio of the radius of curvature R3 of buffer plate 500 to the thickness T3 of silicon carbide epitaxial layer 312, and found that if the value (R3 / T3) obtained by dividing the radius of curvature R3 by the thickness T3 is 5 or more and 10 or less, discharge occurrence can be suppressed and a good life can be obtained. In other words, if the value (R3 / T3) is 5 or more and 10 or less, a good breakdown voltage and life can be obtained. The value (R3 / T3) may also be 6 or more and 9 or less.
[0076] Second Embodiment Next, a second embodiment will be described. The second embodiment differs from the first embodiment mainly in that a transistor is included. FIG. 10 is a top view showing a semiconductor device according to the second embodiment. FIG. 11 is a cross-sectional view showing the semiconductor device according to the second embodiment. FIG. 11 corresponds to a cross-sectional view taken along line XI-XI in FIG. 10.
[0077] As shown in Figures 10 and 11, the semiconductor device 2 of the second embodiment mainly has a heat sink 120, a substrate 110, terminals 101, 102, 103, a case 190, a transistor 200, a diode 300, a buffer plate 400, and a buffer plate 500.
[0078] Terminals 101 and 102 are arranged on the upper surface (surface on the Z1 side) of end wall portion 193, and terminal 103 is arranged on the upper surface (surface on the Z1 side) of end wall portion 194. For example, terminal 102 is arranged on the Y2 side of terminal 101. Terminals 101, 102, and 103 are each made of a metal plate.
[0079] The substrate 110 has an insulating substrate 119, a first conductive pattern 111, a second conductive pattern 112, a third conductive pattern 113, a fourth conductive pattern 114, and a conductive layer 115. The first conductive pattern 111, the second conductive pattern 112, the third conductive pattern 113, the fourth conductive pattern 114, and the conductive layer 115 are made of Cu.
[0080] The first conductive pattern 111, the second conductive pattern 112, the third conductive pattern 113, and the fourth conductive pattern 114 are provided on the Z1 side surface of the insulating substrate 119. The conductive layer 115 is provided on the Z2 side surface of the insulating substrate 119.
[0081] As shown in FIG. 11 , the transistor 200 mainly includes a silicon carbide substrate 210 , a gate electrode 231 , a source electrode 232 , and a drain electrode 233 .
[0082] The silicon carbide substrate 210 has a main surface 210A and a main surface 210B opposite to the main surface 210A. The main surface 210A is on the Z1 side of the main surface 210B. The silicon carbide substrate 210 has, for example, a rectangular parallelepiped shape. The main surfaces 210A and 210B are surfaces parallel to the XY plane. The silicon carbide substrate 210 has a silicon carbide single crystal substrate 211 and a silicon carbide epitaxial layer 212 provided on the silicon carbide single crystal substrate 211. The main surface 210A is on the silicon carbide epitaxial layer 212, and the main surface 210B is on the silicon carbide single crystal substrate 211.
[0083] The gate electrode 231 and the source electrode 232 are provided on the principal surface 210A, and the drain electrode 233 is provided on the principal surface 210B. The source electrode 232 has a principal surface 232B facing the principal surface 210A and a principal surface 232A opposite the principal surface 232B. The principal surface 232A is on the Z1 side of the principal surface 232B. The transistor 200 is provided on the fourth conductive pattern 114. The gate electrode 231 and the source electrode 232 include, for example, an aluminum layer. The gate electrode 231 and the source electrode 232 may include an aluminum alloy layer such as an Al-Si alloy or an Al-Si-Cu alloy instead of the aluminum layer. The drain electrode 233 has an ohmic layer and a bonding layer provided on the ohmic layer. The ohmic layer includes, for example, nickel or a nickel alloy. Nickel or a nickel alloy has good contact resistance with silicon carbide. The bonding layer includes a nickel layer. The bonding layer may further include a gold layer or a silver layer provided on the nickel layer. The drain electrode 233 includes a bonding layer, thereby achieving good bonding between the drain electrode 233 and the fourth conductive pattern 114. The drain electrode 233 is bonded to the fourth conductive pattern 114 using a bonding material 132 such as a silver sintered body or a copper sintered body. The transistor 200 is an example of a semiconductor chip. The silicon carbide substrate 210 is an example of a semiconductor substrate. The source electrode 232 is an example of a main electrode. The main surface 232A is an example of a first main surface.
[0084] The buffer plate 400 is, for example, a laminated material having a first copper layer 410, an iron-nickel alloy layer 420, and a second copper layer 430. The iron-nickel alloy layer 420 is provided on the Z1 side of the first copper layer 410, and the second copper layer 430 is provided on the Z1 side of the iron-nickel alloy layer 420. That is, the iron-nickel alloy layer 420 is provided on the first copper layer 410, and the second copper layer 430 is provided on the iron-nickel alloy layer 420. The iron-nickel alloy layer 420 is, for example, an iron-nickel alloy layer containing 36% by mass of nickel. The iron-nickel alloy layer 420 may contain approximately 0.7% by mass of manganese. The iron-nickel alloy layer 420 may contain approximately 17% by mass of cobalt. The material of the iron-nickel alloy layer 420 may be Invar. The buffer plate 400 has a thickness T4. The thickness T4 is, for example, not less than 0.05 mm and not more than 0.25 mm. For example, the thickness T4 of the buffer plate 400 is smaller than the thickness of the transistor 200. The buffer plate 400 is provided on the source electrode 232. The first copper layer 410 is bonded to the source electrode 232 using a buffer bonding material 134 such as a silver sintered body or a copper sintered body. The buffer bonding material 134 has a thickness T5. The thickness T5 is, for example, not less than 0.02 mm and not more than 0.10 mm. The thickness T4 is an example of a first thickness. The thickness T5 is an example of a second thickness.
[0085] The silicon carbide substrate 210 has a first linear expansion coefficient ρ1', the buffer plate 400 has a second linear expansion coefficient ρ2', and the source electrode 232 has a third linear expansion coefficient ρ3'. Unless otherwise specified, the linear expansion coefficient in this disclosure refers to the linear expansion coefficient in a direction parallel to the main surface 210A at 25°C. Furthermore, unless otherwise specified, the linear expansion coefficient in this disclosure refers to the linear expansion coefficient when the silicon carbide substrate 210, the buffer plate 400, and the source electrode 232 are released from their bonded state and are taken as a single unit. The first linear expansion coefficient ρ1' and the second linear expansion coefficient ρ2' are smaller than the third linear expansion coefficient ρ3'. The second linear expansion coefficient ρ2' may be greater or smaller than the first linear expansion coefficient ρ1', but when the difference between the first linear expansion coefficient ρ1' and the second linear expansion coefficient ρ2' is small, thermal stress applied to the source electrode 232 is easily suppressed. When the second linear expansion coefficient ρ2′ is smaller than the first linear expansion coefficient ρ1′, the life is more likely to be extended than when the second linear expansion coefficient ρ2′ is larger than the first linear expansion coefficient ρ1′. For example, when the first linear expansion coefficient ρ1′ is 4.0×10 -6 / °C, while the second linear expansion coefficient ρ2' is 1.2 × 10 -6 / ℃ or more 3.9 x 10 -6 / °C or less. In this case, the value of "ρ2' - ρ1'" is -2.8 × 10 -6 / ℃ or more -0.1 x 10 -6 / °C or less, and a longer life is likely to be obtained than when the value of "ρ2' - ρ1'" is positive. When the source electrode 232 is made of aluminum, the third linear expansion coefficient ρ3' is 23.1 × 10 -6 / ℃.
[0086] The semiconductor device 2 further includes wires 161, 162, 163, 164, 165, and 166. The number of each of the wires 161, 162, 163, 164, 165, and 166 is not limited, and may be one, or two or more.
[0087] Wire 161 connects gate electrode 231 of transistor 200 to first conductive pattern 111. Wire 162 connects second copper layer 430 of buffer plate 400 to second conductive pattern 112. Wire 163 connects third conductive pattern 113 to fourth conductive pattern 114. Wire 164 connects first conductive pattern 111 to terminal 101. Wire 165 connects second conductive pattern 112 to terminal 102. Wire 166 connects anode electrode 332 of diode 300 to terminal 103. Wires 161, 162, 163, 164, 165, and 166 are, for example, copper wires. Each of wires 161, 162, 163, 164, 165, and 166 has a diameter of, for example, 100 μm or more and 400 μm or less. The wires 161, 162, 163, 164, 165 and 166 are bonded by, for example, ultrasonic bonding.
[0088] In a plan view, the outer edge of the buffer bonding material 134 coincides with the outer edge of the source electrode 232. The entire lower surface of the buffer bonding material 134 and the entire upper surface of the source electrode 232 are in contact with each other. In addition, in a plan view, the outer edge of the buffer plate 400 coincides with the outer edge of the source electrode 232 and the outer edge of the buffer bonding material 134. The entire lower surface of the buffer plate 400 and the entire upper surface of the buffer bonding material 134 are in contact with each other.
[0089] Other configurations of the second embodiment, such as the configurations of the diode 300 and the buffer plate 500, are the same as those of the first embodiment.
[0090] Focusing on thermal deformation of silicon carbide substrate 210 and source electrode 232, because first linear expansion coefficient ρ1' is smaller than third linear expansion coefficient ρ3', source electrode 232 may thermally deform more than silicon carbide substrate 210. Because silicon carbide substrate 210 and source electrode 232 are firmly bonded to each other, the greater the difference between first linear expansion coefficient ρ1' and third linear expansion coefficient ρ3', the greater the thermal stress acting on source electrode 232, making it more likely that internal breakdown will occur in source electrode 232.
[0091] On the other hand, the buffer plate 400 is joined to the source electrode 232 by the buffer bonding material 134, and thermal deformation of the source electrode 232 is restrained by the buffer plate 400. In this embodiment, the outer edge of the buffer plate 400 coincides with the outer edge of the source electrode 232 in a plan view. Therefore, thermal deformation of the source electrode 232 can be significantly suppressed by the buffer bonding material 134. Therefore, according to this embodiment, thermal stress generated in the source electrode 232 due to thermal deformation can be suppressed, and internal destruction of the source electrode 232 can be suppressed.
[0092] As in the modified example of the first embodiment, in a plan view, the outer edge of the buffer plate 400 may overlap with a virtual annular first curve located inward by the sum of the thickness T4 and the thickness T5 from the outer edge of the source electrode 232, or may be outside the first curve, thereby suppressing thermal stress occurring in the source electrode 232 due to thermal deformation and suppressing internal destruction of the source electrode. In a plan view, the outer edge of the buffer plate 400 may overlap with a virtual annular second curve located inward by half the sum of the thickness T4 and the thickness T5 from the outer edge of the source electrode 232, or may be outside the second curve. In a plan view, the outer edge of the buffer plate 400 may overlap with a virtual annular third curve located inward by one-fifth the sum of the thickness T4 and the thickness T5 from the outer edge of the source electrode 232, or may be outside the third curve.
[0093] Even if the outer edge of the buffer plate 400 is outside the outer edge of the source electrode 232 in plan view, thermal stress generated in the source electrode 232 due to thermal deformation can be suppressed, and internal breakdown of the source electrode 232 can be suppressed. However, if the outer edge of the buffer plate 400 overlaps with the p-type layer constituting the guard ring provided in the silicon carbide epitaxial layer 212 in plan view, a large voltage, for example, a voltage of several hundred volts to several thousand volts, can be generated between the buffer plate 400 and the p-type layer, which may result in discharge. The occurrence of discharge leads to a decrease in the breakdown voltage. If the outer edge of the buffer plate 400 is inside the inner edge of the innermost p-type layer in plan view, such a decrease in the breakdown voltage can be suppressed.
[0094] As with the diode 300, when the outer edge of the buffer bonding material 134 overlaps the first curve or is outside the first curve in a plan view, the source electrode 232 and the buffer plate 400 can be easily bonded firmly.
[0095] As in diode 300, if the radius of curvature of the curvature region of buffer plate 400 is R4, then when the value (R4 / T6) obtained by dividing radius of curvature R4 by thickness T6 of silicon carbide epitaxial layer 212 is 5 or greater and 10 or less, discharge occurrence is suppressed and an excellent lifespan is obtained. The value (R4 / T6) may also be 6 or greater and 9 or less.
[0096] It is also possible that the gate electrode 231 is located outside the source electrode 232 in a plan view, and the outer edge of the buffer plate 400 is located on the outer edge of the source electrode 232, but in this case, the buffer plate 400 is not in electrical or mechanical contact with the gate electrode 231. In this case, the outer edge of the buffer plate 400 may be located inside the inner edge of the innermost p-type layer among the p-type layers that make up the guard ring in a plan view.
[0097] Because the source electrode 232 includes an aluminum layer or an aluminum alloy layer, good conductivity is easily achieved in the source electrode 232. Meanwhile, the first linear expansion coefficient ρ1' of the silicon carbide substrate 210 and the second linear expansion coefficient ρ2' of the buffer plate 400 are smaller than the third linear expansion coefficient ρ3' of the source electrode 232, and the second linear expansion coefficient ρ2' is smaller than the first linear expansion coefficient ρ1'. In this case, the source electrode 232 tends to thermally deform to a greater extent than the silicon carbide substrate 210. However, because the second linear expansion coefficient ρ2' is smaller than the first linear expansion coefficient ρ1', the thermal deformation of the source electrode 232 can be effectively suppressed by the buffer bonding material 134. Therefore, thermal stress generated in the source electrode 232 due to thermal deformation can be suppressed, and internal destruction of the source electrode 232 can be suppressed.
[0098] When the buffer bonding material 134 contains a copper sintered body or a silver sintered body, the source electrode 232 and the buffer plate 400 can be easily bonded firmly to each other.
[0099] In this embodiment, by bonding the wire 162 to the buffer plate 400, the wire 162 can be electrically connected to the source electrode 232 via the buffer plate 400. Therefore, even if ultrasonic bonding is used to bond the wire 162, damage to the transistor 200 can be suppressed. If the wire 162 is a copper wire, it is easy to bond the wire 162 to the second copper layer 430 of the buffer plate 400, and it is also easy to obtain low electrical resistance for the wire 162.
[0100] The buffer plate 400 may not include the first copper layer 410 and the second copper layer 430. In other words, the buffer plate 400 may be made of an iron-nickel alloy layer 420 such as Invar.
[0101] A plurality of transistors 200 may be provided on the fourth conductive pattern 114. In this case, the plurality of transistors 200 are electrically connected in parallel to one another.
[0102] In the present disclosure, an aluminum alloy layer may be used instead of the aluminum layer. Furthermore, the material used for the buffer bonding material is not limited. For example, the buffer bonding material may be made of a sintered body of an intermetallic compound containing copper, silver, nickel, or copper and tin. The sintered body of the intermetallic compound containing copper and tin can be obtained, for example, by transient liquid phase sintering.
[0103] The guard ring region 31 of the diode 300 includes a p-type layer 314 disposed electrically between the anode electrode 332 and the p-type layer 314 with an n-type layer 313 sandwiched therebetween. For example, even if a p-type layer is present outside the anode electrode 332 in a plan view, the p-type layer is not included in the guard ring region 31 as long as the p-type layer is electrically connected to the anode electrode 332.
[0104] The guard ring region of transistor 200 includes a p-type layer disposed with an n-type layer electrically sandwiched between it and source electrode 232. For example, even if a p-type layer is located outside source electrode 232 in plan view, the p-type layer is not included in the guard ring region as long as the p-type layer is electrically connected to source electrode 232.
[0105] 12 is a cross-sectional view showing a guard ring region of an example of a transistor 600. The transistor 600 shown in FIG. 12 mainly includes a conductive silicon carbide single crystal substrate 611, a silicon carbide epitaxial layer 612, a gate electrode 622, a source contact electrode 623, a drain electrode 624, and an insulating film 621.
[0106] The silicon carbide epitaxial layer 612 has an n-type layer 613, a plurality of p-wells 616, a plurality of n-type layers 617, a plurality of p-type layers 618, a plurality of p-type layers 614, and a p-type layer 615. The p-well 616 is formed on the surface of the n-type layer 613, and the n-type layer 617 and the p-type layer 618 are formed on the surface of the p-well. The n-type layer 617 is formed so as to surround the p-type layer 618 in a plan view. The p-type layer 618 is in contact with the p-well 616.
[0107] The p-type layer 615 is formed in a ring shape on the surface of the n-type layer 613 so as to surround all of the p-wells 616 in a planar view. The p-type layer 615 contacts some of the p-wells 616. For example, the p-type layer 615 contacts the p-well 616 that is located outermost among the multiple p-wells 616 in a planar view. The multiple p-type layers 614 are formed in a ring shape on the surface of the n-type layer 613 so as to surround the p-type layer 615. The multiple p-type layers 614 are arranged in a multi-layer configuration. A portion of the n-type layer 613 is located between adjacent p-type layers 614. A portion of the n-type layer 613 is also located between the innermost p-type layer 614 and p-type layer 615.
[0108] The insulating film 621 is formed to cover the surfaces of the n-type layer 613, the p-well 616, the n-type layer 617, the p-type layer 614, and the p-type layer 615. The gate electrode 622 is formed on the insulating film 621 to overlap with the adjacent p-well 616. The contact electrode 623 is formed to be in contact with the n-type layer 617 and the p-type layer 618 through openings formed in the insulating film 621. The drain electrode 624 is provided below the silicon carbide single crystal substrate 611 and is in contact with the silicon carbide single crystal substrate 611.
[0109] Although not shown, an interlayer insulating film is formed to cover the gate electrode 622, and a source electrode is provided on the interlayer insulating film. The source electrode is connected to each contact electrode 623. Therefore, the contact electrode 623, n-type layer 617, p-type layer 618, p-well 616, and p-type layer 615 are electrically connected to the source electrode. In the transistor 600, the guard ring region includes the p-type layer 614, but the p-type layer 615 is not included in the guard ring region.
[0110] A portion of the gate electrode 622 may be located outside the contact electrode 623 in plan view. For example, in the transistor shown in FIG. 12 , a portion 625 of the gate electrode 622 may be located outside the contact electrode 623 and above the boundary between the p-well 616 and the p-type layer 615. In this case, the multiple p-type layers 614 are located outside the gate electrode 622 (including the portion 625) in plan view. The p-type layer 615 may or may not extend from the element region toward the guard ring region.
[0111] In the present disclosure, the semiconductor chip may be a silicon carbide chip. Silicon carbide chips have excellent high-temperature resistance and are less likely to break down even when used at high temperatures. Silicon carbide chips also have high mechanical properties. Furthermore, internal breakdown of the main electrode is suppressed, making it easier for the semiconductor device as a whole to have a long life even at high temperatures.
[0112] Although the embodiments have been described in detail above, the present disclosure is not limited to the specific embodiments, and various modifications and changes are possible within the scope of the claims.
[0113] REFERENCE SIGNS LIST 1, 2 Semiconductor device 21 Element region 22 Termination region 30 Schottky barrier diode 31 Guard ring region 32, 52, 62 Straight region 33, 53, 63 Curvature region 41 First curve 42 Second curve 43 Third curve 101, 102, 103 Terminal 110 Substrate 111 First conductive pattern 112 Second conductive pattern 113 Third conductive pattern 114 Fourth conductive pattern 115 Conductive layer 119 Insulating substrate 120 Heat sink 131, 132, 133 Bonding material 134, 135 Buffer bonding material 135E Outer edge 161, 162, 163, 164, 165, 166: Wire 190 Case 191, 192 Side wall portion 193, 194 End wall portion 200, 600 Transistor (semiconductor chip) 210 Silicon carbide substrate (semiconductor substrate) 210A, 210B Main surface 211, 611 Silicon carbide single crystal substrate (single crystal substrate) 212, 612 Silicon carbide epitaxial layer (epitaxial layer) 231, 622 Gate electrode 232 Source electrode (main electrode) 232A Main surface (first main surface) 232B Main surface 233, 624 Drain electrode 300 Diode (semiconductor chip) 310 Silicon carbide substrate (semiconductor substrate) 310A, 310B Main surface 311 Silicon carbide single crystal substrate (single crystal substrate) 312 Silicon carbide epitaxial layer (epitaxial layer) 313, 613, 617 n-type layer 314, 614, 615, 618 p-type layer 314F inner edge 332 anode electrode (main electrode) 332A main surface (first main surface) 332B main surface 332E outer edge 333 cathode electrode 400, 500 buffer plate 410, 510 first copper layer 420, 520 iron-nickel alloy layer 430, 530 second copper layer 500E outer edge 616 p-well 621 insulating film 623 contact electrode 625 part of gate electrode C1, C2, C3 center
Claims
1. A semiconductor device comprising: a semiconductor chip having a semiconductor substrate and a main electrode provided on the semiconductor substrate; a buffer plate having a first thickness; and a buffer bonding material having a second thickness provided between the main electrode and the buffer plate, wherein, in a plan view from a direction perpendicular to the first main surface, an outer edge of the buffer plate overlaps with a virtual annular first curve that is a distance inward by the sum of the first thickness and the second thickness from the outer edge of the main electrode, or is outside the first curve.
2. The semiconductor device according to claim 1, wherein, in a plan view from a direction perpendicular to said first main surface, the outer edge of said buffer plate overlaps with an imaginary annular second curve located 1 / 2 the sum of said first thickness and said second thickness inward from the outer edge of said main electrode, or is outside said second curve.
3. The semiconductor device according to claim 1 or claim 2, wherein the semiconductor substrate has: an element region in which a semiconductor element is provided; and a guard ring region surrounding the element region in a planar view from a direction perpendicular to the first main surface; and wherein an outer edge of the buffer plate is located inside the guard ring region in a planar view from a direction perpendicular to the first main surface.
4. A semiconductor device as claimed in any one of claims 1 to 3, wherein the outer edge of the buffer plate has a straight region and a curved region adjacent to the straight region, the semiconductor substrate has a single crystal substrate and an epitaxial layer having a third thickness provided on the single crystal substrate, and a value obtained by dividing the radius of curvature of the curved region by the third thickness is 5 or more and 10 or less.
5. A semiconductor device according to any one of claims 1 to 4, wherein, in a plan view from a direction perpendicular to the first main surface, the outer edge of the buffer bonding material overlaps with the first curve or is outside the first curve.
6. The semiconductor device according to claim 1, wherein the main electrode includes an aluminum layer or an aluminum alloy layer.
7. The semiconductor device according to claim 6, wherein a first linear expansion coefficient of said semiconductor substrate and a second linear expansion coefficient of said buffer plate are smaller than a third linear expansion coefficient of said main electrode, and said second linear expansion coefficient is smaller than said first linear expansion coefficient.
8. The semiconductor device according to any one of claims 1 to 7, wherein the buffer bonding material includes a copper sintered body or a silver sintered body.
9. A semiconductor chip including a semiconductor substrate and a main electrode provided on the semiconductor substrate, a buffer plate having a first thickness, and a buffer bonding material having a second thickness provided between the main electrode and the buffer plate, wherein the main electrode has a first main surface, and in a plan view perpendicular to the first main surface, an outer edge of the buffer plate overlaps with a virtual annular first curve located inward from the outer edge of the main electrode by the sum of the first thickness and the second thickness, or is outside the first curve, the outer edge of the buffer plate has a straight region and a curvature region connected to the straight region, the semiconductor substrate has a single crystal substrate and an epitaxial layer provided on the single crystal substrate and having a third thickness, wherein a value obtained by dividing the radius of curvature of the curvature region by the third thickness is 5 or more and 10 or less, the main electrode includes an aluminum layer or an aluminum alloy layer, and the first linear expansion coefficient of the semiconductor substrate and the second linear expansion coefficient of the buffer plate are smaller than a third linear expansion coefficient of the main electrode, the second linear expansion coefficient being smaller than the first linear expansion coefficient, and the buffer bonding material includes a copper sintered body or a silver sintered body.
Citation Information
Patent Citations
Semiconductor device