Pot body brazing double-bottom nitriding process
A pot body and brazing technology, which is applied in the direction of metal material coating process, coating, solid-state diffusion coating, etc., can solve the problems of reduced effect, failure, lack of anti-rust effect and beautiful external appearance
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0027] The present invention proposes a pot body brazing compound bottom nitriding process, comprising the following steps:
[0028] 1) Forming auxiliary disk; by stamping a disk-shaped structure that can completely cover the bottom surface of the restoration, it can be used to strengthen the protection of the bottom of the restoration pot body due to the heat transfer plate wrinkling, brittleness, cracking and other problems caused by the change of cold and heat during use , thus greatly prolonging the service life of the pot.
[0029] 2) Double-bottom brazing is performed on the pot body, heat conduction plate, auxiliary flower plate and electric heating tube to make them tightly integrated to obtain the pot body after double-bottom; brazing means to melt the solder in the gaps of each matching layer through high-temperature welding, so that The auxiliary flower plate is closely combined with the electric heating tube, the heat conduction plate and the pot body. Specificall...
Embodiment 2
[0043] A pot body brazing double-bottom nitriding process specifically comprises the following steps:
[0044] 1) Use a 60T mechanical punch to stretch a 0.6mm iron sheet at one time to form an iron faceplate.
[0045] 2) Bake the iron faceplate at high temperature, set the oven temperature to 360°C, and set the baking time to 6 hours.
[0046] 3) Brush the solder on the iron faceplate, aluminum flat plate and aluminum faceplate, the average amount of solder on the contact surface is 9-12g, and the total amount is not less than 30g.
[0047] 4) Preliminary riveting, using a 15T hydraulic press, put the iron faceplate, electric heating tube, aluminum flat plate and aluminum faceplate brushed with solder into the pressing tool to complete the preliminary riveting.
[0048] 5) Apply solder to the aluminum flat plate again, and the amount of brushing is 9-12g of dry powder weight after drying.
[0049] 6) Double-bottom brazing is performed on the pot body, heat conduction plate,...