A shell material right angle bending processing method
By setting up a position avoidance notch and bend reserved part on the aluminum alloy plate, the ductility of the aluminum alloy makes the side bending vertically connected to the rotating shaft bending, solving the problems of wrinkles, cracks and rounded corners during the traditional bending process. Improves the pass rate and aesthetics of the notebook housing, and enhances strength and corrosion resistance.
Patent Information
- Application Number
- CN202410268716.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2024-03-08
- Publication Date
- 2024-11-29
- Estimated Expiration
- 2044-03-08
AI Technical Summary
The shell of a traditional laptop computer is prone to wrinkles, cracks and rounded corners during bending, resulting in low product qualification rate and unsightly. It is prone to cracking and material pile problems when bending at right angles, which cannot meet the high standards of consumers. Require.
A method of right-angle bending of shell material is adopted, including cutting, stretching and convex, shaping, re-extrusion and shrinking of the hole. By setting a position gap and a bend reserved part on the aluminum alloy plate, the aluminum alloy is used. The ductility allows the side bending to be connected vertically with the shaft bending to avoid piles of materials and adjust deformation during the shrinking process to improve connection strength and aesthetics.
It improves the product qualification rate and aesthetics of the notebook shell, while also enhancing the overall strength and corrosion resistance of the shell, reducing manufacturing costs.
Smart Images

Figure CN117920860B_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of shell material processing, and more specifically to a shell material right-angle bending processing method. Background Art
[0002] With the continuous progress of society and the continuous development of communication technology, the application of laptops is becoming more and more common, and people's requirements for laptops are also increasing. At present, most traditional laptop shells are made of aluminum materials, and usually can only be made of CNC aluminum alloy, which will make the manufacturing cost higher. The shell of the notebook operation panel is composed of an upper shell and a lower shell. The outer side of the upper shell will be formed in one step by a bending process during the manufacturing process. Wrinkles and cracks often occur at the bending point. The product qualification rate is very low and cannot meet the high standards of consumers at all. After the bending is completed, due to the defects of the bending technology, the bending connection is generally rounded, which makes the product not beautiful enough. Furthermore, the aluminum notebook upper shell is also prone to cracking and stacking when the shaft assembly side is bent at a right angle. Summary of the invention
[0003] The technical problem to be solved by the present invention is that the outer side of the upper shell of the notebook operating panel is formed in one step by a bending process during the manufacturing process, and wrinkles and cracks often occur at the bending points. The product qualification rate is very low and cannot meet the high standards of consumers at all. After the bending is completed, due to the defects of the bending technology, the bending connection is generally rounded, which makes the product less beautiful. Furthermore, the aluminum notebook upper shell is also prone to cracking and stacking problems when the shaft assembly side is bent at a right angle. In view of the above-mentioned defects of the prior art, a shell material right-angle bending processing method is provided.
[0004] The technical solution adopted by the present invention to solve its technical problem is:
[0005] A shell material right-angle bending processing method is constructed, comprising the following steps:
[0006] S1. Cutting the aluminum alloy plate into a primary body according to the required size and shape, and setting a gap on the outside of the primary body;
[0007] S2. Stretching and embossing, extruding the primary embryo body downward, so that a bending portion is formed on the outer side of the primary embryo body, the bending portion includes a side bend and a shaft bend, and the avoidance notch is provided between the side bend and the shaft bend;
[0008] S3. Shaping, applying pressure to the side bend in the direction of the shaft bend, limiting the shaft bend to limit the bending of the shaft bend, and under the action of pressure, the side bend will be squeezed toward the shaft bend, at this time, the connection between the side bend and the shaft bend will be deformed so that the side bend and the shaft bend are perpendicularly connected to each other;
[0009] S4. back-extrusion, applying pressure to the side bend in the direction of the central axis of the primary embryo body. Under the action of the pressure, the side bend is pushed in the direction of the central axis of the primary embryo body. At this time, the connection between the side bend and the primary embryo body will gradually deform so that the side bend and the primary embryo body are vertically connected to each other;
[0010] S5. A first shrinking, the side bend and the top of the shaft bend are provided with a shrinking portion, a pressure is applied to the top of the side bend and the shaft bend in the direction of the central axis of the primary embryo body, and the pressure is stopped when the top of the side bend and the shaft bend are inclined 30-60 degrees toward the center of the primary embryo body;
[0011] S6. Secondary shrinking: applying a downward pressure to the shrinking portion from top to bottom, so that the shrinking portion bends downward to be parallel to the top surface of the primary embryo body.
[0012] Preferably, a bending reserve portion is provided on the outer side of the preform body. In step S4, the bending reserve portion is pushed toward the central axis direction of the preform body along with the side bending, and the side bending compresses the bending reserve portion.
[0013] Preferably, the width of the bending reserved portion is 10mm-15mm.
[0014] Preferably, the aluminum alloy used in the aluminum alloy plate is a five-series aluminum alloy.
[0015] Preferably, in step S2, when the primary embryo body is pressed downward, a groove is formed in a concave shape on the top surface of the primary embryo body.
[0016] Preferably, the primary embryo body comprises a square aluminum alloy plate, and a mounting groove is formed on one side of the square aluminum alloy plate.
[0017] Preferably, the rotating shaft is bent and arranged on a side of the square aluminum alloy plate where the assembly groove is opened.
[0018] Preferably, the aluminum alloy used in the aluminum alloy plate has a hardness of 65HB-75HB.
[0019] Preferably, in step S2, the second radius between the side bend and the shaft bend is R=1mm-1.5mm.
[0020] Preferably, when the side bend is pressed toward the shaft bend in step S3, the avoidance gap can be continuously adjusted in size to prevent the side bend from overlapping with the shaft bend.
[0021] The beneficial effects of the present invention are:
[0022] 1. The present invention cuts the aluminum alloy plate into a preform body according to the required size and shape, and sets a avoidance gap on the outside of the preform body. When the side bend and the shaft bend are subsequently formed, the avoidance gap can prevent the side bend and the shaft bend from squeezing and piling materials on each other, and the avoidance gap can continue to expand during the side bend and the shaft bend. Therefore, the avoidance gap can be set relatively small before the side bend and the shaft bend are formed. When the avoidance gap is formed during the side bend and the shaft bend, if the avoidance gap is too small, the avoidance gap is further expanded to make the size of the avoidance gap appropriate;
[0023] 2. By utilizing the ductility of the aluminum alloy, a bent portion is formed on the outer side of the preform body without being damaged, and the connection between the side bend and the shaft bend is deformed so that the side bend and the shaft bend are vertically connected to each other, and the connection between the side bend and the preform body is gradually deformed so that the side bend and the preform body are vertically connected to each other; the top of the side bend is bent downward to be parallel to the top surface of the preform body;
[0024] By processing the outer side of the aluminum alloy notebook shell, the side bend of the notebook shell is vertically connected to the embryo body, and the top of the side bend and the top of the shaft bend of the notebook shell are formed with a necking structure parallel to the initial embryo body, thereby saving manufacturing costs and making the notebook shell more beautiful and having higher overall strength. BRIEF DESCRIPTION OF THE DRAWINGS
[0025] In order to more clearly illustrate the embodiments of the present invention or the technical solutions in the prior art, the present invention will be further described below in conjunction with the accompanying drawings and embodiments. The drawings described below are only some embodiments of the present invention. For those of ordinary skill in the art, other drawings can be obtained based on these drawings without creative work:
[0026] Figure 1 It is an axonometric schematic diagram of the aluminum alloy plate of the present invention after cutting.
[0027] Figure 2 The present invention Figure 1 Enlarged schematic diagram of part C of FIG.
[0028] Figure 3 It is an axonometric schematic diagram after stretching and embossing in the present invention.
[0029] Figure 4 The present invention Figure 3 An enlarged schematic diagram of part D of FIG.
[0030] Figure 5 It is an axonometric schematic diagram after plastic surgery in the present invention.
[0031] Figure 6 The present invention Figure 5 An enlarged schematic diagram of part E of FIG.
[0032] Figure 7 It is an axonometric schematic diagram when the necking is 45 degrees in the present invention.
[0033] Figure 8 The present invention Figure 7 An enlarged schematic diagram of part A.
[0034] Fig. 9 It is an axonometric schematic diagram after the necking is completed in the present invention.
[0035] Fig.10 The present invention Fig. 9 An enlarged schematic diagram of part B.
[0036] Fig.11 It is an axonometric diagram after the keyboard hole is punched in the present invention.
[0037] Fig.12 It is an axonometric schematic diagram after punching a through hole at the side bend in the present invention.
[0038] The accompanying drawings are marked as follows:
[0039] 1. Preliminary embryo body; 2. Avoidance notch; 3. Side bend; 4. Axis bend; 5. First fillet; 7. Narrowing portion; 8. Groove body; 9. Assembly groove; Through hole; 10. DETAILED DESCRIPTION
[0040] In order to make the purpose, technical solution and advantages of the present invention clearer, the technical solution of the present invention will be clearly and completely described below in conjunction with the drawings of the present invention. Obviously, the described embodiments are part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0041] In the description of the embodiments of the present application, it should be noted that, unless otherwise clearly specified and limited, the terms "connected" and "connection" should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be directly connected or indirectly connected through an intermediate medium. For ordinary technicians in this field, the specific meanings of the above terms in the embodiments of the present application can be understood according to specific circumstances.
[0042] In the embodiments of the present application, unless otherwise clearly specified and limited, a first feature being "above" or "below" a second feature may mean that the first and second features are in direct contact, or the first and second features are in indirect contact through an intermediate medium. Moreover, a first feature being "above", "above" or "above" a second feature may mean that the first feature is directly above or obliquely above the second feature, or simply means that the first feature is higher in level than the second feature. A first feature being "below", "below" or "below" a second feature may mean that the first feature is directly below or obliquely below the second feature, or simply means that the first feature is lower in level than the second feature.
[0043] In the description of this specification, the description with reference to the terms "one embodiment", "some embodiments", "example", "specific example", or "some examples" etc. means that the specific features, structures, materials or characteristics described in conjunction with the embodiment or example are included in at least one embodiment or example of the embodiments of the present application. In this specification, the schematic representations of the above terms do not necessarily refer to the same embodiment or example. Moreover, the specific features, structures, materials or characteristics described may be combined in any one or more embodiments or examples in a suitable manner. In addition, those skilled in the art may combine and combine the different embodiments or examples described in this specification and the features of the different embodiments or examples, without contradiction.
[0044] Embodiments of the present invention Figure 1-Figure 12 As shown in , a shell material right-angle bending processing method is involved, including the following steps:
[0045] S1. Cutting the aluminum alloy plate into a preformed body 1 according to the required size and shape, and a avoiding notch 2 is provided on the outer side of the preformed body 1;
[0046] S2. Stretching and embossing, the primary embryo body is extruded downward, so that a bending portion is formed on the outer side of the primary embryo body 1, the bending portion includes a side bend 3 and a shaft bend 4, the shaft bend 4 can be used for subsequent assembly, the notebook shaft is installed in the shaft bend 4, and the connection between the side bend 3 and the primary embryo body 1 is a first fillet, the connection between the side bend 3 and the shaft bend 4 is a second fillet 5, and the avoidance notch 2 is arranged between the side bend 3 and the shaft bend 4; further, the primary embryo body can be stamped by a stamping die, because the aluminum alloy has good ductility, the side bend 3 and the shaft bend 4 are formed more effectively, the stamping die includes a lower die and an upper die, the aluminum alloy plate is placed on the lower die, the upper die can extrude the aluminum alloy plate, when the upper die extrude the aluminum alloy plate downward, the primary embryo body 1 moves downward and the outer side is bent to form the side bend 3 and the shaft bend 4;
[0047] S3. Shaping, applying pressure to the side bend 3 toward the shaft bend 4, and providing a limiting device at the shaft bend 4, wherein the limiting device can be used to limit bending at the shaft bend 4, and under the action of pressure, the side bend 3 will be squeezed toward the shaft bend 4, at this time, the connection between the side bend 3 and the shaft bend 4 in step S2 is deformed so that the side bend 3 and the shaft bend 4 are vertically connected to each other, thereby increasing the connection strength and hardness between the side bend 3 and the shaft bend 4; at this time, the avoidance gap 2 can be repaired by patching.
[0048] S4. Back-extrusion, applying pressure to the side bend 3 in the direction of the central axis of the primary embryo body 1. Under the action of the pressure, the side bend 3 is pushed in the direction of the central axis of the primary embryo body 1. At this time, the connection between the side bend 3 and the primary embryo body 1 in step S2 will gradually deform so that the side bend 3 and the primary embryo body 1 are vertically connected to each other; since the side bend 3 squeezes the primary embryo body 1, when the side bend 3 and the primary embryo body 1 form a vertical connection, the connection strength and hardness between the side bend 3 and the primary embryo body 1 are increased, and the corrosion resistance of the aluminum alloy is improved. During the extrusion process, the aluminum alloy plate can remove surface oxide scale and thermal cracks, making the surface of the aluminum material smoother, brighter and more corrosion-resistant. During the back-extrusion process, the metal billet is heated to a higher temperature and then extruded through a die. Compared with traditional cutting processing, back-extrusion can reduce waste and save material costs. Furthermore, the primary embryo body 1 is fixed, and the extrusion die can be used to act on the side bend 3, so that the side bend 3 can be evenly stressed to prevent the side bend 3 from deforming when moving toward the center point of the primary embryo body 1. The extrusion die includes a push plate, and the side area of the push plate is equal to the side area of the side bend 3. Positioning members are provided at the top and bottom of the push plate, and the positioning members can be used to position the push plate on the side bend 3.
[0049] S5. A first shrinking, the side bend 3 and the top of the shaft bend 4 are provided with a shrinking portion 7, a pressure is applied to the top of the side bend 3 and the shaft bend 4 in the direction of the central axis of the primary embryo body 1, and the pressure is stopped when the shrinking portion is inclined 30-60 degrees toward the center of the primary embryo body 1. Preferably, the pressure is stopped when the top of the side bend 3 and the shaft bend 4 is inclined 45 degrees toward the center of the primary embryo body 1.
[0050] S6. Secondary shrinking: applying a downward pressure to the shrinking portion, so that the shrinking portion 7 bends downward to be parallel to the top surface of the primary embryo body 1.
[0051] A bending reserve portion is provided on the outer side of the embryo body. In step S4, the bending reserve portion is pushed toward the central axis direction of the embryo body 1 along with the side bend 3, and the side bend 3 compresses the bending reserve portion, so that the bending reserve portion is tightened and the strength is increased. Furthermore, by pre-setting a suitable reserved portion, the bending angle and the bending position can be more accurately controlled, thereby improving the accuracy and consistency of the final product. The design of the reserved portion can also effectively reduce stress concentration during the bending process and avoid cracks or fractures in the material at the bending position.
[0052] In this embodiment, the width of the bending reserved portion (not shown in the figure) is 10mm-15mm.
[0053] In this embodiment, the aluminum alloy used in the aluminum alloy plate is a five-series aluminum alloy, which has good corrosion resistance and high strength. The five-series aluminum alloy has medium strength in the cold-worked state and is suitable for applications that require a certain strength but also require good forming properties. The specific model of the aluminum alloy may be 5052 or 5B52.
[0054] See also Figure 2-Figure 9 In step S2, when the primary body is extruded downward, a groove body 8 is formed on the top surface of the primary body. In subsequent processing, a stamping die can be used to form multiple keyboard holes in the groove body 8.
[0055] See also Figure 1-Figure 9 The primary body comprises a square aluminum alloy plate, one side of which is provided with an assembly groove 9. The existence of the assembly groove 9 facilitates the combination and connection between the notebook shell and the notebook display screen.
[0056] In this embodiment, the rotating shaft bend 4 is arranged on the side of the square aluminum alloy plate where the assembly groove 9 is opened.
[0057] In this embodiment, the aluminum alloy used in the aluminum alloy plate has a hardness of 65HB-75HB, preferably 70HB.
[0058] In this embodiment, the second fillet R=1mm-1.5mm, preferably 1mm.
[0059] See also Figure 1-Figure 9 In step S3, when the side bend 3 is squeezed toward the shaft bend 4, the avoidance gap 2 can be continuously adjusted in size to prevent the side bend 3 and the shaft bend 4 from overlapping. Furthermore, the avoidance gap 2 can be set relatively small before the side bend 3 and the shaft bend 4 are formed. When the avoidance gap 2 is formed at the side bend 3 and the shaft bend 4, if the avoidance gap 2 is too small, the avoidance gap 2 is further enlarged to make the size of the avoidance gap 2 appropriate.
[0060] Furthermore, in the present invention, a plurality of through holes are opened on the side bend 3 in subsequent processing.
[0061] It should be understood that those skilled in the art can make improvements or changes based on the above description, and all these improvements and changes should fall within the scope of protection of the appended claims of the present invention.
Claims
1. A shell material right-angle bending processing method, It is characterized in that The following steps are involved: S1. Cutting the aluminum alloy plate into a preliminary body (1) according to the required size and shape, wherein the preliminary body comprises a square aluminum alloy plate, and a mounting groove (9) is provided on one side of the square aluminum alloy plate; and a avoiding notch (2) is provided on the outer side of the preliminary body (1); S2. Stretching and embossing, the primary embryo body is pressed downward, so that a bending portion is formed on the outer side of the primary embryo body (1), the bending portion includes a side bend (3) and a shaft bend (4), the shaft bend (4) is arranged on the side of the square aluminum alloy plate where the assembly groove (9) is opened, the connection between the side bend (3) and the primary embryo body (1) is a first rounded corner, the connection between the side bend (3) and the shaft bend (4) is a second rounded corner (5), and the avoidance notch (2) is arranged between the side bend (3) and the shaft bend (4); S3. Shaping, applying pressure to the side bend (3) in the direction of the shaft bend (4), limiting the position at the shaft bend (4) to limit bending at the shaft bend (4), under the action of pressure, the side bend (3) will be squeezed toward the shaft bend (4), at this time, the connection between the side bend (3) and the shaft bend (4) will be deformed so that the side bend (3) and the shaft bend (4) are vertically connected to each other; S4. back-squeezing, applying pressure to the side bend (3) in the direction of the central axis of the primary embryo body (1). Under the action of the pressure, the side bend (3) is pushed in the direction of the central axis of the primary embryo body (1). At this time, the connection between the side bend (3) and the primary embryo body (1) will gradually deform so that the side bend (3) and the primary embryo body (1) are vertically connected to each other; S5. A first shrinking, wherein the top of the side bend (3) and the shaft bend (4) are provided with a shrinking portion (7), and a pressure is applied to the top of the side bend (3) and the shaft bend (4) in a direction toward the central axis of the primary embryo body (1), and the application of pressure is stopped when the top of the side bend (3) and the shaft bend (4) are inclined 30-60 degrees toward the center of the primary embryo body (1); S6. Secondary shrinking: applying a downward pressure to the shrinking portion from top to bottom, so that the shrinking portion (7) bends downward to be parallel to the top surface of the primary embryo body (1).
2. A shell material right-angle bending processing method according to claim 1, It is characterized in that A bending reserve portion is provided on the outer side of the primary embryo body. In step S4, the bending reserve portion is pushed toward the central axis direction of the primary embryo body (1) along with the side bend (3), and the side bend (3) compresses the bending reserve portion.
3. A shell material right-angle bending processing method according to claim 2, It is characterized in that The width of the bending reserved portion is 10mm-15mm.
4. A shell material right-angle bending processing method according to claim 1, It is characterized in that The aluminum alloy used in the aluminum alloy plate is a five-series aluminum alloy.
5. A shell material right-angle bending processing method according to claim 1, It is characterized in that In step S2, when the primary embryo body is pressed downward, a groove body (8) is formed on the top surface of the primary embryo body in a concave manner.
6. A shell material right-angle bending processing method according to claim 1, It is characterized in that The aluminum alloy used in the aluminum alloy plate has a hardness of 65HB-75HB.
7. A shell material right-angle bending processing method according to claim 1, It is characterized in that In step S2, the second fillet between the side bend and the shaft bend is R=1mm-1.5mm.
8. A shell material right-angle bending processing method according to any one of claims 1 to 7, It is characterized in that When the side bend (3) is pressed toward the shaft bend (4) in step S3, the avoidance gap (2) can be continuously adjusted in size to prevent the side bend (3) and the shaft bend (4) from overlapping.
Citation Information
Patent Citations
Right angle extrusion processing method and right angle extrusion processing mould