Trench type power device, preparation method, power module, conversion circuit and vehicle
By using high dielectric constant material as the insulating layer of the polysilicon gate bottom and sidewall in trench power devices, the insulating layer is formed in step by step, which solves the problems of threshold voltage in the device and the insulating layer breakdown in the device, and improves the device control capability and reliability.
Patent Information
- Application Number
- CN202410514565.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2024-04-26
- Publication Date
- 2024-12-06
- Estimated Expiration
- 2044-04-26
AI Technical Summary
There are problems of threshold voltage instability and gate insulating layer breakdown in trench type power devices, resulting in a decrease in gate control capability.
The insulating layer materials using the bottom and side walls of the polycrystalline silicon gate are respectively set as high dielectric constant (high-k) materials, and the insulating layer is formed in steps to ensure the bottom thickness and side wall thinness, and improve the control ability and reliability of the device. sex.
It effectively improves the breakdown problem of the gate insulating layer in trench power devices, improves the control capability and reliability of the devices, and ensures stable operation in high voltage and high frequency scenarios.
Smart Images

Figure CN118431290B_ABST
Abstract
Description
Technical Field
[0001] Embodiments of the present invention relate to the technical field of semiconductor devices, and in particular, to a trench power device, a preparation method, a power module, a conversion circuit, and a vehicle. Background Art
[0002] As a representative of the third generation of semiconductor materials, silicon carbide (SiC) has excellent physical and electrical properties. Compared with silicon materials, SiC materials have a large bandgap, high breakdown electric field, high thermal conductivity, high electron saturation rate, and strong radiation resistance. Therefore, semiconductor devices made of SiC materials can not only operate stably at higher temperatures, but are also suitable for high voltage and high frequency scenarios.
[0003] SiC MOSFET has undergone a process from planar type to trench type. By improving the gate structure, the direction of current flow on the gate has changed from planar to vertical. In the related technology, by additionally etching the source trench, ion implantation is performed on the bottom and sidewalls of the source trench to obtain a P-well region of sufficient depth, and the structure is named a double trench structure (DT-MOS). Compared with the unshielded structure, the double trench structure can reduce the gate oxide electric field, improve the voltage resistance and reduce the specific on-resistance. Whether from the perspective of structural simplicity and process complexity, or from the perspective of device characteristics, the double trench structure achieves a better balance between the two. The introduction of this structure also makes the first step in the commercial development of SiC trench gate MOSFET devices.
[0004] However, the current trench power device has the problem of unstable threshold voltage. In particular, the double trench structure, the electric field concentration effect at the bottom of the gate trench in the blocking state, easily causes the electric field in the gate oxide layer (gate insulating layer) to intensify, thereby causing the gate oxide layer at the bottom of the gate trench to break down in advance. In order to avoid the gate oxide layer at the bottom of the gate trench from being broken down in advance, it is necessary to increase the thickness of the gate oxide layer at the bottom of the gate trench. However, limited to the current process method, the oxidation rate has an important relationship with the crystal plane orientation of SiC. The groove wall of the gate trench is in the self-oxidation process. The thickness of the sidewall oxide layer will be higher than the thickness of the bottom oxide layer, causing the electric field effect at the channel to weaken, thereby reducing the control ability of the gate to the device. Therefore, how to improve the gate insulating layer breakdown problem in the trench power device while ensuring the control ability of the gate to the device is a technical problem that needs to be solved by those skilled in the art. Summary of the invention
[0005] Embodiments of the present invention provide a trench power device, a preparation method, a power module, a conversion circuit and a vehicle, so as to improve the problem of gate insulation layer breakdown in the trench power device while ensuring the control ability of the gate over the device.
[0006] According to one aspect of the present invention, there is provided a trench power device, comprising:
[0007] substrate;
[0008] A semiconductor epitaxial layer, located on one side of the substrate;
[0009] A gate trench is located on a surface of the semiconductor epitaxial layer away from the substrate;
[0010] A trench gate structure is located in the gate trench; the trench gate structure includes a polysilicon gate and a first gate insulating layer located at the bottom of the polysilicon gate and a second gate insulating layer located at the sidewall of the polysilicon gate;
[0011] The dielectric constant of the material of the first gate insulating layer is greater than or equal to the dielectric constant of the material of the second gate insulating layer, and the dielectric constant of the material of the first gate insulating layer is greater than the dielectric constant of silicon oxide.
[0012] Optionally, the dielectric constant of the material of the second gate insulating layer is greater than the dielectric constant of silicon oxide;
[0013] The thickness of the first gate insulating layer is greater than the thickness of the second gate insulating layer located on the sidewall of the polysilicon gate.
[0014] Optionally, the trench power device further includes:
[0015] a third gate insulating layer, the third gate insulating layer being located between the first gate insulating layer and the polysilicon gate;
[0016] The third gate insulating layer is made of the same material as the second gate insulating layer, and the third gate insulating layer and the second gate insulating layer are integrally arranged.
[0017] Optionally, a material of the second gate insulating layer includes silicon oxide.
[0018] Optionally, along the direction of the semiconductor epitaxial layer away from the substrate, the semiconductor outer layer includes a first conductive type first doping region, a second conductive type first doping region and a first conductive type second doping region in sequence; the gate trench extends from a surface of the semiconductor epitaxial layer away from the substrate to the first conductive type first doping region;
[0019] The first conductive type first doping region and the first conductive type second doping region are doped with N-type doping ions; the second conductive type first doping region is doped with P-type doping ions;
[0020] Alternatively, the first conductive type first doping region and the first conductive type second doping region are doped with P-type doping ions; and the second conductive type first doping region is doped with N-type doping ions.
[0021] Optionally, the trench power device further includes:
[0022] A source trench, located at two opposite sides of the gate trench and spaced apart from the gate trench;
[0023] A trench source structure is located in the source trench; the trench source structure comprises a polysilicon source, a first source insulating layer located at the bottom of the polysilicon source, and a second source insulating layer located at the sidewall of the polysilicon source; the material of the first source insulating layer is the same as the material of the first gate insulating layer; the material of the second source insulating layer is the same as the material of the second gate insulating layer;
[0024] The semiconductor epitaxial layer further includes a second conductive type second doping region, and the second conductive type second doping region is located at the bottom and sidewall of the trench source structure.
[0025] Optionally, the trench power device further includes:
[0026] an interlayer insulating layer, located on a side of the semiconductor epitaxial layer away from the substrate and covering the trench gate structure;
[0027] A source electrode, located on a side of the interlayer insulating layer away from the substrate, and on a surface of the semiconductor epitaxial layer not covered by the interlayer insulating layer;
[0028] The drain electrode is located on a surface of the substrate away from the semiconductor epitaxial layer.
[0029] According to another aspect of the present invention, there is provided a method for preparing a trench power device, comprising:
[0030] providing a substrate;
[0031] forming a semiconductor epitaxial layer on one side of the substrate;
[0032] forming a gate trench on a surface of the semiconductor epitaxial layer away from the substrate;
[0033] A trench gate structure is formed in the gate trench, the trench gate structure comprising a polysilicon gate, a first gate insulating layer located at the bottom of the polysilicon gate, and a second gate insulating layer located at the sidewall of the polysilicon gate; wherein the dielectric constant of the material of the first gate insulating layer is greater than or equal to the dielectric constant of the material of the second gate insulating layer, and the dielectric constant of the material of the first gate insulating layer is greater than the dielectric constant of silicon oxide.
[0034] Optionally, forming a trench gate structure in the gate trench includes:
[0035] forming a mask layer on a surface of the semiconductor epitaxial layer away from the substrate and a wall of the gate trench;
[0036] Etching the mask layer at the bottom of the gate trench to expose the bottom of the gate trench;
[0037] forming a first gate initial insulating layer on a surface of the mask layer away from the substrate, a surface of the mask layer in the gate trench away from the sidewall of the gate trench, and a bottom of the gate trench;
[0038] Applying photoresist so that the photoresist covers the surface of the first gate initial insulating layer away from the substrate and fills the gate trench;
[0039] Patterning the photoresist to form a plurality of openings exposing a surface of the first gate initial insulating layer away from the substrate;
[0040] Based on the opening in the photoresist, etching the first gate initial insulating layer and at least a portion of the mask layer;
[0041] Removing the photoresist, and removing the mask layer and the first gate initial insulating layer on the surface of the mask layer by means of an etching solution based on ultrasonic vibration, so as to form a first gate insulating layer at the bottom of the gate trench;
[0042] forming a second gate initial insulating layer on the surface of the semiconductor epitaxial layer away from the substrate, the sidewall of the gate trench, and the surface of the first gate insulating layer; wherein the dielectric constant of the material of the second gate initial insulating layer is greater than the dielectric constant of silicon oxide;
[0043] By dry etching, the second gate initial insulating layer located on the surface of the semiconductor epitaxial layer away from the substrate is removed, and the second gate initial insulating layer located on the surface of the first gate insulating layer away from the substrate is removed, so as to form a second gate insulating layer on the sidewall of the gate trench;
[0044] The gate trench is filled with polysilicon material to form a polysilicon gate.
[0045] Optionally, forming a trench gate structure in the gate trench includes:
[0046] forming a mask layer on a surface of the semiconductor epitaxial layer away from the substrate and a wall of the gate trench;
[0047] Etching the mask layer at the bottom of the gate trench to expose the bottom of the gate trench;
[0048] forming a first gate initial insulating layer on a surface of the mask layer away from the substrate, a surface of the mask layer in the gate trench away from the sidewall of the gate trench, and a bottom of the gate trench;
[0049] Applying photoresist so that the photoresist covers the surface of the first gate initial insulating layer away from the substrate and fills the gate trench;
[0050] Patterning the photoresist to form a plurality of openings exposing a surface of the first gate initial insulating layer away from the substrate;
[0051] Based on the opening in the photoresist, etching the first gate initial insulating layer and at least a portion of the mask layer;
[0052] Removing the photoresist, and removing the mask layer and the first gate initial insulating layer on the surface of the mask layer by means of an etching solution based on ultrasonic vibration, so as to form a first gate insulating layer at the bottom of the polysilicon gate;
[0053] forming a second gate initial insulating layer on the surface of the semiconductor epitaxial layer away from the substrate, the sidewall of the gate trench, and the surface of the first gate insulating layer; wherein the dielectric constant of the material of the second gate initial insulating layer is greater than the dielectric constant of silicon oxide;
[0054] Filling the gate trench with photoresist to cover the second gate initial insulating layer located in the gate trench;
[0055] Removing the second gate initial insulating layer on the surface of the semiconductor epitaxial layer away from the substrate by dry etching to form a second gate insulating layer on the sidewall of the gate trench, and forming a third gate insulating layer on the surface of the first gate insulating layer away from the substrate;
[0056] The gate trench is filled with polysilicon material to form a polysilicon gate.
[0057] Optionally, forming a trench gate structure in the gate trench includes:
[0058] forming a mask layer on a surface of the semiconductor epitaxial layer away from the substrate and a wall of the gate trench;
[0059] Etching the mask layer at the bottom of the gate trench to expose the bottom of the gate trench;
[0060] forming a first gate initial insulating layer on a surface of the mask layer away from the substrate, a surface of the mask layer in the gate trench away from the sidewall of the gate trench, and a bottom of the gate trench;
[0061] Applying photoresist so that the photoresist covers the surface of the first gate initial insulating layer away from the substrate and fills the gate trench;
[0062] Patterning the photoresist to form a plurality of openings exposing a surface of the first gate initial insulating layer away from the substrate;
[0063] Based on the opening in the photoresist, etching the first gate initial insulating layer and at least a portion of the mask layer;
[0064] Removing the photoresist, and removing the mask layer and the first gate initial insulating layer on the surface of the mask layer by means of an etching solution based on ultrasonic vibration, so as to form a first gate insulating layer at the bottom of the polysilicon gate;
[0065] Oxidizing the sidewalls of the gate trench by thermal oxidation to form a second gate insulating layer on the sidewalls of the gate trench; the material of the second gate insulating layer includes silicon oxide;
[0066] The gate trench is filled with polysilicon material to form a polysilicon gate.
[0067] Optionally, etching the semiconductor epitaxial layer to form a gate trench in the semiconductor epitaxial layer also includes:
[0068] Forming source trenches on opposite sides of the gate trench, and the source trench is spaced apart from the gate trench;
[0069] Before forming a trench gate structure in the gate trench, the method further includes:
[0070] Implanting doping ions of a second doping type into the sidewalls and bottom of the source trench to form a second doping region of a second conductivity type;
[0071] While forming a trench gate structure in the gate trench, the method further comprises:
[0072] A trench source structure is formed in the source trench; wherein the trench source structure includes a polysilicon source, a first source insulating layer located at the bottom of the polysilicon source, and a second source insulating layer located at the side wall of the polysilicon source; the first source insulating layer and the first gate insulating layer are formed synchronously in the same process; the material of the second source insulating layer and the second gate insulating layer are formed synchronously in the same process; the polysilicon source and the polysilicon gate are formed synchronously in the same process.
[0073] According to another aspect of the present invention, a power module is provided, comprising a substrate and at least one trench-type power device according to any one of the embodiments of the present invention, wherein the substrate is used for supporting the trench-type power device.
[0074] According to another aspect of the present invention, there is provided a power conversion circuit, the power conversion circuit being used for one or more of current conversion, voltage conversion, and power factor correction;
[0075] The power conversion circuit comprises a circuit board and at least one trench power device as described in any embodiment of the present invention, and the trench power device is electrically connected to the circuit board.
[0076] According to another aspect of the present invention, a vehicle is provided, comprising a load and a power conversion circuit as described in any embodiment of the present invention, wherein the power conversion circuit is used to convert AC power into DC power, convert AC power into AC power, convert DC power into DC power, or convert DC power into AC power and then input it into the load.
[0077] An embodiment of the present invention provides a trench power device, a preparation method, a power module, a conversion circuit and a vehicle, wherein the trench power device includes: a substrate; a semiconductor epitaxial layer, located on one side of the substrate; a gate trench, which is arranged in the semiconductor epitaxial layer from the surface of the semiconductor epitaxial layer away from the substrate side; a trench gate structure, which is located in the gate trench; the trench gate structure includes a polysilicon gate and a first gate insulating layer located at the bottom of the polysilicon gate and a second gate insulating layer located on the side wall of the polysilicon gate; the dielectric constant of the material of the first gate insulating layer is greater than or equal to the dielectric constant of the material of the second gate insulating layer, and the dielectric constant of the material of the first gate insulating layer is greater than the dielectric constant of silicon oxide. The technical solution provided by the embodiment of the present invention can improve the problem that the gate insulation layer at the bottom of the crystalline silicon gate in the trench power device is easily broken down by setting the gate insulation layer at the bottom of the polysilicon gate as a dielectric layer of a high-k material; and the gate insulation layer at the bottom of the polysilicon gate and the gate insulation layer on the side wall of the polysilicon gate are formed step by step, so that the thickness of the gate insulation layer at the bottom and the side wall of the gate trench can be accurately controlled respectively, and the morphology of a thick bottom gate insulation layer and a thin side wall gate insulation layer can be easily obtained, thereby ensuring the gate's control ability over the device.
[0078] It should be understood that the contents described in this section are not intended to identify the key or important features of the embodiments of the present invention, nor are they intended to limit the scope of the present invention. Other features of the present invention will become easily understood through the following description. BRIEF DESCRIPTION OF THE DRAWINGS
[0079] In order to more clearly illustrate the technical solutions in the embodiments of the present invention, the following briefly introduces the drawings required for use in the description of the embodiments. Obviously, the drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without creative work.
[0080] Figure 1 is a schematic cross-sectional view of a trench power device provided by an embodiment of the present invention;
[0081] Figure 2 is a schematic cross-sectional view of another trench power device provided by an embodiment of the present invention;
[0082] Figure 3 is a schematic cross-sectional view of another trench power device provided by an embodiment of the present invention;
[0083] Figure 4 It is a flow chart of a method for preparing a trench power device provided by an embodiment of the present invention;
[0084] Figure 5 is a schematic structural cross-sectional view corresponding to step S120 in a method for preparing a trench power device provided in an embodiment of the present invention;
[0085] Figure 6 is a schematic structural cross-sectional view corresponding to step S130 in a method for preparing a trench power device provided in an embodiment of the present invention;
[0086] Figure 7 is a schematic structural cross-sectional view corresponding to step S1401 in a method for preparing a trench power device provided in an embodiment of the present invention;
[0087] Figure 8 to Figure 13 It is a schematic structural cross-sectional view corresponding to steps S411 to S416, steps S421 to S426 or steps S431 to S436 in step S140 in a method for preparing a trench power device provided in an embodiment of the present invention;
[0088] Fig.14 It is a schematic structural cross-sectional view corresponding to step S417 or step S427 in step S140 of a method for preparing a trench power device provided by an embodiment of the present invention;
[0089] Fig.15 It is a schematic structural cross-sectional view corresponding to step S418 in step S140 of a method for preparing a trench power device provided in an embodiment of the present invention;
[0090] Fig.16It is a schematic structural cross-sectional view corresponding to step S419 in step S140 of a method for preparing a trench power device provided in an embodiment of the present invention;
[0091] Figure 17 to Figure 19 It is a schematic structural cross-sectional view corresponding to steps S428 to S4210 in step S140 of a method for preparing a trench power device provided in an embodiment of the present invention;
[0092] Figure 20 to Figure 23 It is a schematic structural cross-sectional diagram corresponding to steps S437 to S4310 in step S140 of a method for preparing a trench power device provided in an embodiment of the present invention. DETAILED DESCRIPTION
[0093] In order to enable those skilled in the art to better understand the scheme of the present invention, the technical scheme in the embodiments of the present invention will be clearly and completely described below in conjunction with the drawings in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work should fall within the scope of protection of the present invention.
[0094] It should be noted that the terms "first", "second", etc. in the specification and claims of the present invention and the above-mentioned drawings are used to distinguish similar objects, and are not necessarily used to describe a specific order or sequence. It should be understood that the data used in this way can be interchanged where appropriate, so that the embodiments of the present invention described herein can be implemented in an order other than those illustrated or described herein. In addition, the terms "including" and "having" and any variations thereof are intended to cover non-exclusive inclusions, for example, a process, method, system, product or device that includes a series of steps or units is not necessarily limited to those steps or units that are clearly listed, but may include other steps or units that are not clearly listed or inherent to these processes, methods, products or devices.
[0095] An embodiment of the present invention provides a trench power device, characterized by comprising:
[0096] substrate;
[0097] A semiconductor epitaxial layer, located on one side of the substrate;
[0098] A gate trench is located on a surface of the semiconductor epitaxial layer away from the substrate;
[0099] A trench gate structure is located in the gate trench; the trench gate structure includes a polysilicon gate, a first gate insulating layer located at the bottom of the polysilicon gate, and a second gate insulating layer located at the sidewall of the polysilicon gate;
[0100] The dielectric constant of the material of the first gate insulating layer is greater than or equal to the dielectric constant of the material of the second gate insulating layer, and the dielectric constant of the material of the first gate insulating layer is greater than the dielectric constant of silicon oxide.
[0101] Specifically, the material of the substrate may be the same as or different from the material of the semiconductor epitaxial layer. In an embodiment of the present invention, the material of the substrate is the same as the material of the semiconductor epitaxial layer, and both may be SiC. That is, the trench power device in the embodiment of the present invention may be a trench SiC power device. SiC has excellent physical and electrical properties. Compared with silicon materials, SiC materials have a large bandgap, and have the advantages of high breakdown electric field, high thermal conductivity, high electron saturation rate, and strong radiation resistance. Therefore, semiconductor devices prepared using SiC materials can not only operate stably at higher temperatures, but are also suitable for high voltage and high frequency scenarios. In some embodiments of the present invention, the substrate and the semiconductor epitaxial layer can be arranged as one. The substrate and the semiconductor epitaxial layer can be understood as a whole SiC film layer structure formed in the same preparation process. After the front process is performed on the entire SiC film layer structure, the back of the SiC film layer structure is thinned, and the back of the SiC film layer structure is heavily doped with the first conductive type doping ions to form a substrate.
[0102] The semiconductor epitaxial layer includes a first conductive type first doping region, a first conductive type doping region and a first conductive type second doping region. The doping concentration of the first conductive type first doping region is less than the doping concentration of the first conductive type second doping region. The first conductive type first doping region is used to form a drift region of a trench SiC power device; the first conductive type doping region is used to form a well region of a trench SiC power device; the first conductive type second doping region is used to form a contact source region of a trench SiC power device. The trench gate structure extends vertically from the surface of the contact source region to the drift region. The trench gate structure includes a gate insulating layer covering the surface of the gate trench, and a polysilicon gate wrapped by the gate insulating layer.
[0103] Wherein, the gate insulating layer includes a first gate insulating layer located at the bottom of the polysilicon gate and a second gate insulating layer located at the side wall of the polysilicon gate. The dielectric constant of the material of the first gate insulating layer is greater than or equal to the dielectric constant of the material of the second gate insulating layer, and the dielectric constant of the material of the first gate insulating layer is greater than the dielectric constant of silicon oxide. The technical solution provided by the embodiment of the present invention can improve the problem that the gate insulating layer at the bottom of the crystalline silicon gate in the trench power device is easily broken down by setting the first gate insulating layer at the bottom of the crystalline silicon gate as a dielectric layer of high-k material; and the gate insulating layer at the bottom of the polysilicon gate (the first gate insulating layer) and the gate insulating layer at the side wall of the polysilicon gate (the second gate insulating layer) are formed in steps, so that the thickness of the gate insulating layer at the bottom and the side wall of the gate groove can be accurately controlled respectively, and the morphology with thick bottom and thin side wall can be easily obtained, thereby ensuring the control ability of the polysilicon gate over the device.
[0104] The above is the core inventive concept of the present invention. The configuration of the gate insulating layer is described in detail below with reference to the accompanying drawings.
[0105] Based on the above embodiments, in one embodiment of the present invention, Figure 1 is a schematic cross-sectional view of a trench power device provided by an embodiment of the present invention, with reference to Figure 1 The material dielectric constant of the second gate insulating layer 322 is greater than the dielectric constant of silicon oxide; the thickness of the first gate insulating layer 321 is greater than the thickness of the second gate insulating layer 322 located on the side wall of the polysilicon gate 31.
[0106] Specifically, the gate trench is formed by etching the semiconductor epitaxial layer 20, and the surface of the semiconductor epitaxial layer 20 away from the substrate 10 is etched to the first conductive type first doping region 21, and the trench gate structure 30 is formed in the gate trench, so that the trench gate structure 30 extends vertically from the surface contacting the source region to the drift region. After forming a first gate insulating layer 321 at the bottom of the gate trench and forming a second gate insulating layer 322 on the sidewall of the gate trench, a polysilicon material is filled in the gate trench to form a polysilicon gate 31. The polysilicon gate 31, the first gate insulating layer 321 at the bottom of the polysilicon gate 31, and the second gate insulating layer 322 at the sidewall of the polysilicon gate 31 are used to form the trench gate structure 30.
[0107] Among them, the material dielectric constant of the first gate insulating layer 321 is greater than the dielectric constant of silicon oxide, and the material dielectric constant of the second gate insulating layer 322 is greater than the dielectric constant of silicon oxide, that is, the material of the first gate insulating layer 321 and the material of the second gate insulating layer 322 are both high-k materials. k refers to the dielectric constant, which measures the ability of the material to store charge. According to the dielectric constant, it is divided into low dielectric (low-k) materials and high dielectric (high-k) materials. Generally, the dielectric constant of Low-K materials is less than 3.0; high-k materials are relative to SiO2, and the dielectric constant is greater than the dielectric constant of SiO2 of 3.9, which is generally called High-K materials. Exemplary, High-k materials include but are not limited to oxides such as ZrO2, Al2O3, and HfO2. In the embodiment of the present invention, by using a high-k dielectric layer as the gate insulating layer at the bottom of the trench (the first gate insulating layer 321), the gate insulating layer at the bottom of the trench can be prevented from being broken down to a great extent, thereby improving the reliability of the device; and, on the basis of the bottom high-k gate oxide, the high-k dielectric layer is used as the second gate insulating layer 322 on the sidewall of the trench, which can also appropriately improve the electron mobility, thereby improving the turn-on rate of the device. Optionally, the high-k material of the first gate insulating layer 321 can be the same as or different from the high-k material of the second gate insulating layer 322.
[0108] In addition, the first gate insulating layer 321 and the second gate insulating layer 322 are formed asynchronously, so that the thickness of the gate insulating layer at the bottom and sidewall of the gate groove can be precisely controlled, and a morphology with a thick bottom and thin sidewall can be easily obtained, thereby preventing the gate insulating layer at the sidewall of the polysilicon gate 31 from being too thick, causing the problem of weakening the electric field effect at the channel, thereby ensuring the control ability of the polysilicon gate over the device. The thickness of the first gate insulating layer 321 at the bottom of the gate groove is determined by the first high-k material deposition, and the thickness of the second gate insulating layer 322 on the sidewall is determined by the second high-k material deposition.
[0109] Based on the above embodiments, in one embodiment of the present invention, Figure 2 is a schematic cross-sectional view of another trench power device provided by an embodiment of the present invention, with reference to Figure 2 The trench power device also includes: a third gate insulating layer 323, located between the first gate insulating layer 321 and the polysilicon gate 31; the third gate insulating layer 323 and the second gate insulating layer 322 are made of the same material, and the third gate insulating layer 323 and the second gate insulating layer 322 are integrally arranged.
[0110] Specifically, the third gate insulating layer 323 is provided between the first gate insulating layer 321 and the polysilicon gate 31, so that the thickness of the gate insulating layer at the bottom of the polysilicon gate 31 can be increased, thereby further preventing the gate insulating layer at the bottom of the trench from being broken down, thereby improving the reliability of the device. The third gate insulating layer 323 is provided integrally with the second gate insulating layer 322, which can be understood as the third gate insulating layer 323 and the second gate insulating layer 322 are formed in the same preparation process, and the third gate insulating layer 323 and the second gate insulating layer 322 are provided integrally, which can simplify the preparation process of the third gate insulating layer 323 and the second gate insulating layer 322.
[0111] Based on the above embodiments, in one embodiment of the present invention, Figure 3 is a schematic cross-sectional view of another trench power device provided by an embodiment of the present invention, with reference to Figure 3 , the material of the second gate insulating layer 322 includes silicon oxide.
[0112] Specifically, on the basis of using high-k material for the first gate insulating layer 321, the sidewall of the gate trench is directly thermally oxidized to form the second gate insulating layer 322, without the need for an additional high-k material deposition process to form the second gate insulating layer 322, thereby simplifying the process steps, saving production costs, and reducing manufacturing time. Figure 1 and Figure 2 As shown, a second gate insulating layer 322 of high-k material is formed on the side wall of the gate trench. The embodiment of the present invention uses a self-oxidation method to grow the second gate insulating layer 322 of SiO2 material on the side wall of the gate trench. The second gate insulating layer 322 of SiO2 material and the semiconductor epitaxial layer 20 of SiC material have fewer interface defects, which is more conducive to the generation of a channel.
[0113] Based on the above embodiments, Figure 1 to Figure 3 , trench power devices also include:
[0114] A source trench, located at two opposite sides of the gate trench and spaced apart from the gate trench;
[0115] A trench source structure 40 is located in the source trench; the trench source structure 40 includes a polysilicon source 41, a first source insulating layer 421 located at the bottom of the polysilicon source 41, and a second source insulating layer 422 located at the sidewall of the polysilicon source 41; the material of the first source insulating layer 421 is the same as the material of the first gate insulating layer 321; the material of the second source insulating layer 422 is the same as the material of the second gate insulating layer 322;
[0116] The semiconductor epitaxial layer 20 further includes a second conductive type second doping region 24, which is located at the bottom and sidewalls of the trench source structure 40. The doping concentration of the second conductive type second doping region 24 may be greater than the doping concentration of the second conductive type first doping region 22.
[0117] Specifically, the semiconductor epitaxial layer 20 is etched, and while a gate trench is formed in the semiconductor epitaxial layer 20, a source trench is also formed on opposite sides of the gate trench, and the source trench is spaced apart from the gate trench. After the source trench is etched to form the source trench, doping ions of the second doping type are implanted into the sidewall and bottom of the source trench to form a second conductive type second doping region 24. After the second conductive type second doping region 24 is formed, a first source insulating layer 421 and a first gate insulating layer 321 are simultaneously formed in the same process; a second source insulating layer 422 and a second gate insulating layer 322 are simultaneously formed in the same process; and a polysilicon source 41 and a polysilicon gate 31 are simultaneously formed in the same process.
[0118] A depletion region is formed between the second conductive type second doping region 24 and the first conductive type first doping region 21 (drift region), which can play a role in shielding the electric field on the side of the trench gate structure 30, thereby improving the breakdown problem of the second gate insulating layer 322 located on the side wall in the trench power device, and ensuring the reliability of the device operation. Optionally, looking down at the trench power device, the source trench can be an annular trench, arranged around the trench gate structure 30, or the source trench can be a point-shaped trench, and a plurality of source trenches are arranged around the trench gate structure 30. Preferably, the source trench is an annular trench, which can protect the gate insulating layer of the trench gate structure 30 from all directions on the side of the trench gate structure 30.
[0119] Based on any of the above embodiments, Figure 1 to Figure 3 , the first conductive type first doping region 21 and the first conductive type second doping region 23 are doped with N-type doping ions; the second conductive type first doping region 22 and the second conductive type second doping region 24 are doped with P-type doping ions;
[0120] P shown in the figure + 、N + Indicates that the ion doping concentration in this area is high, P - 、N - Indicates that the ion doping concentration in this area is low. Among them, the N-type doping ions can be P (phosphorus) or N (nitrogen) ions, and the P-type doping ions can be Al (aluminum) ions or B (boron) ions. The polysilicon (Poly) material in the gate trench is used to form a polysilicon gate 31, and the polysilicon (Poly) material in the source trench is used to form a polysilicon source 41.
[0121] Alternatively, the first conductive type first doping region 21 and the first conductive type second doping region 23 are doped with P-type doping ions; the second conductive type first doping region 22 and the second conductive type second doping region 24 are doped with N-type doping ions.
[0122] Based on the above embodiments, please continue to refer to Figure 1 to Figure 3 , the trench power device further includes: an interlayer insulating layer ILD, which is located on the side of the semiconductor epitaxial layer 20 away from the substrate 10 and covers the trench gate structure 30; a source electrode S, which is located on the side of the interlayer insulating layer ILD away from the substrate 10, and on the surface of the semiconductor epitaxial layer 20 not covered by the interlayer insulating layer ILD; and a drain electrode D, which is located on the surface of the substrate 10 away from the semiconductor epitaxial layer 20. Among them, the interlayer insulating layer ILD is used to isolate the source electrode S from the trench gate structure 30, and the material of the interlayer insulating layer ILD may include silicon oxide. The material of the source electrode S and the drain electrode D includes metal. When a positive bias voltage is applied to the trench gate structure 30, an N channel is formed between the N-type drift region and the N-type source contact region, and the electron flow is injected from the N-type source contact region, flows through the N-type drift region through the N channel, and the source electrode S is connected to the drain electrode D. The trench power device may also include a passivation layer and a protective layer sequentially located on the source electrode. The material of the passivation layer may include silicon nitride (SiN), and the material of the protection layer may include polyimide (PI).
[0123] The embodiment of the present invention further provides a method for preparing a trench type power device, which is used to prepare the trench type power device described in any of the above embodiments. Figure 4 is a flow chart of a method for preparing a trench power device provided by an embodiment of the present invention, with reference to Figure 4 , the preparation method of the trench power device comprises:
[0124] S110 , providing a substrate.
[0125] S120 , forming a semiconductor epitaxial layer on one side of the substrate.
[0126] Specifically, refer to Figure 5 , along the direction of epitaxial growth of the semiconductor outer layer 20, the semiconductor epitaxial layer 20 sequentially includes a first conductive type first doping region 21, a second conductive type first doping region 22, and a first conductive type second doping region 23. The first conductive type first doping region 21 and the first conductive type second doping region 23 are doped with N-type doping ions; the second conductive type first doping region 22 and the second conductive type second doping region 24 are doped with P-type doping ions. In some embodiments of the present invention, the first conductive type first doping region 21 and the first conductive type second doping region 23 are doped with P-type doping ions; the second conductive type first doping region 22 and the second conductive type second doping region 24 are doped with N-type doping ions.
[0127] S130, forming a gate trench on a surface of the semiconductor epitaxial layer away from the substrate.
[0128] Specifically, refer to Figure 6 , the semiconductor epitaxial layer 20 can be etched by a photolithography process to form a gate trench 01 in the semiconductor epitaxial layer 20; the gate trench 01 extends from the surface of the semiconductor epitaxial layer 20 away from the substrate 10 to the first conductive type first doping region 21. The photolithography process is an important step in the semiconductor device manufacturing process, which uses exposure and development to depict a geometric structure on the photoresist layer, and then transfers the pattern on the photomask to the mask layer through an etching process to achieve patterning of the photomask layer; and then etches the silicon carbide epitaxial layer exposed by the mask layer through an etching process to obtain a groove of a preset shape.
[0129] S140. Form a trench gate structure in the gate trench, the trench gate structure comprising a polysilicon gate and a first gate insulating layer located at the bottom of the polysilicon gate and a second gate insulating layer located at the sidewall of the polysilicon gate; wherein the dielectric constant of the material of the first gate insulating layer is greater than or equal to the dielectric constant of the material of the second gate insulating layer, and the dielectric constant of the material of the first gate insulating layer is greater than the dielectric constant of silicon oxide.
[0130] Specifically, refer to Figure 1 to Figure 3 The trench gate structure 30 includes a polysilicon gate 31, a first gate insulating layer 321 located at the bottom of the polysilicon gate 31, and a second gate insulating layer 322 located at the sidewall of the polysilicon gate 31. The material of the first gate insulating layer 321 is a high-k material with a dielectric constant greater than that of silicon oxide. Figure 1 In the embodiment, the material of the second gate insulating layer 322 is a high-k material having a dielectric constant greater than that of silicon oxide. Figure 2 In the embodiment, the material of the second gate insulating layer 322 is a high-k material having a dielectric constant greater than that of silicon oxide, and a third gate insulating layer 323 is provided between the first gate insulating layer 321 and the polysilicon gate 31, and the third gate insulating layer 323 is integrally provided with the second gate insulating layer 322. Figure 3 In the embodiment, the material of the second gate insulating layer 322 is silicon oxide material.
[0131] for Figure 1 The structure shown, reference Figures 8 to 16 Step S140 forms a trench gate structure 30 in the gate trench 01, specifically comprising:
[0132] S411 , forming a mask layer 50 on the surface of the semiconductor epitaxial layer 20 away from the substrate 10 and the wall of the gate trench 01 .
[0133] S412 , etching the mask layer 50 at the bottom of the gate trench 01 to expose the bottom of the gate trench 01 .
[0134] Specifically, refer to Figure 8 The mask layer 50 is a hard mask, and its material can be, for example, silicon nitride. After the mask layer 50 is formed on the surface of the semiconductor epitaxial layer 20 away from the substrate 10 and the sidewall and bottom of the gate trench 01, the mask layer 50 at the bottom of the gate trench 01 is etched by a photolithography process, thereby exposing the bottom of the gate trench 01.
[0135] S413 , forming a first gate initial insulating layer 61 on the surface of the mask layer 50 away from the substrate 10 , the surface of the mask layer 50 in the gate trench 01 away from the sidewall of the gate trench 01 , and the bottom of the gate trench 01 .
[0136] Specifically, refer to Fig. 9 , a high-k material may be deposited by, for example, an ALD deposition process to form the first gate initial insulating layer 61. Exemplarily, the high-k material includes, but is not limited to, oxides such as ZrO2, Al2O3, and HfO2.
[0137] S414 , forming a photoresist PR on the surface of the first gate initial insulating layer 61 away from the substrate 10 and in the gate trench 01 , and patterning the photoresist PR to form a plurality of openings 03 exposing the surface of the first gate initial insulating layer 61 away from the substrate 10 .
[0138] Specifically, refer to Fig.10 , apply photoresist PR so that the photoresist PR covers the surface of the first gate initial insulating layer 61 away from the substrate 10 and fills the gate trench 01; pattern the photoresist PR through an exposure and development process to form a plurality of openings 03 exposing the surface of the first gate initial insulating layer 61 away from the substrate 10.
[0139] S415 , etching the first gate initial insulating layer 61 and at least a portion of the mask layer 50 based on the opening 03 in the photoresist PR.
[0140] Specifically, refer to Fig.11 Based on the opening 03 in the photoresist PR, the first gate initial insulating layer 61 located on the surface of the mask layer 50 away from the substrate 10 is etched through, and at least a portion of the thickness of the mask layer 50 is continuously etched. Preferably, a portion of the thickness of the mask layer 50 is etched to avoid damage to the surface of the semiconductor epitaxial layer 20 caused by the etching process when the mask layer 50 is etched through.
[0141] S416 , removing the photoresist PR, and removing the mask layer 50 and the first gate initial insulating layer 61 on the surface of the mask layer 50 by means of an etching solution based on ultrasonic oscillation, so as to form a first gate insulating layer 321 at the bottom of the gate trench 01 .
[0142] Specifically, refer to Fig.12 and Fig.13 After removing the photoresist PR, the mask layer 50 is etched by an etching solution under ultrasonic oscillation to remove the mask layer 50 and the first gate initial insulating layer 61 attached to the mask layer 50. Since the first gate initial insulating layer 61 at the bottom of the gate trench 01 is not attached to the mask layer 50, the first gate initial insulating layer 61 at the bottom of the gate trench 01 is retained and used as the first gate insulating layer 321.
[0143] S417, forming a second gate initial insulating layer 62 on the surface of the semiconductor epitaxial layer 20 away from the substrate 10, the sidewall of the gate trench 01 and the surface of the first gate insulating layer 321; wherein the dielectric constant of the material of the second gate initial insulating layer 62 is greater than the dielectric constant of silicon oxide.
[0144] Specifically, refer to Fig.14 , a high-k material may be deposited by, for example, an ALD deposition process to form a second gate initial insulating layer 62. Exemplary, high-k materials include, but are not limited to, oxides such as ZrO2, Al2O3, and HfO2. The high-k material of the second gate initial insulating layer 62 may be the same as or different from the high-k material of the first gate initial insulating layer 61, and this is not limited in the embodiment of the present invention.
[0145] S418, by dry etching, remove the second gate initial insulating layer 62 located on the surface of the semiconductor epitaxial layer 20 away from the substrate 10, and remove the second gate initial insulating layer 62 located on the surface of the first gate insulating layer 321 away from the substrate 10, so as to form a second gate insulating layer 322 on the side wall of the gate trench 01.
[0146] Specifically, refer to Fig.15 , by dry etching, the second gate initial insulating layer 62 located on the surface of the semiconductor epitaxial layer 20 away from the substrate 10 is removed, and the second gate initial insulating layer 62 located on the surface of the first gate insulating layer 321 away from the substrate 10 is removed. The second gate initial insulating layer 62 located on the side wall of the gate trench 01 is retained and used as the second gate insulating layer 322.
[0147] S419, filling the gate trench 01 with polysilicon material to form a polysilicon gate 31. For details, please refer to Fig.16 .
[0148] Compared with conventional devices, the preparation method provided by the embodiment of the present invention can accurately control the thickness of the dielectric layer at the bottom and sidewall of the gate trench 01, so as to easily obtain a dielectric layer morphology with a thick bottom and thin sidewall. The thickness of the dielectric layer at the bottom of the gate trench 01 is determined by the first high-k deposition, and the thickness of the gate oxide layer on the sidewall is determined by the second high-k deposition. On the basis of using high-k material for the bottom gate oxide layer, the gate oxide layer of high-k material is also used for the sidewall of the trench, which can improve the electron mobility and increase the turn-on rate of the device.
[0149] for Figure 2 In the structure shown in FIG. 1 , step S140 forms a trench gate structure 30 in the gate trench 01 , including:
[0150] S421, forming a mask layer 50 on the surface of the semiconductor epitaxial layer 20 away from the substrate 10 and the wall of the gate trench 01. For details, please refer to step S411, which will not be repeated here.
[0151] S422, etching the mask layer 50 at the bottom of the gate trench 01 to expose the bottom of the gate trench 01. For details, please refer to step S412, which will not be described again.
[0152] S423, forming a first gate initial insulating layer on the surface of the mask layer 50 away from the substrate 10, the surface of the mask layer 50 in the gate trench away from the sidewall of the gate trench 01, and the bottom of the gate trench 01. For details, please refer to step S413, which will not be repeated here.
[0153] S424, forming a photoresist on the surface of the first gate initial insulating layer away from the substrate 10 and in the gate trench 01, and patterning the photoresist to form a plurality of openings 03 exposing the surface of the first gate initial insulating layer away from the substrate 10. For details, please refer to step S414, which will not be repeated here.
[0154] S425, based on the opening 03 in the photoresist, etching the first gate initial insulating layer and at least a portion of the mask layer 50. For details, please refer to step S415, which will not be described again.
[0155] S426, remove the photoresist, and remove the mask layer 50 and the first gate initial insulating layer on the surface of the mask layer 50 by etching liquid based on ultrasonic vibration to form a first gate insulating layer 321 at the bottom of the polysilicon gate 31. For details, please refer to step S416, which will not be repeated here.
[0156] S427, forming a second gate initial insulating layer on the surface of the semiconductor epitaxial layer 20 away from the substrate 10, the sidewall of the gate trench 01 and the surface of the first gate insulating layer 321; wherein the dielectric constant of the material of the second gate initial insulating layer is greater than the dielectric constant of silicon oxide. For details, please refer to step S417, which will not be repeated here.
[0157] S428 , filling the gate trench 01 with photoresist to cover the second gate initial insulating layer located in the gate trench 01 .
[0158] Specifically, refer to Fig.17 , fill the gate trench 01 with a photoresist PR, so that the photoresist PR covers the second gate initial insulating layer 62 located in the gate trench 01, that is, covers the second gate initial insulating layer 62 located on the side wall of the gate trench 01 and the second gate initial insulating layer 62 located at the bottom of the gate trench 01. The photoresist PR is used to protect the second gate initial insulating layer 62 located on the side wall of the gate trench 01 and the second gate initial insulating layer 62 located at the bottom of the gate trench 01 when the second gate initial insulating layer 62 located on the surface of the semiconductor epitaxial layer 20 away from the substrate 10 is dry-etched in step S429.
[0159] S429. Remove the second gate initial insulating layer 62 on the surface of the semiconductor epitaxial layer 20 away from the substrate 10 by dry etching to form a second gate insulating layer 322 on the side wall of the gate trench 01, and form a third gate insulating layer 323 on the surface of the first gate insulating layer 321 away from the substrate 10.
[0160] Specifically, refer to Fig.18 Based on the protection of the second gate initial insulating layer 62 located in the gate trench 01 by the photoresist PR, the second gate initial insulating layer 62 located on the surface of the semiconductor epitaxial layer 20 away from the substrate 10 can be removed by dry etching, and the second gate initial insulating layer 62 located in the gate trench 01 is retained, and the second gate initial insulating layer 62 located in the gate trench 01 is used as the second gate insulating layer 322, and the second gate initial insulating layer 62 located at the bottom of the gate trench 01 is used as the third gate insulating layer 323. Remove the photoresist PR.
[0161] S4210, filling the gate trench 01 with polysilicon material to form a polysilicon gate 31. For details, please refer to Fig.19 .
[0162] On the basis of the above-mentioned embodiment, in the embodiment of the present invention, by additionally adding a photolithography step, while depositing an excess high-k dielectric layer on the etching surface, the high-k material deposited for the second time at the bottom of the gate trench 01 is protected by the photoresist PR, thereby avoiding affecting the quality of the bottom gate oxide film during the overall dry etching.
[0163] In one embodiment of the present invention, for Figure 3 In the structure shown in FIG. 1 , step S140 forms a trench gate structure 30 in the gate trench 01 , which specifically includes:
[0164] S431, forming a mask layer 50 on the surface of the semiconductor epitaxial layer 20 away from the substrate 10 and the wall of the gate trench 01. For details, please refer to step S411, which will not be repeated here.
[0165] S432, etching the mask layer 50 at the bottom of the gate trench 01 to expose the bottom of the gate trench 01. For details, please refer to step S412, which will not be repeated here.
[0166] S433, forming a first gate initial insulating layer 61 on the surface of the mask layer 50 away from the substrate 10, the surface of the mask layer 50 in the gate trench away from the sidewall of the gate trench 01, and the bottom of the gate trench 01. For details, please refer to step S413, which will not be repeated here.
[0167] S434, forming a photoresist on the surface of the first gate initial insulating layer away from the substrate 10 and in the gate trench 01, and patterning the photoresist to form a plurality of openings 03 exposing the surface of the first gate initial insulating layer 61 away from the substrate 10. For details, please refer to step S414, which will not be repeated here.
[0168] S435, based on the opening 03 in the photoresist, etching the first gate initial insulating layer 61 and at least a portion of the mask layer 50. For details, please refer to step S415, which will not be described again.
[0169] S436, remove the photoresist PR, and remove the mask layer 50 and the first gate initial insulating layer 61 on the surface of the mask layer 50 by etching liquid based on ultrasonic vibration, so as to form a first gate insulating layer 321 at the bottom of the polysilicon gate 31. For details, please refer to step S416, which will not be repeated here.
[0170] S437, oxidizing the sidewall of the gate trench 01 and the surface of the semiconductor epitaxial layer 20 away from the substrate 10 by thermal oxidation to form a second gate initial insulating layer; the material of the second gate initial insulating layer includes silicon oxide. Fig. 20The sidewalls of the gate trench 01 and the surface of the semiconductor epitaxial layer 20 away from the substrate 10 are oxidized by thermal oxidation to form a second gate initial insulating layer 70 made of silicon oxide.
[0171] S438, filling the gate trench 01 with photoresist to cover the second gate initial insulating layer located in the gate trench 01. Fig.21 .
[0172] S439 , removing the second gate initial insulating layer on the surface of the semiconductor epitaxial layer 20 away from the substrate 10 by dry etching, so as to form a second gate insulating layer 322 on the sidewall of the gate trench 01 .
[0173] Specifically, refer to Fig. 22 Based on the protection of the second gate initial insulating layer 70 located in the gate trench 01 by the photoresist PR, the second gate initial insulating layer 70 located on the surface of the semiconductor epitaxial layer 20 away from the substrate 10 can be removed by dry etching, and the second gate initial insulating layer 70 located on the side wall of the gate trench 01 is retained, and the second gate initial insulating layer 70 located on the side wall of the gate trench 01 is used as the second gate insulating layer 322. Remove the photoresist PR.
[0174] S4310, filling the gate trench 01 with polysilicon material to form a polysilicon gate 31. Fig.23 .
[0175] On the basis of the above-mentioned embodiments, the preparation scheme provided in the embodiments of the present invention grows a SiO2 film layer on the side wall of the gate trench 01 by self-oxidation as the second gate insulating layer 322 of the side wall of the gate trench, without the need for an additional deposition process, thereby simplifying the preparation process of the device, saving production costs, and reducing manufacturing time. In addition, compared with the method of subsequently depositing high-k materials, the interface defects between the self-oxidized SiO2 and SiC are fewer, which is more conducive to the generation of channels.
[0176] Based on any of the above embodiments, the trench power device also includes: a source trench, located on opposite sides of the gate trench and spaced apart from the gate structure; a trench source structure 40, located in the source trench; the trench source structure 40 includes a polysilicon source 41, a first source insulating layer 421 located at the bottom of the polysilicon source 41, and a second source insulating layer 422 located at the side wall of the polysilicon source 41; the material of the first source insulating layer 421 is the same as the material of the first gate insulating layer 321; the material of the second source insulating layer 422 is the same as the material of the second gate insulating layer 322; wherein the semiconductor outer layer also includes a second conductive type second doping region 24, and the second conductive type second doping region 24 is located at the bottom and side wall of the trench source structure 40.
[0177] Therefore, reference Figure 6 , etching the semiconductor epitaxial layer 20, while forming a gate trench 01 in the semiconductor epitaxial layer 20, further comprising: forming a source trench 02 on opposite sides of the gate trench 01, and the source trench 02 is spaced apart from the gate trench 01. Figure 7 Before forming the trench gate structure 30 in the gate trench 01, the method further includes step S1401: implanting doping ions of the second doping type into the sidewall and bottom of the source trench 02 to form a second conductive type second doping region 24. Figure 8 to Figure 23 , while forming the trench gate structure 30 in the gate trench 01, it also includes: forming a trench source structure 40 in the source trench 02. The preparation method of forming the trench source structure 40 in the source trench 02 is the same as the method of forming the trench gate structure 30 in the gate trench 01. Among them, the first source insulating layer 421 and the first gate insulating layer 321 are formed simultaneously in the same process; the material of the second source insulating layer 422 and the second gate insulating layer 322 are formed simultaneously in the same process; the polysilicon source 41 and the polysilicon gate 31 are formed simultaneously in the same process. Figure 2 The semiconductor device shown further includes a third source insulating layer 423 between the polysilicon source 41 and the first source insulating layer 421 .
[0178] Based on the above embodiment, optionally, after step S140, the following further includes:
[0179] S140, forming an interlayer insulating layer ILD on a side of the semiconductor epitaxial layer 20 away from the substrate 10;
[0180] S150 , forming a source electrode S on a side of the interlayer insulating layer ILD away from the substrate 10 and on a surface of the semiconductor epitaxial layer 20 not covered by the interlayer insulating layer; forming a drain electrode D on a surface of the substrate 10 away from the semiconductor epitaxial layer 20 .
[0181] Specifically, an isolation dielectric material, such as SiO2 material, is deposited on the side of the semiconductor epitaxial layer 20 away from the substrate 10, thereby forming an interlayer insulating layer ILD covering the trench gate structure 30; then a source hole is opened. A Ti / TiN / Al metal layer is formed in the source hole as a source electrode S; SiO2 and / or SiN are deposited by PECVD to form a passivation layer, and polyimide is coated on the surface of the passivation layer to form a protective layer; backside thinning, metal deposition and other steps are performed to form a drain electrode D on the surface of the substrate 10 away from the semiconductor epitaxial layer 20.
[0182] An embodiment of the present invention further provides a power module, comprising a substrate and at least one trench-type power device according to any embodiment of the present invention, wherein the substrate is used to carry the trench-type power device. The same technical effects are achieved and will not be described in detail here.
[0183] According to another aspect of the present invention, there is provided a power conversion circuit, the power conversion circuit being used for one or more of current conversion, voltage conversion, and power factor correction;
[0184] The power conversion circuit comprises a circuit board and at least one trench power device as described in any embodiment of the present invention, and the trench power device is electrically connected to the circuit board. The same technical effects are achieved and will not be described in detail here.
[0185] According to another aspect of the present invention, a vehicle is provided, comprising a load and a power conversion circuit as described in any embodiment of the present invention, wherein the power conversion circuit is used to convert AC power into DC power, convert AC power into AC power, convert DC power into DC power, or convert DC power into AC power, and then input the power into the load. The same technical effects are achieved, and no further description is given here.
[0186] Note that the above are only preferred embodiments of the present invention and the technical principles used. Those skilled in the art will understand that the present invention is not limited to the specific embodiments described herein, and that various obvious changes, readjustments and substitutions can be made by those skilled in the art without departing from the scope of protection of the present invention. Therefore, although the present invention has been described in more detail through the above embodiments, the present invention is not limited to the above embodiments, and may include more other equivalent embodiments without departing from the concept of the present invention, and the scope of the present invention is determined by the scope of the appended claims.
Claims
1. A method for preparing a trench power device, characterized in that: include: providing a substrate; forming a semiconductor epitaxial layer on one side of the substrate; forming a gate trench on a surface of the semiconductor epitaxial layer away from the substrate; A trench gate structure is formed in the gate trench, wherein the trench gate structure includes a polysilicon gate, a first gate insulating layer located at the bottom of the polysilicon gate, and a second gate insulating layer located at the sidewall of the polysilicon gate; wherein the dielectric constant of the material of the first gate insulating layer is greater than or equal to the dielectric constant of the material of the second gate insulating layer, and the dielectric constant of the material of the first gate insulating layer is greater than the dielectric constant of silicon oxide; Forming a trench gate structure in the gate trench, comprising: forming a mask layer on a surface of the semiconductor epitaxial layer away from the substrate and a wall of the gate trench; Etching the mask layer at the bottom of the gate trench to expose the bottom of the gate trench; forming a first gate initial insulating layer on a surface of the mask layer away from the substrate, a surface of the mask layer in the gate trench away from the sidewall of the gate trench, and a bottom of the gate trench; Applying photoresist so that the photoresist covers the surface of the first gate initial insulating layer away from the substrate and fills the gate trench; Patterning the photoresist to form a plurality of openings exposing a surface of the first gate initial insulating layer away from the substrate; Based on the opening in the photoresist, etching the first gate initial insulating layer and at least a portion of the mask layer; The photoresist is removed, and the mask layer and the first gate initial insulating layer on the surface of the mask layer are removed by etching solution based on ultrasonic vibration to form a first gate insulating layer at the bottom of the gate trench.
2. The method for preparing a trench power device according to claim 1, characterized in that: forming a trench gate structure in the gate trench, further comprising: forming a second gate initial insulating layer on the surface of the semiconductor epitaxial layer away from the substrate, the sidewall of the gate trench, and the surface of the first gate insulating layer; wherein the dielectric constant of the material of the second gate initial insulating layer is greater than the dielectric constant of silicon oxide; By dry etching, the second gate initial insulating layer located on the surface of the semiconductor epitaxial layer away from the substrate is removed, and the second gate initial insulating layer located on the surface of the first gate insulating layer away from the substrate is removed, so as to form a second gate insulating layer on the sidewall of the gate trench; The gate trench is filled with polysilicon material to form a polysilicon gate.
3. The method for preparing a trench power device according to claim 1, characterized in that: forming a trench gate structure in the gate trench, further comprising: forming a second gate initial insulating layer on the surface of the semiconductor epitaxial layer away from the substrate, the sidewall of the gate trench, and the surface of the first gate insulating layer; wherein the dielectric constant of the material of the second gate initial insulating layer is greater than the dielectric constant of silicon oxide; Filling the gate trench with photoresist to cover the second gate initial insulating layer located in the gate trench; Removing the second gate initial insulating layer on the surface of the semiconductor epitaxial layer away from the substrate by dry etching to form a second gate insulating layer on the sidewall of the gate trench, and forming a third gate insulating layer on the surface of the first gate insulating layer away from the substrate; The gate trench is filled with polysilicon material to form a polysilicon gate.
4. The method for preparing a trench power device according to claim 1, characterized in that: forming a trench gate structure in the gate trench, further comprising: Oxidizing the sidewalls of the gate trench by thermal oxidation to form a second gate insulating layer on the sidewalls of the gate trench; the material of the second gate insulating layer includes silicon oxide; The gate trench is filled with polysilicon material to form a polysilicon gate.
5. The method for preparing a trench power device according to any one of claims 2 to 4, characterized in that: The semiconductor epitaxial layer is etched to form a gate trench in the semiconductor epitaxial layer, and further comprises: Forming source trenches on opposite sides of the gate trench, and the source trench is spaced apart from the gate trench; Before forming a trench gate structure in the gate trench, the method further includes: Implanting doping ions of a second doping type into the sidewalls and bottom of the source trench to form a second doping region of a second conductivity type; While forming a trench gate structure in the gate trench, the method further comprises: A trench source structure is formed in the source trench; wherein the trench source structure includes a polysilicon source, a first source insulating layer located at the bottom of the polysilicon source, and a second source insulating layer located at the side wall of the polysilicon source; the first source insulating layer and the first gate insulating layer are formed synchronously in the same process; the material of the second source insulating layer and the second gate insulating layer are formed synchronously in the same process; the polysilicon source and the polysilicon gate are formed synchronously in the same process.
6. A trench power device, characterized in that: The method for preparing a trench power device according to any one of claims 1 to 5 comprises: substrate; A semiconductor epitaxial layer, located on one side of the substrate; A gate trench is located on a surface of the semiconductor epitaxial layer away from the substrate; A trench gate structure is located in the gate trench; the trench gate structure includes a polysilicon gate and a first gate insulating layer located at the bottom of the polysilicon gate and a second gate insulating layer located at the sidewall of the polysilicon gate; The dielectric constant of the material of the first gate insulating layer is greater than or equal to the dielectric constant of the material of the second gate insulating layer, and the dielectric constant of the material of the first gate insulating layer is greater than the dielectric constant of silicon oxide.
7. The trench power device according to claim 2, characterized in that: The dielectric constant of the material of the second gate insulating layer is greater than the dielectric constant of silicon oxide; The thickness of the first gate insulating layer is greater than the thickness of the second gate insulating layer located on the sidewall of the polysilicon gate.
8. The trench power device according to claim 7, characterized in that: Also includes: a third gate insulating layer, the third gate insulating layer being located between the first gate insulating layer and the polysilicon gate; The third gate insulating layer is made of the same material as the second gate insulating layer, and the third gate insulating layer and the second gate insulating layer are integrally arranged.
9. The trench power device according to claim 6, characterized in that: The material of the second gate insulating layer includes silicon oxide.
10. The trench power device according to claim 6, characterized in that: Along the direction of the semiconductor epitaxial layer away from the substrate, the semiconductor epitaxial layer includes a first conductive type first doping region, a second conductive type first doping region and a first conductive type second doping region in sequence; the gate trench extends from a surface of the semiconductor epitaxial layer away from the substrate to the first conductive type first doping region; The first conductive type first doping region and the first conductive type second doping region are doped with N-type doping ions; The second conductive type first doping region is doped with P-type doping ions; Alternatively, the first conductive type first doping region and the first conductive type second doping region are doped with P-type doping ions; and the second conductive type first doping region is doped with N-type doping ions.
11. The trench power device according to any one of claims 7 to 10, characterized in that: Also includes: A source trench, located at two opposite sides of the gate trench and spaced apart from the gate trench; A trench source structure, located in the source trench; The trench source structure includes a polysilicon source, a first source insulating layer located at the bottom of the polysilicon source, and a second source insulating layer located at the sidewall of the polysilicon source; The material of the first source insulating layer is the same as that of the first gate insulating layer; the material of the second source insulating layer is the same as that of the second gate insulating layer; The semiconductor epitaxial layer further includes a second conductive type second doping region, and the second conductive type second doping region is located at the bottom and sidewall of the trench source structure.
12. The trench power device according to claim 11, characterized in that: Also includes: an interlayer insulating layer, located on a side of the semiconductor epitaxial layer away from the substrate and covering the trench gate structure; A source electrode, located on a side of the interlayer insulating layer away from the substrate, and on a surface of the semiconductor epitaxial layer not covered by the interlayer insulating layer; The drain electrode is located on a surface of the substrate away from the semiconductor epitaxial layer.
13. A power module, characterized in that: It comprises a substrate and at least one trench type power device as claimed in any one of claims 6 to 12, wherein the substrate is used to support the trench type power device.
14. A power conversion circuit, characterized in that: The power conversion circuit is used for one or more of current conversion, voltage conversion, and power factor correction; The power conversion circuit comprises a circuit board and at least one trench power device as claimed in any one of claims 6 to 12, wherein the trench power device is electrically connected to the circuit board.
15. A vehicle, characterized in that: It includes a load and a power conversion circuit as described in claim 14, wherein the power conversion circuit is used to convert AC power into DC power, convert AC power into AC power, convert DC power into DC power, or convert DC power into AC power and then input it into the load.