Electrolytic cathode with hydrophobic microtexture on processing surface

By designing a hydrophobic microtexture on the processing surface of the electrolytic cathode, the problem of reduced electrolyte flow rate is solved and stable and efficient processing of electrolytic milling is achieved.

CN118720303APending Publication Date: 2024-10-01GUANGDONG UNIV OF TECH
View PDF 0 Cites 1 Cited by

Patent Information

Application Number
CN202410978804.2
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-19
Publication Date
2024-10-01

AI Technical Summary

Technical Problem

In the existing electrolytic milling technology, the friction between the electrolyte and the cathode surface causes the flow rate to decrease, affecting the processing speed and stability.

Method used

Design an electrolytic cathode with a hydrophobic micro-texture, including a liquid storage chamber and a cathode sheet. The processed surface of the cathode sheet is provided with a hydrophobic micro-texture, such as a mesh microstructure or a micro-pit array structure, to reduce the interaction between the electrolyte and the cathode sheet. The friction between them increases the flow rate.

Benefits of technology

By reducing friction, the electrolyte can flow at high speed on the processing surface of the cathode sheet, flushing products and heat in time, improving processing speed and stability.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118720303A_ABST
    Figure CN118720303A_ABST
Patent Text Reader

Abstract

The invention discloses an electrolytic cathode with a machining surface provided with a hydrophobic microstructure. The electrolytic cathode comprises a liquid storage cavity used for storing electrolyte and a cathode piece used for electrolytic machining. Wherein the cathode plate is arranged at the bottom of the liquid storage cavity; a liquid outlet is formed in the bottom, close to the machining surface of the cathode plate, of the liquid storage cavity, and electrolyte is sprayed out through the liquid outlet and tightly attached to the machining surface of the cathode plate to enter the machining gap; the machining surface of the cathode piece is provided with a hydrophobic microstructure, during machining, the friction force between electrolyte and the machining surface of the cathode piece can be greatly reduced, it is guaranteed that the electrolyte flows at a high speed on the machining surface of the electrolytic cathode, the electrolyte enters a machining gap at a high flow speed, electrolytic products and electrolytic heat are washed and taken away in time, stable electrolytic milling is guaranteed, and the service life of the electrolytic cathode piece is prolonged. And the processing speed and quality are improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of electrolytic processing, and in particular to an electrolytic cathode with a processed surface having a hydrophobic micro-texture. Background Art

[0002] Electrolytic machining is the removal of metal workpiece materials through anodic dissolution. It has the advantages of high machining efficiency, high surface quality, no tool loss, and no machining force. It is widely used in aerospace, automobile, mold and other fields.

[0003] Electrolytic milling uses simple tools and computer programming to form the workpiece profile with the envelope surface of the tool cathode motion trajectory. It combines the advantages of CNC technology and electrolytic process and has great development potential. Electrolytic milling in the prior art, for example, the invention patent with authorization announcement number CN109332826B discloses an electrolytic milling method and device for processing gaps by direct injection of electrolyte against the wall; this invention patent uses electrolytic milling technology with sheet-shaped cathodes and direct injection of electrolyte against the wall, which has unique technical advantages. The electrolyte is directly injected along the cathode wall to process the gap, which can obtain a higher and more uniform flow field distribution. At the same time, there is no flow field lack of liquid when the cathode "cuts in and out" the workpiece and "adjacent", which solves the key technical problem that electrolytic milling cannot be promoted and applied. However, the above technology also has the following shortcomings in practical applications:

[0004] When the electrolyte flows along the cathode wall, the electrolyte will inevitably generate friction with the cathode surface. When the cathode length increases, the friction resistance of the electrolyte along the cathode wall also increases, which seriously reduces the electrolyte flow rate. Electrolytic machining is extremely sensitive to the electrolyte flow rate. Therefore, reducing the electrolyte flow resistance is of great significance to improving the speed and stability of electrolytic machining. Summary of the invention

[0005] The purpose of the present invention is to overcome the above-mentioned problems and provide an electrolytic cathode with a hydrophobic microtexture on the processing surface. When the electrolytic cathode is processed, the friction between the electrolyte and the processing surface of the electrolytic cathode is reduced, and the electrolyte can flow at a high speed on the processing surface of the electrolytic cathode, so that the electrolyte maintains a high flow rate to enter the processing gap, flush and carry away the electrolytic products and electrolytic heat in time, ensure the stable progress of electrolytic milling, and improve the processing speed.

[0006] The purpose of the present invention is achieved through the following technical solutions:

[0007] An electrolytic cathode with a processed surface having a hydrophobic microtexture comprises a liquid storage chamber for storing electrolyte and a cathode sheet for electrolytic processing; wherein the cathode sheet is arranged at the bottom of the liquid storage chamber; the bottom of the liquid storage chamber is provided with a liquid outlet for draining the electrolyte in the liquid storage chamber to the processed surface of the cathode sheet; the processed surface of the cathode sheet is provided with a hydrophobic microtexture.

[0008] The working principle of the electrolytic cathode with hydrophobic microtexture on the processed surface is:

[0009] During processing, the electrolyte in the liquid storage chamber is sprayed out from the liquid outlet and enters the processing gap closely adhering to the processing surface of the cathode sheet; electrolytic processing is realized, and the electrolyte flows on the processing surface of the cathode sheet. Since the processing surface of the cathode sheet is provided with a hydrophobic microtexture, the friction between the electrolyte and the processing surface of the cathode sheet can be minimized to the greatest extent, thereby reducing the impact on the flow rate of the electrolyte.

[0010] In a preferred embodiment of the present invention, the hydrophobic microtexture is a mesh microstructure. By providing the mesh microstructure, the hydrophobicity of the processed surface of the cathode sheet can be further improved, and the flow rate of the electrolyte can be increased.

[0011] Preferably, the mesh microstructure is composed of a plurality of micro-line pits interwoven and connected. In the above structure, a plurality of micro-line pits are interwoven and connected to form a mesh surface, and the shape of the above structure is a fishing net or fabric. The mesh microstructure is a three-dimensional structure, and a plurality of micro-line pits are interwoven and connected to each other so that the processing surface has a large number of intersections and pores, which can form a plurality of air pockets, and the air pockets can capture and retain air, thereby forming an air layer, which has good air permeability and can significantly enhance the surface hydrophobicity. In addition, the surface roughness of the mesh microstructure is also high, which can increase the contact angle between the electrolyte and the processing surface of the cathode sheet, resulting in the electrolyte showing strong cohesion on the processing surface, so that it is not easy to maintain a stable state on the processing surface, making the processing surface of the cathode sheet more hydrophobic.

[0012] In a preferred embodiment of the present invention, the hydrophobic microtexture is a micro-pit array structure. By providing the micro-pit array structure, the hydrophobicity of the processed surface of the cathode sheet can be further improved, and the flow rate of the electrolyte can be increased.

[0013] Preferably, the micro-pit array structure includes a plurality of micro-grooves arranged on the processing surface of the cathode sheet, and the plurality of micro-grooves are arranged in an array. In the above structure, the plurality of micro-grooves are arranged in an array, that is, the plurality of micro-grooves are neatly arranged on the processing surface and distributed on the processing surface of the cathode sheet in an array form. Each micro-groove of the above structure exists independently, and the droplets of the electrolyte form a high contact angle between the micro-grooves through the action of surface tension, showing excellent hydrophobicity. The micro-pit array structure has a stable structure and high durability.

[0014] Furthermore, the arrangement of the plurality of micro groove arrays is a rectangular array, which makes the micro grooves arranged very evenly, thus ensuring the uniformity of the electrolyte flow.

[0015] Preferably, the upper end of the cathode sheet is inserted into the liquid storage cavity from the bottom of the liquid storage cavity. The above structure is adopted for the purpose of, on the one hand, facilitating the installation of the cathode sheet, and on the other hand, allowing the electrolyte in the liquid storage cavity to cover the processing surface of the cathode sheet, so that the electrolyte can enter the processing gap along the processing surface of the cathode sheet.

[0016] Preferably, the liquid outlet is located on one side of the processing surface of the cathode sheet. In the above structure, the liquid outlet is arranged at the connection between the bottom of the liquid storage cavity and the processing surface of the cathode sheet, so that the electrolyte can be sprayed out from the liquid outlet and enter the processing gap along the processing surface of the cathode sheet to realize electrolytic processing.

[0017] Preferably, a through hole is provided at the bottom of the liquid storage cavity, and the upper end of the cathode sheet extends into the through hole and into the liquid storage cavity; the back of the cathode sheet is tightly fitted and fixedly connected to one side of the through hole, and there is a gap between the processing surface of the cathode sheet and the other side of the through hole, and the gap constitutes the liquid outlet. With the above structure, by setting a through hole, the installation of the cathode sheet is facilitated, the back of the cathode sheet is tightly fitted and fixedly connected to one side of the through hole, and the sealing is ensured, and the electrolyte can be prevented from entering the back of the cathode sheet, and there is a gap between the processing surface of the cathode sheet and the other side of the through hole, and the gap constitutes the liquid outlet, so that during processing, the electrolyte can flow out from the liquid outlet and flow down along the processing surface of the cathode sheet, and enter the processing gap along the processing surface of the cathode sheet to achieve electrolytic processing.

[0018] Preferably, the hydrophobic microtexture is processed by one of laser machining, electrolytic machining, electric spark machining and chemical etching.

[0019] Compared with the prior art, the present invention has the following beneficial effects:

[0020] 1. The electrolytic cathode of the present invention has a processing surface with a hydrophobic microtexture. Since the processing surface of the cathode sheet is provided with a hydrophobic microtexture, the friction between the electrolyte and the processing surface of the cathode sheet can be reduced to the greatest extent, thereby reducing the impact on the flow rate of the electrolyte, thereby ensuring that the electrolyte can maintain a high flow rate, timely flushing and taking away the electrolytic products and electrolytic heat, ensuring the stable progress of electrolytic milling, obtaining a good electrolytic machining effect, and improving the machining speed.

[0021] 2. The electrolytic cathode with a hydrophobic microtexture on the processing surface in the present invention has a novel concept and a simple structure, and can greatly improve the electrolytic processing performance. BRIEF DESCRIPTION OF THE DRAWINGS

[0022] Figure 1 This is a schematic diagram of the internal structure of an electrolytic cathode with a processed surface having a hydrophobic microtexture in the present invention.

[0023] Figure 2 It is a schematic structural diagram of the first specific implementation mode of the cathode sheet in the present invention.

[0024] Figure 3 It is a schematic structural diagram of a second specific implementation mode of the cathode sheet in the present invention. DETAILED DESCRIPTION

[0025] In order to enable those skilled in the art to better understand the technical solution of the present invention, the present invention is further described below in conjunction with embodiments and drawings, but the embodiments of the present invention are not limited thereto.

[0026] Example 1

[0027] See also Figure 1 This embodiment discloses an electrolytic cathode with a processed surface having a hydrophobic microtexture, comprising a liquid storage chamber 1 for storing an electrolyte 2 and a cathode sheet 3 for electrolytic processing; wherein the cathode sheet 3 is arranged at the bottom of the liquid storage chamber 1; the bottom of the liquid storage chamber 1 is provided with a liquid outlet 4 for draining the electrolyte 2 in the liquid storage chamber 1 to the processed surface of the cathode sheet 3; the processed surface of the cathode sheet 3 is provided with a hydrophobic microtexture 5.

[0028] See also Figure 1 The processing surface of the cathode sheet 3 is a surface on which the workpiece is processed. The processing surface of the cathode sheet 3 is a plane or a cylinder, and its purpose is to ensure that the electrolyte 2 always flows closely to the processing surface at a high speed.

[0029] See also Figure 1 The electrolytic cathode in this embodiment has a hydrophobic micro-texture 5 on the processing surface, which has the advantage of low friction resistance, ensuring that the electrolyte 2 can enter the processing gap with minimal speed loss, thereby obtaining a good electrolytic processing effect. If there is no hydrophobic micro-texture 5 on the cathode sheet 3, the electrolyte 2 will directly rush downward from the liquid outlet 4 along the cathode sheet 3. Due to the effect of friction, the flow rate of the liquid will be slower as it goes downward, which has a great impact on the progress of electrolytic processing, especially in the processing of large aspect ratio holes, which will cause the processing products to be unable to be discharged in time, and in severe cases, will cause a short circuit. In this embodiment, processing a hydrophobic micro-texture 5 of about 10μm on the surface of the cathode sheet 3 can effectively improve this problem. The micro-texture of the super-hydrophobic surface can capture and retain air to form a stable gas lubrication layer. This layer of gas is located on the cathode sheet. 3 and the electrolyte 2, reducing the direct contact area between the electrolyte 2 and the cathode sheet 3, and because the viscosity of the gas is much lower than the viscosity of the liquid and the cathode sheet 3, the gas lubrication layer can significantly reduce the friction. The super-hydrophobic surface prevents the electrolyte 2 from forming a continuous liquid film on the surface through high contact angle and low rolling angle, reducing the retention and expansion of the electrolyte 2. This significantly reduces the resistance and friction encountered by the electrolyte 2 when sliding on the processed surface of the cathode sheet 3. Compared with the cathode sheet 3 without micro-texture, the cathode sheet 3 with a processed surface provided with hydrophobic micro-texture 5 increases the flow rate of the electrolyte 2 by 1-2 times.

[0030] See also Figure 1-Figure 2 The hydrophobic microtexture 5 is a mesh microstructure. By providing the mesh microstructure, the hydrophobicity of the processed surface of the cathode sheet 3 can be further improved, and the flow rate of the electrolyte 2 can be increased.

[0031] See also Figure 1-Figure 2 , the mesh microstructure is composed of a plurality of micro-line pits 6 interwoven and connected with each other. In the above structure, a plurality of micro-line pits 6 are interwoven and connected with each other to form a mesh surface. The shape of the above structure is a fishing net or a fabric. The mesh microstructure is a three-dimensional structure. A plurality of micro-line pits 6 are interwoven and connected with each other so that the processing surface has a large number of intersections and pores, which can form a plurality of air pockets. The air pockets can capture and retain air, thereby forming an air layer with good air permeability, which can significantly enhance the surface hydrophobicity. In addition, the surface roughness of the mesh microstructure is also high, which can increase the contact angle between the electrolyte 2 and the processing surface of the cathode sheet 3, resulting in the electrolyte 2 showing strong cohesion on the processing surface, so that it is not easy to maintain a stable state on the processing surface, making the processing surface of the cathode sheet 3 more hydrophobic.

[0032] See also Figure 1 , the upper end of the cathode sheet 3 is inserted into the liquid storage chamber 1 from the bottom of the liquid storage chamber 1. The above structure is adopted for the purpose of, on the one hand, facilitating the installation of the cathode sheet 3, and on the other hand, allowing the electrolyte 2 in the liquid storage chamber 1 to cover the processing surface of the cathode sheet 3, so that the electrolyte 2 can enter the processing gap along the processing surface of the cathode sheet 3.

[0033] See also Figure 1 , the liquid outlet 4 is located on one side of the processing surface of the cathode sheet 3. In the above structure, the liquid outlet 4 is arranged at the connection between the bottom of the liquid storage chamber 1 and the processing surface of the cathode sheet 3, so that the electrolyte 2 can be sprayed out from the liquid outlet 4 and enter the processing gap along the processing surface of the cathode sheet 3 to realize electrolytic processing.

[0034] See also Figure 1 , a through hole is provided at the bottom of the liquid storage chamber 1, and the upper end of the cathode sheet 3 extends into the through hole and into the liquid storage chamber 1; the back of the cathode sheet 3 is tightly fitted and fixedly connected to one side of the through hole, and there is a gap between the processing surface of the cathode sheet 3 and the other side of the through hole, and the gap constitutes the liquid outlet 4. With the above structure, by providing a through hole, the installation of the cathode sheet 3 is facilitated, the back of the cathode sheet 3 is tightly fitted and fixedly connected to one side of the through hole, and the sealing is ensured, and the electrolyte 2 can be prevented from entering the back of the cathode sheet 3, and there is a gap between the processing surface of the cathode sheet 3 and the other side of the through hole, and the gap constitutes the liquid outlet 4, so that during processing, the electrolyte 2 can flow out from the liquid outlet, flow down along the processing surface of the cathode sheet 3, and enter the processing gap along the processing surface of the cathode sheet 3 to achieve electrolytic processing.

[0035] See also Figure 1 The back side of the cathode sheet 3 is a side opposite to the processed side of the cathode sheet 3 , one side of the cathode sheet 3 is the processed side, and the other side is the back side.

[0036] See also Figure 1 The hydrophobic micro texture 5 is processed by one of laser processing, electrolytic processing, electric spark processing and chemical etching.

[0037] See also Figure 1 The electrolytic machining cathode includes a liquid storage tank, and the liquid storage chamber 1 is located inside the liquid storage tank.

[0038] See also Figure 1 The working principle of the electrolytic cathode with hydrophobic microtexture on the processed surface is:

[0039] During processing, the electrolyte 2 in the liquid storage chamber 1 is ejected from the liquid outlet 4 and enters the processing gap closely adhering to the processing surface of the cathode sheet 3; electrolytic processing is realized, and the electrolyte 2 flows on the processing surface of the cathode sheet 3. Since the processing surface of the cathode sheet 3 is provided with a hydrophobic microtexture 5, the friction between the electrolyte 2 and the processing surface of the cathode sheet 3 can be minimized to the greatest extent, thereby reducing the impact on the flow rate of the electrolyte 2.

[0040] Example 2

[0041] See also Figure 1 and Figure 3 The other structures of this embodiment are the same as those of embodiment 1, except that the hydrophobic microtexture 5 is a micro-pit array structure. By providing the micro-pit array structure, the hydrophobicity of the processed surface of the cathode sheet 3 can be further improved, and the flow rate of the electrolyte 2 can be increased.

[0042] See also Figure 1 and Figure 3 , the micro-pit array structure includes a plurality of micro-grooves 7 arranged on the processing surface of the cathode sheet 3, and the plurality of micro-grooves 7 are arranged in an array. In the above structure, the plurality of micro-grooves 7 are arranged in an array, that is, the plurality of micro-grooves 7 are neatly arranged on the processing surface, and are distributed on the processing surface of the cathode sheet 3 in an array form. Each micro-groove 7 of the above structure exists independently, and the droplets of the electrolyte 2 form a high contact angle between the micro-grooves 7 through the action of surface tension, showing excellent hydrophobicity, and the micro-pit array structure has a stable structure and high durability.

[0043] See also Figure 1 and Figure 3 The array arrangement of the plurality of micro grooves 7 is a rectangular array, that is, arranged along the horizontal direction and the vertical direction. The rectangular array makes the micro grooves 7 arranged very evenly, ensuring the uniformity of the flow of the electrolyte 2.

[0044] Example 3

[0045] The other structures of this embodiment are the same as those of the embodiment 1, except that the processed surface of the cathode sheet 3 is provided with a hydrophobic structure imitating the surface of a lotus leaf or an insect. The hydrophobic structure can replace the hydrophobic microtexture 5 in the embodiment 1, or can be provided together with the hydrophobic microtexture 5 in the embodiment 1 to improve the hydrophobic effect. Furthermore, the micro grooves 7 penetrate the cathode sheet 3, and the electrolyte 2 flows on the processed surface of the cathode sheet 3. The high-speed flowing electrolyte 2 will suck the air on the back of the cathode sheet 3 through the micro grooves 7, forming an air film on the processed surface of the cathode sheet 3, which has a hydrophobic effect and greatly reduces friction.

[0046] Example 4

[0047] The hydrophobic micro-texture 5 in this embodiment is a structure that combines the mesh microstructure of Example 1 and the micro-pit array structure of Example 2. The combination of the two further improves the hydrophobic effect. The micro-grooves 7 run through the cathode sheet 3. The micro-grooves 7 are arranged at intersections. The points where a plurality of micro-line pits 6 are intertwined and connected are intersections. A plurality of micro-line pits 6 arranged at 45° are intertwined and connected with a plurality of micro-line pits 6 arranged at 135°. The air on the back of the cathode sheet 3 is sucked in by the micro-grooves 7, and the air can more easily enter the micro-line pits 6, thereby achieving a hydrophobic effect.

[0048] The above is a preferred embodiment of the present invention, but the embodiment of the present invention is not limited to the above content. Any other changes, modifications, substitutions, combinations, and simplifications made without departing from the spirit and principles of the present invention should be equivalent replacement methods and are included in the protection scope of the present invention.

Claims

1. An electrolytic cathode having a processed surface with a hydrophobic microtexture, characterized in that: It comprises a liquid storage chamber for storing electrolyte and a cathode sheet for electrolytic processing; wherein the cathode sheet is arranged at the bottom of the liquid storage chamber; the bottom of the liquid storage chamber is provided with a liquid outlet for draining the electrolyte in the liquid storage chamber to the processing surface of the cathode sheet; the processing surface of the cathode sheet is provided with a hydrophobic microtexture.

2. The electrolytic cathode having a processed surface with a hydrophobic microtexture according to claim 1, characterized in that: The hydrophobic micro-texture is a network micro-structure.

3. The electrolytic cathode with a processed surface having a hydrophobic microtexture according to claim 2, characterized in that: The mesh microstructure is composed of a plurality of micro line pits that are interwoven and connected with each other.

4. The electrolytic cathode with a processed surface having a hydrophobic microtexture according to claim 1, characterized in that: The hydrophobic micro texture is a micro pit array structure.

5. The electrolytic cathode with a processed surface having a hydrophobic microtexture according to claim 4, characterized in that: The micro-pit array structure includes a plurality of micro-grooves arranged on the processing surface of the cathode sheet, and the plurality of micro-grooves are arranged in an array.

6. The electrolytic cathode with a processed surface having a hydrophobic microtexture according to claim 5, characterized in that: The arrangement of the plurality of micro groove arrays is a rectangular array.

7. The electrolytic cathode with a processed surface having a hydrophobic microtexture according to claim 1, characterized in that: The upper end of the cathode sheet is inserted into the liquid storage cavity from the bottom of the liquid storage cavity.

8. The electrolytic cathode with a processed surface having a hydrophobic microtexture according to claim 7, characterized in that: The liquid outlet is located at one side of the processing surface of the cathode sheet.

9. The electrolytic cathode with a processed surface having a hydrophobic microtexture according to claim 1, characterized in that: A through hole is provided at the bottom of the liquid storage cavity, and the upper end of the cathode sheet extends into the through hole and into the liquid storage cavity; the back side of the cathode sheet is tightly fitted and fixedly connected to one side of the through hole, and there is a gap between the processed surface of the cathode sheet and the other side of the through hole, and the gap constitutes the liquid outlet.

10. The electrolytic cathode with a processed surface having a hydrophobic microtexture according to claim 1, characterized in that: The hydrophobic microtexture is processed by one of laser processing, electrolytic processing, electric spark processing and chemical etching.

Citation Information

Cited By

  • Flexible braided electrode and method for electrochemical polishing of complex inner channel