Busbar processing technology and device
Through the process of combining the automatic wrapping machine and the hot press, the air gap between the insulation layer and the conductor core during busbar processing is eliminated, solving the problem of low insulation performance, achieving high-quality coating effect and improving production efficiency. promote.
Patent Information
- Application Number
- CN202410754038.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-06-12
- Publication Date
- 2024-10-01
AI Technical Summary
During the busbar processing process, the insulation performance is reduced due to the air gap between the insulation layer and the conductor core. It is difficult to effectively eliminate the air gap with existing technology, affecting the insulation performance and compactness.
Using a process that combines an automatic wrapping machine and a hot press, preheating the lower heating plate and hot pressing the upper heating plate ensures that the wrapping tape is tightly combined with the inner core of the conductor to eliminate air gaps, and is sintering in a tunnel furnace to form High quality cladding.
Effectively eliminate the air between the conductor core and the insulation layer, improve the insulation performance and compactness, reduce the production cycle, and improve production efficiency and output.
Smart Images

Figure CN118737580A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the technical field of busbar processing, and in particular to a busbar processing technology and device. Background Art
[0002] Busbar, also known as motherboard, is the conductive material on the power distribution equipment, and its main function is to act as a conductor. It is usually made of copper or aluminum, with an insulating coating structure on the surface, and is used to connect the main switch in the electrical cabinet with the switches in each branch circuit to achieve the distribution and transmission of electrical energy.
[0003] The coating methods of the conductor core are generally divided into two methods: overall coating and wrapping according to the characteristics of the insulating material and the requirements of use. Among them, the wrapping process is to wrap various strip-shaped insulation layers spirally onto the conductor core at a specified pitch.
[0004] However, due to the presence of gaps or bubbles in the insulation layer itself and the special-shaped structure of the conductor core, during the wrapping process, the insulation layer forms gaps on the surface of the conductor core, causing air to be wrapped around the conductor core. The air is wrapped between the insulation layer and the conductor core, forming an air gap, which reduces the continuity and density of the insulation layer, thereby reducing the insulation performance of the wrapping. Therefore, a busbar processing technology and device are proposed to solve the above technical problems. Summary of the invention
[0005] The present application provides a busbar processing technology and device, which can effectively eliminate the air in the air gap between the insulation layer and the conductor core, so that the conductor core and the insulation layer are combined into one, thereby increasing the insulation strength and reducing the leakage rate.
[0006] The present application provides a busbar processing technology and device, which adopts the following technical solutions: A busbar processing technology and device, the busbar processing device includes a processing platform, the processing platform is provided with a material guide path for conveying a conductor inner core, the processing platform and along the material guide path are provided with an automatic wrapping machine for automatically wrapping the conductor inner core and a hot press for hot pressing the conductor inner core in sequence, the wrapped conductor inner core along the material guide path and transmitted by the automatic wrapping machine enters a configuration mold on the hot press, the hot press includes a hot pressing frame, the interior of the hot pressing frame is provided with a lower heating plate and an upper heating plate that slides up and down, the configuration mold is placed on the lower heating plate, the configuration mold is first preheated, the heat generated by the preheating is transmitted to the surface of the wrapped conductor inner core in all directions through the configuration mold, and then the wrapped conductor inner core is hot pressed by the upper heating plate that slides up and down, so as to heat the wrapped conductor inner core.
[0007] By adopting the above technical scheme, the inner core of the wrapped conductor in the configuration mold is preheated by the lower heating plate, so that the wrapping tape becomes soft, the wrapping tape and the conductor inner core are tightly combined, and corresponding thermal curing conditions are provided to form a strong bond between the wrapped conductor inner core and the wrapping tape; then, the upper surface of the wrapped conductor inner core is hot-pressed by the upper heating plate, so that the wrapped conductor inner core and the wrapping tape can be combined into one, air gaps and air are eliminated, and a high-quality coating effect is ensured.
[0008] Preferably, a coil unwinding rack is provided on the processing platform, and the coil unwinding rack is located at one side of the conductor inner core input end of the automatic wrapping machine.
[0009] By adopting the above technical solution, the conductor core is automatically input into the automatic wrapping machine through the coil unwinding rack. The setting of the coil unwinding rack can replace part of the manual operation and reduce the demand for human resources.
[0010] Preferably, a tunnel furnace is provided on the processing platform, and the tunnel furnace is located on one side of the output end of the hot press.
[0011] By adopting the above technical solution, after sintering in a tunnel furnace, PTFE is coated on the surface of the hot-pressed conductor inner core to form a sheath, and a sintered conductor inner core is obtained.
[0012] Preferably, the internal sintering temperature of the tunnel furnace is in the range of 400° C.-450° C., and the conveying speed of the conductor core in the tunnel furnace is in the range of 5-8 m / min.
[0013] By adopting the above technical solution, during the hot pressing to sintering process, the internal sintering temperature of the tunnel furnace is significantly higher than the heating temperature of the hot press, and the temperature is gradually increased, which helps to reduce the temperature gradient difference and avoid the generation of thermal stress.
[0014] Preferably, it also includes a traction device arranged on the processing platform, and the traction device is located on one side of the output end of the tunnel furnace.
[0015] By adopting the above technical solution, the sintered conductor core can be conveniently transferred from the inside of the tunnel furnace to the subsequent processing equipment through the traction device, thereby improving the convenience and efficiency of the conductor core transmission.
[0016] Preferably, the conductor inner core sintered in the tunnel furnace is pulled into a coil receiving rack arranged on the processing platform by the pulling device.
[0017] By adopting the above technical solution, a traction device is used to achieve convenient material transportation, thereby improving production efficiency and work efficiency.
[0018] Preferably, a cylinder is provided on the hot pressing frame, and an output end of the cylinder is connected to the upper surface of the upper heating plate.
[0019] By adopting the above technical solution, the upper heating plate is pushed by the cylinder so that the pressure applied by the upper heating plate to the preheated conductor core is constant, thereby ensuring that the preheated conductor core is evenly heated during the hot pressing process, so that the product achieves consistent temperature distribution and heat treatment effect, thereby improving the quality stability of the product.
[0020] Preferably, the preheating temperature range of the lower heating plate is 110° C.-150° C., and the configured mold is preheated for 30-40 minutes.
[0021] By adopting the above technical solution, by preheating the lower heating plate and configuring the mold, the configured mold can reach the required operating temperature range, thereby providing stable heating conditions during the hot pressing process; this helps to ensure the heating uniformity and consistency of the product, thereby improving the stability and reliability of production.
[0022] Preferably, the heating temperature range of the upper heating plate is 120° C.-140° C., and the pressure range is 2.5-4 MPa.
[0023] By adopting the above technical solution, by heating the upper heating plate within an appropriate temperature range and applying appropriate pressure, the hot pressing process can be accelerated and the hot pressing cycle can be shortened; this helps to improve production efficiency.
[0024] Preferably, the processing technology of the busbar processing device comprises the following processing steps: S1: Automatic feeding; First, place the conductor core on the coil unwinding rack for automatic unwinding; S2: Automatic wrapping; The conductor inner core on the coil unwinding rack is straightened by a straightening device on the front section of the automatic wrapping machine, and then the conductor inner core is wrapped to obtain the wrapped conductor inner core; S3: hot pressing treatment; The wrapped conductor core is placed in a configuration mold, preheated in all directions, and hot-pressed by a hot press to obtain a hot-pressed conductor core; S4: sintering treatment; The hot-pressed conductor inner core is wrapped with PTFE and guided into a tunnel furnace through a traction device. After sintering in the tunnel furnace, the PTFE is coated on the surface of the hot-pressed conductor inner core to form a sheath, and a sintered conductor inner core is obtained; S5: Automatic material collection; The sintered conductor core is pulled onto the coil receiving rack by using a pulling device; S6: bending and forming; The sintered conductor core on the coil receiving rack is bent to obtain the finished busbar.
[0025] By adopting the above technical scheme, through the processes of automatic unloading, automatic wrapping, hot pressing, sintering and automatic material collection in sequence, the wrapping tape attached to the outer surface of the conductor inner core is heat-treated, which can effectively eliminate the air in the gap between the conductor inner core and the wrapping tape, and is used to improve the insulation performance of the wrapping, thereby improving the busbar processing quality. Furthermore, the mechanical equipment used in automatic unloading, automatic wrapping, hot pressing, sintering and automatic material collection is integrated on the processing platform, which can reduce the transportation and transfer time of the conductor inner core and optimize the entire production process; this helps to improve production efficiency, reduce production cycle and increase output.
[0026] In summary, this application has the following beneficial effects: 1. The busbar processing device preheats the inner core of the wrapped conductor in the configuration mold through the lower heating plate, so that the wrapping tape becomes soft and tightly combines with the inner core of the conductor, and provides corresponding thermal curing conditions to form a strong bond between the inner core of the wrapped conductor and the wrapping tape; then the upper surface of the inner core of the wrapped conductor is hot-pressed by the upper heating plate, so that the inner core of the wrapped conductor and the wrapping tape can be combined into one, eliminating air gaps and air, and ensuring high-quality coating effects.
[0027] 2. The busbar processing technology, through the processes of automatic unloading, automatic wrapping, hot pressing, sintering and automatic material collection, is used to heat-treat the wrapping tape attached to the outer surface of the conductor inner core, which can effectively eliminate the air in the air gap between the conductor inner core and the wrapping tape, and is used to improve the insulation performance of the wrapping, thereby improving the busbar processing quality; Furthermore, the mechanical equipment used in automatic unloading, automatic wrapping, hot pressing, sintering and automatic material collection is integrated on the processing platform, which can reduce the transportation and transfer time of the conductor core and optimize the entire production process; this helps to improve production efficiency, reduce production cycle and increase output. BRIEF DESCRIPTION OF THE DRAWINGS
[0028] Figure 1 Schematic diagram of the overall structure of the busbar processing device in this embodiment; Figure 2 Schematic diagram of the internal structure of the hot press in this embodiment; Figure 3 is a schematic flow chart of the busbar processing technology in this embodiment; Explanation of the reference numerals: 1. Processing platform; 2. Coil unwinding rack; 3. Automatic wrapping machine; 4. Hot press; 401. Hot press frame; 402. Cylinder; 403. Lower heating plate; 404. Upper heating plate; 5. Tunnel furnace; 6. Traction device; 7. Coil receiving rack; 8. Configuration mold. DETAILED DESCRIPTION
[0029] The present application is further described in detail below in conjunction with the accompanying drawings. It is necessary to point out here that the following specific implementation methods are only used to further illustrate the present application and cannot be understood as limiting the scope of protection of the present application. Technical personnel in this field can make some non-essential improvements and adjustments to the present application based on the above application content. Example
[0030] The present invention discloses a busbar processing technology and device, which is used to wrap a strip-shaped wrapping tape spirally onto a conductor core at a specified pitch, wherein the wrapping tape is a mica tape with a width of 20 mm and a thickness of 0.09 mm. Figure 1 As shown, the busbar processing device includes a processing platform 1, on which is provided a material guide path for conveying the inner core of the conductor, and on the processing platform 1 and from the starting end to the ending end section of the material guide path, a coil unwinding rack 2, an automatic wrapping machine with double heads 3, a hot press 4, a tunnel furnace 5, a traction device 6 and a coil receiving rack 7 are sequentially arranged.
[0031] Among them, the coil unwinding rack 2 is used to automatically unwind the conductor core. Under the action of the coil unwinding rack 2, the conductor core is guided to the interior of the automatic wrapping machine 3 with a double head. When the automatic wrapping machine 3 controls the wrapping, the wrapping tape is evenly covered on the conductor core.
[0032] If the conductor core is not hot-pressed after wrapping, each layer of the conductor core of the mica tape is loose independently, resulting in air being wrapped around the conductor core.
[0033] When air is wrapped between the wrapping tape and the inner core of the conductor, an air gap will be formed, which will reduce the continuity and density of the wrapping tape, thereby reducing the insulation performance of the wrapping, increasing the dielectric loss and leakage current of the medium, resulting in a decline in electrical performance, which will affect the electrical safety performance of the product; and the air wrapped around the inner core of the conductor will cause the texture of the coating to become loose, thereby reducing the mechanical strength and seismic resistance of the product, and easily causing the coating to crack or peel off.
[0034] In order to avoid wrapping air around the inner core of the conductor, the tension of the wrapping machine is controlled to 20N, the running speed is 1m / min and the overlap rate is 50%, which can ensure that the wrapping tape fits tightly to the inner core of the conductor and excludes air, so as to ensure that the wrapping tape completely covers the inner core of the conductor and excludes air, thereby improving the wrapping quality and product performance.
[0035] like Figure 2As shown, further, the traction device 6 is used to guide the wrapped conductor core to the configuration mold 8 set in the hot press 4. The hot press 4 includes a hot press frame 401 with the configuration mold 8. The hot press frame 401 is fixedly installed with a cylinder 402 and a lower heating plate 403 for heating the configuration mold 8. The output end of the cylinder 402 is connected to an upper heating plate 404. The lower heating plate 403 preheats the configuration mold 8 for 30 minutes at a temperature of 120°C. The heat is transferred from the configuration mold 8 to the surface of the wrapped conductor core in all directions, thereby realizing all-round preheating of the wrapped conductor core. Therefore, the lower heating plate 403 is used to preheat the wrapped conductor core in all directions; the lower heating plate 403 preheats the wrapped conductor core in all directions The heated air around the conductor is heated, so that the nearby air is heated. The heated air temperature rises, the volume expands, and the density decreases. The lighter hot air will rise upward and gradually move away from the heating area. As the hot air rises, the surrounding cooler air will gradually drop and replace it, forming a convection cycle. The role of this convection movement is to help transfer heat energy to the surface of the inner core of the wrapped conductor in all directions through the movement of air, so as to achieve uniform temperature distribution. At the same time, convection also helps to stir and mix the surface of the inner core of the wrapped conductor and the cold air around it, reduce the temperature gradient, and achieve a more uniform heating effect. Therefore, during the preheating process, the air on the surface of the inner core of the wrapped conductor will transfer heat energy to the entire surface of the inner core of the wrapped conductor through convection movement, and achieve uniform temperature distribution.
[0036] In addition, the purpose of preheating is to increase the temperature of the inner core of the wrapped conductor, making it softer and more plastic, which is helpful for the subsequent heating and pressing process of the upper heating plate 404; through the control of the cylinder 402, the upper heating plate 404 moves toward the upper surface of the inner core of the wrapped conductor until it is against the upper surface of the lower heating plate 403; during the movement of the upper heating plate 404, it contacts the upper surface of the inner core of the wrapped conductor, heats it to 120°C and applies a pressure of 2.5MPa; once the upper heating plate 404 contacts the inner core of the wrapped conductor, the heating plate will transfer heat energy to the inner core of the wrapped conductor to increase the temperature of the inner core of the wrapped conductor; at the same time, the upper The pressure of the heating plate 404 will press the inner core of the wrapped conductor, making it tightly combined with the wrapping tape, and provide corresponding thermal curing conditions to form a strong bond between the inner core of the wrapped conductor and the wrapping tape; through heating and pressing, the inner core of the wrapped conductor can be fully combined with the wrapping tape, eliminating air gaps and air, ensuring high-quality coating effect; and the hot press 4 provides appropriate temperature and pressure, and the hot pressing of the hot press 4 makes the adhesive in the mica tape bond each layer together at high temperature and combine with the conductor to form a whole, so that the inner core of the wrapped conductor and the wrapping tape are firmly bonded, thereby improving the reliability and durability of the coating.
[0037] The wrapped conductor core is placed in a configuration mold, preheated in all directions, and hot-pressed by a hot press 4 to obtain a hot-pressed conductor core.
[0038] The hot-pressed conductor core is wrapped with PTFE having a width of 15 mm and a thickness of 0.05 mm, and is guided to the tunnel furnace 5 by the traction device 6 for sintering. After each layer of PTFE is sintered for 3 minutes at a temperature of 420°C and a conveying speed of 5 m / min, the PTFE is coated on the surface of the hot-pressed conductor core to form a sheath, and is attached to the outermost conductor core. The sintered PTFE has good waterproof, electrolyte corrosion resistance, and wear resistance, thereby extending the service life of the busbar. Furthermore, PTFE has good high-temperature stability and can maintain stable electrical insulation properties under high temperature conditions. The sintered PTFE can form a dense waterproof layer, which effectively prevents moisture from penetrating into the wire to cause short circuit or damage.
[0039] It is worth mentioning that the hot press 4 removes air, which can effectively expel the gas in the conductor core, make the wrapping tape tighter, and form a uniform and smooth structure on the surface; this can reduce the generation of pores and defects and improve the insulation effect; and the tunnel furnace 5 sintering treatment allows the PTFE to sinter to form a sheath and cover the outermost mica tape.
[0040] The hot press 4 is used first and then the tunnel furnace 5 is used for sintering. On the one hand, the whole process can be made more stable; the hot press 4 can ensure the uniformity and density of the conductor core during the hot pressing process, and the tunnel furnace 5 can provide a high-temperature sintering environment, so that the sintering reaction of PTFE is more complete; this can improve the stability of the process and the consistency of the product; on the other hand, after the sintering reaction of PTFE, adhesion will occur between the PTFE and the outermost mica tape, which is used to eliminate the air wrapped on the outer surface of the mica tape after the PTFE is wrapped.
[0041] Specifically, during the hot pressing to sintering process, the temperature is gradually increased, which helps to reduce the temperature gradient difference and avoid the generation of thermal stress. The temperature gradient difference refers to the temperature difference between different positions of the material during the temperature change process; when the temperature gradient difference is large, different parts of the material will cause stress concentration due to thermal expansion and contraction, thereby generating thermal stress; and gradually increasing the temperature can reduce the temperature gradient difference, thereby reducing the generation of thermal stress, which can effectively improve the structural strength and stability of the material and reduce the risk of thermal damage.
[0042] Finally, under the further traction of the traction device 6, the sintered conductor core is pulled onto the coil material receiving rack 7. The coil material receiving rack 7 is driven to control the movement and positioning of the conductor core, ensuring that the sintered conductor core is accurately delivered to the target position; this is very important for the smooth progress of subsequent processing steps.
[0043] Specifically, the traction device 6 includes two groups of belt drive assemblies arranged vertically, and a traction channel for the conductor core to pass through is formed between the two belt drives. The traction force is transmitted to the conductor core in the traction channel by utilizing the transmission and friction of the belt drive assembly, thereby realizing the traction movement of the conductor core.
[0044] like Figure 3 As shown, based on the above busbar processing device, the processing steps of the busbar processing process include: S1: Automatic feeding; First, the conductor core is placed on the coil unwinding rack 2 for automatic unwinding; S2: Automatic wrapping; The conductor inner core on the coil unwinding rack 2 is straightened by a straightening device on the front section of the automatic wrapping machine 3, and then the conductor inner core is wrapped to obtain the wrapped conductor inner core; S3: hot pressing treatment; The traction device 6 is used to guide the wrapped conductor core to the inside of the configuration mold 8 in the hot press 4. The lower heating plate 403 is first used to preheat the configuration mold 8 in all directions. The heat is transferred to the surface of the wrapped conductor core through the configuration mold 8 to achieve all-round preheating of the wrapped conductor core. Then, the upper heating plate 404 is controlled by the cylinder 402 to move toward the upper surface of the wrapped conductor core until it is against the upper surface of the lower heating plate 403. After hot pressing, the hot pressed conductor core is obtained. S4: sintering treatment; The hot-pressed conductor inner core is wrapped with PTFE and guided into the tunnel furnace 5 through the traction device 6. After sintering in the tunnel furnace 5, the PTFE is coated on the surface of the hot-pressed conductor inner core to form a sheath, and a sintered conductor inner core is obtained; S5: Automatic material collection; Under the further pulling action of the pulling device 6, the sintered conductor inner core is pulled onto the coil receiving rack 7, and is bent by the bending device to obtain a finished busbar.
[0045] Working principle: The operator first places the conductor core on the coil unwinding rack 2 for automatic unwinding; the wrapping tape is wrapped around the outer surface of the conductor core by multiple sets of guide rollers on the automatic wrapping machine 3 to obtain the wrapped conductor core.
[0046] The traction device 6 is used to guide the wrapped conductor core to the interior of the configuration mold 8 in the hot press 4. First, the lower heating plate 403 is used to preheat the configuration mold 8 in all directions. The heat is transferred to the surface of the wrapped conductor core through the configuration mold 8 to achieve all-round preheating of the wrapped conductor core. Then, the upper heating plate 404 is controlled by the cylinder 402 to move toward the upper surface of the wrapped conductor core until it is against the upper surface of the lower heating plate 403. After hot pressing, the hot pressed conductor core is obtained.
[0047] The hot-pressed conductor core is then wrapped with PTFE and guided into the tunnel furnace 5 through the traction device 6. After sintering in the tunnel furnace 5, the PTFE is coated on the surface of the hot-pressed conductor core to form a sheath, and a sintered conductor core is obtained.
[0048] Finally, under the further pulling action of the pulling device 6, the sintered conductor inner core is led to the coil receiving rack 7, and is bent by the bending device to obtain a finished busbar.
[0049] The above are all preferred embodiments of the present application, and the protection scope of the present application is not limited thereto. Therefore, any equivalent changes made according to the structure, shape, and principle of the present application should be included in the protection scope of the present application.
Claims
1. A busbar processing device, comprising a processing platform (1), characterized in that: The processing platform (1) is provided with a material guide path for conveying the conductor core. An automatic wrapping machine (3) for automatically wrapping the conductor core and a hot press machine (4) for hot pressing the conductor core are sequentially provided on the processing platform (1) and along the material guide path. The wrapped conductor core, which is conveyed along the material guide path by the automatic wrapping machine (3), enters a configuration mold (8) on the hot press machine (4). The hot press machine (4) comprises a hot press frame (401). A lower heating plate (403) and an upper heating plate (404) that slides up and down are provided inside the hot press frame (401). The configuration mold (8) is placed on the lower heating plate (403) so that the configuration mold (8) is preheated first. The heat generated by the preheating is transmitted to the surface of the wrapped conductor core in all directions through the configuration mold (8). Then, the wrapped conductor core is hot pressed by the upper heating plate (404) that slides up and down, so as to heat the wrapped conductor core.
2. The busbar processing device according to claim 1, characterized in that: A coil unwinding rack (2) is provided on the processing platform (1), and the coil unwinding rack (2) is located on one side of the conductor core input end of the automatic wrapping machine (3).
3. The busbar processing device according to claim 1, characterized in that: A tunnel furnace (5) is provided on the processing platform (1), and the tunnel furnace (5) is located on one side of the output end of the hot press (4).
4. The busbar processing device according to claim 3, characterized in that: The internal sintering temperature of the tunnel furnace (5) is in the range of 400° C.-450° C., and the conveying speed of the conductor core in the tunnel furnace (5) is in the range of 5-8 m / min.
5. The busbar processing device according to claim 3, characterized in that: It also comprises a traction device (6) arranged on the processing platform (1), wherein the traction device (6) is located on one side of the output end of the tunnel furnace (5).
6. The busbar processing device according to claim 5, characterized in that: The conductor inner core sintered in the tunnel furnace (5) is pulled into a coil receiving rack (7) arranged on the processing platform (1) by means of the pulling device (6).
7. The busbar processing device according to claim 1, characterized in that: The hot pressing frame (401) is provided with a cylinder (402), and the output end of the cylinder (402) is connected to the upper surface of the upper heating plate (404).
8. The busbar processing device according to claim 1, characterized in that: The preheating temperature range of the lower heating plate (403) is 110°C-150°C, and the configuration mold (8) is preheated for 30-40 minutes.
9. The busbar processing device according to claim 1, characterized in that: The upper heating plate (404) has a heating temperature range of 120°C-140°C and a pressure range of 2.5-4MPa.
10. A processing technology for the busbar processing device according to any one of claims 1 to 9, characterized in that: The processing steps include: S1: Automatic feeding; Firstly, the conductor inner core is placed on a coil unwinding rack (2) for automatic unwinding; S2: Automatic wrapping; The conductor inner core on the coil unwinding rack (2) is straightened by a straightening device on the front section of an automatic wrapping machine (3), and then the conductor inner core is wrapped to obtain the wrapped conductor inner core; S3: hot pressing treatment; The wrapped conductor core is placed in a configuration mold, preheated in all directions, and hot-pressed by a hot press (4) to obtain a hot-pressed conductor core; S4: sintering treatment; The hot-pressed conductor inner core is wrapped with PTFE and guided into a tunnel furnace (5) through a traction device (6); after sintering in the tunnel furnace (5), the PTFE is coated on the surface of the hot-pressed conductor inner core to form a sheath, and a sintered conductor inner core is obtained; S5: Automatic material collection; The sintered conductor inner core is pulled onto a coil receiving rack (7) by using a pulling device (6); a finished busbar is obtained by bending.
Citation Information
Patent Citations
Lamination bus for high-power frequency conversion device and manufacture method thereof
CN102867572A
Numerical control automatic continuous wire wrapping machine and wire cutting control method
CN115064323A
Novel high-temperature-resistant insulating busbar and preparation method thereof
CN116936165A
Copper-aluminum bar wrapping connection structure, forming equipment and forming process
CN117012434A
Insulating hot press molding device of copper bar handbag that converges
CN207338037U