Beneficiation method of tailings-free pond
Through the tailings storage-free mineral processing method, photoelectric separation, spiral chute separation, flotation and magnetic separation technologies are used to efficiently recover the available components in the lead and zinc raw ores, solving the problems of traditional mineral processing difficulties and insufficient tailings storage capacity, and realizing tailings The mine warehouse has zero deposits and the lead and zinc extraction rate is increased.
Patent Information
- Application Number
- CN202411023288.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-29
- Publication Date
- 2024-10-29
AI Technical Summary
The processing of lead-zinc sulfide ore contains a large amount of light minerals such as dolomite and calcite, which makes the mineral processing difficult. The traditional process produces high tailings, and the capacity of the tailings reservoir is sharply reduced. Moreover, due to geographical location and environmental reasons, it is impossible to build a new tailings reservoir and the mine Facing problems of survival and development.
A mineral processing method without tailings pond is adopted, including the first screening and optical separation, the second screening and gravity separation, grinding and flotation, combined heavy and flotation magnetic separation, through photoelectric separation, spiral chute separation, and flotation. Chemical adjustment and magnetic separation are used to recover lead concentrate, zinc concentrate and barite concentrate respectively, and finally the tailings are suitable for underground filling.
It achieves high-quality separation of available components in lead-zinc raw ore, recovers 40-50% of available stones, improves the lead-zinc extraction rate, and the tailings are smaller than the maximum absorbable volume of underground filling, achieving zero storage in the tailings reservoir and solving the problem of tailings. The problem of reduced mine storage capacity and difficulty in building new mines.
Smart Images

Figure CN118847348A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to lead-zinc sulfide ore processing, in particular to a ore dressing method without a tailings pond. Background Art
[0002] The processing of lead-zinc sulfide ore contains a large amount of light minerals such as dolomite and calcite, making the selection of lead-zinc ore difficult.
[0003] In the traditional mineral processing technology, three-stage crushing, one-stage grinding, lead flotation, and zinc flotation are processed in sequence, producing 1% lead concentrate and 6% zinc concentrate, and the remaining actual tailings yield is 93%. Among them, 70% of the tailings are filled in the underground empty area as much as possible (that is, 60% of the original ore is used for underground filling as much as possible), and the remaining 30% of the tailings are transported and stored in the tailings pond, resulting in a sharp reduction in the capacity of the tailings pond.
[0004] The capacity of tailings ponds has been drastically reduced, and due to geographical location and surrounding environment, it is impossible to build new tailings ponds. Mining companies are facing survival and development issues. Summary of the invention
[0005] The present invention aims to solve at least one of the above-mentioned technical problems and provide a ore dressing method without a tailings pond, which can fully select the available components in the lead-zinc ore, and each component can be used in the corresponding field.
[0006] In order to achieve the above object, the technical solution adopted by the present invention is:
[0007] A ore dressing method without a tailings pond comprises the following steps:
[0008] First screening and optical separation, the raw ore is screened according to the pore size of α1, α1 = 15 ± 2mm, the raw ore ≥ α1 obtained by the first screening is suitable for photoelectric separation, and the raw ore to be broken and the optical separation stone of white matter are separated, and the optical separation stone accounts for 20-25% of the raw ore;
[0009] Second screening and re-rotation separation, after the raw ore to be crushed is crushed together with the raw ore ≤α1, it is screened according to the α2 sieve hole, α2 = 0.5 ± 0.1 mm, to obtain the second screened ore and the medium ore ≤α2, the second screened ore ≥α2 is suitable for spiral descent in the spiral chute, and the rolling diversion is the gravity separation stone and the medium ore ≥α2, the gravity separation stone accounts for 20-25% of the raw ore, and the light separation stone and the gravity separation stone both include dolomite and calcite, which are suitable for construction and / or sintering;
[0010] Grinding and flotation: grinding the middlings to make the ore fines with a particle size of less than 0.074 mm account for more than 70%. The ore fines are prepared into slurry and flotation reagents are added to recover lead concentrate and zinc concentrate in turn, leaving the remaining ore;
[0011] Gravity-flotation-magnetic separation, the remaining ore is separated into barite concentrate and final tailings in turn by gravity separation column, desulfurization flotation and magnetic separation. The barite concentrate with ≤α2 and more than 70% <0.074mm is suitable for papermaking, textile filler, chemical industry, drilling weighting agent, and the final tailings are suitable for underground filling.
[0012] Compared with the prior art, the beneficial effects of the present application include: the first screen ore is subjected to photoelectric sorting with a particle size of ≥α1, and the first screen ore can be effectively and high-quality separated into two categories: the original ore to be broken and the optically selected stone; the second screen ore with a particle size of ≥α2 can be rolled and spirally descended in the spiral chute without the help of water flow to obtain a dry concentrate, so as to facilitate direct dry grinding to obtain a relatively fine and uniform particle size of mineral powder, which is convenient for effective and sufficient flotation of substantial lead-zinc ore; barite is ≤0.5mm, and more than 70% is <0.074mm, which is much smaller than the minimum standard of 1.9mm for drilling load-bearing agents; barite is the most After selection, the content is ≥95%; optically selected stone and re-selected stone can be recovered, which are suitable for construction raw materials and sintered ore, and the sintered ore can be used for efficient and energy-saving sintering and high-quality sintering of target ore; after the first screening and optical selection and the second screening and re-cyclone separation, 40-50% of the usable stones can be recovered, and the remaining 50-60% of the middlings are lower than the maximum absorptive capacity of underground filling; and the middlings are further refined into lead, zinc and barite, and the final tailings are less than the maximum absorptive capacity of underground filling, the actual tailings output is balanced with the filling absorption capacity, and the tailings pond is zero deposited, that is, there is no tailings pond.
[0013] As an improvement of the above technical solution, the optically selected stone is suitable for building materials, and the heavily selected stone is suitable for sintered ore.
[0014] As an improvement of the above technical solution, the flotation reagent includes lime, zinc sulfate, copper sulfate, butyl xanthate, and No. 2 oil. Lime is added to the middling ore powder, and the limestone and the ore are stirred evenly and reacted for a long time. In the ore pulp corresponding to the uniform ore powder, the limestone on the surface of the mineral makes the butyl xanthate evenly adsorbed on the surface of the mineral, thereby adjusting the pH value of the ore pulp. Lead is used as an inhibitor to inhibit the floating of zinc minerals.
[0015] As an improvement of the above technical solution, in the grinding flotation, lead flotation includes lead roughing, lead scavenging, lead concentration I and lead concentration II, and zinc flotation includes zinc roughing, zinc scavenging, zinc concentration I and zinc concentration II. The tailings obtained from the lead concentration I and the concentrate from the lead scavenging are suitable for returning to the lead roughing, and the tailings from the latter lead concentration are suitable for returning to the previous lead concentration. The tailings obtained from the zinc concentration I and the concentrate from the zinc scavenging are suitable for returning to the zinc roughing, and the tailings from the latter zinc concentration are suitable for returning to the previous zinc concentration.
[0016] As an improvement of the above technical solution, the concentrate obtained from the lead roughing is placed in the lead concentration I after regrinding, and in the regrinding of the concentrate, the ore fines <0.038mm account for 92%.
[0017] As an improvement of the above technical solution, the tailings obtained from the zinc concentration I are placed in zinc roughing after regrinding, and in the regrinding of the tailings, the proportion of ore fines <0.038mm accounts for 77%.
[0018] As an improvement of the above technical solution, the magnetic separation of the gravity-flotation-magnetic separation is a wet magnetic separation, which obtains wet barite. The wet barite is stored so that it can be directly used in papermaking, textile fillers, chemicals, and drilling weighting agents in a wet state.
[0019] As an improvement of the above technical solution, the waste ore is separated into coarse waste ore ≤0.074mm and ≥0.038mm and fine waste ore ≤0.038mm by hydraulic spiral flow, the coarse waste ore is separated into coarse barite and final tailings by gravity flotation and magnetic separation, and the fine waste ore is deslimed and separated into fine barite and final tailings by gravity flotation and magnetic separation.
[0020] As an improvement of the above technical solution, the magnetic separation of the gravity-flotation magnetic separation is first wet weak magnetic separation with a magnetic field strength of 200±10KA / m, and then wet strong magnetic separation with a magnetic field strength of 2±0.1t. BRIEF DESCRIPTION OF THE DRAWINGS
[0021] The specific embodiments of the present invention are further described in detail below in conjunction with the accompanying drawings, wherein:
[0022] Figure 1 This is a flow chart of the mineral processing process according to an embodiment of the present invention;
[0023] Figure 2 for Figure 1 Shows the local process details of the mineral processing process flow chart Figure 1 ;
[0024] Figure 3 for Figure 1 Shows the local process details of the mineral processing process flow chart Figure 2 .
[0025] The accompanying drawings are only one specific embodiment of the present invention, and the form and structure of this specific embodiment should not limit the expansion of other embodiments. DETAILED DESCRIPTION
[0026] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0027] Reference Figures 1 to 3 The present invention provides a ore dressing method without a tailings pond, comprising the following steps:
[0028] First screening and optical separation, the raw ore is screened according to the pore size of α1, α1 = 15 ± 2mm, the raw ore ≥ α1 obtained by the first screening is suitable for photoelectric separation, and the raw ore to be broken and the optical separation stone of white matter are separated, and the optical separation stone accounts for 20-25% of the raw ore;
[0029] Second screening and re-rotation separation, after the raw ore to be crushed is crushed together with the raw ore ≤α1, it is screened according to the α2 sieve hole, α2 = 0.5 ± 0.1 mm, to obtain the second screened ore and the medium ore ≤α2, the second screened ore ≥α2 is suitable for spiral descent in the spiral chute, and the rolling diversion is the gravity separation stone and the medium ore ≥α2, the gravity separation stone accounts for 20-25% of the raw ore, and the light separation stone and the gravity separation stone both include dolomite and calcite, which are suitable for construction and / or sintering;
[0030] Grinding and flotation: grinding the middlings to make the ore fines with a particle size of less than 0.074 mm account for more than 70%. The ore fines are prepared into slurry and flotation reagents are added to recover lead concentrate and zinc concentrate in turn, leaving the remaining ore;
[0031] Gravity-flotation-magnetic separation, the remaining ore is separated into barite concentrate and final tailings in turn by gravity separation column, desulfurization flotation and magnetic separation. The barite concentrate with ≤α2 and more than 70% <0.074mm is suitable for papermaking, textile filler, chemical industry, drilling weighting agent, and the final tailings are suitable for underground filling.
[0032] "Concentrates" such as lead concentrate, zinc concentrate, barite concentrate, etc. are the essence obtained by refining the original ore (lead-zinc ore).
[0033] In a specific case of mineral processing implemented by this method
[0034]
[0035] Dolomite and calcite are both calcium minerals, and their main component is CaCO3. They are similar in appearance and are both relatively white, making them suitable as building materials.
[0036] In addition, the selected stones include dolomite and calcite. When dolomite and calcite are used for sintering ore: A. They can react with silicates in the target ore to produce quartz at high temperature, thereby improving the maturity of the target ore, which can reduce the sintering temperature and reduce coal consumption; B. During the sintering process, the calcium in the selected stone can react with the iron oxide in the iron ore to form fusible calcium iron ore, and can also react with other components to form other substances that are beneficial to sintering. This substance can fill the micropores and cracks in the target ore, increase the density and mechanical strength of the sintered ore, improve the quality and mechanical properties of the sintered ore, and reduce the hygroscopicity and dust generation of the sintered ore, thereby reducing environmental pollution.
[0037] The basic structure and working principle of the photoelectric sorting machine are common knowledge, such as the most common color sorting machine. The working principle of the photoelectric sorting machine is mainly based on photoelectric technology. Photoelectric technology collects the appearance characteristics of products or impurities, such as color, texture, and texture, stores the collected characteristics in the controller, and serves as the basis for big data analysis of photoelectric sorting. Specifically, a photoelectric recognition structure (i.e., a photoelectric detection structure) is set in the middle of the conveyor belt, and a feeder and a rejection structure are set at both ends of the conveyor belt. The feeder is commonly a jitter feeder, and the photoelectric detection structure is commonly a light transceiver detection structure, a CCD imaging structure, an infrared imaging structure, an X-ray imaging structure, and an ultraviolet light structure, such as traditional photoelectric technology color sorters, CCD technology color sorters, infrared technology color sorters, and X-ray technology color sorters. The rejection structure uses blowing, magnetic suction, guide plates / baffles, etc. to act on products or impurities, so that products and impurities fall into corresponding troughs respectively. The feeder continuously spreads a single layer or even a single row of objects to be sorted on the feeding end of the conveyor belt. The objects to be sorted are fed into the photoelectric detection structure through the conveyor belt. The photoelectric detection structure converts the detected optical signal into an electrical signal. The controller performs analysis and processing, and then drives the rejection structure to act (whether the injection valve is open, whether the electromagnet is energized, and whether the guide plate and the baffle are open or closed). In the present invention, the raw ore is rich in dolomite and calcite, which are similar in appearance and are both relatively white; the raw ore ≥α1 obtained by the first screening is photoelectrically sorted and sorted into raw ore to be broken and white optically selected stone.
[0038] In traditional photoelectric technology, the light source emitter emits light, which is reflected by the surface of the object and received by the photoelectric converter. The reflection of the object and the reflection of the colorimetric plate are compared in the electronic mirror. The color difference changes the voltage inside the electronic mirror and is amplified. If the signal difference exceeds the preset value of the automatic control level, the spraying, magnetic attraction and diversion are immediately driven.
[0039] The first screen ore is subjected to photoelectric sorting with a particle size of ≥α1. The first screen ore can be effectively and high-quality separated into two categories: raw ore to be broken and optically selected stone.
[0040] The heavy medium cyclone includes a spiral chute, the upper end of which is suitable for receiving the second-screened ore for gravity cyclone separation. The lower end of the spiral chute is provided with a first discharge nozzle corresponding to the inner flow channel of the spiral chute and a second discharge nozzle corresponding to the outer flow channel of the spiral chute. After the second-screened ore is placed in the spiral chute, it descends in a rolling spiral. The gravity-separated stone and the intermediate ore ≥α2 are centrifugally separated based on different densities / specific gravities. The gravity-separated stone (including dolomite and calcite) is relatively light and tends to the outer flow channel of the spiral chute, and is collected through the second discharge nozzle. The concentrate is relatively heavy and tends to the inner flow channel of the spiral chute, and is collected through the first discharge nozzle.
[0041] The secondary screened ore with a particle size of ≥α2 can be rolled down in the spiral chute without the help of water flow to obtain dry concentrate, which is convenient for direct dry grinding to obtain ore powder with finer and more uniform particle size, which is convenient for effective and sufficient flotation of substantial lead-zinc ore.
[0042] Grinding flotation includes lead flotation and zinc flotation. Flotation reagents are added to the pulp gradually to float out lead concentrate and zinc concentrate in turn. Lead flotation uses lime and zinc sulfate as regulators, butyl xanthate + ethyl thiocyanate as collectors, and No. 2 oil as a frother. Zinc flotation uses lime and copper sulfate as regulators, butyl xanthate as collectors, and No. 2 oil as a frother. In the flotation tank, add a check agent and stir continuously, and the bubbles carry the concentrate to float.
[0043] No. 2 oil, a composite higher alcohol, has the molecular formula R-alkane, and is divided into two types: pine oil and chemical oil. It is widely used as a frother in non-ferrous metal flotation.
[0044] Gravity-flotation-magnetic separation includes gravity separation column, desulfurization flotation and magnetic separation in sequence. The barite concentrate is mainly BASO4. In the present invention, the barite is ≤0.5mm, and more than 70% is <0.074mm, which is much smaller than the minimum standard of 1.9mm for drilling load-bearing agents; the barite is finally selected through multiple processes, and the content is ≥95%. The barite is mixed with drilling mud with high fineness and high specific gravity. The drilling mud has high uniformity and high specific gravity, which facilitates the effective balance of drilling mud with underground oil and gas pressure, improves drilling efficiency, and is also suitable for drilling drug holes and grooving in lead-zinc mines. The barite recovered from lead-zinc mines, namely zinc barium white, is a high-quality white pigment material. With its high specific gravity and high fineness, it can effectively improve the thickness, strength and durability of chemical pigment fillers.
[0045] Gravity separation column is a mineral separation method based on the difference in mineral density. It uses gravity to separate mineral particles of different densities. Specifically, the gravity separation column includes a fish scale screen plate and a crank structure that drives the fish scale screen plate to swing back and forth. The bottom flow is coarse particles and the overflow is fine particles.
[0046] In the desulfurization flotation, the flotation reagents include oxalic acid, butyl xanthate, and No. 2 oil. In some specific implementations, the desulfurization flotation adopts one roughing and three cleaning.
[0047] Barite has certain magnetic properties and can be screened out by magnetic separation.
[0048] In the present invention, optically selected stone and re-selected stone can be recovered, which are suitable for building raw materials and sintered ore. The sintered ore can be used for high-efficiency, energy-saving and high-quality sintering of target ore.
[0049] 15mm≤optical separation stone≤60mm, 0.5mm≤gravity separation stone≤15mm. The optical separation stone is preferably suitable for building materials, and the gravity separation stone is preferably suitable for sintered ore. Gravity separation stone can more effectively heat the target ore, adhere to the target ore for reaction, and fill the pores of the target ore during the sintering of the target ore.
[0050] After the first screening and optical separation and the second screening and gravity separation, 40-50% of the usable stones can be recovered, and the remaining 50-60% of the middlings are lower than the maximum amount of underground filling. After the recovery of optical separation and gravity separation, the lead and zinc refining rate of the middlings can be increased by 2-8%; specifically, the lead flotation rate is increased from 1% to about 1.05, and the zinc flotation rate is increased from 6% to about 6.5%.
[0051] Compared with the prior art, the beneficial effects of the present application include: in the lead and zinc refining process, the minerals derived from each process are cleverly used in construction, sintering, chemical industry, drilling, etc.; the final tailings are smaller than the maximum absorbable amount of underground filling, the actual tailings output is balanced with the filling absorption amount, and there is zero storage in the tailings pond, that is, there is no tailings pond.
[0052] In some embodiments of the present invention, the flotation reagents include lime, zinc sulfate, copper sulfate, butyl xanthate, and No. 2 oil. Lime is added to the middling ore powder, and the limestone and ore are stirred evenly and reacted for a long time. In the ore pulp corresponding to the uniform ore powder, the limestone on the surface of the mineral makes the butyl xanthate evenly adsorbed on the surface of the mineral, adjusts the pH value of the ore pulp, and acts as an inhibitor to inhibit the floating of zinc minerals in lead selection. Flotation and its foaming agents, collectors, and inhibitors are conventional knowledge. On the other hand, the present invention mixes limestone, one of the flotation reagents, into the middling ore in advance, so that it is mixed and squeezed with the middling ore to improve the grinding efficiency and fineness of the middling ore, and evolves together into a powder mixing reaction to provide heat, which is convenient for the uniform limestone on the surface of the mineral.
[0053] In some embodiments of the present invention, in the grinding flotation, lead flotation includes lead roughing, lead scavenging, lead concentration I and lead concentration II, and zinc flotation includes zinc roughing, zinc scavenging, zinc concentration I and zinc concentration II. The tailings obtained from the lead concentration I and the concentrate from the lead scavenging are suitable for returning to the lead roughing, and the tailings from the latter lead concentration are suitable for returning to the previous lead concentration. The tailings obtained from the zinc concentration I and the concentrate from the zinc scavenging are suitable for returning to the zinc roughing, and the tailings from the latter zinc concentration are suitable for returning to the previous zinc concentration, so as to fully extract the lead concentrate and zinc concentrate.
[0054] In some specific implementations, the lead process adopts one roughing selection, four fine selections and two scavenging selections, and the zinc process adopts one roughing selection, three fine selections and two scavenging selections and flotation process.
[0055] In some embodiments of the present invention, the concentrate obtained from the lead roughing is placed in the lead concentration I after regrinding, and in the regrinding of the concentrate, the ore fines <0.038mm account for 92%, so that the dissociation degree of the lead mineral monomer is improved, the floatability of the lead mineral is enhanced, and the separation effect of the lead concentration I is improved.
[0056] In some embodiments of the present invention, the tailings obtained from the zinc concentration I are placed in zinc roughing after regrinding, and in the regrinding of the tailings, the proportion of ore fines <0.038 mm accounts for 77%.
[0057] In some embodiments of the present invention, the magnetic separation of the gravity-flotation magnetic separation is a wet magnetic separation, and the wet magnetic separation obtains wet barite, which is stored so that it can be directly used in papermaking, textile fillers, chemicals, and drilling weighting agents in a wet state, and the barite can be effectively used. The magnetic separation is electromagnetic or permanent magnetic drum magnetic separation.
[0058] Furthermore, the magnetic separation of the gravity-flotation magnetic separation is first wet weak magnetic separation with a magnetic field strength of 200±10KA / m, and then wet strong magnetic separation with a magnetic field strength of 2±0.1t.
[0059] In some embodiments of the present invention, the waste ore is separated into coarse waste ore of ≤0.074mm and ≥0.038mm and fine waste ore of ≤0.038mm by hydraulic spiral flow, the coarse waste ore is separated into coarse barite and final tailings by gravity flotation magnetic separation, and the fine waste ore is separated into fine barite and final tailings by gravity flotation magnetic separation after desludging. Coarse barite can be efficiently used in paint chemicals, and fine barite can be efficiently used in papermaking, textile fillers, drilling weighting agents, etc. The waste ore is classified into coarse waste ore and fine waste ore, and the fine waste ore is further desludged to avoid the influence of mud on the consumption of flotation agents.
[0060] For desludging, screen cyclones, small diameter hydrocyclones, rake thickeners, etc. can be used.
[0061] Gravity-flotation-magnetic separation includes gravity separation column, desulfurization flotation, shaking table and magnetic separation. In shaking table separation, the combined effect of mechanical shaking and water flushing is used to separate the ore particles according to their specific gravity, and the heavy ore particles are further magnetically separated to separate barite.
[0062] The above embodiments are only used to illustrate the technical solution of the present invention rather than to limit it. Any modification or equivalent substitution that does not depart from the spirit and scope of the present invention shall be included in the scope of the technical solution of the present invention.
Claims
1. A ore dressing method without tailings pond, characterized in that: The following steps are involved: First screening and optical separation, the raw ore is screened according to the pore size of α1, α1 = 15 ± 2mm, the raw ore ≥ α1 obtained by the first screening is suitable for photoelectric separation, and the raw ore to be broken and the optical separation stone of white matter are separated, and the optical separation stone accounts for 20-25% of the raw ore; Second screening and re-rotation separation, after the raw ore to be crushed is crushed together with the raw ore ≤α1, it is screened according to the α2 sieve hole, α2 = 0.5 ± 0.1 mm, to obtain the second screened ore and the medium ore ≤α2, the second screened ore ≥α2 is suitable for spiral descent in the spiral chute, and the rolling diversion is the gravity separation stone and the medium ore ≥α2, the gravity separation stone accounts for 20-25% of the raw ore, and the light separation stone and the gravity separation stone both include dolomite and calcite, which are suitable for construction and / or sintering; Grinding and flotation: grinding the middlings to make the ore fines with a particle size of less than 0.074 mm account for more than 70%. The ore fines are prepared into slurry and flotation reagents are added to recover lead concentrate and zinc concentrate in turn, leaving the remaining ore; Gravity-flotation-magnetic separation, the remaining ore is separated into barite concentrate and final tailings in turn by gravity separation column, desulfurization flotation and magnetic separation. The barite concentrate with ≤α2 and more than 70% <0.074mm is suitable for papermaking, textile filler, chemical industry, drilling weighting agent, and the final tailings are suitable for underground filling.
2. The ore dressing method without tailings pond according to claim 1, characterized in that: The optically selected stone is suitable for building materials, and the heavily selected stone is suitable for sintered ore.
3. The ore dressing method without tailings pond according to claim 1, characterized in that: The flotation reagents include lime, zinc sulfate, copper sulfate, butyl xanthate, and No. 2 oil. Lime is added to the middling ore powder, and the limestone and ore are stirred evenly and reacted for a long time. In the ore pulp corresponding to the uniform ore powder, the limestone on the surface of the mineral makes the butyl xanthate evenly adsorbed on the surface of the mineral, adjusting the pH value of the ore pulp. Lead is used as an inhibitor to inhibit the floating of zinc minerals.
4. The ore dressing method without tailings pond according to claim 1, characterized in that: In the grinding flotation, lead flotation includes lead roughing, lead scavenging, lead concentration I and lead concentration II, and zinc flotation includes zinc roughing, zinc scavenging, zinc concentration I and zinc concentration II. The tailings obtained from the lead concentration I and the concentrate from the lead scavenging are suitable for returning to the lead roughing, and the tailings from the latter lead concentration are suitable for returning to the former lead concentration. The tailings obtained from the zinc concentration I and the concentrate from the zinc scavenging are suitable for returning to the zinc roughing, and the tailings from the latter zinc concentration are suitable for returning to the former zinc concentration.
5. The ore dressing method without tailings pond according to claim 4, characterized in that: The concentrate obtained from the lead roughing is put into the lead concentration I after regrinding, and in the regrinding of the concentrate, the ore fines <0.038mm account for 92%.
6. The ore dressing method without tailings pond according to claim 4, characterized in that: The tailings obtained from the zinc concentration I are placed in the zinc roughing after regrinding, and in the regrinding of the tailings, the ore fines <0.038 mm account for 77%.
7. The ore dressing method without tailings pond according to any one of claims 1 to 6, characterized in that: The magnetic separation of the gravity-flotation magnetic separation is a wet magnetic separation, and the wet magnetic separation obtains wet barite, which is stored so that it can be directly used in papermaking, textile fillers, chemicals, and drilling weighting agents in a wet state.
8. The ore dressing method without tailings pond according to any one of claims 1 to 6, characterized in that: The waste ore is separated into coarse waste ore of ≤0.074mm and ≥0.038mm and fine waste ore of ≤0.038mm by hydraulic spiral flow. The coarse waste ore is separated into coarse barite and final tailings by gravity flotation and magnetic separation. The fine waste ore is deslimed and separated into fine barite and final tailings by gravity flotation and magnetic separation.
9. The ore dressing method without tailings pond according to any one of claims 1 to 6, characterized in that: The magnetic separation of the gravity-flotation magnetic separation is first wet weak magnetic separation with a magnetic field strength of 200±10KA / m, and then wet strong magnetic separation with a magnetic field strength of 2±0.1t.
Citation Information
Cited By
Beneficiation method of low-grade refractory lead-zinc oxide ore
CN121623937A
Beneficiation method of low-grade refractory lead-zinc oxide ore
CN121623937B