Lithium battery positive and negative electrode material recovery system based on electromagnetic separation
By adopting an electromagnetic separation system in lithium battery recycling, using a combination of strong electric field and magnetic field, using Lorentz force to separate different powders, combining vibrating screen and ultrasonic vibration tracks, the separation accuracy and impurities in lithium battery recycling are solved. Problem, efficient recycling of positive and negative electrode materials for lithium batteries has been achieved.
Patent Information
- Application Number
- CN202411278628.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-12
- Publication Date
- 2024-11-15
- Estimated Expiration
- 2044-09-12
AI Technical Summary
In traditional lithium battery recycling methods, crawler electrostatic separation equipment can only separate particles of the same particle size in a single layer. The overall lithium battery material recycling accuracy is low, and it cannot effectively remove aluminum powder impurities in tiny particles, affecting battery performance and safety. .
Using an electromagnetic separation system, through the combination of strong electric field and magnetic field, the conductive track and the conductive positive plate form a parallel electrostatic field and a perpendicular magnetic field, the Lorentz force is used to separate different powders, and the vibration screen and ultrasonic vibration track are combined to achieve micron level. Efficient separation of materials.
It improves the recycling accuracy of the positive and negative electrode materials of lithium batteries, effectively removes aluminum powder impurities in tiny particles, improves battery performance and safety, and solves the problems of separation accuracy and impurities in traditional methods.
Smart Images

Figure CN118950248A_ABST
Abstract
Description
Technical Field
[0001] The present application belongs to the field of electrostatic separation, and more specifically, to a lithium battery positive and negative electrode material recovery system based on electromagnetic separation. Background Art
[0002] As the types of separated materials in modern production processes become more and more diverse and the requirements for separation purity are gradually increasing, electrostatic separation technology has also become more diversified and specialized. Especially under the current premise of large-scale waste of lithium batteries, the workload of battery recycling and the purification of battery materials have become important issues.
[0003] At present, the mainstream lithium battery recycling mostly adopts chemical methods, which involves other consumables, and the chemical reaction process is too complicated, and the overall recycling process is costly. In terms of physical sorting, permanent magnetic separation technology has strict requirements on the magnetism of the material itself. Usually only ferromagnetic and non-ferromagnetic materials are suitable for permanent magnetic separation technology, while ternary lithium and lithium iron phosphate are weakly magnetic at room temperature and are not suitable for permanent magnetic separation technology. The usual magnetic field sorting technology has high requirements on the conductivity difference and material size of the material. This principle of eddy current and magnetic field sorting is suitable for the separation of larger flake materials. The current battery recycling process includes multi-stage crushing. This process ensures a high raw material recovery rate and the efficiency of the initial separation of materials, but the corresponding is: the miniaturization of materials, which makes it difficult to use ordinary magnetic field sorting technology to separate tiny particles in the later stage of battery recycling. In the recycled ternary lithium and lithium iron phosphate materials, less metal impurities may also lead to a significant reduction in battery performance, and even cause metal dendrites to form at the negative electrode of the battery, causing internal short circuits in the battery.
[0004] The existing physical recycling method of lithium batteries includes the following processes: 1. Pre-crushing treatment: disassemble the battery and distinguish the positive and negative electrodes; 2. Screening treatment: use a screen to screen the material by size to obtain multiple batches of materials of the same size; 3. Wind separation / flotation treatment: use a wind separation device to sort materials of different looseness; 4. Specific gravity sorting: use a vibrating screen, centrifuge, etc. to sort powders of different densities; 5. Magnetic separation treatment: use a permanent magnet to magnetically separate the material. Due to the different magnetic permeabilities of the materials, this method is usually used to remove ferromagnetic impurities in the material. In the process of recycling lithium iron phosphate, ferromagnetic materials such as γ-Fe2O3 can be removed; in the above-mentioned lithium battery recycling process, the difference between the conductivity of aluminum powder and the positive electrode powder is not used for powder impurity removal. After the positive electrode material is recovered, a certain amount of aluminum powder still exists. Although its impurity content is very low, it will seriously affect the performance of batteries prepared using recycled materials. The negative impact of aluminum powder on batteries is mainly reflected in the following aspects: 1. Aluminum powder will preferentially participate in charging and discharging in the electrochemical reaction, which will lead to abnormal voltage of the battery and a decrease in the overall specific capacity. 2. Aluminum powder may form dendrites at the negative electrode during charging. Unlike lithium dendrites, aluminum dendrites are difficult to avoid by special pore size diaphragms for lithium ions. The formation of aluminum dendrites may cause the diaphragm to be punctured and the battery to short-circuit, which in turn causes battery safety problems. Summary of the invention
[0005] In view of the defects of the prior art, the purpose of this application is to provide a lithium battery positive and negative electrode material recovery system based on electromagnetic separation, which aims to solve the problem that traditional crawler-type electrostatic separation equipment can only achieve charging separation of a single layer of particles of the same particle size and the overall lithium battery material recovery accuracy is low.
[0006] To achieve the above objectives, in a first aspect, the present application provides a lithium battery positive and negative electrode material recovery system based on electromagnetic separation, comprising: a strong electric field generating device, a magnetic field generating device and a material collecting device;
[0007] The strong electric field generating device includes a high voltage power supply, a conductive positive plate and a conductive track; the conductive track is grounded to determine a fixed potential and transfer part of the powder charge to form a net charge accumulation; the conductive track and the conductive positive plate, together with the high voltage power supply, form a parallel electrostatic field to make the powder go back and forth between the conductive positive plate and the conductive track; wherein different types of powder accumulate charge at different rates;
[0008] The magnetic field generating device is used to generate a magnetic field perpendicular to the electric field and parallel to the conductive track. When the powder moves back and forth between the conductive positive plate and the conductive track, the powder is subjected to the Lorentz force to produce orbital deflection, thereby achieving separation of different powders.
[0009] The material collecting devices are respectively located on both sides of the conductive track, near the magnetic field area, for collecting the separated powder; wherein, the area near the magnetic field area is an area less than a preset distance from the magnetic field area.
[0010] Further preferably, there is a preset small angle between the conductive positive plate and the conductive track, so that the powder subjected to a small Lorentz force has a tendency to move laterally due to elastic force during the back-and-forth movement.
[0011] Further preferably, the magnetic field generating device comprises opposite magnetic poles, which are magnetic bars or permanent magnets.
[0012] Further preferably, the powder is a positive and negative electrode material for a lithium battery, including ternary lithium, lithium iron phosphate, aluminum powder, copper powder and graphite.
[0013] Further preferably, the lithium battery positive and negative electrode material recovery system based on electromagnetic separation also includes a vibrating screen arranged at the feed inlet, which is used to make the powder evenly contact the conductive track and the conductive positive plate.
[0014] Further preferably, the conductive track is an ultrasonic vibration track.
[0015] In a second aspect, the present application provides a method for recycling positive and negative electrode materials of lithium batteries based on electromagnetic separation, comprising the following steps:
[0016] The powder is placed on a conductive track, and a DC high voltage is applied between the conductive track and the conductive positive plate to form a parallel electrostatic field, so that the powder moves back and forth between the conductive positive plate and the conductive track;
[0017] When the powder moves back and forth between the conductive positive plate and the conductive track, a magnetic field perpendicular to the electric field and parallel to the conductive track is applied, so that the powder is deflected by the Lorentz force, thereby achieving separation of different powders.
[0018] The separated powder is recovered.
[0019] Further preferably, by controlling the distance between the conductive track and the conductive positive plate, the magnitude of the high voltage DC voltage and the strength of the electrostatic field, the rate at which the powder accumulates charge, the magnitude of the electrostatic force it is subjected to and the speed of traveling back and forth between the conductive positive plate and the conductive track are controlled.
[0020] Further preferably, powder sorting is achieved by controlling the magnetic field strength and the inclination angle between the conductive positive plate and the conductive track.
[0021] In general, the above technical solutions conceived by this application have the following beneficial effects compared with the prior art:
[0022] The present application provides a lithium battery positive and negative electrode material recovery system based on electromagnetic separation, which eliminates the insulating layer of the positive electrode plate so that the powder obtains a positive charge when it reaches the positive electrode plate and returns to the negative electrode track, thereby achieving the effect of the powder quickly moving back and forth between the positive and negative electrode plates. Moreover, since the direction of movement and the net charge change simultaneously during the round-trip process, the Lorentz force they are subjected to during the round-trip process is always in the same direction. However, since the magnitude of the Lorentz force on different powders varies greatly, the powder will eventually be separated by the Lorentz force during multiple round-trip processes.
[0023] The present application provides a lithium battery positive and negative electrode material recovery system based on electromagnetic separation, in which opposite magnetic poles, i.e., strong permanent magnets, are used as magnetic field supply and fixed between a conductive track and a conductive positive electrode plate to provide conditions for the deflection of powder in the magnetic field.
[0024] The present application provides a lithium battery positive and negative electrode material recovery system based on electromagnetic separation, wherein a vibrating screen is added to the feed inlet, and a vibrating track is used in a strong electric field generating device as an electrode for electrostatic separation, thereby avoiding material stacking; compared with traditional track-type electrostatic separation, which is suitable for millimeter-level material separation, the use of a magnetic field can repeatedly exert the advantages of electrostatic separation and improve the separation efficiency of micron-level materials. BRIEF DESCRIPTION OF THE DRAWINGS
[0025] Figure 1 This is a schematic diagram of a lithium battery positive and negative electrode material recovery system based on the electromagnetic separation principle provided in an embodiment of the present application;
[0026] Figure 2 It is a schematic diagram of the principle of using an inclination angle between the conductive positive plate and the conductive track provided in an embodiment of the present application;
[0027] Figure 3 It is a front view of a lithium battery positive and negative electrode material recovery system based on electromagnetic separation provided in an embodiment of the present application;
[0028] Figure 4 It is a side view of a lithium battery positive and negative electrode material recovery system based on electromagnetic separation provided in an embodiment of the present application;
[0029] Figure 5 This is a schematic diagram of powder of lithium battery material recycling provided in an embodiment of the present application;
[0030] Among them, 1-opposite magnetic poles; 2-high voltage DC power supply; 3-conductive positive plate; 4-second conductive track; 5-front stage vibrating screen; 7-rotating shaft; 8-material collecting device. DETAILED DESCRIPTION
[0031] The embodiments of the present application are described below in conjunction with the drawings in the embodiments of the present application.
[0032] like Figure 1As shown, the lithium battery positive and negative electrode material recovery system based on electromagnetic separation provided by the present application is based on the net charge accumulation formed under the electrostatic field when the powder contacts the electrode plate, and travels back and forth between the two electrode plates under the action of the electric field. Since the net charge accumulation rates and round-trip rates of powders with different conductivity are different, the Lorentz forces they are subjected to in the magnetic field are also different. In the process of multiple round trips, the difference in Lorentz force is used to achieve path diversification of the powder and separation.
[0033] A more detailed description is as follows:
[0034] First, the reason why electrostatic separation is theoretically suitable for the separation of small-size materials is explained: electrostatic separation uses high-voltage static electricity to generate a strong electric field. Due to the unique electrostatic balance property of a good conductor, a new charge distribution can be quickly formed when it enters a strong electric field, making the internal electric field strength of the good conductor zero, and the charge is distributed on the surface of the good conductor; for objects with relatively flat dimensions (height not greater than length and width), the relationship between the surface charge density and the field strength of a parallel plate can be approximated: σ = ε·E; that is, when the sample shape is consistent, the surface charge density has nothing to do with the sample size, but only with the electric field strength, so the net charge of the particle can be expressed as follows:
[0035] Q s =∫σds∝E·r 2
[0036] Among them, σ is the surface charge density, ε is the dielectric constant of the material itself, E is the electric field strength, Q S is the net charge of the particle, r is a measure of the particle size (which can generally refer to its radius / length of main feature, etc.);
[0037] Specifically, for a bar-shaped object, the net charge can be expressed as follows:
[0038]
[0039] Where, l is the length of the strip, and D is the diameter of the strip;
[0040] For a flat object, the net charge can be expressed as follows:
[0041]
[0042] Where D is the diameter of the flat object;
[0043] For a spherical object, its net charge can be expressed as follows:
[0044]
[0045] Where D is the diameter of the spherical object (particle);
[0046] Taking a spherical object as an example, the force and acceleration of a particle in an electric field can be expressed as:
[0047]
[0048] It can be concluded from the relationship that the acceleration of the particle is proportional to the square of the electric field strength and inversely proportional to the particle size, so the electrostatic separation system is theoretically more suitable for the separation of small-scale particles;
[0049] Second aspect: Explain why the electrostatic separation system is actually not suitable for stacked powder separation:
[0050] Using metal plates and conductive tracks to connect the positive and negative electrodes of high-voltage static electricity respectively can generate a strong electric field of 100,000 V / m between the parallel plates. When metal particles enter between the parallel plates, due to their high conductivity, they will quickly form an internal electrostatic balance (the total field strength inside the metal is zero). At this time, an unbalanced distribution of charge appears on the surface of the particles, but the net charge is zero, and the electric field force is zero. When metal particles are between the parallel plate electrodes and the surface of the particles contacts the electrodes, the charge on one side of the particles will be conducted to the ground, and the charge is zero. In order to maintain electrostatic balance, the charge on the other side is non-zero, forming a net charge non-zero situation. Under the action of the strong electric field, the metal particles will be attracted to the other side of the plate. The necessary conditions for achieving this goal are: the metal particles must contact the plate to form an uneven net charge distribution. When a large amount of low-conductivity powder and a small amount of high-conductivity powder are stacked, it is not easy for both to accumulate charge, which is why stacked powders are not suitable for electrostatic separation.
[0051] The third aspect: Explain why this solution uses an inclination angle between the conductive positive plate and the conductive track:
[0052] like Figure 2 As shown in the figure, the inclination angle between the conductive positive plate and the conductive track is θ. According to the Comsol simulation results, when the powder with a particle size of about 100 μm contacts the conductive positive plate under the condition of an electric field strength of 10 kV / m, it will generate about 10 -14 C, taking the actual device as an example (voltage is about 20kV, plate spacing is 4.5cm, electric field strength is 444kV / m), the fully charged charge should reach 4.44×10 -13 C.
[0053] In the actual experiment video, the movement speed of aluminum powder is estimated to be about 0.5m / s based on the powder afterimage. The lithium iron phosphate powder is darker in color and has a smaller adsorption amount, so it is not easy to observe its speed. It is temporarily estimated to be 0.22m / s. In the process of back and forth movement, the particles will lose a certain amount of kinetic energy through rebound many times until the speed of movement between the conductive positive plate and the conductive track remains basically constant; in this process, the electrical energy obtained from each round trip between the conductive positive plate and the conductive track is equivalent to the kinetic energy lost due to air friction and rebound.
[0054] like Figure 2As shown in the figure, the inclination angles of the conductive positive plate and the conductive track are both θ. When the particle collides with the conductive positive plate and the conductive track, it should be subjected to an elastic force in the direction of the light reflection law. If there is no intervention of the Lorentz force, the particle will continue to be subjected to elastic force when colliding back and forth between the conductive positive plate and the conductive track, and its component is to the right, eventually causing the particle to accelerate to the right. Only when the Lorentz force causes the final velocity of the particle to deviate from the vertical direction by 2θ, can the influence of the horizontal component of the elastic force be exactly balanced. The optional range of the inclination angle will be calculated as follows:
[0055] Assuming that the inclination angle between the conductive positive plate and the conductive track is θ, when the particle contacts the conductive positive plate and the conductive track, when the angle between the final velocity and the vertical direction is greater than 2θ, the particle will continue to accelerate in the direction of the Lorentz force. When the angle is less than 2θ, the particle will continue to accelerate to the right due to the elastic force.
[0056] According to previous estimates of the net charge of the particle, its charge is approximately: 4.4×10 -13 C. According to Comsol simulation results, the N48 neodymium magnet used in the experimental size can generate a magnetic field strength of 0.15 T at a 7 cm interval. Due to the existence of air resistance, it should be considered that the powder is accelerated in the electric field until it reaches uniform motion. The following calculation process will only consider one acceleration motion; it should be pointed out here that the first result can determine whether the subsequent particles move to the left or right.
[0057] The movement speed of aluminum particles in a magnetic field:
[0058] v Al =0.5m / s
[0059] Due to the different conductivity, the aluminum particles can quickly reach electrostatic equilibrium, and the net charge is:
[0060] q 铝 =4.4×10 -13 C
[0061] Assume that the net charge of lithium iron phosphate is 1 / 5 of that of aluminum powder, that is,
[0062] q LFP =8.8×10 -14 C
[0063] According to the formula of air resistance of an object:
[0064] F=CSρv 2
[0065] It can be obtained that the air resistance of an object is proportional to the square of the relative speed, where C is the air resistance coefficient, S is the windward area of the object, and v is the speed of the object relative to the air. The speed of the lithium iron phosphate powder can be estimated as:
[0066] vLFP =0.22m / s
[0067] Next, calculate the magnitude of the lateral velocity of the powder when it arrives at the conductive track from a conductive positive plate under the action of the Lorentz force:
[0068] Lorentz force: F 洛 =Bvq
[0069] Acceleration due to Lorentz force: a 洛 =Bvq / m
[0070] Through the Lorentz force acceleration it can be determined that two substances can be separated by time;
[0071] The magnitude of the transverse velocity caused by the Lorentz force can be obtained by the following integral:
[0072]
[0073] Where B is the magnetic field strength, q is the total net charge of the particle, h is the distance between the plates, and m is the mass of the particle;
[0074] It can be concluded that the lateral velocity caused by the Lorentz force is proportional to the magnetic field strength, the distance between the conductive positive plate and the conductive track, and the net charge, and inversely proportional to the mass of the particle, but has nothing to do with the speed in this process; that is, whether the speed changes or how it changes in the process of flying to the conductive positive plate or the conductive track, it will not affect the lateral velocity of the particle when it contacts the plate; it should be pointed out that according to the existing lateral velocity, longitudinal velocity and the limit conditions of the inclination angle when contacting the conductive positive plate, the inclination angle can be calculated;
[0075] When the powder contacts the inclined plate due to elastic force, a lateral motion velocity will be generated. Therefore, in order for the Lorentz force to overcome the lateral motion velocity generated by the elastic force, the angle between the final trajectory of the particle movement and the vertical direction needs to be greater than 2θ, so there is the following relationship:
[0076] when: When the Lorentz force overcomes the elastic force, the particle will continue to move in the direction of the Lorentz force, otherwise the particle will be ejected in the direction of the inclined opening;
[0077] In the embodiment of the present application, B=0.15T; h=0.045m; V=20000V; particle diameter is 100μm. According to the above conditions, we can get:
[0078] The critical inclination angle of aluminum powder is: θ Al =3.8×10 -4 Deg
[0079] The critical tilt angle of lithium iron phosphate powder is: θ LFP =1.35×10 -4Deg
[0080] The tilt margin is: 2.45×10 -4 Deg.
[0081] The conditions available in actual industrial applications are: the magnetic field is at the Tesla level, the electrostatic high voltage can reach one million volts, and the distance between the conductive positive plate and the conductive track can be increased to the meter level accordingly. The inclination margin in industrial applications can reach 1°. Between the extreme inclination angles of the two materials, lithium iron phosphate can be ejected toward the open direction by elastic force, and aluminum powder can be ejected toward the narrow direction by Lorentz force, thereby realizing powder sorting.
[0082] Fourth aspect: Powder separation applicable to lithium battery positive and negative electrode material recovery system:
[0083] For lithium iron phosphate powder, an electrostatic equilibrium is formed (taking q = 0.98q max ) takes 35ms; for aluminum powder, the time required to form electrostatic equilibrium is 1.05×10 -19 s; for conductors, electrostatic equilibrium is completed in an instant, and the calculation results are consistent with this common sense; for insulators, such as the commonly used plastic polyethylene, its conductivity is 10 -16 S / cm, and the time for particles of the same particle size to reach electrostatic equilibrium is about 350,000s. Therefore, the issue of whether insulators will be adsorbed by static electricity is generally not considered, so ordinary electrostatic separation will not emphasize letting the powder leave the electrode plate quickly, and usually a conductive track is used for aluminum-plastic separation; based on the example, it can be considered that: materials that reach electrostatic equilibrium within milliseconds are more suitable for the lithium battery positive and negative electrode material recovery system provided in this application. The separated substances are composed of high-conductivity substances (such as metals) and semiconductors (such as lithium iron phosphate). There is an order of magnitude difference in the electrostatic equilibrium time between them, and neither of them is an insulator. Using traditional electrostatic separation methods, it is easy to adsorb two powders at the same time, and it is difficult to achieve sorting.
[0084] In summary, powders with different electrical conductivity can be separated using the lithium battery positive and negative electrode material recovery system provided in this application, and the powder with the worst electrical conductivity should also be able to reach electrostatic equilibrium within 1 s; for example, the value of the powder with poor electrical conductivity should be within (10 -7 S / cm-10 -12 S / cm), too high conductivity will make the sorting effect worse, while too low conductivity will lead to a more suitable electrostatic separation method.
[0085] In order to solve the stacking problem and the problem that traditional electrostatic separation equipment has poor effect in separating semiconductors and conductor mixtures with similar density, the present application uses a vibrating screen feed and an ultrasonic vibration track to allow the powder to evenly contact the surface of the power grid (solve the stacking problem), so that each conductive particle can contact the electrode plate and accumulate charge, and move to the other electrode plate under the action of the electric field, and complete the reverse movement after contacting the other electrode plate, causing the powder to go back and forth between the two electrodes; however, due to the different electrical conductivities of aluminum powder and lithium iron phosphate powder, their respective charge accumulation rates are different. Aluminum powder can accumulate a large amount of charge at the moment of contacting the electrode plate, and its movement speed in the electric field is also very fast. However, since lithium iron phosphate accumulates charge at a slower rate, the amount of charge in the process is small, and the movement speed is slow. At this time, a strong magnetic field is added in the vertical direction of their movement direction, and the Lorentz force they are subjected to will be greatly different, thereby achieving the separation effect of the Lorentz force disproportionate powder path, solving the problem that semiconductors can also accumulate charge in a shorter time, and traditional electrostatic separation methods are difficult to achieve high-precision sorting.
[0086] like Figure 3 As shown, the present application provides a lithium battery positive and negative electrode material recovery system based on electromagnetic separation, including: a strong electric field generating device, a magnetic field generating device and a material collecting device;
[0087] The strong electric field generating device comprises: a high voltage DC power supply 2, a conductive positive plate 3 and a conductive track 4; wherein the conductive track 4 is grounded, and is used to determine a fixed potential and transfer part of the powder charge to form a net charge accumulation; the conductive positive plate 3 and the conductive track 4 are substantially parallel, but there is a slight inclination angle, the purpose is to make the powder with a small Lorentz force have a tendency to move to the left during the back and forth movement;
[0088] The magnetic field generating device includes an opposite magnetic pole 1, which is used to generate a strong magnetic field so that the powder is subjected to the Lorentz force to produce orbital deflection. It can usually be composed of a magnetic bar and a permanent magnet. The direction of the magnetic field is perpendicular to the direction of the electric field and parallel to the running direction of the conveyor belt (conductive crawler);
[0089] The material collection device includes insulating containers to avoid affecting the electromagnetic field, which are placed on both sides of the conveyor belt (conductive track) and close to the magnetic field area to collect the separated powder, such as Figure 4 shown.
[0090] A more complete technical solution is introduced as follows:
[0091] The lithium battery material recovery system based on electrostatic separation and magnetic field regulation provided by the present application is a ternary lithium, lithium iron phosphate positive electrode and graphite negative electrode and Al and Cu impurity sorting system based on the principle of electrostatic separation and with magnetic field regulation as an auxiliary means; the system uses a conductive track, a positive plate and a high-voltage power supply as an electric field generating device, and the conductive track and the positive plate have a certain deflection angle, and cooperate with the high-voltage power supply to form a basically parallel electrostatic field; using a magnetic pole as a magnetic field generating device, a magnetic field perpendicular to the electric field is obtained, and when the powder goes back and forth between the positive and negative poles, the magnetic field provides the Lorentz force required for separation; during operation, the spacing between the conductive track and the positive plate and the voltage of the high-voltage power supply are controlled to control the electric field strength, which determines the rate at which the metal powder accumulates charge, the magnitude of the electrostatic force, and the speed of the plate; by regulating the magnetic field strength and the inclination angle of the positive and negative plates, the competition between the Lorentz force and the elastic force is realized, and the powder sorting is realized. The present application is based on the principle of electrostatic separation and regulation to achieve efficient sorting of lithium-ion battery electrode materials and metal materials.
[0092] Example
[0093] This embodiment provides a lithium battery material recovery system based on electrostatic separation and magnetic field regulation, including an upper plate, a lower plate, a permanent magnet, a high voltage generating device and an insulating material;
[0094] The permanent magnet is an N48 permanent magnet, and its residual magnetic flux density is about 1.3T. In this embodiment, the size of a single magnet is: 20mm*40mm*100mm. Two magnets are stacked to form a permanent magnet to increase the thickness and field strength in the central area. The NS level of the two permanent magnets faces each other with a spacing of 7cm. The simulation results show that the central magnetic field strength is about 0.15T;
[0095] The upper electrode plate and the lower electrode plate are conductive copper foils, wherein the upper electrode plate is formed by folding the conductive copper foil, the thickness of the copper foil is 0.15 mm, and the distance between the electrode plates is 4.5 cm;
[0096] The DC voltage between the plates is provided by a high-voltage package, the parameters of which are: 24V DC to 20kV DC, where the negative electrode is connected to the conductive copper foil of the lower plate, and the positive electrode is connected to the conductive copper foil of the upper plate. It can be concluded that the field strength between the plates is: 444kV / m;
[0097] The powder materials used are: 100μm aluminum powder and lithium iron phosphate samples (the samples contain extremely fine particles, most of which are around 100μm, and a small number of samples have agglomeration). The sample mixing ratio is: the volume ratio of aluminum powder to lithium iron phosphate powder is 1:1, and the mass ratio is 2:1;
[0098] Actual operation:
[0099] Pour a small amount of mixed powder on the lower plate. After power is turned on, a small number of particles are observed to move back and forth between the plates. Use a brush to gently brush the powder and spread it as evenly as possible to ensure that the particles can contact the plates to the greatest extent. In the process of using a brush instead of vibration, a large amount of powder can be observed to move back and forth. After a period of time, some powder appears in the outer area of the plate, and the powder inside the plate returns to calm. Use a brush to collect the powders in the outer area of the plate and the inner area of the plate separately. It is found that the colors of the two powders are significantly different. The aluminum content of the powder in the outer area of the plate is higher, and the frequency of agglomerated lithium iron phosphate is higher. The content of lithium iron phosphate powder in the powder in the inner area of the plate is higher, such as Figure 5 shown.
[0100] The shortcomings of the current solution are that part of the lithium iron phosphate is agglomerated, and part of it seems to be sticky after mixing with aluminum powder. It is necessary to replace the dry lithium iron phosphate sample with a more uniform particle size distribution for testing. The collection device has not been installed yet, resulting in a large part of the powder in the outer area of the plate being wasted and the collection amount is small; the permanent magnet spacing is large, and the magnetic field strength at the center of the permanent magnet with a spacing of 7cm is not large, which may lead to a low separation effect; the plate spacing of 4.5cm is not convenient to adjust for the time being.
[0101] In summary, compared with the prior art, this application has the following advantages:
[0102] The present application provides a lithium battery material recovery system based on electrostatic separation and magnetic field regulation, in which an ultrasonic vibration track, a positive plate and a high-voltage DC power supply are used as a strong electric field generating device, wherein the track is connected to an ultrasonic source using an insulating component to generate high-frequency mechanical vibrations.
[0103] The present application provides a lithium battery material recovery system based on electrostatic separation and magnetic field regulation, in which opposite magnetic poles, i.e., strong permanent magnets, are used as magnetic field supply and fixed between a conductive track and a conductive positive plate to provide conditions for the deflection of powder in the magnetic field.
[0104] The present application provides a lithium battery material recovery system based on electrostatic separation and magnetic field regulation, wherein a vibrating screen is added to the feed inlet, and a vibrating track is used in a strong electric field generating device as an electrode for electrostatic separation to avoid material stacking; compared with traditional track-type electrostatic separation, which is suitable for millimeter-level material separation, the use of a magnetic field can repeatedly exert the advantages of electrostatic separation and improve the separation efficiency of micron-level materials.
[0105] The existing electrostatic separation system is a one-time separation, which is generally a positive plate plus an insulating layer. The positive plate is made into a screen to catch the dust. The voltage between the positive plate and the negative plate is small, and only a small amount of charge accumulation is provided. Subsequently, an ultra-high voltage electric roller is placed at the end of the track to change the trajectory of the powder. These electrostatic separation devices are difficult to guarantee the effect of one-time separation, and the material may be reworked or a multi-stage separation device may be made, and multiple electrostatic separations are performed to improve the separation rate. Because powders of different conductivity acquire charge at different speeds when they contact the negative track, they have different charges when they are attracted to the mid-air between the track and the positive plate, and their round-trip speeds are also different. They will be subject to different Lorentz forces in the magnetic field, which will cause their movement trajectories to be different. However, after calculation, the magnetic field deflection force is much smaller than the electric field force. Therefore, in the process of the powder flying to the positive plate, the trajectory is less affected by the magnetic field. In order to solve this problem, it is necessary to remove the insulating layer of the positive plate so that the powder can obtain positive charge when it reaches the positive plate and return to the negative track, thereby achieving the effect of the powder quickly moving back and forth between the positive and negative plates. And because their movement direction and net charge change simultaneously during the round-trip process, the Lorentz force they are subjected to during the round-trip process is always in the same direction. However, since the magnitude of the Lorentz force on different powders varies greatly, the powder will eventually be separated by the Lorentz force during multiple round-trip processes.
[0106] It should be understood that expressions such as "including" and "may include" that may be used in the present application indicate the existence of the disclosed functions, operations, or constituent elements, and do not limit one or more additional functions, operations, and constituent elements. In the present application, terms such as "including" and / or "having" may be interpreted as indicating specific characteristics, numbers, operations, constituent elements, components, or combinations thereof, but may not be interpreted as excluding the existence or possibility of adding one or more other characteristics, numbers, operations, constituent elements, components, or combinations thereof.
[0107] In addition, in the present application, the expression "and / or" includes any and all combinations of the associated listed words. For example, the expression "A and / or B" may include A, may include B, or may include both A and B.
[0108] In the description of the embodiments of the present application, it should be noted that, unless otherwise clearly specified and limited, the term "connection" should be understood in a broad sense.
[0109] The above is only a specific implementation of the present application, but the protection scope of the present application is not limited thereto. Any person skilled in the art who is familiar with the present technical field can easily think of changes or substitutions within the technical scope disclosed in the present application, which should be included in the protection scope of the present application. Therefore, the protection scope of the present application should be based on the protection scope of the claims.
Claims
1. A lithium battery positive and negative electrode material recovery system based on electromagnetic separation, characterized in that: include: Strong electric field generating device, magnetic field generating device and material collecting device; The strong electric field generating device includes a high voltage power supply, a conductive positive plate and a conductive track; The conductive track is grounded to determine a fixed potential and transfer part of the powder charge to form a net charge accumulation; the conductive track and the conductive positive plate, together with the high voltage power supply, form a parallel electrostatic field to make the powder go back and forth between the conductive positive plate and the conductive track; different types of powder accumulate charge at different rates; The magnetic field generating device is used to generate a magnetic field perpendicular to the electric field and parallel to the conductive track. When the powder moves back and forth between the conductive positive plate and the conductive track, the powder is subjected to the Lorentz force to produce orbital deflection, thereby achieving separation of different powders. The material collecting devices are respectively located on both sides of the conductive track, near the magnetic field area, for collecting the separated powder; wherein, the area near the magnetic field area is an area less than a preset distance from the magnetic field area.
2. The lithium battery positive and negative electrode material recovery system according to claim 1, characterized in that: There is a preset small angle between the conductive positive plate and the conductive track, which is used to make the powder with small Lorentz force have a tendency to move laterally due to elastic force during the back-and-forth movement.
3. The lithium battery positive and negative electrode material recovery system according to claim 1 or 2, characterized in that: The powders include ternary lithium, lithium iron phosphate, aluminum powder, copper powder and graphite.
4. The lithium battery positive and negative electrode material recovery system according to claim 1, characterized in that: It also includes a vibrating screen arranged at the feeding port, which is used to make the powder contact the conductive track and the conductive positive plate evenly.
5. The lithium battery positive and negative electrode material recovery system according to claim 1 or 4, characterized in that: The conductive track is an ultrasonic vibration track.
6. A lithium battery material recycling method based on the lithium battery positive and negative electrode material recycling system according to claim 1, characterized in that: The following steps are involved: The powder is placed on a conductive track, and a DC high voltage is applied between the conductive track and the conductive positive plate to form a parallel electrostatic field, so that the powder moves back and forth between the conductive positive plate and the conductive track; When the powder moves back and forth between the conductive positive plate and the conductive track, a magnetic field perpendicular to the electric field and parallel to the conductive track is applied, so that the powder is deflected in the orbit by the Lorentz force, thereby separating different powders and recovering the separated powder.
7. The method for recycling positive and negative electrode materials of lithium batteries according to claim 6, characterized in that: By controlling the distance between the conductive track and the conductive positive plate, the magnitude of the high voltage DC voltage and the strength of the electrostatic field, the rate at which the powder accumulates charge, the magnitude of the electrostatic force it is subjected to and the speed of traveling back and forth between the conductive positive plate and the conductive track are controlled.
8. The method for recycling positive and negative electrode materials of lithium batteries according to claim 6, characterized in that: Powder sorting is achieved by controlling the magnetic field strength and the inclination angle between the conductive positive plate and the conductive track.
Citation Information
Patent Citations
Recycling method of retired lithium ion battery positive electrode materials
CN110760685A
Device and method for preparing rice protein through magnetic field-assisted electrostatic separation
CN114160303A
Separation and recovery method for positive and negative active substances of waste lithium iron phosphate
CN114700179A
Method for recovering valuable material from lithium ion secondary battery
CN116056811A
Device for separating conductive particles and non-conductive particles based on vertical magnetic field and working method
CN117414945A
Cited By
Detection jig for display screen
CN119845728A