Mold for manufacturing rock-like material containing internal prefabricated cracks and crack manufacturing method

By using positioning bolts and angle height marking in rock sample molds, and casting similar materials in the mold cavity, the problem of large mold consumption and insufficient precision in the prior art is solved, and efficient and accurate Rock sample production enhances the accuracy of rock mechanics tests.

CN118977312AActive Publication Date: 2024-11-19CHINA FIRST METALLURGICAL GROUP
View PDF 8 Cites 0 Cited by

Patent Information

Application Number
CN202411202069.2
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-29
Publication Date
2024-11-19
Estimated Expiration
2044-08-29

AI Technical Summary

Technical Problem

When making rock materials containing internal prefabricated cracks, the mold consumption is large, the cost is high, and the accuracy is insufficient, making it difficult to meet the crack simulation needs of different angles, quantities and spacings, which affects the accuracy of rock mechanics tests.

Method used

A system consisting of rock-like sample molds and prefabricated crack molds was designed to fix ice prefabricated cracks through positioning bolts and angle height identification, and similar materials were poured into the mold cavity to form prefabricated cracks of different numbers, angles and spacings. Rock-like sample.

Benefits of technology

It achieves precise control of the number, spacing and angle of cracks, reduces the test cost, improves the test efficiency and sample integrity, and enhances the research value of the crack expansion mechanism of rock internal cracks.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118977312A_ABST
    Figure CN118977312A_ABST
Patent Text Reader

Abstract

The invention discloses a mold for manufacturing a rock-like material containing internal precracks and a crack manufacturing method.The mold comprises a rock-like sample mold (1), a bottom mold (2) and a precrack mold (3), the rock-like sample mold (1) comprises a first side mold (11) and a second side mold (12), the center of each side mold is provided with a positioning long round hole (13), a positioning bolt (14) can be fixed to each positioning long round hole (13), and the bottom mold (2) is provided with a plurality of through holes (13); an angle height mark (15) is arranged on the outer side of the base; the precrack mold (3) comprises a threading platform (33) and is used for fixing a fine cotton thread (34), an ice precrack (37) with the fine cotton thread (34) is manufactured after water injection and freezing, and the fine cotton threads (34) at the two ends of the ice precrack (37) are tied to the positioning bolts (14) at different positions of the rock sample mold (1), so that precracks with different angles and intervals can be formed. The device is simple in structure, convenient to use and suitable for manufacturing rock-like samples with different numbers of precracks, angles and intervals.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention belongs to the technical field of geotechnical engineering, and more specifically, relates to a mold for making a rock material containing internal prefabricated cracks and a crack making method. Background Art

[0002] As an engineering material, rock mass is widely used in engineering structures such as buildings, roads, bridges, tunnels and dams. However, there are often cracks inside the rock mass. Cracks of different sizes inside the rock mass expand and penetrate under the action of external forces, causing rock rupture, leading to the destruction and instability of engineering structures, and affecting the project. Therefore, the study of cracks inside the rock mass and their expansion mechanism is of great significance for preventing and controlling rock rupture and engineering structure damage.

[0003] At present, indoor tests are mainly used to study the crack propagation mechanism inside the rock mass. By making different rock samples, the initiation, expansion and penetration mechanisms of cracks under different conditions can be systematically studied, providing basic data for understanding the rock mass destruction process. Therefore, the production of rock samples containing internal cracks is crucial. In the prior art, the original rock sample is formed by cutting, and then the internal cracks are made, such as the patent document with the publication number CN201710116338.7. The present invention provides a method for making prefabricated cracks inside a rock sample, comprising the following steps: step one, cutting of the rock sample; step two, crack making: using a machine tool or a water jet to perform prefabricated crack processing, drilling holes on the two end faces of the sample unit, that is, the cutting surface of the rock sample, and then forming cracks; step three, splicing of the sample unit; step four, curing of the spliced ​​sample: after the splicing is completed, normal pressure evaporation curing is adopted. After the curing is completed, it is left to air dry under natural conditions, and then fine sandpaper or a wet rag is used to remove the high-strength cement protruding from the surface of the spliced ​​sample. This method is low in cost, easy to make, and can be mass-produced. However, the method for making the prefabricated cracks is a cutting method, which has high requirements for cutting machinery and high sample production costs; and the final rock sample is spliced ​​by high-strength cement, which affects the integrity of the rock sample, and the difficulty of making a complete rock sample is high. For example, the patent document with the publication number CN201410019613.X discloses a true triaxial rock sample crack prefabrication device, which can make cracks of a predetermined number, position, size and angle on the true triaxial rock sample by adjusting the size of the clamp, which can meet the requirements of different rock sample sizes and different crack prefabrication schemes, and is convenient for conducting experimental research on the expansion of multiple cracks in rocks and their penetration failure mechanism. The present invention has a simple structure, reasonable design, easy use, efficient and feasible crack production, and is particularly suitable for crack prefabrication of true triaxial rock samples of soft rocks. However, this device consumes a transparent mold for each sample it makes, and the mold consumption is large and the cost is high; and the prefabricated cracks are through cracks, not non-penetrating cracks.

[0004] With the proposal of similarity principle, researchers began to use similar materials of rock (such as gypsum and concrete) to simulate the development and penetration mechanism of cracks inside rocks. As disclosed in the patent document with publication number CN202110832252.0, the present invention discloses an adjustable rock-like material crack prefabrication device, including a base fixing mechanism, a material filling mechanism and a variable crack positioning adjustment mechanism, the base fixing mechanism includes a base and a base assembly; the material filling mechanism includes a bearing seat and a filling mold; the filling mold is a rectangular cylinder with adjustable length and width; the variable crack positioning adjustment mechanism includes a crack positioning plate, a crack body assembly and a crack locator, the number of crack body assemblies and crack locators is determined by the number of cracks prepared in the rock-like material, the crack body assembly is vertically arranged between the crack positioning plate and the bearing seat, and the bottom of the crack body assembly is detachably connected to the intersection of the groove of the bearing seat. The present invention can prefabricate cracks of different lengths, widths, numbers, spacings and pattern sizes for rock-like materials, providing convenience for the preparation of samples in rock mechanics tests. However, the device is realized by setting up a fracture body, which has a certain impact on the research of crack diffusion and penetration mechanism. In the prior art, rock mechanics tests require a large number of samples, and the sampling and preparation of rock samples face many difficulties. Similar material samples usually use solid materials such as mica sheets and iron sheets to simulate cracks. These methods have certain limitations, such as the great impact on the research of crack diffusion and penetration mechanism. In addition, the existing mold technology has problems such as large mold consumption, high production cost, insufficient precision, and inflexible design and use of molds when making rock samples with internal prefabricated cracks. It is difficult to meet the needs of crack simulation with different angles, numbers and spacings. In order to more accurately simulate and study the behavior of cracks inside rocks, it is necessary to be able to accurately control the number, spacing and angle of cracks, and the existing technology is difficult to meet this demand. Summary of the invention

[0005] In view of the above defects or improvement needs of the prior art, the present invention provides a mold for making a rock-like material containing internal prefabricated cracks and a crack making method. Ice prefabricated cracks that meet different test requirements are made through the prefabricated crack mold. The ice prefabricated cracks are fixed on the positioning bolts at different positions through the angle height markings and positioning bolts of the rock-like sample mold. Similar materials are poured in the mold cavity to form rock-like samples containing prefabricated cracks of different numbers, angles and spacings.

[0006] In order to achieve the above-mentioned object, according to one aspect of the present invention, a mold for making a rock-like material containing internal prefabricated cracks is provided, comprising a rock-like sample mold for making a similar material sample, a bottom mold and a prefabricated crack mold for making prefabricated cracks, wherein:

[0007] The rock sample mold comprises a first side mold and a second side mold, wherein a positioning oblong hole is provided at the center of the first side mold and the second side mold, and a positioning bolt is fixed thereon, and an angle height mark is provided on the outer side of the positioning oblong hole according to the number, angle and spacing of the prefabricated cracks in the design;

[0008] The prefabricated crack mold includes a water container and a water injection channel, and a threading platform is arranged at the intersection thereof. The threading platform is a cylinder with a notch, which is used to fix fine cotton thread. Water is injected into the prefabricated crack mold and then frozen to form a prefabricated crack with the fine cotton thread. The fine cotton threads at both ends of the prefabricated crack are tied to the positioning bolts at different positions of the rock-like sample mold, and similar materials are poured in the cavity of the rock-like sample mold to form rock-like samples containing prefabricated cracks of different numbers, angles and spacings.

[0009] Furthermore, the rock-like sample mold also includes a first baffle and a second baffle, which are used to close the positioning oblong holes on the first side mold and the second side mold to form a casting cavity with side enclosed, and the thin cotton thread passes through the middle of the first baffle and the second baffle.

[0010] Furthermore, the rock-like sample mold also includes fastening belts for fastening the top and bottom ends of the rock-like sample mold.

[0011] Furthermore, the contact parts of the first side mold and the second side mold are respectively designed with concave and convex grooves with a width and height of 1mm-5mm to ensure that the joints are tight and leak-proof.

[0012] Furthermore, the bottom mold includes circular grooves for placing the first side mold and the second side mold of the rock-like sample mold.

[0013] Furthermore, the prefabricated crack mold also includes a thickness mark provided on the inner wall of the water container for determining the thickness of the prefabricated crack.

[0014] Furthermore, the prefabricated crack mold also includes a crack baffle for adjusting the water level in the water containing device by adjusting the opening of the crack baffle according to test requirements.

[0015] Furthermore, the rock sample mold may be cylindrical or rectangular or may be adjusted to a desired shape according to the test.

[0016] Furthermore, the shape of the prefabricated crack mold is adjusted according to test requirements and matches the rock-like specimen mold.

[0017] According to another aspect of the present invention, a method for making cracks in a rock material containing internal prefabricated cracks is provided, which is implemented by using the above-mentioned mold for making a rock material containing internal prefabricated cracks, and comprises the following steps:

[0018] S100: similar materials for preparing rock samples;

[0019] S200: using the prefabricated crack mold to make a prefabricated crack, firstly passing the fine cotton thread through the threading platform, then installing the crack baffle, then injecting water into the center of the prefabricated crack mold, stopping the water injection after the water level reaches the required thickness mark, putting the entire prefabricated crack mold into a refrigerator to freeze, after the freezing is completed, putting the prefabricated crack mold into warm water for a few seconds, taking out the prefabricated crack together with the fine cotton thread to obtain the prefabricated crack, and then putting the prefabricated crack into the refrigerator to freeze for standby use, and the same method can be used to make a variety of prefabricated cracks of different thicknesses for standby use;

[0020] S300: According to the number, angle and spacing of the designed prefabricated cracks, the angle height mark is determined by calculation, and the positioning bolt is screwed into the positioning oblong hole on the first side mold according to the angle mark to fix it, and then another position is selected according to the height mark, and the positioning bolt is screwed into the positioning oblong hole and fixed, and then the fine cotton thread on the prefabricated crack is tied to the positioning bolt, and the first baffle plate and the second baffle plate of the first side mold are immediately installed, and the same operation is performed on the second side mold; while tying the fine cotton thread, the first side mold and the second side mold are slowly spliced ​​along the notch, and the spliced ​​rock-like mold is placed in the circular groove of the base membrane and fastened with a fastening belt to form a casting cavity;

[0021] S400: Similar materials are poured into the cavity, and after vibration, curing and demolding, uniaxial and triaxial rock samples with real prefabricated cracks in different numbers, angles and spacings can be obtained.

[0022] In general, the above technical solutions conceived by the present invention can achieve the following beneficial effects compared with the prior art:

[0023] 1. The prefabricated crack mold of the present invention can accurately produce prefabricated cracks of different thicknesses through thickness markings, and because the prefabricated cracks are made of ice, real prefabricated cracks are formed in the rock sample, which is more valuable for studying the crack expansion and penetration mechanism inside the real rock mass;

[0024] 2. The rock sample mold structure of the present invention can fix the ice prefabricated cracks on the positioning bolts at different positions by setting the angle height mark and positioning bolts thereon, and pour similar materials in the mold cavity to produce uniaxial and triaxial specimens with different prefabricated crack angles, different prefabricated crack spacings, and different numbers of prefabricated cracks. The operation is simple, the test efficiency is improved, and the sample preparation time and difficulty are reduced;

[0025] 3. The rock sample mold of the present invention can be made not only into a cylindrical shape but also into a cubic shape, thereby meeting the requirements of true triaxial tests and rock samples of different shapes. BRIEF DESCRIPTION OF THE DRAWINGS

[0026] Figure 1 This is a schematic diagram of the three-dimensional structure of a mold for making a rock-like material containing internal prefabricated cracks according to an embodiment of the present invention;

[0027] Figure 2 This is a schematic diagram of a rock sample mold according to an embodiment of the present invention;

[0028] Figure 3 Schematic diagram of the three-dimensional structure of the bottom mold according to an embodiment of the present invention;

[0029] Figure 4 It is a right side view of the first side mold of the embodiment of the present invention when the baffle is not installed;

[0030] Figure 5 It is a right side view of the first side mold when the baffle is installed in the embodiment of the present invention;

[0031] Figure 6 This is a schematic diagram of the three-dimensional structure of a prefabricated crack mold according to an embodiment of the present invention;

[0032] Figure 7 The prefabricated cracks after the embodiment of the present invention is manufactured;

[0033] Figure 8 A cross-sectional view of installing a prefabricated crack in a rock-like specimen mold according to an embodiment of the present invention;

[0034] Fig. 9 The angle marking production principle of the embodiment of the present invention;

[0035] Fig.10 The manufacturing principle of the height mark of the embodiment of the present invention is shown;

[0036] Fig.11 Schematic diagram of a method for producing a rock-like material containing internal prefabricated cracks according to an embodiment of the present invention.

[0037] In all the drawings, the same figure numbers represent the same technical features, specifically: 1-type rock sample mold, 11-first side mold, 12-second side mold, 13-positioning oblong hole, 14-positioning bolt, 15-angle height mark, 16-fastening belt, 17-first baffle, 18-second baffle, 2-bottom membrane, 21-circular groove, 3-prefabricated crack mold, 31-water holding device, 32-water injection channel, 33-threading platform, 34-fine cotton thread, 35-thickness mark, 36-crack baffle, 37-prefabricated crack. DETAILED DESCRIPTION

[0038] In order to make the purpose, technical solutions and advantages of the present invention more clearly understood, the present invention is further described in detail below in conjunction with the accompanying drawings and embodiments. It should be understood that the specific embodiments described herein are only used to explain the present invention and are not intended to limit the present invention. In addition, the technical features involved in the various embodiments of the present invention described below can be combined with each other as long as they do not conflict with each other.

[0039] It should be noted that if the embodiments of the present invention involve directional indications (such as up, down, left, right, front, back, etc.), the directional indications are only used to explain the relative position relationship, movement status, etc. between the components under a certain specific posture (as shown in the accompanying drawings). If the specific posture changes, the directional indication will also change accordingly.

[0040] In addition, if there are descriptions involving "first", "second", etc. in the embodiments of the present invention, the descriptions of "first", "second", etc. are only used for descriptive purposes and cannot be understood as indicating or suggesting their relative importance or implicitly indicating the number of the indicated technical features. Therefore, the features defined as "first" and "second" may explicitly or implicitly include at least one of the features. In addition, the technical solutions between the various embodiments can be combined with each other, but they must be based on the ability of ordinary technicians in the field to implement them. When the combination of technical solutions is contradictory or cannot be implemented, it should be deemed that such a combination of technical solutions does not exist and is not within the scope of protection required by the present invention.

[0041] In this patent, the terms "include", "comprises" or any other variations thereof are intended to cover non-exclusive inclusion, so that a process, method, article or device including a series of elements includes not only those elements, but also includes other elements not explicitly listed, or also includes elements inherent to such process, method, article or device. In the absence of more restrictions, the elements defined by the sentence "includes..." do not exclude the presence of other identical elements in the process, method, article or device including the elements.

[0042] like Figure 1-8As shown, an embodiment of the present invention provides a mold for making a rock-like material containing internal prefabricated cracks, including a rock-like sample mold 1, a bottom mold 2 and a prefabricated crack mold 3. The rock-like sample mold 1 is installed in the groove of the bottom mold 2 to form a similar material casting cavity. The prefabricated crack mold 3 can be used to make ice prefabricated cracks of different thicknesses. According to the number, angle and spacing of the designed prefabricated cracks, the position of the ice prefabricated cracks on the rock sample mold 1 is adjusted and fixed, and then similar materials are cast to form a rock-like sample containing internal prefabricated cracks, so as to realize the production of uniaxial and triaxial compression test specimens containing different prefabricated crack angles, different prefabricated crack spacings and different numbers of prefabricated cracks, and the purpose of producing real prefabricated cracks is achieved by using the prefabricated crack mold, so it is more valuable to study the internal crack expansion and penetration mechanism of real rock mass.

[0043] like Figure 3 As shown, the bottom mold 2 for making the rock sample is a stainless steel plate with a length of 100 mm, a width of 100 mm, and a thickness of 10 mm. A circular groove 21 with an outer diameter of 60 mm (diameter), an inner diameter of 50 mm (diameter), and a depth of 8 mm is provided in the center of the bottom mold 2 for placing the rock-like sample mold 1.

[0044] like Figure 2 As shown, the rock sample model with prefabricated cracks produced in the embodiment of the present invention is a cylinder with a diameter of 50 mm and a height of 100 mm. The rock sample mold 1 includes a first side mold 11, a second side mold 12, a positioning oblong hole 13, a positioning bolt 14, an angle height mark 15, a fastening belt 16, a first baffle 17, and a second baffle 18. The first side mold 11 and the second side mold 12 are semicircular grooves with a thickness of 10mm and a length of 108mm, and the inner diameter (diameter) of the groove is 50mm. The first side mold 11 and the second side mold 12 can be spliced ​​to form a cylinder with an inner cavity size of 50mm in diameter and 108mm in height. The contact parts are designed with concave and convex parts with a width and height of 5mm respectively to ensure that the splicing is tight and does not leak slurry. After the first side mold 11 and the second side mold 12 are spliced, they are placed in the circular groove 21 in the center of the bottom mold 2, and the top and bottom ends are fastened with the fastening belt 16, so that a cylinder with an inner cavity size of 50mm in diameter and 100mm in height is formed, that is, the shape of a standard cylindrical specimen; the first side mold 11 and the second side mold 12 are provided with the positioning oblong hole 13 with a width of 5mm and a length of 80mm at the center, on which the positioning bolt 14 can be fixed. An angle height mark 15 is provided on the outer side of the positioning oblong hole 13. By setting the angle height mark 15 of the first side mold 11 and the angle height mark 15 of the second side mold 12, and then screwing the positioning bolt 14 into the set angle height mark, the number and angle spacing of the prefabricated cracks can be controlled, thereby forming prefabricated cracks of different numbers, angles and spacings.

[0045] like Figure 6 , 7 As shown, the prefabricated crack mold 3 includes a water holding device 31, a water injection channel 32, a threading platform 33, a fine cotton thread 34, a thickness mark 35, a crack baffle 36 and a prefabricated crack 37;

[0046] The water container 31 is a cylindrical water container with an inner diameter (diameter) of 10 mm, an outer diameter of 12 mm, and a height of 8 mm. Two water injection channels 32 with a width of 2 mm and a length of 15 mm are connected to the two sides. The cylindrical water container 31 and the water injection channel 32 are made of stainless steel with a thickness of 2 mm, and are used to inject water to form a cylindrical prefabricated crack 37. A crack baffle 36 and a threading platform 33 with a diameter of 1 mm and a height of 8 mm are respectively arranged at the intersection of the cylindrical water container 31 and the water injection channel 32. The crack baffle 37 can form a complete cylindrical water container with the cylindrical water container 31. The threading platform 33 is a cylinder with a partial notch, and its main function is to facilitate the fixing of the thin cotton thread 35 so as to realize the formation of the thin cotton thread 35 and the prefabricated crack 37 into a whole. The prefabricated crack 37 is a cylindrical ice flake with a diameter of 10 mm and a height of 5 mm. The thickness mark 36 is provided on the inner wall of the cylindrical water holding device 31. The thickness of the prefabricated crack of the cylindrical ice flake can be adjusted according to the test needs by adjusting the opening of the crack baffle 36 to adjust the water level in the cylindrical water holding device 31, and the thickness required for the test is checked and determined by the thickness mark 36. The specific shape of the prefabricated crack of the cylindrical ice flake can also be adjusted by adjusting the shape of the mold.

[0047] like Figure 8 As shown, by tying the fine cotton thread 34 on the prefabricated crack 37 to the positioning bolts 14 at different positions of the first side mold 11 and the second side mold 12, and then installing the first baffle plate 17 and the second baffle plate 18 on both sides of the positioning oblong holes (13) of the first side plate 11 and the second side plate 12, the side plates are closed, and similar materials are cast in the casting cavity of the mold to produce uniaxial and triaxial rock specimens containing prefabricated cracks of different numbers, angles and spacings. The fine cotton thread 34 can pass through the middle of the first baffle plate 17 and the second baffle plate 18.

[0048] Combination Figure 1-8 ,like Fig.11 As shown, the present invention proposes a method for making a rock material containing internal prefabricated cracks, specifically, using the above mold to prepare uniaxial and triaxial rock samples containing prefabricated cracks of different numbers, angles and spacings. The specific steps are as follows:

[0049] S100: similar materials for preparing rock samples;

[0050] S200: using the prefabricated crack mold to make a prefabricated crack, firstly passing the fine cotton thread through the threading platform, then installing the crack baffle, then injecting water into the center of the prefabricated crack mold, stopping the water injection after the water level reaches the required thickness mark, putting the entire prefabricated crack mold into a refrigerator to freeze, after the freezing is completed, putting the prefabricated crack mold into warm water for a few seconds, taking out the prefabricated crack together with the fine cotton thread to obtain the prefabricated crack, and then putting the prefabricated crack into the refrigerator to freeze for standby use, and the same method can be used to make a variety of prefabricated cracks of different thicknesses for standby use;

[0051] S300: According to the number, angle and spacing of the designed prefabricated cracks, the angle height mark is determined by calculation, and the positioning bolt is screwed into the positioning oblong hole on the first side mold according to the angle mark to fix it, and then another position is selected according to the height mark, and the positioning bolt is screwed into the positioning oblong hole and fixed, and then the fine cotton thread on the prefabricated crack is tied to the positioning bolt, and the first baffle plate and the second baffle plate of the first side mold are immediately installed, and the same operation is performed on the second side mold; while tying the fine cotton thread, the first side mold and the second side mold are slowly spliced ​​along the notch, and the spliced ​​rock-like mold is placed in the circular groove of the base membrane and fastened with a fastening belt to form a casting cavity;

[0052] S400: Similar materials are poured into the cavity, and after vibration, curing and demolding, uniaxial and triaxial rock samples with real prefabricated cracks in different numbers, angles and spacings can be obtained.

[0053] A specific embodiment of the present invention is further disclosed below based on a method for producing a rock material containing internal prefabricated cracks according to the present invention.

[0054] An embodiment 1 of the present invention:

[0055] like Fig. 9 As shown, this embodiment of the present invention provides a method for making a rock material containing internal prefabricated cracks, specifically using the above mold to prepare a rock sample containing a single prefabricated crack with an angle A, and the specific steps include:

[0056] S100: similar materials for preparing rock samples;

[0057] S200: using the prefabricated crack mold to make a prefabricated crack, firstly passing the fine cotton thread through the threading platform, then installing the crack baffle, then injecting water into the center of the prefabricated crack mold, stopping the water injection after the water level reaches the required thickness mark, putting the entire prefabricated crack mold into a refrigerator to freeze, after the freezing is completed, putting the prefabricated crack mold into warm water for a few seconds, taking out the prefabricated crack together with the fine cotton thread, and obtaining the borneol prefabricated crack, and then putting the prefabricated crack into the refrigerator to freeze for standby use, and the same method can be used to make a variety of prefabricated cracks of different thicknesses for standby use;

[0058] S300: firstly, the angle marks on the first side mold and the second side mold are determined according to the angle mark principle. The principle of making the angle mark is: the angle A is the angle between the prefabricated crack and the horizontal X direction. It is known that the inner diameter of the rock sample mold is 50 mm. The center of the mold is used as the dividing line. The distance between the extension lines of the two ends of the prefabricated crack on the first side mold and the second side mold is 50 mm×tanA. Based on this, the angle marks are made on the first side mold and the second side mold.

[0059] In the first side mold, first screw the positioning bolt into the positioning oblong hole according to the angle mark to fix it, then take out the borneol prefabricated crack from the refrigerator, tie the fine cotton thread 34 on the prefabricated crack to the positioning bolt, and immediately install the first baffle and the second baffle of the first side mold; similarly, screw the positioning bolt 14 into the positioning oblong hole on the second side mold according to the angle mark to fix it, then tie the fine cotton thread at the other end of the borneol prefabricated crack to the positioning bolt of the second side mold, immediately install the first baffle and the second baffle of the second side mold 12, and slowly splice the first side mold and the second side mold along the groove while tying the fine cotton thread. During the process, pay attention to ensure that the length of the fine cotton thread on both sides of the prefabricated crack should be consistent, so as to ensure that the prefabricated crack is in the exact center of the rock sample, and then place the spliced ​​first side mold and the second side mold in the circular groove of the bottom mold and tighten the top and bottom ends of the rock sample mold with tightening belts to form a casting cavity containing the prefabricated crack.

[0060] S400: Similar materials are poured into the cavity, and after vibration, curing and demolding, uniaxial and triaxial rock specimens with internal real prefabricated cracks with a single angle A can be obtained.

[0061] Another embodiment 2 of the present invention:

[0062] like Fig.10 As shown, in this embodiment of the present invention, a method for making a rock-like material with internal prefabricated cracks is proposed, specifically, using the above mold to prepare rock-like uniaxial and triaxial specimens with different angles E and F and a distance D between the two, and the specific steps include:

[0063] S100: similar materials for preparing rock samples;

[0064] S200: using the prefabricated crack mold to make a prefabricated crack, firstly passing the fine cotton thread through the threading platform, then installing the crack baffle, then injecting water into the center of the prefabricated crack mold, stopping the water injection after the water level reaches the required thickness mark, putting the entire prefabricated crack mold into a refrigerator to freeze, after the freezing is completed, putting the prefabricated crack mold into warm water for a few seconds, taking out the prefabricated crack together with the fine cotton thread, and obtaining the borneol prefabricated crack, and then putting the prefabricated crack into the refrigerator to freeze for standby use, and the same method can be used to make a variety of prefabricated cracks of different thicknesses for standby use;

[0065] S300: First, determine the angle height marks on the first side mold and the second side mold according to the angle height mark principle. The principle of making the angle height marks is: the angles E and F are the angles between the prefabricated cracks and the horizontal X direction, and the spacing refers to the distance between the centers of the two prefabricated cracks in the vertical direction Y. It is known that the inner diameter of the mold is 50 mm, the spacing between the two prefabricated cracks is D, the two angles are E and F, and E is greater than F, then the spacing between the two on the first side mold and the second side mold is G=D-25*(tanE-tanF). In the first side mold, first screw the positioning bolt into the positioning oblong hole according to the angle mark and fix it. Then, select another position according to the height mark and screw the positioning bolt into the positioning oblong hole and fix it. Then, take out two pieces of ice flakes from the refrigerator and tie the fine cotton threads on the prefabricated cracks respectively. On the positioning bolt, immediately install the first baffle plate and the second baffle plate of the first side mold; similarly, in the second side mold, first screw the positioning bolt into the positioning oblong hole according to the angle mark and fix it, then select another position according to the height mark, screw the positioning bolt into the positioning oblong hole and fix it, tie the fine cotton thread at the other end of the two prefabricated cracks to the positioning bolt of the second side mold, immediately install the first baffle plate and the second baffle plate of the second side mold, and splice the first side mold and the second side mold along the groove while tying the fine cotton thread. During the process, pay attention to ensure that the length of the fine cotton thread on both sides of the prefabricated crack should be consistent, so as to ensure that the prefabricated crack is in the exact center of the rock sample, and then place the spliced ​​first side mold and the second side mold in the circular groove of the bottom mold and tighten the top and bottom ends of the rock-like specimen mold with tightening belts to form a casting cavity containing two prefabricated cracks.

[0066] S300: Pour similar materials into the cavity, and after vibration, curing and demolding, uniaxial and triaxial rock samples with two internal real prefabricated cracks with angles E and F and a spacing of D can be obtained.

[0067] According to some other specific embodiments of the present invention, according to different test requirements, the rock-like sample mold is made into a rectangular parallelepiped shape, so that the obtained rock-like sample is a rectangular parallelepiped of 50mm*50mm*100mm.

[0068] It will be easily understood by those skilled in the art that the above description is only a preferred embodiment of the present invention and is not intended to limit the present invention. Any modifications, equivalent substitutions and improvements made within the spirit and principles of the present invention should be included in the protection scope of the present invention.

Claims

1. A mold for making rock materials with internal prefabricated cracks, It is characterized in that The invention comprises a rock sample mold (1) for making a sample of a similar material, a bottom mold (2) and a prefabricated crack mold (3) for making a prefabricated crack, wherein: The rock sample mold (1) comprises a first side mold (11) and a second side mold (12); a positioning oblong hole (13) is provided at the center of each of the first side mold (11) and the second side mold (12); a positioning bolt (14) is fixed on the positioning oblong hole (13); and an angle height mark (15) is provided on the outside of the positioning oblong hole (13) according to the number, angle and spacing of the designed prefabricated cracks; The prefabricated crack mold (3) comprises a water container (31) and a water injection channel (32), and a threading platform (33) is arranged at the intersection thereof. The threading platform (33) is a cylinder with a notch and is used to fix a fine cotton thread (34). Water is injected into the prefabricated crack mold (3) and then frozen to form a prefabricated crack (37) with the fine cotton thread (34). The fine cotton threads (34) at both ends of the prefabricated crack (37) are tied to the positioning bolts (14) at different positions of the rock-like sample mold (1), and similar materials are poured into the cavity of the rock-like sample mold (1), so that rock-like samples containing prefabricated cracks of different numbers, angles and spacings can be formed.

2. A mold for making a rock material containing internal prefabricated cracks according to claim 1, It is characterized in that The rock sample mold (1) further comprises a first baffle (17) and a second baffle (18) for closing the positioning oblong holes (13) on the first side mold (11) and the second side mold (12) to form a casting cavity with closed sides, and the fine cotton thread (34) passes through the middle of the first baffle (17) and the second baffle (18).

3. A mold for making a rock material containing internal prefabricated cracks according to claim 2, It is characterized in that The rock-like sample mold (1) further comprises fastening belts (16) for fastening the top and bottom ends of the rock-like sample mold (1).

4. A mold for making a rock material containing internal prefabricated cracks according to claim 3, It is characterized in that The contact parts of the first side mold (11) and the second side mold (12) are respectively designed with concave and convex grooves with a width and height of 1mm-5mm to ensure that the joints are tight and leak-proof.

5. A mold for making a rock material containing internal prefabricated cracks according to any one of claims 1 to 4, It is characterized in that The bottom mold (2) comprises a circular groove (21) for placing the first side mold (11) and the second side mold (12) of the rock-like sample mold (1).

6. A mold for making a rock material containing internal prefabricated cracks according to any one of claims 1 to 4, It is characterized in that The prefabricated crack mold (3) also includes a thickness mark (35) provided on the inner side wall of the water container (31) for determining the thickness of the prefabricated crack.

7. A mold for making a rock material containing internal prefabricated cracks according to claim 6, It is characterized in that The prefabricated crack mold (3) also includes a crack baffle (36) for adjusting the water level in the water containing device (31) by adjusting the opening of the crack baffle (36) according to test requirements.

8. A mold for making a rock material containing internal prefabricated cracks according to any one of claims 1 to 4, It is characterized in that The rock sample mold (1) can be cylindrical or rectangular, or can be adjusted to a desired shape according to the test.

9. A mold for making a rock material containing internal prefabricated cracks according to any one of claims 1 to 4, It is characterized in that The shape of the prefabricated crack mold (3) is adjusted according to test requirements and matches the rock-like sample mold (1).

10. A method for producing cracks in a rock material containing internal prefabricated cracks, which is achieved by using a mold for producing a rock material containing internal prefabricated cracks as claimed in any one of claims 1 to 9. It is characterized in that The steps include: S100: similar materials for preparing rock samples; S200: using the prefabricated crack mold to make a prefabricated crack, firstly passing the fine cotton thread through the threading platform, then installing the crack baffle, then injecting water into the center of the prefabricated crack mold, stopping the water injection after the water level reaches the required thickness mark, putting the entire prefabricated crack mold into a refrigerator to freeze, after the freezing is completed, putting the prefabricated crack mold into warm water for a few seconds, taking out the prefabricated crack together with the fine cotton thread to obtain the prefabricated crack, and then putting the prefabricated crack into the refrigerator to freeze for standby use, and the same method can be used to make a variety of prefabricated cracks of different thicknesses for standby use; S300: According to the number, angle and spacing of the designed prefabricated cracks, the angle height mark is determined by calculation, and the positioning bolt is screwed into the positioning oblong hole on the first side mold according to the angle mark for fixing, and then the positioning bolt is screwed into the positioning oblong hole after selecting another position according to the height mark and fixed, and then the fine cotton thread on the prefabricated crack is tied to the positioning bolt, and the first baffle plate and the second baffle plate of the first side mold are immediately installed, and the same operation is performed on the second side mold; While tying a thin cotton thread, slowly splice the first side mold and the second side mold along the notch, place the spliced ​​rock-like mold in the circular groove of the base film and fasten it with a fastening belt to form a casting cavity; S400: Similar materials are poured into the cavity, and after vibration, curing and demolding, uniaxial and triaxial rock samples with real prefabricated cracks in different numbers, angles and spacings can be obtained.

Citation Information

Patent Citations

  • True-triaxial rock sample crack prefabricating device

    CN103776673A

  • Making method of internal precrack of rock specimen

    CN106769340A

  • Adjustable rock-like material crack prefabricating device

    CN113532995A

  • Application of natural silica material in preparation of transparent rock and transparent rock body

    CN104502180A

  • Standard rock sample prefabricated crack making device and making method thereof

    CN110376039A