CO2 absorption-mineralization integrated process based on mixed amine solution
By using PZ/AMP mixed amine solution to optimize CO2 absorption-mineralization reaction, the problem that a single amine solvent cannot be compatible with high efficiency absorption rate and large capacity is solved, and efficient CO2 absorption and mineralization is achieved, and the obtained products have good industrial applications. prospect.
Patent Information
- Application Number
- CN202411241862.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-05
- Publication Date
- 2024-11-22
AI Technical Summary
In the prior art, single amine solvents cannot be compatible with fast CO2 absorption rate, large CO2 absorption capacity and good cycling performance at the same time, limiting the efficiency of CO2 absorption-mineralization reaction and industrial applications.
Using PZ/AMP mixed amine solution as the core absorber of CO2 absorption-mineralization process, the CO2 absorption performance and mineralization degree are optimized by regulating the ratio of PZ and AMP, and efficient CO2 absorption and mineralization reaction are achieved, and cycle experiments are carried out. Verify its stability.
High CO2 absorption load, high mineralization rate and good circulation performance were achieved. The resulting calcium carbonate product is a uniform calcite crystal form, with good industrial application prospects, and remains efficient after at least five cycles.
Smart Images

Figure CN118987899A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to a CO2 absorption-mineralization integrated process based on a mixed amine solution, and belongs to the field of CO2 capture and conversion. Background Art
[0002] Greenhouse gas emissions caused by human activities have led to a rapid rise in the global average temperature. Climate warming has become one of the most pressing issues facing the world today. CO2 released during the combustion of traditional fossil fuels is the main cause of global warming. Therefore, capturing and utilizing CO2 to reduce the concentration of CO2 in the atmosphere is a key technical means to mitigate the greenhouse effect.
[0003] In recent years, researchers have proposed the integrated CO2 absorption-mineralization technology (IAM), which combines CO2 mineralization with CO2 absorption by amine solution, and uses amine solution as an intermediate to capture CO2. This technology not only accelerates the absorption rate of CO2, but also reduces the temperature requirement for amine solution regeneration, thereby further promoting the mineralization reaction. However, most studies currently use a single amine solvent for CO2 absorption-mineralization, and a single amine solvent cannot simultaneously be compatible with the advantages of fast CO2 absorption rate, large CO2 absorption capacity, and good cycle performance. Mixed amine solvents can optimize the reaction rate and increase the solvent CO2 absorption load on the basis of a single amine solvent, thereby showing better mineralization performance. Studies have found that the AMP-modified mixed alcohol amine system has excellent CO2 absorption performance; PZ, AMP, and ethanolamine are respectively used to form mixed amine solutions for CO2 absorption experiments, and their CO2 absorption load and absorption rate are better than those of the above-mentioned amine solvents used alone; compared with ethanolamine, AMP-based mixed amine solutions have lower capital expenditures and operating costs, lower regeneration energy, and higher absorption rates, cycle loads, and cycle capacities. It can be seen that the capture of CO2 by mixed amine solvents has been proven to have many advantages.
[0004] At present, the research uses ethanolamine / N-methyldiethanolamine mixed solvent for CO2 absorption-mineralization, which has better CO2 absorption rate and mineralization performance than using ethanolamine and N-methyldiethanolamine alone. However, the research work in this field is still at the stage of research based on ethanolamine mixed amine solvent. It is expected to accelerate the reaction process by selecting amine solutions with better CO2 absorption performance than ethanolamine for mixing for CO2 absorption-mineralization. Therefore, it is necessary to study the use of different types of mixed amine solvents for mineralization. PZ / AMP mixed amine solvent has been proven to be able to expand CO2 absorption load and increase CO2 absorption rate. Combining this mixed amine solvent with mineralization is expected to accelerate the mineralization reaction. Summary of the invention
[0005] The present invention aims to provide an integrated CO2 absorption-mineralization process based on a mixed amine solution, which uses a specially screened and proportioned mixed amine solution as a core absorbent for a mineralization process, and the mixed amine solution has excellent CO2 absorption capacity, and its mineralization efficiency is better than other mixed amine solvents reported in the prior art. In addition, the solution exhibits excellent cyclic stability, and can still maintain efficient CO2 absorption and mineralization capacity after at least five cycles of use. The obtained calcium carbonate product has a uniform calcite crystal form, which can be used as a high-value-added industrial raw material and has good industrial application prospects.
[0006] PZ / AMP mixed amine solution was used as CO2 absorption solvent, CaO was used as mineralization raw material, and CO2 was intermittently introduced into a closed reactor stirring device for mineralization reaction. By adjusting the ratio of PZ and AMP, the CO2 absorption performance and mineralization degree of the mixed amine solution under different ratio conditions were studied, and a certain ratio of mixed amine solution was selected for the circulation experiment.
[0007] The above experimental method comprises the following steps:
[0008] (1) adding piperazine PZ and 2-amino-2-methyl-1-propanol AMP into deionized water, stirring until fully mixed, to prepare a mixed amine solution;
[0009] (2) CaO and the mixed amine solution of step (1) are mixed, and then the mixed solution is added to the inner lining of a reactor and placed in the reactor. Under closed conditions, stirring is started and the temperature is increased. Then CO2 gas is introduced to stabilize the CO2 partial pressure in the reactor, and timing is started at the same time. After the reaction is completed, heating is stopped, and the slurry is separated into solid and liquid by vacuum filtration, and the solid is vacuum dried to obtain CaCO3.
[0010] (3) The filtrate obtained in step (2) is further added with CaO for the next CO2 absorption-mineralization experiment, thereby carrying out a cycle experiment with the same experimental steps and conditions as step (2).
[0011] In the mixed amine solution of step (1), the concentration of PZ is 0.5-2 mol / L, and the concentration of AMP is 0.5-2 mol / L.
[0012] In step (1), the stirring condition is 20-25°C.
[0013] In the mixed solution of step (2), the weight percentage of CaO is 5-10wt%;
[0014] In step (2), the reactor is heated to 40-55°C, the stirring rate is 300-500 rpm, the CO2 gas partial pressure is 0.08-0.12 MPa, and the reaction time is 90-120 minutes;
[0015] In step (2), the vacuum drying temperature is 80-90° C. and the drying time is 10-15 hours.
[0016] In the step (3), after the filtrate and CaO are mixed, the weight percentage of CaO is 5-10wt%.
[0017] The present invention uses a mixed amine solution of PZ and AMP as a CO2 absorption solvent for a CO2 absorption-mineralization integrated process, achieves a high CO2 absorption load, a high mineralization rate and good cycle performance, and the obtained solid product is calcite-type calcium carbonate.
[0018] Compared with the prior art, the present invention has the following beneficial effects:
[0019] (1) The synergistic effect between PZ and AMP makes the solution have a higher liquid phase mass transfer coefficient, thereby increasing the CO2 absorption rate and absorption load, accelerating the mineralization reaction and improving the mineralization rate. The 1.5MPZ / 0.5MAMP mixed amine solution has the highest CO2 load and mineralization rate, where the CO2 load is 1.3 mol (CO2) / mol (amine) and the mineralization rate is 95.32%;
[0020] (2) When the mixed amine solution used in the present invention is used for the CO2 absorption-mineralization cycle reaction, the solution has good regeneration performance and still maintains a mineralization rate of 94% after 5 cycles of reaction. The obtained calcium carbonate product has a uniform calcite crystal form and can be used as a high-value-added industrial raw material with good industrial application prospects. BRIEF DESCRIPTION OF THE DRAWINGS
[0021] Figure 1 The mineralization rate change curves during the reaction of Comparative Example 1, Comparative Example 2 and Example 1;
[0022] Figure 2 The CO2 load variation curves during the reaction of Comparative Example 1, Comparative Example 2 and Example 1;
[0023] Figure 3 This is a graph showing changes in mineralization rate and CO2 load after 5 cycles of experiment in Example 1;
[0024] Figure 4 This is the XRD diagram of the solid calcium carbonate obtained after the reaction in Example 1. DETAILED DESCRIPTION
[0025] The technical solutions in the embodiments of the present invention will be fully described below in conjunction with the embodiments of the present invention. Unless otherwise specified, all technical and scientific terms used herein have the same meanings as those commonly understood by those skilled in the art in the field of the present invention. The described embodiments are only a part of the embodiments of the present invention, rather than all of the embodiments. Based on the embodiments in the present invention, all other embodiments obtained by ordinary technicians in the field without creative work belong to the scope of protection of the present invention.
[0026] Example 1
[0027] A CO2 absorption-mineralization integrated process based on mixed amine solution, the experimental process is as follows:
[0028] Step (1), add PZ and AMP into a beaker, then add deionized water, and stir at 20° C. until dissolved to obtain a 1.5M PZ / 0.5M AMP mixed amine solution;
[0029] Step (2), add 10wt% of CaO and the mixed amine solution prepared in step (1) to the lining of the reactor and then put it into the stirred reactor, then start stirring, set the stirring rate to 300rpm, and set the reaction temperature to 40°C. When the reactor is heated to 40°C, CO2 gas is introduced to stabilize the CO2 partial pressure at 0.1MPa, and the timing is started at the same time, and the reaction time is 120 minutes. Samples are taken from the slurry at 5 minutes, 15 minutes, 35 minutes, 60 minutes, 90 minutes, and 120 minutes of reaction, and 10mL is collected each time. The collected samples are separated into solid and liquid by vacuum filtration, and the solid is vacuum dried at 80°C for 12 hours and then ground.
[0030] Step (3), add 5wt% CaO and the filtrate obtained in step (2) to the lining of the reactor and then put it into the stirred reactor for the next CO2 absorption-mineralization experiment. The experimental steps are the same as step (2), and this cycle is repeated 5 times.
[0031] The mixed amine solution prepared by the present invention was used to carry out a CO2 absorption-mineralization integration test, with a total CO2 load of 1.3 mol / mol and a mineralization rate of 95.32%. After 5 cycles of reaction, the mineralization rate was still maintained at 94%.
[0032] Example 2
[0033] A CO2 absorption-mineralization integrated process based on mixed amine solution, the experimental process is as follows:
[0034] Step (1), add PZ and AMP into a beaker, then add deionized water, and stir at 20° C. until dissolved to obtain a 1M PZ / 1M AMP mixed amine solution;
[0035] Step (2), adding 10wt% of CaO to the lining of the reactor together with the mixed amine solution prepared in step (1) and placing it in a stirred reactor, then starting stirring, setting the stirring rate to 300rpm, and setting the reaction temperature to 40°C. When the reactor is heated to 40°C, CO2 gas is introduced to stabilize the CO2 partial pressure at 0.1MPa, and the timing is started at the same time, and the reaction time is 120 minutes. The slurry is sampled at 5 minutes, 15 minutes, 35 minutes, 60 minutes, 90 minutes, and 120 minutes of reaction, and 10mL is collected each time. The collected samples are separated from the solid by vacuum filtration, and the solid is ground into powder after vacuum drying at 80°C for 12 hours. The mixed amine solution prepared by the present invention is used to carry out a CO2 absorption-mineralization integrated test, and the total CO2 load is 0.87mol / mol and the mineralization rate is 87.22%.
[0036] Example 3
[0037] A CO2 absorption-mineralization integrated process based on mixed amine solution, the experimental process is as follows:
[0038] Step (1), add PZ and AMP into a beaker, then add deionized water, and stir at 20° C. until dissolved to obtain a 0.5 M PZ / 1.5 M AMP mixed amine solution;
[0039] Step (2), add 10wt% of CaO together with the mixed amine solution prepared in step (1) to the lining of the reactor and then place it in a stirred reactor, then start stirring, set the stirring rate to 300rpm, and set the reaction temperature to 40°C. When the reactor is heated to 40°C, introduce CO2 gas to stabilize the CO2 partial pressure at 0.1MPa, and start timing at the same time. The reaction time is 120 minutes. Samples are taken from the slurry at 5 minutes, 15 minutes, 35 minutes, 60 minutes, 90 minutes, and 120 minutes of reaction, and 10mL is collected each time. The collected samples are separated from the solid and the liquid by vacuum filtration, and the solids are ground into powder after vacuum drying at 80°C for 12 hours. The mixed amine solution prepared by the present invention is used to carry out a CO2 absorption-mineralization integrated test, and the total CO2 load is 1.18mol / mol, and the mineralization rate is 95%;
[0040] Example 4
[0041] The difference from Example 1 is that the stirring rate is set to 500 rpm.
[0042] The mixed amine solution prepared by the present invention was used to carry out a CO2 absorption-mineralization integration test, and the total CO2 load was 0.53 mol / mol and the mineralization rate was 55%.
[0043] Example 5
[0044] The difference from Example 1 is that the weight percentage of CaO is 5wt%.
[0045] The mixed amine solution prepared by the present invention was used to carry out a CO2 absorption-mineralization integration test, with a total CO2 load of 0.55 mol / mol and a mineralization rate of 97.3%.
[0046] Comparative Example 1
[0047] The difference from the embodiment is that:
[0048] Step (1), add PZ to a beaker, then add deionized water, and stir at 20°C until the PZ solution with a concentration of 2M is dissolved;
[0049] Step (2), adding 10wt% of CaO to the liner of the reactor together with the amine solution prepared in step (1) and placing it in a stirred reactor, then starting stirring, the stirring rate is set to 300rpm, and the reaction temperature is set to 40°C. When the reactor is heated to 40°C, CO2 gas is introduced to stabilize the CO2 partial pressure at 0.1Mpa, and the timing is started at the same time, and the reaction time is 120 minutes. The slurry is sampled at 5 minutes, 15 minutes, 35 minutes, 60 minutes, 90 minutes, and 120 minutes of reaction, and 10mL is collected each time. The collected samples are separated from the solid by vacuum filtration, and the solid is ground into powder after vacuum drying at 80°C for 12 hours. The amine solution prepared by the present invention is used to carry out CO2 absorption-mineralization integrated test, and the total CO2 load is 0.77mol / mol, and the mineralization rate is 67.58%.
[0050] Comparative Example 2
[0051] The difference from the embodiment is that:
[0052] Step (1), add AMP to a beaker, then add deionized water, and stir at 20° C. until dissolved to obtain a 2M AMP solution;
[0053] Step (2), adding 10wt% of CaO to the liner of the reactor together with the amine solution prepared in step (1) and placing it in a stirred reactor, then starting stirring, setting the stirring rate to 300rpm, and setting the reaction temperature to 40°C. When the reactor is heated to 40°C, CO2 gas is introduced to stabilize the CO2 partial pressure at 0.1MPa, and the timing is started at the same time, and the reaction time is 120 minutes. The slurry is sampled at 5 minutes, 15 minutes, 35 minutes, 60 minutes, 90 minutes, and 120 minutes of reaction, and 10mL is collected each time. The collected samples are separated from the solid by vacuum filtration, and the solid is ground into powder after vacuum drying at 80°C for 12 hours. The mixed amine solution prepared by the present invention is used to carry out a CO2 absorption-mineralization integrated test, and the total CO2 load is 1.18mol / mol, and the mineralization rate is 87.03%.
[0054] Experimental results: Example 1 is the best experimental solution.
[0055] Figure 1 It shows that after 120 minutes of reaction, the mineralization rate of Example 1 is higher than that of Comparative Example 1 and Comparative Example 2. The mineralization rate of Example 1 is 95.32%, while that of Comparative Example 1 and Comparative Example 2 is 67.58% and 87.03%, respectively.
[0056] Figure 2 It shows that after 120 minutes of reaction, the CO2 loading of Example 1 is higher than that of Comparative Example 1 and Comparative Example 2. The CO2 loading of Example 1 is 1.3 mol (CO2) / mol (amine), while that of Comparative Example 1 and Comparative Example 2 are 0.77 mol (CO2) / mol (amine) and 1.18 mol (CO2) / mol (amine), respectively.
[0057] Figure 3 It shows that Example 1 has excellent cycle performance.
[0058] Figure 4 The XRD pattern of the solid calcium carbonate obtained by reacting for 120 minutes in Example 1 is shown, from which it can be seen that the obtained calcium carbonate is a calcite crystal type.
Claims
1. A CO2 absorption-mineralization integrated process based on mixed amine solution, characterized in that: The following steps are involved: (1) adding piperazine PZ and 2-amino-2-methyl-1-propanol AMP into deionized water, stirring until fully mixed, to prepare a mixed amine solution; (2) CaO and the mixed amine solution of step (1) are mixed, and then the mixed solution is added to the inner lining of a reactor and placed in the reactor. Under closed conditions, stirring is started and the temperature is increased. Then CO2 gas is introduced to stabilize the CO2 partial pressure in the reactor, and timing is started at the same time. After the reaction is completed, heating is stopped, and the slurry is separated into solid and liquid by vacuum filtration, and the solid is vacuum dried to obtain CaCO3; (3) The filtrate obtained in step (2) is further added with CaO for the next CO2 absorption-mineralization experiment, thereby carrying out a cycle experiment with the same experimental steps and conditions as step (2).
2. The CO2 absorption-mineralization integrated process based on mixed amine solution according to claim 1, characterized in that: In the mixed amine solution of step (1), the concentration of PZ is 0.5-2 mol / L, and the concentration of AMP is 0.5-2 mol / L.
3. The CO2 absorption-mineralization integrated process based on mixed amine solution according to claim 1, characterized in that: In step (1), the stirring condition is 20-25°C.
4. The CO2 absorption-mineralization integrated process based on mixed amine solution according to claim 1, characterized in that: In the mixed solution of step (2), the weight percentage of CaO is 5-10wt%.
5. The CO2 absorption-mineralization integrated process based on mixed amine solution according to claim 1, characterized in that: In step (2), the reactor is heated to 40-55°C, the stirring rate is 300-500 rpm, the CO2 gas partial pressure is 0.08-0.12 MPa, and the reaction time is 90-120 minutes.
6. The CO2 absorption-mineralization integrated process based on mixed amine solution according to claim 1, characterized in that: In step (2), the vacuum drying temperature is 80-90° C. and the drying time is 10-15 hours.
7. The CO2 absorption-mineralization integrated process based on mixed amine solution according to claim 1, characterized in that: In step (3), after the filtrate and CaO are mixed, the weight percentage of CaO is 5-10wt%.
Citation Information
Cited By
System and method for preparing negative carbon product through cooperation of carbon dioxide capture and solid waste mineralization
CN122141409A