Efficient and environment-friendly method for removing arsenic hydride in copper electrodeposition cell surface waste gas
By using copper sulfate solution in the spray tower to treat hydrogen arsenide in the exhaust gas on the copper electrostatic tank surface, the problem of poor arsenide treatment effect in the prior art was solved, and efficient and environmentally friendly hydrogen arsenide removal was achieved and resource recycling reduces wastewater treatment costs.
Patent Information
- Application Number
- CN202411345219.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-26
- Publication Date
- 2024-11-22
- Estimated Expiration
- 2044-09-26
AI Technical Summary
The prior art has poor effect when treating hydrogen arsenide gas in the exhaust gas on the copper electrostatic tank surface, resulting in excess of the concentration of hydrogen arsenide around the factory, affecting the health of employees, and the treatment method is high and the operation is complicated.
Spray and wash using copper sulfate solution in the spray tower, convert hydrogen arsenide into insoluble compounds through chemical reactions, absorb hydrogen arsenide gas, and reduce the amount of alkaline absorbents by recycling waste electrolyte and sulfuric acid. , reduce the production of high-salt wastewater.
It significantly reduces the amount of alkaline absorbent used, achieves efficient removal of hydrogen arsenide, reduces the pressure and cost of wastewater treatment, and is simple and easy to use in industrial applications.
Smart Images

Figure CN118987941A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of waste gas treatment, and in particular to a method for removing arsenic from waste gas on the surface of a copper electrowinning cell, which is suitable for waste gas treatment containing arsenic. Background Art
[0002] Copper electrolytic refining is a process in which anode copper is continuously dissolved and cathode copper is continuously precipitated. However, as the anode dissolves, other non-copper chemical components in the anode will also dissolve into the electrolyte along with the copper element, but not all elements will precipitate on the cathode. The concentration of some copper ions and some impurities such as arsenic, antimony, and bismuth with a similar potential to copper in the electrolyte continues to increase. Therefore, in order to maintain the concentration of copper and impurities in the electrolyte, it is necessary to start the liquid purification system to reduce the concentration of copper and other impurities in the electrolyte to within the control range of qualified process parameters.
[0003] The main method for removing impurities from clean liquid currently used is the induced arsenic removal method. Induced arsenic removal is to cyclically circulate the electrolyte through the electrolytic cell for the copper removal process, and the copper ions in the electrolyte are precipitated on the cathode. As the concentration of copper ions decreases, the arsenic ions decrease faster, but when the copper ions are reduced to 2g / L, in addition to the precipitation of copper and arsenic, the cathode is also accompanied by the generation of highly toxic arsenic (AsH3) gas, which involves the safety of on-site workers. The current method for treating this gas is to pump the arsenic gas generated on the surface of the copper electrolytic cell to a spray tower, use alkaline solution as the spray liquid, and circulate it in the spray tower through a pump for spraying and washing, thereby achieving gas absorption and treatment. This method is not effective in treating AsH3 gas. The gas discharged after treatment still contains a certain amount of AsH3. The density of AsH3 gas is greater than that of air, and it is easy to deposit around the factory. When using professional equipment to detect around the production operation area, AsH3 exceeds the standard, affecting the health of employees. Therefore, it is necessary to find a method for removing AsH3 from the waste gas on the surface of copper electrowinning cells which is simple in process, easy to operate and low in cost. Summary of the invention
[0004] The invention discloses a method for removing arsenic hydrogen from waste gas on the surface of a copper electrowinning cell with high efficiency and environmental protection, so as to solve any of the above and other potential problems in the prior art.
[0005] In order to solve the above problems, the technical solution of the present invention is: a method for removing arsine from the waste gas on the surface of copper electrowinning tank in an efficient and environmentally friendly manner. Arsenic has a large solubility in copper sulfate solution and easily reacts chemically with copper sulfate and sulfuric acid to form insoluble compounds. The reaction equation is: 2AsH3+3CuSO4=Cu3As2+3H2SO4, thereby achieving the effect of absorbing arsine gas. By utilizing the existing waste gas treatment process equipment, the addition structure of the spray reagent in the existing waste gas treatment process is improved, the amount of reagent added is reduced, the generation of secondary pollutants is reduced, and the arsine in the flue gas is recycled and utilized as a resource. This method is simple to operate, easy to industrialize, environmentally friendly, and has important economic, environmental and social benefits.
[0006] A method for efficiently and environmentally friendly removing arsenic in waste gas from copper electrowinning tank surface, specifically comprising the following steps:
[0007] S1: Mix waste electrolyte, sulfuric acid and water in a certain proportion to obtain a flue gas spray liquid, pump the flue gas spray liquid into a spray tower, spray and wash the waste gas on the copper electrowinning tank surface, and obtain a flue gas spray mixed solution;
[0008] S2: sending the flue gas spray mixed solution into a clarification tank for natural sedimentation to obtain a supernatant and bottom sludge;
[0009] S3: sending the supernatant obtained in step S2 to a clean water tank, adding a certain amount of waste electrolyte, sulfuric acid and water to the clean water tank, and then pumping it into a spray tower for recycling;
[0010] S4: The bottom mud obtained in step S2 is pumped into the filter press, the filtrate is returned to the clarification tank for clarification, and the filter cake is sent to the copper arsenide refining process.
[0011] Preferably, the Cu in the flue gas spray liquid in S1 2+ The concentration is 20-40g / L, the acidity is 120-180g / L, and the liquid-gas ratio is 2-6L / m 3 .
[0012] Preferably, the content of hydrogen arsenide in the flue gas after spraying is ≤0.3 mg / m 3 .
[0013] Preferably, the waste gas from the copper electrowinning tank surface in S1 stays in the spray tower for 1-3 seconds.
[0014] Preferably, the number of sections for spraying waste gas on the copper electrowinning tank surface in S1 is one section, two sections or more sections.
[0015] Preferably, the natural sedimentation time in S2 is 6-12h.
[0016] The beneficial effects of the present invention are:
[0017] 1. The method of the present invention can significantly reduce the addition of alkaline absorbent and reduce the generation of high-salt wastewater in the waste gas treatment process;
[0018] 2. By introducing waste electrolyte to replace the existing alkaline absorbent, arsenic hydrogen is separated from the system in the form of copper arsenide precipitation, and arsenic hydrogen is converted into copper arsenide for resource recovery. At the same time, the spray waste liquid can be recycled after simple sedimentation and addition of waste electrolyte, which reduces the pressure and cost of wastewater treatment;
[0019] 3. The process is simple and reliable, easy to industrialize, and has important economic and social benefits. BRIEF DESCRIPTION OF THE DRAWINGS
[0020] Figure 1 The present invention is a process flow chart of a method for efficiently and environmentally removing arsenic hydrogen from waste gas on the surface of a copper electrowinning cell. DETAILED DESCRIPTION
[0021] The following will be combined with the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. All equal changes and improvements made within the scope of the application of the present invention should still fall within the scope of the patent coverage of the present invention.
[0022] Example 1
[0023] The spent electrolyte A (Cu 2+ The concentration is 43.79g / L, the acidity is 162.58g / L), sulfuric acid and a certain amount of water to prepare Cu 2+ The flue gas spray liquid with a concentration of 20g / L and an acidity of 120g / L is pumped into the spray tower to spray the flue gas, and the liquid-gas ratio is 2L / m 3 , and obtain a flue gas spray mixed solution. Among them, the waste gas from the copper electrowinning tank surface stays in the spray tower for 2s, and the flue gas is treated by a two-stage spraying method. The flue gas washing mixed solution is introduced into the clarification tank for natural sedimentation. After natural sedimentation for 6 hours, the supernatant flows into the clear water tank by gravity. A certain amount of waste electrolyte, sulfuric acid and water are added to the clear water tank and then pumped into the spray tower for recycling. The lower sludge is pumped to the filter press, the filtrate is returned to the clarification tank for clarification, and the filter cake is sent to the copper arsenide refining process.
[0024] The concentration of arsenic in the initial exhaust gas is 0.892 mg / m 3 After the method of removing arsenic hydrogen from the waste gas on the surface of the copper electrowinning tank is adopted, the concentration of arsenic hydrogen gas is 0.188 mg / m 3 The removal rate was 78.92%.
[0025] Example 2
[0026] The spent electrolyte B (Cu 2+ The concentration is 45.24g / L, the acidity is 184.74g / L), sulfuric acid and a certain amount of water to prepare Cu 2+ The flue gas spray liquid with a concentration of 40g / L and an acidity of 180g / L is pumped into the spray tower to spray the flue gas, and the liquid-gas ratio is 6L / m 3 , and obtain a flue gas spray mixed solution. Among them, the waste gas from the copper electrowinning tank surface stays in the spray tower for 3s, and the flue gas is treated by a one-stage spraying method. The flue gas washing mixed solution is introduced into the clarification tank for natural sedimentation. After natural sedimentation for 9 hours, the supernatant flows into the clear water tank by gravity. A certain amount of waste electrolyte, sulfuric acid and water are added to the clear water tank and then pumped into the spray tower for recycling. The lower sludge is pumped to the filter press, the filtrate is returned to the clarification tank for clarification, and the filter cake is sent to the copper arsenide refining process.
[0027] The concentration of arsenic in the initial exhaust gas is 0.787 mg / m 3 After the method of removing arsenic hydrogen from the waste gas on the surface of the copper electrowinning tank is adopted, the concentration of arsenic hydrogen gas is 0.162 mg / m 3 The removal rate was 79.42%.
[0028] Example 3
[0029] The spent electrolyte C (Cu 2+ The concentration is 47.59g / L, the acidity is 196.57g / L), sulfuric acid and a certain amount of water to prepare Cu 2+ The flue gas spray liquid with a concentration of 30g / L and an acidity of 150g / L is pumped into the spray tower to spray the flue gas, and the liquid-to-gas ratio is 4L / m 3 , and obtain a flue gas spray mixed solution. Among them, the waste gas from the copper electrowinning tank surface stays in the spray tower for 1s, and the flue gas is treated by three-stage spraying. The flue gas washing mixed solution is introduced into the clarification tank for natural sedimentation. After natural sedimentation for 12 hours, the supernatant flows into the clear water tank by gravity. A certain amount of waste electrolyte, sulfuric acid and water are added to the clear water tank and then pumped into the spray tower for recycling. The lower sludge is pumped to the filter press, the filtrate is returned to the clarification tank for clarification, and the filter cake is sent to the copper arsenide refining process.
[0030] The concentration of arsenic in the initial exhaust gas is 0.722 mg / m 3 After the method of removing arsenic hydrogen from the waste gas on the surface of the copper electrowinning tank is adopted, the concentration of arsenic hydrogen gas is 0.148 mg / m 3 , the removal rate was 79.50%.
[0031] Finally, it should be noted that the above is only a preferred embodiment of the present invention and is not intended to limit the present invention. Although the present invention has been described in detail with reference to the aforementioned embodiments, it is still possible for those skilled in the art to modify the technical solutions described in the aforementioned embodiments or to make equivalent substitutions for some of the technical features therein. Any modifications, equivalent substitutions, improvements, etc. made within the spirit and principles of the present invention should be included in the protection scope of the present invention.
Claims
1. A highly efficient and environmentally friendly method for removing arsenic in waste gas from copper electrowinning tanks, characterized in that: The specific steps include: S1: Mix waste electrolyte, sulfuric acid and water in a certain proportion to obtain a flue gas spray liquid, pump the flue gas spray liquid into a spray tower, spray and wash the waste gas on the copper electrodeposition tank surface, and obtain a flue gas spray mixed solution; S2: sending the flue gas spray mixed solution into a clarification tank for natural sedimentation to obtain a supernatant and bottom sludge; S3: sending the supernatant obtained in step S2 to a clean water tank, adding a certain amount of waste electrolyte, sulfuric acid and water to the clean water tank, and then pumping it into a spray tower for recycling; S4: The bottom mud obtained in step S2 is pumped into the filter press, the filtrate is returned to the clarification tank for clarification, and the filter cake is sent to the copper arsenide refining process.
2. The method for removing arsenic in waste gas from copper electrowinning cell surface in an efficient and environmentally friendly manner according to claim 1, characterized in that: The Cu in the flue gas spray liquid in S1 2+ The concentration is 20-40g / L, the acidity is 120-180g / L, and the liquid-gas ratio is 2-6L / m 3 .
3. The method for removing arsenic in waste gas from copper electrowinning cell surface in an efficient and environmentally friendly manner according to claim 1, characterized in that: Arsenic content in flue gas after spraying ≤ 0.3 mg / m 3 .
4. The method for removing arsenic in waste gas from copper electrowinning cell surface in an efficient and environmentally friendly manner according to claim 1, characterized in that: The time that the waste gas from the copper electrowinning tank surface in S1 stays in the spray tower is 1-3 seconds.
5. The method for removing arsenic in waste gas from copper electrowinning cell surface in an efficient and environmentally friendly manner according to claim 1, characterized in that: The number of sections for spraying waste gas on the copper electrowinning tank surface in S1 is one section, two sections or more sections.
6. The method for removing arsenic in waste gas from copper electrowinning cell surface in an efficient and environmentally friendly manner according to claim 1, characterized in that: The natural sedimentation time in the S2 is 6-12h.
Citation Information
Patent Citations
Continuous preparation method of refining electrolytic solution for copper electrolysis
CN106011930A
Dry-type purifying method of smelting flue gas containing arsenic and SO3
CN110280125A
Method and device for efficiently absorbing and reducing selenium by sulfurization roasting of copper anode slime
CN112093781A
System and method for boiler flue gas desulfurization and carbon dioxide resource utilization
CN116099342A
Method for sulfating and roasting copper anode slime and extracting selenium and tellurium
CN118343685A