Potassium ferrate complex liquid as well as preparation method and application thereof
Through the hydrothermal reaction between potassium ferrate composite liquid and nitrogen-rich biomass, the stubborn structure of cellulose is destroyed, the humus content is improved, the problem of low humus content of cellulose waste biomass is solved, and resource utilization and environmental protection are achieved The effect of "using waste to control waste" is
Patent Information
- Application Number
- CN202411159350.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-22
- Publication Date
- 2024-11-22
AI Technical Summary
The humus content of products obtained from direct hydrothermal cellulose waste biomass is not high, resulting in low resource utilization efficiency.
Potassium ferrate composite solution is used for pretreatment, combined with nitrogen-rich biomass such as residual sludge, hydrothermal enhancement of humification reaction, destroying the stubborn structure of cellulose and improving humus content.
It increases the humus content of cellulose waste biomass, reduces operating costs, and realizes "use waste to control waste", without the need for additional chemical reagents, and is convenient for promotion and application.
Smart Images

Figure CN118993156A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to a potassium ferrate composite liquid, a preparation method and application thereof, and belongs to the technical field of solid waste resource utilization. Background Art
[0002] Cellulosic waste biomass has the characteristics of huge output and wide sources, including agricultural and forest residues, paper, wood, etc. It can be added value to liquid fuels and other carbon-based materials, and has great utilization potential. However, the natural complex and stubborn structure and high crystallinity of lignocellulose hinder the effective utilization of cellulose waste biomass. Therefore, pretreatment is required to destroy such stubborn structures and realize the resource utilization of cellulose waste biomass. Pretreatment technologies mainly include physical, chemical, and biological methods. Among them, chemical methods have attracted much attention in practical applications due to their convenient operation and low cost. Chemical methods refer to the use of chemical reagents such as acids, alkalis and oxidants to pretreat lignocellulose. Therefore, chemical methods require additional chemical reagent costs, corrosion-resistant equipment, and there is also a risk of environmental pollution.
[0003] The hydrothermal method is an emerging thermochemical conversion technology. It uses water or other solutions as the medium and undergoes a series of reactions under high temperature and high pressure conditions, such as hydrolysis, depolymerization, polymerization, dehydration, decarboxylation, aromatization, etc. It is similar to the natural formation process of humus and is an artificially enhanced humification reaction, especially for biomass containing proteins and polysaccharides. However, the humus content of the product obtained by direct hydrothermal treatment of cellulosic waste biomass is not high because of its stubborn structure and lack of protein substances. For this reason, the hydrothermal humification process is enhanced by pre-treating the cellulosic biomass and then co-hydrothermally treating it with nitrogen-rich biomass such as residual sludge.
[0004] Therefore, there is an urgent need in the art for a potassium ferrate composite liquid, a preparation method and application thereof. Summary of the invention
[0005] The purpose of the present invention is to solve the problem that the humus content of the product obtained by directly hydrothermal cellulose waste biomass in the prior art is not high.
[0006] In order to achieve the purpose of solving the above problems, the technical solution adopted by the present invention is to provide a potassium ferrate composite liquid, a preparation method and application thereof.
[0007] In a first aspect of the present invention, there is provided a potassium ferrate composite solution, wherein OH - , Fe 6+ and ClO - The concentrations are: 0.10~0.15mol / L, 0.010~0.015mol / and 0.18~0.20mol / L respectively.
[0008] The second aspect of the present invention provides a method for preparing a potassium ferrate composite liquid, comprising the following steps:
[0009] Step 1: gradually add KOH solid to NaClO (10% available chlorine) solution and place in ice water with constant stirring;
[0010] Step 2, removing KCl solid and excess KOH in the solution to obtain a KOH-saturated sodium hypochlorite solution;
[0011] Step 3: Pour out the filtrate, heat it in a water bath, and add Fe(NO3)3·9H2O solid in batches under vigorous stirring;
[0012] Step 4: After reacting for 1 to 2 hours, add KOH until a large amount of purple-black solid precipitates, and place in an ice bath;
[0013] Step 5, filter and collect the filtrate, the obtained purple-black solid is potassium ferrate, and the collected purple-red filtrate is the potassium ferrate composite liquid.
[0014] Preferably, in step 1, the mass of KOH solid is 100-110 g, and the volume of NaClO solution is 100 ml.
[0015] Preferably, in step 3, the solid mass of Fe(NO3)3·9H2O is 50-60 g.
[0016] Preferably, in step 4, the mass of KOH solid is 20 to 30 g.
[0017] The third aspect of the present invention provides an application of the above potassium ferrate composite liquid in the preparation of humified organic fertilizer, comprising the following steps:
[0018] Step 1: gravity concentrate the sludge and collect the concentrated supernatant; at the same time, mechanically process the cellulosic waste biomass into debris;
[0019] Step 2, mixing the debris in step 1 with a potassium ferrate composite liquid, performing pretreatment, and obtaining a mixture;
[0020] Step 3, separating the solid from the mixture in step 2, transferring the solid to a hydrothermal reactor, adding the concentrated sludge in step 1 and the supernatant generated in the sludge concentration process, mixing evenly, and conducting a closed hydrothermal reaction;
[0021] Step 4: After the reaction is completed, the mixture is naturally cooled to room temperature, the hydrothermal mixture is separated into solid and liquid, and the obtained solid phase product is washed with deionized water and dried to obtain a humified organic fertilizer.
[0022] Preferably, in step 1, the sludge mainly includes residual sludge from urban sewage treatment plants and domestic sewage treatment plants, and the sludge concentration after concentration is 30 g / L; the cellulosic waste biomass includes agricultural solid waste biomass and wood chips made from waste biomass wood; the diameter of the chips is 0.1-5 cm.
[0023] Preferably, in step 2, the solid-liquid ratio of the debris to the potassium ferrate composite liquid is 1:(5-20), and the pretreatment condition is standing at 15-75° C. for 0.5-6 h.
[0024] Preferably, in step 3, the mass ratio of the debris in the mixture to the concentrated sludge is 1:3-5:1, and the solid content of the mixture is 5-35%; the hydrothermal reaction temperature is 180°C-260°C, and the reaction time is 1h-8h.
[0025] Preferably, in step 4, the solid-liquid separation method is centrifugation or filtration, and the drying condition is oven drying at 105° C. for 2 hours until the moisture content is ≤30%.
[0026] Compared with the prior art, the present invention has the following beneficial effects:
[0027] (1) Cellulosic waste biomass is cheap and readily available, has low operating costs, and is easy to promote and apply.
[0028] (2) Pretreatment of cellulosic waste biomass can destroy the stubborn structure of lignocellulose, improve the progress of the Maillard reaction, and provide favorable conditions for increasing the humus content of hydrothermal products.
[0029] (3) Potassium ferrate composite liquid is the filtrate remaining after the preparation of potassium ferrate, which contains a large amount of OH - , Fe 6+ and ClO - It has the potential to destroy the stubborn structure of wood cellulose and reuses industrial waste liquid without adding additional chemical reagents, which is in line with the concept of "waste treatment with waste". BRIEF DESCRIPTION OF THE DRAWINGS
[0030] Figure 1 Schematic diagram of the process of preparing humified organic fertilizer by pretreating cellulose waste biomass with potassium ferrate composite liquid and hydrothermally treating it
[0031] Figure 2 To improve the organic matter and nutrient elements of biochar by pretreatment with potassium ferrate composite solution;
[0032] Figure 3 To study the effect of adding 10% humified organic fertilizer on the dissolved organic matter content in red soil;
[0033] Figure 4To study the effect of adding 10% humified organic fertilizer on the contents of TC, TN and TP in red soil;
[0034] Figure 5 Comparative photos showing the germination and tillering number of Brassica juncea crops grown in red soil with 10% humified organic fertilizer added (left) and original red soil (right) within 15 days.
[0035] Figure 6 This is a graph showing the change in humic acid content of hydrothermal carbon in the humified organic fertilizers prepared in Example 4 and Comparative Examples 1-4. DETAILED DESCRIPTION
[0036] In order to make the present invention more clearly understood, a preferred embodiment is described in detail with reference to the accompanying drawings as follows:
[0037] Example 1
[0038] A method for preparing humified organic fertilizer by pretreating cellulose waste biomass with potassium ferrate composite liquid and hydrothermally treating the waste biomass, comprising the following steps:
[0039] The residual sludge from the domestic sewage treatment plant was concentrated by gravity to a concentration of 20 g / L. At the same time, the rice straw was mechanically crushed into fine pieces with a diameter of about 2 cm. The pre-treated rice straw was mixed with potassium ferrate complex solution (OH - =0.14mol / L,Fe 6+ =0.013 mol / L), ClO - =0.184mol / L) and allowed to stand for 3h at 25℃ for pretreatment. The pretreated mixture was filtered for solid-liquid separation, and the solid was transferred to a hydrothermal reactor, and the concentrated sludge and the supernatant produced during the sludge concentration process were added to make the mass ratio of the pretreated straw to the residual sludge 1:1, and the solid content of the mixture was 20%. After uniform mixing, a closed hydrothermal reaction was carried out, the reaction temperature was 220℃, and the reaction time was 4h. After the reaction was completed, it was naturally cooled to room temperature, the hydrothermal mixture was centrifuged, and the obtained solid phase product was dried to a moisture content of less than 30%, and humified organic fertilizer was obtained.
[0040] Rice straw that had not been pretreated with potassium ferrate composite solution was mixed with excess sludge in a mass ratio of 1:1 and then transferred to a hydrothermal reactor to prepare biochar under the same reaction conditions. Figure 2 As shown in the figure, the contents of organic matter, humic acid, fulvic acid and total nutrients in the humic organic fertilizer pretreated with potassium ferrate composite solution were significantly increased.
[0041] Example 2
[0042] A method for preparing humified organic fertilizer by pretreating cellulose waste biomass with potassium ferrate composite liquid and hydrothermally treating the waste biomass, comprising the following steps:
[0043] The residual sludge from the domestic sewage treatment plant was concentrated by gravity to a concentration of 30 g / L. At the same time, the rice straw was mechanically crushed into fine pieces with a diameter of about 1.5 cm. The pre-treated rice straw was mixed with potassium ferrate complex solution (OH - =0.15mol / L,Fe 6+ =0.015mol / L), ClO - =0.18mol / L) and allowed to stand for 1h at 50°C for pretreatment. The pretreated mixture was filtered for solid-liquid separation, and the solid was transferred to a hydrothermal reactor. The concentrated sludge and the supernatant produced during the sludge concentration process were added to make the mass ratio of the pretreated straw to the residual sludge 2:1, and the solid content of the mixture was 25%. After uniform mixing, a closed hydrothermal reaction was carried out at a reaction temperature of 220°C and a reaction time of 4h. After the reaction was completed, it was naturally cooled to room temperature, the hydrothermal mixture was centrifuged, and the solid phase product was dried to a moisture content of less than 30%, thereby obtaining a humified organic fertilizer. The prepared humified organic fertilizer was applied to red soil in an amount of 10% of the mass of the red soil, stirred until uniformly mixed, and tap water was added to keep the moisture content of the soil at 70% of the field water holding capacity. After 10 days of cultivation under natural conditions, the changes in the physical and chemical properties of the soil in the control group and the experimental group were detected.
[0044] like Figure 3 , 4 shown. Figure 3 In the figure, region I is a tyrosine-like fluorescent component, region II is a tryptophan-like fluorescent component, region III is a fulvic acid-like fluorescent component, region IV is a soluble microbial metabolite-like fluorescent component, and region V is a humic acid-like fluorescent component. This shows that after applying the humus organic fertilizer of the present invention, the nutrient and humus content of the soil is significantly increased.
[0045] Example 3
[0046] A method for pretreating cellulose waste biomass with potassium ferrate composite liquid and co-hydrothermally preparing humified organic fertilizer to improve soil physical and chemical properties and crop growth performance comprises the following steps:
[0047] The residual sludge from the domestic sewage treatment plant was concentrated by gravity to a concentration of 25 g / L. At the same time, the rice straw was mechanically crushed into fine pieces with a diameter of about 1 cm. The pre-treated rice straw was mixed with potassium ferrate complex solution (OH - =0.145mol / L,Fe 6+=0.010mol / L), ClO - =0.18mol / L) and allowed to stand for 0.5h at 75℃ for pretreatment. The pretreated mixture is filtered for solid-liquid separation, and the solid is transferred to a hydrothermal reactor. The concentrated sludge and the supernatant produced during the sludge concentration process are added to make the mass ratio of the pretreated straw to the residual sludge 1.5:1, and the solid content of the mixture is 30%. After uniform mixing, a closed hydrothermal reaction is carried out, the reaction temperature is 240℃, and the reaction time is 4h. After the reaction is completed, it is naturally cooled to room temperature, the hydrothermal mixture is centrifuged, and the solid phase product is dried to a moisture content of less than 30%, so as to obtain a humified organic fertilizer. The prepared humified organic fertilizer is applied to red soil in an amount of 10% of the mass of the red soil, stirred until uniformly mixed, and tap water is added to keep the moisture content of the soil at 70% of the field water holding capacity. It is cultivated under natural conditions for 7 days to activate the microorganisms in the soil, and then the same number of chicken feather vegetable seeds of the same size are planted, and the growth of the seeds within fifteen days is observed. Figure 5 shown.
[0048] Example 4
[0049] A method for preparing humified organic fertilizer by pretreating cellulose waste biomass with potassium ferrate composite liquid and hydrothermally treating the waste biomass, comprising the following steps:
[0050] The residual sludge from the domestic sewage treatment plant was concentrated by gravity to a concentration of 30 g / L. At the same time, the rice straw was mechanically crushed into fine pieces with a diameter of about 1.5 cm. The pre-treated rice straw was mixed with potassium ferrate complex solution (OH - =0.14mol / L,Fe 6+ =0.012mol / L), ClO - =0.18mol / L) and allowed to stand for 1h at 25°C for pretreatment. The pretreated mixture was filtered for solid-liquid separation, and the solid was transferred to a hydrothermal reactor, and concentrated sludge and supernatant produced during sludge concentration were added to make the mass ratio of pretreated straw to residual sludge 1:1, and the solid content of the mixture was 25%. After uniform mixing, a closed hydrothermal reaction was carried out, the reaction temperature was 220°C, and the reaction time was 4h. After the reaction was completed, it was naturally cooled to room temperature, the hydrothermal mixture was centrifuged, and the obtained solid phase product was dried to a moisture content of less than 30%, and humified organic fertilizer was obtained.
[0051] Comparative Example 1
[0052] Keeping other conditions of Example 4 unchanged, the potassium ferrate in the potassium ferrate composite solution was replaced with potassium permanganate to prepare humified organic fertilizer.
[0053] Comparative Example 2
[0054] Keeping other conditions of Example 4 unchanged, the potassium ferrate in the potassium ferrate composite solution was replaced with OH with the same ion concentration as the potassium ferrate composite solution. - (0.14 mol / L) solution is mixed to prepare humified organic fertilizer.
[0055] Comparative Example 3
[0056] Keeping other conditions of Example 4 unchanged, the potassium ferrate in the potassium ferrate composite solution was replaced with Fe 6+ (0.013 mol / L) were mixed to prepare humified organic fertilizer.
[0057] Comparative Example 4
[0058] Keeping other conditions of Example 4 unchanged, the potassium ferrate in the potassium ferrate composite solution was replaced with ClO with the same ion concentration as the potassium ferrate composite solution. - (0.184 mol / L) were mixed to prepare humified organic fertilizer.
[0059] In the humified organic fertilizers prepared in Example 4 and Comparative Examples 1-4, the changes in the humic acid content of the hydrothermal carbon are as follows: Figure 6 shown.
[0060] The above is only a preferred embodiment of the present invention, and is not any formal or substantial limitation of the present invention. It should be pointed out that ordinary technicians in this technical field can make several improvements and supplements without departing from the present invention, and these improvements and supplements should also be regarded as the protection scope of the present invention. Any technician familiar with this profession, without departing from the spirit and scope of the present invention, can make some changes, modifications and equivalent changes made by using the technical content disclosed above, which are equivalent embodiments of the present invention; at the same time, any changes, modifications and evolutions of any equivalent changes made to the above embodiments based on the essential technology of the present invention are still within the scope of the technical solution of the present invention.
Claims
1. A potassium ferrate composite liquid, characterized in that: Among them OH - , Fe 6+ and ClO - The concentrations are: 0.18~0.20mol / L, 0.010~0.015mol / and 0.10~0.15mol / L respectively.
2. A method for preparing the potassium ferrate composite liquid as claimed in claim 1, characterized in that: The following steps are involved: Step 1: gradually add excess KOH (solid-to-liquid ratio above 1:1) solid into NaClO (available chlorine 10%) solution, and place in ice water with constant stirring; Step 2, removing KCl solid and excess KOH in the solution to obtain a KOH-saturated sodium hypochlorite solution; Step 3: Pour out the filtrate, heat it in a water bath (temperature is about 40°C), and add Fe(NO3)3·9H2O solid in batches under vigorous stirring; Step 4: After reacting for 1 to 2 hours, add KOH until a large amount of purple-black solid precipitates, and place in an ice bath; Step 5, filter and collect the filtrate, the obtained purple-black solid is potassium ferrate, and the collected purple-red filtrate is the potassium ferrate composite liquid.
3. The method for preparing the potassium ferrate composite liquid according to claim 2, characterized in that: In the step 1, the mass of KOH solid is 100-110 g, and the volume of NaClO solution is 100 ml.
4. The method for preparing the potassium ferrate composite liquid according to claim 2, characterized in that: In the step 3, the solid mass of Fe(NO3)3·9H2O is 50-60g.
5. The method for preparing the potassium ferrate composite liquid according to claim 2, characterized in that: In the step 4, the mass of KOH solid is 20 to 30 g.
6. Use of the potassium ferrate composite liquid as claimed in claim 1 in preparing humified organic fertilizer, characterized in that: The following steps are involved: Step 1: gravity concentrate the sludge and collect the concentrated supernatant; at the same time, mechanically process the cellulosic waste biomass into debris; Step 2, mixing the debris in step 1 with a potassium ferrate composite liquid, performing pretreatment, and obtaining a mixture; Step 3, separating the solid from the mixture in step 2, transferring the solid to a hydrothermal reactor, adding the concentrated sludge in step 1 and the supernatant generated in the sludge concentration process, mixing evenly, and conducting a closed hydrothermal reaction; Step 4: After the reaction is completed, the mixture is naturally cooled to room temperature, the hydrothermal mixture is separated into solid and liquid, and the obtained solid phase product is washed with deionized water and dried to obtain a humified organic fertilizer.
7. The use according to claim 6, characterized in that In the step 1, the sludge mainly includes residual sludge from urban sewage treatment plants and domestic sewage treatment plants, and the sludge concentration after concentration is 30g / L; the cellulosic waste biomass includes agricultural solid waste biomass and wood chips made from waste biomass wood; the diameter of the chips is 0.1-5cm.
8. The use according to claim 6, characterized in that In the step 2, the solid-liquid ratio of the debris to the potassium ferrate composite liquid is 1:(5-20), and the pretreatment condition is to stand at 15-75°C for 0.5-6h.
9. The use according to claim 6, characterized in that In step 3, the mass ratio of the debris in the mixture to the concentrated sludge is 1:3-5:1, and the solid content of the mixture is 5-35%; the hydrothermal reaction temperature is 180°C-260°C, and the reaction time is 1h-8h.
10. The use according to claim 6, characterized in that In the step 4, the solid-liquid separation method is centrifugation or filtration, and the drying condition is drying in an oven at 105° C. for 2 hours until the moisture content is ≤30%.
Citation Information
Cited By
Method for preparing fulvic acid type liquid bacterial fertilizer by minute-level decomposition of breeding wastewater
CN122167237A