Wear-resistant polytetrafluoroethylene composite material as well as preparation method and application thereof

By adding surface fluorinated carbon fiber and fluorinated graphene to the polytetrafluoroethylene composite material, combined with high-temperature molding process, a solid surface protective layer is formed, which solves the problem of degradation in a high-radiation environment, and significantly improves the Radiation resistance and wear resistance.

CN118994820APending Publication Date: 2024-11-22GUANGZHOU MECHANICAL ENGINEERING RESEARCH INSTITUTE CO LTD +1

Patent Information

Application Number
CN202411262484.7
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-09-10
Publication Date
2024-11-22

AI Technical Summary

Technical Problem

Polytetrafluoroethylene has deteriorated performance under high energy radiation, making it difficult to maintain wear resistance and mechanical properties in a high-radiation environment, and the prior art is difficult to effectively solve its radiation damage problem.

Method used

Using composite materials including polytetrafluoroethylene, surface fluorinated carbon fiber and fluorinated graphene, the radiation resistance of composite materials is improved through the mutual attraction of fluorine elements and the cross-linking effect of graphene, and a strong composite material is formed through high-temperature molding process. Surface protective layer.

Benefits of technology

It significantly improves the radiation resistance and wear resistance of composite materials, extends the service life in a radiant environment, and enhances the friction coefficient and wear resistance.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader

Abstract

The invention discloses a wear-resistant polytetrafluoroethylene composite material which comprises the following components in parts by weight: 70-95 parts of polytetrafluoroethylene; 5 to 20 parts of surface fluorinated carbon fiber; 5-8 parts of graphite and fluorinated graphene; wherein the weight ratio of the graphite to the fluorinated graphene is (0.5-3): 1. By introducing the surface fluorinated carbon fibers and the graphite in a specific proportion, the surface performance can be remarkably improved, and good radiation resistance is achieved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of polymer materials, and in particular to a wear-resistant polytetrafluoroethylene composite material and a preparation method and application thereof. Background Art

[0002] As an excellent solid lubricant, polytetrafluoroethylene (PTFE) has good chemical corrosion resistance, heat resistance, cold resistance, good tensile strength, flexibility and other mechanical properties and electrical properties. Therefore, polytetrafluoroethylene composite materials can be used to prepare wear-resistant bearings, sealing materials, etc.

[0003] However, polytetrafluoroethylene has poor radiation resistance. It will degrade after being exposed to high-energy radiation, and the basic properties of the polymer (wear resistance, mechanical properties, elongation at break, etc.) will be significantly reduced. High doses of radiation and long exposure time will cause it to break and eventually be reduced to powder. After all, friction coefficient and wear resistance are important working indicators for bearings. The radiation damage threshold of PTFE is 2~7×10 4 rads. Depending on the exposure time, doses above this level will damage the performance of PTFE. Since ordinary PTFE cannot be used in high-radiation environments, how to use other methods to solve the radiation resistance of PTFE is an urgent problem to be solved.

[0004] CN2023100342366 discloses a fluorine-containing composite material for use in a radiation environment, which mainly includes 30-90 parts of polytetrafluoroethylene, 5-20 parts of carbon fiber, 2-3 parts of chromium trioxide, and 1-5 parts of fluorinated graphene. It mainly utilizes the mutual attraction between fluorine in metal fluoride and PTFE fluorine atoms, and the mutual attraction between its metal ions and metal friction pairs is enhanced, so that the PTFE molecular chains are tightly entangled together. At the same time, the fluorinated graphene entangles the PTFE molecular chains together to play a similar effect to cross-linking. When irradiated with gamma rays, the wear rate of the PTFE composite material is effectively reduced and its wear resistance is improved. The two-dimensional dense structure of graphene and metal fluoride (CrF3) jointly improve the cohesive energy, density and surface tension of the composite material, greatly improving the barrier properties, surface bonding and other properties. When irradiated with gamma rays, the composite product changes from unstable to limited stable, and limited stability in many cases will become chemically stable, forming a solid surface protective layer, thereby improving wear resistance and radiation resistance. Summary of the invention

[0005] The object of the present invention is to provide a polytetrafluoroethylene composite material with good radiation resistance.

[0006] The present invention is achieved through the following technical solutions: A wear-resistant polytetrafluoroethylene composite material, comprising the following components in parts by weight: Polytetrafluoroethylene 70-95 parts; Surface fluorinated carbon fiber 5-20 parts; 5-8 parts of graphite and fluorinated graphene; Among them, the weight ratio range of graphite to fluorinated graphene is (0.5-3):1.

[0007] The polytetrafluoroethylene is suspension polytetrafluoroethylene.

[0008] The surface fluorinated carbon fiber is a fluorine-modified acrylonitrile-based carbon fiber.

[0009] Fluorinated graphene and surface fluorinated carbon fiber can be commercially available products or can be obtained according to a homemade method, wherein the homemade method is to disperse graphene (or carbon fiber) in a PTFE solution, stir evenly, filter, and dry. The PTFE solution can be a commercially available product, such as the commercially available brand DF-331Z of Shandong Dongyue.

[0010] The diameter of the surface fluorinated carbon fiber is in the range of 3-15 μm.

[0011] The average particle size of the graphite and fluorinated graphene is in the range of 15-30 μm.

[0012] Preferably, the weight ratio of graphite to fluorinated graphene is in the range of (1-2):1.

[0013] Those skilled in the art can choose whether to add 0-1 part of auxiliary agent according to actual conditions, and the auxiliary agent is selected from antioxidants and lubricants. It is also possible to choose to add a certain amount of other fillers 0-1 part of other fillers, and other fillers can be molybdenum disulfide, black scale, etc.

[0014] The preparation method of the wear-resistant polytetrafluoroethylene composite material of the invention comprises the following steps: uniformly mixing the components according to the proportion, drying, stirring, cold pressing and then high-temperature molding to obtain the wear-resistant polytetrafluoroethylene composite material; the pressure of the cold pressing is 40-60MPa, and the high-temperature molding step comprises heating to 330°C at a rate of 30-60°C / hour, keeping the temperature for 0.5-2 hours, heating to 370-390°C at 40-50°C / hour, keeping the temperature for 1-3 hours; and then cooling to 320-340°C at a rate of 10-50°C / hour, keeping the temperature for 1-2 hours.

[0015] The wear-resistant polytetrafluoroethylene composite material of the invention is used for preparing bearings.

[0016] The present invention has the following beneficial effects: The present invention adds surface fluorinated carbon fiber to polytetrafluoroethylene, so that the fluorine element on the surface of the carbon fiber can have better compatibility with polytetrafluoroethylene. At the same time, the fluorinated graphene is blended with graphite and then blended with polytetrafluoroethylene to improve the dispersion performance and increase the enrichment of the fluorinated graphene and graphite on the surface, thereby improving the radiation resistance and the wear resistance after irradiation. DETAILED DESCRIPTION

[0017] The technical solutions in the embodiments of the present invention are described clearly and completely below. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of them. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0018] The sources of raw materials used in the present invention are as follows: Polytetrafluoroethylene: Daikin Fluorochemical China Co., Ltd., model M-18F; Fluorinated graphene: The average particle size is 25 µm. Graphene was purchased from Sigma-Aldrich Merck Group and was obtained by uniformly mixing graphene with PTFE solution, separating, and drying.

[0019] Graphite: colloidal graphite, purchased from Shanghai Chemical Plant; Carbon fiber: acrylonitrile-based ground carbon fiber, aspect ratio of 7-20, diameter of 5-10µm, Qingdao Yuanhui Composite Materials Co., Ltd., brand name acrylonitrile-based YHP-CD-Ⅲ.

[0020] Surface fluorinated carbon fiber: homemade.

[0021] Embodiment and comparative example A method for preparing a wear-resistant polytetrafluoroethylene composite material: according to a ratio, the components are mixed uniformly, and then dried, stirred, cold pressed, and then high-temperature molded to obtain a polytetrafluoroethylene composite material; the pressure of the cold pressing molding is 40-60MPa, and the high-temperature molding step includes heating to 330°C at a rate of 30-60°C / hour, keeping warm for 0.5-2 hours, continuing to heat to 370-390°C at 40-50°C / hour, keeping warm for 1-3 hours; and then cooling to 320-340°C at a rate of 10-50°C / hour, and keeping warm for 1-2 hours.

[0022] Various test methods: (1) Radiation method: Use γ-ray irradiation of 3000Gy for 50 hours, and then test the tensile strength retention rate and elongation retention rate.

[0023] (2) Friction coefficient: GB 3960 Plastic sliding friction and wear test; (3) Wear amount: GB 3960 Plastic sliding friction and wear test.

[0024] Table 1: Content of each component (parts by weight) and test results of the wear-resistant polytetrafluoroethylene composite material of the embodiment Example 1 Example 2 Example 3 Example 4 Example 5 Example 6 Example 7 Polytetrafluoroethylene 70 80 90 80 80 80 80 Surface fluorinated carbon fiber 8 20 16 20 20 20 20 graphite 2.5 3 4 2 3.6 4 4.5 Fluorinated graphene 2.5 3 4 4 2.4 2 1.5 Initial friction coefficient 0.19 0.19 0.17 0.21 0.18 0.17 0.17 <![CDATA[Initial wear amount (mm 3 / N·m)*10 -5 > 7.0 6.8 5.8 7.4 6.5 6.2 6.1 Friction coefficient after irradiation 0.15 0.14 0.15 0.17 0.14 0.15 0.16 <![CDATA[Wear amount after irradiation (mm 3 / N·m) 10 -5 > 4.2 3.8 3.8 5.9 4.1 4.5 5.1 It can be seen from Examples 2 / 4 / 5 / 6 / 7 that the wear resistance of the polytetrafluoroethylene composite material will be improved within a certain period after being irradiated, and the preferred ratio of graphite / graphene oxide has better radiation resistance.

[0025] Table 2: Content of each component (parts by weight) and test results of wear-resistant polytetrafluoroethylene composite materials in comparative example Comparative Example 1 Comparative Example 2 Comparative Example 3 Comparative Example 4 Comparative Example 5 Polytetrafluoroethylene 80 80 80 80 80 Surface fluorinated carbon fiber 20 20 20 20 Carbon Fiber 20 graphite 3 0 6 1 5 Fluorinated graphene 3 6 0 5 1 Initial friction coefficient 0.20 0.26 0.20 0.23 0.18 <![CDATA[Initial wear amount (mm 3 / N·m)*10 -5 > 6.9 8.3 7.1 7.9 6.4 Friction coefficient after irradiation 0.18 0.21 0.19 0.20 0.18 <![CDATA[Wear amount after irradiation (mm 3 / N·m) * 10 -5 > 6.7 7.6 7.8 7.5 6.6 It can be seen from Comparative Example 1 that the improvement of the corrosion resistance of the composite material by the fluorine-free modified carbon fiber is insufficient.

[0026] It can be seen from Comparative Examples 2-5 that if the ratio of graphite to fluorinated graphene is not within the range of the present invention, the initial wear resistance or radiation resistance is poor.

Claims

1. A wear-resistant polytetrafluoroethylene composite material, characterized in that: By weight, it includes the following components: Polytetrafluoroethylene 70-95 parts; Surface fluorinated carbon fiber 5-20 parts; 5-8 parts of graphite and fluorinated graphene; Among them, the weight ratio range of graphite to fluorinated graphene is (0.5-3):

1.

2. The wear-resistant polytetrafluoroethylene composite material according to claim 1, characterized in that: The polytetrafluoroethylene is suspension polytetrafluoroethylene.

3. The wear-resistant polytetrafluoroethylene composite material according to claim 1, characterized in that: The surface fluorinated carbon fiber is a fluorine-modified acrylonitrile-based carbon fiber.

4. The wear-resistant polytetrafluoroethylene composite material according to claim 1, characterized in that: The diameter of the surface fluorinated carbon fiber is in the range of 3-15 μm.

5. The wear-resistant polytetrafluoroethylene composite material according to claim 1, characterized in that: The average particle size of the graphite and fluorinated graphene is in the range of 15-30 μm.

6. The wear-resistant polytetrafluoroethylene composite material according to claim 1, characterized in that: The weight ratio of graphite to fluorinated graphene is in the range of (1-2):

1.

7. The wear-resistant polytetrafluoroethylene composite material according to claim 1, characterized in that: By weight, it also includes 0-1 part of auxiliary agent, and the auxiliary agent is selected from antioxidants, lubricants, and other fillers.

8. The method for preparing the wear-resistant polytetrafluoroethylene composite material according to any one of claims 1 to 7, characterized in that: The method comprises the following steps: uniformly mixing the components according to the proportion, drying, stirring, cold pressing and then high-temperature molding to obtain a wear-resistant polytetrafluoroethylene composite material; the pressure of the cold pressing is 40-60MPa, and the high-temperature molding step comprises heating to 330°C at a rate of 30-60°C / hour, keeping the temperature for 0.5-2 hours, heating to 370-390°C at 40-50°C / hour, keeping the temperature for 1-3 hours; and then cooling to 320-340°C at a rate of 10-50°C / hour, keeping the temperature for 1-2 hours.

9. Use of the wear-resistant polytetrafluoroethylene composite material according to any one of claims 1 to 7, characterized in that: For the preparation of bearings.

Citation Information

Patent Citations

  • Fluorine-containing composite material used in radiation environment and preparation method and application thereof

    CN116003939A

Cited By

  • Preparation method of wear-resistant polytetrafluoroethylene

    CN121006006A