Method for preparing high-purity Ge-68 by using high-current proton cyclotron
The method for preparing high-purity Ge-68 using a high-current proton cyclotron accelerator, which utilizes sulfuric acid electrolysis and tandem chromatographic column separation, solves the problems of cumbersome operation and poor performance in the existing technology for preparing high-purity Ge-68, and achieves efficient and simple preparation of high-purity Ge-68.
Patent Information
- Application Number
- CN202411003236.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-25
- Publication Date
- 2024-11-22
- Estimated Expiration
- 2044-07-25
AI Technical Summary
Existing technologies for preparing high-purity Ge-68 suffer from problems such as cumbersome and lengthy chemical separation operations, poor preparation results, and high technical difficulty.
A method for preparing high-purity Ge-68 using a high-current proton cyclotron accelerator was developed. This method involves preparing a solid Ga4Ni alloy target, electrolyzing it with sulfuric acid, and then using a tandem chromatographic column separation process with isohydroxime ester resin, cross-linked polyvinylbenzene resin, and AG MP-50 resin to achieve efficient separation and purification.
The chemical separation process is simplified, the preparation efficiency is improved, and a high-purity Ge-68 solution is obtained. The product with suitable acidity can be directly used to prepare Ge-Ga generators, avoiding the multiple acid changes and evaporation concentration operations in traditional methods, and reducing the impurity content.
Smart Images

Figure CN118996167A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of isotope production, and in particular to a method for preparing high-purity Ge-68 by using a high-current proton cyclotron. Background Art
[0002] International Atomic Energy Agency (IAEA) recommended application nat Ga(p,xn) 68 Ge nuclear reaction production 68 Ge, 68 The production of Ge is mainly concentrated in Brookhaven National Laboratory and Los Alamos National Laboratory in the United States, the South African National Accelerator Center and the Obninsk Cyclotron Company in Russia. Due to the special chemical properties of metal Ga, its low melting point and high chemical activity, Brookhaven National Laboratory, Los Alamos National Laboratory and the South African National Accelerator Center produce Ge. 68 Ge, usually prepared by irradiation of metal Ga target wrapped in Nb capsule 68 Ge, and then chemically separated by extraction or volatilization; while the Russian Obninsk Cyclotron Co., Ltd. has been using the Ga4Ni alloy target prepared by the melting method and using copper as the target support for irradiation production. 68 Ge. The preparation of metallic Ga targets has very strict requirements on the grain size, purity and preparation method of the encapsulating material Nb. The preparation of Ga4Ni alloy by melting method is technically difficult and the bonding with the copper target holder is not strong. Ga-Ni alloy targets can also be prepared by electroplating, which can withstand higher irradiation beams than melting method. At the same time, the chromatographic separation process is a commonly used chemical separation method for medical isotopes, which can realize continuous separation operations and is conducive to the design and control of automated separation.
[0003] In 2014, the Institute of Isotopes of the China Institute of Atomic Energy and Atom Hi-Tech Co., Ltd. reported the use of electroplating to prepare Ga-Ni alloy targets (a radioactive 68 Ge solution preparation method), and a layer of metal Ni was plated on the Ga-Ni alloy layer to prevent damage to the target during irradiation. The prepared target was also placed at the Cyclone-30 cyclotron terminal for a small dose irradiation experiment to verify the feasibility of the target. After the target was cooled, the target was electrolyzed, the electrolyte was separated and purified on a silica gel column, and desorbed with a nitric acid solution. 68 Ge. The silica gel column separation method has some disadvantages. First, after the solution is loaded on the silica gel column, it needs to be eluted with sulfuric acid to remove the impurity ions on the silica gel column. The residual sulfate ion content on the silica gel column is very high, which will lead to the preparation of 68 Ge solution cannot be used 68 Ge- 68Preparation of Ga generator. Secondly, even if concentrated nitric acid is used to elute the silica gel column, the sulfate ions on the silica gel column can be removed, but it needs to be continuously desorbed and repeatedly soaked with dilute nitric acid, and the process is time-consuming. Finally, the desorption solution containing nitric acid medium is evaporated to dryness with a polytetrafluoroethylene evaporating dish to remove nitric acid, and then the solid matter in the evaporating dish is soaked with hydrochloric acid solution for one week to prepare 68 Ge- 68 Preparation of the hydrochloric acid medium required for the Ga generator 68 Ge solution. This method changes three acidic media in the middle, and the chemical separation process is complicated and lengthy.
[0004] In 2023, the Institute of Modern Physics of the Chinese Academy of Sciences and Sichuan University used electroplating to prepare Ga-Ni alloy targets (a method based on accelerator irradiation production and preparation in China with Chinese publication number CN114937516 A) 68 Ge method), referring to the dual AG1X8 and Ge method developed by Brookhaven National Laboratory in the United States for Nb capsule-wrapped metal Ga targets. The three-column separation process of G-25 was established by Chelex100 and G-25 resin coupled with a recyclable dual-column separation process was designed and built 68 Ge automated separation device, and the device was used to achieve accelerator irradiation Ga-Ni alloy target 68 Separation of Ge, 68 Ge recovery rate is about 70%, activity is about 5mCi, The final eluent of G-25 is hydrochloric acid medium, which is very suitable for direct preparation 68 Ge- 68 Ga generator. This method also has some problems. BNL uses Nb capsule to wrap the metal Ga target process, which only requires dilute hydrochloric acid and hydrogen peroxide to dissolve the target, while the Ga-Ni alloy target needs to be dissolved with a strong acid solution and hydrogen peroxide mixed system, which takes 8-10 hours; the Ga-Ni alloy target solution is dark blue and transparent, indicating that the copper target holder is dissolved in large quantities, while the Nb capsule wrapped metal Ga target does not have this problem. And because the Cu in the target solution 2+ The concentration is too high. The Chelex 100 column needs to be reused three times to remove a large amount of Cu. 2+ If the large amount of Cu is not removed at the Chelex 100 column stage, 2+ , when the pH is adjusted to alkaline ( Before G-25 column separation), Cu 2+ Being precipitated will not only cause 68 More losses, and 68 Ge products also contain a large amount of citric acid and inorganic impurities.
[0005] ITM Germany is producing68 Ge- 68 Before the Ga generator, the BNL or LANL source is often 68 The Ge stock solution was further finely separated (China Publication No. CN 110612272 A) to prepare high-purity Ge for radiopharmaceutical purposes 68 Ge material method), producing a good manufacturing practice (GMP) 68 Ge-API (API = Active Pharmaceutical Ingredient) solution. The radiochemical method disclosed in the patent is based on the separation of 68 Ge, first purified from organic and metallic impurities by adsorption on Eichrom PreFilter resin in the form of germanium tetrachloride 68 Ge, and then further purified by cation exchange with AG MP-50 resin to make the final 68 Ge-API products meet the regulatory requirements of GMP production specifications.
[0006] At present, there are still a lot of problems in the existing technology for preparing high-purity GE-68, including the complicated and lengthy chemical separation process, the addition of strong acid solution and hydrogen peroxide during the reaction process, which causes a large amount of dissolution of the target support, resulting in poor preparation effect, and the high difficulty of the preparation technology. Summary of the invention
[0007] The technical problem to be solved by the present invention is to provide a method for preparing high-purity Ge-68 using a high-current proton cyclotron, so as to solve the problems of complicated and lengthy chemical separation process, poor preparation effect and high difficulty of preparation technology in the prior art for preparing high-purity Ge-68.
[0008] In order to solve the above problems, the present invention provides a method for preparing high-purity Ge-68 using a high-current proton cyclotron, comprising the following steps:
[0009] S1: Prepare a fixed Ga4Ni alloy target, treat the alloy target with high-current proton irradiation, and then electrolyze and dissolve it in sulfuric acid to obtain a 68 Ge, 68,nat Ga, 56,57,58 Co. 65 Zn, nat Ni and nat Cu electrolyte;
[0010] S2: passing the electrolyte obtained in step S1 into a series of chromatographic columns for separation and purification, wherein the series of chromatographic columns are a hydroxamate resin separation column, a cross-linked polydivinylbenzene resin separation column and an AG MP-50 resin separation column, and collecting the electrolyte containing 68 Ge solution, completing the preparation.
[0011] The present invention discloses a method for preparing high-purity Ge-68 by using a high-current proton cyclotron. The method adopts an inert metal as a base target holder, prepares a solid Ga4Ni alloy target, prepares a high-current proton cyclotron irradiated target, further performs sulfuric acid electrolysis on the target, and establishes a series chromatography column separation process of a hydroxamate resin (Zr resin), a cross-linked polydivinylbenzene resin (Guard resin) and an AG MP-50 resin, so that Ge-68 with high purity can be prepared, and the problems of complicated and lengthy chemical separation process, poor preparation effect and high difficulty of preparation technology in the prior art for preparing high-purity Ge-68 are solved.
[0012] The present invention also provides a fast and efficient target electrolysis method. Most of the target dissolving methods in the prior art use hydrochloric acid and hydrogen peroxide, and heat to assist dissolution to generate GeCl4 solution. GeCl4 has a low boiling point (84°C), which is easy to produce radioactive aerosols. The process is time-consuming and the operation is cumbersome, which brings great trouble. The present invention uses a sulfuric acid electrolysis process, which is easy to operate. The sulfuric acid medium avoids contamination by volatile radioactive substances, and the electrolysis takes a short time. The operation of the present invention is simple and easy to realize automation. The preparation method obtained by the present invention is simple and easy to realize automation. 68 The Ge product has high purity and is a hydrochloric acid medium with appropriate acidity, so it can be used to directly prepare a Ge-Ga generator.
[0013] In a possible implementation, in step S1, the conditions for the high-current proton irradiation treatment are: using a high-current proton accelerator for irradiation, with an energy of 18-30 MeV, a current of 50-300 μA, a time greater than or equal to 3 hours, and a cooling time greater than or equal to 20 days.
[0014] In a possible implementation, in step S1, the structure of the solid Ga4Ni alloy target is as follows 1) or 2):
[0015] 1) comprising at least two layers, including a metal substrate layer and a solid gallium-nickel alloy layer connected in sequence;
[0016] 2) at least three layers, including a metal base layer, a metal protection layer and a solid gallium-nickel alloy layer connected in sequence;
[0017] In 1), the material of the metal base layer is Ta, Ti, Nb or Inconel alloy;
[0018] In the above 2), the material of the metal base layer is Cu or Al;
[0019] The metal protection layer is made of Au or Pt and has a thickness of more than 5 μm.
[0020] In the above possible implementations, in 1), the material of the metal base layer is selected from an inert metal that is conductive, thermally conductive, has high hardness and is corrosion-resistant, thereby improving the conductivity, thermal conductivity, strength and corrosion resistance of the target structure; in 2), the material of the metal base layer is selected from an inert metal that is conductive, thermally conductive, has high hardness and is corrosion-resistant, and in combination with the metal protective layer, an inert metal that is conductive and has strong thermal conductivity is selected, thereby further improving the strength, thermal conductivity, electrical conductivity and corrosion resistance of the target structure.
[0021] In a possible implementation, the solid gallium-nickel alloy layer has a Ga content of not less than 60% by mass and a thickness of more than 20 mg / cm 2 .
[0022] In a possible implementation, the solid gallium-nickel alloy layer is prepared by electroplating, and the preparation method includes:
[0023] A1: Dissolve metallic gallium in HNO3 solution, heat and stir, then add H2SO4 solution with a concentration of more than 98% to obtain Ga2(SO4)3 precipitate;
[0024] A2: dissolving the Ga2(SO4)3 precipitate obtained in step A1 in water, adjusting the pH value of the solution to 2-2.5 with an ammonia solution, heating the solution to 40-50° C., and adding NiSO4 to prepare a final electroplating solution;
[0025] A3: Use constant current electrolysis technology for electrodeposition, and adjust the current density to 20-60mA / cm 2 , the temperature is 25-100°C, and the speed of rotation and stirring is maintained at about 300-800rpm during the electroplating process. After 6-8 hours, a Ga4Ni alloy target is obtained.
[0026] In the above possible implementation, the present invention uses a method for preparing high-purity Ge-68 using a high-current proton cyclotron to prepare a Ga4Ni alloy target that is easy to irradiate and separate by controlling the electroplating method. Based on a corrosion-resistant inert metal substrate, the Ga4Ni alloy target is prepared by an electro-deposition method that is simple to operate and has a stable process. The combination of the electroplating method and the target holder is stronger than the melting method and can withstand a larger irradiation beam. In addition, the use of a Ta target holder substrate can avoid the introduction of inorganic impurities such as copper, aluminum, and gold when dissolving the target, which affects the effect of subsequent chromatographic separation.
[0027] In a possible implementation, in the step A1, the weight ratio of the metal gallium to the NiSO4 is (15-20): (10-15); and the concentration of the HNO3 solution is 9-12M.
[0028] In a possible implementation manner, in step S2, the step of passing the electrolyte into a series of chromatographic columns for separation and purification comprises:
[0029] B1: diluting the electrolyte and performing at least one separation treatment, wherein the separation treatment comprises: passing the electrolyte into the isohydroxamate resin separation column, eluting with H2SO4 and collecting the elution waste liquid, desorbing the elution waste liquid with dilute citric acid to obtain a desorption liquid, and adding H2SO4 to the desorption liquid; after the separation treatment is completed, adding HCl to the desorption liquid for acidification;
[0030] B2: Pass a cross-linked polydivinylbenzene resin separation column into the desorption liquid acidified in step B1, and elute with HCl while collecting the elution waste liquid, then use deionized water to desorb the elution waste liquid to obtain a pure water desorption liquid; finally, pass the pure water desorption liquid into an AG MP-50 resin separation column, add HCl for further desorption, collect the Ge-68 product, and complete the preparation.
[0031] In the above possible implementation manner, the separation treatment is performed 1 to 3 times. Through multiple separation treatments, the treatment effect of waste impurities in the analytical solution can be improved.
[0032] In the above possible implementation manner, in the step B1, since the leaching waste liquid contains a large amount of Ga, Ni, Co, and Zn inorganic impurities, dilute citric acid is used to desorb the leaching waste liquid to remove a large amount of the above impurities; and further in the step B2, the leaching waste liquid collected after eluting with HCl contains a large amount of sulfuric acid, citric acid and organic impurities, so it is desorbed by deionized water to remove a large amount of the above impurities; finally, the trace impurities such as Fe, Ni, Cu, Zn, and Pb in the solution are taken out through the AG MP-50 resin separation column, and further desorbed by HCl again, thereby improving the final purity of the Ge-68 product.
[0033] In a possible implementation, in step B1, the electrolyte is diluted to a H2SO4 concentration of 5-8M; in the elution with H2SO4, the concentration of H2SO4 is 4-5M; the concentration of the dilute citric acid is 0.08-0.15M; in the addition of H2SO4 to the desorption liquid, the concentration of H2SO4 is 5-8M; and the concentration of HCl is 9-10M.
[0034] In a possible implementation manner, in the step B2, the concentration of HCl in the elution with HCl is 9-10M; and the concentration of HCl in the further desorption with HCl is 0.2-0.5M.
[0035] In the above possible implementation, the present invention is based on sulfuric acid electrolyte medium, using three resin chromatographic columns for separation, purification and preparation. 68 Ge solution, while Zr resin will 68 Ge is completely separated from a large number of inorganic impurities such as target materials, substrates, and competitive nuclear reactions. Guard resin completely separates citric acid, sulfuric acid, and organic impurities. AG MP-50 resin separates trace impurities to obtain high-purity products that meet GMP standards. 68 Ge solution.
[0036] In summary, the method for producing high-purity Ge-68 by a high-current proton cyclotron provided in this application has the following advantages:
[0037] 1) Prepare Ga4Ni alloy targets that are easy to irradiate and separate:
[0038] The present invention is based on a corrosion-resistant inert metal substrate and adopts an electrodeposition method with simple operation and stable process to prepare Ga4Ni alloy targets. Compared with the traditional melting method, the target layer of the present invention is more firmly bonded to the target holder and can withstand a larger irradiation beam. In addition, the use of inert metals such as Ta as the target holder substrate can avoid the introduction of inorganic impurities such as copper, aluminum, and gold when dissolving the target, which affects the effect of subsequent chromatographic separation compared with previous methods.
[0039] 2) Fast and efficient electrolytic target method:
[0040] In the past, the target dissolution method often used hydrochloric acid and hydrogen peroxide, and heated to assist dissolution to generate GeCl4 solution. GeCl4 has a low boiling point and is prone to produce radioactive aerosols. In addition, the dissolution process takes a long time and the operation is cumbersome. The present invention adopts the process of sulfuric acid electrolysis, which is easy to operate, and the sulfuric acid medium avoids contamination by volatile radioactive substances, and the electrolysis takes a short time.
[0041] 3) Preparation of high purity 68Ge solution:
[0042] The present invention is based on sulfuric acid electrolyte medium, adopts three resin chromatographic columns to separate, purify and prepare 68 Ge solution. Zr resin 68 Ge is completely separated from a large number of inorganic impurities such as the target material, substrate, and competitive nuclear reaction. Guard resin completely separates citric acid, sulfuric acid, and organic impurities. AG MP-50 resin separates trace impurities to obtain a high-purity 68Ge solution that meets the standards. This invention is easy to operate, avoiding the multiple acid changes and evaporation and concentration required in previous methods. In addition, considering the requirements of the standards for the content of organic matter and metal ions, the three-level resin is used to achieve high purity. 68The separation of Ge avoids the problem of large amounts of citric acid, resin decomposition products and copper ions in the product of the previous method. The invention has a high recovery rate, is easy to realize automation, has high product purity, is a hydrochloric acid medium, has suitable acidity, and can directly prepare a Ge-Ga generator. BRIEF DESCRIPTION OF THE DRAWINGS
[0043] Figure 1 The present invention is a preparation flow chart of a method for preparing high-purity Ge-68 using a high-current proton cyclotron;
[0044] Figure 2 It is a schematic diagram of the structure and principle of the separation device in the embodiment of the present invention. DETAILED DESCRIPTION
[0045] First, those skilled in the art should understand that these implementations are only used to explain the technical principles of the embodiments of the present application, and are not intended to limit the protection scope of the embodiments of the present application. Those skilled in the art can make adjustments to them as needed to adapt to specific application scenarios.
[0046] In the description of the embodiments of the present application, it should be noted that, unless otherwise clearly specified and limited, the terms "connected" and "connection" should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be directly connected or indirectly connected through an intermediate medium. For ordinary technicians in this field, the specific meanings of the above terms in the embodiments of the present application can be understood according to specific circumstances.
[0047] The present invention provides a method for preparing high-purity Ge-68 by using a high-current proton cyclotron, comprising the following steps:
[0048] S1: Prepare a fixed Ga4Ni alloy target, treat the alloy target with high-current proton irradiation, and then electrolyze and dissolve it in sulfuric acid to obtain a 68 Ge, 68,nat Ga, 56,57,58 Co. 65 Zn, nat Ni and nat Cu electrolyte;
[0049] S2: passing the electrolyte obtained in step S1 into a series of chromatographic columns for separation and purification, wherein the series of chromatographic columns are a hydroxamate resin separation column, a cross-linked polydivinylbenzene resin separation column and an AG MP-50 resin separation column, and collecting the electrolyte containing 68 Ge solution, completing the preparation.
[0050] As a preferred solution, in step S1, the conditions for the high-current proton irradiation treatment are: using a high-current proton accelerator for irradiation, with an energy of 18-30 MeV, a current of 50-300 μA, a time greater than or equal to 3 hours, and a cooling time greater than or equal to 20 days.
[0051] As a preferred solution, in step S1, the structure of the solid Ga4Ni alloy target is as follows 1) or 2):
[0052] 1) comprising at least two layers, including a metal substrate layer and a solid gallium-nickel alloy layer connected in sequence;
[0053] 2) at least three layers, including a metal base layer, a metal protection layer and a solid gallium-nickel alloy layer connected in sequence;
[0054] In 1), the material of the metal base layer is Ta, Ti, Nb or Inconel alloy;
[0055] In the above 2), the material of the metal base layer is Cu or Al;
[0056] The metal protection layer is made of Au or Pt and has a thickness of more than 5 μm.
[0057] As a preferred solution, the mass content of Ga in the solid gallium-nickel alloy layer is not less than 60%, and the thickness is greater than 20 mg / cm 2 .
[0058] As a preferred solution, the solid gallium-nickel alloy layer is prepared by electroplating, and the preparation method includes:
[0059] A1: Dissolve metallic gallium in HNO3 solution, heat and stir, then add H2SO4 solution with a concentration of more than 98% to obtain Ga2(SO4)3 precipitate;
[0060] A2: dissolving the Ga2(SO4)3 precipitate obtained in step A1 in water, adjusting the pH value of the solution to 2-2.5 with an ammonia solution, heating the solution to 40-50° C., and adding NiSO4 to prepare a final electroplating solution;
[0061] A3: Use constant current electrolysis technology for electrodeposition, and adjust the current density to 20-60mA / cm 2 , the temperature is 25-100°C, and the speed of rotation and stirring is maintained at about 300-800rpm during the electroplating process. After 6-8 hours, a Ga4Ni alloy target is obtained.
[0062] As a preferred solution, in step A1, the weight ratio of the metal gallium to the NiSO4 is (15-20): (10-15); and the concentration of the HNO3 solution is 9-12M.
[0063] As a preferred solution, in step S2, the step of passing the electrolyte into a series of chromatographic columns for separation and purification comprises:
[0064] B1: diluting the electrolyte and performing at least one separation treatment, wherein the separation treatment comprises: passing the electrolyte into the isohydroxamate resin separation column, eluting with H2SO4 and collecting the elution waste liquid, desorbing the elution waste liquid with dilute citric acid to obtain a desorption liquid, and adding H2SO4 to the desorption liquid; after the separation treatment is completed, adding HCl to the desorption liquid for acidification;
[0065] B2: Pass a cross-linked polydivinylbenzene resin separation column into the desorption liquid acidified in step B1, and elute with HCl while collecting the elution waste liquid, then use deionized water to desorb the elution waste liquid to obtain a pure water desorption liquid; finally, pass the pure water desorption liquid into an AG MP-50 resin separation column, add HCl for further desorption, collect the Ge-68 product, and complete the preparation.
[0066] As a preferred scheme, in the step B1, the condition for diluting the electrolyte is to dilute it to a H2SO4 concentration of 5-8M; in the eluting with H2SO4, the concentration of H2SO4 is 4-5M; the concentration of the dilute citric acid is 0.08-0.15M; when H2SO4 is added to the desorption liquid, the concentration of H2SO4 is 5-8M; the concentration of HCl is 9-10M.
[0067] As a preferred solution, in the step B2, the concentration of HCl in the elution with HCl is 9-10M; and the concentration of HCl in the further desorption with HCl is 0.2-0.5M.
[0068] In the above technical scheme, the present invention mainly provides a method for preparing high-purity Ge-68 by using a high-current proton cyclotron, which mainly comprises the following steps: dissolving gallium salt and nickel salt in a sulfuric acid solution, using the electroplating principle to make gallium and nickel co-deposit on a tantalum target holder to prepare a gallium-nickel alloy target; after the alloy target is irradiated with ACSI-FLEX 30MeV, a target containing 68 The target is placed in a cooling position and then electrolyzed (electrolysis is the reverse process of electroplating); the electrolyte is then separated, purified and desorbed on a series of chromatographic columns to achieve impurity separation and solution medium conversion to obtain high-purity Ge-68.
[0069] The following provides some embodiments in combination with the above data range to further explain the present invention:
[0070] Embodiment 1:
[0071] This embodiment provides a method for producing high-purity Ge-68 using a high-current proton cyclotron, comprising:
[0072] A method for preparing high-purity Ge-68 using a high-current proton cyclotron comprises the following steps:
[0073] S1: preparing a fixed Ga4Ni alloy target, and subjecting the alloy target to high-current proton irradiation treatment. The conditions of the high-current proton irradiation treatment are: using a high-current proton accelerator for irradiation, the energy is 18MeV, the current is 50μA, the time is 3h, and the cooling time is 20 days;
[0074] Then, sulfuric acid electrolysis is performed to obtain 68 Ge, 68,nat Ga, 56,57,58 Co. 65 Zn, nat Ni and nat Cu electrolyte;
[0075] The structure of the solid Ga4Ni alloy target is as follows:
[0076] It comprises two layers, specifically comprising a metal base layer and a solid gallium-nickel alloy layer connected in sequence, wherein the material of the metal base layer is Ta metal;
[0077] The solid gallium-nickel alloy layer is prepared by electroplating, and the mass content of Ga in the solid gallium-nickel alloy layer is 60%, and the thickness is 20 mg / cm 2 , wherein the preparation method comprises:
[0078] A1: Dissolve metallic gallium in a 9M HNO3 solution, heat and stir, then add a 98% H2SO4 solution to obtain a Ga2(SO4)3 precipitate;
[0079] A2: dissolving the Ga2(SO4)3 precipitate obtained in step A1 in water, adjusting the pH value of the solution to 2 with an ammonia solution, heating the solution to 40° C., and adding NiSO4 to prepare a final electroplating solution, wherein the weight ratio of the NiSO4 to the metal gallium is 10:15;
[0080] A3: Use constant current electrolysis technology for electrodeposition and adjust the current density to 20mA / cm 2, the temperature was 25°C, and the rotation and stirring speed was maintained at about 300 rpm during the electroplating process. After 6 hours, a Ga4Ni alloy target was obtained.
[0081] S2: passing the electrolyte obtained in step S1 into a series of chromatographic columns for separation and purification, wherein the series of chromatographic columns are a hydroxamate resin separation column, a cross-linked polydivinylbenzene resin separation column and an AG MP-50 resin separation column, and collecting the electrolyte containing 68 Ge solution, completing the preparation.
[0082] The step of passing the electrolyte into a series of chromatographic columns for separation and purification comprises:
[0083] B1: The electrolyte is diluted to a H2SO4 concentration of 5M and then subjected to a separation treatment, the separation treatment comprising: passing the isohydroxamate resin separation column, eluting with 4M H2SO4 and collecting the elution waste liquid, and then desorbing the elution waste liquid with 0.08M dilute citric acid to obtain a desorption liquid, and adding 5M H2SO4 to the desorption liquid; after the separation treatment is completed, adding 9-10M HCl to the desorption liquid for acidification;
[0084] B2: Pass a cross-linked polydivinylbenzene resin separation column into the desorption liquid acidified in step B1, and elute with 9M HCl and collect the elution waste liquid at the same time, then use deionized water to desorb the elution waste liquid to obtain a pure water desorption liquid; finally, pass the pure water desorption liquid into an AG MP-50 resin separation column, add 0.2M HCl for further desorption, collect the Ge-68 product, and complete the preparation.
[0085] Embodiment 2:
[0086] This embodiment provides a method for producing high-purity Ge-68 using a high-current proton cyclotron, comprising:
[0087] A method for preparing high-purity Ge-68 using a high-current proton cyclotron comprises the following steps:
[0088] S1: preparing a fixed Ga4Ni alloy target, and subjecting the alloy target to high-current proton irradiation treatment, wherein the conditions for the high-current proton irradiation treatment are: using a high-current proton accelerator for irradiation, the energy is 24 MeV, the current is 175 μA, the time is 5 days, and the cooling time is 30 days;
[0089] Then, sulfuric acid electrolysis is performed to obtain 68 Ge, 68,nat Ga, 56,57,58 Co. 65 Zn, nat Ni and natCu electrolyte;
[0090] The structure of the solid Ga4Ni alloy target is as follows:
[0091] It comprises three layers, specifically a metal base layer, a metal protection layer and a solid gallium-nickel alloy layer which are connected in sequence. The material of the metal base layer is Cu; the material of the metal protection layer is Au, and the thickness is 5 μm.
[0092] The solid gallium-nickel alloy layer is prepared by electroplating, and the mass content of Ga in the solid gallium-nickel alloy layer is 65%, and the thickness is 25 mg / cm 2 , wherein the preparation method comprises:
[0093] A1: Dissolve metallic gallium in a 10.5M HNO3 solution, heat and stir, then add a 98.5% H2SO4 solution to obtain a Ga2(SO4)3 precipitate;
[0094] A2: dissolving the Ga2(SO4)3 precipitate obtained in step A1 in water, adjusting the pH value of the solution to 2.3 with an ammonia solution, heating the solution to 45° C., adding NiSO4 to prepare a final electroplating solution, wherein the weight ratio of the NiSO4 to the metal gallium is 12.5:17.5;
[0095] A3: Use constant current electrolysis technology for electrodeposition and adjust the current density to 40mA / cm 2 , the temperature was 62.5°C, and the rotation and stirring speed was maintained at about 550 rpm during the electroplating process. After 7 hours, a Ga4Ni alloy target was obtained.
[0096] S2: passing the electrolyte obtained in step S1 into a series of chromatographic columns for separation and purification, wherein the series of chromatographic columns are a hydroxamate resin separation column, a cross-linked polydivinylbenzene resin separation column and an AG MP-50 resin separation column, and collecting the electrolyte containing 68 Ge solution, completing the preparation.
[0097] The step of passing the electrolyte into a series of chromatographic columns for separation and purification comprises:
[0098] B1: diluting the electrolyte to a H2SO4 concentration of 6.5M and then performing two separation treatments, the separation treatments comprising: passing the isohydroxamate resin separation column, eluting with 4.5M H2SO4 and collecting the elution waste liquid, and then desorbing the elution waste liquid with 0.115M dilute citric acid to obtain a desorption liquid, and adding 6.5M H2SO4 to the desorption liquid; after the separation treatment is completed, adding 9.5M HCl to the desorption liquid for acidification;
[0099] B2: Pass a cross-linked polydivinylbenzene resin separation column into the desorption liquid acidified in step B1, and elute with 9.5M HCl and collect the elution waste liquid at the same time, then use deionized water to desorb the elution waste liquid to obtain a pure water desorption liquid; finally, pass the pure water desorption liquid into an AG MP-50 resin separation column, add 0.35M HCl for further desorption, collect the Ge-68 product, and complete the preparation.
[0100] Embodiment 3:
[0101] This embodiment provides a method for producing high-purity Ge-68 using a high-current proton cyclotron, comprising:
[0102] A method for preparing high-purity Ge-68 by using high-current proton cyclotron comprises the following steps:
[0103] S1: preparing a fixed Ga4Ni alloy target, and subjecting the alloy target to high-current proton irradiation treatment, wherein the conditions for the high-current proton irradiation treatment are: using a high-current proton accelerator for irradiation, with an energy of 30 MeV, a current of 300 μA, a time of 15 days, and a cooling time of 40 days;
[0104] Then, sulfuric acid electrolysis is performed to obtain 68 Ge, 68,nat Ga, 56,57,58 Co. 65 Zn, nat Ni and nat Cu electrolyte;
[0105] The structure of the solid Ga4Ni alloy target is as follows:
[0106] The invention comprises two layers, specifically a metal base layer and a solid gallium-nickel alloy layer connected in sequence, wherein the metal base layer is made of Ta metal; the solid gallium-nickel alloy layer is prepared by electroplating, and the mass content of Ga in the solid gallium-nickel alloy layer is less than 70%, and the thickness is 30 mg / cm 2 , wherein the preparation method comprises:
[0107] A1: Dissolve metallic gallium in a 12M HNO3 solution, heat and stir, then add a 99% H2SO4 solution to obtain a Ga2(SO4)3 precipitate;
[0108] A2: dissolving the Ga2(SO4)3 precipitate obtained in step A1 in water, adjusting the pH value of the solution to 2.5 with an ammonia solution, heating the solution to 50° C., adding NiSO4 to prepare a final electroplating solution, wherein the weight ratio of the NiSO4 to the metal gallium is 15:20;
[0109] A3: Use constant current electrolysis technology for electrodeposition and adjust the current density to 60mA / cm 2 , the temperature is 100°C, and the rotation and stirring speed is maintained at about 800 rpm during the electroplating process. After 8 hours, a Ga4Ni alloy target is obtained.
[0110] S2: passing the electrolyte obtained in step S1 into a series of chromatographic columns for separation and purification, wherein the series of chromatographic columns are a hydroxamate resin separation column, a cross-linked polydivinylbenzene resin separation column and an AG MP-50 resin separation column, and collecting the electrolyte containing 68 Ge solution, completing the preparation.
[0111] The step of passing the electrolyte into a series of chromatographic columns for separation and purification comprises:
[0112] B1: diluting the electrolyte to a H2SO4 concentration of 8M and then performing at least one separation treatment, the separation treatment comprising: passing the isohydroxamate resin separation column, eluting with 4-5M H2SO4 and collecting the elution waste liquid, and then desorbing the elution waste liquid with 0.15M dilute citric acid to obtain a desorption liquid, and adding 8M H2SO4 to the desorption liquid; after the separation treatment is completed, adding 10M HCl to the desorption liquid for acidification;
[0113] B2: Pass a cross-linked polydivinylbenzene resin separation column into the desorption liquid acidified in step B1, and elute with 10M HCl and collect the elution waste liquid at the same time, then use deionized water to desorb the elution waste liquid to obtain a pure water desorption liquid; finally, pass the pure water desorption liquid into an AG MP-50 resin separation column, add 0.5M HCl for further desorption, collect the Ge-68 product, and complete the preparation.
[0114] Based on the method of producing high-purity Ge-68 by a high-current proton cyclotron, the following embodiment of the present invention provides a method based on a cartridge design. 68 Ge separation automation system solution, such as Figure 2 As shown, it includes a liquid extraction unit, a conveying unit, a separation unit, a collection unit and a control unit. 68 There are many steps in the separation of Ge nuclides. A disposable cartridge with 18 holes is designed, which is composed of three 6-way 3-way valves. The process uses 16 holes. The liquid extraction unit and the collection unit include several liquid storage containers and liquid delivery pipelines; the delivery unit includes at least one injection pump and three 6-way 3-way valves; the separation unit includes at least three identical or different separation columns; the collection unit includes several collection containers and liquid recovery pipelines; the control unit includes a host computer, a programmable logic controller (PLC), control software and communication protocols, specifically including:
[0115] Example 4
[0116] S1: Preparation of Ga4Ni alloy target by electroplating
[0117] A1: Dissolve 18g of metallic gallium in 10M HNO3, keep heating and stirring, then add 98% H2SO4 to obtain precipitated Ga2(SO4)3;
[0118] A2: Dissolve the Ga2(SO4)3 precipitate in water and adjust the pH of the solution to 2 with ammonia solution. Heat the solution to 45°C and add 12g NiSO4 to prepare the final plating solution. The final volume of the plating solution is 450mL.
[0119] A3: Ga-Ni is electroplated using constant current electrolysis technology with a current density adjusted to 25 mA / cm 2 , the temperature is 60°C, and the rotation and stirring speed is maintained at about 500 rpm during the electroplating process. After 8 hours, a Ga4Ni alloy target is obtained.
[0120] The radioactive Ga4Ni alloy target was prepared by irradiating the Ga4Ni alloy target with ACSI-FLEX 30MeV. 68 Ge alloy target; Ga4Ni alloy target after irradiation by sulfuric acid electrolysis using the reverse process of electroplating.
[0121] S2: Separation and purification of electrolyte using series chromatography columns, which includes the following automated control steps:
[0122] B1:
[0123] Electrolyte loading Zr resin: dilute the H2SO4 concentration of the solid target after electrolysis to 5M, and then inject it into the separation device stock solution bottle A1. Connect the A1-V1-V2-P1 loop, and the injection pump extracts the electrolytic dilution from the stock solution bottle A1; connect the P1-V2-V3-V4-V5-V6-V7-V8-Zr resin-V9-V10-V11-V12-V13-waste liquid bottle A3 loop, and the injection pump injects the electrolytic dilution into the waste liquid bottle A3. 68 Ge combines with the isohydroxamate ester group and is loaded onto the Zr resin separation column, and the waste liquid flows into the waste liquid bottle A3; the nitrogen source-V1-V2-V3-V4-V5-V6-V7-V8-Zr resin-V9-V10-V11-V12-V13-waste liquid bottle A3 loop is turned on, nitrogen purges the liquid loop, and the residual electrolytic waste liquid flows into the waste liquid bottle A3.
[0124] Sulfuric acid elution: open the P1-V2-V3-B1 loop, and the injection pump extracts 5M H2SO4 from B1; open the P1-V2-V3-V4-V5-V6-V7-V8-Zr resin-V9-V10-V11-V12-V13-waste liquid bottle A3 loop, and the injection pump injects 4M H2SO4 to elute the Zr resin separation column, and the waste liquid flows into the waste liquid bottle A3; open the nitrogen source-V1-V2-V3-V4-V5-V6-V7-V8-Zr resin-V9-V10-V11-V12-V13-waste liquid bottle A3 loop, and nitrogen purges the liquid loop. The residual elution waste liquid flows into the waste liquid bottle A3. The sulfuric acid elution waste liquid contains a large amount of Ga, Ni, Co, and Zn inorganic impurities.
[0125] Citric acid desorption: connect the P1-V2-V3-V4-B2 loop, and use the injection pump to extract 0.1M dilute citric acid from B2; connect the P1-V2-V3-V4-V5-V6-V7-V8-Zr resin-V9-V10-desorption bottle A2 loop, and use the injection pump to inject 0.1M dilute citric acid. 68 Ge is complexed with citric acid and desorbed from the Zr resin separation column. 68 The Ge desorption liquid flows into the desorption bottle A2; the nitrogen source-V1-V2-V3-V4-V5-V6-V7-V8-Zr resin-V9-V10-desorption bottle A2 loop is turned on, the nitrogen purges the liquid loop, and the residual desorption liquid flows into the desorption bottle A2.
[0126] Zr resin circulation: turn on the P1-V2-V3-B1 loop, and use the injection pump to extract 5M H2SO4 from B1; turn on the P1-V2-V3-V4-V5-V6-V7-V8-V9-V10-desorption bottle A2 loop, and use the injection pump to pump 5M H2SO4 is injected into the desorption bottle A2 to adjust the pH value; the P1-V2-V3-V4-V5-V6-V7-V8-V9-V10-desorption bottle A2 loop is opened, and the injection pump extracts the desorption liquid after adjusting the pH; the P1-V2-V3-V4-V5-V6-V7-V8-Zr resin-V9-V10-V11-V12-V13-waste liquid bottle A3 loop is opened, and the injection pump loads the desorption liquid after adjusting the pH on the Zr resin separation column again, and the waste liquid flows into the waste liquid bottle A3; the nitrogen source-V1-V2-V3-V4-V5-V6-V7-V8-Zr resin-V9-V10-V11-V12-V13-waste liquid bottle A3 loop is opened, and nitrogen purges the liquid loop, and the residual waste liquid flows into the waste liquid bottle A3. According to the actual situation, sulfuric acid elution and citric acid desorption can be carried out, and the separation cycle can be 0-2 times.
[0127] B2:
[0128] Desorption liquid loaded Guard resin: open the P1-V2-V3-V4-V5-B3 loop, and use the injection pump to extract 9M HCl from B3; open the P1-V2-V3-V4-V5-V6-V7-V8-V9-V10-desorption bottle A2 loop, and use the injection pump to pump 9M HCl is injected into desorption bottle A2 to adjust the pH value; the P1-V2-V3-V4-V5-V6-V7-V8-V9-V10-desorption bottle A2 loop is opened, and the injection pump extracts the desorption liquid after adjusting the pH; the P1-V2-V3-V4-V5-V6-V7-V8-V9-V10-V11-Guard resin-V12-V13-waste liquid bottle A3 loop is opened, and the injection pump injects the desorption liquid after adjusting the pH with hydrochloric acid, loads the Guard resin separation column, and the waste liquid flows into the waste liquid bottle A3; the nitrogen source-V1-V2-V3-V4-V5-V6-V7-V8-V9-V10-V11-Guard resin-V12-V13-waste liquid bottle A3 loop is opened, nitrogen gas is purged into the liquid loop, and the residual waste liquid flows into the waste liquid bottle A3.
[0129] Hydrochloric acid elution: open the P1-V2-V3-V4-V5-B3 loop, and use the injection pump to extract 9M HCl from B3; open the P1-V2-V3-V4-V5-V6-V7-V8-V9-V10-V11-Guard resin-V12-V13-waste liquid bottle A3 loop, and use the injection pump to inject 9M HCl to elute the Guard resin separation column, replace the acidic medium, wash the sulfate and citric acid, and the waste liquid flows into the waste liquid bottle A3; open the nitrogen source-V1-V2-V3-V4-V5-V6-V7-V8-V9-V10-V11-Guard resin-V12-V13-waste liquid bottle A3 loop, and use nitrogen to purge the liquid loop, and the residual eluent flows into the waste liquid bottle A3. The waste liquid from hydrochloric acid elution contains a large amount of sulfuric acid, citric acid and organic impurities.
[0130] Pure water desorption and loading of AG MP-50 resin: open the P1-V2-V3-V4-V5-V6-B4 loop, and use the injection pump to extract pure water from B4; open the P1-V2-V3-V4-V5-V6-V7-V8-V9-V10-V11-Guard resin-V12-V13-V14-AG MP 50 resin-V15-V16-waste liquid bottle A4 loop, and use the injection pump to inject pure water. 68Ge is hydrolyzed to desorb from the Guard resin separation column, the desorption liquid is loaded on the AG MP-50 resin, and the waste liquid flows into the waste liquid bottle A3; the nitrogen source-V1-V2-V3-V4-V5-V6-V7-V8-V9-V10-V11-Guard resin-V12-V13-V14-AG MP 50 resin-V15-V16-waste liquid bottle A4 loop is turned on, and the nitrogen purges the liquid loop, and the residual waste liquid flows into the waste liquid bottle A3. The pure water desorption liquid is passed into the AG MP-50 resin separation column to further separate trace impurities such as Fe, Ni, Cu, Zn, and Pb.
[0131] Desorption with dilute hydrochloric acid: Open the P1-V2-V3-V4-V5-V6-V7-B5 loop, and use the injection pump to extract 0.2M HCl from B5; open the P1-V2-V3-V4-V5-V6-V7-V8-V9-V10-V11-V12-V13-V14-AG MP 50 resin-V15-V16-product bottle A5 loop, and use the injection pump to inject dilute hydrochloric acid. 68 Ge is acidified to desorb from the AG MP-50 resin separation column and the product is collected in a bottle 68 Ge product, which is a hydrochloric acid medium with suitable acidity and can be directly used to prepare Ge-Ga generator without further purification.
[0132] exist 68 After Ge purification was completed, the 68 Ge was used for relevant determination to determine the amount of specific metal ions and organic compounds in the final product. As shown in Tables 1 and 2, it can be seen that the contents of several common metal ions in the target material, target holder and mineral acid are extremely low, and the contents of possible solvents, mineral oils, resin decomposition products or organic acids in several common extraction or column chromatography separation methods are all below the detection limit (DL) and are not detected, which meets the standard requirements.
[0133] The measurement results are shown in Table 1 and Table 2 below:
[0134] Among them, sample I, sample II, and sample III correspond to the finished products of embodiment 2, embodiment 1, and embodiment 3 of the present invention respectively.
[0135] Table 1:
[0136]
[0137] Table 2:
[0138]
[0139] In the description of the embodiments of the present application, it should be noted that in the description of the present application, terms such as "inside" and "outside" indicating directions or positional relationships are based on the directions or positional relationships shown in the drawings. This is only for the convenience of description, and does not indicate or imply that the device or component must have a specific orientation, be constructed and operated in a specific orientation. Therefore, it cannot be understood as a limitation on the present application.
[0140] In the description of the present application, the description with reference to the terms "one embodiment", "some embodiments", "in the present embodiment", "specific example", or "some examples" etc. means that the specific features, mechanisms, materials or characteristics described in conjunction with the embodiment or example are included in at least one embodiment or example of the present application. In this specification, the schematic representations of the above terms do not necessarily refer to the same embodiment or example. Moreover, the specific features, mechanisms, materials or characteristics described may be combined in a suitable manner in any one or more embodiments or examples. In addition, those skilled in the art may combine and combine the different embodiments or examples described in this specification and the features of the different embodiments or examples, without contradiction.
[0141] The above is only a specific implementation of the present application, but the protection scope of the present application is not limited thereto. Any changes or substitutions that can be easily thought of by a person skilled in the art within the technical scope disclosed in the present application should be included in the protection scope of the present application. Therefore, the protection scope of the present application shall be based on the protection scope of the claims.
Claims
1. A method for preparing high-purity Ge-68 using a high-current proton cyclotron, characterized in that: The following steps are involved: S1: Prepare a fixed Ga4Ni alloy target, treat the alloy target with high-current proton irradiation, and then electrolyze and dissolve it in sulfuric acid to obtain a 68 Ge, 68,nat Ga, 56,57,58 Co. 65 Zn, nat Ni and nat Cu electrolyte; S2: passing the electrolyte obtained in step S1 into a series of chromatographic columns for separation and purification, wherein the series of chromatographic columns are a hydroxamate resin separation column, a cross-linked polydivinylbenzene resin separation column and an AG MP-50 resin separation column, and collecting the electrolyte containing 68 Ge solution, completing the preparation.
2. The method for preparing high-purity Ge-68 using a high-current proton cyclotron according to claim 1, characterized in that: In step S1, the conditions of the high-current proton irradiation treatment are: using a high-current proton accelerator for irradiation, the energy is 18-30 MeV, the current is 50-300 μA, the time is greater than or equal to 3 hours, and the cooling time is greater than or equal to 20 days.
3. The method for preparing high-purity Ge-68 using a high-current proton cyclotron according to claim 1, characterized in that: In the step S1, the structure of the solid Ga4Ni alloy target is as follows 1) or 2): 1) comprising at least two layers, including a metal substrate layer and a solid gallium-nickel alloy layer connected in sequence; 2) at least three layers, including a metal base layer, a metal protection layer and a solid gallium-nickel alloy layer connected in sequence; In 1), the material of the metal base layer is Ta, Ti, Nb or Inconel alloy; In the above 2), the material of the metal base layer is Cu or Al; The metal protection layer is made of Au or Pt and has a thickness of more than 5 μm.
4. The method for preparing high-purity Ge-68 using a high-current proton cyclotron according to claim 3, characterized in that: The solid gallium-nickel alloy layer has a Ga content of not less than 60% by mass and a thickness of more than 20 mg / cm 2 .
5. The method for preparing high-purity Ge-68 using a high-current proton cyclotron according to claim 3, characterized in that: The solid gallium-nickel alloy layer is prepared by electroplating, and the preparation method comprises: A1: Dissolve metallic gallium in HNO3 solution, heat and stir, then add H2SO4 solution with a concentration of more than 98% to obtain Ga2(SO4)3 precipitate; A2: dissolving the Ga2(SO4)3 precipitate obtained in step A1 in water, adjusting the pH value of the solution to 2-2.5 with an ammonia solution, heating the solution to 40-50° C., and adding NiSO4 to prepare a final electroplating solution; A3: Use constant current electrolysis technology for electrodeposition, and adjust the current density to 20-60mA / cm 2 , the temperature is 25-100°C, and the speed of rotation and stirring is maintained at about 300-800rpm during the electroplating process. After 6-8 hours, a Ga4Ni alloy target is obtained.
6. The method for preparing high-purity Ge-68 using a high-current proton cyclotron according to claim 4, characterized in that: In the step A1, the weight ratio of the metal gallium to the NiSO4 is (15-20): (10-15); the concentration of the HNO3 solution is 9-12M.
7. The method for preparing high-purity Ge-68 using a high-current proton cyclotron according to claim 1, characterized in that: In step S2, the step of passing the electrolyte into a series of chromatographic columns for separation and purification comprises: B1: diluting the electrolyte and performing at least one separation treatment, wherein the separation treatment comprises: passing the electrolyte into the isohydroxamate resin separation column, eluting with H2SO4 and collecting the elution waste liquid, desorbing the elution waste liquid with dilute citric acid to obtain a desorption liquid, and adding H2SO4 to the desorption liquid; after the separation treatment is completed, adding HCl to the desorption liquid for acidification; B2: Pass a cross-linked polydivinylbenzene resin separation column into the desorption liquid acidified in step B1, and elute with HCl while collecting the elution waste liquid, then use deionized water to desorb the elution waste liquid to obtain a pure water desorption liquid; finally, pass the pure water desorption liquid into an AG MP-50 resin separation column, add HCl for further desorption, collect the Ge-68 product, and complete the preparation.
8. The method for preparing high-purity Ge-68 using a high-current proton cyclotron according to claim 7, characterized in that: The separation process is performed 1 to 3 times.
9. The method for preparing high-purity Ge-68 using a high-current proton cyclotron according to claim 7, characterized in that: In the step B1, the electrolyte is diluted to a concentration of 5-8M H2SO4; in the elution with H2SO4, the concentration of H2SO4 is 4-5M; the concentration of the dilute citric acid is 0.08-0.15M; when H2SO4 is added to the desorption solution, the concentration of H2SO4 is 5-8M; the concentration of HCl is 9-10M.
10. The method for preparing high-purity Ge-68 using a high-current proton cyclotron according to claim 7, characterized in that: In the step B2, the concentration of HCl in the elution with HCl is 9-10M; the concentration of HCl in the further desorption with HCl is 0.2-0.5M.
Citation Information
Patent Citations
Preparation method for radioactive 68Ge solution
CN102382994A
METHOD FOR THE MANUFACTURE OF HIGHLY PURIFIED 68Ge MATERIAL FOR RADIOPHARMACEUTICAL PURPOSES
CN110612272A
A method for production and preparation based on accelerator irradiation 68 Ge's method
CN114937516A
Cited By
Solid target system for simultaneously producing Ge-68 nuclides and PET nuclides under high-power beam
CN119170316A
A solid target system for simultaneous production of Ge-68 and PET nuclides under high power beam
CN119170316B