Lightweight composite material gas storage device and production method thereof

By designing the inner liner and composite material layers, the problems of heavy metal gas storage tanks and poor welding were solved, resulting in a lightweight gas storage device with high pressure resistance, and the welding is solid, meeting high pressure requirements.

CN118998588AInactive Publication Date: 2024-11-22ZHEJIANG SHIDING RUBBER IND CO LTD
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
CN202411278690.7
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-09-12
Publication Date
2024-11-22
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

The metal air tanks in existing automotive braking systems are heavy, prone to rust, and have problems such as weak welding, incomplete welding, and missing welding at the welded parts, which cannot meet the pressure resistance requirements.

Method used

The design incorporates an inner liner and a composite material layer. The inner liner is formed by welding an upper shell and a lower shell, and is covered with a composite material layer. The composite material layer is prepared by a winding molding process and then coated with epoxy resin to improve pressure resistance and reduce weight.

Benefits of technology

The gas storage device achieves lightweighting and weight reduction, significantly improves pressure resistance, has robust welding, meets high-pressure requirements, and enhances overall performance.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118998588A_ABST
    Figure CN118998588A_ABST
Patent Text Reader

Abstract

The invention relates to the technical field of gas storage devices, and discloses a light-weight composite material gas storage device and a production method thereof.The gas storage device comprises an inner container and a composite material layer, the inner container comprises an upper shell and a lower shell, the upper shell and the lower shell are welded to form the inner container, and the composite material layer wraps the outer portion of the inner container; the manufacturing method comprises an inner container preparation step and a composite material layer preparation step, the inner container preparation step comprises the steps of preparing an upper shell and a lower shell respectively and welding the upper shell and the lower shell to form the inner container, and the composite material layer preparation step comprises the steps of coating the outer part of the inner container with a composite material layer and covering a welding bead with the composite material layer. The upper shell and the lower shell are welded, so that the precision of the upper shell and the lower shell is conveniently controlled, the liner meeting the enough precision requirement is conveniently obtained, then the liner is externally coated with the composite material layer, the pressure resistance of the gas storage device is improved by utilizing the composite material layer, the weight reduction effect is obvious, the light weight of the whole vehicle is conveniently realized, and the cost is reduced. And meanwhile, the pressure-resistant performance is good.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the technical field of gas storage devices, and in particular to a lightweight composite material gas storage device and a production method thereof. Background Art

[0002] The air tank is a gas pressure device in the automobile braking system, which is used to store the gas compressed by the air compressor (air pump). The air tank has four major functions: energy storage, filtration, voltage stabilization and temperature reduction. The existing air tanks for automobile brake devices are formed by metal (iron or aluminum alloy) stamping and welding. They are heavy. The iron material will rust when exposed to the outside of the car. Due to the presence of moisture in the compressed air, the air tank will rust and become ineffective. The air tank is usually set in two parts, which are welded after being produced separately. However, there are problems such as loose welding, false welding, leaking welding, welding stress, etc. at the welding site, which cannot meet the pressure resistance requirements. Summary of the invention

[0003] In view of the deficiencies in the prior art, the object of the present invention is to provide a lightweight composite material gas storage device and a production method thereof, which has the characteristics of being lightweight, having good weight reduction effect, and having high pressure resistance.

[0004] To achieve the above object, the present invention provides the following technical solutions:

[0005] A lightweight composite material gas storage device, comprising

[0006] The liner comprises an upper shell and a lower shell, and the upper shell and the lower shell are welded to form the liner;

[0007] A composite material layer is coated on the outside of the liner.

[0008] A method for manufacturing a lightweight composite gas storage device, providing a lightweight composite gas storage device, comprising an inner liner and a composite material layer, wherein the inner liner comprises an upper shell and a lower shell, the upper shell and the lower shell are welded to form the inner liner, and the composite material layer is coated on the outside of the inner liner;

[0009] The manufacturing method comprises

[0010] Inner liner preparation step: prepare an upper shell and a lower shell respectively, and weld the upper shell and the lower shell to form an inner liner;

[0011] The composite material layer preparation step is: coating the composite material layer on the outside of the liner, wherein the composite material layer covers the weld bead.

[0012] Furthermore, an annular connecting portion is formed on both the upper shell and the lower shell, the shapes of the two connecting portions are adapted to each other, and one of the connecting portions is sleeved on the outside of the other connecting portion.

[0013] Furthermore, the upper shell and the lower shell are injection molded respectively, the upper shell is provided with a drain port and a plurality of air inlets and outlets, the upper shell and the positions corresponding to the drain port and the air inlets and outlets are respectively pre-embedded with inserts, and the drain port and the air inlets and outlets are respectively connected by threads.

[0014] Furthermore, the insert is configured to be made of metal material, and the metal material includes aluminum alloy.

[0015] Furthermore, the composite material layer covers the connection portion between the upper shell and the lower shell, and the connection portion between the insert and the upper shell.

[0016] Furthermore, the upper shell and the lower shell are injection molded separately.

[0017] Furthermore, the inner shell is subjected to a pressure holding test after welding, and is required to meet the pressure holding of 1 bar@1 min and the leakage volume <25 ml / min.

[0018] Furthermore, the composite material layer is specifically prepared by a winding molding process, and the winding molding process includes a wet winding molding process and a dry winding molding process.

[0019] Furthermore, the manufacturing method also includes a surface treatment step, which includes polishing the composite material layer, then spraying epoxy resin on the surface of the composite material layer, and polishing again after curing to obtain a gas storage device with a smooth surface.

[0020] Beneficial effects of the present invention:

[0021] The present invention facilitates the control of the precision of the upper shell and the lower shell by welding between the upper shell and the lower shell, and the connection is convenient, so that an inner liner with sufficient precision requirements can be obtained. Then, a composite material layer is coated on the outside of the inner liner, and the composite material layer is used to improve the pressure resistance of the gas storage device. Compared with the existing metal gas storage devices on the market, the composite material gas storage device has obvious weight reduction effect, which is convenient for achieving lightweight of the entire vehicle and has good pressure resistance. The composite material is heated and cured by a winding molding process, which is convenient for relieving the stress of the inner liner and improving the overall performance of the gas storage device. BRIEF DESCRIPTION OF THE DRAWINGS

[0022] Figure 1 It is a schematic diagram of the overall structure of the lightweight composite material gas storage device of the present invention;

[0023] Figure 2 It is a schematic diagram of the overall cross-sectional structure of the lightweight composite material gas storage device of the present invention;

[0024] Figure 3It is a schematic diagram of the production process of the manufacturing method of the lightweight composite material gas storage device of the present invention;

[0025] Figure 4 It is a schematic diagram of the process of the winding molding process in the present invention.

[0026] Reference numerals:

[0027] 1. Inner liner; 2. Upper shell; 3. Lower shell; 4. Composite material layer; 5. Air inlet and outlet; 6. Drain outlet. DETAILED DESCRIPTION

[0028] The present invention is further described in detail below in conjunction with the accompanying drawings and embodiments. The same parts are represented by the same reference numerals. It should be noted that the words "front", "rear", "left", "right", "upper" and "lower" used in the following description refer to directions in the accompanying drawings, and the words "bottom surface" and "top surface", "inner" and "outer" refer to directions toward or away from the geometric center of a specific component, respectively.

[0029] like Figure 1-Figure 2 As shown, a lightweight composite gas storage device of this embodiment includes an inner liner 1 and a composite material layer 4. The inner liner 1 includes an upper shell 2 and a lower shell 3, and the upper shell 2 and the lower shell 3 are welded to form the inner liner 1. The composite material layer 4 is coated on the outside of the inner liner 1.

[0030] An annular connection portion is formed on both the upper shell 2 and the lower shell 3. The shapes of the two connection portions are adapted, and one connection portion is sleeved outside the other connection portion. The provision of the annular connection portion facilitates increasing the contact area between the upper shell 2 and the lower shell 3, making the welding stable, thereby providing a stable connection effect.

[0031] In this embodiment, the upper shell 2 and the lower shell 3 are respectively manufactured by injection molding. Alternatively, they can be manufactured by rotational molding or extrusion molding. However, the inner liner 1 obtained by rotational molding or extrusion molding has poor manufacturing accuracy and sealing performance, which is lower than that of the injection molding process.

[0032] The upper shell 2 is provided with a drain port 6 and a plurality of air inlets and outlets 5. In order to facilitate connection, inserts are pre-buried in the upper shell 2 and the corresponding parts of the drain port 6 and the air inlets and outlets 5. The setting of the insert will not affect the injection molding process, that is, it will not affect the molding process of the upper shell 2, and the connection between the insert and the upper shell 2 is stable, which can ensure the sealing performance and is easy to implement. The inserts corresponding to the drain port 6 and the air inlets and outlets 5 are threadedly connected. The insert is provided with an internal thread, and the air inlets and outlets 5, the drain port 6 and the insert are connected by threaded connection. The connection is convenient and it is easy to obtain good sealing performance. In this embodiment, the insert is set to a metal material, and the insert will not be deformed during the injection molding process, and the injection temperature has little effect on the insert. In addition, in the selection of the material of the insert, considering that the deformation difference between the metal material and the plastic cannot be too large, a material with a thermal expansion coefficient close to that of the upper shell 2 material is selected, and the selected metal material includes aluminum alloy. The composite material layer 4 covers the connection part between the upper shell 2 and the lower shell 3, and the connection part between the insert and the upper shell 2.

[0033] The upper and lower shells 3 are formed into an integral gas storage device liner 1 through a laser welding process, which can meet the pressure maintenance of 1 bar@1 min and the leakage is less than 25 ml / min.

[0034] like Figure 3 and Figure 4 As shown, a method for manufacturing a lightweight composite material gas storage device includes an inner liner preparation step, a composite material layer 4 preparation step and a surface treatment step.

[0035] The inner liner preparation step includes preparing an upper shell 2 and a lower shell 3 respectively, and welding the upper shell 2 and the lower shell 3 to form an inner liner 1;

[0036] The step of preparing the composite material layer 4 includes coating the composite material layer 4 on the outside of the liner 1, wherein the composite material layer 4 covers the weld bead;

[0037] The surface treatment step includes polishing the composite material layer 4, and then spraying epoxy resin on the surface of the composite material layer 4, and polishing again after curing to obtain a gas storage device with a smooth surface.

[0038] In the liner preparation step, the upper and lower shells 3 are processed by injection molding, and when preparing the upper shell 2, an insert is preset in the mold of the upper shell 2. The sealing can be ensured by installing the metal insert and the screws of the counterpart. The upper shell 2 and the metal insert have different thermal expansion coefficients due to different materials, so through the embedded structure design, a metal material with a thermal expansion coefficient close to that of the upper shell 2 material is selected. After the liner 1 is formed by welding, the liner 1 needs to be pressure tested. After the liner 1 is welded, a pressure test is performed, which requires a pressure of 1 bar @ 1 min and a leakage of < 25 ml / min.

[0039] In the step of preparing the composite material layer 4, the composite material layer 4 is specifically prepared by a winding molding process, and the winding molding process includes a wet winding molding process and a dry winding molding process. The step of preparing the composite material layer 4 can increase the pressure resistance, and the pressure resistance can reach 62.5 bar after winding molding. In the preparation process of the composite material layer 4, a fiber material is specifically used, and the fiber material impregnated with resin is cross-wound on the outside of the inner liner 1, and heated and cured after the winding is completed. The fiber material can be glass fiber, basalt fiber, carbon fiber or a mixed fiber thereof. It can meet the pressure resistance requirements. At present, the thickness of the composite material layer 4 is 1.5 mm.

[0040] In the surface treatment step, the first grinding is to make the surface regular and rough, increase the contact area between the composite material layer 4 and the epoxy resin, so that the connection effect is good and the coating is not easy to fall off. Then the epoxy resin is sprayed on the surface of the composite material layer 4, and the second grinding is performed after curing. The purpose of the second grinding is to improve the smoothness of the surface to obtain a gas storage device with a smooth surface.

[0041] The gas storage device produced by the above method has the following characteristics:

[0042] 1. Good weight reduction effect: The gas storage device is formed by non-metallic materials. Compared with the lightest aluminum alloy gas storage device among the existing metal materials on the market, the composite material gas storage device can reduce the weight of 40L gas storage device by 35%, and the 50L gas storage device can reduce shock by 40%. Considering the lightweight of the whole vehicle, the product is more competitive in the market;

[0043] 2. Good pressure resistance, able to meet the pressure requirements of gas storage devices, and the pressure resistance can reach 62.5 bar after winding.

[0044] The above are only preferred embodiments of the present invention. The protection scope of the present invention is not limited to the above embodiments. All technical solutions under the concept of the present invention belong to the protection scope of the present invention. It should be pointed out that for ordinary technicians in this technical field, some improvements and modifications without departing from the principle of the present invention should also be regarded as the protection scope of the present invention.

Claims

1. A lightweight composite material gas storage device, Features: include An inner liner (1), the inner liner (1) comprising an upper shell (2) and a lower shell (3), the upper shell (2) and the lower shell (3) being welded to form the inner liner (1); A composite material layer (4), the composite material layer (4) being coated on the outside of the inner liner (1).

2. A lightweight composite material gas storage device according to claim 1, Features: An annular connecting portion is formed on both the upper shell (2) and the lower shell (3), the two connecting portions are matched in shape, and one of the connecting portions is sleeved on the outside of the other connecting portion.

3. A lightweight composite material gas storage device according to claim 1, Features: The upper shell (2) and the lower shell (3) are respectively injection molded, and the upper shell (2) is provided with a drain port (6) and a plurality of air inlets and outlets (5). Inserts are respectively pre-buried at the positions of the upper shell (2) corresponding to the drain port (6) and the air inlets and outlets (5), and the drain port (6) and the air inlets and outlets (5) are respectively connected by threads corresponding to the inserts.

4. A lightweight composite material gas storage device according to claim 3, Features: The insert is configured to be made of a metal material, and the metal material includes an aluminum alloy.

5. A lightweight composite material gas storage device according to claim 1, Features: The composite material layer (4) covers the connection portion between the upper shell (2) and the lower shell (3), and the connection portion between the insert and the upper shell (2).

6. A method for manufacturing a lightweight composite material gas storage device, Features: Provided is a lightweight composite gas storage device, comprising an inner liner (1) and a composite material layer (4), the inner liner (1) comprising an upper shell (2) and a lower shell (3), the upper shell (2) and the lower shell (3) being welded to form the inner liner (1), and the composite material layer (4) being coated on the outside of the inner liner (1); The manufacturing method comprises Inner liner preparation step: preparing an upper shell (2) and a lower shell (3) respectively, and welding the upper shell (2) and the lower shell (3) to form an inner liner (1); The composite material layer (4) preparation step is as follows: the composite material layer (4) is coated on the outside of the inner liner (1), wherein the composite material layer (4) covers the weld bead.

7. A method for manufacturing a lightweight composite material gas storage device according to claim 6, Features: The upper shell (2) and the lower shell (3) are respectively injection molded.

8. A method for manufacturing a lightweight composite material gas storage device according to claim 6, Features: After welding, the inner liner (1) is subjected to a pressure holding test, which is required to meet the pressure holding of 1 bar @ 1 min and the leakage volume of < 25 ml / min.

9. The method for manufacturing a lightweight composite material gas storage device according to claim 6, Features: The composite material layer (4) is specifically prepared by a winding forming process, wherein the winding forming process includes a wet winding forming process and a dry winding forming process.

10. The method for manufacturing a lightweight composite material gas storage device according to claim 6, Features: The manufacturing method further comprises a surface treatment step, wherein the surface treatment step comprises polishing the composite material layer (4), then spraying epoxy resin on the surface of the composite material layer (4), and polishing again after curing to obtain a gas storage device with a smooth surface.

Citation Information

Patent Citations

  • Fiber winding reinforced full-plastic air cylinder for automobile braking device

    CN107351835A

  • High-pressure composite light-weight hydrogen storage bottle

    CN111998220A

  • Air reservoir adopting composite material

    CN112124284A

  • Low weight high performance composite vessel and method of making same

    US20040026431A1

  • Composite pressure container and method for production thereof

    WO2013168080A1