Metal gate device and manufacturing method
By using mask layer and chemical mechanical grinding method in metal gate devices, combined with the use of polysilicon and metal gates, the problem of large differences in gate thickness in the input and output regions is solved, and the electrical stability of the device is improved.
Patent Information
- Application Number
- CN202411091524.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-09
- Publication Date
- 2024-11-22
AI Technical Summary
In the prior art, the gate thickness of the metal gate device in the input and output regions varies greatly, affecting the electrical stability of the device.
By forming a first polysilicon gate and a high pattern density second polysilicon gate on a semiconductor substrate, and forming a dielectric layer therebetween, the metal gate material layer is removed by mask layer covering and chemical mechanical grinding method to form a Metal gate, metal gates are used in low-graphic density areas, and polysilicon gates are used in high-graphic density areas, controlling the grinding rate to reduce thickness differences.
It effectively reduces the thickness difference of the gate with high pattern density, improves the electrical stability of the device, and still retains the metal gate in the device area, without affecting device performance.
Smart Images

Figure CN119008528A_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the technical field of semiconductors and relates to a metal gate device and a manufacturing method thereof. Background Art
[0002] During the gate manufacturing process of metal gate devices, the metal gate material layer needs to be chemically mechanically polished to form the device gate. For aluminum gate devices, a high selectivity polishing liquid is usually used, and the polishing rate ratio of aluminum to oxide is not less than 20. It is sensitive to the load behavior of pattern density. The polishing rate is low in low pattern density areas, and high in high pattern density areas, resulting in large differences in gate thickness in high pattern density areas, affecting the electrical stability of the device.
[0003] The conventional method for preparing a metal gate device includes the following steps: Figure 1a to Figure 1d Explanation: 1) Figure 1a As shown, a first polysilicon gate 200 is formed in the device region 100 of the semiconductor substrate 1, and a second polysilicon gate 201 is formed in the input / output region 101 of the semiconductor substrate 1, and a dielectric layer 3 is filled between adjacent polysilicon gates, wherein the pattern density of the second polysilicon gate 201 is greater than the pattern density of the first polysilicon gate 200; 2) as Figure 1b As shown, the first polysilicon gate 200 and the second polysilicon gate 201 are removed; 3) as shown Figure 1c As shown, a metal gate material layer 8 is formed; 4) as Figure 1d As shown, chemical mechanical polishing is used to remove the metal gate material layer 8 located above the dielectric layer 3, and the retained metal gate material layer 8 constitutes the metal gate 10. Since the pattern density of the second polysilicon gate 201 is large, the polishing rate of the metal gate material layer 8 in the input-output region 101 is fast during chemical mechanical polishing, which leads to a large difference in gate thickness in the input-output region 101, affecting the electrical stability of the device.
[0004] Therefore, how to provide a metal gate device and a manufacturing method to improve the difference in gate thickness in the input and output regions and enhance the electrical stability of the device has become a technical problem that needs to be urgently solved by those skilled in the art.
[0005] It should be noted that the above introduction to the technical background is only for the convenience of providing a clear and complete description of the technical solutions of the present application and facilitating the understanding of those skilled in the art. It cannot be considered that the above technical solutions are well known to those skilled in the art simply because they are described in the background technology section of the present application. Summary of the invention
[0006] In view of the above-mentioned shortcomings of the prior art, an object of the present invention is to provide a metal gate device and a manufacturing method thereof, so as to solve the problems of large difference in gate thickness in input and output regions and poor electrical stability of the device in the prior art.
[0007] To achieve the above object and other related objects, the present invention provides a method for manufacturing a metal gate device, comprising the following steps:
[0008] Providing a semiconductor substrate, the semiconductor substrate is divided into a device area and an input-output area, a first polysilicon gate is formed on the device area, a second polysilicon gate is formed on the input-output area, the pattern density of the second polysilicon gate is greater than the pattern density of the first polysilicon gate, wherein a dielectric layer is formed between adjacent first polysilicon gates and / or second polysilicon gates;
[0009] forming a mask layer covering the second polysilicon gate, wherein the mask layer exposes the first polysilicon gate;
[0010] Removing the first polysilicon gate to form an opening, forming a metal gate material layer in the opening, wherein the metal gate material layer is also formed above the dielectric layer;
[0011] The metal gate material layer located above the dielectric layer is removed by chemical mechanical polishing, and the metal gate material layer located in the opening constitutes a metal gate.
[0012] Optionally, the metal gate material layer is made of aluminum.
[0013] Optionally, the mask layer includes an organic base layer, an anti-reflection layer and a photoresist layer stacked from bottom to top.
[0014] Optionally, after removing the first polysilicon gate and before forming the metal gate material layer, the method further includes a step of removing the mask layer.
[0015] Optionally, the mask layer is removed by an ashing method.
[0016] Optionally, before forming the metal gate material layer, the method further includes forming a work function metal layer on the inner wall of the opening.
[0017] Optionally, a functional layer is formed under the first polysilicon gate, and the functional layer includes a SiO2 layer, a HfO2 layer and a TiN layer stacked from bottom to top.
[0018] Optionally, a stress SiN layer is formed between the dielectric layer and the semiconductor substrate.
[0019] Optionally, sidewalls of the first polysilicon gate and the second polysilicon gate are both formed with sidewall spacers.
[0020] The present invention also provides a metal gate device, which is manufactured by any of the manufacturing methods described above, and includes: a semiconductor substrate, which is divided into a device area and an input-output area, a metal gate is provided on the device area, and a second polysilicon gate is provided on the input-output area, and the pattern density of the second polysilicon gate is greater than the pattern density of the metal gate.
[0021] As described above, in the metal gate device and manufacturing method of the present invention, by changing the material of the high-pattern-density gate, the low-pattern-density gate adopts a metal gate, and the high-pattern-density gate adopts a polysilicon gate. When the metal gate material layer is ground, the grinding rate of the grinding liquid on polysilicon is low, which effectively reduces the thickness difference of the high-pattern-density gate and improves the electrical stability of the device; and the polysilicon gate is confined to the input and output area, and the metal gate is still used in the device area, which will not reduce the device performance. BRIEF DESCRIPTION OF THE DRAWINGS
[0022] Figures 1a to 1d A schematic diagram showing the process of manufacturing a metal gate device using conventional technology.
[0023] Figure 2 Shown is a process flow chart of a method for manufacturing a metal gate device in an embodiment of the present invention.
[0024] Figure 3 It is a schematic diagram showing the formation of a dielectric layer according to an embodiment of the present invention.
[0025] Figure 4 It is a schematic diagram showing the process of polishing the medium layer to reveal the first polysilicon gate and the second polysilicon gate according to an embodiment of the present invention.
[0026] Figure 5 It is a schematic diagram showing the formation of a mask layer to cover the second polysilicon gate in an embodiment of the present invention.
[0027] Figure 6 It is a schematic diagram showing the removal of the first polysilicon gate according to an embodiment of the present invention.
[0028] Figure 7 It is a schematic diagram showing the formation of a metal gate material layer according to an embodiment of the present invention.
[0029] Figure 8 It is a schematic diagram showing the process of grinding a metal gate material layer to form a metal gate according to an embodiment of the present invention.
[0030] Component number description
[0031] 1 Semiconductor substrate
[0032] 100 Device Area
[0033] 101 Input and Output Area
[0034] 102 Source Area
[0035] 103 Leakage Area
[0036] 200 First polysilicon gate
[0037] 201 Second polysilicon gate
[0038] 3 Dielectric layer
[0039] 4 Functional Layer
[0040] 500 First side wall
[0041] 501 Second side wall
[0042] 6 Stress SiN layer
[0043] 7 Mask layer
[0044] 8 Metal gate material layer
[0045] 9 Work function metal layer
[0046] 10 Metal Gate
[0047] Steps S1 to S4 DETAILED DESCRIPTION
[0048] The following describes the embodiments of the present invention through specific examples, and those skilled in the art can easily understand other advantages and effects of the present invention from the contents disclosed in this specification. The present invention can also be implemented or applied through other different specific embodiments, and the details in this specification can also be modified or changed in various ways based on different viewpoints and applications without departing from the spirit of the present invention.
[0049] For example, when describing the embodiments of the present invention in detail, for the sake of convenience, the cross-sectional view showing the device structure will not be partially enlarged according to the general scale, and the schematic view is only an example, which should not limit the scope of protection of the present invention. In addition, in actual production, the three-dimensional space dimensions of length, width and depth should be included.
[0050] In the context of the present application, a structure in which a first feature is described as being "above" a second feature may include embodiments in which the first feature and the second feature are formed in direct contact, and may also include embodiments in which additional features are formed between the first feature and the second feature, such that the first feature and the second feature may not be in direct contact.
[0051] See also Figures 2 to 8It should be noted that the illustrations provided in this embodiment are only used to illustrate the basic concept of the present invention in a schematic manner, and the drawings only show components related to the present invention rather than being drawn according to the number, shape and size of components in actual implementation. In actual implementation, the type, quantity and proportion of each component may be changed arbitrarily, and the component layout may also be more complicated.
[0052] This embodiment provides a method for manufacturing a metal gate device. Figure 2 , the method for manufacturing the metal gate device comprises the following steps:
[0053] S1: providing a semiconductor substrate, wherein the semiconductor substrate is divided into a device region and an input / output region, a first polysilicon gate is formed on the device region, a second polysilicon gate is formed on the input / output region, a pattern density of the second polysilicon gate is greater than a pattern density of the first polysilicon gate, wherein a dielectric layer is formed between adjacent first polysilicon gates and / or second polysilicon gates;
[0054] S2: forming a mask layer covering the second polysilicon gate, wherein the mask layer exposes the first polysilicon gate;
[0055] S3: removing the first polysilicon gate to form an opening, and forming a metal gate material layer in the opening, wherein the metal gate material layer is also formed above the dielectric layer;
[0056] S4: removing the metal gate material layer located above the dielectric layer by chemical mechanical polishing, so that the metal gate material layer located in the opening constitutes a metal gate.
[0057] The method for manufacturing the metal gate device of this embodiment is described in detail below with reference to the specific drawings.
[0058] First, see Figure 4 , perform step S1: provide a semiconductor substrate 1, the semiconductor substrate 1 is divided into a device area 100 and an input-output area 101, a first polysilicon gate 200 is formed on the device area 100, a second polysilicon gate 201 is formed on the input-output area 101, the pattern density of the second polysilicon gate 201 is greater than the pattern density of the first polysilicon gate 200, wherein a dielectric layer 3 is formed between adjacent first polysilicon gates 200 and / or second polysilicon gates 201.
[0059] As an example, the device area 100 (Device area) is used to form active electronic components, such as transistors, diodes and MOSFETS, to constitute core parts such as logic gates, storage units, amplifiers, etc. to realize device functions; the input and output area 101 (I / O area) is used to realize connection and communication with external devices. In addition, driving circuits and receiving circuits can be formed in the input and output area 101 according to device requirements.
[0060] As an example, the pattern density of the second polysilicon gate 201 is greater than the pattern density of the first polysilicon gate 200 , that is, the area occupied by the second polysilicon gate 201 in the input-output region 101 is greater than the area occupied by the first polysilicon gate 200 in the device region 100 .
[0061] As an example, Figure 3 As shown, in the process of forming the dielectric layer 3 between adjacent polysilicon gates, the dielectric layer 3 is also formed above the first polysilicon gate 200 and the second polysilicon gate 201; Figure 4 As shown, the dielectric layer 3 is polished by chemical mechanical polishing (CMP) to expose the first polysilicon gate 200 and the second polysilicon gate 201 .
[0062] As an example, the material of the dielectric layer 3 includes undoped silicate glass (USG) or any other suitable insulating medium.
[0063] As an example, a functional layer 4 is formed under the first polysilicon gate 200, and the functional layer 4 includes a SiO2 layer, a HfO2 layer and a TiN layer stacked from bottom to top, wherein the SiO2 layer can prevent the impurities that may exist in the HfO2 layer from diffusing into the semiconductor substrate 1, maintaining the purity and performance of the semiconductor, and the SiO2 layer can provide a good interface passivation effect, which helps to reduce the interface state density, thereby reducing the interface charge traps of the device and the scattering caused by the interface state, and improving the performance of the device; the HfO2 layer, as a high-K dielectric layer, can provide a larger capacitance, thereby enhancing the gate control ability of the transistor, and the HfO2 has a high dielectric constant, which can reduce the thickness of the HfO2 layer while maintaining sufficient capacitance, which helps to reduce the gate leakage current and improve the power consumption efficiency of the device; the TiN layer is used as a protective layer to protect the HfO2 layer to prevent the metal atoms in the subsequently formed metal gate structure from diffusing into the HfO2 layer. A gate oxide layer is formed under the second polysilicon gate 201.
[0064] As an example, a shallow trench isolation structure (not shown in the figure) is also formed in the semiconductor substrate 1 to isolate the device area 100 and the input-output area 101; of course, a shallow trench isolation structure can also be formed in the device area 100 and the input-output area 101 to isolate different functional areas in the device area 100 and the input-output area 101.
[0065] As an example, a well region is formed in the semiconductor substrate 1 , an active region 102 and a drain region 103 are formed in the well region, and the source region 102 and the drain region 103 are separately arranged on both sides of a corresponding polysilicon gate.
[0066] As an example, the sidewalls of the first polysilicon gate 200 and the second polysilicon gate 201 are both provided with sidewalls, which can protect the polysilicon gate, define the source and drain ion implantation area, prevent the self-aligned silicide from causing bridging, and prevent the source / drain area from being implanted too close to the channel during high-intensity and high-dose injection, resulting in source / drain penetration, etc. In this embodiment, the sidewalls include a stacked first sidewall 500 and a second sidewall 501, the first sidewall 500 is made of a SiO2 layer, and the second sidewall 501 is made of a SiN layer, forming an ON sidewall; in other examples, the material and number of layers of the sidewalls can be changed according to actual needs, and are not limited to this embodiment.
[0067] As an example, a lightly doped drain (LDD) can also be formed in the semiconductor substrate 1 located below the sidewall to effectively control the electric field distribution of the transistor and reduce the electric field peak when the transistor operates at a high voltage, thereby reducing the breakdown risk and improving the reliability of the device.
[0068] As an example, before forming the dielectric layer 3, a step of forming a stressed SiN layer 6 on the semiconductor substrate 1 is also included, wherein the stressed SiN layer 6 covers the exposed surfaces of the semiconductor substrate 1, the sidewalls, the first polysilicon gate 200, and the second polysilicon gate 201. By forming the stressed SiN layer 6, stress is introduced to improve the carrier mobility of the transistor and the device performance. In the process of polishing the dielectric layer 3 to expose the first polysilicon gate 200 and the second polysilicon gate 201 by chemical mechanical polishing, the stressed SiN layer 6 located above the first polysilicon gate 200 and the second polysilicon gate 201 is polished and removed.
[0069] Next, see Figure 5 , executing step S2: forming a mask layer 7 covering the second polysilicon gate 201 , wherein the mask layer 7 exposes the first polysilicon gate 200 .
[0070] As an example, the mask layer 7 includes an organic bottom layer (ODL layer), an anti-reflection layer (SIARC layer) and a photoresist layer (PR layer) stacked from bottom to top, wherein the organic bottom layer helps to form a flatter surface, improve the uniformity of the photoresist layer, improve the fidelity of the pattern during the photolithography process, and ensure the accurate transmission of fine patterns; the anti-reflection layer can reduce light reflection during the photolithography process and improve the resolution and contrast of the photolithography process. In other examples, the material and number of layers of the mask layer 7 can be changed according to demand, and are not limited to this embodiment.
[0071] Specifically, in the present embodiment, a mask layer covering the first polysilicon gate 200 and the second polysilicon gate 201 is formed and patterned, and the patterned mask layer 7 covers the second polysilicon gate 201, exposing the first polysilicon gate 200; in other examples, a mask layer may be formed only on the second polysilicon gate 201, and no mask layer is formed on the first polysilicon gate 200, which also falls within the protection scope of the present invention.
[0072] Next, see Figure 6 and Figure 7 , executing step S3: removing the first polysilicon gate 200 to form an opening, forming a metal gate material layer 8 in the opening, and the metal gate material layer 8 is also formed above the dielectric layer 3.
[0073] As an example, Figure 6 As shown, the first polysilicon gate 200 is removed by etching or other suitable methods. Since the mask layer 7 is formed on the second polysilicon gate 201, the second polysilicon gate 201 will not be damaged during the removal of the first polysilicon gate 200. After removing the first polysilicon gate 200, the step of removing the mask layer 7 is also included, and the mask layer 7 is removed by ashing (Ash) or other suitable methods.
[0074] As an example, Figure 7 As shown, before forming the metal gate material layer 8 , a step of forming a work function metal layer 9 on the inner wall of the opening is also included, and the work function metal layer 9 is also formed above the dielectric layer 3 .
[0075] As an example, the metal gate material layer 8 is made of aluminum (Al).
[0076] Next, see Figure 8 , executing step S4: removing the metal gate material layer 8 located above the dielectric layer 3 by chemical mechanical polishing, and the metal gate material layer 8 located in the opening constitutes a metal gate 10 .
[0077] As an example, the metal gate material layer 8 is ground using a high selectivity grinding liquid to form the metal gate 10 , and the grinding rate ratio of aluminum to oxide is not less than 20.
[0078] As an example, since the input-output area 101 in the high pattern density area adopts the second polysilicon gate 201 as the gate, and the device area 100 in the low pattern density area adopts the metal gate 10 as the gate, during the grinding of the metal gate material layer 8, the grinding rate of the grinding liquid on the second polysilicon gate 201 is low, which effectively reduces the thickness difference of the high pattern density gate (the second polysilicon gate 201) and improves the electrical stability of the device.
[0079] In the manufacturing method of the metal gate device of the present embodiment, by changing the material of the high-pattern-density gate, the low-pattern-density gate adopts a metal gate, and the high-pattern-density gate adopts a polysilicon gate. When the metal gate material layer is ground, the grinding rate of the grinding liquid on polysilicon is low, which effectively reduces the thickness difference of the high-pattern-density gate and improves the electrical stability of the device. In addition, the polysilicon gate is confined to the input and output area, and the metal gate is still used in the device area, which will not reduce the device performance.
[0080] At this point, a metal gate device is obtained. Figure 8 The metal gate device includes a semiconductor substrate 1, which is divided into a device area 100 and an input-output area 101. A metal gate 10 is provided on the device area 100, and a second polysilicon gate 201 is provided on the input-output area 101. The pattern density of the second polysilicon gate 201 is greater than the pattern density of the metal gate 10.
[0081] As an example, the graphic density of the second polysilicon gate 201 is greater than the graphic density of the metal gate 10 , that is, the area proportion of the second polysilicon gate 201 in the input-output region 101 is greater than the area proportion of the metal gate 10 in the device region 100 .
[0082] As an example, a shallow trench isolation structure (not shown in the figure) is also provided in the semiconductor substrate 1 to isolate the device area 100 and the input-output area 101; of course, a shallow trench isolation structure can also be formed in the device area 100 and the input-output area 101 to isolate different functional areas in the device area 100 and the input-output area 101.
[0083] As an example, a well region is further provided in the semiconductor substrate 1 , and a source region 102 and a drain region 103 are provided in the well region. The source region 102 and the drain region 103 are separately provided on two sides of a corresponding gate.
[0084] As an example, a dielectric layer 3 is disposed between adjacent metal gates 10 and / or the second polysilicon gates 201 , and the material of the dielectric layer 3 includes undoped silicate glass (USG) or any other suitable insulating medium.
[0085] As an example, a functional layer 4 is disposed under the metal gate 10 , and the functional layer 4 includes a SiO 2 layer, a HfO 2 layer and a TiN layer stacked from bottom to top; a gate oxide layer is disposed under the second polysilicon gate 201 .
[0086] As an example, the side walls of the metal gate 10 and the second polysilicon gate 201 are both provided with side walls. In this embodiment, the side walls include a stacked first side wall 500 and a second side wall 501. The first side wall 500 is made of a SiO2 layer, and the second side wall 501 is made of a SiN layer to form an ON side wall. In other examples, the material and number of layers of the side wall can be changed according to actual needs and are not limited to this embodiment.
[0087] As an example, a lightly doped drain (LDD) is also provided in the semiconductor substrate 1 below the sidewall to effectively control the electric field distribution of the transistor and reduce the electric field peak when the transistor operates at a high voltage, thereby reducing the breakdown risk and improving the reliability of the device.
[0088] As an example, a stress SiN layer 6 is further provided between the semiconductor substrate 1 and the dielectric layer 3 , and the stress SiN layer 6 also covers the sidewalls of the spacer.
[0089] As an example, the material of the metal gate 10 is aluminum, and a work function metal layer 9 is disposed between the metal gate 10 and the functional layer 4 , and the work function metal layer 9 also extends to the side wall of the metal gate 10 .
[0090] In summary, in the metal gate device and manufacturing method of the present invention, by changing the material of the high-pattern-density gate, the low-pattern-density gate uses a metal gate, and the high-pattern-density gate uses a polysilicon gate. When the metal gate material layer is polished, the polishing rate of the polishing liquid on the polysilicon is low, which effectively reduces the thickness difference of the high-pattern-density gate and improves the electrical stability of the device; and the polysilicon gate is confined to the input and output area, and the metal gate is still used in the device area, which will not reduce the performance of the device. Therefore, the present invention effectively overcomes various shortcomings in the prior art and has a high industrial utilization value.
[0091] The above embodiments are merely illustrative of the principles and effects of the present invention, and are not intended to limit the present invention. Anyone familiar with the art may modify or alter the above embodiments without departing from the spirit and scope of the present invention. Therefore, all equivalent modifications or alterations made by a person of ordinary skill in the art without departing from the spirit and technical concept disclosed by the present invention shall still be covered by the claims of the present invention.
Claims
1. A method for manufacturing a metal gate device, characterized in that: The following steps are involved: Providing a semiconductor substrate, the semiconductor substrate is divided into a device area and an input-output area, a first polysilicon gate is formed on the device area, a second polysilicon gate is formed on the input-output area, the pattern density of the second polysilicon gate is greater than the pattern density of the first polysilicon gate, wherein a dielectric layer is formed between adjacent first polysilicon gates and / or second polysilicon gates; forming a mask layer covering the second polysilicon gate, wherein the mask layer exposes the first polysilicon gate; Removing the first polysilicon gate to form an opening, forming a metal gate material layer in the opening, wherein the metal gate material layer is also formed above the dielectric layer; The metal gate material layer located above the dielectric layer is removed by chemical mechanical polishing, and the metal gate material layer located in the opening constitutes a metal gate.
2. The method for manufacturing a metal gate device according to claim 1, characterized in that: The material of the metal gate material layer includes aluminum.
3. The method for manufacturing a metal gate device according to claim 1, wherein: The mask layer includes an organic bottom layer, an anti-reflection layer and a photoresist layer stacked from bottom to top.
4. The method for manufacturing a metal gate device according to claim 1, wherein: After removing the first polysilicon gate and before forming the metal gate material layer, the method further includes removing the mask layer.
5. The method for manufacturing a metal gate device according to claim 4, characterized in that: The mask layer is removed by an ashing method.
6. The method for manufacturing a metal gate device according to claim 1, wherein: Before forming the metal gate material layer, the method further includes forming a work function metal layer on the inner wall of the opening.
7. The method for manufacturing a metal gate device according to claim 1, characterized in that: A functional layer is formed under the first polysilicon gate, and the functional layer includes a SiO2 layer, a HfO2 layer and a TiN layer stacked from bottom to top.
8. The method for manufacturing a metal gate device according to claim 1, characterized in that: A stress SiN layer is formed between the dielectric layer and the semiconductor substrate.
9. The method for manufacturing a metal gate device according to claim 1, characterized in that: Sidewalls of the first polysilicon gate and the second polysilicon gate are both formed with sidewall spacers.
10. A metal gate device, characterized in that: The metal gate device is manufactured by the manufacturing method described in any one of claims 1 to 9, comprising: a semiconductor substrate, the semiconductor substrate is divided into a device area and an input-output area, a metal gate is provided on the device area, a second polysilicon gate is provided on the input-output area, and the pattern density of the second polysilicon gate is greater than the pattern density of the metal gate.
Citation Information
Cited By
Semiconductor device and manufacturing method thereof
CN119677161A