Glass substrate structure and preparation method thereof
By setting blind holes and conductive column structures on the glass substrate, using their adjustable thermal expansion coefficient and low dielectric loss factor, the problem of warping of the connection of the silicon-based intermediate layer packaging substrate is solved, and a smaller size package and higher Package dielectric performance reduces processing difficulty and cost.
Patent Information
- Application Number
- CN202310601569.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2023-05-26
- Publication Date
- 2024-11-26
AI Technical Summary
The existing silicon-based intermediate layer packaging substrates are unadjustable when the chip is connected to the packaging substrate, which increases the processing difficulty and cost.
Using a glass substrate structure, by setting blind holes, wiring interconnection layers and conductive column structures on the glass substrate, the adjustable thermal expansion coefficient and low dielectric loss factor of the glass substrate are used to reduce the risk of connection warping and improve the packaging dielectric performance.
A smaller size package is realized, reducing the connection warping problem between the package substrate and the chip, improving the dielectric performance of the package, and reducing processing difficulty and cost.
Smart Images

Figure CN119028829A_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the technical field of semiconductor integrated circuit manufacturing, and in particular relates to a glass substrate structure and a preparation method thereof. Background Art
[0002] With the rapid development of electronic technology, the number of chip I / Os has increased dramatically, making the industry's requirements for packaging substrates higher and higher. At this time, traditional packaging can no longer meet the needs, and advanced packaging technology has begun to become the mainstream of the current era. As a connecting mechanism between the chip and the PCB board, the packaging substrate has higher and higher requirements for the precision of its circuits. At the same time, as the integration of the chip becomes higher and higher, the connection accuracy requirements between the chip and the packaging substrate are also more stringent.
[0003] The existing technology uses the form of embedding a silicon-based intermediate layer to interconnect the chip and the packaging substrate through TSV (Through Silicon Via), but the production and embedding process of the silicon-based intermediate layer faces the problems of difficult processing technology and high processing cost. In addition, the CTE (Coefficient of Thermal Expansion) of the silicon-based intermediate layer cannot be adjusted, which makes the chip and the packaging substrate expand and contract differently when interconnecting and matching, resulting in a certain risk of warping, displacement or shedding, leading to open circuit or short circuit.
[0004] It should be noted that the above introduction to the technical background is only for the convenience of providing a clear and complete description of the technical solutions of the present application and for the convenience of understanding by those skilled in the art. It cannot be considered that the above technical solutions are well known to those skilled in the art simply because these solutions are described in the background technology part of the present application. Summary of the invention
[0005] In view of the above shortcomings of the prior art, an object of the present invention is to provide a glass substrate structure and a preparation method thereof, so as to solve the problem of warping risk between the through silicon via packaging substrate and the chip in the prior art.
[0006] To achieve the above object, the present invention provides a method for preparing a glass substrate structure, the method comprising:
[0007] Providing a glass substrate, the glass substrate comprising a first surface and a second surface arranged opposite to each other, and a first blind hole is arranged on the first surface of the glass substrate;
[0008] Disposing a wiring interconnection layer on the first surface of the glass substrate;
[0009] A first conductive column structure is provided on the wiring interconnection layer, thereby forming a glass core board;
[0010] A temporary substrate is arranged on the first conductive column structure, and the temporary substrate is bonded to the glass core board through the first conductive column structure;
[0011] Thinning the second surface of the glass substrate until the bottom of the first blind hole is exposed;
[0012] Disposing a back pre-plating layer on the thinned second surface;
[0013] Disposing a second conductive column structure on the back pre-plating layer;
[0014] removing the back pre-plating layer not covered by the second conductive column structure;
[0015] The temporary substrate is removed, thereby obtaining the glass substrate structure.
[0016] Optionally, the first blind hole is provided by a laser induced deep etching process.
[0017] Optionally, the glass substrate is one of alkali-free glass, alkaline glass, aluminum oxide glass, high borosilicate glass and quartz glass.
[0018] Optionally, the method for setting the wiring interconnection layer includes:
[0019] Disposing a first pre-plating layer on the first surface of the glass substrate, wherein the first pre-plating layer covers the first surface and the surface of the first blind hole;
[0020] Disposing a first conductive layer on the first pre-plating layer, wherein the first conductive layer fills the first blind hole and covers the surface of the first pre-plating layer;
[0021] Grinding and polishing the first conductive layer so that the first conductive layer above the position on the first surface where the first blind hole is not provided has a preset thickness;
[0022] A patterned second conductive layer is provided on the first conductive layer of a preset thickness, wherein the second conductive layer forms an effective electrical connection with the first conductive layer; and the first conductive layer and the first pre-plating layer on the first surface that are not covered by the second conductive layer are removed;
[0023] A first insulating layer is provided on the first surface, the first insulating layer covers the exposed first surface and the second conductive layer, a second blind hole is provided on the first insulating layer, the second blind hole extends to the second conductive layer, and a portion of the second conductive layer is exposed;
[0024] A second pre-plating layer is disposed on the first insulating layer, and the second pre-plating layer covers the surface of the first insulating layer and the second blind hole, thereby forming a first wiring layer.
[0025] Optionally, the wiring interconnection layer includes one or more wiring layers, and effective electrical connections are formed between adjacent wiring layers in the multiple wiring layers.
[0026] Optionally, the first conductive pillar structure includes a first copper pillar and a first protective layer, the first copper pillar forms an effective electrical connection with the wiring interconnection layer, and the first protective layer is arranged at an end of the first copper pillar away from the wiring interconnection layer.
[0027] Optionally, after removing the back pre-plating layer not covered by the second conductive column structure, a back adhesive protective film is provided to wrap the second conductive column structure; after removing the temporary substrate, the back adhesive protective film is removed.
[0028] Optionally, the temporary substrate includes a bonding layer and a glass carrier layer, the bonding layer wraps the first conductive column structure, and the glass carrier layer is arranged on a side of the bonding layer away from the first conductive column structure.
[0029] Optionally, the bonding layer includes a bonding layer and a release layer, the bonding layer is in contact with the first conductive column structure of the formed glass core board, and the release layer is arranged on a side of the bonding layer away from the glass core board.
[0030] The present invention also provides a glass substrate structure, which is obtained by any one of the above-mentioned preparation methods, and comprises: a glass substrate, a wiring interconnection layer, a first conductive column structure and a second conductive column structure;
[0031] The glass substrate comprises a first surface and a second surface which are arranged opposite to each other, the wiring interconnection layer is arranged on the first surface of the glass substrate, the first conductive column structure is arranged on the wiring interconnection layer, and the second conductive column structure is arranged on the second surface of the glass substrate;
[0032] A first blind hole is provided in the glass substrate, and the wiring interconnection layer forms an effective electrical connection with the second conductive column structure through the first blind hole, and the first conductive column structure forms an effective electrical connection with the wiring interconnection layer.
[0033] As described above, the glass substrate structure and the preparation method thereof of the present invention have the following beneficial effects:
[0034] The present invention uses a glass substrate as a packaging substrate and utilizes the characteristics of the glass substrate, such as adjustable format size, adjustable thermal expansion coefficient, and low dielectric loss factor, to achieve smaller size packaging, reduce the risk of connection warping problems between the packaging substrate and the chip, and improve the dielectric properties of the package, thereby reducing processing difficulty and processing costs. BRIEF DESCRIPTION OF THE DRAWINGS
[0035] Figure 1 It is a schematic diagram of the structure presented in step 1 of the present invention.
[0036] Figure 2 It is a schematic diagram of the structure presented by setting the first pre-plating layer in the optional example of step 2 in the present invention.
[0037] Figure 3 It is a schematic diagram of the structure presented by setting the first conductive layer in the optional example of step 2 in the present invention.
[0038] Figure 4 It is a schematic diagram of the structure presented by grinding the first conductive layer in the optional example of step 2 in the present invention.
[0039] Figure 5 Shown is a schematic diagram of the structure presented by setting a graphic first photoresist in the optional example of step 2 in the present invention.
[0040] Figure 6 It is a schematic diagram of the structure presented by setting the second conductive layer in the optional example of step 2 in the present invention.
[0041] Figure 7 It is a schematic diagram of the structure presented by removing the first photoresist and the first pre-plating layer in the optional example of step 2 in the present invention.
[0042] Figure 8 It is a schematic diagram of the structure presented by setting the first insulating layer in the optional example of step 2 in the present invention.
[0043] Fig. 9 It is a schematic diagram of the structure presented by setting the second pre-plating layer in the optional example of step 2 in the present invention.
[0044] Fig.10 It is a schematic diagram of the structure presented by forming the second wiring layer in the optional example of step 2 in the present invention.
[0045] Fig.11 It is a schematic structural diagram of the first conductive column structure provided in step 3 of the present invention.
[0046] Fig.12 It is a schematic diagram of the structure presented by setting up a temporary substrate and a bonding layer in the optional example of step 4 in the present invention.
[0047] Fig.13 It is a schematic diagram showing the structure of the thinned glass substrate in step 5 of the present invention.
[0048] Fig.14 It is a schematic diagram of the structure presented by setting the back pre-plating layer in step 6 of the present invention.
[0049] Fig.15It is a schematic structural diagram showing the second conductive pillar structure provided in step 7 of the present invention.
[0050] Fig.16 It is a schematic diagram of the structure presented by removing the back pre-plating layer in step 8 of the present invention.
[0051] Fig.17 It is a schematic diagram of the structure presented by providing a back adhesive protective film in an optional example of step 8 in the present invention.
[0052] Fig.18 It is a schematic diagram of the structure presented by removing the release layer and the temporary substrate in an optional example of step 9 in the present invention.
[0053] Fig.19 It is a schematic diagram of the structure presented by removing the bonding layer in an optional example of step 9 in the present invention.
[0054] Fig. 20 It is a schematic diagram showing the structure presented by cutting the glass substrate structure in an optional example of step 9 of the present invention.
[0055] Fig.21 It is a schematic diagram of the structure presented by removing the adhesive protective film in an optional example of step 9 in the present invention.
[0056] Component number description
[0057] 10. Glass substrate; 11. First surface; 12. Second surface; 13. First blind hole; 14. First pre-plating layer; 15. Back pre-plating layer;
[0058] 21. first conductive layer; 22. first photoresist; 23. second conductive layer; 24. first insulating layer; 25. second blind hole; 26. second pre-plating layer;
[0059] 31. third conductive layer; 32. second insulating layer; 33. third blind hole; 34. third pre-plating layer;
[0060] 40. first conductive pillar structure; 41. first copper pillar; 42. first protective layer; 43. second photoresist;
[0061] 50, temporary substrate; 51, bonding layer; 511, bonding layer; 512, release layer; 52, glass carrier layer;
[0062] 60. Second conductive column structure; 61. Second copper column; 62. Second protective layer; 63. Third photoresist; 64. Back glue protective film. DETAILED DESCRIPTION
[0063] The following describes the embodiments of the present invention through specific examples, and those skilled in the art can easily understand other advantages and effects of the present invention from the contents disclosed in this specification. The present invention can also be implemented or applied through other different specific embodiments, and the details in this specification can also be modified or changed in various ways based on different viewpoints and applications without departing from the spirit of the present invention.
[0064] For example, when describing the embodiments of the present invention in detail, for the sake of convenience, the schematic diagrams showing the device structure will not be partially enlarged according to the general scale, and the schematic diagrams are only examples, which should not limit the scope of protection of the present invention. In addition, in actual production, the three-dimensional dimensions of length, width and depth should be included.
[0065] For convenience of description, spatially relative terms such as "under", "below", "below", "below", "above", "on", etc. may be used herein to describe the relationship of one element or feature shown in the drawings to other elements or features. It will be understood that these spatially relative terms are intended to encompass other orientations of the device in use or operation in addition to the orientation depicted in the drawings.
[0066] In the context of the present application, a structure in which a first feature is described as being "above" a second feature may include embodiments in which the first and second features are in direct contact, and may also include embodiments in which additional features are formed between the first and second features, such that the first and second features may not be in direct contact.
[0067] It should be noted that the illustrations provided in this embodiment are only used to illustrate the basic concept of the present invention in a schematic manner, and therefore the illustrations only show components related to the present invention rather than being drawn according to the number, shape and size of components in actual implementation. In actual implementation, the type, quantity and proportion of each component may be changed arbitrarily, and the component layout may also be more complicated.
[0068] like Figure 1-Figure 20 As shown, the present invention provides a method for preparing a glass substrate 10 structure, the preparation method comprising:
[0069] Step 1: providing a glass substrate 10, wherein the glass substrate 10 comprises a first surface 11 and a second surface 12 disposed opposite to each other, and a first blind hole 13 is disposed on the first surface 11 of the glass substrate 10;
[0070] Step 2: Disposing a wiring interconnection layer on the first surface 11 of the glass substrate 10;
[0071] Step 3: a first conductive column structure 40 is provided on the wiring interconnection layer, thereby forming a glass core board;
[0072] Step 4: a temporary substrate 50 is disposed on the first conductive column structure 40 , and the temporary substrate 50 is bonded to the glass core board through the first conductive column structure 40 ;
[0073] Step 5: thinning the second surface 12 of the glass substrate 10 until the bottom of the first blind hole 13 is exposed;
[0074] Step 6: Disposing a back pre-plating layer 15 on the thinned second surface 12;
[0075] Step 7: Disposing a second conductive column structure 60 on the back pre-plating layer 15;
[0076] Step 8: removing the back pre-plating layer 15 not covered by the second conductive column structure 60;
[0077] Step 9: removing the temporary substrate 50 , thereby obtaining the glass substrate 10 structure.
[0078] The preparation method of the glass substrate 10 structure of the present invention will be described in detail below with reference to the accompanying drawings. It should be noted that the above sequence does not strictly represent the sequence of the preparation method of the glass substrate 10 structure protected by the present invention, and those skilled in the art may change it according to the actual preparation steps.
[0079] First, if Figure 1 As shown, step 1 is performed to provide a glass substrate 10 . The glass substrate 10 includes a first surface 11 and a second surface 12 that are opposite to each other. A first blind hole 13 is disposed on the first surface 11 of the glass substrate 10 .
[0080] In the prior art, a silicon-based intermediate layer is used as the connection structure between the packaging substrate and the chip. Since the thermal expansion coefficient of the silicon-based intermediate layer cannot be adjusted, the chip and the packaging substrate may have different expansion and contraction ratios during the interconnection matching process. Therefore, the connection part between the chip and the packaging substrate may be warped, causing the connection structure to shift or even fall off, resulting in short circuit or open circuit defects. This phenomenon is more obvious in small-sized packaging structures. The present invention uses a glass substrate 10 as a packaging substrate and utilizes the adjustable thermal expansion coefficient of the glass substrate 10 to reduce the risk of warping problems between the packaging substrate and the chip while achieving a smaller-sized package. At the same time, since the Df (Dissipation Factor) of the glass substrate 10 is much smaller than the Df of the silicon-based intermediate layer structure, the use of the glass substrate 10 can improve the dielectric properties of the package and reduce the difficulty and cost of processing. In addition, since the glass substrate 10 can achieve larger-sized production, its production efficiency can be improved.
[0081] In one embodiment, the first blind hole 13 is formed by using a LIDE (Laser-Induced-Deep Etching) process.
[0082] In one embodiment, the glass substrate 10 is one of alkali-free glass, alkali glass, aluminum oxide glass, high borosilicate glass and quartz glass.
[0083] In one embodiment, the glass substrate 10 has a thickness of 700 micrometers to 800 micrometers.
[0084] Specifically, the thermal expansion coefficient of the glass substrate 10 is between 1 ppm / °C and 10 ppm / °C, and the thermal conductivity is between 1 W / m·K and 5 W / m·K.
[0085] In one embodiment, the first blind hole 13 is obtained by disposing PSPI (Photosensitive Polyimides, photosensitive insulating material) and then performing photolithography and development.
[0086] In one embodiment, the blind hole 13 in the glass substrate 10 is a cylindrical blind hole 13 , which has better reliability and structural coordination, and is conducive to giving full play to its excellent performance.
[0087] Then, step 2 is performed to dispose a wiring interconnection layer on the first surface 11 of the glass substrate 10 .
[0088] In one embodiment, Figure 2-Figure 10As shown, the method for setting the wiring interconnection layer includes: setting a first pre-plating layer 14 on the first surface 11 of the glass substrate 10, the first pre-plating layer 14 covers the first surface 11 and the surface of the first blind hole 13; setting a first conductive layer 21 on the first pre-plating layer 14, the first conductive layer 21 fills the first blind hole 13 and covers the surface of the first pre-plating layer 14; grinding and polishing the first conductive layer 21 so that the first conductive layer 21 above the position on the first surface 11 where the first blind hole 13 is not set has a preset thickness; setting a patterned second conductive layer 23 on the first conductive layer 21 of the preset thickness, the second conductive layer 23 and the first conductive layer 23 are parallel to each other. The first conductive layer 21 forms an effective electrical connection; the first conductive layer 21 and the first pre-plated layer 14 on the first surface 11 that are not covered by the second conductive layer 23 are removed; a first insulating layer 24 is arranged on the first surface 11, the first insulating layer 24 covers the exposed first surface 11 and the second conductive layer 23, a second blind hole 25 is arranged on the first insulating layer 24, the second blind hole 25 extends to the second conductive layer 23, and a portion of the second conductive layer 23 is exposed; a second pre-plated layer 26 is arranged on the first insulating layer 24, the second pre-plated layer 26 covers the surface of the first insulating layer 24 and the second blind hole 25, and thus a first wiring layer is formed.
[0089] The present invention ensures good electrical connection by providing the first conductive layer 21 to fill the first blind hole 13, thereby avoiding the risk of gaps and open circuits in subsequent manufacturing processes due to the height difference caused by the first blind hole 13 and large surface roughness.
[0090] Specifically, Figure 5-Figure 7 As shown, the method for setting a graphic second conductive layer 23 includes: setting a graphic first photoresist 22 on the first conductive layer 21; setting a second conductive layer 23 on the first photoresist 22, wherein the second conductive layer 23 fills the gaps in the first photoresist 22; and removing the first photoresist 22 and the second conductive layer 23 thereon to obtain a graphic second conductive layer 23.
[0091] Specifically, the first photoresist 22 and the first conductive layer 21 and the first pre-plating layer 14 on the first surface 11 that are not covered by the second conductive layer 23 are removed by differential etching (flash etching).
[0092] Specifically, the first pre-plating layer 14 includes a titanium layer and a copper layer. The titanium layer contacts the glass substrate 10 to form a better adhesion with the glass substrate 10 as a transition layer, which is convenient for the subsequent growth of the first conductive layer 21 .
[0093] In one embodiment, the first pre-plating layer 14 is obtained by physical vapor deposition or wet chemical metallization.
[0094] In one embodiment, the wiring interconnection layer includes one or more wiring layers, and effective electrical connections are formed between adjacent wiring layers in the multi-layer wiring layers.
[0095] In one embodiment, two wiring layers are provided, such as Fig.10 As shown, after the first wiring layer is formed, the third conductive layer 31, the second insulating layer 32, the third blind hole 33 and the third pre-plating layer 34 are respectively arranged according to the above method.
[0096] The present invention realizes a high-density integrated packaging structure by setting a wiring interconnection layer on the glass substrate 10, which avoids the warping of the connection between the packaging substrate and the chip due to different thermal stresses under the conditions of small size and high integration, thereby improving the reliability of the packaging structure, expanding the application scenarios of the glass substrate 10, and facilitating the market expansion of the glass substrate 10 in the packaging substrate.
[0097] Then, if Fig.11 As shown, step 3 is performed to dispose a first conductive column structure 40 on the wiring interconnection layer, thereby forming a glass core board.
[0098] In one embodiment, the first conductive pillar structure 40 includes a first copper pillar 41 and a first protective layer 42. The first copper pillar 41 forms an effective electrical connection with the wiring interconnection layer. The first protective layer 42 is disposed at one end of the first copper pillar 41 away from the wiring interconnection layer.
[0099] Specifically, Fig.11 As shown, the first conductive pillar structure 40 is obtained by photolithography and development of the second photoresist 43 .
[0100] In one embodiment, the first protection layer 42 is tin or silver.
[0101] Specifically, the first conductive column structure 40 is disposed in the topmost blind hole on the wiring interconnection layer, and forms an effective electrical connection with the conductive layer exposed under the blind hole.
[0102] Then, step 4 is performed to dispose a temporary substrate 50 on the first conductive column structure 40 , and the temporary substrate 50 is bonded to the glass core board through the first conductive column structure 40 .
[0103] In one embodiment, the temporary substrate 50 includes a bonding layer 51 and a glass carrier layer 52 . The bonding layer 51 wraps the first conductive column structure 40 , and the glass carrier layer 52 is disposed on a side of the bonding layer 51 away from the first conductive column structure 40 .
[0104] In one embodiment, Fig.12 As shown, the bonding layer 51 includes a bonding layer 511 and a release layer 512 . The bonding layer 511 contacts the first conductive column structure 40 of the formed glass core board, and the release layer 512 is arranged on a side of the bonding layer 511 away from the glass core board.
[0105] The present invention provides the bonding layer 511 on the glass core board to protect the glass core board, so that the solvent in the subsequent debonding step will not damage the glass core board; at the same time, the release layer 512 is provided to improve the subsequent debonding efficiency.
[0106] In one embodiment, the method for bonding the temporary substrate 50 to the glass core board is: firstly apply a bonding layer 511 on the glass core board, and heat to solidify the bonding layer 511; then apply a release layer 512, place the glass core board on the release layer 512, and heat to solidify the release layer 512, thereby forming a temporary bond between the temporary substrate 50 and the glass core board.
[0107] In one embodiment, the temporary substrate 50 has a thickness of 600 micrometers to 700 micrometers.
[0108] Then, if Fig.13 As shown, step 5 is performed to thin the second surface 12 of the glass substrate 10 until the bottom of the first blind hole 13 is exposed.
[0109] Then, if Fig.14 As shown, step 6 is performed to provide a back pre-plating layer 15 on the thinned second surface 12 .
[0110] Then, if Fig.15 As shown, step 7 is performed to dispose a second conductive column structure 60 on the back pre-plating layer 15 .
[0111] In one embodiment, the second conductive pillar structure 60 includes a second copper pillar 61 and a second protection layer 62 , and the second protection layer 62 is tin or silver.
[0112] Specifically, the first protective layer 42 and the second protective layer 62 are respectively used to protect the copper pillars under their corresponding conductive pillar structures.
[0113] Specifically, Fig.15 As shown, the second conductive pillar structure 60 is obtained by photolithography and development of the third photoresist 63 .
[0114] Then, if Fig.16 As shown, step 8 is performed to remove the back pre-plating layer 15 not covered by the second conductive column structure 60 .
[0115] In one embodiment, Fig.17 As shown, after removing the back pre-plating layer 15 not covered by the second conductive column structure 60 , a back adhesive protection film 64 is provided to wrap the second conductive column structure 60 .
[0116] Finally, step 9 is performed to remove the temporary substrate 50 , thereby obtaining the glass substrate 10 structure.
[0117] In one embodiment, when the temporary substrate 50 is bonded to the glass substrate 10, a bonding layer 51 is provided and the bonding layer 51 includes a bonding layer 511 and a release layer 512, the step of removing the temporary substrate 50 is as follows: Fig.18 As shown, firstly, an excimer beam is irradiated on the release layer 512 to cause the release layer 512 to bubble. At this time, its peeling strength is reduced, and the temporary substrate 50 can be separated from the glass substrate 10 by a physical method; Fig.19 As shown, the glass substrate 10 is then immersed in a special organic solvent to dissolve the bonding layer 511, thereby achieving the effect of removing the bonding layer 511.
[0118] In one embodiment, Fig. 20 As shown, after the adhesive protective film 64 is provided, the glass substrate 10 structure is cut; Fig.21 As shown, after removing the temporary substrate 50 , the adhesive protective film 64 is removed.
[0119] Specifically, the glass substrate 10 is cut to be divided into units of a plurality of glass substrates 10 .
[0120] The present invention also provides a glass substrate 10 structure, which is obtained by any one of the above-mentioned preparation methods, and the glass substrate 10 structure comprises: a glass substrate 10, a wiring interconnection layer, a first conductive column structure 40 and a second conductive column structure 60;
[0121] The glass substrate 10 includes a first surface 11 and a second surface 12 which are arranged opposite to each other, the wiring interconnection layer is arranged on the first surface 11 of the glass substrate 10, the first conductive column structure 40 is arranged on the wiring interconnection layer, and the second conductive column structure 60 is arranged on the second surface 12 of the glass substrate 10;
[0122] The glass substrate 10 is provided with a first blind hole 13 , and the wiring interconnection layer is effectively electrically connected to the second conductive column structure 60 through the first blind hole 13 , and the first conductive column structure 40 is effectively electrically connected to the wiring interconnection layer.
[0123] In summary, the glass substrate structure and preparation method of the present invention can use a glass substrate as a packaging substrate and utilize the characteristics of the glass substrate, such as adjustable format size, adjustable thermal expansion coefficient, and low dielectric loss factor, to achieve smaller size packaging, reduce the risk of connection warping problems between the packaging substrate and the chip, and improve the dielectric properties of the package, thereby reducing processing difficulty and processing costs.
[0124] Therefore, the present invention effectively overcomes various shortcomings in the prior art and has high industrial utilization value.
[0125] The above embodiments are merely illustrative of the principles and effects of the present invention, and are not intended to limit the present invention. Anyone familiar with the art may modify or alter the above embodiments without departing from the spirit and scope of the present invention. Therefore, all equivalent modifications or alterations made by a person of ordinary skill in the art without departing from the spirit and technical concept disclosed by the present invention shall still be covered by the claims of the present invention.
Claims
1. A method for preparing a glass substrate structure, It is characterized in that The preparation method comprises: Providing a glass substrate, the glass substrate comprising a first surface and a second surface arranged opposite to each other, and a first blind hole is arranged on the first surface of the glass substrate; Disposing a wiring interconnection layer on the first surface of the glass substrate; A first conductive column structure is provided on the wiring interconnection layer, thereby forming a glass core board; A temporary substrate is arranged on the first conductive column structure, and the temporary substrate is bonded to the glass core board through the first conductive column structure; Thinning the second surface of the glass substrate until the bottom of the first blind hole is exposed; Disposing a back pre-plating layer on the thinned second surface; Disposing a second conductive column structure on the back pre-plating layer; removing the back pre-plating layer not covered by the second conductive column structure; The temporary substrate is removed, thereby obtaining the glass substrate structure.
2. The method for preparing a glass substrate structure according to claim 1, It is characterized in that The first blind hole is provided by a laser induced deep etching process.
3. The method for preparing a glass substrate structure according to claim 1, It is characterized in that The glass substrate is one of alkali-free glass, alkaline glass, aluminum oxide glass, high borosilicate glass and quartz glass.
4. The method for preparing a glass substrate structure according to claim 1, It is characterized in that The method for setting the wiring interconnection layer comprises: Disposing a first pre-plating layer on the first surface of the glass substrate, wherein the first pre-plating layer covers the first surface and the surface of the first blind hole; Disposing a first conductive layer on the first pre-plating layer, wherein the first conductive layer fills the first blind hole and covers the surface of the first pre-plating layer; Grinding and polishing the first conductive layer so that the first conductive layer above the position on the first surface where the first blind hole is not provided has a preset thickness; A patterned second conductive layer is provided on the first conductive layer of a preset thickness, wherein the second conductive layer forms an effective electrical connection with the first conductive layer; and the first conductive layer and the first pre-plating layer on the first surface that are not covered by the second conductive layer are removed; A first insulating layer is provided on the first surface, the first insulating layer covers the exposed first surface and the second conductive layer, a second blind hole is provided on the first insulating layer, the second blind hole extends to the second conductive layer, and a portion of the second conductive layer is exposed; A second pre-plating layer is disposed on the first insulating layer, and the second pre-plating layer covers the surface of the first insulating layer and the second blind hole, thereby forming a first wiring layer.
5. The method for preparing a glass substrate structure according to claim 1, It is characterized in that The wiring interconnection layer includes one or more wiring layers, and effective electrical connections are formed between adjacent wiring layers in the multi-layer wiring layer.
6. The method for preparing a glass substrate structure according to claim 1, It is characterized in that The first conductive column structure includes a first copper column and a first protective layer. The first copper column forms an effective electrical connection with the wiring interconnection layer. The first protective layer is arranged at one end of the first copper column away from the wiring interconnection layer.
7. The method for preparing a glass substrate structure according to claim 1, It is characterized in that After removing the back pre-plating layer not covered by the second conductive column structure, a back adhesive protective film is provided to wrap the second conductive column structure; after removing the temporary substrate, the back adhesive protective film is removed.
8. The method for preparing a glass substrate structure according to claim 1, It is characterized in that The temporary substrate comprises a bonding layer and a glass carrier layer, the bonding layer wraps the first conductive column structure, and the glass carrier layer is arranged on a side of the bonding layer away from the first conductive column structure.
9. The method for preparing a glass substrate structure according to claim 8, It is characterized in that The bonding layer includes a bonding layer and a release layer. The bonding layer is in contact with the first conductive column structure of the formed glass core board, and the release layer is arranged on a side of the bonding layer away from the glass core board.
10. A glass substrate structure, It is characterized in that The glass substrate structure is obtained by the preparation method according to any one of claims 1 to 9, and the glass substrate structure comprises: a glass substrate, a wiring interconnection layer, a first conductive column structure and a second conductive column structure; The glass substrate comprises a first surface and a second surface which are arranged opposite to each other, the wiring interconnection layer is arranged on the first surface of the glass substrate, the first conductive column structure is arranged on the wiring interconnection layer, and the second conductive column structure is arranged on the second surface of the glass substrate; A first blind hole is provided in the glass substrate, and the wiring interconnection layer forms an effective electrical connection with the second conductive column structure through the first blind hole, and the first conductive column structure forms an effective electrical connection with the wiring interconnection layer.
Citation Information
Cited By
Optical waveguide device based on glass substrate
CN121028281A
An optical waveguide device based on a glass substrate
CN121028281B
Multifunctional photonic device based on glass substrate
CN121028282A
A multifunctional photonic device based on a glass substrate
CN121028282B
Substrate temporary carrier fixing method based on vacuum adsorption