Adsorbent for preserving coffee and preparation method thereof
By using the adsorbents of reduced iron powder, sodium chloride, modified hexacyclic stone powder, modified Jiaoling stone powder and calcium hydroxide particles in coffee packaging, the oxidation caused by oxygen entering coffee beans and coffee powder during packaging is solved. Problem, better freshness and taste protection have been achieved.
Patent Information
- Application Number
- CN202411373560.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-29
- Publication Date
- 2024-11-29
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
During the packaging process, the use of a one-way air-suit valve causes oxygen to enter, resulting in the oxidation of oil and oxidation of odor, affecting the taste. At the same time, the coffee powder is prone to gas and oxidation of oxidation during transportation.
Adopt a coffee preservation adsorbent, including reduced iron powder, sodium chloride, modified hexacyclic stone powder, modified Jiaoling stone powder, calcium hydroxide particles and catalysts, through the combination of these materials, the oxygen in the packaging bag is adsorbed. , carbon dioxide and carbon monoxide prevent water from transferring to coffee, and form an interpenetrating network through the fermentation broth of bacterial cellulose to enhance adsorption capacity.
Effectively remove oxygen and carbon dioxide from packaging bags, prevent oil oxidation, improve the freshness effect of coffee, reduce the oxidation odor of haematozoa, and prolong the transportation stability of coffee powder.
Smart Images

Figure CN119034677A_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the technical field of coffee production, and in particular relates to an adsorbent for coffee preservation and a preparation method thereof. Background Art
[0002] Currently, coffee beans are packaged in aluminum foil bags with one-way air valves. After coffee is roasted, carbon dioxide and carbon monoxide gases are produced, causing the bag to bulge. After using a one-way air valve, although the gas in the bag can be discharged and the pressure can be released, the corresponding oxygen in the air will also enter to a certain extent, causing the oil in the coffee beans to oxidize, and a rancid oxidation smell will appear, affecting the taste. Coffee powder products are currently vacuum-packed after shaping, and need to maintain their square shape during transportation. Coffee powder will also produce gas and oxidative corruption. The present application invents an adsorbent for coffee preservation, which can achieve the goal of no residual oxygen in the bag, and the generated carbon dioxide and carbon monoxide are adsorbed. Summary of the invention
[0003] The present invention provides an adsorbent for coffee preservation, aiming to solve the above-mentioned problem.
[0004] The present invention is implemented as follows: an adsorbent for coffee preservation comprises the following raw materials in parts by weight: 80-100 parts of reduced iron powder, 2-5 parts of sodium chloride, 8-12 parts of modified hexacyclic stone powder, 5-10 parts of modified jiaoling stone powder, 10-20 parts of calcium hydroxide particles, 2-5 parts of catalyst, and 6-12 parts of water.
[0005] Preferably, the following raw materials are included in parts by weight: 85-95 parts of reduced iron powder, 2.5-4.5 parts of sodium chloride, 9-11 parts of modified hexacyclic stone powder, 6-9 parts of modified jiaoling stone powder, 12-18 parts of calcium hydroxide particles, 2.5-4.5 parts of catalyst, and 7-11 parts of water.
[0006] Preferably, the following raw materials are included in parts by weight: 90 parts of reduced iron powder, 3.5 parts of sodium chloride, 10 parts of modified hexacyclic stone powder, 7.5 parts of modified jiaoling stone powder, 15 parts of calcium hydroxide particles, 3.5 parts of catalyst, and 8 parts of water.
[0007] Preferably, the preparation method of the modified hexacyclic stone powder is as follows: take hexacyclic stone, clean the surface, dry it and then perform preliminary crushing; then place it in a muffle furnace and program the temperature to 700-800°C, calcine it at a constant temperature for 1-2 hours, and grind it to a particle size of 200-300 mesh after cooling; then add 25-35vt% hydrochloric acid solution and soak it for 2-3 hours; after filtering, add it to 6-10 times the weight of deionized water, add 10-15wt% vinyltrimethoxysilane solution, and ultrasonically disperse it until it is uniform to obtain a mixture; mix propylene glycol with deionized water; then slowly add it to the mixture, heat it to 60-80°C, stir the reaction for 3-5 hours, and obtain modified hexacyclic stone powder after filtering.
[0008] The variable-valent metal Fe in Liuhuan Stone is prone to redox reactions, which can consume the oxygen in the packaging bag and combine with water molecules in the environment to form a large number of negative ions, which can play a bactericidal role and improve the preservation effect.
[0009] First, the six-ring stone is roasted to remove water in different states in the six-ring stone structure, so that the internal structure becomes loose and porous and the specific surface area is increased. Then, the surface of the six-ring stone is modified by hydrochloric acid corrosion to form a stable porous structure on the surface of the six-ring stone particles. Then, it is modified with polyhydroxy propylene glycol to obtain six-ring stone with a large amount of hydroxyl groups adsorbed inside, on the surface and in the pores. The modified six-ring stone can absorb more water and iron powder, so that the iron powder is under good humidity conditions and fully reacts with oxygen, while preventing moisture from being transferred to coffee.
[0010] Preferably, the mass ratio of glycerol to deionized water is 1:6-10.
[0011] Preferably, the preparation method of the modified jiaoling stone powder is as follows: 15-20 parts of jiaoling stone powder by weight are placed in a closed container, 60-70 parts of hypochlorous acid with a concentration of 10-15% are added, the closed container is pressurized to 1-2atm, heated in a water bath at 30-35°C and a light source is set in the closed container for illumination, fully stirred for 20-30min, depressurized after cooling, filtered and washed with deionized water 2-3 times, dried at 50-60°C, the dried product is placed in a culture vessel and injected with bacterial cellulose fermentation liquid, wrapped, and cultured at 25-30°C for 3-5 days, the culture product is rinsed with deionized water, the residual culture liquid is removed, and it is soaked in deionized water for 3-5h, and finally filtered, dried, and ground to obtain the modified jiaoling stone powder. By adding hypochlorous acid, heating and light, hypochlorous acid decomposes to produce oxygen and hydrochloric acid. Soaking in hydrochloric acid makes the jellyfish porous, impurities in the particle channels are dissolved, the pores are unblocked, and the adsorption capacity is improved. The generated oxygen forms small bubbles, enters the interlayers of the jellyfish, and generates pressure, which makes the wall layer of the jellyfish have a larger space, improves the adsorption capacity, and prevents water from being transferred to the coffee. After absorbing water, the jellyfish expands, providing a larger attachment area for more iron powder to adhere, reducing the accumulation of iron powder. Through the fermentation process, bacterial cellulose grows into the jellyfish to form an interlaced interpenetrating network with a larger water absorption space. The dual effects of adsorption and diffusion of bacterial cellulose are used to provide sufficient water for the iron powder to react with oxygen.
[0012] Preferably, the preparation method of the bacterial cellulose fermentation liquid is as follows: inoculating Gluconacetobacter species into the culture liquid, the temperature is 25-28°C, the stirring speed is 200-240r / min, and the culture time is 24-36h to obtain seed liquid; the seed liquid with a volume of 6-10% of the culture liquid is added to the culture liquid, mixed and set aside, to obtain bacterial cellulose fermentation liquid.
[0013] Preferably, the catalyst is a copper catalyst, which can oxidize and decompose carbon monoxide gas, converting carbon monoxide into carbon dioxide, which is absorbed by calcium hydroxide, further improving the preservation effect of the adsorbent.
[0014] The present invention also provides a method for preparing the above-mentioned adsorbent for coffee preservation, comprising the following steps: Weigh each raw material according to the ratio; The modified hexacyclic stone powder, the modified jiaoling stone powder and the calcium hydroxide particles are uniformly mixed to obtain a mixture A; Mixing reduced iron powder, sodium chloride, calcium hydroxide particles and a catalyst uniformly to obtain a mixture B; Mix the mixture A and the mixture B, then add water, stir and mix evenly, and put the mixture into a packaging bag to obtain the desired adsorbent.
[0015] Preferably, before the mixture A and the mixture B are mixed, the mixture A is evenly spread on the ground electrode in the low-temperature plasma treatment device, and treated for 30-40 minutes under the conditions of power frequency 21-25kHz, working voltage 22-26kV, and discharge power 80-90W; after taking out, 3-5 times the weight of mannitol is added, transferred to an ultrasonic instrument for 40-50 minutes, filtered and dried. After being treated by the low-temperature plasma treatment device, the surface of the mixture A is rougher, the specific surface area is further increased, a three-dimensional network space is formed, and the adsorption is further improved.
[0016] Compared with the prior art, the embodiments of the present application have the following beneficial effects: The coffee preservation adsorbent provided by the present invention can remove oxygen by reducing iron powder to react with oxygen in the packaging bag, can adsorb carbon dioxide gas in the packaging bag by adding calcium hydroxide particles, can oxidize and decompose carbon monoxide gas by adding a catalyst, so that carbon monoxide is converted into carbon dioxide and absorbed by calcium hydroxide, thereby further improving the preservation effect of the adsorbent, and by adding modified hexacyclic stone powder, the variable valence metal Fe in the powder is easy to undergo redox reaction, can consume oxygen in the packaging bag, and combine with water molecules in the environment to form a large number of negative ions, which can play a bactericidal role and improve the preservation effect, can adsorb more water and iron powder, so that the iron powder is in good humidity conditions and fully reacts with oxygen, and also prevents water from being transferred to the coffee, and by adding modified jiaoling stone powder, the adsorption is good, the jiaoling stone expands after absorbing water, and provides a larger attachment area for more iron powder to attach, and bacterial cellulose grows into the jiaoling stone to form a staggered interpenetrating network with a larger water absorption space, and the dual effects of adsorption and diffusion of bacterial cellulose are utilized to provide sufficient water for the iron powder to react with oxygen, and more fully absorb oxygen in the packaging bag, thereby improving the preservation effect. BRIEF DESCRIPTION OF THE DRAWINGS
[0017] Figure 1 This is a flow chart of the preparation of an adsorbent for coffee preservation provided in Examples 1-5 of the present invention.
[0018] Figure 2 This is a flow chart for preparing an adsorbent for coffee preservation provided in Example 6 of the present invention. DETAILED DESCRIPTION
[0019] Unless otherwise defined, all technical and scientific terms used herein have the same meaning as those commonly understood by technicians in the technical field of this application; the terms used in the specification of the application herein are only for the purpose of describing specific embodiments and are not intended to limit this application; the terms "including" and "having" and any variations thereof in the specification and claims of this application and the above-mentioned drawings are intended to cover non-exclusive inclusions. The terms "first", "second", etc. in the specification and claims of this application or the above-mentioned drawings are used to distinguish different objects, not to describe a specific order.
[0020] Reference to "embodiments" herein means that a particular feature, structure, or characteristic described in conjunction with the embodiments may be included in at least one embodiment of the present application. The appearance of the phrase in various locations in the specification does not necessarily refer to the same embodiment, nor is it an independent or alternative embodiment that is mutually exclusive with other embodiments. It is explicitly and implicitly understood by those skilled in the art that the embodiments described herein may be combined with other embodiments.
[0021] Example 1 The embodiment of the present invention provides an adsorbent for coffee preservation, such as Figure 1 As shown, the following raw materials are included in parts by weight: 80 parts of reduced iron powder, 2 parts of sodium chloride, 8 parts of modified Liuhuan stone powder, 5 parts of modified Jiaoling stone powder, 10 parts of calcium hydroxide particles, 2 parts of catalyst, and 6 parts of water. The preparation method thereof comprises the following steps: Weigh each raw material according to the ratio; The modified hexacyclic stone powder, the modified jiaoling stone powder and the calcium hydroxide particles are uniformly mixed to obtain a mixture A; Mixing reduced iron powder, sodium chloride, calcium hydroxide particles and a catalyst uniformly to obtain a mixture B; Mix the mixture A and the mixture B, then add water, stir and mix evenly, and put the mixture into a packaging bag to obtain the desired adsorbent.
[0022] Among them, the preparation method of the modified hexacyclic stone powder is as follows: take hexacyclic stone, clean the surface, dry it and then perform preliminary crushing; then place it in a muffle furnace and program the temperature to 700°C, calcine it at a constant temperature for 1 hour, and grind it to a particle size of 200 mesh after cooling; then add 25vt% hydrochloric acid solution and soak it for 2 hours; after filtering, add it to 6 times the weight of deionized water, add 10wt% vinyltrimethoxysilane solution, and ultrasonically disperse it until it is uniform to obtain a mixture; mix propylene glycol and deionized water in a mass ratio of 1:6; then slowly add it to the mixture, heat it to 60°C, stir the reaction for 3 hours, and obtain modified hexacyclic stone powder after filtering.
[0023] Specifically, the preparation method of the modified Jiaoling stone powder is as follows: 15 parts of Jiaoling stone powder are taken by weight and placed in a closed container, 60 parts of hypochlorous acid with a concentration of 10% are added, the closed container is pressurized to 1atm, heated in a water bath at 30°C and a light source is set in the closed container for illumination, fully stirred for 20 minutes, depressurized after cooling, filtered and washed with deionized water twice, dried at 50°C, the dried product is placed in a culture vessel and injected with bacterial cellulose fermentation liquid, wrapped, and cultured at 25°C for 3 days, the culture product is rinsed with deionized water, the residual culture liquid is removed, and it is soaked in deionized water for 3 hours, and finally filtered, dried, and ground to obtain the modified Jiaoling stone powder.
[0024] Furthermore, the preparation method of the bacterial cellulose fermentation liquid is as follows: inoculate Gluconacetobacter species into the culture liquid, the temperature is 25°C, the stirring speed is 200r / min, and the culture time is 24h to obtain seed liquid; the seed liquid with a volume of 6% of the culture liquid is added to the culture liquid, mixed and set aside, to obtain bacterial cellulose fermentation liquid.
[0025] In this embodiment, the catalyst is a copper catalyst, which can oxidize and decompose carbon monoxide gas, converting carbon monoxide into carbon dioxide, which is absorbed by calcium hydroxide, further improving the preservation effect of the adsorbent.
[0026] Example 2 The embodiment of the present invention provides an adsorbent for coffee preservation, such as Figure 1 As shown, the following raw materials are included in parts by weight: 85 parts of reduced iron powder, 2.5 parts of sodium chloride, 9 parts of modified Liuhuan stone powder, 6 parts of modified Jiaoling stone powder, 12 parts of calcium hydroxide particles, 2.5 parts of catalyst, and 7 parts of water. The preparation method thereof comprises the following steps: Weigh each raw material according to the ratio; The modified hexacyclic stone powder, the modified jiaoling stone powder and the calcium hydroxide particles are uniformly mixed to obtain a mixture A; Mixing reduced iron powder, sodium chloride, calcium hydroxide particles and a catalyst uniformly to obtain a mixture B; Mix the mixture A and the mixture B, then add water, stir and mix evenly, and put the mixture into a packaging bag to obtain the desired adsorbent.
[0027] Among them, the preparation method of the modified hexacyclic stone powder is as follows: take hexacyclic stone, clean the surface, dry it and then perform preliminary crushing; then place it in a muffle furnace and program the temperature to 700°C, calcine it at a constant temperature for 1 hour, and grind it to a particle size of 200 mesh after cooling; then add 25vt% hydrochloric acid solution and soak it for 2 hours; after filtering, add it to 6 times the weight of deionized water, add 10wt% vinyltrimethoxysilane solution, and ultrasonically disperse it until it is uniform to obtain a mixture; mix propylene glycol and deionized water in a mass ratio of 1:6; then slowly add it to the mixture, heat it to 60°C, stir the reaction for 3 hours, and obtain modified hexacyclic stone powder after filtering.
[0028] Specifically, the preparation method of the modified Jiaoling stone powder is as follows: 15 parts of Jiaoling stone powder are taken by weight and placed in a closed container, 60 parts of hypochlorous acid with a concentration of 10% are added, the closed container is pressurized to 1atm, heated in a water bath at 30°C and a light source is set in the closed container for illumination, fully stirred for 20 minutes, depressurized after cooling, filtered and washed with deionized water twice, dried at 50°C, the dried product is placed in a culture vessel and injected with bacterial cellulose fermentation liquid, wrapped, and cultured at 25°C for 3 days, the culture product is rinsed with deionized water, the residual culture liquid is removed, and it is soaked in deionized water for 3 hours, and finally filtered, dried, and ground to obtain the modified Jiaoling stone powder.
[0029] Furthermore, the preparation method of the bacterial cellulose fermentation liquid is as follows: inoculate Gluconacetobacter species into the culture liquid, the temperature is 25°C, the stirring speed is 200r / min, and the culture time is 24h to obtain seed liquid; the seed liquid with a volume of 6% of the culture liquid is added to the culture liquid, mixed and set aside, to obtain bacterial cellulose fermentation liquid.
[0030] In this embodiment, the catalyst is a copper catalyst, which can oxidize and decompose carbon monoxide gas, converting carbon monoxide into carbon dioxide, which is absorbed by calcium hydroxide, further improving the preservation effect of the adsorbent.
[0031] Example 3 The embodiment of the present invention provides an adsorbent for coffee preservation, such as Figure 1 As shown, the raw materials include the following in parts by weight: 90 parts of reduced iron powder, 3.5 parts of sodium chloride, 10 parts of modified Liuhuan stone powder, 7.5 parts of modified Jiaoling stone powder, 15 parts of calcium hydroxide particles, 3.5 parts of catalyst, and 8 parts of water. The preparation method includes the following steps: Weigh each raw material according to the ratio; The modified hexacyclic stone powder, the modified jiaoling stone powder and the calcium hydroxide particles are uniformly mixed to obtain a mixture A; Mixing reduced iron powder, sodium chloride, calcium hydroxide particles and a catalyst uniformly to obtain a mixture B; Mix the mixture A and the mixture B, then add water, stir and mix evenly, and put the mixture into a packaging bag to obtain the desired adsorbent.
[0032] Among them, the preparation method of the modified hexacyclic stone powder is as follows: take hexacyclic stone, clean the surface, dry it and then perform preliminary crushing; then place it in a muffle furnace and program the temperature to 750°C, calcine it at a constant temperature for 1.5 hours, and grind it to a particle size of 200 mesh after cooling; then add 30vt% hydrochloric acid solution and soak it for 2.5 hours; after filtering, add it to 8 times the weight of deionized water, add 12.5wt% vinyltrimethoxysilane solution, and ultrasonically disperse it until it is uniform to obtain a mixture; mix propylene glycol and deionized water in a mass ratio of 1:8; then slowly add it to the mixture, heat it to 70°C, stir the reaction for 4 hours, and obtain modified hexacyclic stone powder after filtering.
[0033] Specifically, the preparation method of the modified jiaoling stone powder is as follows: 17.5 parts of jiaoling stone powder are taken by weight and placed in a closed container, 65 parts of hypochlorous acid with a concentration of 12.5% are added, the closed container is pressurized to 1.5atm, heated in a water bath at 32°C and a light source is set in the closed container for illumination, fully stirred for 25 minutes, depressurized after cooling, filtered and washed twice with deionized water, dried at 55°C, the dried product is placed in a culture vessel and injected with bacterial cellulose fermentation liquid, wrapped, and cultured at 28°C for 4 days, the culture product is rinsed with deionized water, the residual culture liquid is removed, and it is soaked in deionized water for 4 hours, and finally filtered, dried, and ground to obtain the modified jiaoling stone powder.
[0034] Furthermore, the preparation method of the bacterial cellulose fermentation liquid is as follows: inoculate Gluconacetobacter species into the culture liquid, the temperature is 26°C, the stirring speed is 220r / min, and the culture time is 30h to obtain seed liquid; the seed liquid with a volume of 8% of the culture liquid is added to the culture liquid, mixed and set aside to obtain bacterial cellulose fermentation liquid.
[0035] In this embodiment, the catalyst is a copper catalyst, which can oxidize and decompose carbon monoxide gas, converting carbon monoxide into carbon dioxide, which is absorbed by calcium hydroxide, further improving the preservation effect of the adsorbent.
[0036] Example 4 The embodiment of the present invention provides an adsorbent for coffee preservation, such as Figure 1 As shown, the following raw materials are included in parts by weight: 95 parts of reduced iron powder, 4.5 parts of sodium chloride, 11 parts of modified Liuhuan stone powder, 9 parts of modified Jiaoling stone powder, 18 parts of calcium hydroxide particles, 4.5 parts of catalyst, and 11 parts of water. The preparation method thereof comprises the following steps: Weigh each raw material according to the ratio; The modified hexacyclic stone powder, the modified jiaoling stone powder and the calcium hydroxide particles are uniformly mixed to obtain a mixture A; Mixing reduced iron powder, sodium chloride, calcium hydroxide particles and a catalyst uniformly to obtain a mixture B; Mix the mixture A and the mixture B, then add water, stir and mix evenly, and put the mixture into a packaging bag to obtain the desired adsorbent.
[0037] Among them, the preparation method of the modified hexacyclic stone powder is as follows: take hexacyclic stone, clean the surface, dry it and then perform preliminary crushing; then place it in a muffle furnace and program the temperature to 800°C, calcine it at a constant temperature for 2 hours, and grind it to a particle size of 300 mesh after cooling; then add 35vt% hydrochloric acid solution and soak it for 3 hours; after filtering, add it to 10 times the weight of deionized water, add 15wt% vinyltrimethoxysilane solution, and ultrasonically disperse it until it is uniform to obtain a mixture; mix propylene glycol and deionized water in a mass ratio of 1:10; then slowly add it to the mixture, heat it to 80°C, stir and react for 5 hours, and obtain modified hexacyclic stone powder after filtering.
[0038] Specifically, the preparation method of the modified Jiaoling stone powder is as follows: take 20 parts of Jiaoling stone powder by weight and put them in a closed container, add 70 parts of hypochlorous acid with a concentration of 15%, pressurize the closed container to 2atm, heat in a water bath at 35°C and set a light source in the closed container for illumination, stir thoroughly for 30 minutes, release the pressure after cooling, filter and wash with deionized water 3 times, dry at 60°C, put the dried product into a culture vessel and inject bacterial cellulose fermentation liquid, wrap it, and culture it at 30°C for 5 days, rinse the culture product with deionized water, remove the residual culture liquid, soak it with deionized water for 5 hours, and finally filter, dry and grind to obtain the modified Jiaoling stone powder.
[0039] Furthermore, the preparation method of the bacterial cellulose fermentation liquid is as follows: inoculate Gluconacetobacter species into the culture liquid, the temperature is 28°C, the stirring speed is 240r / min, and the culture time is 36h to obtain seed liquid; the seed liquid with a volume of 10% of the culture liquid is added to the culture liquid, mixed and set aside, to obtain bacterial cellulose fermentation liquid.
[0040] In this embodiment, the catalyst is a copper catalyst, which can oxidize and decompose carbon monoxide gas, converting carbon monoxide into carbon dioxide, which is absorbed by calcium hydroxide, further improving the preservation effect of the adsorbent.
[0041] Example 5 The embodiment of the present invention provides an adsorbent for coffee preservation, such as Figure 1As shown, the following raw materials are included in parts by weight: 100 parts of reduced iron powder, 5 parts of sodium chloride, 12 parts of modified Liuhuan stone powder, 10 parts of modified Jiaoling stone powder, 20 parts of calcium hydroxide particles, 5 parts of catalyst, and 12 parts of water. The preparation method thereof comprises the following steps: Weigh each raw material according to the ratio; The modified hexacyclic stone powder, the modified jiaoling stone powder and the calcium hydroxide particles are uniformly mixed to obtain a mixture A; Mixing reduced iron powder, sodium chloride, calcium hydroxide particles and a catalyst uniformly to obtain a mixture B; Mix the mixture A and the mixture B, then add water, stir and mix evenly, and put the mixture into a packaging bag to obtain the desired adsorbent.
[0042] Among them, the preparation method of the modified hexacyclic stone powder is as follows: take hexacyclic stone, clean the surface, dry it and then perform preliminary crushing; then place it in a muffle furnace and program the temperature to 800°C, calcine it at a constant temperature for 2 hours, and grind it to a particle size of 300 mesh after cooling; then add 35vt% hydrochloric acid solution and soak it for 3 hours; after filtering, add it to 10 times the weight of deionized water, add 15wt% vinyltrimethoxysilane solution, and ultrasonically disperse it until it is uniform to obtain a mixture; mix propylene glycol and deionized water in a mass ratio of 1:10; then slowly add it to the mixture, heat it to 80°C, stir and react for 5 hours, and obtain modified hexacyclic stone powder after filtering.
[0043] Specifically, the preparation method of the modified Jiaoling stone powder is as follows: take 20 parts of Jiaoling stone powder by weight and put them in a closed container, add 70 parts of hypochlorous acid with a concentration of 15%, pressurize the closed container to 2atm, heat in a water bath at 35°C and set a light source in the closed container for illumination, stir thoroughly for 30 minutes, release the pressure after cooling, filter and wash with deionized water 3 times, dry at 60°C, put the dried product into a culture vessel and inject bacterial cellulose fermentation liquid, wrap it, and culture it at 30°C for 5 days, rinse the culture product with deionized water, remove the residual culture liquid, soak it with deionized water for 5 hours, and finally filter, dry and grind to obtain the modified Jiaoling stone powder.
[0044] Furthermore, the preparation method of the bacterial cellulose fermentation liquid is as follows: inoculate Gluconacetobacter species into the culture liquid, the temperature is 28°C, the stirring speed is 240r / min, and the culture time is 36h to obtain seed liquid; the seed liquid with a volume of 10% of the culture liquid is added to the culture liquid, mixed and set aside, to obtain bacterial cellulose fermentation liquid.
[0045] In this embodiment, the catalyst is a copper catalyst, which can oxidize and decompose carbon monoxide gas, converting carbon monoxide into carbon dioxide, which is absorbed by calcium hydroxide, further improving the preservation effect of the adsorbent.
[0046] Example 6 The embodiment of the present invention provides an adsorbent for coffee preservation, such as Figure 2 As shown, the raw materials include the following in parts by weight: 90 parts of reduced iron powder, 3.5 parts of sodium chloride, 10 parts of modified Liuhuan stone powder, 7.5 parts of modified Jiaoling stone powder, 15 parts of calcium hydroxide particles, 3.5 parts of catalyst, and 8 parts of water. The preparation method includes the following steps: Weigh each raw material according to the ratio; The modified hexacyclic stone powder, the modified jiaoling stone powder and the calcium hydroxide particles are uniformly mixed to obtain a mixture A; The mixture A was evenly spread on the ground electrode in the low-temperature plasma treatment device, and treated for 350 minutes under the conditions of power frequency of 23kHz, working voltage of 24kV, and discharge power of 85W; after taking it out, 4 times the weight of mannitol was added, and it was transferred to an ultrasonic instrument for 45 minutes, filtered and dried; Mixing reduced iron powder, sodium chloride, calcium hydroxide particles and a catalyst uniformly to obtain a mixture B; The mixture A and the mixture B treated with low temperature plasma are mixed, and then water is added, and the mixture is stirred and mixed evenly, and the mixture is packed into a packaging bag to obtain the desired adsorbent.
[0047] Among them, the preparation method of the modified hexacyclic stone powder is as follows: take hexacyclic stone, clean the surface, dry it and then perform preliminary crushing; then place it in a muffle furnace and program the temperature to 750°C, calcine it at a constant temperature for 1.5 hours, and grind it to a particle size of 200 mesh after cooling; then add 30vt% hydrochloric acid solution and soak it for 2.5 hours; after filtering, add it to 8 times the weight of deionized water, add 12.5wt% vinyltrimethoxysilane solution, and ultrasonically disperse it until it is uniform to obtain a mixture; mix propylene glycol and deionized water in a mass ratio of 1:8; then slowly add it to the mixture, heat it to 70°C, stir the reaction for 4 hours, and obtain modified hexacyclic stone powder after filtering.
[0048] Specifically, the preparation method of the modified jiaoling stone powder is as follows: 17.5 parts of jiaoling stone powder are taken by weight and placed in a closed container, 65 parts of hypochlorous acid with a concentration of 12.5% are added, the closed container is pressurized to 1.5atm, heated in a water bath at 32°C and a light source is set in the closed container for illumination, fully stirred for 25 minutes, depressurized after cooling, filtered and washed twice with deionized water, dried at 55°C, the dried product is placed in a culture vessel and injected with bacterial cellulose fermentation liquid, wrapped, and cultured at 28°C for 4 days, the culture product is rinsed with deionized water, the residual culture liquid is removed, and it is soaked in deionized water for 4 hours, and finally filtered, dried, and ground to obtain the modified jiaoling stone powder.
[0049] Furthermore, the preparation method of the bacterial cellulose fermentation liquid is as follows: inoculate Gluconacetobacter species into the culture liquid, the temperature is 26°C, the stirring speed is 220r / min, and the culture time is 30h to obtain seed liquid; the seed liquid with a volume of 8% of the culture liquid is added to the culture liquid, mixed and set aside to obtain bacterial cellulose fermentation liquid.
[0050] In this embodiment, the catalyst is a copper catalyst, which can oxidize and decompose carbon monoxide gas, converting carbon monoxide into carbon dioxide, which is absorbed by calcium hydroxide, further improving the preservation effect of the adsorbent.
[0051] Comparative Example 1: Compared with Example 3, the modified hexacyclic stone powder is replaced by ordinary hexacyclic stone powder.
[0052] Comparative Example 2: Compared with Example 3, the modified gypsum powder is replaced with ordinary gypsum powder.
[0053] Comparative Example 3: Compared with Example 3, the modified Liuhuan stone powder is replaced by ordinary Liuhuan stone powder and the modified Jiaoling stone powder is replaced by ordinary Jiaoling stone powder.
[0054] Comparative Example 4: A commercially available coffee preservative adsorbent.
[0055] test The deoxygenation and carbon dioxide removal performance tests of the adsorbent are shown in the following table: Test Group Deoxygenation efficiency (mL / g) Carbon dioxide removal efficiency (mL / g) Example 1 25 148 Example 2 26 149 Example 3 24 152 Example 4 23 150 Example 5 27 149 Example 6 20 195 Comparative Example 1 12 122 Comparative Example 2 13 125 Comparative Example 3 12 106 Comparative Example 4 0 210 From the above results, it can be seen that the adsorbent of the present invention has good performance in removing oxygen and carbon dioxide, especially by adding modified hexacyclic stone powder and modified Jiaoling stone powder, the two have a synergistic effect and can enhance the efficiency of assisting reduced iron powder and calcium hydroxide in removing oxygen and carbon dioxide.
[0056] It should be noted that, for the above embodiments, for the sake of simplicity, they are all described as a series of action combinations, but those skilled in the art should know that the present invention is not limited by the described order of actions, because according to the present invention, some steps may be performed in other orders or simultaneously. Secondly, those skilled in the art should also know that the embodiments described in the specification are all preferred embodiments, and the actions and modules involved are not necessarily required by the present invention.
[0057] The above embodiments are only used to illustrate the technical solutions of the present invention, rather than to limit the scope of protection of the invention. Obviously, the described embodiments are only some embodiments of the present invention, rather than all embodiments. Based on these embodiments, all other embodiments obtained by ordinary technicians in this field without making creative work are within the scope of protection of the present invention. Although the present invention has been described in detail with reference to the above embodiments, ordinary technicians in this field can still combine, add, delete or make other adjustments to the features in the various embodiments of the present invention according to the circumstances without conflict, without making creative work, so as to obtain different other technical solutions that do not deviate from the concept of the present invention in essence, and these technical solutions also belong to the scope of protection of the present invention.
Claims
1. An adsorbent for coffee preservation, It is characterized in that The invention comprises the following raw materials in parts by weight: 80-100 parts of reduced iron powder, 2-5 parts of sodium chloride, 8-12 parts of modified hexacyclic stone powder, 5-10 parts of modified jiaoling stone powder, 10-20 parts of calcium hydroxide particles, 2-5 parts of catalyst and 6-12 parts of water.
2. The adsorbent for coffee preservation according to claim 1, It is characterized in that The invention comprises the following raw materials in parts by weight: 85-95 parts of reduced iron powder, 2.5-4.5 parts of sodium chloride, 9-11 parts of modified hexacyclic stone powder, 6-9 parts of modified jiaoling stone powder, 12-18 parts of calcium hydroxide particles, 2.5-4.5 parts of catalyst and 7-11 parts of water.
3. The adsorbent for coffee preservation according to claim 2, It is characterized in that The invention comprises the following raw materials in parts by weight: 90 parts of reduced iron powder, 3.5 parts of sodium chloride, 10 parts of modified hexacyclic stone powder, 7.5 parts of modified jiaoling stone powder, 15 parts of calcium hydroxide particles, 3.5 parts of catalyst and 8 parts of water.
4. The adsorbent for coffee preservation according to claim 1, It is characterized in that The preparation method of the modified hexacyclic stone powder is as follows: take hexacyclic stone, clean the surface, dry it and then perform preliminary crushing; then place it in a muffle furnace and program the temperature to 700-800°C, calcine it at a constant temperature for 1-2 hours, and grind it to a particle size of 200-300 mesh after cooling; then add 25-35vt% hydrochloric acid solution and soak it for 2-3 hours; after filtering, add it to 6-10 times the weight of deionized water, add 10-15wt% vinyltrimethoxysilane solution, and ultrasonically disperse it until it is uniform to obtain a mixture; mix propylene glycol with deionized water; then slowly add it to the mixture, heat it to 60-80°C, stir it for reaction for 3-5 hours, and obtain the modified hexacyclic stone powder after filtering.
5. The adsorbent for coffee preservation according to claim 4, It is characterized in that The mass ratio of the glycerol to the deionized water is 1:6-10.
6. The adsorbent for coffee preservation according to claim 1, It is characterized in that The preparation method of the modified jiaoling stone powder is as follows: 15-20 parts of jiaoling stone powder are taken by weight and placed in a closed container, 60-70 parts of hypochlorous acid with a concentration of 10-15% are added, the closed container is pressurized to 1-2atm, heated in a water bath at 30-35°C and a light source is set in the closed container for illumination, fully stirred for 20-30min, cooled and depressurized, filtered and washed with deionized water for 2-3 times, dried at 50-60°C, the dried product is placed in a culture vessel and injected with bacterial cellulose fermentation liquid, wrapped, and cultured at 25-30°C for 3-5 days, the culture product is rinsed with deionized water, the residual culture liquid is removed, and it is soaked in deionized water for 3-5h, and finally filtered, dried, and ground to obtain the modified jiaoling stone powder.
7. The adsorbent for coffee preservation according to claim 6, It is characterized in that The preparation method of the bacterial cellulose fermentation liquid is as follows: inoculating Gluconacetobacter species into a culture liquid, the temperature is 25-28°C, the stirring speed is 200-240r / min, and the culture time is 24-36h to obtain a seed liquid; the seed liquid with a volume of 6-10% of the culture liquid is introduced into the culture liquid, mixed and set aside, and the bacterial cellulose fermentation liquid is obtained.
8. The adsorbent for coffee preservation according to claim 7, It is characterized in that The catalyst is a copper catalyst.
9. A method for preparing a coffee freshness-keeping adsorbent according to any one of claims 1 to 8, It is characterized in that The steps include: Weigh each raw material according to the ratio; The modified hexacyclic stone powder, the modified jiaoling stone powder and the calcium hydroxide particles are uniformly mixed to obtain a mixture A; Mixing reduced iron powder, sodium chloride, calcium hydroxide particles and a catalyst uniformly to obtain a mixture B; Mix the mixture A and the mixture B, then add water, stir and mix evenly, and put the mixture into a packaging bag to obtain the desired adsorbent.
10. The method for preparing the adsorbent for coffee preservation according to claim 9, It is characterized in that Before mixing mixture A and mixture B, mixture A is evenly spread on the ground electrode in a low-temperature plasma treatment device, and treated for 30-40 minutes under the conditions of power frequency 21-25kHz, working voltage 22-26kV, and discharge power 80-90W; after taking out, 3-5 times the weight of mannitol is added, transferred to an ultrasonic instrument for ultrasonication for 40-50 minutes, filtered and then dried.
Citation Information
Cited By
Method for recycling and recycling calcium fluoride sludge
CN119841342A