Aluminum alloy caliper blank casting mold and casting method

By setting up a shrinkage riser and an S-shaped long runner structure in the aluminum alloy caliper blank casting mold, combined with a rapid cooling system, the problems of bubbles, slag inclusions and cold separators in aluminum alloy caliper casting are solved, and the caliper is loose. Improved the internal quality of the aluminum alloy calipers.

CN119035454APending Publication Date: 2024-11-29HUNAN JIANGBIN MASCH GRP CORP LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411359338.6
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-09-27
Publication Date
2024-11-29

AI Technical Summary

Technical Problem

During the casting of aluminum alloy calipers, too large the runner cross-section and too long the runner lead to bubbles, slag inclusions and cold septum defects inside the calipers, while shrinking the runner may cause loose calipers, which is difficult for the existing technology to solve these problems at the same time.

Method used

An aluminum alloy caliper blank casting mold was designed, including a retractable riser above the middle of the cavity and a runner structure located at both ends of the long direction of the cavity. The cross-section of the long runner is smaller than that of the transverse runner, and an S-shaped structure is used to uniformize it. The liquid aluminum flows and quickly cools the liquid aluminum through the cooling system to avoid reflux and temperature loss.

Benefits of technology

It effectively reduces bubbles, slag inclusions and cold separator defects inside the caliper blank, while avoiding caliper looseness and improving the internal quality of the aluminum alloy caliper.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119035454A_ABST
    Figure CN119035454A_ABST
Patent Text Reader

Abstract

The invention discloses an aluminum alloy caliper blank casting mold and a casting method.The casting mold forms a casting system used for forming an aluminum alloy caliper blank, and the casting system comprises a feeding head located above the middle of a cavity and two pouring gate structures located at the two ends of the cavity in the length direction; each pouring gate structure comprises an inner pouring gate, a transverse pouring gate, a long pouring gate and an outer pouring gate which are sequentially communicated, the inner pouring gates are connected with the cavity, the transverse pouring gates are transversely arranged along the cavity and used for feeding in the blank forming process, the section size of the long pouring gates is smaller than that of the transverse pouring gates, and the outer pouring gates are used for allowing molten aluminum to enter. According to the aluminum alloy caliper blank casting mold and the casting method, the defects of bubbles, cold shut and the like in the caliper blank can be reduced, and the defect of looseness of the caliper cannot be generated.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present application relates to the field of casting technology, and in particular to a casting mold and a casting method for an aluminum alloy caliper blank. Background Art

[0002] Aluminum alloy calipers (such as fixed aluminum alloy calipers on cars) have the function of slowing down the moving wheels and keeping them stopped, and are indispensable safety parts for cars. Aluminum alloy caliper blanks are obtained by casting. Since aluminum alloy calipers are safety parts on cars, the internal quality of the caliper body is required to be high. During casting, defects such as looseness and pores are not allowed inside the caliper to avoid affecting the structural strength of the caliper.

[0003] However, there are several technical problems with the thick and long runners used in current aluminum alloy caliper castings.

[0004] One is that the runner cross section is too large, which causes the aluminum liquid to flow through the runner and fail to fill the runner, which will cause air entrainment in the runner and cause bubble defects in the caliper. However, the runner cross section cannot be reduced, otherwise the runner will not be able to compensate for the caliper's shrinkage enough, causing the caliper to become loose.

[0005] The second is that the runner is too long. The length of the runner is significantly longer than the length of the caliper, which is about 1.5 times the longest dimension of the caliper. The aluminum liquid will continue to accelerate when flowing through the runner. A runner that is too long will cause the aluminum liquid to flow into the caliper too fast. The aluminum liquid flowing too fast will cause air entrainment and oxidation slag defects in the aluminum liquid flowing into the caliper, causing the caliper to be scrapped due to bubbles or slag inclusions. However, the runner length of the existing solution cannot be reduced, otherwise the runner will not be able to compensate for the shrinkage of the caliper enough, causing the caliper to become loose.

[0006] Third, the runner is too long. The aluminum liquid will continue to cool down as it flows through the runner. An overly long runner will cause excessive temperature loss of the aluminum liquid, causing the temperature of the aluminum liquid entering the caliper to be too low, resulting in a cold shut defect in the caliper.

[0007] Therefore, the current aluminum alloy caliper's long runner cross-section is too large and the long runner is too long. Although this is an effective measure to improve the looseness of the caliper, it will cause defects such as bubbles, slag inclusions and cold shuts in the caliper blank.

[0008] Therefore, how to solve the defects such as bubbles, slag inclusions and cold shuts inside the caliper blank without causing loose caliper defects is a technical problem that must be solved at present. Summary of the invention

[0009] In order to solve the above technical problems, the purpose of the present invention is to provide an aluminum alloy caliper blank casting mold and casting method, which can reduce defects such as bubbles and cold shuts inside the caliper blank and will not cause loose caliper defects.

[0010] The technical solution provided by the present invention is as follows: A casting mold for an aluminum alloy caliper blank, the casting mold forming a casting system for molding the aluminum alloy caliper blank, the casting system comprising a shrinkage feeding riser located above the middle of a cavity and two runner structures located at both ends of the cavity in the long direction, each runner structure comprising an inner gate, a cross runner, a long runner, and an outer gate connected in sequence, the inner gate connecting the cavity, the cross runner being arranged transversely along the cavity for shrinkage feeding during the blank molding process, the long runner having a smaller cross-sectional size than the cross runner, and the outer gate for allowing aluminum liquid to enter.

[0011] Preferably, there are multiple feeding risers arranged longitudinally along the cavity.

[0012] Preferably, the casting system further comprises a slag collecting riser located at the outermost protruding portion in the middle of the cavity for compensating shrinkage and accumulating slag.

[0013] Preferably, the long runner is an S-shaped structure, so that the flow speed of the aluminum liquid is more uniform.

[0014] Preferably, it comprises an upper mold, a lower mold and a sand core, wherein the upper mold, the lower mold and the sand core together form a mold cavity and a casting system, and a feeding channel for forming a feeding riser is provided on the upper part of the sand core.

[0015] Preferably, it also includes a pouring cup for placing aluminum liquid, and the pouring cup is fixed to the lower mold.

[0016] Preferably, a positioning structure for positioning on the lower mold is provided at the bottom of the sand core.

[0017] Preferably, it also includes a cooling system, which includes a lower mold cooling water channel, a first upper mold cooling water channel, a second upper mold cooling water channel, and a third upper mold cooling water channel. The second upper mold cooling water channel and the third upper mold cooling water channel are located in the central part of the upper mold, and are used to cool the middle part of the upper model cavity to achieve gradual solidification of the blank from the middle to the outside; the lower mold cooling water channel and the first upper mold cooling water channel are respectively arranged below and above the long runner, and are close to the external gate, and are used to immediately pass water after the casting is completed to quickly cool the molten aluminum in the long runner to prevent the molten aluminum from flowing back from the cavity to the pouring cup.

[0018] A method for casting an aluminum alloy caliper blank adopts the casting mold as described above, and the casting method comprises: fixing a lower mold and opening an upper mold upward; placing a sand core in a lower mold cavity and fixing it; moving an upper mold downward, closing the upper mold with a lower mold, and pressing the sand core with the upper mold cavity to fix the sand core in the mold cavity, and the mold is in a horizontal state at this time; pouring a certain amount of aluminum liquid into a pouring cup; tilting the mold 90 degrees to allow the aluminum liquid to flow into the mold cavity; after the aluminum liquid in the mold cavity is completely solidified, the upper mold moves upward to open the mold, and then the casting is taken out to obtain a caliper blank.

[0019] A casting method for an aluminum alloy caliper blank adopts the casting mold as described above, and the casting method comprises: a lower mold is fixed, and an upper mold is opened upward; a sand core is placed in a lower mold cavity and fixed; an upper mold moves downward, and the upper mold and the lower mold are molded together, and at the same time, the upper mold cavity presses the sand core to fix the sand core in the mold cavity, and the mold is in a horizontal state at this time; a certain amount of aluminum liquid is poured into a pouring cup; the mold is tilted 90 degrees to allow the aluminum liquid to flow into the mold cavity; after the aluminum liquid is filled, water is immediately passed through the cooling water channel of the lower mold and the first upper mold cooling water channel; after the water passing is completed, the mold is reset to a horizontal state, waiting for the aluminum liquid in the mold cavity to solidify; after the aluminum liquid in the mold cavity is solidified, the upper mold moves upward to open the mold, and then the casting is taken out to obtain the caliper blank.

[0020] Compared with the prior art, the aluminum alloy caliper blank casting mold and casting method of the present invention, by setting a feeding riser above the middle of the cavity, the runner structure located at both ends of the cavity in the long direction is provided with a cross runner and a long runner, the cross section of the long runner is smaller than the cross runner, so that the aluminum liquid can fill the long runner to avoid aluminum liquid air entrainment, and the aluminum liquid can quickly flow through the long runner to reduce the temperature loss of the aluminum liquid to avoid the caliper cold shut defect, the feeding riser and the cross runner are used to feed the shrinkage during the blank forming process to avoid the caliper loose defect. Therefore, it can reduce the defects such as bubbles and cold shut inside the caliper blank, and will not cause the caliper loose defect. BRIEF DESCRIPTION OF THE DRAWINGS

[0021] In order to more clearly illustrate the embodiments of the present application or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments recorded in the present application. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.

[0022] Figure 1 This is a schematic structural diagram of a casting mold for an aluminum alloy caliper blank according to an embodiment of the present invention; Figure 2 for Figure 1 A three-dimensional schematic diagram of the cavity and the casting system in the casting mold shown; Figure 3 for Figure 2 A top view of the mold cavity and the gating system shown; Figure 4 for Figure 2 The front view of the cavity and the casting system shown; Figure 5 for Figure 2 A side view of the cavity and the gating system shown; Figure 6 for Figure 2 A three-dimensional schematic diagram of the cavity and casting system in the casting mold and the sand core in the lower mold; Figure 7 for Figure 1 A three-dimensional schematic diagram of a sand core in a casting mold shown; Figure 8 for Figure 7 The schematic diagram of the position of the sand core, the cavity and the casting system is shown; Fig. 9 It is a schematic diagram of the process of casting the aluminum alloy caliper blank according to an embodiment of the present invention. DETAILED DESCRIPTION

[0023] In order to enable those skilled in the art to better understand the technical solutions in this application, the technical solutions in the embodiments of this application will be clearly and completely described below. Obviously, the described embodiments are only part of the embodiments of this application, not all of them. Based on the embodiments in this application, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of this application.

[0024] It should be noted that when an element is referred to as being "fixed on" or "set on" another element, it can be directly on the other element or indirectly set on the other element; when an element is referred to as being "connected to" another element, it can be directly connected to the other element or indirectly connected to the other element.

[0025] It should be understood that the orientation or position relationship indicated by terms such as "length", "width", "up", "down", "front", "back", "left", "right", "vertical", "horizontal", "top", "bottom", "inside" and "outside" are based on the orientation or position relationship shown in the drawings, and are only for the convenience of describing the present application and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore should not be understood as a limitation on the present application.

[0026] In addition, the terms "first" and "second" are used for descriptive purposes only and should not be understood as indicating or implying relative importance or implicitly indicating the number of technical features indicated. Therefore, a feature defined as "first" or "second" may explicitly or implicitly include one or more of the features. In the description of this application, "multiple" and "several" mean two or more, unless otherwise clearly and specifically defined.

[0027] It should be noted that the structures, proportions, sizes, etc. illustrated in the drawings of this specification are only used to match the contents disclosed in the specification for people familiar with this technology to understand and read, and are not used to limit the conditions under which this application can be implemented. Therefore, they have no substantive technical significance. Any structural modification, change in proportional relationship or adjustment of size should still fall within the scope of the technical content disclosed in this application without affecting the effects and purposes that can be achieved by this application.

[0028] like Figures 1 to 8 As shown, an embodiment of the present invention provides an aluminum alloy caliper blank casting mold, which forms a cavity 1 and a casting system 2 for forming the aluminum alloy caliper blank. The cavity 1 is used to form the aluminum alloy caliper blank, and the casting system 2 is used to supply aluminum liquid to flow into the cavity 1 during the blank forming process.

[0029] like Figures 2 to 6 As shown, the casting system 2 includes a feeding riser 21 located above the middle of the cavity 1, a slag collecting riser 22 located at the outermost protruding part of the middle of the cavity 1, and two runner structures symmetrically arranged at both ends of the long direction of the cavity 1. In this embodiment, there are three feeding risers 21 (other numbers may also be used in other embodiments), which are arranged longitudinally along the cavity 1 and are used for feeding during the blank forming process. The slag collecting riser 22 is used for feeding and accumulating slag, that is, feeding the caliper blank and accumulating slag generated when the aluminum liquid flows during the filling.

[0030] Each runner structure includes an inner gate 23, a cross runner 24, a long runner 25, and an outer gate 26 connected in sequence. The inner gate 23 is connected to the cavity 1. The cross runner 24 is arranged horizontally along the cavity 1 and is used to compensate for shrinkage during the blank forming process. The outer gate 26 is used to allow aluminum liquid to enter. The cross-sectional size of the long runner 25 is smaller than that of the cross runner 24 (the cross-sectional diameter of the long runner 25 can be φ15-20mm). The small cross-sectional size can make the aluminum liquid fill the long runner 25 to avoid aluminum liquid entrainment. At the same time, the aluminum liquid can quickly flow through the long runner 25 into the cross runner 24 and then enter the caliper through the inner gate 23 to reduce the temperature loss of the aluminum liquid and avoid the caliper cold shut defect. The long runner 25 is an S-shaped structure, which makes the aluminum liquid flow more uniformly (if it is a straight structure, it is easy to impact the cross runner 24), avoiding the aluminum liquid slag inclusion defect. In this embodiment, the long runner 25 does not compensate the shrinkage of the caliper blank, but the cross runner 24 is used to compensate the shrinkage.

[0031] like Figure 1 As shown, in this embodiment, the casting mold includes an upper mold 3, a lower mold 4, a sand core 5, a pouring cup 6, a cooling system, an upper mold connecting plate 81, an upper mold ejection mechanism 82, a lower mold connecting plate 91, and a lower mold ejection mechanism 92. The upper mold 3, the lower mold 4, and the sand core 5 together form a mold cavity 1 and a casting system 2.

[0032] Combined with Figure 7, Figure 8 As shown, in this embodiment, the sand core 5 is used to form the middle inner end surface of the caliper blank and the internal oil pipe and oil hole and other structures. Three shrinkage channels 51 for forming three shrinkage risers 21 are provided on the upper part of the sand core 5. Since the thermal conductivity of the sand core 5 material is low, which is much lower than that of the metal mold, the aluminum liquid in the shrinkage channel solidifies slowly, which can produce a shrinkage effect on the caliper blank. A positioning structure for positioning on the lower mold is provided at the bottom of the sand core 5. In this embodiment, the positioning structure includes a first positioning protrusion 52 with a circular cross-section and a second positioning protrusion 53 with a square cross-section. The first positioning protrusion 52 and the second positioning protrusion 53 have different shapes, so as to have the function of positioning and preventing errors.

[0033] In this embodiment, the pouring cup 6 is used to place the aluminum liquid and is fixed to the lower mold 4 and is located at the outer gate 26.

[0034] In this embodiment, the cooling system includes a lower mold cooling water channel 71, a first upper mold cooling water channel 72, a second upper mold cooling water channel 73, and a third upper mold cooling water channel 74. The second upper mold cooling water channel 73 and the third upper mold cooling water channel 74 are located in the central part of the upper mold, and are used to cool the middle part of the upper mold cavity 1 to achieve the gradual solidification of the blank from the middle to the outside. The lower mold cooling water channel 71 and the first upper mold cooling water channel 72 are respectively arranged below and above the long runner 25, and are located close to the external gate 26. After the casting is completed, water is immediately passed to quickly cool the aluminum liquid in the long runner 25 to prevent the aluminum liquid from flowing back from the mold cavity 1 to the pouring cup. In other embodiments, the cooling system may also adopt other structures.

[0035] like Fig. 9 As shown, this embodiment also provides a method for casting an aluminum alloy caliper blank, using the casting mold as described above, and the casting method includes: Step 1: fix the lower mold 4 and open the upper mold 3 upwards (such as Fig. 9 (middle S1); Step 2: The sand core 5 is placed and fixed in the lower mold cavity 1 (eg Fig. 9 (S2); Step 3: The upper mold 3 moves downward, and the upper mold 3 and the lower mold 4 are molded together. At the same time, the upper mold cavity 1 presses the sand core 5 to fix the sand core 5 in the mold cavity 1. At this time, the mold is in a horizontal state (such as Fig. 9 (S3); Step 4: Pour a certain amount of aluminum liquid into the pouring cup 6 (such as Fig. 9 in S4); Step 5: Tilt the mold 90° to allow the aluminum liquid to flow into the mold cavity 1 (such as Fig. 9 (S5); Step 6: After the aluminum liquid is filled into the mold, water is immediately passed through the lower mold cooling water channel 71 and the first upper mold cooling water channel 72; Step 7: After the water is passed, the mold is reset to a horizontal state and waits for the aluminum liquid in the mold cavity 1 to solidify (such as Fig. 9 (S6); Step 8: After the aluminum liquid in the mold cavity 1 is solidified, the upper mold 3 moves upward to open the mold, and at the same time, the upper mold ejection mechanism 82 ejects the casting 10 downward, so that the caliper casting 10 remains in the lower mold 4 (such as Fig. 9 (S7); Step 9: The lower die ejection mechanism 92 ejects the casting 10, and then takes out the casting 10 to obtain a caliper blank (such as Fig. 9 (S8).

[0036] The above description of the disclosed embodiments enables one skilled in the art to implement or use the present invention. Various modifications to these embodiments will be apparent to one skilled in the art, and the general principles defined herein may be implemented in other embodiments without departing from the spirit or scope of the present invention. Therefore, the present invention will not be limited to the embodiments shown herein, but rather to the widest scope consistent with the principles and novel features disclosed herein.

Claims

1. A casting mold for an aluminum alloy caliper blank, characterized in that: The casting mold forms a casting system for molding an aluminum alloy caliper blank. The casting system includes a shrinkage feeder located above the middle of the cavity and two runner structures located at both ends of the cavity in the long direction. Each runner structure includes an inner gate, a cross runner, a long runner, and an outer gate that are connected in sequence. The inner gate connects the cavity, and the cross runner is arranged horizontally along the cavity for shrinkage feeding during the blank molding process. The cross-sectional size of the long runner is smaller than that of the cross runner, and the outer gate is used for allowing aluminum liquid to enter.

2. The aluminum alloy caliper blank casting mold according to claim 1, characterized in that: There are a plurality of feeding risers arranged longitudinally along the cavity.

3. The aluminum alloy caliper blank casting mold according to claim 1, characterized in that: The casting system also includes a slag collecting riser located at the outermost protruding part of the middle part of the cavity and used for shrinkage compensation and accumulation of slag.

4. The aluminum alloy caliper blank casting mold according to claim 1, characterized in that: The long runner is an S-shaped structure, which makes the flow speed of the aluminum liquid more uniform.

5. The aluminum alloy caliper blank casting mold according to any one of claims 1 to 4, characterized in that: The mold comprises an upper mold, a lower mold and a sand core, wherein the upper mold, the lower mold and the sand core together form a mold cavity and a casting system, and a shrinkage feeding channel for forming a shrinkage feeding riser is arranged on the upper part of the sand core.

6. The aluminum alloy caliper blank casting mold according to claim 5, characterized in that: It also includes a pouring cup for placing aluminum liquid, and the pouring cup is fixed to the lower mold.

7. The aluminum alloy caliper blank casting mold according to claim 6, characterized in that: The bottom of the sand core is provided with a positioning structure for positioning on the lower mold.

8. The aluminum alloy caliper blank casting mold according to claim 6, characterized in that: It also includes a cooling system, which includes a lower mold cooling water channel, a first upper mold cooling water channel, a second upper mold cooling water channel, and a third upper mold cooling water channel. The second upper mold cooling water channel and the third upper mold cooling water channel are located in the central part of the upper mold, and are used to cool the middle part of the upper model cavity to achieve gradual solidification of the blank from the middle to the outside; the lower mold cooling water channel and the first upper mold cooling water channel are respectively arranged below and above the long runner, and are located close to the external gate, and are used to immediately pass water after the casting is completed to quickly cool the aluminum liquid in the long runner to prevent the aluminum liquid from flowing back from the cavity to the pouring cup.

9. A method for casting an aluminum alloy caliper blank, characterized in that: Using the casting mold as described in claim 6 or 7, the casting method includes: the lower mold is fixed, and the upper mold is opened upward; the sand core is placed in the lower mold cavity and fixed; the upper mold moves downward, and the upper mold and the lower mold are closed, and at the same time the upper mold cavity presses the sand core to fix the sand core in the mold cavity, and the mold is in a horizontal state; a certain amount of aluminum liquid is poured into the pouring cup; the mold is tilted 90° to allow the aluminum liquid to flow into the mold cavity; after the aluminum liquid in the mold cavity is solidified, the upper mold moves upward to open the mold, and then the casting is taken out to obtain a caliper blank.

10. A method for casting an aluminum alloy caliper blank, characterized in that: The casting mold as described in claim 8 is used, and the casting method includes: the lower mold is fixed, and the upper mold is opened upward; the sand core is placed in the lower mold cavity and fixed; the upper mold moves downward, and the upper mold and the lower mold are molded together, and at the same time the upper mold cavity presses the sand core to fix the sand core in the mold cavity, and the mold is in a horizontal state; a certain amount of aluminum liquid is poured into the pouring cup; the mold is tilted 90° to allow the aluminum liquid to flow into the mold cavity; after the aluminum liquid is filled, the lower mold cooling water channel and the first upper mold cooling water channel are immediately passed water; after the water is passed, the mold is reset to a horizontal state, waiting for the aluminum liquid in the mold cavity to solidify; after the aluminum liquid in the mold cavity is solidified, the upper mold moves upward to open the mold, and then the casting is taken out to obtain a caliper blank.