Full-color multifunctional Micro-LED display device and method based on photoetching technology and light source device

Through photolithography technology combined with red, green, and near-infrared quantum dot pixel arrays, the problem of missing high-resolution full-color display and sensing functions of Micro-LED display devices is solved, and high-efficiency full-color display and multi-function integration are achieved , expanding the application scenarios of smart devices.

CN119050243AActive Publication Date: 2024-11-29MINDU INNOVATION LAB

Patent Information

Application Number
CN202411221902.8
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-09-02
Publication Date
2024-11-29
Estimated Expiration
2044-09-02

AI Technical Summary

Technical Problem

The existing Micro-LED display devices lack high-resolution full-color display and sensing functions, and the infrared light source integration cost is high and the conversion efficiency is low, making it difficult to meet the multifunctional needs of smart devices.

Method used

Through photolithography technology, combined with red, green, and near-infrared quantum dot pixel arrays, blue light is converted into red, green, and near-infrared light by using the blue light Micro-LED excitation layer to realize full color display, and integrate facial recognition and physiological parameter detection functions.

Benefits of technology

It realizes high-resolution full-color display, enhances visual experience, and gives the equipment facial recognition and health detection functions, expands application scenarios, and the high efficiency and fine patterning of lithography technology support the manufacturing of high-resolution display devices.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119050243A_ABST
    Figure CN119050243A_ABST
Patent Text Reader

Abstract

The invention discloses a full-color multifunctional Micro-LED display device and method based on the photoetching technology and a light source device, red, green and near-infrared quantum dot pixel arrays are integrated through the photoetching technology, the display effects of high resolution, high color gamut, high contrast and low energy consumption are achieved, and the full-color multifunctional Micro-LED display device further has the additional functions of face recognition and multi-parameter physiological monitoring. The method comprises the steps that a Micro-LED blue light chip array is accurately patterned, quantum dot photoresist is used as a light conversion layer to achieve full-color display, and the touch sensing function and the flexible display function are integrated. By optimizing photoetching process parameters, uniform and fine quantum dot patterns can be formed on the Micro-LED blue light chip array, and color expressive force and energy efficiency are remarkably improved. The preparation method also has the advantages of high cost effectiveness, high production efficiency and high yield.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the fields of display technology and optoelectronic sensor technology, and in particular to a method for forming red, green and near-infrared quantum dot pixel arrays on a blue light Micro-LED chip by photolithography technology, which can not only realize full-color display of Micro-LED, but also integrate multiple functions of facial recognition and detection. In particular, it relates to a full-color multifunctional Micro-LED display device and method based on photolithography technology, and a light source device. Background Art

[0002] With the rapid development of information technology and smart devices, display technology has become an important medium for human-computer interaction. Although commercial display technologies such as liquid crystal (LCD) and organic light-emitting diode (OLED) have made significant progress in brightness and color, they still have problems such as insufficient color saturation and high energy consumption. In addition, with the rapid rise of biosensing technologies such as facial recognition and health monitoring in recent years, the market demand for multifunctional devices that integrate display and sensing functions is increasing.

[0003] As a new generation of display panel technology, Micro-LED has attracted widespread attention due to its many advantages such as high brightness, high color gamut, low energy consumption, and long life. However, it is extremely difficult to grow RGB three-color chips on a large-area epitaxial substrate at the same time. In order to overcome the problem of mass transfer, blue light Micro-LED is usually used as the excitation light source, and the red and green two-color quantum dot pixel array is used as the light conversion layer to convert blue light into red and green light to achieve high-efficiency full-color display. At present, the methods of using quantum dots to form a light conversion layer mainly include nanoimprint technology, inkjet printing technology, and photolithography technology. However, nanoimprint technology has disadvantages such as low processing efficiency, low precision, and uncontrollable transfer. Inkjet printing technology has problems such as easy jitter and clogging of the needle tip, and easy formation of coffee rings of ink droplets. Therefore, photolithography technology is considered to be the most likely solution to achieve large-area, high-efficiency, and high-precision Micro-LED full-colorization. In addition, most of the popular Micro-LED display devices lack sensing functions, which limits their application potential in the field of smart devices.

[0004] Infrared light sources integrated into mobile phone screens have huge application market value, which is mainly reflected in the following aspects: 1. Biometric technology: Infrared light sources are widely used in biometric technology in smartphones, such as security features such as facial recognition and iris recognition, which improves the security and convenience of the device. For example, Apple's iPhone implements FaceID facial recognition technology. 2. Camera system: Infrared light sources can enhance the performance of mobile phone cameras in low-light environments and provide clearer night shooting effects. 3. Data transmission: Infrared light sources are also used in data transmission. For example, infrared communication can be used to transfer files or settings between devices. 4. Medical health monitoring: As health monitoring functions become more and more popular in smartphones, infrared light sources can be used to monitor physiological indicators such as heart rate and blood pressure. The application of infrared light sources is constantly expanding, including consumer electronics including smartphones, smart cockpits / advanced driver assistance systems, autonomous driving, industrial / logistics / home appliance automation and other fields. In summary, the application of infrared light sources in the field of smartphones not only enhances the functions of mobile phones, but also promotes the development of related technologies and the expansion of the market. With the continuous advancement of technology and the growth of market demand, the application value of infrared light sources in the mobile phone market will continue to increase.

[0005] Common infrared light sources generally have the disadvantages of high cost, low conversion efficiency, and large devices that are difficult to integrate into the screen. Summary of the invention

[0006] The present invention combines infrared quantum dots with Micro-LED technology through photolithography technology to overcome the above difficulties. Quantum dots are a type of semiconductor nanomaterials with unique physical and chemical properties. They are usually composed of materials such as II-VI (such as CdSe, CdTe), III-V (such as InP, InAs) or IV-VI (such as PbS, PbSe). The size of quantum dots can range from a few nanometers to tens of nanometers. This tiny size gives them a unique quantum confinement effect. By regulating the size of quantum dots, ultraviolet light or blue light can be converted into different light color emissions from visible light to near infrared. Quantum dots have the characteristics of wide absorption range, adjustable wavelength, high color purity, and high fluorescence efficiency. They have received widespread attention in the fields of biological imaging, detection, backlight display, white light LED, and sensing. Near-infrared quantum dots have high penetration and low autofluorescence background in biological tissues, making them ideal materials for facial recognition and physiological parameter detection.

[0007] The specific implementation scheme of the present invention is as follows: A full-color multifunctional Micro-LED display device based on photolithography technology, the device comprising a blue light Micro-LED excitation layer, a substrate, a quantum dot light conversion layer, a Micro-LED blue light chip, and a protective layer; A substrate is disposed on the blue light Micro-LED excitation layer, and the substrate and the blue light Micro-LED excitation layer form a cavity; a plurality of array-arranged Micro-LED blue light chips are disposed on the blue light Micro-LED excitation layer and are located in the cavity; The quantum dot light conversion layer includes a plurality of array-arranged red light quantum dot pixels, green light quantum dot pixels, and near-infrared light quantum dot pixels; the quantum dot light conversion layer also includes a protective layer; the quantum dot light conversion layer is located on the substrate; The red light quantum dot pixel is used to convert the blue light emitted by the blue light Micro-LED chip array into red light; The green light quantum dot pixel is used to convert the blue light emitted by the blue light Micro-LED chip array into green light; Near-infrared quantum dot pixels are used to convert the blue light emitted by the blue light Micro-LED chip array into near-infrared light; The red light quantum dot pixels, the green light quantum dot pixels, and the near-infrared light quantum dot pixels are encapsulated with an external protective layer, and the protective layer is a colorless and transparent material.

[0008] The present invention also proposes a method for preparing a full-color multifunctional Micro-LED display device based on photolithography technology, and the specific steps of the method are as follows: Step S1: patterning a Micro-LED blue light chip on the Micro-LED excitation layer; Step S2: cleaning the substrate and chemically modifying the surface of the substrate; placing the substrate on the Micro-LED excitation layer so that the Micro-LED blue light chip is located in the cavity formed by the blue light Micro-LED excitation layer and the substrate; Step S3: adding surfactant, inorganic additive and light scattering particles into the photoresist mother solution according to the formula amount, stirring until fully dissolved to obtain the photoresist mother solution containing additives; Step S4: dispersing the red quantum dots in the photoresist mother solution containing the above-mentioned surfactant and inorganic additive according to the formula amount, and dispersing evenly to obtain the red quantum dot photoresist; the same operation steps are followed to obtain the green quantum dot photoresist and the near-infrared quantum dot photoresist; Step S5: coating the red quantum dot photoresist obtained in step S4 on the substrate to obtain a uniformly distributed red quantum dot photoresist film; Step S6: subjecting the red quantum dot photoresist film obtained in step S5 to pre-baking, local exposure, development and post-baking, the red quantum dot photoresist film is solidified to form a quantum dot light conversion layer of red pixel points; repeating the operations of steps S5 and S6 to obtain quantum dot light conversion layers of green and near-infrared pixel points; Step S7: ALD or MOCVD is used to vapor-deposit a water-proof and oxygen-proof inorganic oxide film on the fluorescent material coating to protect the fluorescent material.

[0009] Compared with the prior art, the present invention has the following beneficial effects: In the prior art, the display device of Micro-LED based on blue light chip usually integrates only red and green quantum dots to form a pixel array, which is generally realized by inkjet printing technology. Although this method saves materials and has low cost, its working efficiency is also relatively low. It is only suitable for application in low-resolution display devices and is difficult to meet the needs of high-resolution display. In view of the limitations of the prior art, the present invention proposes a new method for preparing a display device to further expand the application scope of Micro-LED display technology. The present invention innovatively introduces near-infrared quantum dots into the red and green quantum dot light conversion layer of the existing Micro-LED of the blue light chip, and uses advanced photolithography technology to accurately form a red, green and near-infrared three-color pixel array. Through this improvement, the present invention can not only realize full-color display and enhance the visual experience of the display device, but more importantly, the newly introduced near-infrared quantum dots give the display device advanced functions of facial recognition and physiological parameter detection. These additional functions greatly expand the application scenarios of Micro-LED display devices, making them have potential application value in fields such as security authentication and health detection. In addition, compared with inkjet printing technology, photolithography technology has more significant advantages in preparing high-resolution pixel arrays. Photolithography technology can achieve finer patterning with high efficiency and is supported by mature mass production equipment, which is suitable for manufacturing high-resolution display devices. The method for preparing the display device of the present invention not only improves the display quality and adds practical functions by introducing near-infrared quantum dots and adopting photolithography technology, but also ensures high efficiency and low cost of the preparation process, providing a new direction for the development of Micro-LED display technology, and has broad application prospects in the fields of smart terminals, security monitoring, medical health, etc. BRIEF DESCRIPTION OF THE DRAWINGS

[0010] Figure 1 : Schematic diagram of the display device; Figure 2 : Emission spectrum of red quantum dot pixels under 450 nm excitation; Figure 3 : Emission spectrum of green quantum dot pixels under 450 nm excitation; Figure 4 : Emission spectrum of near-infrared quantum dot pixels under 450 nm excitation.

[0011] Among them, 1 is the blue light Micro-LED excitation layer, 2 is the substrate, 3 is the quantum dot light conversion layer, 301 is the red light quantum dot pixel, 302 is the green light quantum dot pixel, 303 is the near-infrared light quantum dot pixel, 4 is the protective layer, and 5 is the Micro-LED blue light chip. DETAILED DESCRIPTION

[0012] The present invention is further described in detail below in conjunction with specific examples. It should be understood that the following examples are only exemplary descriptions and explanations of the present invention, but these examples should not be interpreted as limiting the scope of protection of the present invention. Any modifications, equivalent substitutions, improvements, etc. made within the spirit and principles of the present invention should all be included in the scope of protection of the present invention.

[0013] The present invention proposes a full-color multifunctional Micro-LED display device based on photolithography technology, such as Figure 1 As shown, the device includes a blue light Micro-LED excitation layer 1, a substrate 2, a quantum dot light conversion layer 3, a Micro-LED blue light chip 5, and a protective layer 4.

[0014] A substrate 2 is arranged on the blue light Micro-LED excitation layer 1, and the substrate 2 and the blue light Micro-LED excitation layer 1 form a cavity; a plurality of array-arranged Micro-LED blue light chips 5 are arranged on the blue light Micro-LED excitation layer 1 and are located in the cavity; the structure can effectively improve the luminous efficiency and uniformity of the Micro-LED.

[0015] The blue light Micro-LED excitation layer 1 includes array-arranged blue light Micro-LED chips 5, whose emission wavelength is between 430-470 nm and the chip size is between 1 and 50 μm.

[0016] The substrate 2 may be a hard substrate such as transparent glass or a flexible substrate such as a polyimide film. Before preparing the quantum dot light conversion layer 3 on the substrate 2 , it needs to be cleaned and subjected to ultraviolet ozone treatment.

[0017] The quantum dot light conversion layer 3 includes a plurality of array-arranged red light quantum dot pixels 301, green light quantum dot pixels 302, and near-infrared light quantum dot pixels 303; a protective layer 4 is also disposed on the quantum dot light conversion layer 3; the quantum dot light conversion layer 3 is located on the substrate 2; The red quantum dot pixel 301 is used to convert the blue light emitted by the blue Micro-LED chip array into red light; The green quantum dot pixel 302 is used to convert the blue light emitted by the blue Micro-LED chip array into green light; The near-infrared quantum dot pixel 303 is used to convert the blue light emitted by the blue light Micro-LED chip array into near-infrared light; The red light quantum dot pixel 301 , the green light quantum dot pixel 302 , and the near-infrared light quantum dot pixel 303 are encapsulated with an external protective layer 4 , and the protective layer 4 is a colorless and transparent material.

[0018] The present invention further proposes a method for preparing a full-color multifunctional Micro-LED display device based on photolithography technology, and the specific steps of the method are as follows: Step S1: patterning a Micro-LED blue light chip 5 on a Micro-LED excitation layer 1; Step S2: cleaning the substrate 2 and chemically modifying the surface of the substrate; placing the substrate 2 on the Micro-LED excitation layer 1 so that the Micro-LED blue light chip 5 is located in the cavity formed by the blue light Micro-LED excitation layer 1 and the substrate 2; Step S3: adding surfactant, inorganic additive and light scattering particles into the photoresist mother solution according to the formula amount, stirring until fully dissolved to obtain the photoresist mother solution containing additives; Step S4: dispersing the red quantum dots in the photoresist mother solution containing the above-mentioned surfactant and inorganic additive according to the formula amount, and dispersing evenly to obtain the red quantum dot photoresist; the same operation steps are followed to obtain the green quantum dot photoresist and the near-infrared quantum dot photoresist; Step S5: coating the red quantum dot photoresist obtained in step S4 on the processed substrate 2 to obtain a uniformly distributed red quantum dot photoresist film; Step S6: subjecting the red quantum dot photoresist film obtained in step S5 to pre-baking, local exposure, development and post-baking, the red quantum dot photoresist film is solidified to form a quantum dot light conversion layer of red pixel points; repeating the operations of steps S5 and S6 to obtain quantum dot light conversion layers of green and near-infrared pixel points; Step S7: ALD or MOCVD is used to vapor-deposit a water-proof and oxygen-proof inorganic oxide film on the fluorescent material coating to protect the fluorescent material.

[0019] Furthermore, the photoresist mother solution includes a main resin and a solvent.

[0020] Furthermore, the main resin can be selected from one or more of epoxy resin, acrylic resin, phenolic resin, and polyvinyl cinnamate; the solvent can be selected from one or more of ethylene glycol butyl ether, propylene glycol methyl ether, propylene glycol butyl ether, propylene glycol ethyl ether, dipropylene glycol methyl ether, propylene glycol methyl ether acetate, ethylene glycol ethyl ether acetate, xylene, dimethylformamide, dimethyl sulfoxide, and methyl isobutyl ketone.

[0021] Furthermore, the mass fraction of the quantum dots is 1-30%.

[0022] Furthermore, the green and red quantum dots are one or more of II-VI semiconductor quantum dots, III-V semiconductor quantum dots and perovskite quantum dot materials, wherein the emission wavelength of the red quantum dots is 610-640 nm, and the half-peak width is <40 nm, and the emission wavelength of the green quantum dots is 510-540 nm, and the half-peak width is <40 nm. The near-infrared quantum dots are one or more of II-VI semiconductor quantum dots, III-V semiconductor quantum dots, IV-VI semiconductor quantum dots, I-III-VI semiconductor quantum dots, perovskite quantum dots and carbon quantum dot materials, and their emission wavelength is 800-2000 nm, and the half-peak width is less than 100 nm.

[0023] Furthermore, the mass fraction of the inorganic additive is 0.01-10%.

[0024] Furthermore, the mass fraction of the surfactant is 0.1-2%.

[0025] Furthermore, the mass fraction of the light scattering particles is 0.01-1%.

[0026] Furthermore, the surfactant can be selected from two major categories: nonionic and ionic. Nonionic surfactants usually contain long nonpolar hydrocarbon groups and short polar groups, such as fatty acid polyoxyethylene alcohol esters and polyols. Ionic surfactants include anionic (such as stearates and phosphates), cationic (such as hexadecyl trimethyl ammonium bromide and dodecyl pyridinium hydrochloride) and zwitterionic (such as amino acids, betaine and imidazoline).

[0027] Furthermore, the inorganic additive can be selected from one or more of lithium chloride, magnesium chloride, aluminum chloride, calcium chloride, vanadium chloride, zinc chloride, cadmium chloride, mercuric chloride, lead chloride, lithium bromide, magnesium bromide, aluminum bromide, calcium bromide, zinc bromide, cadmium bromide, calcium nitrate, cadmium nitrate, and silver nitrate.

[0028] Furthermore, the light scattering particles are a mixture of one or more of organic photosilicon, silicon dioxide, and calcium carbonate.

[0029] Furthermore, the exposure light source in step S6 is an ultraviolet light source with a wavelength of 365 nm, 405 nm or 436 nm, and the exposure energy is 50-1500 mJ / cm 2 .

[0030] Furthermore, the development in step S6 is to use a developer to wash away uncured photoresist to form a quantum dot pixel array; the developer is an alkaline reagent selected from but not limited to potassium hydroxide aqueous solution and tetramethylammonium hydroxide aqueous solution; the development time is 5 to 200 s.

[0031] Furthermore, in step S6, the pre-baking treatment is baking at a temperature of 80-110°C for 30-300 s; the post-baking treatment is baking at a temperature of 130-200°C for 10-100 min to further solidify the quantum dot photoresist film; the film thickness of the formed quantum dot light conversion layer is 1-20 μm, and its line width is 1-200 μm.

[0032] Furthermore, the substrate cleaning in step S2 is specifically as follows: placing the substrate in a cleaning agent, isopropanol, ethanol and deionized water in turn, ultrasonically cleaning for 5-10 minutes, blowing the cleaned substrate dry with nitrogen, and baking it in an 80°C oven for 2 hours; placing the treated substrate into the cavity of a UV ozone cleaning machine with a power of 50~300W for 10-30 minutes, further cleaning the surface of the substrate with ultraviolet light and ozone, and chemically modifying the surface of the substrate to improve the hydrophilicity of the substrate.

[0033] The present invention also proposes a full-color multifunctional Micro-LED display device based on photolithography technology, including a blue light Micro-LED substrate, a photoresist mother liquid, red quantum dots, green quantum dots, near-infrared (hereinafter referred to as NIR) quantum dots uniformly dispersed in the photoresist mother liquid, and inorganic additives, surfactants and light diffusers. The surfactant can form a homogeneous system with the quantum dots in the photoresist mother liquid by stirring, thereby improving the polarity of the quantum dots and dispersing them in polar solvent esters commonly used in photoresists, such as PGMEA, to maintain the long-term colloidal stability of the nanoparticles in the photoresist; at the same time, the inorganic additive can be used as a ligand to form coordination with the dangling bonds on the surface of the quantum dots, reduce the surface defects of the quantum dots, and improve the fluorescence efficiency of the quantum dots; in addition, light scattering particles are usually added to the light conversion layer made of the quantum dot photoresist to improve the light cycle of blue light in the conversion layer, increase the absorption of the excitation light by the quantum dots, increase the light conversion efficiency, and improve the color purity of the output light.

[0034] The present invention also proposes a Micro-LED multifunctional colorful display and infrared light source device based on a variety of fluorescent materials. The micro-LED structure includes a driving circuit and a full-color multifunctional Micro-LED display device prepared based on photolithography technology from bottom to top. Specific embodiment 1 Embodiment 1 of the present invention provides a red quantum dot photoresist, which includes a photoresist mother liquor, red quantum dots, inorganic additives, surfactants and light scattering particles uniformly dispersed in the photoresist mother liquor. The solid content of the photoresist is 40%, and it includes a main rubber and a solvent, wherein the main rubber is an acrylic resin and a phenolic resin, and the solvent is propylene glycol encrypted acetate; the red quantum dots are CdSe, with an emission wavelength of 630 nm and a half-peak width of 23 nm, and the mass fraction of the photoresist is 20%; the inorganic additive is magnesium bromide, and the mass fraction of the photoresist is 1%; the surfactant is hexadecyltrimethylammonium bromide, and the mass fraction of the photoresist is 0.5%; the light scattering particles are silicon dioxide, and the mass fraction of the photoresist is 0.05%. Figure 2 As shown, it is the emission spectrum diagram of the red quantum dot pixel under 450 nm excitation of the present invention. Specific embodiment 2 Embodiment 2 of the present invention provides a green quantum dot photoresist, which includes a photoresist mother liquor, green quantum dots, inorganic additives, surfactants and light scattering particles uniformly dispersed in the photoresist mother liquor. The photoresist has a solid content of 40%, and includes a main rubber and a solvent, wherein the main rubber is an acrylic resin and a phenolic resin, and the solvent is propylene glycol encrypted acetate; the green quantum dots are CdSe, with an emission wavelength of 525 nm and a half-peak width of 20 nm, and the mass fraction of the photoresist is 20%; the inorganic additive is magnesium bromide, and the mass fraction of the photoresist is 1%; the surfactant is hexadecyltrimethylammonium bromide, and the mass fraction of the photoresist is 0.5%; the light scattering particles are silicon dioxide, and the mass fraction of the photoresist is 0.05%. Figure 3 Shown is the emission spectrum of green quantum dot pixels under 450 nm excitation. Specific embodiment 3 Embodiment 3 of the present invention provides a near-infrared quantum dot photoresist, which includes a photoresist mother liquor, near-infrared quantum dots, inorganic additives, surfactants and light scattering particles uniformly dispersed in the photoresist mother liquor. The photoresist has a solid content of 40%, and includes a main rubber and a solvent, wherein the main rubber is an acrylic resin and a phenolic resin, and the solvent is propylene glycol encrypted acetate; the near-infrared quantum dots are PbS, with an emission wavelength of 1200 nm and a half-peak width of 70 nm, and the mass fraction of the photoresist is 20%; the inorganic additive is magnesium bromide, and the mass fraction of the photoresist is 1%; the surfactant is hexadecyltrimethylammonium bromide, and the mass fraction of the photoresist is 0.5%; the light scattering particles are silicon dioxide, and the mass fraction of the photoresist is 0.05%. Figure 4As shown, this is the emission spectrum of near-infrared quantum dot pixels under 450 nm excitation.

[0038] A method for preparing a full-color multifunctional Micro-LED display device based on photolithography technology, the specific steps are: Step S1: patterning a Micro-LED blue light chip 5 on the Micro-LED excitation layer 1; Step S2: cleaning the substrate 2 and chemically modifying the surface of the substrate 2; placing the substrate 2 on the Micro-LED excitation layer 1 so that the Micro-LED blue light chip 5 is located in the cavity formed by the blue light Micro-LED excitation layer 1 and the substrate 2; Step S3: adding surfactant, inorganic additive and light scattering particles into the photoresist mother solution according to the formula amount, stirring until fully dissolved to obtain a photoresist mother solution containing additives; Step S4: dispersing the red quantum dots in the photoresist mother solution containing the above-mentioned surfactant and inorganic additive according to the formula amount, and dispersing evenly to obtain the red quantum dot photoresist; the same operation steps are followed to obtain the green quantum dot photoresist and the near-infrared quantum dot photoresist; Step S5: coating the red quantum dot photoresist obtained in step S4 on the blue light Micro-LED substrate to obtain a uniformly distributed red quantum dot photoresist film; Step S6: heat-treat the red quantum dot photoresist film obtained in step S5 at 90°C for 120s; then heat-treat the film at a wavelength of 365 nm and an energy of 200 mJ / cm 2 The photoresist film was exposed to an ultraviolet light source; after the exposure, an aqueous solution of tetramethylammonium hydroxide with a mass fraction of 2.38% was used as a developer for development for 40 s, thereby washing away the uncured photoresist; after the development, the quantum dot photoresist film was placed at 140°C and baked for 30 min for further curing, thereby forming a quantum dot light conversion layer of red pixel dots; the operations of steps S5 and S6 were repeated to obtain quantum dot light conversion layers of green and near-infrared pixel dots; the quantum dot light conversion layer with a red, green and near-infrared three-color pixel array obtained by photolithography had a thickness of 4.3 μm and a line width of 10 μm.

[0039] Step S7: using the ALD method, vapor-deposit a layer of aluminum oxide film on the entire fluorescent material coating as a water-proof and oxygen-proof layer to protect the fluorescent material.

[0040] Furthermore, the wavelength of the Micro-LED blue light chip 5 is 450 nm, and the size of the chip is 20 μm.

[0041] Furthermore, the cleaning of the substrate 2 in step S2 is specifically as follows: placing the glass substrate in a cleaning agent, isopropanol, ethanol and deionized water in turn, ultrasonically cleaning them for 10 minutes respectively, blowing the cleaned substrate dry with nitrogen, and baking it in an oven at 80°C for 2 hours; placing the treated glass substrate in the cavity of an ultraviolet ozone cleaning machine with a power of 100 W for 30 minutes, further cleaning the surface of the glass substrate with ultraviolet light and ozone, and chemically modifying the surface of the glass substrate to improve the hydrophilicity of the glass substrate.

Claims

1. A full-color multifunctional Micro-LED display device based on photolithography technology, It is characterized in that The device includes a blue light Micro-LED excitation layer, a substrate, a quantum dot light conversion layer, a Micro-LED blue light chip, and a protective layer; A substrate is disposed on the blue light Micro-LED excitation layer, and the substrate and the blue light Micro-LED excitation layer form a cavity; a plurality of array-arranged Micro-LED blue light chips are disposed on the blue light Micro-LED excitation layer and are located in the cavity; The quantum dot light conversion layer includes a plurality of array-arranged red light quantum dot pixels, green light quantum dot pixels, and near-infrared light quantum dot pixels; the quantum dot light conversion layer also includes a protective layer; the quantum dot light conversion layer is located on the substrate; The red light quantum dot pixel is used to convert the blue light emitted by the blue light Micro-LED chip array into red light; The green light quantum dot pixel is used to convert the blue light emitted by the blue light Micro-LED chip array into green light; Near-infrared quantum dot pixels are used to convert the blue light emitted by the blue light Micro-LED chip array into near-infrared light; The red light quantum dot pixels, the green light quantum dot pixels, and the near-infrared light quantum dot pixels are encapsulated with an external protective layer, and the protective layer is a colorless and transparent material.

2. The device according to claim 1, It is characterized in that The Micro-LED blue light chip is suitable for a wavelength of 430-470 nm and a chip size between 1 and 50 μm.

3. A method for preparing a full-color multifunctional Micro-LED display device based on photolithography technology, It is characterized in that The specific steps of the method are as follows: Step S1: patterning a Micro-LED blue light chip on the Micro-LED excitation layer; Step S2: cleaning the substrate and chemically modifying the surface of the substrate; placing the substrate on the Micro-LED excitation layer so that the Micro-LED blue light chip is located in the cavity formed by the blue light Micro-LED excitation layer and the substrate; Step S3: adding surfactant, inorganic additive and light scattering particles into the photoresist mother solution according to the formula amount, stirring until fully dissolved to obtain the photoresist mother solution containing additives; Step S4: dispersing the red quantum dots in the photoresist mother solution containing the above-mentioned surfactant and inorganic additives according to the formula amount, and dispersing them evenly to obtain the red quantum dot photoresist; The same operation steps are used to obtain green quantum dot photoresist and near-infrared quantum dot photoresist; Step S5: coating the red quantum dot photoresist obtained in step S4 on the substrate to obtain a uniformly distributed red quantum dot photoresist film; Step S6: subjecting the red quantum dot photoresist film obtained in step S5 to pre-baking, local exposure, development and post-baking, the red quantum dot photoresist film is solidified to form a quantum dot light conversion layer of red pixel points; repeating the operations of steps S5 and S6 to obtain quantum dot light conversion layers of green and near-infrared pixel points; Step S7: ALD or MOCVD is used to vapor-deposit a water-proof and oxygen-proof inorganic oxide film on the fluorescent material coating to protect the fluorescent material.

4. The method according to claim 3, It is characterized in that The photoresist mother liquor comprises a main resin and a solvent; the main resin is selected from one or more of epoxy resin, acrylic resin, phenolic resin, and polyvinyl cinnamate; the solvent is selected from one or more of ethylene glycol butyl ether, propylene glycol methyl ether, propylene glycol butyl ether, propylene glycol ethyl ether, dipropylene glycol methyl ether, propylene glycol methyl ether acetate, ethylene glycol ethyl ether acetate, xylene, dimethylformamide, dimethyl sulfoxide, and methyl isobutyl ketone.

5. The method according to claim 3, It is characterized in that The mass fraction of the quantum dots is 1-30%.

6. The method according to claim 3, It is characterized in that The green and red quantum dots are one or more of II-VI semiconductor quantum dots, III-V semiconductor quantum dots and perovskite quantum dot materials, wherein the emission wavelength of the red quantum dots is 610-640 nm, and the half-peak width is <40 nm; the emission wavelength of the green quantum dots is 510-540 nm, and the half-peak width is <40 nm; the near-infrared quantum dots are one or more of II-VI semiconductor quantum dots, III-V semiconductor quantum dots, IV-VI semiconductor quantum dots, I-III-VI semiconductor quantum dots, perovskite quantum dots and carbon quantum dot materials, and their emission wavelength is 800-2000 nm, and the half-peak width is less than 100 nm.

7. The method according to claim 3, It is characterized in that The mass fraction of the inorganic additive is 0.01-10%.

8. The method according to claim 3, It is characterized in that The mass fraction of the surfactant is 0.1-2%.

9. The method according to claim 3, It is characterized in that The mass fraction of the light scattering particles is 0.01-1%.

10. The method according to claim 3, It is characterized in that The surfactant is selected from two categories: nonionic and ionic; nonionic surfactants contain long nonpolar hydrocarbon groups and short polar groups, preferably fatty acid polyoxyethylene alcohol esters and polyols, and ionic surfactants include anionic surfactants, preferably stearates and phosphates, cationic surfactants, preferably hexadecyltrimethylammonium bromide and dodecylpyridinium hydrochloride, and zwitterionic surfactants, preferably amino acids, betaine and imidazoline.

11. The method according to claim 3, It is characterized in that The inorganic additive is selected from one or more of lithium chloride, magnesium chloride, aluminum chloride, calcium chloride, vanadium chloride, zinc chloride, cadmium chloride, mercuric chloride, lead chloride, lithium bromide, magnesium bromide, aluminum bromide, calcium bromide, zinc bromide, cadmium bromide, calcium nitrate, cadmium nitrate and silver nitrate.

12. The method according to claim 3, It is characterized in that The light scattering particles are a mixture of one or more of organic photosilicon, silicon dioxide and calcium carbonate.

13. The method according to claim 3, It is characterized in that The exposure light source in step S6 is a UV light source with a wavelength of 365 nm, 405 nm or 436 nm, and the exposure energy is 50-1500 mJ / cm 2 .

14. The method according to claim 3, It is characterized in that The development in step S6 is to use a developer to wash away the uncured photoresist to form a quantum dot pixel array; the developer is an alkaline reagent selected from but not limited to a potassium hydroxide aqueous solution and a tetramethylammonium hydroxide aqueous solution; the development time is 5 to 200 s.

15. The method according to claim 3, It is characterized in that In step S6, the pre-baking treatment is baking at a temperature of 80-110°C for 30-300 s; the post-baking treatment is baking at a temperature of 130-200°C for 10-100 min to further solidify the quantum dot photoresist film; the film thickness of the formed quantum dot light conversion layer is 1-20 μm, and its line width is 1-200 μm.

16. The method according to claim 3, It is characterized in that Cleaning the substrate and chemically modifying the substrate surface are specifically as follows: placing the substrate in a cleaning agent, isopropanol, ethanol and deionized water in turn, ultrasonically cleaning for 5-10 minutes, blowing the cleaned substrate dry with nitrogen, and baking it in an 80°C oven for 2 hours; selecting highly transparent glass as the substrate; placing the treated substrate into the cavity of an ultraviolet ozone cleaning machine with a power of 50~300W for 10-30 minutes, further cleaning the substrate surface with ultraviolet light and ozone, and chemically modifying the substrate surface to improve the hydrophilicity of the substrate.

17. A Micro-LED multifunctional colorful display and infrared light source device based on multiple fluorescent materials, It is characterized in that The device comprises, from bottom to top, a driving circuit and a display device according to any one of claims 1 to 2.

Citation Information

Patent Citations

  • Color conversion layer and preparation method and application thereof

    CN113140556A

  • Display device

    CN114628441A

  • Micro-LED full-color display device manufacturing method based on microfluidics and quantum dot photoetching

    CN115986036A

  • Full-Color Display Module with Ultra-Wide Color Gamut

    US20210384254A1

Cited By

  • Micro-LED-based high-confidentiality key system and high-confidentiality key generation and detection method