Lamination preparation method of photovoltaic module
Through the lamination preparation method, the low-temperature solder layer and low-flowability film are used to solve the problem of thermal expansion of welding tape and special-shaped welding tape control in traditional welding processes, and the stable electrical connection and efficient production of photovoltaic modules are achieved.
Patent Information
- Application Number
- CN202411239363.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-05
- Publication Date
- 2024-12-03
AI Technical Summary
In the production process of traditional photovoltaic modules, the thermal expansion and deformation of the welding tape lead to unstable welding, and the direction consistency of the special-shaped welding tape cannot be effectively controlled, resulting in low welding accuracy and dummy welding. Traditional string welding machines are unable to be compatible with special-shaped welding tape and cannot meet the requirements. Serial welding requirements for stacking grid batteries.
By using the lamination preparation method, by setting the inter-chip connecting strips of the low-temperature solder layer on the front of the battery cell, the battery cells are laminated and bonded directly to avoid welding operations, and the low-temperature solder layer is used to form electrical connections during the lamination process. Combined with low-flow film to prevent position deviation, electrical connection is achieved.
It realizes good electrical connections of photovoltaic modules, reduces string welding equipment and processes, reduces thermal impact and false welding risks, and improves the stability and appearance quality of the modules.
Smart Images

Figure CN119069577A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of solar cell modules, and in particular to a lamination preparation method of a photovoltaic module. Background Art
[0002] In the traditional photovoltaic module manufacturing process, the stringing method is: the welding ribbon and the battery cell are placed alternately in sequence, and the length of the welding ribbon is about 2 times the width of the battery cell, so that half of the welding ribbon is on the front of a battery cell and the other half is on the back of the adjacent battery cell, forming a battery string with multiple battery cells and the upper and lower sides (i.e., positive and negative electrodes) connected in series in sequence. The battery string is then transferred to the welding station through the adsorption track. Generally, multiple pressing wires are used to compact the upper and lower welding ribbons and the battery cell, and the welding ribbon is welded to the surface electrode of the battery cell through infrared heating. When welding the welding ribbon to the battery cell, the battery cell is generally placed flat on a flat bearing surface, and the welding ribbon is mainly pressed with the wire mesh perpendicular to the direction of the welding ribbon to contact the battery cell to complete the welding. The pressure points are several scattered points on the welding ribbon. The parts without pressure will not ensure effective contact. When the welding ribbon is heated, it is easy to expand thermally, causing the welding ribbon to bend or deform, and welding cannot be achieved. In addition, in photovoltaic modules, triangular welding ribbons and other special-shaped welding ribbons with optical advantages are increasingly used. In traditional welding processes, it is difficult to ensure the consistency of the direction of triangular welding ribbons and other special-shaped welding ribbons through clamping, transportation, and pressing. It is difficult to ensure that triangular welding ribbons and other special-shaped welding ribbons do not flip over on the entire surface of the battery cell. Therefore, the application of special-shaped welding ribbons, especially ultra-fine special-shaped welding ribbons, requires new welding methods and processes to effectively control the consistency of the orientation of the welding ribbons to achieve effective welding of special-shaped welding ribbons.
[0003] In traditional components, the number of grid lines of battery cells is relatively small. Traditional stringing machines use conventional flat welding strips to connect the positive and negative poles of battery cells to form strings. The disadvantage of traditional processes is that the conventional battery stringing has low precision, and it is easy for the flat welding strip to deviate from the main grid of the battery cell, resulting in white spots and cold soldering. Conventional stringing machines cannot pull out hundreds of welding strips at the same time, and are not compatible with special-shaped welding strips. The number of conductive wires in stacked-grid batteries is large and densely arranged. Conventional stringing machines cannot use conductive strips to connect the positive and negative poles of stacked-grid batteries together, so they can only be made into independent battery units through other stringing methods. With the emergence of cost-reduced stacked-grid batteries, the traditional stringing method of stringing machines can no longer meet the stringing requirements. Summary of the invention
[0004] In order to solve the above technical problems, the present invention provides a lamination preparation method for photovoltaic modules for battery types that cannot be stacked in series using conventional string welding methods due to the increase in the number of main grids / welding strips or the use of special-shaped welding strips or special battery designs. The method of the present invention can replace the traditional welding string method. The present invention does not use string welding, and direct lamination after stacking can achieve good electrical connection of photovoltaic modules.
[0005] In order to achieve the above objectives, the present invention is implemented through the following technical solutions: A lamination preparation method for a photovoltaic module comprises the following steps: S1. Provide a battery cell, wherein both the front and back sides of the battery cell include a plurality of conductive wires, and only the front side of the battery cell has an inter-sheet connecting strip; The inter-sheet connecting strip connects the plurality of conductive wires on the front side of the battery unit; The structure of the inter-chip connecting strip includes an inner conductive connecting strip and a low-temperature solder layer wrapped on the surface of the inner layer; S2, laying a front adhesive film on the front substrate, and stacking the front-side downward swing sheets of the plurality of battery cells on the front adhesive film to form a plurality of columns of stacked parts according to the requirements of the module circuit connection. The swing sheets of two adjacent battery cells in the same column are stacked in a manner that the inter-sheet connecting strip of one battery cell is overlapped on the plurality of conductive wires on the back of another battery cell to form a positive and negative electrode overlap. There is no need to perform welding operations between the stacked battery cells and between the stacked parts like conventional modules, and then directly laying the back adhesive film and the back substrate on the plurality of columns of the stacked parts in sequence to form a module stacking structure; S3. Directly laminating the component stacking structure to bond them into a whole.
[0006] Furthermore, the overlapping width of two adjacent battery cells in the same column in S2 is 0.5-1 mm.
[0007] Furthermore, S2 also includes the operation of fixing two adjacent battery cells in each column of the stacked components with adhesive tape after stacking. The adhesive tape fixation makes the sheets bonded to each other to prevent position deviation when the strings are put into the laminator, so as to ensure the string spacing.
[0008] Furthermore, S2 also includes the operation of pre-fixing each column of the stacked components on the front adhesive film. The stacked components can be pre-fixed on the front adhesive film by using adhesive tape, or the front adhesive film can be softened or partially melted to allow the battery unit to form contact with it and produce a fixing effect during the cooling process.
[0009] Furthermore, the conductive wire is a metal wire, and the cross-sectional shape of the metal wire is one of a triangle, a semicircle, a trapezoid, a rectangle, and a sawtooth; The material of the low temperature solder layer is a conductive solder whose curing temperature or melting point is lower than the lamination processing temperature. The low temperature solder layer is formed by coating a conductive solder, such as conductive glue, silver paste, low temperature solder paste, etc.
[0010] Preferably, the material of the low-temperature solder layer is selected from conductive glue or low-temperature solder paste, the melting point of the low-temperature solder paste is lower than 143°C, and the curing temperature of the conductive glue is lower than 143°C; the coating thickness of the low-temperature solder paste or the conductive glue on the surface of the conductive wire is 100-150μm; preferably, the coating thickness is 110-120μm.
[0011] Furthermore, the front substrate is photovoltaic glass; the back substrate is photovoltaic glass or photovoltaic backplane; The front adhesive film is a multi-layer co-extruded high-transmittance adhesive film or a high-transmittance adhesive film with a pre-crosslinking degree of at least 15%, and the light transmittance of the high-transmittance adhesive film in the 380-1100nm band is ≥91%, and the light transmittance in the 290-380nm band is ≥75%; The back adhesive film is a multi-layer co-extruded high-cutoff adhesive film or a high-cutoff adhesive film with a pre-crosslinking degree of at least 15%, and the light transmittance of the high-cutoff adhesive film in the 380-1100nm band is ≥91%, and the light transmittance in the 290-380nm band is ≤30%; The laying amount of the front film and the back film is 340-450g / ㎡. The front film and the back film are selected as low-fluidity pre-crosslinked films. The heating temperature of lamination can further promote the crosslinking of the film and further reduce the fluidity, which can prevent the conductive wire from being offset or flipped during the lamination process due to the selection of inappropriate high-fluidity films, thereby affecting the electrical connection between the conductive seed layer and the conductive wire of the stacked grid battery. Within the pre-crosslinking degree range, the probability of poor appearance such as no bubbles in the component after lamination is extremely small, and the bonding force to the component after lamination is better, providing a guarantee for the long-term stable use of the component.
[0012] Furthermore, before forming the component stacking structure, a bus bar is placed under the multiple columns of the stacking parts to form a series connection for the multiple columns of the stacking parts. The bus bar is pre-fixed to the multiple columns of the stacking parts, and then electrode wires are led out for connection with an external junction box to complete the circuit.
[0013] Furthermore, after the lamination process, the process also includes installing a junction box, a component frame, and packaging.
[0014] Furthermore, the lamination process is to evacuate the stacked structure of the components for 5-10 minutes, with the lamination temperature set at 145-160° C. and the lamination time set at 5-20 minutes.
[0015] Furthermore, the conductive wires on the front and the conductive wires on the back are staggered. Specifically: the conductive wires on the front and the conductive wires on the back of the same battery cell are staggered; in the same column of stacked parts, the conductive wires on the front and the conductive wires on the back of the adjacent battery cell are staggered. In a column of stacked parts, the conductive wires on the front and the conductive wires on the back are not one-to-one corresponding, but staggered, so that it is convenient to use an inter-sheet connecting strip to connect the conductive wires on the front and the back of two adjacent battery cells to form a positive and negative electrical connection.
[0016] Beneficial technical effects: The present invention does not need to perform series welding on multiple battery cells in advance, but sets a low-temperature solder layer on the surface of the conductive connecting strip on the front edge of the battery cell to form an inter-sheet connecting strip, and stacks the battery cells by swinging the sheets on the laid adhesive film, that is, the swinging sheet stacking method of two adjacent battery cells: the inter-sheet connecting strip of one battery cell is overlapped on multiple conductive wires on the back of another battery cell to form a positive and negative electrode overlap, and the conductive wires on the front and the conductive wires on the back of a column of stacked parts are staggered, so that the conductive wires of two adjacent battery cells are connected to form a positive and negative electrode electrical connection in a subsequent lamination process by using an inter-sheet connecting strip; the stacked battery cells of the present invention do not need to be welded like conventional components, and can be directly laminated, so as to achieve a good electrical connection between the inter-sheet connecting strip and the negative electrode conductive wire, and the electrical connection between each battery cell is achieved through the inter-sheet connecting strip during the lamination process; In addition, direct lamination needs to be combined with the following main points: ① The low-temperature solder layer on the surface of the inter-sheet connecting strip can ensure full contact during the lamination process, and the temperature of the low-temperature conductive material must be lower than the lamination temperature, so that the low-temperature solder layer can be melted by the temperature of the laminator during the lamination process and the individual battery cells can be effectively connected to form an electrical connection; ② The front and back adhesive films use low-fluidity adhesive films to prevent excessive fluidity of the adhesive film from causing positional offset between the sheets and the adhesive film from penetrating between the inter-sheet connecting strip and the negative electrode conductive wire, causing poor welding; prevent positional offset when the string is put into the laminator, fix the battery cells, and pre-fix the stacked parts on the front adhesive film; The present invention can reduce string soldering equipment and typesetting machine equipment, reduce heat effects, hidden cracks, fragments, cold solder joints, battery string sickle bends, etc. caused by string soldering, and reduce the stacking repair process. BRIEF DESCRIPTION OF THE DRAWINGS
[0017] Figure 1 A top view of the front side of the battery unit; Figure 2 is a side view of a battery unit; Figure 3 A schematic diagram of stacking the swing plates to form a stacked component; Figure 4Schematic diagram of the exploded structure of the stack during the lamination preparation process. DETAILED DESCRIPTION
[0018] The following will be combined with the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, rather than all the embodiments. The following description of at least one exemplary embodiment is actually only illustrative and is by no means intended to limit the present invention and its application or use. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0019] Unless otherwise specifically stated, the numerical value set forth in these embodiments does not limit the scope of the present invention. The technology and method known to those of ordinary skill in the relevant art may not be discussed in detail, but in appropriate cases, the technology and method should be considered as a part of the specification. In all examples shown and discussed here, any specific value should be interpreted as being merely exemplary, rather than as a limitation. Therefore, other examples of exemplary embodiments may have different values.
[0020] The experimental methods in the following examples without specifying specific conditions are usually measured in accordance with national standards; if there is no corresponding national standard, the method is carried out in accordance with the general standard requirements or general methods. Example 1
[0021] A lamination preparation method for a photovoltaic module comprises the following steps: S1. Provide a battery cell, the front view of the battery cell is as follows Figure 1 As shown, the side view is as Figure 2 As shown, the battery cell has two surfaces, a front surface of the battery cell and a back surface of the battery cell, both of which include a plurality of conductive wires made of metal materials, and only the front surface of the battery cell has a conductive connecting strip; the conductive wires on the front surface of the battery cell and the conductive wires on the back surface of the battery cell of the same sheet are staggered, which is not shown in the figure; The conductive connecting strip connects the multiple conductive wires on the front side of the battery cell (i.e., the conductive wires and the conductive connecting strip are in a vertical relationship); and the surface of the conductive connecting strip has a low-temperature solder layer, and is named as an inter-sheet connecting strip (i.e., the structure of the inter-sheet connecting strip includes an inner conductive connecting strip and a low-temperature solder layer wrapped on the surface of the inner layer); In this case: the material of the low-temperature solder layer is a low-temperature solder paste with a melting point lower than 143°C. The low-temperature solder paste is coated on the surface of the conductive wire to form a low-temperature solder layer. The coating thickness of the low-temperature solder paste on the surface of the conductive wire is 110-120μm. The cross-sectional shape of the conductive wire is a triangle. S2, according to Figure 4The exploded diagram structure shown forms a component stacking structure: a front adhesive film is laid on the front substrate, and the front-facing downward swing sheets of multiple battery cells are stacked on the front adhesive film according to the component circuit connection requirements to form multiple columns of stacked parts. The swing sheets of two adjacent battery cells are stacked in a manner that the inter-sheet connecting strip of one battery cell (only available on the front of the battery cell) is overlapped on the multiple conductive wires on the back of another battery cell to form a positive and negative overlap. The overlap width of the overlap is 1mm. The structure of the stacking part is as follows Figure 3 As shown, in the actual production process, in the same column of stacked parts: the front conductive wire of one battery cell and the back conductive wire of the adjacent battery cell are staggered (not shown in the figure), so that it is convenient to use an inter-sheet connecting strip to connect two adjacent battery cells to form a positive and negative electrical connection; In order to prevent the positional displacement between the structures of the stacked parts after entering the laminator, the two adjacent battery cells in the formed stacked parts are fixed with tape after being stacked, and the battery cells are bonded to each other by the tape fixing, and the stacked parts are pre-fixed on the front adhesive film. The pre-fixation is performed by tape fixing, and the front adhesive film can also be softened or partially melted to make the battery cells contact with it and produce a fixing effect during the cooling process; Then, multiple columns of stacked parts are connected and soldered using a reflow bar, and then electrode wires are led out for connection to an external junction box, thereby completing the circuit; Then, a back adhesive film and a back substrate are laid directly on the stacked component in sequence to form a component stacking structure; In this case: the front substrate is photovoltaic glass; the back substrate is photovoltaic glass; the front and back adhesive films are both low-fluidity pre-cross-linked adhesive films: The front adhesive film is a high-transmittance adhesive film with a pre-crosslinking degree of at least 15%, and the transmittance in the 380~1100nm band is ≥91%, and the transmittance in the 290~380nm band is ≥75%. Specifically, WE855 high-transmittance EVA adhesive film (Lukang Biochemical Co., Ltd.) is selected; The back film is a high cut-off film with a pre-crosslinking degree of at least 15%, and a transmittance of ≥91% in the 380-1100nm band and a transmittance of ≤30% in the 290-380nm band. Specifically, WE856 high cut-off EVA film (Lukang Biochemical Co., Ltd.) is selected; The laying amount of the front film is 380-420g / ㎡, and the laying amount of the back film is 380-420g / ㎡; S3. The stacked structure of the arranged components is directly laminated. During the lamination process, vacuum is drawn for 7 minutes, and then lamination is performed at 145°C for 12 minutes. During the lamination process, pressure is continuously applied to bond them into a whole. After the lamination process, the process also includes installing a junction box, a component frame, and packaging operations to finally obtain a photovoltaic component. Example 2
[0022] A lamination preparation method for a photovoltaic module comprises the following steps: S1. Provide a battery cell, the front view of the battery cell is as follows Figure 1 As shown, the side view is as Figure 2 As shown, the battery cell has two surfaces, a front surface of the battery cell and a back surface of the battery cell, both of which include a plurality of conductive wires made of metal materials, and only the front surface of the battery cell has a conductive connecting strip; the conductive wires on the front surface of the battery cell and the conductive wires on the back surface of the battery cell of the same sheet are staggered, which is not shown in the figure; The conductive connecting strip connects the multiple conductive wires on the front side of the battery unit (i.e., the conductive wires and the conductive connecting strip are in a vertical relationship); and the surface of the conductive connecting strip has a low-temperature solder layer, and is named as an inter-sheet connecting strip; In this case: the material of the low-temperature solder layer is a conductive adhesive with a curing temperature lower than 143°C. The conductive adhesive is coated on the surface of the conductive wire to form a low-temperature solder layer with a coating thickness of 120μm (greater than or equal to the height of the conductive wire on the back side of 120μm); the cross-sectional shape of the conductive wire is a triangle; S2, according to Figure 4 The exploded diagram structure shown forms a component stacking structure: a front adhesive film is laid on the front substrate, and the front-facing downward swing sheets of multiple battery cells are stacked on the front adhesive film according to the component circuit connection requirements to form multiple columns of stacked parts. The swing sheets of two adjacent battery cells are stacked in a manner that the inter-sheet connecting strip of one battery cell (only available on the front of the battery cell) is overlapped on the multiple conductive wires on the back of another battery cell to form a positive and negative overlap. The overlap width of the overlap is 1mm. The structure of the stacking part is as follows Figure 3 As shown, in the actual production process, in the same column of stacked parts: the front conductive wire of one battery cell and the back conductive wire of the adjacent battery cell are staggered (not shown in the figure), so that it is convenient to use an inter-sheet connecting strip to connect two adjacent battery cells to form a positive and negative electrical connection; In order to prevent the positional displacement between the structures of the stacked parts after entering the laminator, the two adjacent battery cells in the formed stacked parts are fixed with tape after being stacked, and the battery cells are bonded to each other by the tape fixing, and the stacked parts are pre-fixed on the front adhesive film. The pre-fixation is performed by tape fixing, and the front adhesive film can also be softened or partially melted to make the battery cells contact with it and produce a fixing effect during the cooling process; Then, multiple columns of stacked parts are connected and soldered using a reflow bar, and then electrode wires are led out for connection to an external junction box, thereby completing the circuit; Then, a back adhesive film and a back substrate are laid directly on the stacked component in sequence to form a component stacking structure; In this case: the front substrate is photovoltaic glass; the back substrate is photovoltaic glass; the front and back adhesive films are both low-fluidity pre-cross-linked adhesive films: The front film is a multi-layer co-extruded high-transmittance film with a transmittance of ≥91% in the 380~1100nm band and a transmittance of ≥75% in the 290~380nm band. Specifically, WM912 high-transmittance EPE (three-layer co-extruded encapsulation film, Lukang Biochemical Co., Ltd.) is selected; The back film is a multi-layer co-extruded high-cutoff film, and the transmittance in the 380~1100nm band is ≥91%, and the transmittance in the 290~380nm band is ≤30%. The specific choice is WM913 high-cutoff EPE (three-layer co-extruded encapsulation film, Lukang Biochemical Co., Ltd.); The laying amount of the front film is 380-420g / ㎡, and the laying amount of the back film is 360-400g / ㎡; S3. The stacked structure of the arranged components is directly laminated. During the lamination process, vacuum is drawn for 10 minutes, and then lamination is performed at 150° C. for 10 minutes. During the lamination process, pressure is continuously applied to bond them into a whole. After the lamination process, the process also includes installing a junction box, a component frame, and packaging operations to finally obtain a photovoltaic component. Example 3
[0023] A lamination preparation method for a photovoltaic module comprises the following steps: S1. Provide a battery cell, the front view of the battery cell is as follows Figure 1 As shown, the side view is as Figure 2 As shown, the battery cell has two surfaces, a front surface of the battery cell and a back surface of the battery cell, both of which include a plurality of conductive wires made of metal materials, and only the front surface of the battery cell has a conductive connecting strip; the conductive wires on the front surface of the battery cell and the conductive wires on the back surface of the battery cell of the same sheet are staggered, which is not shown in the figure; The conductive connecting strip connects the multiple conductive wires on the front side of the battery unit (i.e., the conductive wires and the conductive connecting strip are in a vertical relationship); and the surface of the conductive connecting strip has a low-temperature solder layer, and is named as an inter-sheet connecting strip; In this case: the material of the low-temperature solder layer is a low-temperature solder paste with a melting point lower than 143°C. The low-temperature solder paste is coated on the surface of the conductive wire to form a low-temperature solder layer. The coating thickness of the low-temperature solder paste on the surface of the conductive wire is 110-120μm. The cross-sectional shape of the conductive wire is a triangle. S2, according to Figure 4The exploded diagram structure shown forms a component stacking structure: a front adhesive film is laid on the front substrate, and the front-facing downward swing sheets of multiple battery cells are stacked on the front adhesive film according to the component circuit connection requirements to form multiple columns of stacked parts. The swing sheets of two adjacent battery cells are stacked in a manner that the inter-sheet connecting strip of one battery cell (only available on the front of the battery cell) is overlapped on the multiple conductive wires on the back of another battery cell to form a positive and negative overlap. The overlap width of the overlap is 1mm. The structure of the stacking part is as follows Figure 3 As shown, in the actual production process, in the same column of stacked parts: the front conductive wire of one battery cell and the back conductive wire of the adjacent battery cell are staggered (not shown in the figure), so that it is convenient to use an inter-sheet connecting strip to connect two adjacent battery cells to form a positive and negative electrical connection; In order to prevent the positional displacement between the structures of the stacked parts after entering the laminator, the two adjacent battery cells in the formed stacked parts are fixed with tape after being stacked, and the battery cells are bonded to each other by the tape fixing, and the stacked parts are pre-fixed on the front adhesive film. The pre-fixation is performed by tape fixing, and the front adhesive film can also be softened or partially melted to make the battery cells contact with it and produce a fixing effect during the cooling process; Then, multiple columns of stacked parts are connected and soldered using a reflow bar, and then electrode wires are led out for connection to an external junction box, thereby completing the circuit; Then, a back adhesive film and a back substrate are laid directly on the stacked component in sequence to form a component stacking structure; In this case: the front substrate is photovoltaic glass; the back substrate is photovoltaic glass; the front and back adhesive films are both low-fluidity pre-cross-linked adhesive films: The front adhesive film is a high-transmittance adhesive film with a pre-crosslinking degree of at least 15%, and a light transmittance of ≥91% in the 380~1100nm band and a light transmittance of ≥75% in the 290~380nm band. The specific choice is TF4N POE adhesive film (Foster); The back film is a multi-layer co-extruded high-cutoff film, and the transmittance in the 380~1100nm band is ≥91%, and the transmittance in the 290~380nm band is ≤30%. The specific choice is WM913 high-cutoff EPE (three-layer co-extruded encapsulation film, Lukang Biochemical Co., Ltd.); The laying amount of the front film is 380-420g / ㎡, and the laying amount of the back film is 360-420g / ㎡; S3. The stacked structure of the arranged components is directly laminated. During the lamination process, vacuum is drawn for 5 minutes, and then lamination is performed at 160° C. for 8 minutes. During the lamination process, pressure is continuously applied to bond them into a whole. After the lamination process, the process also includes installing a junction box, a component frame, and packaging operations to finally obtain a photovoltaic component.
[0024] The photovoltaic modules prepared in the above cases have no appearance and EL defects, and have passed a series of aging tests: TC200, DH1000, TC50+HF10, etc. all meet the IEC61215 standard (TC200: no obvious appearance defects, power attenuation <4%; DH1000: no obvious appearance defects, power attenuation <4%; DH1000+mechanical load: no obvious appearance defects, power attenuation <5%; TC50+HF10: no obvious appearance defects, power attenuation <5%), and the appearance and EL of the modules are not defective after aging. The present invention does not need to form a series of welding, and the electrical connection can be formed by only placing and pre-fixing. The present invention can reduce the equipment for series welding and typesetting machines, reduce the heat impact, hidden cracks, fragments, cold welding, battery string sickle bending, etc. caused by series welding, and reduce the process of stacking and repairing.
[0025] The above description is only a preferred specific implementation manner of the present invention, but the protection scope of the present invention is not limited thereto. Any technician familiar with the technical field can make equivalent replacements or changes according to the technical scheme and inventive concept of the present invention within the technical scope disclosed by the present invention, which should be covered by the protection scope of the present invention.
Claims
1. A lamination preparation method for a photovoltaic module, It is characterized in that The steps include: S1. Provide a battery cell, wherein both the front and back sides of the battery cell include a plurality of conductive wires, and only the front side of the battery cell has an inter-sheet connecting strip; The inter-sheet connecting strip connects the plurality of conductive wires on the front side of the battery unit; The structure of the inter-chip connecting strip includes an inner conductive connecting strip and a low-temperature solder layer wrapped on the surface of the inner layer; S2, laying a front adhesive film on the front substrate, and stacking the front-side downward swing sheets of the plurality of battery cells on the front adhesive film to form a plurality of columns of stacked parts according to the requirements of the module circuit connection, and the swing sheets of the two adjacent battery cells in the same column are stacked in a manner that the inter-sheet connecting strip of one battery cell is overlapped on the plurality of conductive wires on the back of another battery cell to form a positive and negative electrode overlap, without welding, and then directly laying a back adhesive film and a back substrate on the plurality of columns of the stacked parts in sequence to form a module stacking structure; S3. Directly laminating the component stacking structure to bond them into a whole.
2. A lamination preparation method for a photovoltaic module according to claim 1, It is characterized in that The overlapping width of two adjacent battery cells in the same column in S2 is 0.5-1 mm.
3. A lamination preparation method for a photovoltaic module according to claim 2, It is characterized in that S2 also includes the operation of fixing two adjacent battery cells in each column of the stacked components with adhesive tape after stacking them.
4. A lamination preparation method for a photovoltaic module according to claim 2, It is characterized in that S2 also includes the operation of pre-fixing each column of the stacked components on the front adhesive film.
5. A lamination preparation method for a photovoltaic module according to claim 1, It is characterized in that The conductive wire is a metal wire, and the cross-sectional shape of the metal wire is one of a triangle, a semicircle, a trapezoid, a rectangle, and a sawtooth; The material of the low-temperature solder layer is a conductive solder whose curing temperature or melting point is lower than the lamination processing temperature, and the low-temperature solder layer is formed by coating the conductive solder.
6. A lamination preparation method for a photovoltaic module according to claim 5, It is characterized in that The material of the low-temperature solder layer is selected from conductive glue or low-temperature solder paste, the melting point of the low-temperature solder paste is lower than 143°C, and the curing temperature of the conductive glue is lower than 143°C; the coating thickness of the low-temperature solder paste or the conductive glue on the surface of the conductive wire is 100-150μm.
7. A lamination preparation method for a photovoltaic module according to claim 1, It is characterized in that The front substrate is photovoltaic glass; the back substrate is photovoltaic glass or photovoltaic backplane; The front adhesive film is a multi-layer co-extruded high-transmittance adhesive film or a high-transmittance adhesive film with a pre-crosslinking degree of at least 15%, and the light transmittance of the high-transmittance adhesive film in the 380-1100nm band is ≥91%, and the light transmittance in the 290-380nm band is ≥75%; The back adhesive film is a multi-layer co-extruded high-cutoff adhesive film or a high-cutoff adhesive film with a pre-crosslinking degree of at least 15%, and the light transmittance of the high-cutoff adhesive film in the 380-1100nm band is ≥91%, and the light transmittance in the 290-380nm band is ≤30%; The laying amount of the front adhesive film and the back adhesive film is 340-450g / ㎡.
8. A lamination preparation method for a photovoltaic module according to claim 1, It is characterized in that Before forming the component stacking structure, a bus bar is placed under the multiple columns of the stacking components to form a series connection between the multiple columns of the stacking components. The bus bar is pre-fixed to the multiple columns of the stacking components, and then electrode wires are led out for connection with an external junction box to complete the circuit.
9. A lamination preparation method for a photovoltaic module according to claim 1, It is characterized in that After the lamination process, the process also includes installing a junction box, a component frame, and packaging.
10. A lamination preparation method for a photovoltaic module according to any one of claims 1 to 9, It is characterized in that The lamination process is to evacuate the stacked structure of the components arranged for 5-10 minutes, with the lamination temperature set at 145-160° C. and the lamination time being 5-20 minutes.
11. A lamination preparation method for a photovoltaic module according to claim 1, It is characterized in that The conductive threads on the front side and the conductive threads on the back side are staggered.