Synthesis and fluorescence application of platinum compound with precise structure

Through the coordination reaction of platinum compounds with phosphine-containing ligands, the thermal stability and fluorescent performance challenges in supramolecular solid preparation are solved, and high yield and efficient preparation of fluorescent supramolecular materials are achieved, suitable for fluorescent materials and devices.

CN119080844APending Publication Date: 2024-12-06BEIJING UNIV OF CHEM TECH
View PDF 0 Cites 1 Cited by

Patent Information

Application Number
CN202411274714.1
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-09-12
Publication Date
2024-12-06

AI Technical Summary

Technical Problem

In the field of new functional materials, it is challenging to prepare ordered supramolecular solids with novel structures, excellent performance and practical value, especially in the field of luminescent coordination polymers. The existing technology is difficult to predict the microscopic process of chemical reactions, and affects the impact of The thermal stability and fluorescence properties of the material are obtained.

Method used

Using a phosphine-containing platinum compound, the platinum metal atom is coordinated with 2-(dicyclohexylphosphine)biphenyl ligand and chlorine ligand to form a triac-climbic supramolecular system, using methanol and Solvent combination of dichloromethane is controlled to control the reaction conditions to prepare fluorescent supramolecular with high thermal stability and good fluorescent quantum yield.

Benefits of technology

Fluorescent supramolecular compounds with high thermal stability and high fluorescent quantum yields can yield more than 80%. They are suitable for the preparation of fluorescent materials and devices, and the preparation method is simple.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119080844A_ABST
    Figure CN119080844A_ABST
Patent Text Reader

Abstract

The invention discloses synthesis and fluorescence application of a platinum compound with a precise structure, and belongs to the technical field of supramolecular fluorescent materials. The chemical composition of the supramolecule containing the phosphine ligand is Pt1C48H61P2Cl, the supramolecule containing the phosphine ligand is composed of a platinum metal atom, two 2-(dicyclohexylphosphino) biphenyl ligands and a chlorine ligand, and the platinum metal atom is coordinated with P atoms, Cl atoms, C atoms and P atoms respectively; the supramolecule containing the phosphine ligand belongs to a triclinic system, the space group is P-1, the cell parameters are # imgabs 0 # alpha = 85.242 degrees, beta = 81.586 degrees, gamma = 89.594 degrees and # imgabs 1 #, a solid sample of the ordered supramolecular compound prepared by the method provided by the invention exists stably, the ordered supramolecular compound has high thermal stability and good fluorescence quantum yield, the yield can reach 80% or above, the preparation method is simple, the cost is low, and the preparation method is suitable for industrial production. The method is suitable for preparing fluorescent materials and devices.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of supramolecular fluorescent materials, and in particular to the synthesis and fluorescent application of a platinum compound with precise structure. Background Art

[0002] In the field of new functional materials, metal-organic coordination supramolecular materials based on metal salts and multifunctional organic molecules are driven by not only coordination bonds, but also a variety of interactions such as hydrogen bonds, π···π stacking, and van der Waals forces. The spatial structure of supramolecular materials is complex and diverse, which determines their rich, diverse, and excellent physical and chemical properties. From the perspective of preparation, since there are many conditions and factors that affect the microscopic process of chemical reactions, the periodic arrangement and spatial geometric orientation of crystalline materials during their formation have been difficult to predict so far. Therefore, it is a challenging task to prepare functional ordered supramolecular solids with novel structures, excellent performance, and certain practical value.

[0003] Luminescent coordination polymers have received increasing attention in recent years because they can be widely used in optoelectronic devices, fluorescent sensors, fluorescent probes, etc. Compared with pure organic ligands, coordination polymer materials show better thermal stability and low solubility. At the same time, the coordination between metals and ligands can also affect the luminescent properties of organic molecules, which has broad research value. Summary of the invention

[0004] The purpose of the present invention is to provide a synthesis and fluorescence application of a platinum compound with precise structure to solve the above-mentioned problems in the background technology. The ordered supramolecular compound prepared by the method provided by the present invention has a stable solid sample, high thermal stability and good fluorescence quantum yield, the yield of which can reach more than 80%, and the preparation method is simple, which is suitable for preparing fluorescent materials and devices.

[0005] To achieve the above object, the present invention provides the following technical solutions:

[0006] One of the technical solutions of the present invention is to provide a supramolecule containing a phosphine ligand, wherein the chemical composition of the supramolecule containing a phosphine ligand is Pt 1 C 48 H 61 P 2 Cl, composed of a platinum metal atom, two 2-(dicyclohexylphosphino)biphenyl ligands, and a chlorine ligand, the platinum metal atom is coordinated with P, Cl, C, and P atoms respectively; the supramolecule containing the phosphine ligand belongs to the triclinic system, the space group is P-1, and the unit cell parameters are α=85.242°, β=81.586°, γ=89.594°,

[0007] In the crystal structure of the supramolecular containing phosphine ligand, Pt 1 ···C 1 Distance is about Pt 1 ···Cl 1 Distance is about Pt 1 ···P 1 Distance is about Pt 1 ···P 2 Distance is about

[0008] The second technical solution of the present invention is to provide a method for preparing the supramolecule containing the phosphine ligand, wherein the supramolecule is prepared by platinum salt, 2-(dicyclohexylphosphino)biphenyl (C 24 H 31 P) was used as raw material and prepared by one-pot method.

[0009] Preferably, the method for preparing the supramolecule containing phosphine ligands comprises the following steps:

[0010] Dissolving 2-(dicyclohexylphosphino)biphenyl in dichloromethane to obtain a ligand solution;

[0011] Platinum salt and methanol are mixed to obtain a platinum salt solution, and then a ligand solution is added to obtain a precursor solution, react, and separate the solid and liquid to obtain the supramolecule containing the phosphine ligand;

[0012] The platinum salt is chloroplatinic acid hexahydrate (H 2 PtCl 6 .6H 2 O); the structural formula of the 2-(dicyclohexylphosphino)biphenyl is as follows:

[0013]

[0014] Preferably, the solid-liquid separation further includes washing and drying steps, and the washing includes washing with dichloromethane.

[0015] Preferably, the molar ratio of the platinum salt to 2-(dicyclohexylphosphino)biphenyl in the precursor solution is 1:2-1:4.

[0016] Preferably, the volume ratio of methanol to dichloromethane in the precursor solution is 6:1-7:1.

[0017] The inventors have found through testing that in the reaction system of the present invention, when methanol is used alone as a solvent, the solubility of the raw material is very low, and when dichloromethane is used alone as a solvent, the reaction is affected due to the excessively fast volatilization rate during the reaction. Therefore, the present invention designs a solvent solution that is more suitable for the present invention by limiting the simultaneous addition of methanol and dichloromethane and limiting the addition amounts of the two.

[0018] Preferably, the reaction temperature is 50-120° C. and the reaction time is 3-8 h.

[0019] The third technical solution of the present invention is to provide an application of the above-mentioned supramolecule containing phosphine ligand in the field of fluorescent materials.

[0020] The beneficial technical effects of the present invention are as follows:

[0021] The fluorescent supramolecular compound containing phosphine ligands provided by the present invention forms supramolecular aggregates through abundant hydrogen bond interactions between coordinated molecules. The present invention provides a novel synthesis method of platinum-based fluorescent supramolecular solid compounds, which forms molecules through Pt-C, Pt-Cl and Pt-P coordination bonds, and through abundant CH···Cl and CH···π, the obtained molecules form a two-dimensional supramolecular polymerization network.

[0022] The ordered supramolecular compound prepared by the method provided by the present invention has a stable solid sample, high thermal stability and good fluorescence quantum yield, the yield of which can reach more than 80%, and the preparation method is simple, suitable for preparing fluorescent materials and devices. The crystalline sample exhibits brighter yellow fluorescence under ultraviolet light; the yellow fluorescence emission peak wavelength is at 564nm, and the fluorescence quantum yield is 26.83%. BRIEF DESCRIPTION OF THE DRAWINGS

[0023] In order to more clearly illustrate the embodiments of the present invention or the technical solutions in the prior art, the drawings required for use in the embodiments will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.

[0024] Figure 1 It is the ultraviolet absorption spectrum of the product of Example 1.

[0025] Figure 2 The X-ray powder diffraction pattern of the product in Example 1 is shown in FIG.

[0026] Figure 3 This is the infrared spectrum of the product of Example 1.

[0027] Figure 4 This is a perspective view of the coordination structure of the product of Example 1.

[0028] Figure 5 This is a hydrogen bonding perspective diagram of the product of Example 1.

[0029] Figure 6 This is a perspective view of the two-dimensional supramolecular network of the product of Example 1.

[0030] Figure 7 This is the room temperature solid-state fluorescence spectrum of the product of Example 1.

[0031] Figure 8 This is the fluorescence lifetime diagram of the product of Example 1. DETAILED DESCRIPTION

[0032] Now, various exemplary embodiments of the present invention are described in detail, and this detailed description should not be considered as a limitation of the present invention, but should be understood as a more detailed description of certain aspects, characteristics and embodiments of the present invention. It should be understood that the terms described in the present invention are only for describing specific embodiments and are not used to limit the present invention.

[0033] In addition, for the numerical range in the present invention, it is understood that each intermediate value between the upper and lower limits of the range is also specifically disclosed. The intermediate value in any stated value or stated range, and each smaller range between any other stated value or intermediate value in the range is also included in the present invention. The upper and lower limits of these smaller ranges can be independently included or excluded in the scope.

[0034] Unless otherwise specified, all technical and scientific terms used herein have the same meaning as commonly understood by those skilled in the art to which the invention pertains. Although only preferred methods and materials are described herein, any methods and materials similar or equivalent to those described herein may also be used in the practice or testing of the present invention.

[0035] The words “include,” “including,” “have,” “contain,” etc. used in the present invention are open-ended terms, meaning including but not limited to.

[0036] The present invention provides a method for preparing a fluorescent supramolecule containing a phosphine ligand:

[0037] Mixing 0.1 mol of chloroplatinic acid hexahydrate with 14-30 mL of methanol to obtain a first solution;

[0038] Mix 0.3 mol of 2-(dicyclohexylphosphino)biphenyl with 2-5 mL of dichloromethane to obtain a second solution;

[0039] The first solution and the second solution were placed in a 25 mL polytetrafluoroethylene liner and sealed in a stainless steel reactor sleeve. The reactor was placed in an electric blast oven and heated to 50-120°C. After reacting for 3-8 hours, the mixture was naturally cooled to room temperature. The solid-liquid separation was then performed by centrifugation. The solid product was collected and dried in a 60°C electric blast oven to obtain a fluorescent supramolecule containing a phosphine ligand.

[0040] The present invention performs an X-ray single crystal diffraction test on the final product to analyze its precise electronic structure; and performs a series of characterizations such as infrared, X-ray powder diffraction, and fluorescence on the final product to determine that its chemical composition is Pt 1 C 48 H 61 P 2 Cl. With H 2 PtCl 6 .6H 2 The yield is calculated based on the amount of O used, that is, the mass of the coordination supramolecule that should be obtained theoretically is calculated according to the proportion of the substance amount of Pt in the product composition, and the ratio of the actual product mass to the former is the yield.

[0041] The "room temperature" in the present invention is 10-30°C unless otherwise specified.

[0042] All raw materials used in the following examples and comparative examples of the present invention are commercially available products.

[0043] Example 1

[0044] A method for preparing fluorescent supramolecules containing phosphine ligands:

[0045] Mix 0.1 mol of chloroplatinic acid hexahydrate with 15 mL of methanol to obtain a first solution;

[0046] Mix 0.3 mol of 2-(dicyclohexylphosphino)biphenyl with 5 mL of dichloromethane to obtain a second solution;

[0047] The first solution and the second solution were placed in a 25 mL polytetrafluoroethylene liner and sealed in a stainless steel reactor sleeve. The reactor was placed in an electric blast oven and heated to 60°C. After reacting for 6 hours, it was naturally cooled to room temperature. Then, solid-liquid separation was performed by centrifugation, and the solid product was collected and placed in a 60°C electric blast oven for drying to obtain a fluorescent supramolecule containing a phosphine ligand (the theoretical mass of the product should be 93.045 mg, and the actual mass of the product is 75 mg).

[0048] Effect verification

[0049] (1) Test the prepared crystal sample using a UV-visible spectrophotometer. The test results are as follows: Figure 1 shown.

[0050] Figure 1 It is the ultraviolet absorption spectrum of the product of Example 1.

[0051] Figure 1 In the figure, the horizontal axis represents wavelength and the vertical axis represents intensity.

[0052] Depend on Figure 1 It can be seen that the sample has an obvious absorption peak at 375nm.

[0053] (2) The prepared crystal samples were subjected to powder diffraction test using an X-ray diffractometer. The test results are as follows: Figure 2 shown.

[0054] Figure 2 The X-ray powder diffraction pattern of the product in Example 1 is shown in FIG.

[0055] Figure 2 In the figure, the horizontal axis represents the angle and the vertical axis represents the diffraction intensity.

[0056] Depend on Figure 2 It can be seen that the peaks of the test spectrum match well with the peaks of the crystal structure simulation spectrum (software diamond), indicating that the structure of the obtained crystalline sample is the same as the structure obtained from the single crystal data and the sample has high purity.

[0057] (3) Determination of single crystal structure: Select appropriate single crystals, test them on a single crystal diffractometer, and collect X-ray diffraction data at low temperature. The main crystallographic data are shown in Table 1.

[0058] Table 1 Main crystallographic data

[0059]

[0060] (4) FT-IR spectrometer with KBr as base at 400-4000cm -2 Infrared spectrum test is carried out within the range. The test results are as follows Figure 3 shown.

[0061] Figure 3 This is the infrared spectrum of the product of Example 1.

[0062] Figure 3 In the figure, the horizontal axis represents the wave number and the vertical axis represents the transmittance.

[0063] (5) From the crystal samples obtained in Example 1, suitable single crystals were selected, and X-ray single crystal diffraction data were collected and analyzed to obtain the crystal structure of the supramolecular polymer (see Figure 6 ). In its coordination structure ( Figure 4), with Pt atoms coordinated to P, Cl, C, and P atoms, respectively. The perspective view shows that these Pt complexes adopt a distorted planar geometry, in which the platinum and chlorine atoms are coplanar with the carbon atoms of 2-(dicyclohexylphosphino)biphenyl.

[0064] Figure 4 This is a perspective view of the coordination structure of the product of Example 1.

[0065] Figure 5 This is a hydrogen bonding perspective diagram of the product of Example 1.

[0066] Figure 6 This is a perspective view of the two-dimensional supramolecular network of the product of Example 1.

[0067] Through the strong hydrogen bonds between CH···Cl molecules, Pt 1 C 48 H 61 P 2 Cl forms a two-dimensional supramolecular network. Further, through these strong hydrogen bonds and π···π interactions, a three-dimensional supramolecular aggregate is finally woven. Coordination bonds, hydrogen bonds, and π···π interactions enhance the thermal stability of the supramolecular system. The above characteristics lay a material foundation for the further application of the supramolecular containing phosphine ligands of the present invention.

[0068] (6) The fluorescence properties of the supramolecular crystalline sample prepared in Example 1 were tested at room temperature under ultraviolet light (364 nm). Figure 7-8 shown.

[0069] Figure 7 This is the room temperature solid-state fluorescence spectrum of the product of Example 1.

[0070] Figure 7 In the figure, the horizontal axis represents the wavelength and the vertical axis represents the fluorescence intensity.

[0071] Figure 8 This is the fluorescence lifetime diagram of the product of Example 1.

[0072] Figure 7-8 It shows that under 364nm light excitation, the sample exhibits brighter yellow fluorescence, the yellow fluorescence emission peak wavelength is at 564nm, the fluorescence quantum yield is 26.83%, and the fluorescence lifetime is 50.26μs. Good thermal stability and fluorescence properties show that the new substance of the present invention has good application prospects in fluorescent materials and devices.

[0073] The embodiments described above are only descriptions of the preferred modes of the present invention, and are not intended to limit the scope of the present invention. Without departing from the design spirit of the present invention, various modifications and improvements made to the technical solutions of the present invention by ordinary technicians in this field should all fall within the protection scope determined by the claims of the present invention.

Claims

1. A supramolecule containing a phosphine ligand, characterized in that: The chemical composition of the supramolecular containing phosphine ligand is Pt1C 48 H 61 P2Cl, composed of a platinum metal atom, two 2-(dicyclohexylphosphino)biphenyl ligands, and a chlorine ligand, the platinum metal atom is coordinated with P, Cl, C, and P atoms respectively; The supramolecule containing phosphine ligands belongs to the triclinic system, the space group is P-1, and the unit cell parameters are α=85.242°, β=81.586°, γ=89.594°, 2. A method for preparing a supramolecule containing a phosphine ligand according to claim 1, characterized in that: The supramolecule is prepared by a one-pot method using platinum salt and 2-(dicyclohexylphosphino)biphenyl as raw materials.

3. The preparation method according to claim 2, characterized in that: The following steps are involved: Dissolving 2-(dicyclohexylphosphino)biphenyl in dichloromethane to obtain a ligand solution; Platinum salt and methanol are mixed to obtain a platinum salt solution, and then a ligand solution is added to obtain a precursor solution, react, and separate the solid and liquid to obtain the supramolecule containing the phosphine ligand; The platinum salt is chloroplatinic acid hexahydrate.

4. The preparation method according to claim 3, characterized in that: The molar ratio of the platinum salt to 2-(dicyclohexylphosphino)biphenyl in the precursor solution is 1:2-1:

4.

5. The preparation method according to claim 3, characterized in that: The volume ratio of methanol to dichloromethane in the precursor solution is 6:1-7:

1.

6. The preparation method according to claim 3, characterized in that: The reaction temperature is 50-120°C and the reaction time is 3-8h.

7. Use of the supramolecule containing phosphine ligands according to claim 1 in the field of fluorescent materials.

Citation Information

Cited By

  • Fluorescent silver-platinum nano-cluster material as well as preparation method and application thereof

    CN119735620A