Yellow plastic color master batch
By configuring plastic materials with specific weight components, the existing yellow plastic masterbatches have been solved, and the yellow plastic masterbatches with high color concentration, flame retardancy and oxidation resistance are achieved to meet market demand.
Patent Information
- Application Number
- CN202411957096.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-12-29
- Publication Date
- 2025-03-21
AI Technical Summary
The existing yellow plastic masterbatches have poor color concentration, flame retardancy and oxidation resistance, which cannot meet market demand.
Yellow plastic masterbatches with high color concentration, flame retardant and antioxidant are prepared by configuring specific weight components of ABS terpolymer, polyethylene low molecular wax, vinyl bisstearamide, zinc stearate, titanium dioxide, iron oxide yellow, macromolecular yellow, permanent yellow, flame retardant and antioxidant.
It significantly improves the color concentration, flame retardancy and oxidation resistance of plastics, meeting the market demand for these properties.
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of plastic masterbatches, in particular to yellow plastic masterbatches. Background Art
[0002] The existing yellow plastic masterbatch has poor color concentration, poor flame retardancy and antioxidant properties, and cannot meet market requirements. It is urgent to develop a plastic masterbatch with high yellow color concentration, good flame retardancy and antioxidant properties to meet market demand and improve product adaptability. Summary of the invention
[0003] The purpose of the invention is to provide a yellow plastic masterbatch to solve the technical problems of poor color concentration, flame retardancy and oxidation resistance of traditional yellow plastic masterbatch.
[0004] To achieve the above purpose, the present invention provides the following technical scheme: comprising the following components by weight: 880-960 parts of ABS terpolymer, 20-40 parts of polyethylene low molecular weight wax, 5-15 parts of vinyl bisstearamide, 5-15 parts of zinc stearate, 20-40 parts of titanium dioxide, 1-5 parts of iron oxide yellow, 1-5 parts of macromolecular yellow, 1-5 parts of permanent yellow, 1-5 parts of flame retardant, and 1-5 parts of antioxidant. ABS is a terpolymer of three monomers: acrylonitrile (A), butadiene (B), and styrene (S).
[0005] Furthermore, 900-940 parts of ABS terpolymer, 25-35 parts of polyethylene low molecular weight wax, 7-13 parts of vinyl bisstearamide, 7-13 parts of zinc stearate, 25-35 parts of titanium dioxide, 2-4 parts of iron oxide yellow, 2-4 parts of macromolecular yellow, 2-4 parts of permanent yellow, 2-4 parts of flame retardant, and 2-4 parts of antioxidant.
[0006] Furthermore, 910-930 parts of ABS terpolymer, 28-32 parts of polyethylene low molecular weight wax, 8-12 parts of vinyl bisstearamide, 8-12 parts of zinc stearate, 28-32 parts of titanium dioxide, 2.5-3.5 parts of iron oxide yellow, 2.5-3.5 parts of macromolecular yellow, 2.5-3.5 parts of permanent yellow, 2.5-3.5 parts of flame retardant, and 2.5-3.5 parts of antioxidant.
[0007] Furthermore, the flame retardant is brominated polystyrene.
[0008] Furthermore, the antioxidant is octadecyl β-(3,5-di-tert-butyl-4-carboxyphenyl) propionate.
[0009] Compared with the prior art, the beneficial effects of the present invention are: by configuring multiple components, the color concentration, flame retardancy and oxidation resistance of plastics are improved. DETAILED DESCRIPTION
[0010] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0011] Example 1
[0012] The invention provides a technical solution for a yellow plastic masterbatch, which comprises the following components by weight: 880-960 parts of ABS terpolymer, 20-40 parts of polyethylene low-molecular wax, 5-15 parts of vinyl bisstearamide, 5-15 parts of zinc stearate, 20-40 parts of titanium dioxide, 1-5 parts of iron oxide yellow, 1-5 parts of macromolecular yellow, 1-5 parts of permanent yellow, 1-5 parts of flame retardant and 1-5 parts of antioxidant.
[0013] The flame retardant is brominated polystyrene.
[0014] The antioxidant is octadecyl β-(3,5-di-tert-butyl-4-carboxyphenyl) propionate.
[0015] Example 2
[0016] It comprises the following components by weight: 900-940 parts of ABS terpolymer, 25-35 parts of polyethylene low molecular weight wax, 7-13 parts of vinyl bisstearamide, 7-13 parts of zinc stearate, 25-35 parts of titanium dioxide, 2-4 parts of iron oxide yellow, 2-4 parts of macromolecular yellow, 2-4 parts of permanent yellow, 2-4 parts of flame retardant and 2-4 parts of antioxidant.
[0017] Example 3
[0018] It includes the following components by weight: 910-930 parts of ABS terpolymer, 28-32 parts of polyethylene low molecular weight wax, 8-12 parts of vinyl bisstearamide, 8-12 parts of zinc stearate, 28-32 parts of titanium dioxide, 2.5-3.5 parts of iron oxide yellow, 2.5-3.5 parts of macromolecular yellow, 2.5-3.5 parts of permanent yellow, 2.5-3.5 parts of flame retardant and 2.5-3.5 parts of antioxidant.
[0019] Although the present invention has been described in detail with reference to the aforementioned embodiments, it is still possible for those skilled in the art to modify the technical solutions described in the aforementioned embodiments, or to make equivalent substitutions for some of the technical features therein. Any modifications, equivalent substitutions, improvements, etc. made within the spirit and principles of the present invention should be included in the protection scope of the present invention.
Claims
1. A yellow plastic masterbatch, characterized in that: It comprises the following components by weight: 880-960 parts of ABS terpolymer, 20-40 parts of polyethylene low molecular weight wax, 5-15 parts of vinyl bisstearamide, 5-15 parts of zinc stearate, 20-40 parts of titanium dioxide, 1-5 parts of iron oxide yellow, 1-5 parts of macromolecular yellow, 1-5 parts of permanent yellow, 1-5 parts of flame retardant and 1-5 parts of antioxidant.
2. The yellow plastic masterbatch according to claim 1, characterized in that: ABS terpolymer 900-940 parts, polyethylene low molecular weight wax 25-35 parts, vinyl bisstearamide 7-13 parts, zinc stearate 7-13 parts, titanium dioxide 25-35 parts, iron oxide yellow 2-4 parts, macromolecular yellow 2-4 parts, permanent yellow 2-4 parts, flame retardant 2-4 parts, antioxidant 2-4 parts.
3. The yellow plastic masterbatch according to claim 2, characterized in that: ABS terpolymer 910-930 parts, polyethylene low molecular weight wax 28-32 parts, vinyl bisstearamide 8-12 parts, zinc stearate 8-12 parts, titanium dioxide 28-32 parts, iron oxide yellow 2.5-3.5 parts, macromolecular yellow 2.5-3.5 parts, permanent yellow 2.5-3.5 parts, flame retardant 2.5-3.5 parts, antioxidant 2.5-3.5 parts.
4. The yellow plastic masterbatch according to claim 1, characterized in that: The flame retardant is brominated polystyrene.