Cooperative treatment and resource utilization process for CO2 in industrial solid waste and tail gas
Through the static reaction method of polyacids and catalytic accelerator, the alumina and iron oxide in industrial solid waste are converted into soluble salts. Combined with ammonia replacement and activated carbon catalysts, the problems of low comprehensive utilization rate of industrial solid waste and serious carbon dioxide emissions are solved, and efficient resource utilization and carbon dioxide recovery are achieved.
Patent Information
- Application Number
- CN202510443944.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2025-04-09
- Publication Date
- 2025-07-04
- Estimated Expiration
- 2045-04-09
AI Technical Summary
In the prior art, the comprehensive utilization rate of industrial solid waste such as fly ash, gasified slag and coal gangue is low, and carbon dioxide emissions are severe, and effective coordinated governance and resource utilization methods are lacking.
The alumina and iron oxide in the gasified slag is converted into soluble salts by static reaction, and the ammonia displacement method is used to separate iron hydroxide and aluminum hydroxide. activate carbon is used as a catalyst to absorb carbon dioxide to produce silica acid and sodium carbonate, thereby achieving efficient extraction and recovery of resources.
It has achieved efficient resource utilization of gasified slag, fly ash and coal gangue, and generated high-value-added products such as alumina, sodium silicate and activated carbon, reducing carbon dioxide emissions and reducing environmental pollution.