Synthetic polymer waterproof coiled material

By using folding protective film and handle structure in synthetic polymer waterproof rolls, combining metal grid layer and PVDF film layer, the dust adsorption problem at the joints is solved, the waterproof performance and service life are improved, and the waterproofing of construction projects is ensured. quality.

CN222252567UActive Publication Date: 2024-12-27LONGYAN ZHONGYI FOOD & DRUG PACKAGE CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202420264994.7
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2024-02-02
Publication Date
2024-12-27
Estimated Expiration
2034-02-02

AI Technical Summary

Technical Problem

During the construction process of synthetic polymer waterproof coils, dust and oil stains are easily adsorbed at the joints, which affects the waterproof performance and leads to leakage.

Method used

A synthetic polymer waterproof coil material is designed, using a folding protective film and handle structure, which ensures cleanliness and seals at the joints through electrostatic adsorption and adhesive connections. Combining the metal grid layer and the PVDF film layer, improves waterproof performance and Weather resistance.

Benefits of technology

It effectively reduces dust entering the joints, ensures waterproof performance, improves the waterproof quality of construction projects, and enhances the anti-puncture, weather resistance and crack resistance of the coil, extending its service life.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN222252567U_ABST
    Figure CN222252567U_ABST
Patent Text Reader

Abstract

The utility model relates to the technical field of waterproof coiled materials, and discloses a synthetic polymer waterproof coiled material. The synthetic polymer waterproof coiled material comprises a coiled material body, a curing agent layer is arranged at the top of the coiled material body, an upper folding protective film is arranged at the top of the curing agent layer through electrostatic adsorption, an upper handle is fixedly connected to the left side of the upper folding protective film, and an HNP adhesive tape is arranged at the bottom of the coiled material body. A lower folding protective film is arranged at the bottom of the HNP adhesive tape through electrostatic adsorption, a lower handle is fixedly connected to the left side of the lower folding protective film, and a PE protective film is arranged at the bottom of the coiled material body. When the waterproof coiled material is used, the upper folding protective film and the lower folding protective film are arranged, and the upper handle and the lower handle are pulled at the same time, so that the curing agent layer and the HNP adhesive tape are contacted and cured, the seam of the two coiled material bodies is stably lapped, dust entering the seam is reduced during lapping, the waterproof performance of the seam is ensured, and the service life of the coiled material is prolonged. And the waterproof quality of constructional engineering is improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model relates to the technical field of waterproof coiled materials, in particular to a synthetic polymer waterproof coiled material. Background Art

[0002] Waterproof membrane is mainly used for building walls, roofs, tunnels, roads, landfills, etc. It is a flexible building material product that can be rolled into a roll to resist the seepage of external rainwater and groundwater. As a leak-free connection between the project foundation and the building, it is the first barrier to waterproofing the entire project and plays a vital role in the entire project.

[0003] Among them, synthetic polymer waterproofing membrane is a composite sheet waterproofing material that is made of synthetic polymer materials as the main raw material and is compounded with synthetic fibers to form two or more layers of rollable composite sheet waterproofing materials.

[0004] When currently laying synthetic polymer waterproof membranes, in order to keep the joints sealed, self-adhesive edges are usually set on both sides of the synthetic polymer waterproof membrane for pasting, or a hot air gun is used to heat the edge hot melt adhesive for pasting, and the joint joint needs to be larger than 80mm. When making the joints, it is necessary to ensure that the pasting area is flat, dry, clean, and free of oil, dust and other debris. If dust and oil are mixed into the joints, it will inevitably affect the waterproof performance of the joint gaps and leakage will easily occur. However, due to the limitations of the construction site environment, there will be a lot of dust in the environment. In order to protect the joints from dust absorption, a film is usually applied to the self-adhesive edges or hot melt adhesives for protection. However, when the protective film is removed, the pasting area will still absorb dust, resulting in gaps when the joints are pasted, thereby affecting the waterproof quality of the construction project. Utility Model Content

[0005] In order to make up for the above shortcomings, the utility model provides a synthetic polymer waterproof membrane, which solves the problem mentioned in the above background technology that when the joints are pasted and spliced, the joints will absorb a large amount of dust in the environment, affecting the waterproof performance of the joints.

[0006] To achieve the above objectives, the utility model is implemented through the following technical solutions: a synthetic polymer waterproof roll, including a roll body, a curing agent layer is arranged on the top of the roll body, a folded upper protective film is arranged on the top of the curing agent layer by electrostatic adsorption, an upper handle is fixedly connected to the left side of the folded upper protective film, an HNP rubber strip is arranged at the bottom of the roll body, a folded lower protective film is arranged at the bottom of the HNP rubber strip by electrostatic adsorption, a lower handle is fixedly connected to the left side of the folded lower protective film, and a PE protective film is arranged at the bottom of the roll body.

[0007] As a further description of the above technical solution:

[0008] The coil body includes an adhesive backing layer, the bottom of the adhesive backing layer is arranged on the top of the PE protective film, the top of the adhesive backing layer is fixedly connected to a synthetic polymer material layer, the top of the synthetic polymer material layer is fixedly connected to a non-woven fabric layer, the top of the non-woven fabric layer is fixedly connected to a metal mesh layer, the top of the metal mesh layer is fixedly connected to a PVDF film layer, and the top of the PVDF film layer is fixedly connected to a synthetic fiber protective layer.

[0009] As a further description of the above technical solution:

[0010] The folding upper protective film and the folding lower protective film are both formed by folding a long strip of protective film in the middle, and the overlapping folded parts are only in contact. The right side of the upper handle is fixedly connected to the left end of the upper layer of the folded upper protective film, and the right side of the lower handle is fixedly connected to the left end of the lower layer of the folded lower protective film.

[0011] As a further description of the above technical solution:

[0012] The upper handle is made of PE material, with adhesive provided on the bottom. The upper handle is bent and adhered to the bottom of the PE protective film. The lower handle is made of PE material, with adhesive provided on the top. The lower handle is bent and adhered to the top of the coil body.

[0013] As a further description of the above technical solution:

[0014] Pull holes are provided on the surfaces of the upper handle and the lower handle, and the shapes of the two groups of pull holes are matched.

[0015] As a further description of the above technical solution:

[0016] The width of the HNP adhesive strip and the curing agent layer are both ninety millimeters.

[0017] As a further description of the above technical solution:

[0018] The synthetic polymer material layer is made of any one of ethylene vinyl acetate copolymer, vinyl alcohol ester-vinyl ether alcohol ester copolymer, olefin-polyester elastomer, and high-density polyethylene.

[0019] As a further description of the above technical solution:

[0020] The metal mesh layer is woven from 2mm metal wires, and the metal wires are made of copper wires and aluminum wires.

[0021] The utility model has the following beneficial effects:

[0022] 1. In the utility model, by providing a folding upper protective film and a folding lower protective film, the upper handle and the lower handle are pulled at the same time, so that the curing agent layer and the HNP adhesive strip are contacted and cured, so that the joints of the two coil bodies are firmly overlapped, and when overlapping, the dust entering the overlapped joint is reduced, the waterproof performance of the joint is guaranteed, and the waterproof quality of the construction project is improved.

[0023] 2. In the present invention, a metal mesh layer is provided to ensure the puncture resistance of the roll body, and a PVDF film layer is provided to ensure the weather resistance and crack resistance of the roll body, thereby improving the service life of the waterproof roll and enhancing the performance of the waterproof roll. BRIEF DESCRIPTION OF THE DRAWINGS

[0024] Figure 1 This is a schematic diagram of the overall front three-dimensional structure of the utility model;

[0025] Figure 2 This is a schematic diagram of the partial three-dimensional structure of the front side of the folded upper protective film of the utility model;

[0026] Figure 3 This is a schematic diagram of the partial three-dimensional structure of the left side of the folded lower protective film of the utility model;

[0027] Figure 4 This is a schematic diagram of the three-dimensional structure of the bottom surface of the coil body of the utility model;

[0028] Figure 5 It is a schematic diagram of the three-dimensional structure of the left side of the coil body of the utility model.

[0029] Legend:

[0030] 1. Coil body; 11. Synthetic polymer material layer; 12. Adhesive layer; 13. Non-woven fabric layer; 14. Metal mesh layer; 15. PVDF film layer; 16. Synthetic fiber protective layer; 2. Curing agent layer; 3. Folding upper protective film; 4. Upper handle; 5. HNP adhesive strip; 6. Folding lower protective film; 7. Lower handle; 8. PE protective film. DETAILED DESCRIPTION

[0031] The following will be combined with the drawings in the embodiments of the utility model to clearly and completely describe the technical solutions in the embodiments of the utility model. Obviously, the described embodiments are only part of the embodiments of the utility model, not all of the embodiments. Based on the embodiments in the utility model, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the utility model.

[0032] See also Figure 1 and Figure 4The utility model provides a synthetic polymer waterproof coiled material, including a coiled material body 1, a curing agent layer 2 is arranged on the top of the coiled material body 1, a folded upper protective film 3 is adhered to the top of the curing agent layer 2 by electrostatic adsorption, an upper handle 4 is fixedly connected to the left side of the folded upper protective film 3, an HNP adhesive strip 5 is arranged at the bottom of the coiled material body 1, the width of the HNP adhesive strip 5 and the curing agent layer 2 are both ninety millimeters, HNP adhesive is a special adhesive for polymer waterproof coiled materials, it can be cured in a humid environment, and has excellent weather resistance, water resistance, corrosion resistance and good bonding performance, when the bottom surface of the HNP adhesive strip 5 contacts the top surface of the curing agent layer 2, it will cure quickly, so that the gap has good waterproof performance, a folded lower protective film 6 is adhered to the bottom of the HNP adhesive strip 5 by electrostatic adsorption, a lower handle 7 is fixedly connected to the left side of the folded lower protective film 6, and a PE protective film 8 is adhered to the bottom of the coiled material body 1.

[0033] See also Figure 2-Figure 3 The folded upper protective film 3 and the folded lower protective film 6 are both formed by folding in the middle of a long strip of protective film, and the folded overlapping parts are only in contact. The right side of the upper handle 4 is fixedly connected to the left end of the upper layer of the folded upper protective film 3. The upper handle 4 is made of PE material and has glue at the bottom. The upper handle 4 is bent and glued to the bottom of the PE protective film 8 to fix the folded upper protective film 3. The glue at the bottom of the upper handle 4 is weak, and the upper handle 4 can be directly peeled off from the bottom of the PE protective film 8. The right side of the lower handle 7 is fixedly connected to the left end of the lower layer of the folded lower protective film 6. The lower handle 7 is made of PE material and has glue at the top. The lower handle 7 is bent and glued to the top of the coil body 1 to fix the folded lower protective film 6. The glue at the top of the lower handle 7 is weak, and the lower handle 7 can be directly peeled off from the top of the coil body 1. Pull holes are opened on the surfaces of the upper handle 4 and the lower handle 7, and the shapes of the two groups of pull holes are matched.

[0034] See also Figure 1 and Figure 5The coil body 1 includes a back adhesive layer 12, the bottom of the back adhesive layer 12 is arranged on the top of the PE protective film 8, and the PE protective film 8 can ensure that the back adhesive layer 12 is clean and tidy before use before being opened. The top of the back adhesive layer 12 is fixedly connected with a synthetic polymer material layer 11, and the synthetic polymer material layer 11 is made of any one of ethylene vinyl acetate copolymer, vinyl alcohol ester-vinyl ether alcohol ester copolymer, olefin-polyester elastomer, and high-density polyethylene. Ethylene vinyl acetate copolymer (EVA) is an elastic, transparent plastic with good softness and weather resistance. Vinyl alcohol ester-vinyl ether alcohol Ethylene glycol copolymer (ECB) is a polymer with excellent aging resistance, UV resistance and chemical corrosion resistance. Olefin-polyester elastomer (TPO) is an elastomeric material with excellent weather resistance and UV resistance, and also has the characteristics of thermal welding. High-density polyethylene (HDPE) is a high-density polyethylene plastic with excellent corrosion resistance, chemical resistance and wear resistance. Ethylene vinyl acetate copolymer, vinyl alcohol ester-vinyl ether alcohol ester copolymer, olefin-polyester elastomer and high-density polyethylene have different characteristics and uses, but all have good waterproof function.

[0035] See also Figure 5 A non-woven fabric layer 13 is fixedly connected to the top of the synthetic polymer material layer 11, and a metal mesh layer 14 is fixedly connected to the top of the non-woven fabric layer 13. The metal mesh layer 14 is woven from two-millimeter metal wires, and the metal wires are made of copper wires and aluminum wires. The metal mesh layer 14 can improve the tensile strength of the coil body 1, reduce the degree of heat shrinkage, and extend the service life to a certain extent, so that the puncture ability of the coil body 1 is improved. A PVDF film layer 15 is fixedly connected to the top of the metal mesh layer 14. The PVDF film has excellent weather resistance and corrosion resistance, and improves the crack resistance of the coil body 1. A synthetic fiber protective layer 16 is fixedly connected to the top of the PVDF film layer 15. The synthetic fiber protective layer 16 is in the outermost layer of the coil body 1 to provide protection for the coil body 1.

[0036] Working principle: When you want to lay the synthetic polymer coil and make it easier to join the seams so that it is not easily contaminated by dust, first clean the dust in the surrounding environment, peel off the upper handle 4 from under the PE protective film 8, then peel off the PE protective film 8, stick the adhesive layer 12 on the required surface, spread out multiple synthetic polymer coils in sequence, overlap the long sides of the synthetic polymer coils, overlap the folded lower protective film 6 on the folded upper protective film 3, ensure that the overlap between the folded lower protective film 6 and the folded upper protective film 3 is greater than 80mm, peel off the lower handle 7 from above the coil body 1, overlap the pull holes of the upper handle 4 and the lower handle 7, and put your fingers Put it into the pulling hole between the upper handle 4 and the lower handle 7, pull out the upper handle 4 and the lower handle 7 to the left, and the upper handle 4 and the lower handle 7 simultaneously drive the contacting part of the folded upper protective film 3 and the folded lower protective film 6 to the right. At this time, the lower layer of the folded upper protective film 3 is separated from the curing agent layer 2, and the upper layer of the folded lower protective film 6 is separated from the HNP adhesive strip 5. The curing agent layer 2 is in contact with the HNP adhesive strip 5, and then the overlapping edge of the coil body 1 is squeezed to fully mix the HNP adhesive strip 5 and the curing agent layer 2, and solidify them, so that the two pieces of synthetic polymer coils are overlapped and fixed, and the waterproof performance of the joint will not be reduced due to dust.

[0037] Finally, it should be noted that the above is only a preferred embodiment of the present invention and is not intended to limit the present invention. Although the present invention has been described in detail with reference to the aforementioned embodiments, those skilled in the art can still modify the technical solutions described in the aforementioned embodiments or make equivalent substitutions for some of the technical features therein. Any modifications, equivalent substitutions, improvements, etc. made within the spirit and principles of the present invention should be included in the protection scope of the present invention.

Claims

1. A synthetic polymer waterproofing roll, comprising a roll body (1), characterized in that: A curing agent layer (2) is arranged on the top of the coiled material body (1), a folding upper protective film (3) is adhered to the top of the curing agent layer (2) by electrostatic adsorption, an upper handle (4) is fixedly connected to the left side of the folding upper protective film (3), an HNP adhesive strip (5) is arranged on the bottom of the coiled material body (1), a folding lower protective film (6) is adhered to the bottom of the HNP adhesive strip (5) by electrostatic adsorption, a lower handle (7) is fixedly connected to the left side of the folding lower protective film (6), and a PE protective film (8) is adhered to the bottom of the coiled material body (1).

2. The synthetic polymer waterproofing coiled material according to claim 1, characterized in that: The coil body (1) comprises an adhesive backing layer (12), the bottom of the adhesive backing layer (12) is arranged on the top of the PE protective film (8), the top of the adhesive backing layer (12) is fixedly connected to a synthetic polymer material layer (11), the top of the synthetic polymer material layer (11) is fixedly connected to a non-woven fabric layer (13), the top of the non-woven fabric layer (13) is fixedly connected to a metal mesh layer (14), the top of the metal mesh layer (14) is fixedly connected to a PVDF film layer (15), and the top of the PVDF film layer (15) is fixedly connected to a synthetic fiber protective layer (16).

3. The synthetic polymer waterproofing coiled material according to claim 1, characterized in that: The folded upper protective film (3) and the folded lower protective film (6) are both formed by folding a long strip of protective film in the middle, and the folded overlapping parts are only in contact. The right side of the upper handle (4) is fixedly connected to the left end of the upper layer of the folded upper protective film (3), and the right side of the lower handle (7) is fixedly connected to the left end of the lower layer of the folded lower protective film (6).

4. The synthetic polymer waterproofing coiled material according to claim 1, characterized in that: The upper handle (4) is made of PE material, with adhesive provided on the bottom. The upper handle (4) is bent and adhered to the bottom of the PE protective film (8). The lower handle (7) is made of PE material, with adhesive provided on the top. The lower handle (7) is bent and adhered to the top of the coil body (1).

5. The synthetic polymer waterproofing coiled material according to claim 1, characterized in that: Pull holes are provided on the surfaces of the upper handle (4) and the lower handle (7), and the shapes of the two groups of pull holes are matched.

6. The synthetic polymer waterproofing coiled material according to claim 1, characterized in that: The width of the HNP rubber strip (5) and the curing agent layer (2) are both ninety millimeters.

7. The synthetic polymer waterproofing coiled material according to claim 2, characterized in that: The synthetic polymer material layer (11) is made of any one of ethylene vinyl acetate copolymer, vinyl glycolate-vinyl ether glycolate copolymer, olefin-polyester elastomer, and high-density polyethylene.