Modified metal oxide particulate material and method for producing same

The modified metal oxide particle material, featuring a silicon-containing compound with a phenyl group, addresses the challenge of achieving high dispersibility with minimal modifying material by suppressing reaction progression, resulting in improved performance and reduced agglomeration in resin and organic solvent systems.

WO2024236674A1PCT designated stage expired Publication Date: 2024-11-21ADMATECHS CO LTD

Patent Information

Application Number
PCT/JP2023/018022
Authority / Receiving Office
WO · WO
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-05-12
Publication Date
2024-11-21

AI Technical Summary

Technical Problem

Existing metal oxide particle materials face challenges in achieving high dispersibility in resin compositions with reduced amounts of modifying materials, which can impact electrical properties and performance.

Method used

A modified metal oxide particle material is developed by interposing a silicon-containing compound with a phenyl group between the metal oxide particles, allowing for improved dispersibility even with a small amount of modifying material, achieved by suppressing reaction progression through reduced heating temperature and time during surface treatment.

Benefits of technology

The modified material exhibits enhanced dispersibility and performance in resin materials and organic solvents, maintaining effectiveness with reduced modifying material usage, as evidenced by decreased C/H values and grain gauge measurements.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure JPOXMLDOC01-APPB-T000001
    Figure JPOXMLDOC01-APPB-T000001
Patent Text Reader

Abstract

The present invention addresses the problem of providing a modified metal oxide particulate material having high dispersibility even when the amount of a modified material is small. The dispersibility can be improved by interposing a modifying material between particles of the metal oxide particulate material. In particular, by suppressing the reaction between pieces of the modifying material, a sufficient effect was successfully exhibited even if the amount of the modifying material was reduced. Specifically, this modified metal oxide particulate material comprises: a metal oxide particulate material having, on the surface thereof, a functional group other than a phenyl group; and a modifying material that comprises a silicon-containing compound having a phenyl group and that adheres to the surface of the metal oxide particulate material. After the modified metal oxide particulate material is washed with methyl ethyl ketone, the value of C / H calculated from the surface area H (m2) and the carbon content C (mass%) per gram is reduced by at least 0.03 but less than 0.1, the particle gauge is 20 μm or less, and the post-wash C / H value is not more than 0.07.
Need to check novelty before this filing date? Find Prior Art

Description

Modified metal oxide particulate material and method for producing same

[0001] The present invention relates to a modified metal oxide particulate material that can be used by dispersing it in a resin material or an organic solvent, and a method for producing the same.

[0002] Conventionally, resin compositions in which a filler material made of a metal oxide is dispersed in a resin material have been widely used. Dispersing a filler material made of a metal oxide improves the mechanical properties of the resin composition and its cured product (see, for example, Patent Document 1). It is desirable for the filler material to be uniformly dispersed in such a resin composition. To obtain such a resin composition, the filler material can be directly dispersed in the resin material, or a slurry composition in which the filler material is dispersed in an organic solvent can be produced and then mixed with the resin material to form a resin composition. To solve the above-mentioned problems, the present applicant has developed a technology for improving dispersibility by attaching a modifying material to the surface of a surface-treated metal oxide particulate material (see, for example, Patent Document 2).

[0003] Patent No. 6603777 International Publication No. 2021 / 210628

[0004] The technology disclosed in Patent Document 2 achieves high dispersibility in a resin material. However, since reducing the amount of modifier has advantages such as improving electrical properties, there are applications in which a small amount of modifier attached to the surface of the particulate material is preferable, and there has been a demand for reducing the amount of modifier. The present invention was completed in light of the above-mentioned circumstances, and an object of the present invention is to provide a modified metal oxide particulate material that is a metal oxide particulate material that is highly dispersible even with a small amount of modifier, and a method for producing the same.

[0005] The present inventors conducted extensive research to solve the above-mentioned problems. As a result, they discovered that the effect of Patent Document 2, in which a modifying material consisting of a silicon-containing compound having a phenyl group is interposed between metal oxide particulate materials and then dispersed in a resin material or organic solvent, can facilitate the penetration of the resin material or organic solvent between the metal oxide particulate materials, thereby improving dispersibility, can be fully achieved by suppressing the reaction between the modifying materials, even if the amount of the modifying material attached is reduced. If a reaction occurs between the modifying materials, the inherent performance of the modifying material cannot be fully achieved. Specifically, they discovered that by reducing the heating temperature and heating time when attaching the modifying material to the surface of the metal oxide particulate material, the reaction between the modifying materials can be suppressed, and sufficient effects can be achieved with a small amount of the modifying material, leading to the completion of the following invention.

[0006] (1) That is, the modified metal oxide particulate material of the present invention, which solves the above-mentioned problems, comprises a metal oxide particulate material having functional groups other than phenyl groups on the surface thereof, and a modifying material comprising a silicon-containing compound having a phenyl group and adhering to the surface of the metal oxide particulate material, and has a surface area H (m 2 The C / H value calculated from the carbon content C (mass%) and the particle size (grain size) of the sintered product is 0.07 or less after washing with methyl ethyl ketone.

[0007] The modified metal oxide particulate material of the present invention may have one or more of the components described in (2) to (8) below.

[0008] (2) It is preferable that (dielectric loss tangent) / H is 0.0005 or less. (3) The modified metal oxide particle material can be prepared by applying a modifying material solution, in which the modifying material is dissolved or dispersed in A mL of solvent, to the metal oxide particle material, and then heating and drying the resulting mixture at T°C for m minutes (where T × m ÷ A is 150 or less).

[0009] (4) The silicon-containing compound constituting the modifying material is a silane compound having a phenyl group, or a condensation product of a silane compound having a phenyl group and a silane compound having a hydrocarbon group directly bonded to Si.

[0010] (5) The silane compound having a phenyl group is ((C 6 H 5 ) X) n -Si-OR (4-n) The silane compound having a hydrocarbon group is represented by R n -Si-OR (4-n) (X is a direct bond or -(CH 2 ) q - or -O-; q is an integer of 0 to 3; n is an integer of 1 to 3 selected independently for each molecule; and R is a hydrocarbon group having 1 to 3 carbon atoms selected independently for each functional group.

[0011] (6) The silicon-containing compound constituting the modifying material is represented by the general formula (1): R1-O-(SiZ1Z2O) n -(SiZ3Z4O) m -R2. (Wherein, Z1 is (C 6 H 5 ) X-; Z2 to Z4 each independently represent (C 6 H 5 ) X-, a hydrocarbon group having 1 to 3 carbon atoms, an alkoxy group having 1 to 3 carbon atoms, and -O which bonds to other Z2 to Z4 r - (CH 2 ) p -O t -; X is a direct bond or -(CH 2 ) q (7) The metal oxide particle material is surface-treated with a silane compound. (8) The volume average particle size is 0.01 μm or more and 5 μm or less.

[0012] (9) A method for producing a modified metal oxide particulate material of the present invention that solves the above-mentioned problems comprises the steps of: a surface treatment step of surface-treating a metal oxide particulate material with a silane compound to produce a surface-treated metal oxide particulate material; a dispersion step of dispersing a silicon-containing compound having a phenyl group in a dispersion slurry obtained by dispersing the surface-treated metal oxide particulate material in A mL of a dispersion medium; and a drying step of drying the dispersion medium by heating at T°C for m minutes after the dispersion step to adhere a modifying material consisting of the silicon-containing compound to the surface of the surface-treated metal oxide particulate material to produce a modified metal oxide particulate material, wherein T × m ÷ A is 150 or less.

[0013] The modified metal oxide particulate material of the present invention can improve dispersibility in resin materials and organic solvents by previously interposing a modifying material between metal oxide particulate materials. Because the reaction between the interposed modifying material is suppressed, a small amount can be used to achieve a high effect.

[0014] The modified metal oxide particulate material and its manufacturing method of the present invention will be described in detail below based on embodiments. The modified metal oxide particulate material of this embodiment is a material that can be suitably used as a filler material to be dispersed in a resin material or an organic solvent. It is particularly preferable that it is provided in a dry state. The modified metal oxide particulate material is preferably one that is dispersed in a resin material or an organic solvent during use, so that the modifying material that adheres to the surface of the modified metal oxide particulate material migrates into the organic solvent or the like and exerts its effect.

[0015] (Modified Metal Oxide Particulate Material) The modified metal oxide particulate material of this embodiment includes a surface-treated metal oxide particulate material and a modifying material. The modified metal oxide particulate material desirably has a high sphericity, for example, preferably 0.8 or more, 0.9 or more, 0.95 or more, or 0.99 or more.

[0016] The surface-treated metal oxide particulate material is a metal oxide particulate material that has been surface-treated. Examples of metal oxide particulate materials include silica, alumina, zirconia, titania, and composite oxides thereof. Examples of composite oxides include calcium titanate, barium titanate, and zeolite. The particle size of the metal oxide particulate material is not particularly limited, but it is desirable for the metal oxide particulate material to have a particle size distribution suitable for use as a filler material. For example, it can be 0.01 μm or more and 5 μm or less. The lower limit can be 0.01 μm, 0.05 μm, 0.1 μm, 0.3 μm, or 0.5 μm, and the upper limit can be 2 μm, 3 μm, 4 μm, or 5 μm. These upper and lower limits can be combined in any combination.

[0017] The surface-treated metal oxide particulate material has functional groups other than phenyl groups on its surface. Examples of functional groups other than phenyl groups include carbon-containing functional groups such as alkyl groups, vinyl groups, epoxy groups, methacrylic groups, amino groups, and isocyanate groups. The method for introducing these functional groups is not particularly limited, but they can be introduced by surface-treating the metal oxide particulate material with a silane compound having these functional groups. For example, the silane compound can be directly brought into contact with the surface of the metal oxide particulate material, or a solution of the silane compound can be prepared using a solvent and brought into contact with the surface. The mixture can then be left to stand or heated until the reaction is complete.

[0018] When a functional group is introduced using a silane compound, it is expected that the functional group will react with and bond to OH groups present on the surface of the metal oxide particulate material, and it is preferable that 50% or more of the OH groups disappear through the reaction, more preferably 70% or more, even more preferably 90% or more, and particularly preferably 100%. Note that, if a functional group other than a phenyl group is introduced, a portion of the phenyl group may be introduced.

[0019] The modifying material is a material that adheres to the surface of the surface-treated metal oxide particulate material. The term "adhesion" means that physical adsorption is predominant, with a small amount of chemical reaction occurring. Whether physical adsorption is predominant or not is determined by whether 30% or more (preferably 50% or more, more preferably 70% or more) of the modifying material is released by mass when dispersed in an organic solvent.

[0020] A part of the modifying material may react with the surface of the surface-treated metal oxide particulate material. For example, the surface area H (m 2 The reaction can be carried out until the C / H value calculated from the carbon content C (mass%) after washing is in the range of 0.07 or less, and can also be carried out until the value is in the range of 0.06 or less, 0.05 or less, 0.04 or less, 0.03 or less, or 0.02 or less. The washing conditions are as follows: 5 g of the modified metal oxide particulate material is put into 35 mL of methyl ethyl ketone (MEK), and ultrasonic waves are applied for 5 minutes to wash the material. The type and amount of the modifying material are determined by the surface area H (m 2 The C / H value calculated from the carbon content C (mass%) and the carbon content C (mass%) changes by 0.01 or more but less than 0.1 before and after washing with MEK, and examples of lower limits include 0.015, 0.020, 0.025, 0.035, 0.040, and 0.45, while examples of upper limits include 0.90, 0.80, 0.70, and 0.65. These upper and lower limits can be combined arbitrarily. Note that the carbon content C here also includes carbon derived from compounds having functional groups other than phenyl groups bonded to the surface of the surface-treated metal oxide particulate material.

[0021] In the case of a silane compound containing one silicon atom, a silane compound having two phenyl groups is preferred. For example, diphenyldialkoxysilane. The alkoxy group is preferably a methoxy group or an ethoxy group, and a methoxy group is particularly preferred. An additive (modifier) ​​having two phenyl groups can improve dispersibility by increasing steric hindrance compared to an additive having one phenyl group, and can also reduce reactivity, preventing the additive from firmly bonding to the surface of the surface-treated metal oxide particulate material.

[0022] The modifying material may be a silane compound having a phenyl group or a condensate of a silane compound having a phenyl group with a silane compound having a hydrocarbon group directly bonded to silicon. The condensate may be produced, for example, by mixing and reacting silane compounds each having one silicon atom. The reaction is preferably carried out in the presence of a catalyst. Examples of the catalyst include a noble metal catalyst such as platinum, and an alkali.

[0023] For example, a silane compound having a phenyl group is ((C 6 H 5 ) X) n -Si-OR (4-n) Examples of the silane compound having a hydrocarbon group include R n -Si-OR (4-n) (X is a direct bond or -(CH 2 ) q (X is preferably directly bonded. For example, diphenyldialkoxysilane is a compound in which X is directly bonded and n is 2.)

[0024] Furthermore, the silicon-containing compound constituting the modifying material is represented by the general formula (1): R1-O-(SiZ1Z2O) n -(SiZ3Z4O) m -R2 can be used. (Wherein, Z1 is (C 6 H 5 ) X-; Z2 to Z4 each independently represent (C 6 H 5 ) X-, a hydrocarbon group having 1 to 3 carbon atoms, an alkoxy group having 1 to 3 carbon atoms, and -O which bonds to other Z2 to Z4 r - (CH 2 ) p -O t -; X is a direct bond or -(CH 2 ) q- or -O-; n and p are integers of 1 or greater; m is an integer of 0 or greater; q is an integer of 0 or greater that is independently selected; r and t are each independently selected from 0 or 1; R1 and R2 are each independently selected hydrocarbon groups having 1 to 3 carbon atoms or alkoxy groups having 1 to 3 carbon atoms).

[0025] The modified metal oxide particle material of this embodiment preferably has a (dielectric loss tangent) / specific surface area ratio of 0.0005 or less, more preferably 0.0004 or less, and even more preferably 0.003 or less. The dielectric loss tangent was measured in accordance with JIS C 2138 (2007). Specifically, the relative permittivity and dielectric loss tangent at 1 GHz were measured using a Keysight Network Analyzer (product name "E5071C") and a cavity resonator perturbation method. This measurement was performed in accordance with ASTM D2520 (JIS C 2565 (1992)).

[0026] The modified metal oxide particulate material of this embodiment has a particle size measured with a particle gauge of 20 μm or less. The particle size is measured by mixing 10 g of epoxy resin (manufactured by Nippon Steel Chemical & Materials Co., Ltd., model number ZX-1059), 20 g of MEK, and 10 g of the modified metal oxide particulate material in a planetary mixer, and then evaluating the mixture with the particle gauge. The evaluation using the particle gauge is performed in accordance with JIS K 56000-2-5. The particle gauge measurement value correlates with the particle size of the aggregates.

[0027] (Method for Producing Modified Metal Oxide Particulate Material) The method for producing the modified metal oxide particulate material of this embodiment includes a surface treatment step, a dispersion step, and a drying step.

[0028] The surface treatment process is a process in which a metal oxide particulate material is surface-treated with a silane compound to produce a surface-treated metal oxide particulate material. The method for producing the metal oxide particulate material is not particularly limited, but examples include the VMC method (Vaporized Metal Combustion Method) and the melting method. Metal oxide particulate materials produced by the VMC method are dense, have low water absorption, and have excellent electrical properties. The VMC method is a method for producing a metal oxide particulate material by introducing particles made of the metal that constitutes the metal oxide particulate material into a flame in an oxidizing atmosphere and burning them.

[0029] The surface treatment step is a step of introducing functional groups other than phenyl groups onto the surface. If functional groups other than phenyl groups are present, they can also be introduced by adding phenyl groups. The method of introducing functional groups is preferably to perform surface treatment using a silane compound having the functional group to be introduced. The surface treatment can be carried out by contacting the surface of the metal oxide particulate material with a surface treatment agent having the functional group to be introduced. The contact can be carried out by contacting the surface of the metal oxide particulate material with the surface treatment agent in liquid or gaseous form as is, or as a solution dissolved in some kind of solvent. The amount of surface treatment agent is not particularly limited, but an amount sufficient to achieve the aforementioned residual rate of OH groups present on the surface of the metal oxide particulate material can be used.

[0030] The dispersion step is a step of dispersing the surface-treated metal oxide particulate material in a dispersion medium to form a dispersion slurry, and dispersing a silicon-containing compound in the dispersion slurry. The silicon-containing compound and the amount thereof can be those described above in connection with the modified metal oxide particulate material of this embodiment.

[0031] Examples of dispersion media for the dispersion slurry include MEK, isopropyl alcohol, propylene glycol monomethyl ether acetate, cyclohexanone, methyl isobutyl ketone, toluene, N-methylpyrrolidone, N-ethylpyrrolidone, and gamma-butyrolactone. The content of the surface-treated metal oxide particulate material contained in the dispersion slurry is not particularly limited, but can be approximately 10% to 80% based on the total mass. The lower limit can be 10%, 30%, or 50%, and the upper limit can be 60%, 70%, or 80%. These upper and lower limit values ​​can be combined in any desired manner.

[0032] In preparing the dispersion slurry and dispersing the modifying material in the dispersion slurry, stirring or shear force may be applied or ultrasonic waves may be irradiated.

[0033] The drying step is a step of removing the dispersion medium. The method for removing the dispersion medium is not particularly limited. When the drying time until the dispersion medium is completely removed is m minutes, the temperature at that time is T°C, and the volume of the dispersion medium is A mL, T × m ÷ A is 150 or less, with upper limits of 140, 130, 120, 110, 100, 90, and 80. By keeping the temperature below these upper limits, the progress of the reaction between the modifying materials is suppressed. If the progress of the reaction is equivalent to when the temperature is below these upper limits, modified metal oxide particulate materials produced by other methods can be considered to be the modified metal oxide particulate material of this embodiment, although they cannot be said to have been produced by the method for producing the modified metal oxide particulate material of this embodiment. The temperature T is the average temperature of the dispersed slurry during the drying time. The start of the drying time is when the temperature T of the dispersed slurry reaches or exceeds the starting temperature after the dispersed slurry is prepared in the dispersion step. The end of the drying time, which is considered to be the end of the drying time, is when the dispersion medium reaches or exceeds 1% by mass. Even when the temperature of the dispersion slurry reaches or exceeds the starting temperature, if it subsequently falls below the starting temperature, it is excluded from the drying time until it reaches or exceeds the starting temperature again. Here, the starting temperature is 110 ° C., and 105 ° C., 100 ° C., 80 ° C., 60 ° C., and 40 ° C. can also be used. Specific heating methods are not limited, but include a method of simply heating and a method of simultaneously reducing pressure while heating. In particular, spray drying using a disk rotor or pressure nozzle can be used during heating, which is preferable because it can effectively shorten the drying time (minutes).

[0034] By drying, the silicon-containing compound is converted into a modifying material. The modifying material may be either a material that dissolves in the dispersion medium or a material that does not dissolve in the dispersion medium. If the modifying material dissolves, it will precipitate and become particles as the modifying material as the dispersion medium dries. If the silicon-containing compound does not dissolve in the dispersion medium, the silicon-containing compound will adhere to the surface of the surface-treated metal oxide particulate material as it is.

[0035] The modified metal oxide particulate material and the method for producing the same of the present invention will be described in detail below with reference to examples.

[0036] Examples 1 to 7, Comparative Examples 1 to 7 (Sample Preparation) Spherical silica or spherical alumina having the particle sizes shown in Table 1 were used as the metal oxide particulate material. All were manufactured by Admatechs Co., Ltd. using the VMC method, with model numbers SO-C1 for spherical silica with a volume average particle size of 0.3 μm, SO-C2 for spherical silica with a volume average particle size of 0.5 μm, and SO-C6 for spherical silica with a volume average particle size of 2.0 μm. For spherical alumina with a volume average particle size of 2.0 μm, a powder obtained by mixing AO-502 and AO-509 in a mass ratio of 8:2 was used. Surface-treated metal oxide particulate material was obtained by adding KBM-1003 (vinyltrimethoxysilane, manufactured by Shin-Etsu Chemical Co., Ltd.) as a surface treatment agent to 100 parts by mass of this metal oxide particulate material. The amount of surface treatment agent added was 1 part by mass for spherical silica with a volume average particle size of 0.3 μm, 1 part by mass for spherical silica with a volume average particle size of 0.5 μm, and 0.3 parts by mass for spherical silica with a volume average particle size of 2.0 μm, relative to 100 parts by mass of the metal oxide particulate material, and 0.5 parts by mass for spherical alumina. By reacting these amounts, the amount of surface treatment agent per unit surface area was kept constant. Vinyl groups were introduced onto the surface of the obtained surface-treated metal oxide particulate material (surface treatment process).

[0037] A dispersion slurry was prepared by mixing 100 parts by mass of the surface-treated metal oxide particulate material and 64.4 parts by mass (80 mL) of methyl ethyl ketone (MEK). The surface area (1 m 2 ) was added a silicon-containing compound shown in Table 1 (manufactured by Shin-Etsu Chemical Co., Ltd., identified by product number; functional groups are confirmed in the catalog: KBM-202SS is a monomer whose functional group is diphenyl, and KR-9218 is an oligomer whose functional groups are phenyl and methyl) so as to obtain the amount C before washing shown in Table 1, and the mixture was dispersed for 2 minutes using a Clearmix CLM-2.2S manufactured by M Technique Co., Ltd. (17,000 rpm) (dispersion step).

[0038] Thereafter, the powder was dried by heating at 110°C for the time (m minutes) shown in Table 1 (drying step), and the obtained powder was used as a test sample for each of the Examples and Comparative Examples.

[0039] For the test samples of each Example and Comparative Example, the carbon amount before cleaning (C amount before cleaning), the carbon amount after cleaning (C amount after cleaning), the carbon amount after MEK cleaning of the surface-treated metal oxide particulate material (original powder) before the modification material was attached (C amount of original powder), and the dielectric loss tangent (Df) were measured. Furthermore, the dispersibility was measured using a particle gauge. The dispersibility evaluation using a particle gauge is a test conducted in accordance with JIS K 56000-2-5, and the particle gauge value is a value that correlates with the particle size of the aggregates. In other words, a larger particle gauge value indicates that larger aggregates are formed. Furthermore, for the test samples of each Example and Comparative Example, the value of (dielectric loss tangent) / (specific surface area) (Df / SSA), temperature (T°C) × drying time (m min) ÷ volume of dispersion medium (A mL) was calculated and is shown in Table 1.

[0040]

[0041] When spherical silica was used as the metal oxide particle material, the results of Examples 1 to 3 and Comparative Example 2 showed that by setting the temperature × drying time ÷ dispersion medium volume (= T × m ÷ A) to 150 or less, the particle gauge value was small and high dispersibility could be achieved even with a small amount of modifier added. In Comparative Example 2, despite the small decrease in C / H value after washing of 0.05, the long heating time resulted in a particle gauge of 25 μ or more, resulting in aggregation. The results of Comparative Example 1 showed that when (T × m ÷ A) exceeded 150, the C content before washing was 1.8% and the C content after washing was 0.2%, indicating that a larger amount of modifier was required to attach compared to the Examples to reduce the particle gauge value, i.e., to suppress aggregation. Comparison of Examples 4 and 5 with Comparative Examples 3 and 4 revealed that, similar to Examples 1 to 3 and Comparative Example 1, when heating for a long period of time (when (T × m ÷ A) exceeded 150), even if the particle size was different, in order to suppress aggregation (to achieve similar particle gauge values), a larger amount of modifier was required than in the Examples. From the results of Example 6 and Comparative Example 5, it was found that even when a modifier having phenyl and methyl groups instead of diphenyl as functional groups was used, when heating was performed for a long period of time, a larger amount of modifier was required to suppress aggregation than in the examples. A similar tendency was observed when spherical alumina was used as the metal oxide particle material as when spherical silica was used. Specifically, compared to Comparative Examples 6 and 7, it was found that Example 7, by setting the temperature × drying time ÷ dispersion medium volume (= T × m ÷ A) to 150 or less, exhibited small particle gauge values ​​and high dispersibility even with a small amount of modifier added. Furthermore, it was found that by adding a larger amount of modifier than in Example 7, as in Comparative Example 6, aggregation could be suppressed to a certain extent even when heating was performed for a long period of time (when (T × m ÷ A) exceeded 150). As described above, it was found that by setting (T × m ÷ A) to 150 or less, dispersibility could be improved even with a small amount of modifier added.

Claims

1. A metal oxide particulate material having a functional group other than a phenyl group on its surface, and a modifying material comprising a silicon-containing compound having a phenyl group and adhering to the surface of the metal oxide particulate material, and having a surface area H (m 2 a C / H value calculated from the mass percent of the modified metal oxide particles and the carbon content C (mass%) is reduced by 0.001 or more and less than 0.1 after washing with methyl ethyl ketone, the particle size is 20 μm or less on a grain gauge, and the C / H value after washing is 0.07 or less.

2. The modified metal oxide particulate material according to claim 1, wherein (dielectric tangent) / H is 0.0005 or less.

3. The modified metal oxide particle material according to claim 1, which can be prepared by applying a modifying material liquid in which the modifying material is dissolved or dispersed in A mL of a solvent to the metal oxide particle material, and then heating and drying at T°C for m minutes (wherein T×m÷A is 150 or less).

4. The modified metal oxide particulate material according to claim 1, wherein the silicon-containing compound constituting the modified material is a silane compound having a phenyl group, or a condensation product of a silane compound having a phenyl group and a silane compound having a hydrocarbon group directly bonded to Si.

5. The silane compound having a phenyl group is ((C 6 H 5 ) X) n -Si-OR (4-n) The silane compound having a hydrocarbon group is represented by R n -Si-OR (4-n) The modified metal oxide particulate material of claim 4, wherein X is a direct bond or a -(CH 2 ) q - or -O-; q is an integer from 0 to 3; n is an integer from 1 to 3 selected independently for each molecule; R is a hydrocarbon group having 1 to 3 carbon atoms selected independently for each functional group.

6. The silicon-containing compound constituting the modifying material has the general formula (1): R1-O-(SiZ1Z2O) n -(SiZ3Z4O) m 2. The modified metal oxide particulate material of claim 1, wherein Z1 is (C 6 H 5) X-; Z2 to Z4 each independently represent (C 6 H 5 ) X-, a hydrocarbon group having 1 to 3 carbon atoms, an alkoxy group having 1 to 3 carbon atoms, and -O which bonds to other Z2 to Z4 r - (CH 2 ) p -O t -; X is a direct bond or -(CH 2 ) q - or -O-; n and p are integers of 1 or greater; m is an integer of 0 or greater; q is an integer of 0 or greater that is independently selected; r and t are each independently selected from 0 or 1; R1 and R2 are each independently selected from a hydrocarbon group having 1 to 3 carbon atoms or an alkoxy group having 1 to 3 carbon atoms).

7. The modified metal oxide particulate material of claim 1, wherein said metal oxide particulate material is surface treated with a silane compound.

8. The modified metal oxide particulate material according to claim 1, having a volume average particle size of 0.01 μm or more and 5 μm or less.

9. A method for producing a modified metal oxide particulate material according to any one of claims 1 to 8, comprising: a surface treatment step of surface-treating a metal oxide particulate material with a silane compound to obtain a surface-treated metal oxide particulate material; a dispersion step of dispersing a silicon-containing compound having a phenyl group in a dispersion slurry obtained by dispersing the surface-treated metal oxide particulate material in A mL of a dispersion medium; and a drying step of drying the dispersion medium by heating at T°C for m minutes after the dispersion step, thereby adhering a modifying material consisting of the silicon-containing compound to the surface of the surface-treated metal oxide particulate material to obtain a modified metal oxide particulate material (wherein T×m÷A is 150 or less).

Citation Information

Patent Citations

  • Dispersion liquid containing surface-modified inorganic particle, silicone resin composition, cured body, optical member, light-emitting device, display device and surface-modified inorganic particle

    JP2017115111A

  • Modified metal oxide particle material and method for producing same

    WO2021210176A1

  • Modified metal oxide particle material and method for producing same

    WO2021210628A1

Cited By

  • Modified metal oxide particulate material and method for producing same

    WO2026203373A1