PROCESSO PARA SEPARAR E RECUPERAR PELO MENOS UM COMPONENTE DE POLÍMERO A PARTIR DE UMA FUSÃO DE UM NÚMERO MÚLTIPLO DE COMPONENTES DE POLÍMEROS
The described process effectively separates and recovers individual polymer components from mixed streams by shearing a molten mixture with an aqueous solution, addressing the challenge of recycling incompatible polymers and enabling their reuse.
Patent Information
- Application Number
- BR122026025052
- Authority / Receiving Office
- BR · BR
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2021-06-22
- Filing Date
- 2022-06-17
- Publication Date
- 2026-11-10
AI Technical Summary
Existing recycling methods struggle to separate and recover individual polymer components from mixed streams of incompatible polymers, making it difficult to recycle multicomponent polymer articles effectively.
A process involving the shearing of a molten mixture of multiple polymer components with a pressurized aqueous solution containing water and a dispersing agent, followed by separation and recovery of a desired single-component polymer stream.
Enables the efficient separation and recovery of individual polymer streams, allowing for effective recycling and reuse of enriched single-component polymer streams in new applications.
Description
1 / 40 PROCESS FOR SEPARATING AND RECOVERING AT LEAST ONE POLYMER COMPONENT FROM A MELTS OF MULTIPLE POLYMER COMPONENTS “Divided from BR 11 2023 024280 0, filed on 05 / 17 / 2022” FIELD
[0001] The present invention relates to an aqueous process for separating at least one separate and distinct single-component polymer stream from a molten mixed polymer stream having a mixture of multiple polymer components. The aqueous process allows recycling the at least one separate and distinct single-component polymer stream that is separated from the molten mixed polymer stream. BACKGROUND
[0002] In an effort to reduce the amount of plastic waste generated in the environment, there is a desire to reuse (recycle) plastic articles such as post-consumer disposable plastic products, including, for example, packaging and multilayer films that are commonly applied in single-use applications and then discarded. Typically, a mixture of incompatible polymer components is present in disposable products, as disposable products are generally manufactured from materials comprising a combination of different types of incompatible polymer components. The incompatible polymer components are combined, for example, by compounding the different polymer components together to form a component blend; or by combining (e.g., by lamination) two or more layers of different polymer components together to form a multilayer system.
[0003] Generally, an article is produced from multiple different polymer components to allow the article to meet specific application requirements. However, the problem with disposable articles and products produced from multiple polymer components is that such multicomponent polymer articles / products are generally undesirable for recycling because such articles / products made from polymer of Petition 870260101801, dated 02 / 10 / 2026, page 11 / 102 2 / 40 Multiple components generate a mixed stream of different incompatible polymer components that make the mixed stream difficult to reuse in new applications. Furthermore, it is difficult to separate a desired single-polymer component stream from the incompatible mixed polymer component stream. For example, when a blend or mixture of different polymers is used to manufacture an article incorporating the mixture of different polymers, such as a multilayer packaging or a multilayer film; such an article typically cannot be directly recycled due to the incompatibility of the different polymers that form the article.To employ an effective recycling method to obtain reusable articles (e.g., multilayer packaging / films) produced from a blend of different polymer components, the polymer component blend of the articles must be separated into one or more separate single-polymer component streams; then, the desired single-polymer component stream can be separated from the other undesired blend of polymer components in the stream. Once the desired single-polymer component stream is separated from the blended polymer stream, the desired single-polymer component stream can be recovered for reuse (recycling).
[0004] It would be advantageous for the recycling sector to be able to consider a disposable article or product (e.g., packaging or film) produced from incompatible polymer components and separate the incompatible polymer components into separate and distinct single-component polymer streams to facilitate the recovery of the desired single-component polymer stream for recycling. It is therefore desirable to provide an effective separation and recovery process, including the step of shearing a molten fluid liquid composition of a mixture (blend) of multiple different incompatible polymer components (originating, for example, from one or more thermoplastic polymer articles) to separate the mixture or blend of different polymer components into separate single-component polymer streams; and then recovering, from the blend of Petition 870260101801, dated 02 / 10 / 2026, page 12 / 102 3 / 40 different polymer components, the desired single-component polymer stream has an enriched single-component polymer to allow recyclers to reuse the recovered enriched single-component polymer stream in a new application. SUMMARY
[0005] The process of the present invention provides a solution to the problem of prior art processes by enabling the isolation of a desired polymer component stream, such as a PE stream, from a composition of mixed polymer components. Consequently, the present invention disclosed herein relates to an innovative and efficient process for separating and recovering one or more individual single component streams from a molten material (or melt) comprising a molten mixture of at least two or more different incompatible polymer component streams. The melt is generated from the processing of a thermoplastic source.For example, the thermoplastic source may be a thermoplastic article or a plurality of thermoplastic articles (e.g., a laminate, composite, film, or packaging material); wherein the thermoplastic source includes a mixture, blend, or combination of multiple (e.g., two or more) polymer components (herein referred to as multipolymer components or abbreviated as multiple PCs); and wherein the multiple PCs of the thermoplastic source are typically incompatible.
[0006] The thermoplastic source is subjected to heating / melting to form a multi-PC melt; and then the multi-PC melt is subjected to the innovative process described above to generate at least one separate single-polymer component stream for recovery and subsequent use. In this way, one embodiment to solve the incompatibility problem encountered with the use of prior art processes is to use the novel separation / recovery process described above which includes, for example, the shearing step of the multi-PC melt in the presence of a separation fluid such as a liquid solution of aqueous separation fluid that is pressurized to maintain the aqueous solution in liquid form. Shearing the formulation or the Petition 870260101801, dated 02 / 10 / 2026, page 13 / 102 4 / 40 blend composition, additive, combination or mixture of: (I) at least the melt of multiple PCs and (II) at least the aqueous solution (hereinafter abbreviated as the MAS mixture) forms at least one desired single-component polymer stream that can be readily separated from the other polymer components present in the melt of multiple PCs.
[0007] In one embodiment, the process for separating and recovering at least one single polymer component from a melt of multiple PCs (which, as described above, has been obtained from one or more thermoplastic articles) that has a mixture of multiple different polymer components includes the steps of: (A) shearing the MAS mixture (i.e., shearing the mixture comprising the melt of multiple PCs and aqueous solution); wherein the melt of multiple PCs comprises at least one first polymer component and at least one second polymer component; wherein the melt of multiple PCs has two or more thermal melting temperatures (Tm), two or more glass transition temperatures (Tg), or combinations thereof; wherein the pressurized aqueous solution comprises an aqueous liquid mixture of: (i) water, and (ii) at least one dispersing agent;(A) whereby shearing the MAS mixture forms a dispersion, particles, or filaments of at least one first polymer component having an enriched first polymer component concentration; and (B) after shearing in step (A), separating the dispersion, particles, or filaments of at least one first polymer component having an enriched first polymer component concentration from the other melt components (e.g., water, at least one dispersing agent, at least one second polymer component, and any remaining thermoplastic polymer resin components and / or optional components).
[0008] In another embodiment, the process for separating and recovering at least one single-polymer component stream having a polymer-enriched concentration of the single-polymer component from a multi-PC melt stream having a mixture of multiple (e.g., two or more) different polymer components includes the steps of: (a) providing by Petition 870260101801, dated 02 / 10 / 2026, page 14 / 102 5 / 40 less a multi-PC thermoplastic article or a combination of two or more thermoplastic articles comprising at least one first polymer component and at least one second polymer component; (b) melting the multi-PC thermoplastic article or the combination of two or more thermoplastic articles to form a flowable liquid multi-PC melt stream; wherein the multi-PC melt stream comprises a blend or mixture of at least one first polymer component melt stream and at least one second polymer component melt stream; wherein the multi-PC melt stream exhibits two or more peaks in the second heat cycle of the second multi-PC melt stream using differential scanning calorimetry; (c) providing a pressurized aqueous solution;wherein the aqueous solution comprises an aqueous mixture of liquid fluid solution of: (i) water, and (ii) at least one dispersing agent; (for example, a mixture of ethylene oxide (EO) / propylene oxide (PO) or an ethylene copolymer); wherein the pressure in the aqueous solution is sufficient to maintain the aqueous solution in liquid phase at a working temperature; (d) mixing the pressurized aqueous solution of step (c) with the melt of multiple PCs of step (b) to form the MAS mixture; (e) shearing the MAS mixture of step (d) (i.e., the mixture of (i) melt of multiple PCs of step (b) in contact with (ii) the pressurized aqueous solution of step (c)); wherein the shearing of the MAS mixture forms a dispersion, particles, or filaments of at least one first polymer component stream having an enriched first polymer component concentration;(f) after shearing in step (e), separate (e.g., by mechanical or physical means) the dispersion, particles or filaments of at least one first polymer component having an enriched first polymer concentration from the other components present in the MAS mixture (e.g., water, at least one dispersing agent, at least one second polymer component, any remaining thermoplastic polymer resin components from the melting of multiple PCs and / or any optional components); and (g) recover the dispersion, particles or filaments separated from step (f). Petition 870260101801, dated 02 / 10 / 2026, page 15 / 102 6 / 40
[0009] One objective is to provide an innovative and effective separation / recovery process for separating at least one single-polymer component from multiple-polymer components present in a multi-PC melt; and to recover the single-polymer component to enable the effective recycling of the recovered single-polymer component. BRIEF DESCRIPTION OF THE DRAWINGS
[0010] Figure 1 is a schematic flowchart of the process of the present invention. DETAILED DESCRIPTION
[0011] Ambient temperature (TA) and local temperature in the present invention mean a temperature between 20 °C and 26 degrees Celsius (°C), unless otherwise specified.
[0012] The terms fused, fusion and melted with reference to a polymer resin are used interchangeably herein.
[0013] The term thermal transition, with reference to a polymer resin, in this document means melting or melting temperature (Tm) and / or glass transition temperature (Tg).
[0014] The term second heat cycle in this document refers to the heating operation of a DSC after a first heat cycle in which a sample is heated from ambient conditions to above a temperature at which the sample is in its melting state and then the sample is cooled below its thermal transitions.
[0015] A broad embodiment of the process of the present invention includes processing a thermoplastic article or a combination of two or more thermoplastic articles wherein each of the articles may be constructed from a multiple number (e.g., at least two or more) of thermoplastic polymer components. The process includes separating and recovering at least one of the thermoplastic polymer components from the multiple number of thermoplastic polymer components present in one or more of the thermoplastic items. Petition 870260101801, dated 02 / 10 / 2026, p. 16 / 102 7 / 40
[0016] In one embodiment, the thermoplastic article(s) comprise(s) a blend, combination, composite or mixture of multiple (e.g., two or more) polymer components (hereinafter referred to as multipolymer components or abbreviated as multiple PCs, as previously mentioned). Typically, the multiple PCs of the items are incompatible. The article or combination of two or more articles produced from at least two or more thermoplastic polymer components are melted to form a multiPC melt. The multiPC melt is then contacted and treated with a separation fluid (e.g., an aqueous separation liquid solution) comprising a mixture of (i) water and (ii) at least one dispersing agent.Next, the fusion of multiple PCs in the presence of the aqueous solution is subjected to shearing to separate the multiple polymer components of the article into separate single-component polymer streams; and then, recovering the desired single-component polymer streams from all other polymer streams created during the shearing process described above. In some embodiments, the process allows for the recycling of the recovered single-component polymer streams.
[0017] In a preferred embodiment, the process for separating and recovering at least one single polymer component from an article constructed of a multiple number of polymer components includes the steps of: (a) providing at least one multi-PC thermoplastic article having at least one first polymer component and at least one second polymer component; (b) melting the at least one multi-PC thermoplastic article to form a molten or melted multi-PC article (herein referred to as a multi-PC melt); wherein the resulting multi-PC melt, originating from the at least one multi-PC article, comprises a blend of at least one first melt stream of polymer components and at least one second stream of polymer material; wherein the multi-PC melt exhibits two or more peaks in the second heat cycle of the melt using differential scanning calorimetry; (c) providing a Petition 870260101801, dated 02 / 10 / 2026, p. 17 / 102 8 / 40 aqueous solution, under a predetermined pressure, including a pressurized aqueous liquid mixture of: (i) water, and (ii) at least one dispersing agent; (d) adding the multi-PC melt from step (b) to the pressurized aqueous liquid solution from step (c) to form a formulation or a mixture composed of (i) the aqueous solution and (ii) the multi-PC melt (i.e., the MAS mixture); (e) shearing the MAS mixture to form, in the MAS mixture, a dispersion, particles or filaments of at least one first polymer component stream having an enriched first polymer component concentration;(f) after shearing in step (e), separate the dispersion, particles or filaments from at least one first polymer component stream that has a first concentration of enriched polymer component from the other components present in the MAS mixture (e.g., water, at least one dispersing agent, at least one second polymer component, any remaining thermoplastic polymer resin components from the melting of multiple PCs and / or any optional components in the MAS mixture); and (g) recover the dispersion, particles or filaments separated from step (f).
[0018] In some preferred embodiments, the process includes, for example, a shear of step (e) occurring at a temperature of 105 °C to 300 °C; a shear of step (e) occurring at a useful pressure of at least 100 kilopascals (kPa); and a shear of step (e) occurring for a period of less than 20 minutes (min).
[0019] In a preferred embodiment of the process, the separation of step (f) may comprise a flotation process, a filtration process or a flocculation process.
[0020] In a preferred embodiment of the process, the first polymer component of the melt is a polyolefin component; and the polyolefin component is selected from the group consisting of high-density polyethylene; low-density polyethylene; linear low-density polyethylene; ethylene copolymers; or mixtures thereof.
[0021] With reference to Figure 1, a flowchart is shown, usually indicated Petition 870260101801, dated 02 / 10 / 2026, page 18 / 102 9 / 40 by reference number 10, of an embodiment of the process of the present invention including flow streams indicated by numbers 11 to 16. For example, the first step of the process shown in Figure 1, generally indicated by reference number 20, begins with a thermoplastic material which may include a group or a combination of one or more thermoplastic polymer articles 21 to be subjected to the process. The articles 21 comprise, and are constructed from, a blend or mixture of multiple polymer components in the structure of the article 21. The articles 21 may be rigid articles, flexible articles and mixtures thereof.
[0022] Articles 21 are passed to a densification step, usually indicated by reference number 30, via stream 11. The densification step 30 can be performed using any conventional equipment to convert articles 21 into a plurality of smaller parts 31, i.e., the parts 31 are smaller compared to the size of the original source of thermoplastic material (e.g., articles 21). For example, the densification step 30 can form the parts 31 by grinding (not shown) the articles 21 to form flakes 31. Other embodiments of the densification step 30 may include, for example, crushing the articles (not shown) 21 to form crushed pieces (not shown); pelletizing (not shown) the articles 21 to form pellets (not shown); and / or comminuting (not shown) the articles 21 to form a powder (not shown). In some forms, the flake size 31 can be, for example, smaller than 200 microns (µm).
[0023] As shown in Figure 1 again, the flakes 31 are passed, through the stream 12, to an extrusion stage generally indicated by the reference number 40 including an extruder 41 and feed hopper 42. The extruder 41 is a twin-screw extruder 41, however, the extruder 41 may include a single-screw extruder or other types of extruders. Although not shown in Figure 1, various auxiliary elements and equipment may be included in the extrusion operation 40; for example, the extruder 41 may include one or more elements of Petition 870260101801, dated 02 / 10 / 2026, page 19 / 102 10 / 40 heating / cooling, one or more feed ports, one or more pumps and other conventional equipment known to those skilled in the art of extrusion. The flakes 31 in solid form are passed, via the current 12, into the feed hopper 42 of the extruder 41; and then the solid flakes 31 are passed through a heating zone within the extruder 41 by the screws 43. The flakes 31 are passed through the heating zone to melt the flakes 31 and form a flowable liquid melt (not shown) exiting the extruder outlet port 44.
[0024] To continue the process, as shown in Figure 1, the melt (resulting from the melting of one or more molten articles 21) in the form of a molten stream (or melt) is formed in a heating zone (not shown) in the extruder 41. A stream 13 of aqueous solution (i.e., the liquid solution of aqueous separation fluid) is introduced into the extruder 41, maintained under a predetermined pressure and mixed with the molten flake stream in the extruder 41 to form a MAS mixture exiting the extruder 41 as stream 14 forms the exit port 44 of the extruder 41. The aqueous solution stream 13 can be introduced into the extruder 41 through a feed port (not shown) before or in front of the flake stream 12; after or subsequent to the flake stream 12 (as shown in Figure 1); simultaneously with the flake stream 12; and / or before or after the melt flake stream is formed in the heating zone of extruder 41.
[0025] The MAS mixture (i.e., the combined aqueous solution and the fusion of multiple PCs) is passed through stream 14 to a separation step generally indicated by the reference number 50. The separation step 50 may include various conventional mechanical separation processes known to those skilled in the art, including, for example, but not limited to, a flotation process, a filtration process, a flocculation process, or a combination thereof. Figure 1 shows an embodiment of a separation process 50 which includes, but is not limited to, a flotation process 50 in which the MAS mixture stream 14 undergoes separation by flotation in a reservoir 51. In the flotation separation step 50, the mixture of Petition 870260101801, dated 02 / 10 / 2026, page 20 / 102 11 / 40 Multiple types of polymer components in the melt of multiple PCs that are present in the mixture MAS as polymer component streams are separated into at least one or more single polymer component streams that are distinct polymer component streams for each of the polymer types present in the melt of multiple PCs.
[0026] Figure 1 shows that the MAS mixture, generally indicated by reference number 52, from stream 14 was separated into two distinct layers – a desired plurality of solids layer 53 and an undesired liquid layer 54 in reservoir 51. The desired solids layer 53 comprises a desired layer of a plurality of floating solids components that are separated and removed from the other components in the MAS mixture. For example, the desired solids layer may include particle dispersion; a plurality of micron-sized particles, flakes or pellets; or a plurality of filaments of at least one single polymer component that separates from the other components in the MAS mixture. The undesired liquid layer 54 may also contain solids that are not floating and are undesirable.In one embodiment, for example, the solids (e.g., PE particles) that form the solid layer 53 float to the top of the liquid solution layer 54 to form the desired plurality of solids (e.g., a large quantity of particles) 53.
[0027] After separation step 50, the particle layer 53 is recovered and can be recycled (reused) by passing the particles 53 through stream 15 to a recycling system (not shown) to form a new product 55. In some embodiments, the new product 55 may be, for example, an article similar to the original article 21 (for example, a bottle container, a film or packaging article) or the new product may be some other article different from article 21. Alternatively, the particle layer 53 may be sent to a different processing step, such as a drying step before the particles 53 are used. The liquid solution layer 54 may comprise the residue or rejects from the melting of multiple PCs after treatment of the melt with aqueous liquid solution during the step of Petition 870260101801, dated 02 / 10 / 2026, page 21 / 102 12 / 40 shear (e). After separation step 50, the liquid layer 54 can be recovered and sent, via stream 16, to another processing step 56, as a recovery step to recover other components in the liquid phase 54 or the liquid 54 can be discarded, if desired.
[0028] To illustrate the process of the present invention, and not to be limited by it, in one embodiment, for example, an article or a mixture of articles, such as a plastic bottle (or bottles) or a mixture of different articles, such as rigid plastic bottles and flexible plastic bags (see article 21) produced from multiple polymer components such as a blend of polypropylene (PP) and polyethylene (PE), can be separated into a PP stream and a PE stream using the separation process 50. In other embodiments, the separation process 50 is used to produce at least one stream (e.g., stream 14) of a single polymer component that has an enriched concentration of the single polymer component in the stream.In a preferred embodiment, for example, the PE polymer component stream (layer 53) having an enriched PE concentration in the stream can be passed (e.g., through stream 15 of Figure 1) to a recycling system to enable the recycling (reuse) of such a single polymer-enriched component stream.
[0029] The melting of multiple PCs comprises a blending or mixing of multiple molten polymer components; and the molten material is useful as a feed stream for the shearing step (see shearing operation 40 of Figure 1) of the process described above. The melting of multiple PCs may be a mixture of at least two or more polymer components, that is, at least one first polymer component and at least one second polymer component; wherein at least one of the first or second polymer components (e.g., the at least one first polymer component) may be melted and reformed into a new or different article. In a preferred embodiment, the first and second polymer components are Petition 870260101801, dated 02 / 10 / 2026, page 22 / 102 13 / 40 Polymer components that do not crystallize, that is, no cocrystallization occurs between the desired polymer component and any other polymer component. The terms crystallize, crystallization, crystallizing, and cocrystallization, with reference to a polymer, in this document, mean forming an ordered domain by solidifying a molten phase. Cocrystallization can be determined using a differential scanning calorimeter (DSC), and cocrystallization can be readily identified by whether or not multiple melting temperatures or glass transition temperature events can be observed using DSC. For example, if a single melting peak is observed for a molten material, the molten material can be considered cocrystallized. In another example, if two melting peaks are observed for a molten material, the molten material can be considered non-cocrystallized.
[0030] In some embodiments, the melt feed stream of multiple PCs in the shearing stage of the process comprises, for example, at least one first polymer component; and in a preferred embodiment, the at least one first polymer component is a polymer component that is capable of being melted and reformed. The first polymer component of the melt material can be selected, for example, from the group that includes polyolefins; acrylics; styrenic copolymers; styrene copolymers; polyamides; thermoplastic urethanes; thermoplastic silicones; and combinations thereof.
[0031] Examples of polyolefins useful in the process include ethylene polymers and copolymers; and propylene polymers and copolymers. Particularly useful in the process are polyolefins such as high-density polyethylene (HDPE), low-density polyethylene (LDPE), linear low-density polyethylene (LLDPE), medium-density polyethylene (MDPE), linear ultra-low-density polyethylene (ULDPE), PP, copolymers of ethylene with another monomer, copolymers of propylene with another monomer, and mixtures thereof; and the like.
[0032] The term LDPE can also be referred to as LDPE polymer Petition 870260101801, dated 02 / 10 / 2026, page 23 / 102 14 / 40 high-pressure ethylene or highly branched polyethylene is defined to mean that the polymer is partially or completely homopolymerized or copolymerized in autoclave or tubular reactors at pressures above 14,500 pounds per square inch (psi) (100 megapascals [MPa]) with the use of free radical initiators such as peroxides (see, for example, US Patent No. 4,599,392). LDPE resins typically have a density in the range of 0.916 grams per cubic centimeter (g / cm3) to 0.935 g / cm3.
[0033] The term LLDPE includes both resin produced using traditional Ziegler-Natta catalyst systems and from chromium-based catalyst systems, as well as single-site catalysts, including, but not limited to, bis-metallocene catalysts (occasionally referred to as m-LLDPE) and limited geometry catalysts, and includes linear, substantially linear, or heterogeneous polyethylene copolymers or homopolymers. LLDPEs contain fewer long-chain branches than LDPEs and include the substantially linear ethylene polymers that are further defined, for example, in U.S. Patents Nos. 5,272,236; 5,278,272; 5,582,923; and 5,733,155; the homogeneously branched linear ethylene polymer compositions, such as those in U.S. Patent No. 3,645,992; heterogeneously branched ethylene polymers, such as those prepared according to the process disclosed in U.S. Patent No. 4,076.698, and / or mixtures thereof (such as those disclosed in U.S. Patent No. 3,914,342 or 5,854,045). LLDPEs can be produced via gas-phase, solution-phase, or slurry polymerization, or any combination thereof, using any type of reactor or reactor configuration known in the art.
[0034] The term MDPE refers to polyethylenes that have densities of 0.926 g / cm3 to 0.935 g / cm3. MDPEs are typically made using chromium or Ziegler-Natta catalysts or using single-site catalysts including, but not limited to, bis-metallocene catalysts and restricted geometry catalysts; and MDPEs typically have a Petition 870260101801, dated 02 / 10 / 2026, p. 24 / 102 15 / 40 molecular weight distribution (MWD) greater than (>) 2.5.
[0035] The term HDPE refers to polyethylenes that have densities greater than 0.935 g / cm3 up to 0.970 g / cm3; and are generally prepared with Ziegler-Natta catalysts, chromium catalysts or single-site catalysts, including, but not limited to, bis-metallocene catalysts and restricted geometry catalysts.
[0036] The term ULDPE refers to polyethylenes that have densities of 0.880 g / cm3 to 0.912 g / cm3 and are generally prepared with Ziegler-Natta catalysts, chromium catalysts or single-site catalysts, including, but not limited to, bis-metallocene catalysts and restricted geometry catalysts.
[0037] The term PP refers to polypropylene polymers comprising more than 50% by weight of units derived from an ethylene monomer. Such polymers include polypropylene homopolymers or copolymers (meaning units derived from two or more comonomers). Common forms of polypropylene known in the art include homopolymer polypropylene (hPP), random copolymer polypropylene (rcPP), impact copolymer polypropylene (hPP + at least one elastomeric impact modifier) (ICPP) or high impact polypropylene (HIPP), high melt strength polypropylene (HMS-PP), isotactic polypropylene (iPP), syndiotactic polypropylene (sPP), and combinations thereof.
[0038] In some preferred embodiments, the first polymer component present in the multi-PC melt feed stream is a polyolefin or a polyolefin copolymer. In other preferred embodiments, the polyolefin component is selected from the group consisting of: HDPE, LDPE, LLDPE, ethylene copolymers or mixtures thereof. In still other preferred embodiments, the polymers useful as the first polymer component in the process are polymeric materials with a melting index of 0.5 grams per 10 minutes (g / 10 min) to 80 g / 10 min; and a melting temperature of 60 °C to 150 °C. Petition 870260101801, dated 02 / 10 / 2026, page 25 / 102 16 / 40
[0039] In other embodiments, the first polymer component present in the multi-PC melt feed stream may include commercially available polyolefins or polyolefin copolymers, such as VERSIFY (a random copolymer available from The Dow Chemical Company); INTUNE (an ethylene block copolymer, also available from The Dow Chemical Company); and mixtures thereof.
[0040] In some embodiments, the second polymer component present in the multi-PC melt feed stream may be selected from other polymers that have a melt index of 0.5 g / 10 min to 400 g / 10 min; and a higher melt temperature than the first polymer component material. For example, the second polymer component may include polyesters, polyethylene terephthalate, polyamides, metallized forms of oriented films, such as metallized PET film or metallized PP film, PP and mixtures thereof.
[0041] Some of the preferred multiple polymer blends or polymer combinations used as the melt feed stream for multiple PCs in the process may include, for example, polypropylene / polyethylene (PP / PE), polyethylene terephthalate / polyethylene (PET / PE), metallized oriented polyethylene terephthalate film / polyethylene (m-PET / PE); polyamide / polyethylene (PA / PE), and mixtures thereof.
[0042] In some embodiments, the multiple polymer blends or polymer combinations used as the melt feed stream for multiple PCs in the process can be obtained from post-consumer products or post-industrial recycled products.
[0043] The process for separating and recovering polymer components from the melt of multiple PCs includes the step of providing an aqueous separation fluid solution (hereinafter abbreviated as aqueous solution) that can be pressurized to a pressure sufficient to maintain the aqueous solution in liquid form. In one embodiment, the aqueous solution includes an aqueous liquid mixture of: (i) water, and (ii) at least one dispersing agent; and (iii) any other optional additive or component, as desired. The additives Petition 870260101801, dated 02 / 10 / 2026, p. 26 / 102 17 / 40 desired optional additives are additives that can more easily allow the formation, in aqueous solution, of a dispersion, particles or filaments of at least one first polymer component, such as PE, wherein the resulting first polymer component stream has an enriched concentration of first polymer component (e.g., PE).
[0044] In a preferred embodiment, the water used in the aqueous solution of the process can be water from any source including, for example, deionized water. The water acts as a diluent in the aqueous solution.
[0045] The amount of water used to form the aqueous solution is from 50% by weight to 99.9% by weight in one general embodiment; from 65% by weight to 99.5% by weight in another embodiment; and from 85% by weight to 97.5% by weight in yet another embodiment.
[0046] In one embodiment, the aqueous solution includes at least one dispersing agent (which may also be called a surfactant), component (ii). The dispersing agent may include, for example, a mixture of ethylene oxide (EO) / propylene oxide (PO); an ethylene copolymer; other conventional dispersing agents known in the art; and mixtures thereof.
[0047] The dispersing agent useful in the process may be conventional dispersing agents used in the art for polymer dispersions. For example, the dispersing agent may comprise at least one carboxylic acid, a salt of at least one carboxylic acid, or a carboxylic acid ester or carboxylic acid ester salt. The carboxylic acid, the salt of the carboxylic acid, or the carboxylic acid portion of the carboxylic acid ester or the salt of such ester may have up to 60 carbon atoms (C), or up to 50 C, or up to 40 C, or up to 30 C, or up to 25 C. The carboxylic acid, the salt of the carboxylic acid, or the carboxylic acid portion of the carboxylic acid ester or the salt of such ester may have at least less than 12 C, at least or at least 15 C, or at least 20 C, or at least 25 C. If in salt form, the dispersing agent comprises a cation selected from the group consisting of an alkali metal cation, alkaline earth metal cation, or ammonium or alkyl ammonium cation.The dispersing agent can be an olefin carboxylic acid polymer (e.g., Petition 870260101801, dated 02 / 10 / 2026, page 27 / 102 18 / 40 ethylene), or its salt, such as ethylene acrylic acid copolymers or ethylene methacrylic acid copolymers. Alternatively, the dispersing agent may be selected from alkyl ether carboxylates, petroleum sulfonates, sulfonated polyoxyethylene alcohols, sulfated or phosphated polyoxyethylene alcohols, ethylene oxide / propylene oxide dispersing agents, primary and secondary alcohol ethoxylates, alkyl glycosides and alkyl glycerides. Combinations of the above dispersing agents may also be used.
[0048] The amount of dispersing agent (or combinations of more than one dispersing agent) used to form the aqueous solution is from 0.1% by weight to 35% by weight in one general embodiment; from 0.5% by weight to 25% by weight in another embodiment; and from 3% by weight to 10% by weight in yet another embodiment.
[0049] A dispersing agent (or combinations of more than one dispersing agent) is used in amounts of at least 0.1% by weight, or at least 1% by weight, or at least 2% by weight, or at least 3% by weight to 35% by weight, or up to 30% by weight, or up to 20% by weight, or up to 10% by weight based on the total weight of contaminated thermoplastic, dispersing agent and any optional components (i.e., weight of the combination excluding water).
[0050] Although the aqueous solution, in a general embodiment, includes the two components (i) and (ii), the aqueous solution may be formulated with a wide variety of optional additives to enable the performance of specific functions while maintaining the excellent benefits / properties / performance of the aqueous solution. The optional component(s), component (iii), may be added to component (i) of the aqueous solution; or the optional component(s) may be added to component (ii) of the aqueous solution; or the optional component(s) may be added to both components (i) and (ii) of the aqueous solution. For example, in one embodiment, the optional additives, component (iii), useful in the aqueous solution may include enzymes, catalysts, other surfactants or dispersing agents other than those described above, pH modifiers, Petition 870260101801, dated 02 / 10 / 2026, p. 28 / 102 19 / 40 compatibilizers and mixtures thereof.
[0051] For example, in one embodiment, the other optional surfactants that can be used in the process can be any conventional surfactant known in the art, including cationic, nonionic, anionic, and mixtures thereof. The concentration of the optional surfactant can be from 0% by weight to 30% by weight in a general embodiment; and from 0.05% by weight to 30% by weight in another embodiment. In a preferred embodiment, the concentration of the optional surfactant can be towards the lower end of the general concentration range to avoid further impact on the final mechanical properties of the desired manufactured product.
[0052] A compatibilizer may be used in addition to the dispersing agent. For example, when non-ionic dispersing agents, such as ethylene oxide / propylene oxide copolymers, are used, an additional compatibilizer may be particularly desirable. A compatibilizer may also be used in combination with anionic or cationic dispersing agents.
[0053] The compatibilizer can improve the compatibility between the dispersing agent and the thermoplastic. The compatibilizer can be, for example, an acid-functionalized wax. The compatibilizer will generally have a lower amount of acid functionality than the dispersing agent or, alternatively, a higher acid equivalent weight. The compatibilizer may have an acid number of 10 to 70. Acid number is the number of milligrams of potassium hydroxide required to neutralize the free acid present in one gram of the material (in this case, the compatibilizer). The compatibilizer may have a melting index of 500 to 5,000,000 g / 10 min at 190 °C with a 2.16 kg charge.Non-limiting examples of compatibilizers include acid-modified polyolefin wax, maleic anhydride copolymer wax, maleic anhydride-modified polyethylene wax, maleic anhydride-modified polypropylene wax, and mixtures thereof. A commercial example of a compatibilizer includes: Maleic anhydride-stabilized graft wax. Petition 870260101801, dated 02 / 10 / 2026, p. 29 / 102 20 / 40 LICOCENE™ 431 (sometimes referred to as MA-g-PE), available from Clariant Corporation. The amount of optional compatibilizer can be 0% by weight, or 0.5% by weight up to 15% or up to 10% by weight based on the total weight of the thermoplastic, dispersing agent and contaminated compatibilizer and any other optional components (i.e., weight of the combination excluding water).
[0054] With certain dispersing or compatibilizing agents, it may be desirable to include a neutralizer to improve the effectiveness of the dispersing agent. For example, a base, such as a metal hydroxide (e.g., KOH), may be added. The amount of neutralizing agent or base may be from 60 to 120 percent (%) based on the cumulative acid number of the dispersing agent and any compatibilizer.
[0055] In a general embodiment, the amount of other optional additives, component (iii), useful to add to the aqueous solution, may generally be in the range of 0% by weight to 5% by weight in one embodiment; from 0.01% by weight to 2.5% by weight in another embodiment; and from 1% by weight to 1.5% by weight in yet another embodiment based on the total weight of the components in the pressurized aqueous solution.
[0056] The aqueous liquid solution used in the process has several advantageous properties and benefits when used to treat the thermoplastic polymers used in the process. For example, the aqueous liquid solution allows for reduced interfacial tension between the polymer and water phases to enable dispersion.
[0057] The process includes a melting step to melt at least one multi-PC thermoplastic article under process conditions to form a molten or melted multi-PC article (described above as a multi-PC melt) before combining the multi-PC melt with the aqueous solution; and before the shearing and separation steps. In some embodiments, the temperature used is, for example, sufficient to convert the multi-PC thermoplastic articles into a melt. In other embodiments, for example, the temperature used to form the multi-PC melt may be above the melting temperature by at least the Petition 870260101801, dated 02 / 10 / 2026, p. 30 / 102 21 / 40 first polymer component of the multi-PC melt up to 280 °C depending on the first polymer component. In a preferred embodiment, the melt temperature should be maintained below a temperature at which degradation of the multi-PC melt may occur. For example, the melt point (MP) temperature of the first polymer component in the multi-PC melt feed stream may be up to 300 °C. In some embodiments, the MP temperature of the first polymer component may be from 40 °C to 250 °C in one embodiment; from 90 °C to 190 °C in another embodiment; and from 110 °C to 140 °C in yet another embodiment. Thus, in some embodiments, the melting temperature used in the process may be, for example, at least 105 °C, or at least 110 °C, or at least 130 °C, or at least 150 °C, or at least 160 °C up to 300 °C, or up to 280 °C, or up to 250 °C, or up to 240 °C, or up to 230 °C, or up to 220 °C, or up to 210 °C, or up to 200 °C.
[0058] The process includes an addition step, for example, step (d) of the process described above. In the addition step, the aqueous liquid solution may be added to the melt of multiple PCs in concentrations and under process conditions sufficient to form a formulation or mixture composed of: (I) at least the aqueous solution and (II) at least the melt of multiple PCs (i.e., the MAS mixture described above). The addition step may be performed before the shearing and separation steps. Furthermore, in some embodiments, the aqueous solution is added to the melt of multiple PCs under process conditions to maintain the MAS mixture in a flowable liquid form. The temperature of the addition step may be equal to the melting temperature described above.Therefore, in some embodiments, the temperature used during the addition step may be, for example, at least 105 °C, or at least 110 °C, or at least 130 °C, or at least 150 °C, or at least 160 °C up to 300 °C, or up to 280 °C, or up to 250 °C, or up to 240 °C, or up to 230 °C, or up to 220 °C, or up to 210 °C, or up to 200 °C.
[0059] In a preferred embodiment, the aqueous solution is pressurized Petition 870260101801, dated 02 / 10 / 2026, p. 31 / 102 22 / 40 to keep the aqueous solution in liquid form. In some embodiments, for example, the pressure applied to the aqueous solution during the addition step may be at least 15 pounds per square inch (psig) (1.034 bar), or at least 20 psig (1.378 bar), or at least 50 psig (3.447 bar), or at least 80 psig (5.515 bar), or at least 100 psig (6.894 bar), or at least 150 psig (10.342 bar), or at least 200 psig (13.789 bar) up to 1,000 psig (68.947 bar), or up to 600 psig (41.368 bar), or up to 500 psig (34.473 bar), or up to 450 psig (31.0264 bar), or up to 400 psig (27.5790 bar), or up to 350 psig (24,131 bar) or up to 300 psig (20,684 bar). Alternatively, the pressure may be at least 100 kPa, or at least 150 kPa, or at least 200 kPa, or at least 500 kPa, or at least 1,000 kPa up to 7 MPa, or up to 4 MPa, or up to 3.5 MPa, or up to 3 MPa.
[0060] After the addition step described above, where the aqueous solution is combined or mixed with the melt of multiple PCs to form the MAS mixture, the process includes subjecting the MAS mixture to a shearing step at a temperature above the melting temperature of a first polymer component of the melt of multiple PCs. Consequently, the MAS mixture is subjected to shearing at a high temperature above the melting temperature of at least the first polymer component in the melt of multiple PCs; and at a high pressure to keep the water and any other optional liquid additives present in the aqueous solution or the MAS mixture in a flowable liquid form as the MAS mixture is being subjected to shearing.
[0061] In some embodiments, for example, the temperature applied to the MAS mixture (i.e., the mixture of the melt composition of multiple PCs and aqueous liquid solution) during the shearing step may be the same as the melting step and the addition step temperatures described above. For example, the shearing step of the melt of multiple PCs in the presence of the aqueous liquid solution may be carried out at a temperature above the melting temperature of at least one polymer component (e.g., at least the first polymer component) of the melt. Petition 870260101801, dated 02 / 10 / 2026, page 32 / 102 23 / 40 multiple PCs consisting of at least two or more polymer components that have multiple melting temperature peaks, glass transition temperature peaks, or combinations thereof, and up to 280 °C depending on the first polymer component. Consequently, in some embodiments, the temperature used during the shearing step may be, for example, from 60 °C to 280 °C in one general embodiment; from 90 °C to 190 °C in another embodiment; and from 140 °C to 170 °C in yet another embodiment. In other embodiments, the temperature of the shearing stage may be at least 105 °C, or at least 110 °C, or at least 130 °C, or at least 150 °C, or at least 160 °C up to 280 °C, or up to 250 °C, or up to 240 °C, or up to 230 °C, or up to 220 °C, or up to 210 °C, or up to 200 °C.
[0062] Furthermore, in some embodiments, for example, the pressure applied to the MAS mixture during the shearing stage may be equal to the melting stage and the pressures of the addition stage. Therefore, in some embodiments, the pressure used during the shearing stage may be, for example, at least 15 psig (1.034 bar), or at least 20 psig (1.378 bar), or at least 50 psig (3.447 bar), or at least 80 psig (5.515 bar), or at least 100 psig (6.894 bar), or at least 150 psig (10.342 bar), or at least 200 psig (13.789 bar) up to 1,000 psig (68.947 bar), or up to 600 psig (41.368 bar), or up to 500 psig (34.473 bar), or up to 450 psig (31.0264 bar), or up to 400 psig (27.5790 bar), or up to 350 psig (24.131 bar). or up to 300 psig (20,684 bar). Alternatively, the pressure may be at least 100 kPa, or at least 150 kPa, or at least 200 kPa, or at least 500 kPa, or at least 1,000 kPa up to 7 MPa, or up to 4 MPa, or up to 3.5 MPa, or up to 3 MPa.
[0063] The shear of the MAS mixture occurs with the fusion of multiple PCs in the melt form. The amount of shear must be sufficient to break the multiple polymer components in the fusion of multiple PCs into small particles in the presence of the aqueous solution. For example, the specific mechanical energy input in the MAS mixture may be at least 0.01 kilowatt hours per kilogram (kWh / kg), or at least 0.05 kWh / kg. Petition 870260101801, dated 02 / 10 / 2026, page 33 / 102 24 / 40 minus 0.08 kWh / KG. The specific mechanical energy can be up to 0.5 kWh / KG, or up to 0.4 kWh / KG, or up to 0.3 kWh / KG. In a preferred embodiment, when an extruder system is used to perform the shearing step (for example, see the extruder shown as number 41 in Figure 1), the specific mechanical energy for an extruder can be calculated using the following mathematical equation: {(nominal motor power in kilowatts) x [(actual applied torque) / (maximum torque for the extruder)] x [(screw speed) / (maximum screw speed for the extruder)] x extruder system efficiency} / [material throughput rate in the extruder (kilograms per hour)].
[0064] The efficiency of the extruder system is the efficiency of transferring the energy from the motor to the melting of multiple PCs. For example, certain energy losses can occur, for example, in gearboxes or other mechanical components.
[0065] In some embodiments, the MAS mixing stream is exposed to shear for a period of less than (<) 20 min in one general embodiment; < 10 min in another embodiment; and < 6 min in yet another embodiment. In other embodiments, the shearing of the MAS mixing stream may be carried out for a period of 1 min to 30 min in one general embodiment; from 2 min to 12 min in another embodiment; and from 4 min to 10 min in yet another embodiment.
[0066] During the shearing stage of the MAS mixture (i.e., the melting of multiple PCs in contact with the pressurized aqueous solution), a dispersion, particles or filaments of at least one polymer component in the melting of multiple PCs (e.g., at least one first polymer component) are formed with an enriched polymer concentration.
[0067] During the shearing stage, the aqueous solution is present in the MAS mixture at a concentration of 1% by weight to 50% by weight in one general embodiment; from 2.5% by weight to 35% by weight in another embodiment; and Petition 870260101801, dated 02 / 10 / 2026, page 34 / 102 25 / 40 from 5% by weight to 25% by weight in yet another modality.
[0068] Any or all of the process steps can be carried out as a batch process using conventional batch equipment in one embodiment; or the process can be carried out as a continuous process using conventional continuous equipment in another embodiment. In a preferred embodiment, the shearing step is conducted using an extruder on a continuous basis.
[0069] The shearing of the MAS mixture (i.e., the mixture comprising the fusion of multiple PC and aqueous solution; including any other optional ingredients), at elevated temperature and pressure, can occur in any device that can provide shear, pressure control, and temperature control. The device may be, for example, a conventional extruder system such as an extruder that has a shear zone and an extraction zone. Other conventional auxiliary equipment known to those skilled in the art of extrusion may include, for example, an extruder coupled to a back pressure regulator, a melt pump, or a gear pump.
[0070] In one embodiment, and with reference to Figure 1 again, an extruder system 40 is shown including, for example, a single twin-screw extruder to perform the melting, shearing, and extraction steps of the process of the present invention. However, the extruder system may include one or more extruders to provide the melting, shearing, and extraction steps. Different types of extruders, such as a single-screw extruder, a twin-screw extruder, and combinations thereof may be used. In a preferred embodiment, a single twin-screw extruder is used to perform the process as shown in Figure 1.
[0071] In some embodiments, before using an extruder to generate a multi-PC melt derivative by melting multi-PC thermoplastic articles or materials to form the multi-PC melt, the multi-PC thermoplastic articles or materials are supplied in solid form, such as in the form of solid pellets (i.e., not melted), powder or flakes by Petition 870260101801, dated 02 / 10 / 2026, p. 35 / 102 26 / 40 Processing of thermoplastic articles or multi-PC materials through a densification process, such as grinding, milling or pelletizing of the articles or materials. Then, the solid pellets, powder or flakes can be fed, for example, through a feed hopper to an extruder feed inlet. Additional solid ingredients, for example, an optional solid surfactant, an optional solid compatibilizer or other desired optional solid materials can also be added with the pellets, powder or flakes at the extruder feed inlet or near the extruder feed inlet through a separate extruder inlet.For example, the other solid ingredients can be blended or combined with the solid pellets, powder, or flakes, and the combined materials can be added to the extruder feed inlet; or the other solid ingredients can be added to the extruder separately from the solid pellets, powder, or flakes through a separate extruder inlet.
[0072] In some embodiments, the multi-PC thermoplastic articles or materials are melted to form a multi-PC melt in the first portion (melting zone) of the extruder; and the aqueous solution and any other desired ingredients may be simultaneously fed substantially into the extruder to come into contact with the multi-PC melt. Alternatively, a multi-PC melt may first be prepared separately, and the other desired ingredients may be fed into the extruder to come into contact with the multi-PC melt before or after the multi-PC melt is formed. In another embodiment, for example, at least two extruders may be used to perform the process, including a first extruder and a second extruder. For example, the multi-PC melt may be formed in the first extruder; and then the multi-PC melt may be fed into another different second extruder coupled to the first extruder.The aqueous solution and any other desired ingredients can be fed substantially simultaneously, or separately, to the second extruder with the melting of multiple PCs. The melting of multiple PCs (with... Petition 870260101801, dated 02 / 10 / 2026, page 36 / 102 27 / 40 any other desired ingredients that have been added) can then be applied to a shear zone and an extraction zone of, for example, the second extruder, when two extruders are used; or to the shear zone and portions of the extraction zone of a single extruder.
[0073] The temperature setting for the first portion (melting zone) of the extruder (or for a previous feed from the first extruder into the shear and extraction zone of a second extruder) is sufficient to convert the densified thermoplastic articles or materials of multiple PCs into a melt. For example, the temperature may be at least 105 °C, or at least 110 °C, or at least 130 °C, or at least 150 °C, or at least 160 °C to 300 °C, or up to 280 °C, or up to 250 °C, or up to 240 °C, or up to 230 °C, or up to 220 °C, or up to 210 °C, or up to 200 °C.
[0074] The temperature setting in the shear and extraction zone may be equal to the first portion of the extruder or it may be lower, but still above the melting temperature. For a small-scale extruder, the temperature may be substantially the same across the initial portion of the extruder and the shear / extraction zones. The temperature profile of the extruder system may include any number of heating zones to heat the feed material at the start of the extruder and any number of cooling zones to cool the feed material after the shear and extraction zones. For example, one or more initial zones may be at a temperature of 25 °C to 100 °C, increasing in increments until reaching the desired melting and / or shear temperature and extraction temperature. Similarly, optional cooling zones may be from about 100 °C to 25 °C in increments as desired.The sheared mixture can be further diluted with additional water or other ingredients added through optional extruder inlets from optional reservoirs in an optional end zone after the extruder zone for cooling and / or dilution.
[0075] In some embodiments, the pressure applied to the MAS mixture during the shearing stage (in the extruder shear zone) may be at least 15 psig (1,034 bar), or at least 20 psig (1,378 bar), or at least 50 Petition 870260101801, dated 02 / 10 / 2026, p. 37 / 102 28 / 40 psig (3,447 bar), or at least 80 psig (5,515 bar), or at least 100 psig (6,894 bar), or at least 150 psig (10,342 bar), or at least 200 psig (13,789 bar) up to 1,000 psig (68,947 bar), or up to 600 psig (41,368 bar), or up to 500 psig (34,473 bar), or up to 450 psig (31,0264 bar), or up to 400 psig (27,5790 bar), or up to 350 psig (24,131 bar) or up to 300 psig (20,684 bar). Alternatively, the pressure may be at least 100 kPa, or at least 150 kPa, or at least 200 kPa, or at least 500 kPa, or at least 1,000 kPa up to 7 MPa, or up to 4 MPa, or up to 3.5 MPa, or up to 3 MPa.
[0076] In other embodiments, additional ingredient(s) in liquid or solid form may be added to the extruder from one or more reservoirs through one or more extruder inlets via one or more feed hoppers or pumps. Although the extruder inlet may be at the beginning of the shear and extraction zone, optionally, for example, the aqueous solution may be added from a reservoir stream from the shear and extraction zones in a portion of the extruder after the multi-PC thermoplastic articles or materials have been melted to form the multi-PC melt. In other embodiments, the liquid ingredients of the aqueous solution and any desired optional components, such as an optional compatibilizer, optional cleaning agent, optional base, may also be supplied from separate reserve reservoirs via separate pumps. Any suitable pump may be used.For example, a pump that provides a flow of approximately 150 cubic centimeters per minute (cm3 / min) at a pressure of 240 bar (24 MPa) can be used to supply the ingredients to the extruder. As another example, a liquid injection pump provides a flow of 300 cm3 / min at 200 bar (20 MPa) or 600 cm3 / min at 133 bar (13.3 MPa). In another embodiment, the liquid ingredients can optionally be preheated in a preheater.
[0077] In general, to maintain pressure in the shear and extraction zone, there would be no extruder ventilation. However, in a system with two extruders in series - one extruder to convert the articles or materials Petition 870260101801, dated 02 / 10 / 2026, page 38 / 102 29 / 40 thermoplastics of multiple PCs in a melt and a second extruder to shear the MAS blend combination (i.e., the melt of multiple PCs and the aqueous solution; and any optional components) - or in a long extruder system, venting may be present in the portion of the system where the thermoplastic polymer blend resin is being converted into a melt. Additionally, in a long system, venting may be present towards the end of the final zone for cooling - for example, to dehydrate the blend to some extent.
[0078] After the shearing stage of the process and the formation of dispersion, particles or filaments in the MAS mixture, a separation stage is used in the process to separate the dispersion, particles or filaments of at least one first polymer component that has a first concentration of enriched polymer component, from the other components in the MAS mixture including, for example, water, at least one dispersing agent, at least one second polymer component, any remaining thermoplastic polymer resin components and / or any remaining optional components. For example, the polymer dispersion (e.g., PE), particles or filaments are physically separated from the MAS mixture. In a preferred embodiment, the separation stage can be carried out through a conventional process such as a flotation process, a centrifugal separation process, a filtration process or a flocculation process.
[0079] The first polymer component of the multi-PC melt formed after shearing the MAS mixture, namely, the enriched first polymer component stream formed and present in the MAS mixture after shearing, can be separated from the other components present in the MAS mixture; and subsequently, the enriched polymer component stream can be collected / recovered. The other components present in the MAS mixture may include, for example, water, the second polymer component, and other remaining resin components. Methods for separating and collecting the desired enriched polymer component stream include, Petition 870260101801, dated 02 / 10 / 2026, page 39 / 102 30 / 40 for example: (1) a process that first allows the desired enriched polymer component stream to float to the top of the MAS mixture, the desired enriched polymer component stream generally being a solid material in the form of large particles, and then collecting the material by removing the top layer of material from the top of the MAS mixture or filtering the top layer of material from the MAS mixture; (2) a process in which the material is first elongated to collect small particles of material and then agglomerating the small particles to form larger particles (agglomerations) that can be collected using a filtration process; (3) a centrifugation process to separate the material through centrifugal forces, either continuously or in batches; and / or (4) an extrusion process to separate the material in an extruder by diverting water or other liquids from the material in the extruder.The separated enriched polymer component stream (e.g., the first polymer component stream having a first enriched polymer concentration) can be dried to form a powder or can be processed through a pelletizer to form a plurality of pellets. The powder can be further sieved to remove larger or smaller sized contaminants.
[0080] In general, the separation step in some embodiments, to separate the dispersion, particles, or filaments of at least one first polymer component that has a first concentration of enriched polymer component, from the other components in the MAS mixture, can be carried out with a short period such as < 20 min in one general embodiment; < 10 min in another embodiment; and < 6 min in yet another embodiment. In other embodiments, the separation step can be carried out during a period of 1 min to 30 min in one general embodiment; from 2 min to 12 min in another embodiment; and from 4 to 5 min in yet another embodiment.
[0081] The process includes a step to recover dispersions, particles or filaments separated from at least one primary polymer component that Petition 870260101801, dated 02 / 10 / 2026, page 40 / 102 31 / 40 has an initial concentration of enriched polymer component formed in the shearing step of the process and separated in the separation step of the process. For example, in one embodiment, the resulting dispersion, particles, or separated filaments formed in the process are subjected to a drying step to remove any extraneous water present in the dispersion, particles, or filaments; and to facilitate further processing of the dried dispersion, particles, or filaments, such as subjecting the dried particles or filaments to a recycling process.
[0082] In some embodiments, the process may include one or more additional processing steps, such as step (h), subjecting the recovered stream from step (g) to drying; pelleting; devolatilization extrusion; steam removal; joint removal; recycling; or combinations thereof.
[0083] One of the advantages of the process of the present invention described above is that the process steps can be carried out by various conventional processes and equipment known in the art. Furthermore, another advantage of the process is that a delamination process or delamination step is not necessary before carrying out the separation step using the process. Therefore, the process is less complicated than a delamination process or dissolution process.
[0084] Some of the other advantages of the separation / recovery process include, for example: (1) the process allows the enrichment of a desired single-polymer component stream; (2) the process allows the separation of the desired enriched single-polymer component stream from other components remaining in the melt; (3) the desired enriched single-polymer component stream can be passed through further processing functions; (4) the desired enriched single-polymer component stream can be recycled; (5) the process provides optional additional formulation steps, such as blending the desired separated single-polymer component stream with other components, including, for example, virgin resin, odor scavenger additives, antioxidants, UV stabilizers, Petition 870260101801, dated 02 / 10 / 2026, page 41 / 102 32 / 40 inorganic fillers, slip agents, antiblocking agents and the like; (6) the aqueous liquid solution mixture used in the process to treat the melting of multiple PCs is a water-based (i.e., solvent-free) formulation as opposed to a solvent-based formulation; and the water-based formulation of the process beneficially reduces environmental impact issues; and (7) the process provides the option of using a continuous extruder-based process which has the advantage of allowing separation on a shorter timescale (e.g., from 1 minute to < 1 hour [h]) compared with other types of processes such as batch diffusion-based processes which may take, for example, up to several hours (e.g., 1 hour to 15 hours) to allow separation.
[0085] The first separated polymer component, collected and recovered from the melting of multiple PCs in the form of a dispersion, particles or filaments of the first polymer component formed during the shearing step of the process and recovered in the recovery step of the process comprises a first polymer component stream that is enriched in the desired first polymer component and recovered for further processing, such as processing the first polymer component through a recycling process. By enriched, enriching or enriching, it is understood that the concentration of at least one first polymer component is increased from a first-level concentration to a second-level concentration greater than the first-level concentration.For example, the concentration of at least one first polymer component of a multi-PC melt, before the multi-PC melt is passed through the process, is at a first level; and then the first-level concentration increases to a second-level concentration after the multi-PC melt has passed through the process.
[0086] In general, the first polymer component that has not been processed as described in this document to produce the first polymer component stream in the form of a dispersion, particles or filaments of the multi-PC thermoplastic polymer blend is enriched in the amount of at least 1% by weight in one embodiment and at least Petition 870260101801, dated 02 / 10 / 2026, page 42 / 102 33 / 40 10% by weight in another embodiment. In other embodiments, the stream of the first enriched polymer component can be enriched from 50% by weight to 100% in one embodiment, from 90% by weight to 99% by weight in another embodiment, and from 50% by weight to 90% by weight in yet another embodiment.
[0087] In some embodiments, the average particle size of the first enriched polymer component collected, if collected from dispersion or particles, may be at least 0.1 µm, at least 1 µm, at least 5 µm, or at least 10 µm. The average particle size may be up to 600 µm, up to 400 µm, up to 200 µm, or up to 150 µm. The particle size may be measured using standard particle size measuring instruments such as a Beckman Coulter particle size analyzer. If filaments of the first enriched polymer component are collected, the filament size may be readily measured by other conventional size measuring equipment known to those skilled in the art to measure the length (L) and diameter (D) of the filaments as an L / D ratio.
[0088] In some embodiments, after the recovery step (g) of the process, the dispersion, particles or separated filaments recovered from at least one first polymer component stream that has a first concentration of enriched polymer component from step (f), may optionally be formulated or mixed with one or more components selected from the group consisting of virgin resin, odor-scavenging additives, antioxidants, UV stabilizers, inorganic fillers and combinations thereof.
[0089] In some embodiments, after the recovery step (g) of the process, the process may optionally include an additional processing step (h). For example, the recovered stream from step (g) may be subjected to one or more additional steps, including drying; pelletizing; devolatilization extrusion; steam removal; joint removal; recycling; or combinations thereof. In a preferred embodiment, the Petition 870260101801, dated 02 / 10 / 2026, p. 43 / 102 34 / 40 The first stream of enriched polymer component in the form of a dispersion, particles or filaments from the multi-PC melt described above, after being separated and recovered from the second non-enriched polymer from the multi-PC melt, is passed to a recycling system and beneficially subjected to a recycling process. For example, the dispersion, particles or filaments of the desired separated polymer component stream collected and recovered in step (g) of the process above can be fed to the recycling system to form a recycle material (recycler) from the dispersion, particles or filaments. Then, the recycled material produced from the dispersion, particles or filaments can be used to manufacture another new article different from the recycled material, i.e., the recycled material.For example, a multilayer package, film, or article produced from layers of different thermoplastic polymers can be processed using this process; and then, the dispersion, particles, or filaments produced according to the process can be used to manufacture a new package, film, or different article that may include new single-layer or multilayer products. In general, the processes for reusing or recycling the dispersion, particles, or filaments are conventional processes known to those skilled in the art of recycling. The above recycling process is useful and desirable for reducing the amount of plastic waste for the benefit of protecting the environment. Examples
[0090] The following inventive examples (Ex. Inv.) and comparative examples (Ex. Comp.) (collectively, the Examples) are presented in the present invention to further illustrate the features of the present invention, but are not intended to be interpreted, either explicitly or by implication, as limiting the scope of the claims. Inventive Examples are identified by Arabic numerals and Comparative Examples are represented by letters of the alphabet. The following experiments analyze the performance of the composition embodiments described in this document. Unless stated otherwise, all parts and percentages are in Petition 870260101801, dated 02 / 10 / 2026, page 44 / 102 35 / 40 weight on a total weight basis.
[0091] The raw materials used in the Examples are identified in Table I. Table I - Raw materials Ingredient Brief description Supplier DOWLEX™ 2035G Linear Low-Density Polyethylene (LDPE) Resin The Dow Chemical Company (Dow) DOW™ dmda8940-NT-7 High-Density Polyethylene (HDPE) Resin Dow dow™ dmda8907-NT-7 High-Density Polyethylene (HDPE) Resin Dow Braskem PP 6D43 Random Copolymer of Polypropylene (PP) Braskem ENGAGE™ 8411 Polyolefin Elastomer Dow Silver Duralar Metallized Polyester Film Grafix PRIMACOR™ 5980i Ethylene Acrylic Acid Copolymer Dispersing Agent SK Pluronic F-108 Ethylene Oxide-Propylene Oxide (EO-PO) Copolymer Dispersing Agent BASF Licocene 431 Anhydride Grafted Polyethylene (PE) Wax Compatibilizer maleic (MAH) Clariant
[0092] The following polymers and polymer blends are used in Examples: (1) A packaging material marked as PA / PE used for packaging pet food: a 5-layer PE / PA film consisting of 25.8% LDPE, 60% LLDPE, a 7.8% PA and a 6.4% LLDPE bonding layer; (2) A containment bag packaging material marked PET / PE: a PET PE film structure including, for example, 23.7% LDPE, 55.3% LLDPE and 21% PET; (3) A metallized polyester m-PET / PE, including, for example, 90% DOWLEX™ 2035G and 10% Silver Dura-Lar; (4) a 50 / 50 blend of, for example, HDPE DMDA-8940-NT-7; and HDPE DMDA-8907-NT-7 identified as HDPE 8940 and HDPE 8907, respectively; (5) A 50 / 50 mixture of Braskem PP 6D43 identified as PP; and HDPE DMDA 8940-NT-7 identified as HDPE 8940 and (6) a 50 / 50 mixture of Engage 8411 and HDPE DMDA 8940NT-7 identified as HDPE 8940.
[0093] The blends are compounded in a twin-screw extruder in Petition 870260101801, dated 02 / 10 / 2026, page 45 / 102 36 / 40 pellets using standard processing techniques prior to feeding in the disclosed shearing process.
[0094] The following materials are used in the Examples: (1) PRIMACOR™ 5980i (ethylene acrylic acid copolymer, 20% by weight comonomer, density = 0.958 g / cm3, melt flow index = 300 g / 10 min, melting point = 77.2 °C from SK Global); and (2) Pluronic™ F-108 (ethylene oxide / propylene oxide copolymer, melting point 60 °C, number average molecular weight (Mn) = 14,600, from BASF).
[0095] A base is also used in the Examples and can generally be any base material. For example, in the Examples, a potassium hydroxide base (30% in water) is used.
[0096] A compatibilizer is used in the Examples and can generally be any compatibilizing material. For example, in the Examples, a compatibilizer, Licocene 431 (commercially available from Clariant), is used. General Procedure for Conducting Tests
[0097] The completed tests for the Examples are performed on a 25 millimeter (mm) twin-screw extruder with 12 Berstorff zones. The multi-PC composition feed is supplied to the system as a pellet or flake via a large Schenk feeder that drops into the feed throat. Other solids, such as the dispersing agent or optional additives, are supplied as a pellet or powder using a KQX K-tron feeder that also drops into the extruder's feed throat. Water or other liquid components are supplied via an ISCO 500D pump through an injector. Additional water is supplied to the extruder via a large Hydracell pump through an injector further down the extruder.
[0098] The resulting composition of the polymer dispersions (Dispersion Numbers 1 to 5, abbreviated as Disp. 1 - 5, which constitute the inventive examples contained herein; and Comparative Dispersions A and B, abbreviated as Comp. Disp. A - B) used in the Examples are described in Table II. The energy Petition 870260101801, dated 02 / 10 / 2026, p. 46 / 102 37 / 40 specific mechanical energy was between 0.09 kWh / kg and 0.17 kWh / kg for dispersion examples. General Measurement Procedure
[0099] The Δη ratio and Tm values of the starting material and the enriched polymeric material are measured using a Q100 DSC (a differential scanning calorimeter, available from TA Instruments, Inc., Newcastle, DE, USA). Measurement conditions are -90 °C to 250 °C at a heating rate of 10 degrees Celsius per minute (°C / min) and after running for 2 cycles. Results are reported from the second cycle onwards. General Procedures for Separation Methods
[0100] The separation methods used in the Examples to separate the dispersion, particles or filaments formed after shearing include, for example, (1) a flotation method or (2) a filtration method described below: (1) Float Method
[0101] For the flotation method, the resulting material exiting the extruder is collected in a reservoir and then allowed to cool and settle for 24 hours in the reservoir. During the cooling period, particles float to the top of the container and reposition themselves on the surface of the material. The particles that float to the top of the material are collected using a scoop. Then, the collected material is washed with water in a Buchner funnel using vacuum filtration. The washed material is then allowed to air dry for 24 hours before further characterization of the dried material. (2) Filtration Method
[0102] For the filtration method, the resulting material exiting the extruder is first collected in a reservoir. Then, the material is mixed; and the mixture is deposited through a mesh filter bag (800 µm mesh size) to isolate the dispersion or small particles from large polymer filaments. The large polymer filaments remain in the filter bag. The Petition 870260101801, dated 02 / 10 / 2026, page 47 / 102 38 / 40 of the remaining material in the filter bag is left to air dry for 72 hours before further characterization of the dried material.
[0103] As previously mentioned, Table II describes the dispersion process used for the various polymer blends. The resulting material, i.e., the dispersion, particles or filaments, exiting the extruder is separated and recovered; and then the properties of the resulting material are measured.
[0104] Table III describes the enriched PE characterization of the dispersion samples prepared in the Examples. Petition 870260101801, dated 02 / 10 / 2026, page 48 / 102 39 / 40 Table II - Dispersion Process for Polymer Blends Example No. Disp. No. Resin Rate (grams per minute [g / min]) Ex. 1 Rate (g / min) Ex. 2 Rate (g / min) Ex. 3 Rate (g / min) Base (30% KOH) (milliliters per minute [ml / min]) Water (%) Water Rate (ml / min) Dilution Water Rate (ml / min) Temp. (°C) Enriched Polymer Form Factor Ex. Inv. 1 Disp. 1 PET / PE 52.97 Primacor 5980i 15.13 7.32 25 19.6 91 190 Large Particles (LP) Ex. Inv. 2 Disp. 2 PA / PE 52.97 Primacor 5980i 15.13 7.32 25 19.6 90 190 LP Ex. Inv. 3 Disp. 3 mPET / PE 60.536 Primacor 5980i 15.134 10.98 25 19.6 105 190 LP Ex. Inv. 4 Disp. 4 HDPE 8940 26.485 PP 26.485 Primacor 5980i 22.7 10.98 15 4.25 105 160 Dispersion Ex. Inv. 5 Disp. 5 HDPE 8940 30.27 PP 30.27 Pluroni c F108 7.57 Licoce ne 431 7.57 1.06 15 12.47 90 160 Dispersion Ex. Comp. A Ex. Disp. A HDPE 8940 30.27 HDPE 8907 30.27 Primacor 5980i 15.13 10.98 15 4.25 105 160 Dispersion (0.6 pm) Ex. Comp. B Ex. Disp. B HDPE 8940 30.27 ENGA GE 8411 30.27 Primacor 5980i 15.13 10.98 15 4.25 105 160 Dispersion (0.8 pm) 39 / 40 Petition 870260101801, dated 02 / 10 / 2026, page 49 / 102 40 / 40 Table III - Characterization of Enriched PE Example No. Dispersion No. Separation Method DSC Area of PE (Starting Material) Δη (%) DSC Area of PE (after separation) ΔH (%) Melting Temperature (Tm) 1st Tm (°C) 2nd Tm (°C) Ex. Inv. 1 Disp. 1 Float 91.5 98.2 116 246 Ex. Inv. 2 Disp. 2 Float 96.3 99.3 118 191 Ex. Inv. 3 Disp. 3 Float 92.4 98.5 124 240 Ex. Inv. 4 Disp. 4 Filtration 74.0 99.0 128 141 Ex. Inv. 5 Disp. 5 Filtration 74.0 98.5 128 141 Ex. Comp. A Ex. Disp. A Dispersion (Without separation) 100.0 100.0 130 Ex. Comp. B Ex. Disp. B Dispersion (Without Separation) 100.0 100.0 123
[0105] The key results from the data in the Examples above are the two observed melting temperature peaks, and the increase in the DSC δη area showing the enrichment. Petition 870260101801, dated 02 / 10 / 2026, pp. 50 / 102
Claims
1 / 3 CLAIMS 1. A process for separating and recovering at least one polymer component from a melt of multiple polymer components, characterized in that it comprises the steps of: (a) providing a multi-component thermoplastic article having at least one first polymer component and at least one second polymer component; (b) melting the multi-component thermoplastic article to form a multi-component thermoplastic article melt; wherein the melt comprises at least one first polymer component melt stream and at least one second polymer component melt stream; wherein the multi-component melt has at least two melt temperatures, at least two glass transition temperatures, or combinations thereof;(c) provide a pressurized aqueous solution comprising an aqueous liquid mixture of: (i) water, and (ii) at least one slip agent; (d) add the melt from step (b) to the pressurized aqueous solution from step (c); (e) shear the melt of multiple polymer components from step (b) in the presence of the pressurized aqueous solution from step (c); wherein the shearing of the melt of multiple polymer components in contact with the pressurized aqueous solution forms a dispersion, particles or filaments of at least one stream of the first polymer component having an enriched first polymer component concentration;(f) after shearing in step (e), separate the dispersion, particles or filaments from at least one first stream of polymer components having a first concentration of water-enriched polymer component, at least one dispersing agent, at least one second polymer component and any remaining components in the mixture of multi-polymer component melt and pressurized aqueous solution; Petition 870260101801, 10 / 02 / 2026, p. 51 / 102 2 / 3 and (g) recover the dispersion, particles or filaments separated from step (f).; 2. Process according to claim 1, characterized in that the pressurized aqueous solution comprises from 50 percent by weight to 99.9 percent by weight of the water of component (i) and from 0.5 percent by weight to 35 percent by weight of the dispersing agent of component (ii) based on the total weight of the components in the pressurized aqueous solution.
3. Process according to claim 1, characterized in that the first polymer component of the melt is selected from the group consisting of polyolefins; acrylics; polystyrene; styrene copolymers; polyamides; thermoplastic urethane; thermoplastic silicones; and combinations thereof.
4. Process according to claim 1, characterized in that the first polymer component of the melt is a polyolefin; and wherein the polyolefin component has a density less than 1, a melting index of 0.5 grams per 10 minutes to 80 grams per 10 minutes and a melting temperature of 60 °C to 150 °C.
5. Process according to claim 1, characterized in that the pressure during the shearing step (e) is sufficient to maintain the aqueous liquid solution in the liquid phase at the working temperature or to maintain the water present in the aqueous liquid mixture below the boiling point of water at the process temperature during the shearing step (e).
6. Process according to claim 1, characterized in that the shearing of step (e) occurs in at least one extruder.
7. Process according to claim 1, characterized in that the specific mechanical energy imparted during the shearing of step (e) is at least 0.01 kilowatt-hour per kilogram.
8. Process according to claim 1, characterized in that the pressurized aqueous solution of step (c) includes one or more components selected from the group consisting of a second dispersing agent, a dispersing agent, a compatibilizer, a cleaning agent, a neutralizing agent and mixtures thereof.
9. Process according to claim 1, characterized in that the shearing step (e) is a batch process or a continuous process. Petition 870260101801, dated 02 / 10 / 2026, p. 53 / 102