Dewatering method in production process of vulcanization promoter CZ
A rubber vulcanization and production process technology, applied in the field of rubber vulcanization accelerator CZ production, can solve the problems of affecting production efficiency, large energy consumption, and large amount of washing water, so as to reduce the amount of washing water, increase the filtration rate, and reduce the oil phase The effect of content
Patent Information
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Publication Date
- 2013-02-13
- Estimated Expiration
- Not applicable · inactive patent
Smart Images
Figure 1 Figure 2
Abstract
Description
technical field
[0001] The invention relates to the technical field of production of rubber vulcanization accelerator CZ, in particular to a dehydration method in the production process of rubber vulcanization accelerator CZ. Background technique
[0002] Rubber vulcanization accelerator CZ, scientific name N-cyclohexyl-2-benzothiazole sulfenamide. It is a post-effect rubber vulcanization accelerator, which has the characteristics of long scorch time and fast vulcanization speed, and is widely used in various rubber processing industries. When the vulcanization temperature is above 138°C, the accelerating effect is very strong, and it is often used as the second accelerator in combination with accelerator TMTD, accelerator D or other basic accelerators. The synthesis method of CZ is industrially mostly adopted four methods of sodium hypochlorite oxidation method, hydrogen peroxide oxidation method, non-oxidant synthesis method, and oxygen oxidation method. At present, the ...
Examples
Embodiment 1
[0014] like figure 2 In the technical route shown, non-ionic surfactant sorbitan monooleate (span80) is added to the CZ suspension containing rubber vulcanization accelerator, and the addition amount is 0.75% of the solid phase mass in the CZ suspension. Stir evenly to fully mix the accelerator CZ suspension with the surfactant, and then use vacuum filtration to dehydrate once. The water content of the accelerator CZ filter cake is relatively lower than that of the CZ suspension without surfactant. 11.36% (wt).
Embodiment 2
[0016] like figure 2 In the technical route shown, the non-ionic surfactant span80 is added to the rubber vulcanization accelerator CZ suspension, and the addition amount is 0.5% of the solid phase mass in the CZ suspension. Stir evenly to fully mix the accelerator CZ suspension with the surfactant, and then use vacuum filtration to dehydrate once. The water content of the accelerator CZ filter cake is relatively lower than that of the CZ suspension without surfactant. 8.3% (wt).
Embodiment 3
[0018] like figure 2 In the technical route shown, the non-ionic surfactant span80 is added to the rubber vulcanization accelerator CZ suspension, and the addition amount is 0.25% of the solid phase mass in the CZ suspension. Stir evenly to fully mix the accelerator CZ suspension with the surfactant, and then dehydrate once by vacuum filtration. The water content of the accelerator CZ filter cake is relative to the water content of the filter cake when the CZ suspension without surfactant is filtered. decreased by 7.86% (wt).