A grid-type hollow press quenching die
By designing a grid-type hollow press quenching die, and employing a pressure sensor and a multi-pipe cooling system, the problems of deformation and insufficient cooling performance of the press quenching die during workpiece press quenching are solved, achieving precise positioning and efficient cooling, and meeting the design requirements of the workpiece.
Patent Information
- Application Number
- CN201711403274.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2017-12-22
- Publication Date
- 2024-11-12
- Estimated Expiration
- 2037-12-22
AI Technical Summary
Existing pressure quenching dies are prone to deformation during workpiece pressure quenching, and their cooling performance and accuracy are not high, failing to meet design requirements.
A grid-type hollowed-out pressure quenching mold was designed. The pressure is detected by a pressure sensor, the grid-type hollowed-out plate increases the contact area, and rapid quenching is achieved through a multi-pipe cooling system. The contact area is adjusted by an adjustment device to achieve precise positioning and efficient cooling.
It achieves precise control of the pressing force, improves the accuracy and cooling performance of the mold, and ensures that the workpiece does not deform during the pressing and quenching process, thus meeting the design requirements.
Smart Images

Figure CN107937680B_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of hollow press quenching dies, and in particular to a grid type hollow press quenching die. Background Art
[0002] At present, automobile parts generally need to be press-quenched during production to improve their hardness. Traditional press-quenching dies are prone to cause deformation of the workpiece during press-quenching, which fails to meet the design requirements and affects the performance of the product.
[0003] After searching, the Chinese patent application number CN 103555898 A discloses a high-grade cone quenching die, including a die core and a die base, the outer diameter of the die core corresponds to the inner diameter of the workpiece, the outer ring of the die core and the upper plane of the die base are perpendicular to each other, the upper part of the workpiece is sleeved on the die core, and the bottom of the workpiece is located on the upper plane of the die base. There are a number of upper positioning holes evenly distributed on the die core, and a number of lower positioning holes evenly distributed on the die base, and the upper positioning holes correspond to the lower positioning holes. The above patent has the following shortcomings: poor cooling performance and low precision, therefore, a grid-type hollow quenching die is urgently needed. Summary of the invention
[0004] The purpose of the present invention is to solve the problems of poor cooling performance and low precision in the prior art, and to propose a grid-type hollow press quenching die.
[0005] In order to achieve the above object, the present invention adopts the following technical solutions:
[0006] A grid-type hollow quenching die comprises a base, a lower die seat is fixed to the top of the base by bolts, and a mounting hole is opened on the top of the lower die seat, an expansion shaft is placed in the mounting hole, and the outer diameter of the expansion shaft is smaller than the inner diameter of the mounting hole, a fixing tube is welded to the bottom of the expansion shaft, and the bottom end of the fixing tube is welded to the base, four detection devices are arranged on the top of the base, and the four detection devices are distributed on the base in a ring shape, the detection device comprises a fixing block, a pressure sensor is fixed to the top outer wall of the fixing block by bolts, and a protective plate is welded to the top of the pressure sensor, the tops of the four protective plates are welded to the same fixing plate, and the edges of the fixing plate are connected to the expansion A gap is left between the shafts, a grid-type hollow plate is welded on the outer wall of the expansion shaft, an upper die seat is fixed to the top of the lower die seat by bolts, the cross-section of the upper die seat is a trapezoidal structure, the lower die seat, the upper die seat and the grid-type hollow plate form an oil chamber, a first through hole is opened on one side of the outer wall of the lower die seat, and one end of the first through hole is connected to the oil chamber, a second through hole is opened on one side of the outer wall of the lower die seat, and a second oil inlet pipe is inserted in the second through hole, a clamping block is placed on the top of the upper die seat, a handle is welded on the top of the clamping block, a mold core is welded at the center of the bottom outer wall of the clamping block, and an adjusting device with equal distance distribution is welded on the outer wall of the mold core;
[0007] Preferably, a first oil inlet pipe is inserted into the first through hole, and the first oil inlet pipe is connected to the oil chamber, and a second connector is welded on a side of the first oil inlet pipe away from the oil chamber;
[0008] Preferably, one end of the second oil inlet pipe is connected to the second connector, and one end of the second oil inlet pipe away from the second connector is connected to the bottom of the expansion shaft;
[0009] Preferably, a third through hole is opened on the outer wall of one side of the lower mold base, and an oil outlet pipe is inserted into the third through hole, one end of the oil outlet pipe is connected to the oil chamber, and a first connector is welded to the end of the oil outlet pipe away from the oil chamber, and the first connector and the second connector are both located on the outer wall of the lower mold base.
[0010] Preferably, the protection plate is an arc-shaped structure, and the width of the protection plate is greater than the diameter of the pressure sensor.
[0011] Preferably, four positioning holes are opened on the top of the fixing plate, and the four positioning holes are distributed in a ring shape on the fixing plate.
[0012] Preferably, the adjustment device comprises an adjustment block, and an adjustment hole is opened on the outer wall of the adjustment block away from the mold core, a first spring is welded on the inner wall of the adjustment hole, and a first adjustment plate is welded on the end of the first spring away from the mold core.
[0013] Preferably, the bottom end of the first adjustment plate is welded with second springs distributed at equal distances, and the bottom end of the second spring is welded with a second adjustment plate, and the diameter of the second adjustment plate is smaller than that of the first adjustment plate.
[0014] Compared with the prior art, the present invention provides a grid-type hollow press quenching die, which has the following beneficial effects:
[0015] 1. The grid-type hollow press-quenching mold can detect the pressure applied to the fixed plate during the press-molding process through the pressure sensor, so as to accurately control the force. The positioning holes can also accurately position the mold, thus improving the accuracy of the device.
[0016] 2. The grid-type hollow press-quenching mold can quickly quench the mold by means of the first oil inlet pipe, the second oil inlet pipe and the grid-type hollow plate, and the grid-type hollow plate can increase the contact area between the mold and the oil, thereby improving the quenching effect and the cooling performance of the device.
[0017] 3. The grid-type hollow quenching mold can adjust the contact area between the device and the bottom through the first adjustment plate, the second adjustment plate and the first spring, and the adjustment is convenient, practical and novel.
[0018] The parts not involved in the device are the same as the existing technology or can be implemented by using the existing technology. The present invention has a simple structure and is easy to operate. It can detect the pressure exerted on the fixed plate during die pressing so as to accurately control the force. The positioning hole can also accurately position the mold, thereby improving the accuracy of the device and enhancing the cooling performance. BRIEF DESCRIPTION OF THE DRAWINGS
[0019] Figure 1 This is a schematic cross-sectional view of a grid-type hollow press-quenching die proposed by the present invention;
[0020] Figure 2 This is a schematic structural diagram of a grid-type hollow press-quenching die fixing plate proposed by the present invention.
[0021] In the figure: 1 base, 2 lower die base, 3 expansion shaft, 4 detection device, 5 fixed plate, 6 fixed block, 7 pressure sensor, 8 protection plate, 9 first connector, 10 oil outlet pipe, 11 second oil inlet pipe, 12 oil chamber, 13 grid-type hollow plate, 14 second connector, 15 first oil inlet pipe, 16 upper die base, 17 clamping block, 18 core, 19 adjustment block, 20 first adjustment plate, 21 second spring, 22 second adjustment plate, 23 positioning hole. DETAILED DESCRIPTION
[0022] The technical solutions in the embodiments of the present invention will be described clearly and completely below in conjunction with the drawings in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, rather than all the embodiments.
[0023] In the description of the present invention, it is necessary to understand that the terms "upper", "lower", "front", "back", "left", "right", "top", "bottom", "inside", "outside", etc., indicating the orientation or position relationship are based on the orientation or position relationship shown in the drawings, and are only for the convenience of describing the present invention and simplifying the description, rather than indicating or implying that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore cannot be understood as a limitation on the present invention.
[0024] Reference Figure 1-2 A grid-type hollow quenching die comprises a base 1, a lower die seat 2 is fixed to the top of the base 1 by bolts, and a mounting hole is opened on the top of the lower die seat 2, an expansion shaft 3 is placed in the mounting hole, and the outer diameter of the expansion shaft 3 is smaller than the inner diameter of the mounting hole, a fixing tube is welded to the bottom of the expansion shaft 3, and the bottom end of the fixing tube is welded to the base 1, four detection devices 4 are arranged on the top of the base 1, and the four detection devices 4 are distributed on the base 1 in a ring shape, the detection device 4 comprises a fixing block 6, a pressure sensor 7 is fixed to the outer wall of the top of the fixing block 6 by bolts, and is used to detect the pressure applied to the fixing plate during die pressing, so as to accurately control the force, and a protective plate 8 is welded to the top of the pressure sensor 7, and the tops of the four protective plates 8 are welded with the same fixing plate 5, and a gap is left between the edge of the fixing plate 5 and the expansion shaft 3, A grid-type hollow plate 13 is welded on the outer wall of the expansion shaft 3. The grid-type hollow plate 13 can increase the contact area between the mold and the oil, improve the quenching effect, and improve the cooling performance of the device. The top of the lower die base 2 is fixed with an upper die base 16 by bolts. The cross-section of the upper die base 16 is a trapezoidal structure. The lower die base 2, the upper die base 16 and the grid-type hollow plate 13 form an oil chamber 12. A first through hole is opened on the outer wall of one side of the lower die base 2, and one end of the first through hole is connected to the oil chamber 12. A second through hole is opened on the outer wall of one side of the lower die base 2, and a second oil inlet pipe 11 is inserted in the second through hole. A clamping block 17 is placed on the top of the upper die base 16, and a handle is welded on the top of the clamping block 17. A mold core 18 is welded at the center of the bottom outer wall of the clamping block 17, and an adjusting device with equal distance distribution is welded on the outer wall of the mold core 18.
[0025] In the present invention, the protection plate 8 is an arc-shaped structure, and the width of the protection plate 8 is greater than the diameter of the pressure sensor 7. Four positioning holes 23 are opened on the top of the fixed plate 5, and the four positioning holes 23 are distributed in a ring shape on the fixed plate 5. The first through hole is plugged with the first oil inlet pipe 15, and the first oil inlet pipe 15 is connected to the oil chamber 12. The side of the first oil inlet pipe 15 away from the oil chamber 12 is welded with a second connector 14, one end of the second oil inlet pipe 11 is connected to the second connector 14, and the end of the second oil inlet pipe 11 away from the second connector 14 is connected to the bottom of the expansion shaft 3, and a third through hole is opened on the outer wall of one side of the lower mold base 2, and the oil outlet pipe 1 is plugged into the third through hole. 0, one end of the oil outlet pipe 10 is connected to the oil chamber 12, and the end of the oil outlet pipe 10 away from the oil chamber 12 is welded with a first connector 9, the first connector 9 and the second connector 14 are both located on the outer wall of the lower die base 2, the adjusting device includes an adjusting block 19, and an adjusting hole is opened on the outer wall of the adjusting block 19 away from the mold core 18, a first spring is welded on the inner wall of the adjusting hole, a first adjusting plate 20 is welded on the end of the first spring away from the mold core 18, and second springs 21 distributed equidistantly are welded at the bottom end of the first adjusting plate 20, and a second adjusting plate 22 is welded at the bottom end of the second spring 21, and the diameter of the second adjusting plate 22 is smaller than the diameter of the first adjusting plate 20.
[0026] The above description is only a preferred specific implementation manner of the present invention, but the protection scope of the present invention is not limited thereto. Any technician familiar with the technical field can make equivalent replacements or changes according to the technical scheme and inventive concept of the present invention within the technical scope disclosed by the present invention, which should be covered by the protection scope of the present invention.
Claims
1. A grid-type hollow press quenching die, comprising a base (1), characterized in that: The top of the base (1) is fixed with a lower die base (2) by bolts, and a mounting hole is opened at the top of the lower die base (2), an expansion shaft (3) is placed in the mounting hole, and the outer diameter of the expansion shaft (3) is smaller than the inner diameter of the mounting hole, a fixing tube is welded at the bottom of the expansion shaft (3), and the bottom end of the fixing tube is welded to the base (1), four detection devices (4) are arranged at the top of the base (1), and the four detection devices (4) are distributed on the base (1) in a ring shape, the detection device (4) comprises a fixing block (6), a pressure sensor (7) is fixed to the outer wall of the top of the fixing block (6) by bolts, and a protective plate (8) is welded to the top of the pressure sensor (7), the tops of the four protective plates (8) are welded with the same fixing plate (5), and a gap is left between the edge of the fixing plate (5) and the expansion shaft (3), the expansion shaft ( 3) is welded with a grid-type hollow plate (13), the top of the lower die seat (2) is fixed with an upper die seat (16) by bolts, the cross section of the upper die seat (16) is a trapezoidal structure, the lower die seat (2), the upper die seat (16) and the grid-type hollow plate (13) form an oil chamber (12), a first through hole is opened on one side of the outer wall of the lower die seat (2), and one end of the first through hole is connected to the oil chamber (12), a second through hole is opened on one side of the outer wall of the lower die seat (2), and a second oil inlet pipe (11) is inserted into the second through hole, a clamping block (17) is placed on the top of the upper die seat (16), a handle is welded on the top of the clamping block (17), a mold core (18) is welded at the center of the bottom outer wall of the clamping block (17), and an adjustment device distributed at equal distances is welded on the outer wall of the mold core (18); A first oil inlet pipe (15) is inserted into the first through hole, and the first oil inlet pipe (15) is connected to the oil chamber (12); a second connector (14) is welded to a side of the first oil inlet pipe (15) away from the oil chamber (12); One end of the second oil inlet pipe (11) is connected to the second connector (14), and one end of the second oil inlet pipe (11) away from the second connector (14) is connected to the bottom of the expansion shaft (3); A third through hole is formed on one side outer wall of the lower die base (2), and an oil outlet pipe (10) is inserted into the third through hole. One end of the oil outlet pipe (10) is connected to the oil chamber (12), and a first connector (9) is welded to the end of the oil outlet pipe (10) away from the oil chamber (12). The first connector (9) and the second connector (14) are both located on the outer wall of the lower die base (2).
2. The grid-type hollow press quenching die according to claim 1, characterized in that: The protection plate (8) is an arc-shaped structure, and the width of the protection plate (8) is greater than the diameter of the pressure sensor (7).
3. The grid-type hollow press quenching die according to claim 1, characterized in that: Four positioning holes (23) are formed on the top of the fixing plate (5), and the four positioning holes (23) are distributed in a ring shape on the fixing plate (5).
4. The grid-type hollow press quenching die according to claim 1, characterized in that: The adjusting device comprises an adjusting block (19), wherein an adjusting hole is formed on an outer wall of the adjusting block (19) away from the mold core (18), a first spring is welded on an inner wall of the adjusting hole, and a first adjusting plate (20) is welded on an end of the first spring away from the mold core (18).
5. The grid-type hollow press quenching die according to claim 4, characterized in that: The bottom end of the first adjustment plate (20) is welded with second springs (21) distributed at equal distances, and the bottom end of the second spring (21) is welded with a second adjustment plate (22), and the diameter of the second adjustment plate (22) is smaller than the diameter of the first adjustment plate (20).