Cross-linked thermoplastic dielectrics for chip packaging

By using highly filled cross-linked thermoplastic materials as dielectric structures in chip packaging, the problems of insufficient electrical reliability and mechanical thermal stability of packaging in the existing technology are solved, higher electrical insulation and thermal conductivity are achieved, and extended improves the package life.

CN110277353BActive Publication Date: 2024-10-11INFINEON TECHNOLOGIES AG
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN201910186959.1
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Priority Date
2018-03-13
Filing Date
2019-03-13
Publication Date
2024-10-11
Estimated Expiration
2039-03-13

AI Technical Summary

Technical Problem

Existing chip packages have deficiencies in the electrical reliability and mechanical thermal stability of sealing materials and dielectric structures, especially in high-temperature and high-power applications, which are prone to damage to electrical and mechanical interfaces.

Method used

A highly filled cross-linked thermoplastic material is used as the dielectric structure. The mechanical and thermal stability of the material is improved through the cross-linking process, and its properties are adjusted by adding filler particles to make it an optically opaque electrical insulating material for chip packaging. Sealing and dielectric layers.

Benefits of technology

Significantly improves the electrical reliability and mechanical stability of the package, reduces humidity, enhances dielectric strength and thermal conductivity, prevents undesired optical interference and radiation effects, and extends the life of the package.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN110277353B_ABST
    Figure CN110277353B_ABST
Patent Text Reader

Abstract

A package (100) includes an electronic chip (108) and a dielectric structure (104) including a highly filled cross-linked thermoplastic material (106).
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to a package and a method of manufacturing a package. Background Art

[0002] Packages used, for example, in automotive applications provide physical enclosure for one or more electronic chips including one or more integrated circuit components. Examples of packaged integrated circuit components are field effect transistors, insulated gate bipolar transistors (IGBTs), diodes, and passive components (such as inductors, capacitors, resistors). Moreover, such packages can be used to produce system-level packages.

[0003] In order to produce the package, at least one electronic chip can be encapsulated by a suitable sealing material. For this purpose, a curable epoxy resin is used as a sealing material in many cases. The advantage of this is that it is appropriately processable and mechanically stable.

[0004] However, there is still potential room for improving package reliability, particularly with respect to the properties of the encapsulation material or another dielectric structure of the package. Summary of the invention

[0005] There is a need for chip packages that have suitable electrical reliability while being mechanically and thermally robust.

[0006] According to an exemplary embodiment, a package is provided, which comprises an electronic chip and a dielectric structure comprising a highly filled cross-linked thermoplastic material, in particular filled with filler particles.

[0007] According to another exemplary embodiment, a package is provided that includes a chip carrier, an electronic chip mounted on the chip carrier, and a dielectric structure covering at least a portion of at least one of the chip carrier and the electronic chip and including an optically opaque cross-linked thermoplastic material.

[0008] According to another exemplary embodiment, a method of manufacturing a package is provided, wherein the method includes mounting an electronic chip on a chip carrier and forming a dielectric structure covering at least part of at least one of the chip carrier and the electronic chip by cross-linking a highly filled thermoplastic material.

[0009] According to yet another exemplary embodiment, a method of manufacturing a package is provided, wherein the method comprises forming a dielectric structure covering at least a portion of an electronic chip (and / or a chip carrier on which the chip may be mounted) by cross-linking an opaque thermoplastic material.

[0010] According to an exemplary embodiment, a highly filled cross-linked thermoplastic material is used as a dielectric structure for chip encapsulation. This electrically insulating material, which can be used, for example, as a sealing material and / or a dielectric layer, synergistically combines many technical advantages. On the one hand, compared with conventional materials such as epoxy resins, thermoplastic materials allow the humidity in the dielectric material to be significantly reduced. At the same time, compared with conventional curable epoxy resins, the electrical insulation properties of this material can be significantly improved. This significantly improves the electrical reliability of the package, and in particular improves the dielectric strength of the package. By specifically and artificially triggering the cross-linking of this thermoplastic material (which itself does not occur in the thermoplastic material), the mechanical stability and thermal stability of the dielectric material can be improved. Descriptively speaking, the cross-linked chains of the thermoplastic material can allow the favorable properties of the thermosetting material to be combined in terms of mechanical stability and thermal stability, while improving electrical reliability and moisture resistance.

[0011] Very advantageously, such a dielectric structure can include, in addition to the crosslinked thermoplastic material, a large number of filler particles, which allow the properties of the dielectric structure to be specifically adapted to the chip encapsulation function. As a result, a highly filled crosslinked thermoplastic is provided as a dielectric structure for high-performance chip encapsulation applications.

[0012] Also advantageously, the dielectric structure comprising the cross-linked thermoplastic material can be opaque. It has been shown that for many electronic applications, in particular for power semiconductor applications, the propagation of considerable amounts of visible light into the interior of the package can induce undesirable reactions and effects there and can therefore interfere with the electronic function. By making the dielectric structure substantially optically opaque, the electrical reliability of the package and the operation of the package can be improved. In particular, making the dielectric structure substantially opaque can safely prevent the chip package from radiation-induced electronic malfunctions.

[0013] Description of Further Exemplary Embodiments

[0014] In the following, further exemplary embodiments of the package and the method will be explained.

[0015] In the context of the present application, the term "package" may particularly denote at least one partially or completely encapsulated and / or coated electronic chip having at least one direct or indirect external electrical contact.

[0016] In the context of the present application, the term "electronic chip" may particularly refer to a chip (more specifically a semiconductor chip) that provides an electronic function. An electronic chip may be an active electronic component. In one embodiment, the electronic chip is configured as a controller chip, a processor chip, a memory chip, a sensor chip, or a micro-electromechanical system (MEMS). In an alternative embodiment, the electronic chip may also be configured as a power semiconductor chip. Therefore, an electronic chip (e.g., a semiconductor chip) may be used for power applications in, for example, the automotive field, and may, for example, have at least one integrated insulated gate bipolar transistor (IGBT) and / or at least one transistor of another type (e.g., MOSFET, JFET, etc.) and / or at least one integrated diode. Such an integrated circuit element may, for example, be made in silicon technology or based on a wide bandgap semiconductor (e.g., silicon carbide, gallium nitride, or gallium nitride on silicon). A semiconductor power chip may include one or more field effect transistors, diodes, inverter circuits, half bridges, full bridges, drivers, logic circuits, other devices, etc. An electronic chip may be a bare die or may have been packaged or encapsulated.

[0017] In the context of the present application, the term "chip carrier" may particularly denote an at least partially electrically conductive structure which simultaneously serves as a mounting base for one or more electronic chips and also facilitates the electrical connection of the electronic chips to the electronic environment of the package. In other words, the chip carrier may fulfill both a mechanical support function and an electrical connection function. A preferred embodiment of the carrier is a lead frame.

[0018] In the context of the present application, the term "thermoplastic material" may particularly refer to a plastic material, in particular a polymer, which becomes molten, flowable or moldable above a certain temperature and solidifies when cooled. The polymer chains of thermoplastic materials are associated by intermolecular forces, which rapidly weaken as the temperature rises, thereby producing a viscous liquid, and / or are associated by mechanical entanglement of the individual polymer chains. Therefore, thermoplastics can be reshaped by heating and can be subjected to polymer processing techniques, such as injection molding or compression molding. Thermoplastics are different from thermosetting polymers (such as curable epoxy resins), which form irreversible chemical bonds during the curing process. Therefore, thermosetting plastics and thermoplastics have very different properties. The physical difference is that thermoplastics can be remelted into liquids, while thermosetting plastics remain in a permanent solid state. Thermosetting plastics contain polymers with chemically reactive structures of groups that are cross-linked together during the curing process to form irreversible chemical bonds. Thermoplastics soften when heated and become more fluid when additional heat is applied. The curing process is completely reversible since no chemical bonding occurs.

[0019] In the context of the present application, the term "crosslinked material" may particularly refer to a material comprising crosslinks. The term crosslinking may refer to the bonds that connect one polymer chain to another polymer chain. They may be covalent bonds or ionic bonds. When the term "crosslinking" is used in the field of (particularly synthetic) polymers, it may refer to the use of crosslinking to promote differences in the physical properties of the polymer.

[0020] In the context of the present application, the term "crosslinked thermoplastic material" may particularly refer to a thermoplastic material that has been specially treated so as to form crosslinks between chains of the thermoplastic material. Descriptively speaking, such a crosslinked thermoplastic material may be a hybrid structure having thermoplasticity and thermosetting properties. Compared to pure thermosetting materials, thermoplastic materials do not intrinsically undergo crosslinking. However, the thermoplastic material may be induced to form crosslinked chains by applying an energy beam (particularly a high-energy electron beam) and / or by adding a functionalized crosslinking agent (e.g., a peroxide) to force the chains of the thermoplastic material to crosslink.

[0021] In the context of the present application, the term "highly filled material" may particularly denote a dielectric material comprising a matrix of a cross-linked thermoplastic material, which matrix is ​​filled with a considerable amount of particles and additives. In particular, the fractional weight or volume of the filler particles of the highly filled material may be greater than the fractional weight or volume of the matrix of the thermoplastic material. The filler particles may be added to adjust or tune the properties of the dielectric structure, in particular to provide thermal conductivity, increase mechanical stability, promote adhesion, etc.

[0022] In the context of the present application, the term "optically opaque material" may particularly denote a material that is substantially opaque at least for visible light. Thus, such an optically opaque material may prevent visible light from propagating through the optically opaque material.

[0023] In one embodiment, the cross-linked thermoplastic material includes chains connected by a cross-linking structure. The term "cross-linking structure" may particularly refer to a chemical compound that connects different chains of the thermoplastic material and is obtained as a reaction product of a cross-linking agent (e.g., peroxide) added during the manufacture of the dielectric structure. In other words, the cross-linking structure may be formed due to a cross-linking reaction between the cross-linking agent and the chains of the thermoplastic material.

[0024] In one embodiment, the degree of crosslinking of the crosslinked thermoplastic material is in the range of 2% to 90%, in particular in the range of 5% to 50%. The degree of crosslinking may indicate the percentage of repeating monomer units in the crosslinked thermoplastic material chain. With the mentioned ranges, the advantageous properties of the encapsulated dielectric structure obtained by triggering crosslinking of the thermoplastic material as described above can be very significant.

[0025] In one embodiment, the dielectric structure comprises filler particles, in particular at least 50 weight percent of filler particles relative to the total weight of the dielectric structure, more particularly in the range of 80 weight percent to 95 weight percent of filler particles relative to the total weight of the dielectric structure. Dielectric structures with very advantageous properties can already be obtained with very small amounts of cross-linked thermoplastic material, for example already 5 weight percent. Thus, circuit designers can have a high degree of freedom to add various types and amounts of filler particles and additives without compromising the performance of the chip package, in particular for power semiconductor applications.

[0026] In one embodiment, the filler particles comprise at least one of the group consisting of highly thermally conductive filler particles (particularly at least one of aluminum oxide (Al2O3) particles, aluminum nitride (AlN) particles, silicon oxide (SiO2) particles and boron nitride (BN) particles), colorants (particularly carbon black for obtaining an opaque or black encapsulation, or titanium dioxide (TiO2) for obtaining a white encapsulation), adhesion promoters (particularly silane-based) and catalysts (for accelerating chemical reactions, such as accelerating crosslinking). Additionally or alternatively, many other types of filler particles and / or additives may be added to the thermoplastic material to promote at least one of its physical properties, such as mechanical stability. For example, filler particles or additives may also be added that adjust the value of the coefficient of thermal expansion of the dielectric structure relative to the material of the electronic chip (particularly silicon) and / or relative to the material of the chip carrier (particularly copper in the case of a lead frame).

[0027] In one embodiment, the dielectric structure is substantially opaque, in particular having an optical transparency of less than 2%. In the context of the present application, the term "optical transparency" may in particular denote the ratio between the intensity of visible light transmitted through the dielectric structure divided by the intensity of visible light provided to the dielectric structure. In particular, the dielectric structure may absorb and / or reflect at least 98% of the provided light intensity. Thus, visible light (i.e., electromagnetic radiation in the wavelength range of 400 nm to 800 nm) may be largely prevented from propagating into the package. This may stabilize the functionality of the package and may suppress undesirable artifacts.

[0028] In one embodiment, the dielectric structure has a thermal conductivity value of at least 0.5 W / (mK), in particular at least 1 W / (mK). Such high thermal conductivity values ​​can be obtained by adding corresponding filler particles with sufficiently high thermal stability. As a result, heat generated inside the package, for example heat dissipated during operation of an electronic chip, in particular a power semiconductor chip, can be effectively removed from the package via the dielectric structure. Therefore, the dielectric structure can also contribute to the thermal performance of the package.

[0029] In one embodiment, the dielectric structure is configured as a sealing material that at least partially encapsulates at least one of the electronic chip and the carrier. This may be advantageous for, for example, protecting sensitive devices such as GaN / SiC devices. In the context of the present application, the term "sealing material" may particularly refer to a substantially electrically insulating and preferably thermally conductive material surrounding a portion of the electronic chip and / or chip carrier to provide mechanical protection, electrical insulation, and optionally contribute to heat removal during operation. Such a sealing material may be, for example, a molding compound. For encapsulation by molding, a cross-linked thermoplastic material may be used, as described herein. Filler particles (e.g., SiO2, Al2O3, Si3N4, BN, AlN, diamond, etc.), for example, to improve thermal conductivity, may be embedded in a plastic-based matrix of the sealing material.

[0030] In one embodiment, the package includes an additional sealing material that at least encapsulates at least a portion of the sealing material. In particular, the additional sealing material may include a thermosetting material, such as an epoxy-based material and / or a silicon-based material. Therefore, this additional sealing material can be made of a thermosetting material so as to increase the mechanical stability of the package as a whole. Alternatively, the additional sealing material may also include or consist of an additional highly filled and / or opaque cross-linked thermoplastic material.

[0031] In one embodiment, the dielectric structure is a layer structure covering at least a portion of at least one of the electronic chip and the carrier. For example, this layer structure can be a continuous layer or a patterned layer. This layer structure can be particularly applied to a part of the package where reliable electrical insulation is required locally. The favorable properties of the dielectric structure (high mechanical and electrical reliability, while allowing the properties of the dielectric structure to be particularly addressed by freely selecting a large number of filler particles and additives) allow us to also obtain a layer structure for covering a certain part of the package.

[0032] In one embodiment, the layer structure is covered by a heat sink. For example, such a heat sink can be a high thermal conductor, such as a copper plate or an aluminum plate, or an alloy of one or more metals. The heat sink can also be a high thermal conductor to which a group of heat sinks are attached for effective heat dissipation. In one embodiment, a portion of a chip carrier (e.g., a lead frame) that carries an electronic chip and extends outside the sealing material can be covered with a layered dielectric structure. In such an embodiment, it is very advantageous that the material of the dielectric structure is a reliable electrical insulator (for preventing electrical short circuits via the dielectric structure) and / or has a sufficiently high thermal conductivity (for significantly helping to remove heat generated by one or more electronic chips, for example, during operation from the interior of the package).

[0033] In one embodiment, the layer structure is arranged to electrically insulate different conductive parts of the carrier from each other. Advantageously, parts of the dielectric structure (e.g. islands that are not connected to each other) can be applied between different parts of the chip carrier (in particular different leads, die pads, etc.) to ensure reliable electrical insulation between such parts.

[0034] In one embodiment, the dielectric structure is configured to be thermally stable at least up to 260°C, in particular at least up to 300°C, more particularly at least up to 350°C. In many packaging applications, the package is connected to a mounting base such as a printed circuit board by welding. During welding, temperatures of about 250°C may typically occur. When the dielectric structure is thermally stable at least at such a temperature and preferably above this temperature, any undesired melting or delamination or damage phenomena during welding can be safely prevented. The lifetime and reliability of the package can thereby be significantly improved. The mentioned high thermal stability can be obtained by cross-linking the thermoplastic material and optionally providing filler particles that contribute to the thermal stability.

[0035] In one embodiment, the thermoplastic material comprises at least one of the following group consisting of: polyamide, polyetheretherketone, polyethylene terephthalate, polybutylene terephthalate, polyimide, polysulfone, high-density polyethylene, polyoxymethylene, polypropylene and polystyrene. Thus, in view of its limited thermomechanical stability, such thermoplastic materials are not suitable for chip packaging by themselves, especially for power semiconductor applications. However, when cross-linking thermoplastic materials, the desired properties can be obtained by combining the favorable properties of thermoplastic materials and thermosetting materials. By adding filler particles to the thermoplastic materials mentioned for crosslinking, the physical properties and usability of (especially power) chip packaging can be further improved.

[0036] In one embodiment, the at least one electronic chip comprises a semiconductor chip, in particular a power semiconductor chip. In particular, when the at least one electronic chip is a power semiconductor chip, a large amount of heat generated during packaging operation may cause thermal loads on the electrical and mechanical interfaces of the package. However, due to the dielectric structure disclosed herein, damage to the package can be prevented even under such harsh conditions.

[0037] In one embodiment, the electronic chip comprises at least one, in particular at least three or at least eight transistors, such as field effect transistors, in particular metal oxide semiconductor field effect transistors.In general, an electronic chip may comprise a plurality of transistors.

[0038] In one embodiment, the carrier comprises a lead frame and / or a ceramic sheet which is covered with respective metal layers on two opposite main surfaces (particularly a direct aluminum bonding (DAB) substrate and / or a direct copper bonding (DCB) substrate).

[0039] In one embodiment, the carrier is a lead frame. Such a lead frame can be a sheet metal structure, which can be patterned to form one or more mounting portions for mounting one or more electronic chips of the package, and one or more lead portions for electrically connecting the package to the electronic environment when the electronic chip is mounted on the lead frame. In one embodiment, the lead frame can be a metal plate (especially made of copper), which can be patterned, for example by stamping or etching. Forming the chip carrier as a lead frame is a cost-saving and mechanically and electrically very advantageous configuration, in which the low-ohmic connection of at least one electronic chip can be combined with the robust support capability of the lead frame. In addition, the lead frame can contribute to the thermal conductivity of the package, and the heat generated during the operation of the electronic chip can be eliminated due to the high thermal conductivity of the metal (especially copper) material of the lead frame.

[0040] However, other carriers can also be implemented. For example, a direct copper bonding substrate (DCB substrate) or a direct aluminum bonding substrate (DAB substrate) can be used as well as the basis for the carrier.

[0041] In one embodiment, the method includes initiating crosslinking by adding a crosslinking agent to the thermoplastic material and activating the crosslinking agent (e.g., heat). Crosslinking can be represented by the process of chemically connecting two or more molecules or chains by chemical (particularly covalent) bonds. Accordingly, the crosslinking agent can be represented by a substance that initiates crosslinking of the thermoplastic material. For example, the crosslinking agent includes at least one of the group consisting of peroxides, azo structures, and silanes. However, other crosslinking agents may also be implemented.

[0042] In one embodiment, the method includes activating the crosslinking agent by heating, particularly melting the mixture of thermoplastic material and crosslinking agent, to cause crosslinking. Therefore, the mixture of preformed thermoplastic material (such as one or more in the above-mentioned polymer group) and crosslinking agent (such as one or more in the above-mentioned group) can be liquefied to heat-induced crosslinking. The liquefied mixture can be, for example, supplied to a processing chamber (such as a mold) to cause crosslinking and form a dielectric structure covering at least a portion of an electronic chip and / or at least a portion of a chip carrier. Therefore, the process of crosslinking and forming a solidified dielectric structure can be carried out simultaneously, and therefore carried out in an efficient manner.

[0043] In addition to providing one or more cross-linking agents or as an alternative, the method may also include initiating cross-linking by irradiating the (e.g., already hardened) thermoplastic material with an energy beam, particularly a high-energy electron beam. In other words, cross-linking can be initiated by an electron beam or an electromagnetic radiation beam that propagates to the thermoplastic material and is configured to initiate its cross-linking. Cross-linking can therefore be initiated by radiation chemistry, so that the thermoplastic material is chemically changed by radiation. Therefore, radiation can be used to cross-link thermoplastic materials, particularly polymers thereof. Before, during, or after the thermoplastic material is supplied to a processing chamber (e.g., a molding tool) to cover at least a portion of at least one electronic chip and / or at least a portion of a chip carrier, the energy beam can be irradiated onto the thermoplastic material.

[0044] In one embodiment, forming the dielectric structure comprises at least one of the group consisting of molding (particularly injection molding), coating, and casting. Molding can be referred to as a process of manufacturing by shaping a liquid or pliable raw material using a rigid frame, which can be referred to as a mold. The mold can be a hollowed-out block or a set of tools, the internal hollow volume of which is filled with a liquid or pliable material. The liquid hardens inside the mold, thereby adopting its shape.

[0045] In one embodiment, the package comprises at least one electrically conductive connection element, in particular at least one of a bonding wire, a bonding tape and a clip, electrically connecting the electronic chip to a carrier, in particular to a lead portion of a lead frame. The clip may be a three-dimensional curved plate-type connection element having two planar portions connected to the upper main surface of the respective electronic chip and to the upper main surface of the chip carrier, wherein the two mentioned planar portions are interconnected by an inclined connection portion. As an alternative to such a clip, a bonding wire or a bonding tape may be used, which is a flexible electrically conductive wire or strip, one end portion of which is connected to the upper main surface of the respective chip and the opposite other end portion is electrically connected to the chip carrier. Within the sealing material, the electrically conductive connection may be formed by a connection element between a chip pad on the upper main surface of a chip mounted on a mounting portion of the carrier on the one hand and a lead portion of the carrier on the other hand.

[0046] As a substrate or wafer forming the basis of the electronic chip, a semiconductor substrate, preferably a silicon substrate, can be used. Alternatively, a silicon oxide or another insulator substrate can be provided. A germanium substrate or a III-V semiconductor material can also be implemented. For example, exemplary embodiments can be implemented in GaN or SiC technology.

[0047] In addition, exemplary embodiments can utilize standard semiconductor processing techniques, such as appropriate etching techniques (including isotropic and anisotropic etching techniques, in particular plasma etching, dry etching, wet etching), patterning techniques (which may involve photolithography masks), deposition techniques (such as chemical vapor deposition (CVD), plasma enhanced chemical vapor deposition (PECVD), atomic layer deposition (ALD), sputtering, etc.).

[0048] The above and other objects, features and advantages of the present invention will become apparent from the following description and appended claims taken in conjunction with the accompanying drawings, in which like parts or elements are designated by like reference numerals. BRIEF DESCRIPTION OF THE DRAWINGS

[0049] The accompanying drawings illustrate exemplary embodiments and are included to provide a further understanding of exemplary embodiments and constitute a part of this specification.

[0050] In the figure:

[0051] Figure 1 A cross-sectional view of a preform of a package is shown according to an exemplary embodiment.

[0052] Figure 2 According to an exemplary embodiment, Figure 1 Cross-sectional view of the fabricated package.

[0053] Figure 3 A cross-sectional view of a package according to another exemplary embodiment is shown.

[0054] Figure 4 A cross-sectional view of a package according to yet another exemplary embodiment is shown.

[0055] Figure 5 A cross-sectional view of a package according to yet another exemplary embodiment is shown. DETAILED DESCRIPTION

[0056] The illustrations in the drawings are schematic.

[0057] Before describing other exemplary embodiments in further detail, some basic concepts of the present invention will be summarized based on which exemplary embodiments have been developed.

[0058] According to exemplary embodiments, a polymer-based dielectric structure for chip packaging (particularly semiconductor packaging) is provided, which allows low moisture absorption, high mechanical stability and / or high electrical insulation (particularly high breakdown strength). It is further desired to obtain high UPH for such polymers in semiconductor packaging applications.

[0059] Typically, thermosetting materials (preferably epoxy resins) are used to form dielectric structures for semiconductor device packaging. Such thermosetting materials are formed in situ by applying heat to enable these materials to crosslink and harden, thereby providing them with their thermosetting properties. However, the disadvantages of such thermosetting materials are generally high hygroscopicity, limited and small process temperature range (about 150°C to 200°C), limited dielectric strength, high stress levels on the device during reliability, and limited UPH based on relatively high curing times within the mold cavity during transfer molding. In addition, it is difficult or impossible to dissolve thermosetting polymers in organic solvents, so it is difficult to achieve coating from liquids as a film or layer.

[0060] The main point of the exemplary embodiment is to use a thermoplastic polymer for chip encapsulation (especially for semiconductor encapsulation), which can be mixed with a hardener (also expressed as a cross-linking agent) for cross-linking and / or can be cross-linked by subsequent electron radiation to transfer the thermoplastic polymer in a cross-linked thermoplastic material, which has the properties of a thermosetting material and additional advantageous properties due to the thermoplastic characteristics. For example, the corresponding dielectric structure can be used for encapsulation, coating or electrical insulation layer. Very advantageously, such a dielectric structure can be made with a high percentage of filler particles and additives, which can be freely selected and can be combined with a cross-linked thermoplastic material to adjust the properties of the dielectric structure. For example, the optical opacity of the dielectric structure can be enhanced by adding one or more colorants (such as black carbon). This optical opacity improves the electrical properties of the chip package. It is also advantageous to add a large amount of filler particles, for example, to increase the thermal conductivity of the dielectric structure, promote adhesion, and / or add other or another function.

[0061] Descriptively speaking, the gist of the exemplary embodiments is a hybrid combination of the benefits of thermoplastic materials and the benefits of thermoset materials for designing dielectric structures for chip packages.

[0062] In particular, conventional thermoplastic systems suffer from the great disadvantage of limited thermomechanical stability due to their low melting temperature or glass transition temperature (Tg) and low temperature stability. However, thermoplastics generally have a very low tendency to absorb moisture (e.g., thermoplastics with less polarity absorb very little moisture), but the temperature stability is insufficient. Further advantageously, when used for encapsulated dielectric structures, thermoplastics can improve the electrical breakdown strength (especially considering the fact that thermoplastics with less polarity generally show significantly higher electrical breakdown or insulation strength). In addition, thermoplastics can reduce the process temperature (the process temperature of many polar thermoplastics is much lower than 200°C, or even lower than 150°C). Compared with conventional thermosetting materials, thermoplastics have a much higher UPH for injection molding (for thermoplastics) than for transfer or compression molding (for thermosetting plastics). In terms of the stress buffer layer between the encapsulation compound and the chip, wire and chip carrier, thermoplastics are generally softer than thermosetting materials (i.e., have a lower Young's modulus). Protecting sensitive materials such as SiC and GaN from the negative effects of conventional epoxy molding compounds in terms of electrical functionality or even mechanical chip cracks can be very important. Another advantage of thermoplastic polymers is that they are easily soluble in dedicated and suitable solvents.

[0063] By providing a dielectric structure comprising a crosslinked thermoplastic material, which is very advantageously highly filled with filler particles and additives, it is possible to obtain in combination reduced hygroscopicity, increased dielectric strength and a high flexibility in selecting a suitable thermoplastic system accordingly, in order to equip it with a crosslinker and / or subject it to electron irradiation in order to transfer it to a thermoset material with higher thermal and mechanical stability.

[0064] Therefore, the gist of the exemplary embodiments is to use a thermoplastic polymer equipped with a cross-linking agent and functionality for basic encapsulation using a simple process for thermoplastic processing (eg, injection molding, coating, casting, etc.).

[0065] Preferred polymers that can be used as a basis for designing dielectric structures are technical thermoplastics, such as polyamides; or high-performance polymers, such as PEEK (polyetheretherketone), which already exhibit good thermal and mechanical properties as simple thermoplastics; or highly crystalline polymers, such as HD-PE (high-density polyethylene) or POM (polyoxymethylene), which have very low hygroscopicity due to their low polarity and highly crystalline structure. All these materials are compatible with cross-linking additives and / or irradiated by energy beams to create dielectric structures with highly favorable properties in terms of high thermal, high mechanical and high electrical properties.

[0066] According to an exemplary embodiment, a thermoplastic-based polymer material can be used as a dielectric structure for packaging, in particular for encapsulation, as a primary buffer and / or for protective coating or external electrical insulation. In particular, the dielectric structure according to the exemplary embodiment can be used to insulate the exposed pad from the outside of a heat sink attached to the outside of one or more packages. The crosslinking of the corresponding materials can be carried out in situ by treatment (e.g. encapsulation), or after treatment to form a high-performance polymer similar to a thermoset. This can be achieved by mixing the thermoplastic material with one or more crosslinking agents (such as silanes, peroxides, azo groups, etc.) and / or by simple irradiation with an energy beam (e.g., by electron radiation, β-radiation or even electromagnetic radiation).

[0067] Figure 1 A cross-sectional view of a preform of a package 100 is shown according to an exemplary embodiment.

[0068] Figure 1 A chip carrier 102 is shown, which is embodied here as a lead frame made of copper. Four electronic chips 108, which are configured here as power semiconductor chips (any other number is also possible), are mounted (e.g. soldered) on the upper main surface of the chip carrier 102. A plurality of conductive pads 150 are formed on the electronic chips 108 and are mounted facing upwards, i.e. facing away from the mounting surface of the chip carrier 102.

[0069] Next, it will be described how to form a dielectric structure 104 embodied as a molded encapsulation material to encapsulate an exposed surface portion of the electronic chip 108 and a portion of the exposed surface of the chip carrier 102. In the following, different embodiments of forming the dielectric structure 104 will be described:

[0070] exist Figure 1, a substrate 160 for forming a dielectric structure 104 is shown. The substrate 160 is composed of a mixture of a thermoplastic material 106 (e.g., PEEK), a crosslinking agent 124 (e.g., peroxide) for initiating crosslinking of the thermoplastic material 106 when melted by heating, a large amount (e.g., at least 60 weight percent relative to the total weight of the substrate 160) of filler particles 114 (e.g., aluminum nitride particles for improving the thermal conductivity of the dielectric structure 104 to be manufactured, and carbon black as a colorant for making the dielectric structure 104 to be manufactured optically opaque or light-proof), and other additives (not shown). The substrate 160 is heated to be melted and then supplied to a molding chamber of a molding tool (not shown), in which the assembly of the chip carrier 102 and the electronic chip 108 is also accommodated. The crosslinking of the thermoplastic material 106 is initiated by providing sufficient heat during the molding process to activate the crosslinking agent 124. Thus, the presence of the crosslinking agent 124 will force the chains 110 in the polymer thermoplastic material 106 to form a crosslinked structure 112 (compare Figure 2 After the cross-linking reaction is completed, the dielectric structure 104 hardens and forms a sealing material 116, such as Figure 2 shown.

[0071] Additionally or alternatively, such as Figure 1 , cross-linking can be induced by irradiating the thermoplastic material 106 with a high-energy electron beam 154 generated by an electron beam source 156. A substrate 162 is provided consisting of a mixture of a thermoplastic material 106 (e.g. PEEK) and a large amount (e.g. at least 60 weight percent relative to the total weight of the substrate 162) of filler particles 114 (e.g. aluminum nitride particles for improving the thermal conductivity of the dielectric structure 104, and carbon black as a colorant for making the dielectric structure 104 to be manufactured optically opaque or light-proof), and other additives (not shown). The substrate 162 is heated so as to be melted and then supplied to a molding chamber of a molding tool (not shown), in which the assembly of the chip carrier 102 and the electronic chip 108 is also accommodated. The semi-finished product thus obtained comprises the thermoplastic material 106 (still substantially free of cross-linking) with the filler particles 114 embedded therein. When the hardened semi-finished product (already covered with the electronic chip 108 and the chip carrier 102) is irradiated with a high-energy electron beam 154, crosslinking of the thermoplastic material 106 is initiated, so that a film corresponding to Figure 2 The dielectric structure 104 of detail 152 is different, however, in that no cross-linking structure 112 is present, since no cross-linking agent 124 is provided in the matrix 162. Also by this treatment, a cross-linked thermoplastic material 106 is obtained.

[0072] In a third alternative, it is possible to combine crosslinking initiated by the crosslinking agent 124 and crosslinking initiated by the high-energy electron beam 154. This may allow obtaining a high degree of crosslinking and therefore a dielectric structure with highly advantageous properties.

[0073] Figure 2 Shows when executing reference Figure 1 A cross-sectional view of the package 100 according to an exemplary embodiment is obtained when the first or third alternative is described.

[0074] The package 100 shown is composed of a chip carrier 102, an electronic chip 108 mounted on the chip carrier 102, and an encapsulant-type dielectric structure 104 covering a portion of the chip carrier 102 and the electronic chip 108 and including a highly filled cross-linked thermoplastic material 106. As can be seen from detail 152, the cross-linked thermoplastic material 106 includes polymer chains 110 connected by cross-link structures 112, which are composed of Figure 1 The crosslinking agent 124 shown in FIG. Figure 1 By adjusting the process parameters of the initiated cross-linking process (particularly the amount of the cross-linking agent 124 and / or the intensity of the high-energy electron beam 154 ), the cross-linked thermoplastic material 106 may have a cross-linking degree in the range of 2% to 90% (eg, 20%).

[0075] The highly filled dielectric structure 104 comprises a considerable amount of filler particles 114. Due to the supply of carbon black or another suitable colorant as additive or filler particles 114 to the dielectric structure 104, the dielectric structure 104 is substantially optically opaque, for example its optical transparency is only 1%. This prevents light from propagating into the package 100, which increases the electrical reliability of the package 100. Due to the supply of aluminum nitride filling particles 114 to the dielectric structure 104, the dielectric structure 104 can have a high thermal conductivity value, for example 1 or 2 W / (mK). As a result, the heat generated during operation of the power semiconductor-type electronic chip 108 during operation of the package 100 can be effectively removed from the package 100, so as to improve the thermal performance of the package 100. Due to the crosslinking of the thermoplastic material 106, the obtained dielectric structure 104 has a high mechanical stability and is thermally stable, for example at least up to 300°C. As a result, the package 100 can be soldered to a mounting base (e.g., a printed circuit board, not shown), for example, at a typical soldering temperature of 260° C. without degrading the overall performance of the dielectric structure 104 or the package 100. Furthermore, the cross-linked thermoplastic material 106 advantageously prevents moisture from entering the package 100. The electrical insulation properties of the dielectric structure 104 are also highly reliable, which has a positive impact on the electrical performance of the package 100.

[0076] therefore, Figure 1 and Figure 2The embodiments provide a cross-linked thermoplastic material 106 for encapsulating (or in other words, as an encapsulation material 116) the chip carrier 102 and the electronic chip 108. Thus, the embodiments provide a cross-linked thermoplastic for device encapsulation.

[0077] In one embodiment, a protective coating for, for example, wire bonding or clamp bonding devices may also be formed with the crosslinked thermoplastic material 106 on the lead frame or other chip carrier 102 (eg, by forming a corresponding layer with a thickness ranging between 10 μm and 100 μm).

[0078] Crosslinking can be achieved by providing a crosslinking agent 124 (such as peroxide, azo structure, etc.) which can be decomposed by temperature or UV radiation into free radical structures, i.e. structures with unpaired electrons, to cause the thermoplastic chains 110 to react into a crosslinked thermoset dielectric structure 104 that still has thermoplastic properties. Alternatively, such crosslinking can be caused by any subsequent electron radiation (so a crosslinking agent 124 is not required in a thermoplastic formulation, but is still possible).

[0079] Figure 3 A cross-sectional view of a package 100 according to another exemplary embodiment is shown.

[0080] Figure 3 Examples and Figure 2 The difference of the embodiment is that Figure 3 The embodiment further includes an additional sealing material 118 encapsulating a portion of the aforementioned sealing material 116. For example, the additional sealing material 118 includes a thermosetting material, such as an epoxy-based material and / or a silicon-based material.

[0081] Figure 4 A cross-sectional view of a package 100 according to yet another exemplary embodiment is shown.

[0082] In accordance with Figure 4 In the package 100, the electronic chip 108 is mounted on a die pad 170 of a lead frame type chip carrier 102 via a connection structure 164 such as a solder material or glue. The pads 150 on the upper main surface of the electronic chip 108 can be electrically connected to the lead portion 172 of the chip carrier 102 through the conductive connection element 166 (here embodied as a bonding wire). The chip carrier 102, the electronic chip 108 and parts of the conductive connection element 166 are encapsulated by another sealing material 168 (e.g., a conventional epoxy-based molding compound).

[0083] Furthermore, a layered dielectric structure 104 comprising a highly filled optically opaque cross-linked thermoplastic material 106 is applied to cover the exposed lower major surface of the die pad 170 of the chip carrier 102. Figure 4In the embodiment of the present invention, the dielectric structure 104 is configured as a layer structure 120 (here embodied as a single continuous layer) covering the exposed portion of the carrier 102. The layer structure 120 may in turn be covered by a heat sink 122 to further improve the thermal performance of the package 100. In the embodiment shown, the heat sink 122 includes a thermally conductive plate-like body 174 integrally formed with a plurality of fins 176. However, alternatively, a simple copper plate may also be used as the heat sink 122 attached to the dielectric structure 104 for cooling. In the embodiment shown, the layer dielectric structure 104 provides high electrical breakdown strength and low moisture absorption.

[0084] Figure 5 A cross-sectional view of a package 100 according to yet another exemplary embodiment is shown.

[0085] exist Figure 5 In the embodiment of the present invention, the layer structure 120 includes dielectric islands 178, 180, which are arranged to electrically insulate different conductive parts 132, 134, 136 of the carrier 102 from each other. In the embodiment shown, the chip carrier 102 is configured as a DCB substrate, i.e. a sandwich arrangement of a central thermally conductive and electrically insulating layer 140 (e.g. a ceramic plate), which is covered with corresponding conductive layers 144, 142 (e.g. copper plates) on its two opposite main surfaces. The conductive layer 142 is patterned into conductive parts 132, 134, 136. Between the conductive parts 132, 134, the dielectric islands 178 including the highly cross-linked thermoplastic material 106 can ensure proper electrical decoupling. Between the conductive parts 134, 136, the dielectric islands 180 including the highly cross-linked thermoplastic material 106 can also ensure proper electrical decoupling. As can be seen from the detail 184, the dielectric islands 178, 180 can be arranged according to Figures 2 to 4 The dielectric structure 104 is composed of components.

[0086] Thus, the dielectric structure 104 can provide electrical breakdown protection for the DCB device shown. In other words, an insulating cross-linked thermoplastic is provided for high electrical insulation strength between the copper metallization layers shown. Also in this embodiment, the cross-linking can be done by electron irradiation of a batch process. As an alternative, a complete coating with a cross-linked thermoplastic material 106 can be performed after chip bonding and wire bonding to serve as a complete electrical insulation layer protection.

[0087] It should be noted that the term "comprising" does not exclude other elements or features, and "a" or "an" does not exclude a plurality. Elements described in connection with different embodiments may also be combined. It should also be noted that the reference numerals should not be interpreted as limiting the scope of the claims. In addition, the scope of the present application is not intended to be limited to the particular embodiments of the processes, machines, manufactures, compositions of matter, devices, methods and steps described in the specification. Therefore, the appended claims are intended to include such processes, machines, manufactures, compositions of matter, devices, methods or steps within their scope.

Claims

1. A package comprising: Electronic chips; as well as A dielectric structure comprising a highly filled cross-linked thermoplastic material, wherein the dielectric structure comprises or consists of an encapsulation material at least partially encapsulating the electronic chip, wherein the cross-linked thermoplastic material comprises chains connected by cross-linked structures, wherein the degree of cross-linking of the cross-linked thermoplastic material is in the range of 2% to 90%, and wherein the degree of cross-linking is the percentage of repeating monomer units in the chains of the cross-linked thermoplastic material.

2. The package according to claim 1, wherein: The dielectric structure includes at least 50 weight percent of filler particles relative to the total weight of the dielectric structure.

3. The package according to claim 2, wherein: The filler particles include at least one of the group consisting of: high thermal conductivity filler particles, a colorant, an adhesion promoter, and a catalyst.

4. The package according to claim 1, wherein: The dielectric structure is opaque.

5. The package of claim 1, comprising a further encapsulation material encapsulating at least part of the encapsulation material.

6. The package according to claim 5, wherein: The further sealing material comprises a thermosetting material.

7. The package according to claim 1, wherein: The dielectric structure comprises a layer structure which covers at least a portion of the electronic chip.

8. The package according to claim 7, wherein: The layer structure is arranged to electrically insulate different electrically conductive parts of a chip carrier of the package, on which the electronic chip is mounted, from one another.

9. The package according to claim 1, wherein: The thermoplastic material includes at least one of the group consisting of polyamide, polyetheretherketone, polyethylene terephthalate, polybutylene terephthalate, polyimide, polysulfone, high-density polyethylene, polyoxymethylene, polypropylene, and polystyrene.

10. The package of claim 1, comprising a chip carrier, the electronic chip being mounted on the chip carrier.

11. The package according to claim 10, wherein: The dielectric structure covers at least a portion of at least one of the electronic chip and the chip carrier.

12. A package comprising: Electronic chips; as well as A dielectric structure covering at least a portion of the electronic chip and comprising an optically opaque cross-linked thermoplastic material, wherein the cross-linked thermoplastic material comprises chains connected by cross-linking structures, wherein the degree of cross-linking of the cross-linked thermoplastic material is in the range of 2% to 90%, and wherein the degree of cross-linking is the percentage of repeating monomer units in the chains of the cross-linked thermoplastic material.

13. A method of manufacturing a package, the method comprising: mounting the electronic chip on a chip carrier; as well as A dielectric structure covering at least a portion of the electronic chip is formed by cross-linking a highly filled thermoplastic material, wherein cross-linking the highly filled thermoplastic material comprises connecting chains through cross-linked structures, wherein the degree of cross-linking of the highly filled thermoplastic material is in the range of 2% to 90%, and wherein the degree of cross-linking is a percentage of repeating monomer units in the chains of the highly filled thermoplastic material.

14. The method according to claim 13, wherein: The method comprises initiating the crosslinking by adding a crosslinking agent to the thermoplastic material and by activating the crosslinking agent.

15. The method according to claim 14, wherein: The cross-linking agent includes at least one selected from the group consisting of a peroxide, an azo structure, and a silane.

16. The method according to claim 14, wherein: Activating the cross-linking agent includes heating a mixture of the thermoplastic material and the cross-linking agent.

17. The method according to claim 13, wherein: The method comprises initiating the cross-linking by irradiating the thermoplastic material with an energy beam.

18. The method according to claim 13, wherein: Forming the dielectric structure includes at least one of the group consisting of: molding, coating, and casting.