Integrated Chip
By adopting a mesa structure and diffusion layer design with sidewall spaced apart in the III-V semiconductor device integrated chip, the problem of the technological maturity and high cost of the III-V semiconductor devices in the integrated chip is solved, and the device is improved Performance and manufacturing efficiency.
Patent Information
- Application Number
- CN201810947971.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Priority Date
- 2018-07-02
- Filing Date
- 2018-08-20
- Publication Date
- 2024-11-12
- Estimated Expiration
- 2039-01-07
AI Technical Summary
The application of existing Group III-V semiconductor devices in integrated chips is limited by the maturity of technology and high cost, and traditional etching processes have problems such as metal diffusion, high resistance and low power efficiency.
Using an integrated chip design including epitaxial stacking, metal structure and etching stop layer, the sidewall spaced mesa structure and diffusion layer are formed through the metal stripping process, and wet or chemical etching is used to avoid contamination and electricity caused by ion bombardment. Short-circuit problem.
It realizes reducing metal diffusion and resistance, improving the efficiency and power efficiency of Group III-V semiconductor devices without reducing the etching rate and improving the manufacturing yield, and reducing the cost of chip manufacturing.
Smart Images

Figure CN110676246B_ABST
Abstract
Description
Technical Field
[0001] An embodiment of the present invention relates to an integrated chip. Background Art
[0002] In the past few decades, semiconductor devices based on silicon have been regarded as the standard. However, semiconductor devices based on alternative materials have received increasing attention due to their advantages over silicon-based semiconductor devices. For example, semiconductor devices based on III-V semiconductor materials have received increasing attention due to their high electron mobility and direct bandgap compared to silicon-based semiconductor devices.
[0003] Although semiconductor devices based on alternative materials are gaining more and more attention, they are not as technologically mature as silicon-based semiconductor devices. As a result, the application of semiconductor devices based on alternative materials is more limited and more expensive. Therefore, integrated chips that include semiconductor devices based on both silicon and alternative materials can be used to alleviate the above concerns. Summary of the invention
[0004] In some embodiments, the present application provides an integrated chip, which includes: a substrate; a mesa structure located on the substrate and comprising a semiconductor material; a bump structure located between the substrate and the mesa structure, wherein the bump structure comprises a conductive material; and a diffusion layer recessed into the mesa structure and located between the bump structure and the mesa structure, wherein the diffusion layer comprises a semiconductor material and a conductive material respectively from the mesa structure and the bump structure, and the sidewalls of the diffusion layer are spaced apart from the sidewalls of the mesa structure.
[0005] In some embodiments, the present application provides a method for forming an integrated chip, the method comprising: forming a chip including an epitaxial stack and a first metal bump located on the epitaxial stack, wherein the first metal bump is positioned at a mesa region of the epitaxial stack; forming a second metal bump on a substrate; bonding the chip to the substrate at an interface where the first metal bump and the second metal bump contact each other; and performing etching on the chip to define a mesa structure at the mesa region of the epitaxial stack, wherein the sidewalls of the mesa structure are laterally offset relative to the sidewalls of the first metal bump.
[0006] In some embodiments, the present application provides another method for forming an integrated chip, the method comprising: forming a chip including an epitaxial stack, an etch stop layer and a metal layer, wherein the etch stop layer is located between the epitaxial stack and the metal layer; forming a first metal bump on a substrate; bonding the chip to the substrate so that the metal layer is located between the first metal bump and the epitaxial stack; performing etching on the epitaxial stack to define a mesa structure, wherein the etching stops on the etch stop layer; patterning the etch stop layer to transfer the pattern of the mesa structure to the etch stop layer; and patterning the metal layer to form a second metal bump between the first metal bump and the mesa structure. BRIEF DESCRIPTION OF THE DRAWINGS
[0007] The accompanying drawings are included to provide a further understanding of the present invention and are incorporated in and constitute a part of this specification. The drawings illustrate embodiments of the present invention and together with the description serve to explain the principles of the present invention.
[0008] The various aspects of the present invention will be best understood by reading the following detailed description in conjunction with the accompanying drawings. It should be noted that, in accordance with standard practice in the industry, the various features are not drawn to scale. In fact, the size of the various features may be arbitrarily increased or reduced for clarity of discussion.
[0009] Figure 1 Cross-sectional views of some embodiments of integrated chips that utilize pre-patterned mesa-side bumps to bond III-V devices to a substrate are shown.
[0010] Figure 2 Show Figure 1 A top view of some embodiments of front-side contacts for III-V devices is shown.
[0011] Figure 3 Show Figure 1 A top view of some embodiments of mesa-side bumps and substrate-side bumps for a III-V device is shown.
[0012] Figure 4A and Figure 4B The III-V device has an etch stop layer. Figure 1 Cross-sectional views of various alternative embodiments of integrated chips are shown.
[0013] FIG. 5A to FIG. 5C The invention is shown comprising bonding to a substrate and according to Figure 1 , Figure 4A and Figure 4B Cross-sectional views of various embodiments of integrated chips of multiple III-V devices each configured to illustrate a more detailed embodiment of a III-V device.
[0014] Fig. 6A , Figure 6B , Fig. 7A , Figure 7B , Figure 8 , Fig. 9A , Fig. 9B , Fig.10 , Fig.11A , Fig. 11B ,and Figure 12 to Figure 25 A series of figures showing some embodiments of a method of forming an integrated chip including multiple III-V devices bonded to a substrate using pre-patterned mesa side bumps.
[0015] Fig.26 Show Fig. 6A , Figure 6B , Fig. 7A , Figure 7B , Figure 8 , Fig. 9A , Fig. 9B , Fig.10 , Fig.11A , Fig. 11B ,and Figure 12 to Figure 25 Block diagram of some embodiments of the illustrated method.
[0016] Figure 27 to Figure 34 A series of cross-sectional views illustrating some embodiments of a method of forming an integrated chip including multiple III-V devices bonded to a substrate and having an etch stop layer.
[0017] Fig.35 Show Figure 27 to Figure 34 Block diagram of some embodiments of the illustrated method.
[0018] Figure 36 to Figure 40 A series of cross-sectional views illustrating some embodiments of methods of forming an integrated chip including multiple III-V devices bonded to a substrate using pre-patterned mesa side bumps and the multiple III-V devices having an etch stop layer.
[0019] Fig.41 Show Figures 36 to 40 Block diagram of some embodiments of the illustrated method.
[0020] Description of Figure Numbers
[0021] 100, 400A, 400B, 500A, 500B, 500C, 1000, 1200, 1300, 1400, 1500, 1600, 1700, 1800, 1900, 2000, 2100, 2200, 2300, 2400, 2500, 2700, 2800, 2900, 3000, 3100, 3200, 3300, 3400, 3600, 3700, 3800, 3900, 4000: Sectional view
[0022] 102: III-V devices
[0023] 102a: The first III-V device
[0024] 102b: Second III-V Device
[0025] 104: Substrate
[0026] 106: Pad
[0027] 106a: First pad
[0028] 106b: Second pad
[0029] 106c: The third pad
[0030] 108: Table structure
[0031] 110: Bump structure
[0032] 112: Table side bump
[0033] 112a: first bump section
[0034] 112b: second bump section
[0035] 114: Substrate side bump
[0036] 116: Combined interface
[0037] 118: Diffusion layer
[0038] 120: Back side contact
[0039] 122: Front contact
[0040] 124: Conductive structure
[0041] 124v, 518: through hole
[0042] 124w, 516: Wiring
[0043] 126: Dielectric Structure
[0044] 128: Contact opening
[0045] 130: The first Bragg reflector
[0046] 132: Second Bragg reflector
[0047] 134: Active layer
[0048] 136: First reflector layer
[0049] 138: Second reflector layer
[0050] 140: Reflector layer pair
[0051] 200, 300: Top view
[0052] 402: Etching stop layer / second etching stop layer
[0053] 502: Hard mask
[0054] 504: Sidewall spacer
[0055] 508: semiconductor substrate / second semiconductor substrate
[0056] 510: Semiconductor devices
[0057] 512: Internal connection structure
[0058] 514: Interconnect dielectric layer 600A, 700A, 900A, 1100A: Figure / Top view layout 600B, 700B, 900B, 1100B: Figure / Cross-sectional view
[0059] 602: The first workpiece
[0060] 604, 904: die area
[0061] 606: first semiconductor substrate
[0062] 608: First etch stop layer
[0063] 610: Epitaxial stacking
[0064] 702: Countertop area
[0065] 704, 1102, 1702, 2104, 2302, 2402, 2502, 2804: Photoresist masks
[0066] 706: Mesa side bump layer
[0067] 706a: first mesa side bump layer
[0068] 706b: second mesa side bump layer
[0069] 800: Top view layout
[0070] 802: Chip
[0071] 902: Second Workpiece
[0072] 1002: First contact layer
[0073] 1004: Seed layer
[0074] 1402: Protective layer
[0075] 1602: Hard mask layer
[0076] 2102: Through hole opening
[0077] 2404: Second contact layer
[0078] 2504: Conductive layer
[0079] 2600, 3500, 4100: Block Diagram
[0080] 2602, 2604, 2606, 2608, 2610, 2612, 2614, 2616, 2618, 2620, 3502, 3504, 3506, 3508, 3510, 3512, 3514, 3516, 3518, 3520, 3522, 3524, 4102, 4104, 4106, 4108, 4110, 4112, 4114, 4116, 4118, 4120, 4122, 4124: Step 2802: Countertop opening
[0081] A, B: Line
[0082] D: Distance
[0083] D1, D2: diameter
[0084] ID: inner diameter
[0085] OD: Outer Diameter
[0086] OS: Overlying displacement DETAILED DESCRIPTION
[0087] The present invention provides many different embodiments or examples for implementing the different features of the present invention. Specific examples of components and arrangements are described below to simplify the present disclosure. Of course, these are only examples and are not intended to be limiting. For example, the following description of forming a first feature "on" or "on" a second feature may include an embodiment in which the first feature and the second feature are formed to be in direct contact, and may also include an embodiment in which an additional feature may be formed between the first feature and the second feature, thereby making the first feature and the second feature may not be in direct contact. In addition, the present invention may reuse reference numbers and / or letters in various examples. This repetition is for the purpose of brevity and clarity, rather than itself representing the relationship between the various embodiments and / or configurations discussed.
[0088] Furthermore, for ease of description, spatially relative terms such as "beneath," "below," "lower," "above," and "upper" may be used herein to describe the relationship of one element or feature to another (other) element or feature as shown in the figures. The spatially relative terms are intended to encompass different orientations of the device in use or operation in addition to the orientation depicted in the figures. The device may have other orientations (rotated 90 degrees or at other orientations), and the spatially relative descriptors used herein should be interpreted accordingly.
[0089] According to a method of forming an integrated circuit (IC) chip having both a silicon semiconductor device and a III-V semiconductor device, a chip including a III-V epitaxial stack and a metal layer is formed. A silicon-based complementary metal-oxide-semiconductor (CMOS) device is formed on a wafer, an interconnect structure covering the silicon-based complementary metal-oxide-semiconductor device and the wafer is formed, and a wafer metal bump is formed on the interconnect structure. The chip is positioned so that the metal layer is located between the wafer metal bump and the III-V epitaxial stack and is then bonded to the die region of the wafer via the wafer metal bump. A dry etch is performed into the chip to define a mesa structure and further define the chip metal bump. The mesa structure at least partially defines individual III-V semiconductor devices, which may be, for example, vertical-cavity surface-emitting lasers (VCSELs) or some other suitable devices. Each chip metal bump is used for each III-V semiconductor device, and each III-V semiconductor device is electrically coupled to an adjacent wafer metal bump. A wet etch is performed to shrink the chip metal bumps, and then the wafer is separated into a plurality of individual integrated circuit chips.
[0090] The challenge of the method is that the metal from the metal layer diffuses into the epitaxial stack and forms a diffusion layer that is difficult to be chemically etched. For example, the diffusion layer may include a combination of nickel, germanium, gold, gallium, and arsenic. Therefore, dry etching is performed using ion bombardment. However, ion bombardment is messy and causes the etched material to be redeposited on the sidewalls of the etching process chamber and on the sidewalls of the wafer bumps. The redeposition may cause electrical shorting of the wafer bumps, which may result in a low manufacturing yield. In addition, the redeposition may reduce the etching rate and / or may contaminate other wafers used in the etching process chamber. Another challenge is that wet etching may significantly reduce the chip bumps. Typically, the chip bumps include individual nickel / gold segments and individual gold segments adjacent to the nickel / gold segments. Relatively speaking, the etchant used for wet etching may etch the gold region at a higher rate than the nickel / gold region, and thus the size of the gold region may be significantly reduced, which in turn may cause high resistance and negatively affect the performance and power efficiency of III-V semiconductor devices.
[0091] Various embodiments of the present application relate to a method of forming an integrated chip that bonds a III-V device to a substrate, and the integrated chip obtained by the method. In some embodiments, the method includes: forming a chip including an epitaxial stack, forming a metal structure on the epitaxial stack, and forming a diffusion layer between the metal structure and the epitaxial stack; bonding the chip to the substrate so that the metal structure is located between the substrate and the epitaxial stack during bonding; and performing etching into the mesa region of the epitaxial stack to form a mesa structure with sidewalls spaced apart from the diffusion layer. The diffusion layer includes metal from the metal structure and also includes semiconductor material from the epitaxial stack.
[0092] In some embodiments, the metal structure is a metal bump, and the forming chip includes forming the metal structure by a metal liftoff process before combining. In some embodiments, the forming chip includes depositing an etch stop layer on the epitaxial stack and patterning the etch stop layer to form an opening positioned to the mesa region and spaced apart from the side boundary of the mesa region. For example, an etch stop layer can be used as an etch stop for the etching. In other embodiments, an etch stop layer is not formed. In some embodiments where the metal structure is a metal bump, the metal structure is formed by performing a metal liftoff process in the opening before combining. In some embodiments, the metal structure is a metal layer, and the forming chip includes forming a metal structure covering the etch stop layer and filling the opening before combining. In this embodiment, after etching, the metal structure is patterned into a metal bump.
[0093] The diffusion layer is formed by diffusing metal from the metal structure into the epitaxial stack. By using a metal stripping process to form a metal structure as a metal bump, the metal structure can be limited to contacting the epitaxial stack at a contact interface that is positioned to the mesa region and spaced from the side boundaries of the mesa region. Therefore, the diffusion of metal into the epitaxial stack can be limited to the contact interface. In addition, the diffusion layer can be positioned to form the contact interface and thus spaced from the side boundaries of the mesa region. By forming a metal structure on an etch stop layer as a metal layer, the etch stop layer can partially space the metal structure from the epitaxial stack so that the metal structure is limited to contacting the epitaxial stack at a contact interface in the opening of the etch stop layer. Since the opening of the etch stop layer is positioned to the mesa region and spaced from the side boundaries of the mesa region, the contact interface is also positioned to the mesa region and spaced from the side boundaries of the mesa region. Therefore, as described above, the diffusion of metal into the epitaxial stack can be limited to the contact interface. In addition, the diffusion layer can be positioned to form the contact interface and thus spaced from the side boundaries of the mesa region.
[0094] By forming a diffusion layer spaced apart from the side boundaries of the mesa region, the etching can be performed without etching through the diffusion layer. In this way, the sidewalls of the mesa structure can be formed to be spaced apart from the diffusion layer. In some embodiments, the semiconductor material from the epitaxial stack is combined with the metal from the metal structure in a manner that makes it difficult for the diffusion layer to be etched and / or removed by a wet etchant and / or a chemical etchant. By forming a diffusion layer spaced apart from the side boundaries of the mesa region, the etching can be performed by a wet etchant and / or a chemical etchant. Otherwise, the etching can be performed by ion bombardment. However, since the kinetic energy from the ions is transferred to the etched material, ion bombardment is messier than wet etching and / or chemical etching. For example, the etched material may be redeposited and cause electrical shorts between pads and / or contacts. As another example, the etched material may be redeposited on the sidewalls of the etching process chamber, and the material etched on the sidewalls may reduce the etching rate and / or may contaminate other structures processed in the etching process chamber. Therefore, performing etching by wet etching and / or chemical etching avoids the challenges associated with ion bombardment.
[0095] As described above, in some embodiments, the metal structure is a metal bump formed before bonding. By forming the metal structure in this way, other bumps and / or structures on the substrate will not be damaged and / or reduced due to the etching process that patterns the metal structure into the metal bump after etching.
[0096] Reference Figure 1 , a cross-sectional view 100 of some embodiments of an integrated chip that combines a III-V device 102 to a substrate 104 is provided. The substrate 104 includes a first pad 106a and a second pad 106b along a top surface of the substrate 104. In some embodiments, the substrate 104 includes a semiconductor substrate (not shown), a semiconductor device located on the semiconductor substrate (not shown), and an internal connection structure covering the semiconductor substrate and the semiconductor device. The internal connection structure can, for example, electrically couple the first pad 106a and the second pad 106b to the semiconductor device.
[0097] The III-V device 102 overlies the first pad 106a and includes a mesa structure 108 and a bump structure 110. The mesa structure 108 overlies the bump structure 110 and may be or include, for example, indium gallium arsenide, aluminum gallium arsenide, some other III-V material, or any combination thereof. The bump structure 110 includes a mesa-side bump 112 and a substrate-side bump 114 bonded together at a bonding interface 116. The mesa-side bump 112 and the substrate-side bump 114 are conductive and may be or include, for example, gold, nickel, titanium, some other suitable metal, some other suitable conductive material, or any combination thereof.
[0098] In some embodiments, the mesa side bump 112 includes a first bump section 112a, and also includes a second bump section 112b overlying the first bump section 112a. The first bump section 112a may be or include, for example, gold, titanium, some other suitable metal, or any combination thereof, and / or may, for example, include a gold layer and a titanium layer overlying the gold layer. In some embodiments, the substrate side bump 114 is or includes the same material as the first bump section 112a. In addition, the first bump section 112a may, for example, have a thickness of about 50 nanometers to 800 nanometers or some other suitable thickness. The second bump section 112b may be or include, for example, nickel, gold, some other suitable metal, or any combination thereof, and / or may, for example, include a gold layer, a first nickel layer overlying the gold layer, a germanium-gold layer overlying the first nickel layer, and a second nickel layer overlying the germanium-gold layer. In addition, the second bump section 112b may, for example, have a thickness of about 50 nanometers to 500 nanometers or some other suitable thickness. In some embodiments, the substrate side bump 114 is or includes gold and / or some other suitable metal, and / or has a thickness between about 0.5 micrometers to 5.0 micrometers or some other suitable thickness.
[0099] As will be seen below, the mesa side bump 112 may be formed, for example, by a metal stripping process before forming the mesa structure 108. By forming the mesa side bump 112 by such a process, the mesa side bump 112 and the substrate side bump 114 may not be damaged by etching. For example, if the mesa side bump 112 is not formed by a metal stripping process before forming the mesa structure 108, a wet etching process may be performed after forming the mesa structure 108 to form the mesa side bump from the metal layer. However, relatively speaking, the wet etchant may have a higher selectivity to the substrate side bump 114 and the first bump section 112a than to the second bump section 112b, whereby the wet etchant may shrink the substrate side bump 114 and / or form a first bump section 112a that is substantially smaller than the second bump section 112b. This in turn may result in a smaller contact area at the bonding interface 116. In addition, the resistance between the mesa-side bump 112 and the substrate-side bump 114 may be high and the power efficiency may be low. Therefore, forming the mesa-side bump 112 by a metal stripping process before forming the mesa structure 108 may result in low resistance between the mesa-side bump 112 and the substrate-side bump 114 and may result in high power efficiency.
[0100] The diffusion layer 118 is recessed into the underside of the mesa structure 108 between the mesa structure 108 and the bump structure 110. In addition, the diffusion layer 118 is laterally spaced apart from the outer sidewalls of the mesa structure 108 by a distance D. As will be seen below, the diffusion layer 118 is formed by diffusion of metal from the mesa-side bumps 112 into adjacent portions of the mesa structure 108. Thus, the diffusion layer 118 includes the III-V material from the mesa structure 108, and further includes the metal from the mesa-side bumps 112. For example, the diffusion layer 118 may include germanium, gallium, arsenide, or any combination thereof from the mesa structure 108, and may also include nickel, gold, or any combination thereof from the mesa-side bumps 112.
[0101] As will be seen below, an etching process may be performed to the stack of one or more III-V layers to form a mesa structure 108 from the mesa region of the III-V stack. In addition, as will be seen below, a mesa side bump 112 may be formed on the III-V stack by a metal stripping process prior to the etching process. By forming the mesa side bump 112 using a metal stripping process prior to the etching process, a diffusion layer 118 may be formed locally to the mesa side bump 112 and spaced apart from the side boundaries of the mesa region. This in turn enables the etching process to be performed without etching through the diffusion layer 118.
[0102] In some embodiments, the III-V material from the mesa structure 108 is combined with the metal from the mesa side bump 112 in a manner that makes the diffusion layer 118 difficult to etch and / or remove by a wet etchant. Therefore, in the case where the etching process can be performed without etching through the diffusion layer 118, the etching process can be performed by a wet etchant. Otherwise, the etching process can be performed using ion bombardment. However, since the kinetic energy from the ions is transferred to the etched material, ion bombardment is messier than wet etching. For example, the etched material may be redeposited and electrically short the first pad 106a and the second pad 106b. As another example, the etched material may be redeposited on the sidewalls of the etching process chamber, where the etched material may reduce the etching rate and / or may cause contamination to other structures processed in the etching process chamber. Therefore, by forming the mesa side bump 112 using a metal stripping process prior to the etching process, the challenges associated with ion bombardment can be avoided.
[0103] The backside contact 120 is located on the back side of the III-V device 102, between the first pad 106a and the bump structure 110, and is electrically coupled to the first pad 106a. The frontside contact 122 is located on the front side of the III-V device 102, opposite to the back side of the III-V device 102, and is electrically coupled to the second pad 106b. For example, the frontside contact 122 can be electrically coupled to the second pad 106b through a conductive structure 124 extending from the second pad 106b to the frontside contact 122. In some embodiments, the top view layout of the frontside contact 122 is a square ring, a circular ring, or some other suitable shape. The frontside contact 122 and the backside contact 120 can be or include, for example, titanium, tungsten, copper, some other suitable conductive material, or any combination thereof. In some embodiments, the backside contact 120 includes a titanium layer, a copper layer overlying the titanium layer, and a titanium-tungsten layer overlying the copper layer. In some embodiments, the backside contact 120 has a thickness of about 2000 to 5000 angstroms, about 3200 angstroms, or some other suitable thickness.
[0104] The dielectric structure 126 surrounds the III-V device 102 and, in some embodiments, defines a contact opening 128 on the front side of the III-V device 102. As will be seen below, the III-V device 102 may, for example, emit radiation (e.g., visible light or some other suitable radiation) from the front side of the III-V device 102, such that the contact opening 128 allows the radiation to pass unimpeded through the dielectric structure 126. The dielectric structure 126 may be or include, for example, a molding compound, some other suitable conductive material, or any combination thereof.
[0105] In some embodiments, the III-V device 102 is a vertical cavity surface emitting laser and includes a first Bragg reflector 130, a second Bragg reflector 132, and an active layer 134. The active layer 134 is located between the first Bragg reflector 130 and the second Bragg reflector 132 and may, for example, include one or more quantum wells. The active layer 134 may, for example, have a thickness of about 1 nanometer to 20 nanometers or some other suitable thickness. The active layer 134 may be or contain, for example, indium gallium arsenide and / or some other suitable III-V material. In some embodiments, the active layer 134 is or contains [Indium gallium arsenide] x GaAs] y , wherein x is about 0.1 to 0.9 and y is about 1 to 5.
[0106] The first Bragg reflector 130 and the second Bragg reflector 132 are located on the back side of the III-V device 102 and on the front side of the III-V device 102, respectively. In addition, the first Bragg reflector 130 and the second Bragg reflector 132 are defined by a plurality of first reflector layers 136 and a plurality of second reflector layers 138. For ease of illustration, only one of the first reflector layers 136 is labeled as 136, and only one of the second reflector layers 138 is labeled as 138. The first reflector layers 136 and the second reflector layers 138 are interleaved and stacked, and the first reflector layers 136 may have, for example, different properties (e.g., refractive index or some other suitable properties) from the second reflector layers 138. The first reflector layers 136 and the second reflector layers 138 may be or include, for example, aluminum gallium arsenide, some other suitable III-V materials, or any combination thereof.
[0107] In some embodiments, the first reflector layers 136 are each Al x GaAs, where x is about 0 to 0.9. In addition, in some embodiments, each of the first reflector layers 136 has a thickness between 4 nanometers and 100 nanometers, or some other suitable thickness. In some embodiments, each of the second reflector layers 138 is Al xIn some embodiments, the reflector layer pairs 140 on the front side of the III-V device 102 are repeated 0 to 100 times to increase the second Bragg reflector 132, and / or the reflector layer pairs (not labeled) on the back side of the III-V device 102 are repeated 0 to 100 times to increase the first Bragg reflector 130.
[0108] Reference Figure 2 , a top view 200 of some embodiments of the front contact 122 is provided. The front contact 122 has an annular layout and is located on the mesa structure 108. However, alternative layouts are also acceptable in other embodiments. In some embodiments, the inner diameter ID of the front contact 122 is about 8 microns to 10 microns, about 9 microns, or some other suitable value. In some embodiments, the outer diameter OD of the front contact is about 10 microns to 14 microns, about 12 microns, or some other suitable value. When viewed in cross section (see, e.g. Figure 1 ), the front side contact 122 may, for example, directly contact the mesa structure 108. In some of such embodiments, the contact area between the mesa structure 108 and the front side contact 122 is about 50 square microns to 200 square microns, about 50 square microns, or some other suitable area.
[0109] Reference Figure 3 , a top view 300 of some embodiments of the mesa side bump 112 and the substrate side bump 114 is provided. The mesa side bump 112 is located on the substrate side bump 114 and in some embodiments, the mesa side bump 112 and the substrate side bump 114 have an overlay shift OS. The overlay shift OS can be, for example, about 0 microns to 6 microns, about 1 micron to 6 microns, or some other suitable overlay shifts. In addition, the mesa side bump 112 and the substrate side bump 114 have a circular layout. However, alternative layouts are also acceptable in other embodiments. In some embodiments, the diameter D1 of the mesa side bump 112 is about 10 microns to 14 microns, about 12 microns, or some other suitable values. In some embodiments, the diameter D2 of the substrate side bump 114 is the same as or approximately the same as the diameter D1 of the mesa side bump 112, and / or is about 10 microns to 14 microns, about 12 microns, or some other suitable values. When observed in a cross section (see, for example, Figure 1), the mesa side bump 112 and the substrate side bump 114 may, for example, be in direct contact. In some of such embodiments, the contact area between the mesa side bump 112 and the substrate side bump 114 is about 44 square microns to 114 square microns, about 400 to 500 square microns, or some other suitable area.
[0110] Reference Figure 4A , providing a method in which the mesa side bump 112 protrudes through the etch stop layer 402 to the diffusion layer 118 Figure 1 Cross-sectional view 400A of some alternative embodiments of the integrated chip shown. Etch stop layer 402 may be or include, for example, silicon nitride, silicon oxide, silicon oxynitride, some other suitable dielectric, some other suitable etch stop material, or any combination thereof. Etch stop layer 402 may, for example, have a thickness of about 10 nanometers to 500 nanometers or some other suitable thickness. In some embodiments, the mesa side bump 112 wraps around the corner of the etch stop layer 402 and / or has a greater width than the substrate side bump 114. In some embodiments, the second bump section 112b of the mesa side bump 112 has a greater width than the first bump section 112a of the mesa side bump 112, and / or the first bump section 112a has a greater width than the substrate side bump 114.
[0111] As will be seen below, the etch stop layer 402 is used as an etch stop during the formation of the mesa structure 108. For example, an etching process may be performed into a stack formed of one or more III-V layers and may stop on the etch stop layer to form the mesa structure 108 from a mesa region of the III-V stack. Additionally, as will be seen below, the etch stop layer 402 may enable the diffusion layer 118 to be formed to be spaced apart from the side boundaries of the mesa region. This in turn enables the etching process to be performed without etching through the diffusion layer 118. Thus, in some embodiments where the III-V material from the mesa structure 108 is combined with the metal from the mesa side bumps 112 in a manner that makes the diffusion layer 118 difficult to etch and / or remove by wet etching, challenges associated with ion bombardment may be avoided (see Figure 1 discussed).
[0112] Reference Figure 4B , providing a method in which the mesa side bumps 112 do not wrap around the corners of the etch stop layer 402 Figure 4A Cross-sectional view 400B of some alternative embodiments of the integrated chip is shown. In addition, in some embodiments, the width of the bump structure 110 increases from top to bottom, and / or the substrate-side bump 114 has an inverted T-shaped profile. However, other profiles are also acceptable in other embodiments.
[0113] As will be seen below, the mesa side bumps 112 may be formed by a metal stripping process before forming the mesa structure 108. By forming the mesa side bumps 112 in this manner, the mesa side bumps 112 and the substrate side bumps 114 are not damaged by etching to form the mesa side bumps 112. Figure 1 As discussed, such damage may cause a smaller contact area between the mesa-side bump 112 and the substrate-side bump 114 at the bonding interface 116. In addition, the resistance between the mesa-side bump 112 and the substrate-side bump 114 may be high and the power efficiency may be low. Therefore, forming the mesa-side bump 112 by a metal stripping process before forming the mesa structure 108 may result in low resistance between the mesa-side bump 112 and the substrate-side bump 114 and may result in high power efficiency.
[0114] Reference Figure 5A , a cross-sectional view 500A of some embodiments of an integrated chip including a first III-V device 102a and a second III-V device 102b bonded to a substrate 104 is provided. The first III-V device 102a overlies and is electrically coupled to a first pad 106a, and the second III-V device 102b overlies and is electrically coupled to a third pad 106c. In addition, the second pad 106b is located between the first III-V device 102a and the second III-V device 102b and is electrically coupled to the first III-V device 102a and the second III-V device 102b through a conductive structure 124. In some embodiments, the conductive structure 124 has a T-shaped profile, but other profiles are acceptable in other embodiments.
[0115] The first III-V device 102a and the second III-V device 102b are based on Figure 1 1. The embodiment of the present invention is configured to provide a more detailed embodiment of the III-V device 102 shown in FIG. 1 and thus also includes a hard mask 502 and sidewall spacers 504. The hard mask 502 overlies the mesa structure 108 and in some embodiments at least partially defines the contact opening 128. The sidewall spacers 504 line the sidewalls of the mesa structure 108 and the sidewalls of the bump structure 110. As will be seen below, the hard mask 502 may be used, for example, as a mask to define the mesa structure 108, and / or the sidewall spacers 504 may protect the mesa structure 108 and the bump structure 110 while, for example, defining the backside contact 120. The hard mask 502 and the sidewall spacers 504 may be or include, for example, silicon nitride, silicon oxide, silicon oxynitride, some other suitable dielectric, or any combination thereof. In some embodiments, the hard mask 502 and the sidewall spacers 504 are the same material.
[0116] The substrate 104 includes a semiconductor substrate 508, a plurality of semiconductor devices 510 located on the semiconductor substrate 508, and an interconnect structure 512 located on the semiconductor substrate 508 and the semiconductor devices 510. For ease of illustration, only some of the semiconductor devices 510 are labeled as 510. The semiconductor substrate 508 can be, for example, a bulk single crystal silicon substrate, a silicon-on-insulator (SOI) substrate, or some other suitable semiconductor substrate. The semiconductor device 510 can be or include, for example, a metal-oxide-semiconductor field-effect transistor (MOSFET), some other suitable metal-oxide-semiconductor (MOS) device, some other suitable insulated-gate field-effect transistor (IGFET), a complementary metal-oxide-semiconductor device, some other suitable semiconductor device, or any combination thereof.
[0117] The interconnect structure 512 includes an interconnect dielectric layer 514, a plurality of wires 516, a plurality of vias 518, and a plurality of pads. For ease of illustration, only some of the wires 516 are labeled as 516, and only some of the vias 518 are labeled as 518. The interconnect dielectric layer 514 may be or include, for example, borophosphosilicate glass (BPSG), phosphorus-silicate glass (PSG), undoped silicon glass (USG), some other low dielectric constant (k) dielectric, silicon oxide, silicon carbide, some other suitable dielectric, or any combination thereof. The low dielectric constant dielectric used herein may be or include, for example, a dielectric having a dielectric constant of less than about 3.9, 3, 2, or 1. The pads include a first pad 106a, a second pad 106b, and a third pad 106c, and wiring 516, vias 518, and the pads are stacked alternately in the interconnect dielectric layer 514. The wiring 516 and vias 518 define a conductive path for interconnecting and / or connecting the semiconductor device 510 to the pads. The wiring 516, vias 518, and the pads may be or include, for example, copper, aluminum copper, aluminum, titanium, tungsten, some other suitable metal, or any combination thereof.
[0118] Reference Figure 5B , wherein the first III-V group device 102a and the second III-V group device 102b are provided according to Figure 4A A more detailed embodiment of the III-V device 102 is shown configured Figure 5A A cross-sectional view 500B of some alternative embodiments of the integrated chip is shown. Figure 5A As in FIG. 1 , the hard mask 502 is located on the mesa structure 108 and the sidewall spacers 504 are located on the sidewalls of the mesa structure 108. However, Figure 5A In contrast, the sidewall spacers 504 are not located on the sidewalls of the bump structure 110 .
[0119] Reference Figure 5C , wherein the first III-V group device 102a and the second III-V group device 102b are provided according to Figure 4B A more detailed embodiment of the III-V device 102 is shown configured Figure 5A A cross-sectional view 500C of some alternative embodiments of the integrated chip is shown. Figure 5A As in FIG. 1 , the hard mask 502 is located on the mesa structure 108 and the sidewall spacers 504 are located on the sidewalls of the mesa structure 108 and the sidewalls of the bump structure 110. However, Figure 5A Instead, the bump structure 110 has an inverted T-shaped profile. However, other suitable profiles are also acceptable in other embodiments.
[0120] although Figure 1 , Figure 4A ,and Figure 4B A III-V device 102 is described, however, it should be appreciated that a device based on semiconductor materials other than III-V materials may be used in place of the III-V device 102. For example, a silicon-based device may be used in place of the III-V device 102, whereby the mesa structure 108 may be or include silicon. Similarly, although 5A to 5C describe a first III-V device 102a and a second III-V device 102b, it should be appreciated that a device based on semiconductor materials other than III-V materials may be used in place of the first III-V device 102a and the second III-V device 102b.
[0121] Reference Fig. 6A , Figure 6B , Fig. 7A , Figure 7B , Figure 8 , Fig. 9A , Fig. 9B , Fig.10 , Fig.11A , Fig. 11B ,and Figure 12 to Figure 25 , a series of figures illustrate some embodiments of methods for forming an integrated chip including a plurality of III-V devices bonded to a substrate using pre-patterned mesa side bumps. In other embodiments, the method may form and / or use devices based on semiconductor materials other than III-V materials in place of III-V devices. The integrated chip may be, for example, as described with reference to Figure 5A Although described with reference to a method Fig. 6A , Figure 6B , Fig. 7A , Figure 7B , Figure 8 , Fig. 9A , Fig. 9B , Fig.10 , Fig.11A , Fig. 11B ,and Figure 12 to Figure 25 , but you should know that Fig. 6A , Figure 6B , Fig. 7A , Figure 7B , Figure 8 , Fig. 9A , Fig. 9B , Fig.10 , Fig.11A , Fig. 11B ,and Figure 12 to Figure 25 The structures shown in are not limited to the described methods and can be independent.
[0122] If Fig. 6A and Figure 6B As shown in FIGS. 600A and 600B , a first workpiece 602 is formed. Fig. 6A A top view layout 600A of some embodiments of a first workpiece 602 is shown, and Figure 6B Shown along Fig. 6A A cross-sectional view 600B of some embodiments of a first workpiece 602 taken along line A in FIG.
[0123] Focus on Fig. 6A , the first workpiece 602 includes a plurality of die areas 604. For ease of illustration, only some of the die areas 604 are labeled 604. The die areas 604 can, for example, each have the same layout and / or configuration. In some embodiments, the first workpiece 602 has a circular top view layout and / or a diameter of approximately 6 inches. In other embodiments, the first workpiece 602 has some other top view layout and / or some other size.
[0124] Focus on Figure 6B, the first workpiece 602 also includes a first semiconductor substrate 606, a first etch stop layer 608, and an epitaxial stack 610. The first etch stop layer 608 overlies the first semiconductor substrate 606, and the epitaxial stack 610 overlies the first etch stop layer 608. At least at this stage of the method, the first semiconductor substrate 606 may, for example, also be referred to as a first semiconductor wafer. The first semiconductor substrate 606 may, for example, be a gallium arsenide substrate, some other suitable III-V group substrate, or some other suitable semiconductor substrate. In addition, the first semiconductor substrate 606 may, for example, have a thickness of about 200 microns, but other thicknesses are also acceptable in other embodiments. The first etch stop layer 608 may, for example, be or include gallium indium phosphide, some other suitable III-V group material, some other suitable etch stop material, or any combination thereof. The epitaxial stack 610 includes one or more epitaxial layers. Furthermore, epitaxial stack 610 may be or include, for example, aluminum gallium arsenide, indium gallium arsenide, some other suitable III-V material, some other suitable semiconductor material, or any combination thereof.
[0125] In some embodiments, a vertical cavity surface emitting laser is formed from an epitaxial stack 610. In some of such embodiments, the epitaxial stack 610 includes a first Bragg reflector 130, a second Bragg reflector 132, and an active layer 134. The active layer 134 is sandwiched between the first Bragg reflector 130 and the second Bragg reflector 132. The active layer 134 may, for example, include one or more quantum wells and / or may, for example, include indium gallium arsenide and / or some other suitable III-V group material. The first Bragg reflector 130 and the second Bragg reflector 132 are defined by a plurality of first reflector layers 136 and a plurality of second reflector layers 138. For ease of illustration, only some of the first reflector layers 136 are labeled 136, and only some of the second reflector layers 138 are labeled 138. The first reflector layers 136 are interleaved with the second reflector layers 138 and may have, for example, different properties (e.g., refractive index or some other suitable properties) than the second reflector layers 138. The first reflector layer 136 and the second reflector layer 138 can be or include, for example, aluminum gallium arsenide, some other suitable III-V material, or any combination thereof.
[0126] If Fig. 7A and Figure 7B As shown in FIGS. 700A and 700B, on the first workpiece 602, the table area 702 (see Figure 7B ) to form a mesa side protrusion 112. Fig. 7A A top view layout 700A of some embodiments of the first workpiece 602 and the mesa-side bump 112 is shown, and Figure 7B Shown along Fig. 7AA cross-sectional view 700B of some embodiments of the first workpiece 602 and the mesa side protrusion 112 is taken along the line A in FIG. Fig. 7A Only some of the mesa side bumps 112 are labeled as 112. The mesa side bumps 112 are conductive and can be or include, for example, nickel, gold, some other suitable metal, or any combination thereof. In some embodiments, the mesa side bumps 112 include individual first bump segments 112a and individual second bump segments 112b located below the first bump segments 112a. The first bump segments 112a can be or include, for example, gold and / or some other suitable metal, and / or the second bump segments 112b include nickel, gold, some other suitable metal, or any combination thereof.
[0127] In some embodiments, when the mesa-side bumps 112 are formed, the material of the mesa-side bumps 112 diffuses into the epitaxial stack 610 and defines a diffusion layer 118 for each of the mesa-side bumps 112. Thus, the diffusion layer 118 includes material from both the epitaxial stack 610 and the mesa-side bumps 112. For example, the diffusion layer 118 may include germanium, gallium, arsenide, or any combination thereof from the epitaxial stack 610, and / or may include nickel, gold, or any combination thereof from the mesa-side bumps 112. In some embodiments, the material from the epitaxial stack 610 is combined with the material from the mesa-side bumps 112 in such a way that the diffusion layer 118 is difficult to etch and / or remove by a wet etchant.
[0128] Focus on Figure 7B , in some embodiments, the mesa side bump 112 is formed by a metal stripping process. However, other methods for forming the mesa side bump 112 in other embodiments are also acceptable. In some embodiments, the metal stripping process includes: forming a photoresist mask 704 having an opening at the mesa region 702 on the epitaxial stack 610; depositing a mesa side bump layer 706 on the photoresist mask 704 and in the opening while the photoresist mask 704 is in place; and removing the photoresist mask 704. In some embodiments, the mesa side bump layer 706 includes a first mesa side bump layer 706a and a second mesa side bump layer 706b corresponding to the first bump section 112a and the second bump section 112b, respectively. By removing the photoresist mask 704, the portion of the mesa side bump layer 706 located on the photoresist mask 704 is stripped, and the portion of the mesa side bump layer 706 located in the opening remains to define the mesa side bump 112. The deposition may be performed, for example, by sputtering, electron-beam physical vapor deposition (EBPVD), some other suitable deposition process, or any combination thereof.
[0129] By forming the mesa side bumps 112 using a metal lift-off process, metal can be diffused into only a portion of the epitaxial stack 610 located at the mesa side bumps 112. In this way, the diffusion layer 118 can be formed to be spaced a distance D from the side boundaries of the mesa region 702. As will be seen below, this enables the mesa structure to be formed without ion bombardment that is messy and can cause a lot of problems.
[0130] If Figure 8 As shown in the top view layout 800, the die area 604 (see Fig. 7A ) into a plurality of chips 802. The separation may be performed, for example, by a die saw or some other suitable tool.
[0131] If Fig. 9A and Fig. 9B As shown in FIGS. 900A and 900B , a second workpiece 902 is formed. Fig. 9A A top view layout 900A of some embodiments of a second workpiece 902 is shown, and Fig. 9B Shown along Fig. 9A A cross-sectional view 900B of some embodiments of the second workpiece 902 is taken along line B in FIG.
[0132] Focus on Fig. 9A , the second workpiece 902 includes a plurality of die areas 904. For ease of illustration, only some of the die areas 904 are labeled 904. The die areas 904 can, for example, each have the same layout and / or configuration. In some embodiments, the second workpiece 902 has a circular top view layout and / or a diameter of approximately 12 inches. In other embodiments, the second workpiece 902 has some other top view layout and / or some other size. Fig. 6A In some embodiments where the first workpiece 602 and the second workpiece 902 are shown to have a circular top view configuration, the second workpiece 902 has a diameter that is larger than the diameter of the first workpiece 602 .
[0133] Focus on Fig. 9BAs shown in the cross-sectional view 900B, the second workpiece 902 also includes a second semiconductor substrate 508, a plurality of semiconductor devices 510 located on the second semiconductor substrate 508, and an interconnect structure 512 located on the second semiconductor substrate 508 and the semiconductor devices 510. For ease of illustration, only some of the semiconductor devices 510 are labeled as 510. At least at this stage of the method, the second semiconductor substrate 508 may also be referred to as a second semiconductor wafer, for example. The second semiconductor substrate 508 may be, for example, a bulk single crystal silicon substrate, a silicon-on-insulator substrate, or some other suitable semiconductor substrate. The semiconductor device 510 may be or include, for example, a complementary metal oxide semiconductor device, some other suitable semiconductor device, or any combination thereof.
[0134] The interconnect structure 512 includes an interconnect dielectric layer 514, a plurality of wires 516, a plurality of vias 518, and a plurality of pads 106. For ease of illustration, only some of the wires 516 are labeled 516, and only some of the vias 518 are labeled 518. The wires 516, vias 518, and pads 106 are stacked in an alternating pattern in the interconnect dielectric layer 514, and the wires 516 and vias 518 define conductive paths that interconnect the semiconductor device 510 and / or connect the semiconductor device 510 to the pads 106. The wires 516, vias 518, and pads 106 may be or include, for example, copper, aluminum copper, aluminum, titanium, tungsten, some other suitable metal, some other suitable conductive material, or any combination thereof.
[0135] If Fig.10 As shown in the cross-sectional view 1000, a first contact layer 1002 and a seed layer 1004 are formed in a stacked manner on the second workpiece 902. The seed layer 1004 overlies the first contact layer 1002 and may be or include, for example, gold, some other suitable metal, some other suitable conductive material, or any combination thereof. The first contact layer 1002 may be or include, for example, titanium, tungsten, copper, some other suitable metal, some other suitable conductive material, or any combination thereof. The first contact layer 1002 and the seed layer 1004 may be formed, for example, by chemical vapor deposition (CVD), physical vapor deposition (PVD), some other suitable deposition process, or any combination thereof.
[0136] If Fig.11A and Fig. 11B As shown in FIGS. 1100A and 1100B, on the second workpiece 902, the corresponding pad 106 (see Fig. 11B ) to form a substrate side bump 114. Fig.11AA top view layout 1100A showing some embodiments of the second workpiece 902 and the substrate-side bumps 114 is shown, and Fig. 11B Shown along Fig.11A A cross-sectional view 1100B of some embodiments of the second workpiece 902 and the substrate-side bump 114 is taken along line B in FIG. Fig.11A Only some of the substrate-side bumps 114 are labeled as 114. The substrate-side bumps 114 are conductive and are or include a conductive layer that is connected to the seed layer 1004 (see Fig. 11B )same materials.
[0137] Focus on Fig. 11B , the substrate side bump 114 is formed by a plating process. However, other ways for forming the substrate side bump 114 are also acceptable in other embodiments. In some embodiments where the substrate side bump 114 is formed by a plating process, a photoresist mask 1102 having openings at the pads 106 corresponding to the substrate side bump 114 is formed on the seed layer 1004. A plating process is then performed to grow the substrate side bump 114 from the seed layer 1004 while the photoresist mask 1102 is in place, and then the photoresist mask 1102 is removed. The plating process may be, for example, electroplating, electroless plating, or some other suitable plating process.
[0138] If Fig.12 As shown in the cross-sectional view 1200, an etch back is performed to remove the seed layer 1004 (see Fig. 11B ), while leaving the substrate-side bumps 114. The etch back may be performed, for example, by wet etching or trimming and / or some other suitable etching process.
[0139] If Fig.13 As shown in the cross-sectional view 1300, the chip 802 (see Figure 8 ) is flipped and bonded to the second workpiece 902 at the bonding interface 116 where the substrate-side bumps 114 and the mesa-side bumps 112 make contact. In an embodiment where the second semiconductor substrate 508 is a wafer, the bonding may be, for example, referred to as chip-to-wafer (C2W) bonding. The bonding may be performed, for example, by metal-to-metal bonding and / or some other suitable bonding process.
[0140] If Fig.14As shown in the cross-sectional view 1400, a protective layer 1402 is formed around the chip 802, and the protective layer 1402 has a top surface that is concave and lower than the top surface of the chip 802. The protective layer 1402 may be, for example, or include an organic anti-reflective coating (ARC), an inorganic anti-reflective coating, some other suitable protective material, or any combination thereof. The protective layer 1402 may be formed, for example, by sputtering, chemical vapor deposition, physical vapor deposition, some other suitable deposition process, or any combination thereof.
[0141] If Fig.15 As shown in the cross-sectional view 1500, with the protection layer 1402 in place, the first semiconductor substrate 606 (see Fig.14 ) and the first etch stop layer 608 (see Fig.14 ) to remove the first semiconductor substrate 606 and the first etch stop layer 608. In some embodiments, the etching process includes performing a first etch on the first semiconductor substrate 606 to remove the first semiconductor substrate 606, and then performing a second etch into the first etch stop layer 608 to remove the first etch stop layer 608. In such an embodiment, the first etch stop layer 608 may, for example, serve as an etch stop for the first etch. In other embodiments, the etching process is limited to a single etch or includes more than the first etch and the second etch.
[0142] If Fig.16 As shown in the cross-sectional view 1600, the protective layer 1402 is removed (see Fig.15 ). The removal may be performed, for example, by an etching process and / or some other suitable removal process.
[0143] In addition, if Fig.16 As shown in the cross-sectional view 1600, a hard mask layer 1602 is formed on the epitaxial stack 610. The hard mask layer 1602 can be or include, for example, silicon oxide, silicon nitride, silicon oxynitride, some other suitable hard mask material, or any combination thereof. The hard mask layer 1602 can be formed, for example, by chemical vapor deposition, physical vapor deposition, oxidation, some other suitable deposition process, or any combination thereof. In some embodiments, the hard mask layer 1602 is positioned to the top surface of the epitaxial stack 610. In some embodiments of such embodiments, the hard mask layer 1602 is deposited by plasma enhanced physical vapor deposition to achieve such positioning.
[0144] If Fig.17 As shown in the cross-sectional view 1700, the hard mask layer 1602 (see Fig.16) is patterned to form a hard mask 502 on the mesa region 702 of the epitaxial stack 610. The patterning may be performed, for example, by a photolithography / etching process and / or some other suitable patterning process. The photolithography / etching process may, for example, include forming a photoresist mask 1702 on the hard mask layer 1602, etching the hard mask layer 1602 with the photoresist mask 1702 in place, and then stripping the photoresist mask 1702.
[0145] If Fig.18 As shown in the cross-sectional view 1800, with the hard mask 502 in place, the epitaxial stack 610 (see Fig.17 ) performs an etching process to form a mesa region 702 (see Fig.17 ) to form a mesa structure 108. The etching process may be performed, for example, by wet etching and / or some other suitable etching. As shown above, since the mesa side bump 112 may be formed by a metal stripping process, the metal may be diffused only into a portion of the epitaxial stack 610 positioned to the mesa side bump 112 and the diffusion layer 118 may be formed to be spaced apart from the side boundary of the mesa region 702. Therefore, the etching process may be performed without etching the diffusion layer 118.
[0146] In some embodiments, the material from the epitaxial stack 610 is combined with the material from the mesa side bump 112 in a manner that makes the diffusion layer 118 difficult to etch and / or remove by a wet etchant. Therefore, in the case where the etching process is performed without etching the diffusion layer 118, the etching process can be performed by wet etching. Otherwise, the etching process can be performed using ion bombardment. However, since the kinetic energy from the ions is transferred to the etched material, ion bombardment is messier than wet etching. For example, the etched material may be redeposited on the pad 106 and electrically short the pad 106. As another example, the etched material may be redeposited on the sidewalls of the etching process chamber, where the material etched on the sidewalls may reduce the etching rate and / or may cause contamination to other structures processed in the etching process chamber. Therefore, by forming the mesa side bump 112 using a metal stripping process, the above challenges associated with ion bombardment can be avoided.
[0147] If Fig.19As shown in the cross-sectional view 1900, sidewall spacers 504 are formed on the sidewalls of the mesa structure 108, the sidewalls of the mesa side bumps 112, and the sidewalls of the substrate side bumps 114. The sidewall spacers 504 may be or include, for example, silicon oxide, silicon nitride, silicon oxynitride, some other suitable dielectric, or any combination thereof. In some embodiments, the process of forming the sidewall spacers 504 includes depositing a sidewall spacer layer and then performing an etch back into the sidewall spacer layer. The deposition may be performed, for example, by chemical vapor deposition, physical vapor deposition, some other suitable deposition process, or any combination thereof.
[0148] If Fig. 20 As shown in the cross-sectional view 2000, the first contact layer 1002 (see Fig.19 ) to form backside contacts 120 respectively under each substrate-side bump 114. The etching process includes applying an etchant to the first contact layer 1002 and using the sidewall spacers 504 and the hard mask 502 as masks to form the backside contacts 120. The sidewall spacers 504 and the hard mask 502 also protect the mesa structure 108 during the etching process. The etching process can be performed, for example, by wet etching, dry etching, some other suitable etching, or any combination thereof.
[0149] Likewise, Fig. 20 As shown in the cross-sectional view 2000, a dielectric structure 126 is formed around the mesa structure 108. The dielectric structure 126 can be or include, for example, a molding compound, some other suitable conductive material, or any combination thereof. In some embodiments, the process of forming the dielectric structure 126 includes depositing the dielectric structure 126 by chemical vapor deposition, physical vapor deposition, sputtering, some other deposition process, or any combination thereof. In some embodiments, the process also includes chemical mechanical polishing (CMP) or some other suitable planarization process performed on the upper surface or top surface of the dielectric structure 126.
[0150] If Fig.21 As shown in the cross-sectional view 2100, the dielectric structure 126 is patterned to form a through-hole opening 2102 located between adjacent mesa structures 108 and exposing one of the pads 106. The patterning may be performed, for example, by a photolithography / etching process and / or some other suitable patterning process. The photolithography / etching process may, for example, include forming a photoresist mask 2104 on the dielectric structure 126, etching the dielectric structure 126 with the photoresist mask 2104 in place, and then stripping the photoresist mask 2104.
[0151] If Fig. 22As shown in the cross-sectional view 2200, a through hole 124v is formed in the through hole opening 2102. The through hole 124v may be or include, for example, titanium, tungsten, copper, aluminum copper, some other suitable conductive material, or any combination thereof. In some embodiments, the through hole 124v is formed by a plating process using a corresponding one of the pads 106 as a seed. The plating process may be, for example, electroplating, electroless plating, some other suitable plating process, or any combination thereof. In other embodiments, the through hole 124v is formed by depositing a metal layer covering the dielectric structure 126 and filling the through hole opening 2102; and then performing a planarization on the metal layer until the upper surface or top surface of the metal layer is approximately flush with the dielectric structure 126. Although the through hole 124v is formed using the above two processes, other processes are also acceptable in other embodiments.
[0152] If Fig.23 As shown in the cross-sectional view 2300, the dielectric structure 126 and the hard mask 502 are patterned to form the contact opening 128 exposing the mesa structure 108. The patterning may be performed, for example, by a photolithography / etching process and / or some other suitable patterning process. The photolithography / etching process may, for example, include forming a photoresist mask 2302 on the dielectric structure 126, etching the dielectric structure 126 and the hard mask 502 with the photoresist mask 2302 in place, and then stripping the photoresist mask 2302.
[0153] If Fig.24 As shown in the cross-sectional view 2400, on the mesa structure 108, the contact opening 128 (see Fig.23 ) to form a front contact 122. In some embodiments, the top view layout of the front contact 122 is a square ring, a circular ring, or some other suitable shape. The front contact 122 can be or include, for example, titanium, tungsten, copper, some other suitable conductive material, or any combination thereof.
[0154] In some embodiments, the front side contact 122 is formed by a metal stripping process. However, other ways for forming the front side contact 122 are also acceptable in other embodiments. In some embodiments, the metal stripping process includes: forming a photoresist mask 2402 having an opening corresponding to the front side contact 122; depositing a second contact layer 2404 on the photoresist mask 2402 and in the opening while the photoresist mask 2402 is in place; and removing the photoresist mask 2402. By removing the photoresist mask 2402, the portion of the second contact layer 2404 located on the photoresist mask 2402 is stripped, and the portion of the second contact layer 2404 located in the opening remains to define the front side contact 122. The deposition can be performed, for example, by sputtering, EB physical vapor deposition, some other suitable deposition process, or any combination thereof.
[0155] If Fig.25 As shown in the cross-sectional view 2500, a wire 124w is formed to electrically couple the via 124v to the front side contact 122. The wire 124w may be or include, for example, titanium, tungsten, copper, aluminum copper, some other suitable conductive material, or any combination thereof.
[0156] In some embodiments, the wiring 124w is formed by a metal stripping process. However, other ways for forming the wiring 124w in other embodiments are also acceptable. In some embodiments, the metal stripping process includes: forming a photoresist mask 2502 having an opening corresponding to the wiring 124w; depositing a conductive layer 2504 on the photoresist mask 2502 and in the opening while the photoresist mask 2502 is in place; and removing the photoresist mask 2502. By removing the photoresist mask 2502, the portion of the conductive layer 2504 located on the photoresist mask 2502 is stripped, and the portion of the conductive layer 2504 located in the opening remains to define the wiring 124w. The deposition can be performed, for example, by sputtering, electron beam physical vapor deposition, some other suitable deposition process, or any combination thereof.
[0157] In some embodiments, after forming the wiring 124w, the die region 904 (see Fig.11A ) into integrated circuit chips. The separation can be performed, for example, by a die saw or some other suitable tool.
[0158] Reference Fig.26 ,supply Fig. 6A , Figure 6B , Fig. 7A , Figure 7B , Figure 8 , Fig. 9A , Fig. 9B , Fig.10 , Fig.11A , Fig. 11B ,and Figure 12 to Figure 25 Block diagram 2600 of some embodiments of the method is shown.
[0159] At 2602, a first workpiece is formed including a semiconductor substrate and an epitaxial stack on the semiconductor substrate. Fig. 6A and Figure 6B .
[0160] At 2604, mesa side bumps are formed on the epitaxial stack. See e.g. Fig. 7A and Figure 7B .
[0161] At 2606, the first workpiece is singulated to define chips. See, e.g. Figure 8 .
[0162] At 2608, a second workpiece is formed. See, e.g. Fig. 9A and Fig. 9B .
[0163] At 2610, a contact layer and substrate-side bumps are formed on the second workpiece. Fig.10 , Fig.11A , Fig. 11B ,and Fig.12 .
[0164] At 2612, the chip is bonded to a second workpiece at an interface where the mesa-side bumps make contact with the substrate-side bumps. Fig.13 .
[0165] At 2614, the semiconductor substrate is removed. See e.g. Figure 14 to Figure 16 .
[0166] At 2616, the epitaxial stack is patterned to define mesa structures for each of the mesa side bumps. See, e.g. Figure 16 to Figure 18 .
[0167] At 2618, the contact layer is patterned to form a backside contact. See, e.g. Fig.19 and Fig. 20 .
[0168] At 2620, a conductive structure is formed that electrically couples the upper surface of the mesa structure to the second workpiece. See, e.g. Figure 20 to Figure 25 .
[0169] Although this article will Fig.26 The block diagram 2600 shown is shown and described as a series of actions or events, but it should be understood that the order of such actions or events should not be interpreted as having a limiting meaning. For example, some actions may occur in different orders and / or synchronously with other actions or events other than those shown and / or described herein. In addition, not all of the actions shown may be required to implement one or more aspects or embodiments described herein, and one or more of the actions shown herein may be implemented in one or more separate actions and / or stages.
[0170] Reference Figure 27 to Figure 34 , a series of cross-sectional views 2700 to 3400 illustrate some embodiments of a method of forming an integrated chip including a plurality of III-V devices bonded to a substrate and having an etch stop layer. In other embodiments, the method may form and / or use devices based on semiconductor materials other than III-V materials to replace III-V devices. The integrated chip may be, for example, as described with reference to Figure 5B Although described with reference to a method Figure 27 to Figure 34, but you should know that Figure 27 to Figure 34 The structures shown in are not limited to the described methods and can be independent.
[0171] If Fig. 27 As shown in the cross-sectional view 2700, a first workpiece 602 is formed. The first workpiece 602 may be, for example, Fig. 6A and Figure 6B As shown and described above. In addition, a second etch stop layer 402 is formed on the first workpiece 602. The second etch stop layer 402 can be or include, for example, silicon nitride, silicon oxide, silicon oxynitride, some other suitable dielectric, some other suitable etch stop material, or any combination thereof. In some embodiments, the second etch stop layer 402 is formed by chemical vapor deposition, physical vapor deposition, sputtering, some other suitable deposition process, or any combination thereof.
[0172] If Fig.28 As shown in the cross-sectional view 2800, the second etch stop layer 402 is patterned to form a mesa opening 2802 that exposes the mesa region 702 of the epitaxial stack 610. The patterning may be performed, for example, by a photolithography / etching process and / or some other suitable patterning process. The photolithography / etching process may, for example, include forming a photoresist mask 2804 on the second etch stop layer 402, performing an etch into the second etch stop layer 402 with the photoresist mask 2804 in place, and then stripping the photoresist mask 2804.
[0173] If Fig.29 As shown in the cross-sectional view 2900, a second etch stop layer 402 is formed to cover the mesa opening 2802 (see Fig.28 ) is used to line the mesa side bump layer 706. The mesa side bump layer 706 may be or include, for example, gold, nickel, titanium, some other suitable metal, some other suitable conductive material, or any combination thereof. In some embodiments, the mesa side bump layer 706 includes a first mesa side bump layer 706a and a second mesa side bump layer 706b. The mesa side bump layer 706 may be formed, for example, by chemical vapor deposition, physical vapor deposition, electroplating, electroless plating, some other suitable deposition and / or plating process, or any combination thereof.
[0174] In some embodiments, when the mesa side bump layer 706 is formed, the material of the mesa side bump layer 706 diffuses into the epitaxial stack 610 and defines the diffusion layer 118 of each mesa region 702. Therefore, the diffusion layer 118 includes materials from both the epitaxial stack 610 and the mesa side bump 112. In some embodiments, the material from the epitaxial stack 610 is combined with the material from the mesa side bump layer 706 in a manner that makes the diffusion layer 118 difficult to etch and / or remove by a wet etchant. By forming the mesa side bump layer 706 on the second etch stop layer 402, the second etch stop layer 402 spaces the mesa side bump layer 706 from the portion of the epitaxial stack 610 to the side of the mesa region 702. Therefore, the second etch stop layer 402 forms the diffusion layer 118 to be spaced a distance D from the side boundary of the mesa region 702.
[0175] If Fig.30 As shown in the cross-sectional view 3000, as shown and described above, the execution Figure 8 , Fig. 9A , Fig. 9B , Fig.10 , Fig.11A , Fig. 11B ,and Fig.13 Action at, but not executed Fig.12 In the execution Figure 8 At the same time as the action at Fig.29 ) is divided into a plurality of chips 802. In executing Fig. 9A and Fig. 9B At the same time as the action at the position, the second workpiece 902 is formed. Fig.10 At the same time as the actions shown, a first contact layer 1002 and a seed layer 1004 are formed on the second workpiece 902. Fig.11A and Fig. 11B At the same time as the operation at the second workpiece 902, a substrate-side bump 114 is formed on the second workpiece 902 at the corresponding pad 106 of the second workpiece 902. Fig.13 Simultaneously with the action at the top, one of the chips 802 is flipped in the vertical direction and bonded to the second workpiece 902 at the bonding interface 116 where the substrate-side bump 114 makes contact with the mesa-side bump layer 706 .
[0176] If Fig.31 As shown in the cross-sectional view 3100, as shown and described above, the execution Figures 14 to 18 Action at the location. Fig.14 and Fig.15 The first etch stop layer 608 and the first semiconductor substrate 606 are removed by the action at Figure 16 to Figure 18 The action at will epitaxial stack 610 (see Fig.30 ) is patterned to form a mesa region 702 (see Fig.30 ) defines a mesa structure 108 at a portion of the epitaxial stack 610. The patterning includes forming a hard mask 502 on the epitaxial stack 610, and then performing an etch toward the epitaxial stack 610 with the hard mask 502 in place. During the etching, the second etch stop layer 402 is used as an etch stop. The etching may be performed, for example, by a wet etching process or a chemical etching process, and / or may be performed by some other suitable etching process.
[0177] In some embodiments, material from the epitaxial stack 610 is combined with material from the mesa side bumps 112 in a manner that makes the diffusion layer 118 difficult to etch and / or remove by a wet etchant. In the case where the etching is performed without etching through the diffusion layer 118, the etching can be performed by wet etching. Otherwise, the etching can be performed, for example, using ion bombardment. However, because the kinetic energy from the ions is transferred to the etched material, ion bombardment is messier than wet etching. For example, the etched material may be redeposited on the pads 106 and / or the substrate side bumps 114 and electrically short the pads 106 and / or the substrate side bumps 114. As another example, the etched material may be redeposited on the sidewalls of the etching process chamber, where the etched material may reduce the etching rate and / or may cause contamination to other structures. Because the second etch stop layer 402 positions the diffusion layer 118 to form the mesa region 702 (see Fig.30 ) and thus positioned to be formed to the mesa structure 108, the etching can therefore be performed without etching through the diffusion layer 118 and the above challenges associated with ion bombardment can be avoided.
[0178] If Fig.32 As shown in the cross-sectional view 3200, the second etch stop layer 402 is patterned according to the layout of the hard mask 502. The patterning may be performed, for example, by an etching process and / or some other suitable patterning process. The etching process may, for example, include applying a wet etchant, a dry etchant, some other suitable etchant, or any combination thereof to the second etch stop layer 402.
[0179] In addition, if Fig.32 As shown in the cross-sectional view 3200, a sidewall spacer 504 is formed on the sidewall of the mesa structure 108 and the sidewall of the second etch stop layer 402. In some embodiments, the process of forming the sidewall spacer 504 includes depositing a sidewall spacer layer and then performing an etch back on the sidewall spacer layer. The deposition can be performed, for example, by chemical vapor deposition, physical vapor deposition, some other suitable deposition process, or any combination thereof.
[0180] If Fig.33 As shown in the cross-sectional view 3300, the mesa side bump layer 706 (see Fig.32) is patterned to form a mesa side bump 112 of each mesa structure 108. In some embodiments, the mesa side bump 112 includes a respective first bump segment 112a formed by the first mesa side bump layer 706a, and also includes a respective second bump segment 112b located below the first bump segment 112a and formed by the second mesa side bump layer 706b. In addition, the seed layer 1004 (see Fig.32 ). The patterning of the mesa side bump layer 706 and the removal of the seed layer 1004 may be performed, for example, by an etching process in which the hard mask 520 and the sidewall spacer 504 protect the mesa structure 108 and act as a mask. However, other methods for performing the patterning are also acceptable in other embodiments. The etching process may be, for example, a wet etching process, a dry etching process, or some other suitable etching process. In some embodiments, during the etching process, the size of the substrate side bump 114 is reduced. In addition, in some embodiments, during the etching process, the first bump segment 112a is etched more than the second bump segment 112b, so that the first bump segment 112a has a reduced width relative to the second bump segment 112b.
[0181] If Fig.34 As shown in the cross-sectional view 3400, as shown and described above, the execution Figure 20 to Figure 25 In the execution Fig. 20 At the same time as the action at Fig.33 ) is patterned to form a backside contact 120. In addition, a dielectric structure 126 is formed around the mesa structure 108. Fig.21 At the same time as the operation at , the dielectric structure 126 is patterned to form a through hole opening located between adjacent mesa structures 108 and exposing one of the pads 106. Fig. 22 At the same time as the action at the through hole, a through hole 124v is formed in the through hole opening. Fig.23 At the same time as the operation at 108, the dielectric structure 126 and the hard mask 502 are patterned to form contact openings that expose the mesa structure 108. Fig.24 At the same time as the operation at the top, a front contact 122 is formed on the mesa structure 108 and in the contact opening. Fig.25 Simultaneously with the action at the front side, a wiring 124w is formed that electrically couples the via 124v to the front side contact 122.
[0182] Reference Fig.35 ,supply Figure 27 to Figure 34 Block diagram 3500 of some embodiments of the method shown.
[0183] At 3502, a first workpiece is formed including a semiconductor substrate and an epitaxial stack on the semiconductor substrate. Fig. 27 .
[0184] At 3504, an etch stop layer is formed on the epitaxial stack, wherein the etch stop layer has openings at the mesa regions of the epitaxial stack. Fig. 27 and Fig.28 .
[0185] At 3506, a mesa side bump layer is formed on the etch stop layer to line the opening. Fig.29 .
[0186] At 3508, the first workpiece is singulated to define chips. See, e.g. Fig.30 .
[0187] At 3510, a second workpiece is formed. See, e.g. Fig.30 .
[0188] At 3512, a contact layer and substrate-side bumps are formed on the second workpiece. Fig.30 .
[0189] At 3514, the chip is bonded to a second workpiece at an interface where the mesa-side bump layer makes contact with the substrate-side bump. Fig.30 .
[0190] At 3516, the semiconductor substrate is removed. See, e.g. Fig.31 .
[0191] At 3518, an etch is performed toward the epitaxial stack to form respective mesa structures of the mesa regions, wherein the etch stops on the etch stop layer. See, e.g. Fig.31 .
[0192] At 3520, the etch stop layer and the mesa side bump layer are patterned, wherein the patterning of the mesa side bump layer forms mesa side bumps. Fig.32 and Fig.33 .
[0193] At 3522, the contact layer is patterned to form a backside contact. See, e.g. Fig.34 .
[0194] At 3524, a conductive structure is formed to electrically couple the upper surface of the mesa structure to the second workpiece. See, e.g. Fig.35 .
[0195] Although this article will Fig.35The block diagram 3500 shown is shown and described as a series of actions or events, but it should be understood that the order of such actions or events should not be interpreted as limiting. For example, some actions may occur in different orders and / or synchronously with other actions or events other than those shown and / or described herein. In addition, not all of the actions shown may be required to implement one or more aspects or embodiments described herein, and one or more of the actions shown herein may be performed in one or more separate actions and / or stages.
[0196] Reference Figures 36 to 40 , a series of cross-sectional views 3600 to 4000 illustrate some embodiments of a method of forming an integrated chip including a plurality of III-V devices bonded to a substrate using pre-patterned mesa side bumps and having an etch stop layer. In other embodiments, the method may form and / or use devices based on semiconductor materials other than III-V materials to replace III-V devices. The integrated chip may be, for example, as described with reference to Figure 5C Although described with reference to a method Figures 36 to 40 , however, you should know that Figure 36 to Figure 40 The structures shown in are not limited to the described methods and can be independent.
[0197] If Fig.36 As shown in the cross-sectional view 3600, a first workpiece 602 is formed. The first workpiece 602 may be, for example, as shown in FIG. Fig. 6A and Figure 6B In addition, according to the reference Fig. 27 and Fig.28 The illustrated and described actions form a second etch stop layer 402 on the first workpiece 602 and pattern the second etch stop layer 402. Fig. 27 At the same time as the action at the step 602, a second etch stop layer 402 is formed on the first workpiece 602. Fig.28 Simultaneously with the action at , the etch stop layer is patterned to form mesa openings 2802 exposing the mesa regions 702 of the epitaxial stack 610 .
[0198] If Fig.37 As shown in the cross-sectional view 3700, on the first workpiece 602, the table opening 2082 (see Fig.36) to form a mesa side bump 112 in the epitaxial stack 610. In some embodiments, the mesa side bump 112 includes a respective first bump section 112a and a respective second bump section 112b located below the first bump section 112a. In some embodiments, when forming the mesa side bump 112, the material of the mesa side bump 112 diffuses into the epitaxial stack 610 and defines a diffusion layer 118 for each of the mesa side bumps 112. In some embodiments, the material from the epitaxial stack 610 is combined with the material from the mesa side bump 112 in such a way that the diffusion layer 118 is difficult to etch and / or remove by a wet etchant.
[0199] In some embodiments, the mesa side bump 112 is formed by a metal stripping process. However, other methods for forming the mesa side bump 112 in other embodiments are also acceptable. In some embodiments, the metal stripping process includes: forming a photoresist mask 704 having an opening at the mesa region 702 on the epitaxial stack 610; depositing a mesa side bump layer 706 on the photoresist mask 704 and in the opening while the photoresist mask 704 is in place; and removing the photoresist mask 704. In some embodiments, the mesa side bump layer 706 includes a first mesa side bump layer 706a and a second mesa side bump layer 706b corresponding to the first bump section 112a and the second bump section 112b, respectively. By removing the photoresist mask 704, the portion of the mesa side bump layer 706 located on the photoresist mask 704 is stripped, and the portion of the mesa side bump layer 706 located in the opening remains to define the mesa side bump 112. By forming mesa side bump layer 706 over second etch stop layer 402, second etch stop layer 402 spaces mesa side bump layer 706 from portions of epitaxial stack 610 to the sides of mesa region 702. Thus, second etch stop layer 402 spaces diffusion layer 118 a distance D from side boundaries of mesa region 702.
[0200] If Fig.38 As shown in the cross-sectional view 3800, as shown and described above, the execution Figure 8 , Fig. 9A , Fig. 9B , Fig.10 , Fig.11A , Fig. 11B ,and Fig.13 Action at, but not executed Fig.12 In the execution Figure 8 At the same time as the action at Fig.37 ) is divided into a plurality of chips 802. In executing Fig. 9A and Fig. 9B At the same time as the action at the position, the second workpiece 902 is formed. Fig.10At the same time as the operation at the second workpiece 902, a first contact layer 1002 and a seed layer 1004 are formed on the second workpiece 902. Fig.11A and Fig. 11B At the same time as the operation at the second workpiece 902, a substrate-side bump 114 is formed on the second workpiece 902 at the corresponding pad 106 of the second workpiece 902. Fig.13 Simultaneously with the action at the second workpiece 902 , one of the chips 802 is flipped in the vertical direction and bonded to the second workpiece 902 at the bonding interface 116 where the substrate-side bumps 114 and the mesa-side bumps 112 make contact.
[0201] If Fig.39 As shown in the cross-sectional view 3900, as shown and described above, the execution Figures 14 to 18 Action at the location. Fig.14 and Fig.15 The first etch stop layer 608 and the first semiconductor substrate 606 are removed by the action at Figure 16 to Figure 18 The action at will epitaxial stack 610 (see Fig.38 ) is patterned to form a mesa region 702 (see Fig.38 ) defines a mesa structure 108 at a portion of the epitaxial stack 610. The patterning includes forming a hard mask 502 on the epitaxial stack 610, and then performing an etch toward the epitaxial stack 610 with the hard mask 502 in place. During the etching, the second etch stop layer 402 is used as an etch stop. The etching may be performed, for example, by a wet etching process or a chemical etching process, and / or may be performed, for example, by some other suitable etching process.
[0202] In some embodiments, the material from the epitaxial stack 610 is combined with the material from the mesa side bumps 112 in a manner that makes the diffusion layer 118 difficult to etch and / or remove by a wet etchant. In the case where the etching can be performed without etching through the diffusion layer 118, the etching can be performed by wet etching. Otherwise, the etching can be performed, for example, using ion bombardment. However, ion bombardment introduces a certain number of challenges as described above. Due to the second etch stop layer 402, the diffusion layer 118 is locally formed to the mesa region 702 (see Fig.39 ) and thus are formed locally to the mesa structure 108, so the etching can be performed without etching through the diffusion layer 118 and the challenges associated with ion bombardment can be avoided.
[0203] In addition, if Fig.39 As shown in the cross-sectional view 3900, the second etch stop layer 402 is patterned according to the layout of the hard mask 502. The patterning may be performed, for example, by an etching process and / or some other suitable patterning process. The etching process may, for example, include applying a wet etchant, a dry etchant, some other suitable etchant, or any combination thereof to the second etch stop layer 402.
[0204] If Fig.40 As shown in the cross-sectional view 4000, as shown and described above, the execution Figure 19 to Figure 25 In the execution Fig.19 At the same time as the above operation, sidewall spacers 504 are formed on the sidewalls of the mesa structure 108, the sidewalls of the mesa-side bumps 112, and the sidewalls of the substrate-side bumps 114. Fig. 20 At the same time as the action at Fig.39 ) and the first contact layer 1002 (see Fig.39 ) is patterned to form a backside contact 120. In addition, a dielectric structure 126 is formed around the mesa structure 108. Fig.21 At the same time as the operation at , the dielectric structure 126 is patterned to form a through hole opening located between adjacent mesa structures 108 and exposing one of the pads 106. Fig. 22 At the same time as the action at the through hole, a through hole 124v is formed in the through hole opening. Fig.23 At the same time as the operation at 108, the dielectric structure 126 and the hard mask 502 are patterned to form contact openings that expose the mesa structure 108. Fig.24 At the same time as the operation at the top, a front contact 122 is formed on the mesa structure 108 and in the contact opening. Fig.25 Concurrently with the actions shown, wiring 124w is formed that electrically couples via 124v to front side contact 122.
[0205] Reference Fig.41 ,supply Figure 36 to Figure 40 Block diagram 4100 of some embodiments of the method shown.
[0206] At 4102, a first workpiece is formed including a semiconductor substrate and an epitaxial stack on the semiconductor substrate. Fig.36 .
[0207] At 4104, an etch stop layer is formed on the epitaxial stack, wherein the etch stop layer has openings at the mesa regions of the epitaxial stack. Fig.36 .
[0208] At 4106, mesa side bumps are formed on the epitaxial stack and in each opening. Fig.37 .
[0209] At 4108, the first workpiece is singulated to define chips. See, e.g. Fig.38 .
[0210] At 4110, a second workpiece is formed. See, e.g. Fig.38 .
[0211] At 4112, a contact layer and substrate-side bumps are formed on the second workpiece. Fig.38 .
[0212] At 4114, the chip is bonded to a second workpiece at an interface where the mesa-side bumps make contact with the substrate-side bumps. Fig.38 .
[0213] At 4116, the semiconductor substrate is removed. See e.g. Fig.39 .
[0214] At 4118, an etch is performed toward the epitaxial stack to form respective mesa structures of the mesa regions, wherein the etch stops on the etch stop layer. See, e.g. Fig.39 .
[0215] At 4120, the etch stop layer is patterned according to the layout of the mesa structure. See e.g. Fig.39 .
[0216] At 4122, the contact layer is patterned to form a backside contact. See e.g. Fig.40 .
[0217] At 4124, a conductive structure is formed to electrically couple the upper surface of the mesa structure to the second workpiece. See, e.g. Fig.40 .
[0218] Although this article will Fig.41 The block diagram 4100 shown is shown and described as a series of actions or events, but it should be understood that the order of such actions or events should not be interpreted as having a limiting meaning. For example, some actions can occur in different orders and / or occur synchronously with other actions or events other than those shown and / or described herein. In addition, all of the actions shown may not be required to implement one or more aspects or embodiments described herein, and one or more of the actions shown herein can be implemented in one or more separate actions and / or stages.
[0219] In some embodiments, the present application provides an integrated chip, the integrated chip comprising: a substrate; a mesa structure located on the substrate and comprising a semiconductor material; a bump structure located between the substrate and the mesa structure, wherein the bump structure comprises a conductive material; and a diffusion layer recessed into the mesa structure and located between the bump structure and the mesa structure, wherein the diffusion layer comprises a semiconductor material and a conductive material from the mesa structure and the bump structure, respectively, and the sidewall of the diffusion layer is spaced apart from the sidewall of the mesa structure. In some embodiments, the integrated chip further comprises: an etch stop layer located on the mesa structure, and the etch stop layer is between the mesa structure and the substrate, wherein the bump structure protrudes through the etch stop layer to the diffusion layer. In some embodiments, the bump structure wraps around the adjacent corners of the etch stop layer. In some embodiments, the etch stop layer is dielectric, and wherein the bump structure comprises metal. In some embodiments, the diffusion layer comprises germanium, gallium, arsenic, or any combination thereof from the mesa structure, and the diffusion layer further comprises nickel, gold, or any combination thereof from the bump structure. In some embodiments, the sidewalls of the bump structure are laterally offset relative to the sidewalls of the mesa structure. In some embodiments, the mesa structure comprises an interleaved stack of different III-V family layers. In some embodiments, the integrated chip further comprises: a conductive contact located on the mesa structure, wherein the mesa structure is located between the conductive contact and the bump structure; and a conductive structure extending from the substrate to the conductive contact. In some embodiments, the substrate comprises: a semiconductor substrate; a complementary metal oxide semiconductor device located on the semiconductor substrate; and an internal wiring structure covering the semiconductor substrate and the complementary metal oxide semiconductor device.
[0220] In some embodiments, the present application provides a method for forming an integrated chip, the method comprising: forming a chip including an epitaxial stack and a first metal bump located on the epitaxial stack, wherein the first metal bump is positioned to a mesa region of the epitaxial stack; forming a second metal bump on a substrate; bonding the chip to the substrate at an interface where the first metal bump and the second metal bump contact each other; and performing etching on the chip to define a mesa structure at the mesa region of the epitaxial stack, wherein the sidewall of the mesa structure is laterally offset relative to the sidewall of the first metal bump. In some embodiments, the forming of the chip comprises forming the first metal bump on the epitaxial stack by a metal stripping process. In some embodiments, the forming of the second metal bump comprises: forming a metal seed layer on the substrate; forming a mask on the metal seed layer, wherein the mask defines an opening, the opening exposing the metal seed layer; and performing a plating process to form the second metal bump in the opening, wherein the metal seed layer becomes a seed for the second metal bump during the plating process. In some embodiments, the method of forming an integrated chip further includes: performing a second etch into the seed layer to remove a portion of the seed layer not covered by the second metal bump, wherein the second etch is performed before the combining. In some embodiments, the method of forming an integrated chip further includes: performing a second etch into the seed layer to remove a portion of the seed layer not covered by the second metal bump, wherein the second etch is performed after the etching. In some embodiments, the forming of the chip includes: depositing an etch stop layer on the epitaxial stack; patterning the etch stop layer to define an opening at the mesa region of the epitaxial stack; and forming the first metal bump in the opening by a metal stripping process, wherein etching stops on the etch stop layer.
[0221] In some embodiments, the present application provides another method for forming an integrated chip, the method comprising: forming a chip including an epitaxial stack, an etch stop layer and a metal layer, wherein the etch stop layer is located between the epitaxial stack and the metal layer; forming a first metal bump on a substrate; bonding the chip to the substrate so that the metal layer is located between the first metal bump and the epitaxial stack; performing etching on the epitaxial stack to define a mesa structure, wherein the etching stops on the etch stop layer; patterning the etch stop layer to transfer the pattern of the mesa structure to the etch stop layer; and patterning the metal layer to form a second metal bump between the first metal bump and the mesa structure. In some embodiments, the forming of the chip comprises: depositing the etch stop layer on the epitaxial stack; patterning the etch stop layer to define an opening at the mesa region of the epitaxial stack; and depositing the metal layer covering the etch stop layer and filling the opening. In some embodiments, the forming of the first metal bump includes: forming a seed layer on the substrate; forming a mask on the seed layer, wherein the mask defines an opening, the opening exposing the seed layer; and performing a plating process to form the first metal bump in the opening, wherein the seed layer becomes a seed for the first metal bump during the plating process. In some embodiments, the method further includes: patterning the seed layer to remove portions of the seed layer not covered by the first metal bump, wherein the patterning of the seed layer is performed after the etching. In some embodiments, the method further includes: forming a dielectric structure surrounding the mesa structure; forming a through hole extending through the dielectric structure to the substrate; forming a contact on the mesa structure, wherein the contact has a ring layout; and forming a wiring that electrically couples the contact to the through hole.
[0222] The features of several embodiments are summarized above so that those skilled in the art can better understand the various aspects of the present invention. Those skilled in the art will appreciate that they can easily use the present invention as a basis for designing or modifying other processes and structures to implement the same purposes and / or achieve the same advantages as the embodiments described herein. Those skilled in the art will also recognize that these equivalent constructions do not depart from the spirit and scope of the present invention, and that they can make various changes, substitutions and modifications thereto without departing from the spirit and scope of the present invention.
Claims
1. An integrated chip, characterized in that: include: A substrate, the substrate comprising a semiconductor substrate, a complementary metal oxide semiconductor (CMOS) device and an internal connection structure, the complementary metal oxide semiconductor (CMOS) device is located on the semiconductor substrate, and the internal connection structure covers the semiconductor substrate and the complementary metal oxide semiconductor device; a mesa structure located on the substrate and comprising a semiconductor material; a bump structure located between the substrate and the mesa structure, wherein the bump structure comprises a conductive material; as well as a diffusion layer, which is recessed into the mesa structure and located between the bump structure and the mesa structure, wherein the diffusion layer comprises semiconductor material and conductive material from the mesa structure and the bump structure, respectively, and A sidewall of the diffusion layer is spaced apart from a sidewall of the mesa structure.
2. The integrated chip according to claim 1, characterized in that: Also includes: An etch stop layer is located on the mesa structure and between the mesa structure and the substrate, wherein the bump structure protrudes through the etch stop layer to the diffusion layer.
3. The integrated chip according to claim 2, characterized in that: The bump structure wraps around adjacent corners of the etch stop layer.
4. The integrated chip according to claim 2, characterized in that: The etch stop layer is dielectric, and wherein the bump structure comprises metal.
5. The integrated chip according to claim 1, characterized in that: The diffusion layer comprises germanium, gallium, arsenic, or any combination thereof from the mesa structure, and The diffusion layer further includes nickel, gold, or any combination thereof from the bump structure.
6. The integrated chip according to claim 1, characterized in that: The sidewalls of the bump structure are laterally offset relative to the sidewalls of the mesa structure.
7. The integrated chip according to claim 1, characterized in that: The mesa structure includes a staggered stack of different III-V family layers.
8. The integrated chip according to claim 1, characterized in that: Also includes: A conductive contact member located on the mesa structure, wherein the mesa structure is located between the conductive contact member and the bump structure; as well as A conductive structure extends from the substrate to the conductive contact.
9. A method for forming an integrated chip, characterized in that: The method comprises: forming a chip including an epitaxial stack and a first metal bump on the epitaxial stack, wherein the first metal bump is localized to a mesa region of the epitaxial stack; forming a second metal bump on the substrate; bonding the chip to the substrate at an interface where the first metal bump and the second metal bump contact each other; and Etching into the chip is performed to define a mesa structure at the mesa region of the epitaxial stack, wherein sidewalls of the mesa structure are laterally offset relative to sidewalls of the first metal bump.
10. The method according to claim 9, characterized in that The forming of the chip includes forming the first metal bump on the epitaxial stack by a metal lift-off process.
11. The method according to claim 9, characterized in that The forming of the second metal bump comprises: forming a metal seed layer on the substrate; forming a mask on the metal seed layer, wherein the mask defines an opening that exposes the metal seed layer; and A plating process is performed to form the second metal bump in the opening, wherein the metal seed layer becomes a seed of the second metal bump during the plating process.
12. The method according to claim 11, characterized in that Also includes: A second etch is performed into the seed layer to remove portions of the seed layer not covered by the second metal bump, wherein the second etch is performed before the bonding.
13. The method according to claim 11, characterized in that Also includes: A second etch is performed into the seed layer to remove a portion of the seed layer not covered by the second metal bump, wherein the second etch is performed after the etching.
14. The method according to claim 9, characterized in that The forming of the chip comprises: depositing an etch stop layer on the epitaxial stack; patterning the etch stop layer to define openings at the mesa regions of the epitaxial stack; and The first metal bump is formed in the opening by a metal lift-off process, wherein etching stops on the etch stop layer.
15. The integrated chip according to claim 9, characterized in that: The mesa structure includes a staggered stack of different III-V family layers.
16. A method for forming an integrated chip, characterized in that: The method comprises: forming a chip including an epitaxial stack, an etch stop layer and a metal layer, wherein the etch stop layer is located between the epitaxial stack and the metal layer; forming a first metal bump on the substrate; bonding the chip to the substrate such that the metal layer is between the first metal bump and the epitaxial stack; performing an etch into the epitaxial stack to define a mesa structure, wherein the etch stops on the etch stop layer; patterning the etch stop layer to transfer the pattern of the mesa structure to the etch stop layer; and The metal layer is patterned to form a second metal bump between the first metal bump and the mesa structure.
17. The method according to claim 16, characterized in that The forming of the chip comprises: depositing the etch stop layer on the epitaxial stack; patterning the etch stop layer to define openings at mesa regions of the epitaxial stack; and The metal layer is deposited covering the etch stop layer and filling the opening.
18. The method according to claim 16, characterized in that The forming of the first metal bump comprises: forming a seed layer on the substrate; forming a mask on the seed layer, wherein the mask defines an opening that exposes the seed layer; and A plating process is performed to form the first metal bump in the opening, wherein the seed layer becomes a seed of the first metal bump during the plating process.
19. The method according to claim 18, characterized in that Also includes: The seed layer is patterned to remove portions of the seed layer not covered by the first metal bump, wherein the patterning of the seed layer is performed after the etching.
20. The method according to claim 16, characterized in that Also includes: forming a dielectric structure surrounding the mesa structure; forming a via extending through the dielectric structure to the substrate; forming a contact on the mesa structure, wherein the contact has a ring-shaped layout; and forming wiring that electrically couples the contact to the through hole.
21. An integrated chip, characterized in that: include: substrate; a mesa structure overlying the substrate and comprising a semiconductor material; a bump structure located between the substrate and the mesa structure, wherein the bump structure includes a conductive material located on top thereof; as well as A diffusion layer is located between the bump structure and the mesa structure, wherein the diffusion layer is recessed into the mesa structure and comprises the semiconductor material and the conductive material, wherein a sidewall of the diffusion layer is laterally offset relative to an adjacent semiconductor sidewall of the mesa structure, the adjacent semiconductor sidewall comprises the semiconductor material, and wherein the sidewall has an edge, the edge is raised relative to a bottom edge of the adjacent semiconductor sidewall, and the edge is recessed relative to a top edge of the adjacent semiconductor sidewall.
22. The integrated chip according to claim 21, characterized in that: Also includes: An etch stop layer is located on the mesa structure and between the mesa structure and the substrate, wherein the bump structure extends through the etch stop layer to the diffusion layer.
23. The integrated chip according to claim 22, characterized in that: The bump structure wraps around adjacent corners of the etch stop layer.
24. The integrated chip according to claim 21, characterized in that: The mesa structure includes a semiconductor layer, and the diffusion layer is recessed into the semiconductor layer.
25. The integrated chip according to claim 21, characterized in that: The mesa structure includes a first staggered stack formed of different III-V family layers, an active III-V family layer overlying the first staggered stack, and a second staggered stack formed of different III-V family layers, and the second staggered stack overlying the active III-V family layer.
26. The integrated chip according to claim 21, characterized in that: Also includes: A conductive contact member located on the mesa structure, wherein the mesa structure is located between the conductive contact member and the bump structure; as well as A conductive structure extends from the substrate to the conductive contact, wherein the conductive structure has a T-shaped profile.
27. The integrated chip according to claim 21, characterized in that: The substrate comprises: Semiconductor substrate; a semiconductor device on the semiconductor substrate; and The inner connection structure covers the semiconductor substrate and the semiconductor device.
28. The integrated chip according to claim 21, characterized in that: The bottom edge of the sidewall is flush with the bottom edge of the adjacent semiconductor sidewall.
29. An integrated chip, characterized in that: include: substrate; A mesa structure overlying the substrate and comprising a semiconductor layer; A conductive bump structure, located between the substrate and the mesa structure; as well as A diffusion layer is located between the conductive bump structure and the mesa structure, wherein the diffusion layer is recessed into the bottom of the semiconductor layer, and the width of the diffusion layer is smaller than the width of the semiconductor layer at the bottom, and wherein the diffusion layer includes the semiconductor material of the semiconductor layer and further includes a conductive material diffused from the conductive bump structure to the diffusion layer.
30. The integrated chip according to claim 29, characterized in that: The diffusion layer directly contacts the conductive bump structure at an interface, and wherein the conductive bump structure has the conductive material at the interface.
31. The integrated chip according to claim 29, characterized in that: The diffusion layer directly contacts the conductive bump structure at an interface, and wherein the interface has an inverted U-shaped profile.
32. The integrated chip according to claim 29, characterized in that: The mesa structure includes a pair of Bragg reflectors and an active semiconductor layer, and the active semiconductor layer is vertically stacked between the pair of Bragg reflectors.
33. The integrated chip according to claim 29, characterized in that: Also includes: An etch stop layer is located on the bottom of the mesa structure, wherein the conductive bump structure protrudes through the etch stop layer.
34. An integrated chip, characterized in that: include: substrate; a vertical cavity surface emitting laser overlying the substrate, wherein the vertical cavity surface emitting laser comprises a semiconductor layer located on a bottom surface thereof; a bump structure located between the substrate and the VCSEL, wherein the bump structure includes a conductive material located on a top surface thereof; as well as a diffusion layer located between the bump structure and the VCSEL, wherein the diffusion layer is in direct contact with the top surface of the bump structure and includes the conductive material and the semiconductor material of the semiconductor layer; The semiconductor layer wraps around adjacent corners of the diffusion layer from the sidewalls of the diffusion layer to the top surface of the diffusion layer.
35. The integrated chip according to claim 34, characterized in that: The diffusion layer is a region of the semiconductor layer into which the conductive material is diffused and in which the conductive material is mixed with the semiconductor material.
36. The integrated chip according to claim 34, characterized in that: The top surface of the bump structure has a widthwise center aligned with a widthwise center of the diffusion layer.
37. The integrated chip according to claim 34, characterized in that: The conductive material includes a semiconductor.
38. The integrated chip according to claim 34, characterized in that: The diffusion layer directly contacts the bottom surface of the VCSEL.
39. The integrated chip according to claim 34, characterized in that: The diffusion layer includes germanium, gallium, arsenic, or any combination thereof from the vertical cavity surface emitting laser, and wherein the diffusion layer further includes nickel, gold, or any combination thereof from the bump structure.
40. The integrated chip according to claim 34, characterized in that: The bump structure has an inverted T-shaped profile.