A composite smooth aluminum sheathed high voltage cable hot melt adhesive coating device and coating method thereof
Through the composite smooth aluminum sleeve high-voltage cable hot melt adhesive coating device, the hot melt adhesive is applied in two times, which solves the problem of cable sheath arching, ensures the appearance quality and safety of the cable, and realizes the aluminum sleeve and outer layer The tight contact and electric field of the sheath are evenly distributed, achieving a lightweight design of high-voltage cables.
Patent Information
- Application Number
- CN201911017333.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2019-10-24
- Publication Date
- 2024-11-26
- Estimated Expiration
- 2039-10-24
AI Technical Summary
Smooth aluminum-covered high-voltage cables are prone to arching or wrinkling after being coated with asphalt, which affects the appearance quality of the cable and may crush the inner insulation layer, and may endanger safe operation during construction.
Using composite smooth aluminum sleeve high-voltage cable hot melt adhesive coating device, the hot melt adhesive is coated in two times through argon arc welding production line and extruder, and the hot melt adhesive on the surface of the aluminum sleeve is preheated before the second coating. , so that it is about to be hot melted, and the two layers of hot melt adhesives are fused to each other and then entered the extruder for double-layer co-extrusion.
Eliminates the arching or wrinkling of the cable sheath, ensures the appearance quality of the cable, achieves close contact between the aluminum sleeve and the outer sleeve, uniforms the electric field distribution, avoids partial discharge, and realizes the lightweight design of high-voltage cables. .
Smart Images

Figure CN110739106B_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of cable manufacturing. Background Art
[0002] When the existing corrugated aluminum sheathed high-voltage cable is coated with asphalt, there will be no cable surface quality problems when the cable is normally reeled in. The cable is easy to bend, and the sheath surface on the inner side of the cable will not be bulged or wrinkled.
[0003] However, when producing smooth aluminum sheathed high-voltage cables, the finished cables coated with asphalt are wound up and the sheath is continuously arched. It is found that one occurs every one meter or so, which seriously affects the appearance and quality of the cable. After the aluminum sheath is arched or wrinkled, it may damage the insulation layer inside the cable after winding and winding, causing the cable to fail the factory test; in addition, when the cable is bent during construction, the sheath of the cable may be more seriously arched or wrinkled, which will endanger the safe operation of the cable. After many trials, this sheath arching phenomenon cannot be eliminated when the smooth aluminum sheath is coated with asphalt. Summary of the invention
[0004] The technical problem to be solved by the present invention is to provide a hot melt adhesive coating device for a composite smooth aluminum sheathed high-voltage cable to eliminate the phenomenon of the sheath of the cable being bulged or wrinkled.
[0005] In order to solve the above technical problems, the present invention adopts the following technical solutions: a composite smooth aluminum sheathed high-voltage cable hot melt adhesive coating device, comprising a argon arc welding production line and an extruder, the argon arc welding production line comprising a welding gun part and a traction part, and also comprising:
[0006] The first hot melt adhesive coating device is arranged between the welding gun part and the pulling part, and comprises a hot melt adhesive groove, an adhesive blocking die, a drawing die, and an electric heating temperature control component. The adhesive blocking die and the drawing die are arranged on two opposite side walls of the hot melt adhesive groove. The hot melt adhesive groove is filled with hot melt adhesive particles, which are heated by the electric heating temperature control component to turn the hot melt adhesive particles into liquid and completely immerse the aluminum sleeve. The aluminum sleeve enters the first hot melt adhesive coating device to perform a drawing process and is coated with hot melt adhesive for the first time at the same time;
[0007] The second hot melt adhesive coating device is arranged at the front side of the extruder inlet, and includes a hot melt adhesive groove, a glue blocking mold, a coating mold, and an electric heating temperature control component. The glue blocking mold and the coating mold are arranged on two opposite side walls of the hot melt adhesive groove. The hot melt adhesive groove is filled with hot melt adhesive particles. The hot melt adhesive particles are heated by the electric heating temperature control component to become liquid and completely immerse the aluminum sleeve. The aluminum sleeve enters the second hot melt adhesive coating device for a second coating of hot melt adhesive.
[0008] Optionally, a hot melt adhesive preheating device is provided before the second hot melt adhesive coating device, which is used to preheat the hot melt adhesive on the surface of the cable composite aluminum sheath before the second hot melt adhesive coating, so that the hot melt adhesive on the surface of the composite aluminum sheath is in a state of being about to melt.
[0009] Optionally, the hot melt adhesive preheating device includes an annular bracket and thermoplastic air guns uniformly distributed along the circumference of the annular bracket.
[0010] Optionally, the hot melt adhesive preheating device further comprises a base, the base is connected to a telescopic rod, the annular bracket is connected to the telescopic rod, and the height of the annular bracket is adjusted by the telescopic rod.
[0011] Optionally, the annular bracket is a square, and four thermoplastic air guns are respectively installed at the midpoints of the four sides of the annular bracket.
[0012] Optionally, the hot melt adhesive groove is rectangular, and the adhesive blocking mold and the drawing mold or the coating mold are arranged on the side walls on both sides of the width of the hot melt adhesive groove.
[0013] The present invention also provides a method for coating a composite smooth aluminum sheath high-voltage cable with hot melt adhesive, which is coated by using the composite smooth aluminum sheath high-voltage cable hot melt adhesive coating device. After the aluminum sheath is welded on an argon arc welding production line, the composite aluminum sheath enters a first hot melt adhesive coating device for a drawing process and is coated with hot melt adhesive for the first time. Then the composite aluminum sheath enters a hot melt adhesive preheating device for preheating the cable aluminum sheath, heating the aluminum sheath coated with hot melt adhesive for the first time so that the hot melt adhesive on the surface of the aluminum sheath is in a state of being about to be hot-melted. When the composite aluminum sheath with the hot melt adhesive on the surface in a hot-melt state enters a second hot melt adhesive coating device, the temperatures of the two parts of the hot melt adhesive are close, the two layers of coated hot melt adhesive are fused together, and then enter an extruder for double-layer co-extrusion of an outer sheath and a conductive layer.
[0014] Optionally, the thickness of the hot melt adhesive coated by the second hot melt adhesive coating device is 0.1-0.3 mm.
[0015] Optionally, the temperature difference between the two parts of the hot melt adhesive is controlled within ±1°C.
[0016] Optionally, the temperature of the hot air blown out by the thermoplastic air gun in the hot melt adhesive preheating device is controlled at 100+2°C.
[0017] The present invention adopts the above technical solution and has the following beneficial effects:
[0018] 1. The first hot melt adhesive coating device and the second hot melt adhesive coating device are used to coat the hot melt adhesive twice. Because the composite aluminum sleeve coated with hot melt adhesive for the first time passes through the jaw-type traction machine, the hot melt adhesive surface has slight indentations of the jaw die, and these indentations appear regularly and continuously. In order to smooth these indentations, the second coating of hot melt adhesive is designed before the extruder. As a result, the smooth aluminum sleeve and the outer sheath are tightly integrated, and no bowing or wrinkling occurs during cable bending, winding and construction, ensuring the appearance quality of the cable; the high-voltage cable design uses a smooth aluminum sleeve coated with hot melt adhesive, so that the semi-conductive buffer layer and the inner surface of the smooth aluminum sleeve are in close contact as a whole. The electric field distribution is more uniform, avoiding local discharge on the insulating shielding surface; the smooth aluminum sleeve cable has a more compact structure, and the outer diameter is smaller than the wrinkled aluminum sleeve cable, realizing the lightweight design of the high-voltage cable.
[0019] 2. However, the first layer of aluminum sleeve coated with hot melt adhesive has solidified and cooled when it reaches the extruder. During the second coating, the hot melt adhesive and the solidified cold hot melt adhesive have not been completely fused. For this reason, a cable aluminum sleeve hot melt adhesive preheating device is designed before the second hot melt adhesive coating device, which is used to preheat the cable composite aluminum sleeve before the second hot melt adhesive coating, and heat the aluminum sleeve coated with hot melt adhesive for the first time, so that the hot melt adhesive on the surface of the aluminum sleeve is about to be hot-melted. When the composite aluminum sleeve with the hot melt adhesive on the surface in the hot melt state enters the second hot melt adhesive coating device, the temperatures of the two parts of the hot melt adhesive are close, and the two layers of hot melt adhesive are firmly fused, and then quickly enter the extruder, and then double-layer co-extrude the outer sheath and the conductive layer. .
[0020] The specific technical solutions and beneficial effects of the present invention will be described in detail in the following specific embodiments in conjunction with the accompanying drawings. BRIEF DESCRIPTION OF THE DRAWINGS
[0021] The present invention will be further described below in conjunction with the accompanying drawings and specific embodiments:
[0022] Figure 1 is a structural schematic diagram of a first hot melt adhesive coating device;
[0023] Figure 2 is a structural schematic diagram of a second hot melt adhesive coating device;
[0024] Figure 3 This is a schematic diagram of the structure of the hot melt adhesive preheating device. DETAILED DESCRIPTION
[0025] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, rather than all the embodiments. The following description of at least one exemplary embodiment is actually only illustrative and is by no means intended to limit the present invention and its application or use. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0026] Those skilled in the art will appreciate that, in the absence of conflict, the features in the following embodiments and implementations may be combined with each other.
[0027] In the present invention, unless otherwise clearly specified and limited, the terms "installation", "connection", "fixation" and the like should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection, or it can be an indirect connection through an intermediate medium, or it can be the internal communication of two components. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.
[0028] In addition, the terms "first" and "second" are used for descriptive purposes only and should not be understood as indicating or implying relative importance or implicitly indicating the number of the indicated technical features. Therefore, a feature defined as "first" or "second" may explicitly or implicitly include one or more of the features. In the description of the present invention, unless otherwise specified, "plurality" means two or more, unless otherwise clearly specified.
[0029] Embodiment 1
[0030] like Figure 1 and Figure 2 As shown, a hot melt adhesive coating device for a composite smooth aluminum sheathed high voltage cable comprises a argon arc welding production line and an extruder. The argon arc welding production line comprises a welding gun part and a traction part, and also comprises two hot melt adhesive coating devices 1, namely:
[0031] The first hot melt adhesive coating device is arranged between the welding gun part and the pulling part, and comprises a hot melt adhesive groove 11, a glue blocking die 12, a drawing die 14, and an electric heating temperature control component 13. The glue blocking die and the drawing die are arranged on two opposite side walls of the hot melt adhesive groove. The hot melt adhesive groove is filled with hot melt adhesive particles, which are heated by the electric heating temperature control component to turn the hot melt adhesive particles into liquid and completely immerse the aluminum sleeve. The aluminum sleeve enters the first hot melt adhesive coating device for the drawing process and is coated with hot melt adhesive for the first time;
[0032] The second hot melt adhesive coating device is arranged at the front side of the extruder inlet, and includes a hot melt adhesive groove 11, a glue blocking mold 12, a coating mold 15, and an electric heating temperature control component 13. The glue blocking mold and the coating mold are arranged on two opposite side walls of the hot melt adhesive groove. The hot melt adhesive groove is filled with hot melt adhesive particles, which are heated by the electric heating temperature control component to turn the hot melt adhesive particles into liquid and completely immerse the aluminum sleeve. The aluminum sleeve enters the second hot melt adhesive coating device for the second hot melt adhesive coating. The designed smooth aluminum sleeve cable hot melt adhesive coating device is composed of two parts.
[0033] The first hot melt adhesive coating device is installed in the middle of the welding gun part and the jaw-type traction part of the argon arc welding production line, and enters the drawing process immediately after the welding of the aluminum sleeve is completed. According to the properties of the aluminum sleeve, the shrinkage of the aluminum sleeve during drawing generally cannot exceed 8%, and the shrinkage rate should be as small as possible. Due to the characteristics of welding, the inner diameter of the welded pipe is more than 5mm larger than the cable core to ensure the welding quality and not burn the cable core. The smooth aluminum sleeve after drawing is tightly attached to the surface of the buffer layer of the insulating wire core. After the buffer layer is drawn and tightened by the aluminum sleeve, the gap between the insulating wire core and the aluminum sleeve is the thickness of the buffer layer after compression. Because the buffer layer is composed of fluffy cotton and carbon black, although the thickness of the thermal expansion coefficient of the insulating layer is still left in the middle, it can still ensure that the buffer layer is in close contact with the inner surface of the aluminum sleeve after drawing.
[0034] In order to ensure that the surface of the aluminum sleeve is smooth and round after drawing, hot melt adhesive particles are poured into the hot melt adhesive tank, and the hot melt adhesive particles are heated to become liquid. The amount of liquid is sufficient as long as the aluminum sleeve is completely immersed. At this time, the liquid hot melt adhesive is used as a lubricant during drawing. After passing through the aluminum sleeve drawing die, a thin layer of hot melt adhesive is coated on the surface of the aluminum sleeve, with a thickness of about 0.1 to 0.2 mm. The smooth drawing sleeve coated with hot melt adhesive is transported to the die mouth of the extruder through a jaw-type traction machine. This is the function of the first part of the design of the hot melt adhesive coating device.
[0035] However, when the smooth aluminum sleeve coated with hot-melt adhesive is transported to the die mouth of the extruder through the jaw-type traction machine, the hot-melt adhesive on the surface of the aluminum sleeve has begun to solidify. At this time, if it enters the extruder directly, the extruded outer sheath and the aluminum sleeve are still not completely bonded. Because the hot-melt adhesive solidifies and cools when entering the extruder head, the outer sheath and the aluminum sleeve are still not completely bonded into a whole. In this way, after the finished cable is wound up and put on the coil, the inner surface of the cable may still have the phenomenon of sheath arching or wrinkling.
[0036] For this purpose, the second part of the hot melt adhesive coating device is designed in front of the extruder. This device is not much different from the first part, except that the drawing die is changed into a coating die. The diameter of the drawing die is smaller than that of the coating die, and the inner hole of the drawing die is trumpet-shaped. It is mainly used to draw and reduce the diameter of the aluminum sleeve after welding, so that the aluminum sleeve is evenly attached to the surface of the cable buffer layer; while the diameter of the coating die is larger than that of the drawing die, so that the thickness of the hot melt adhesive coated on the surface of the aluminum sleeve after drawing is uniform and the surface is smooth.
[0037] The second hot-melt adhesive coating device is mainly used to coat the composite smooth aluminum sleeve that has been coated with hot-melt adhesive with a thin layer of hot-melt adhesive, with a thickness of about 0.1 to 0.3 mm, before passing through the extruder. The purpose of designing to coat the hot-melt adhesive twice is that after the composite aluminum sleeve that has been coated with hot-melt adhesive for the first time passes through the jaw-type traction machine, slight indentations of the jaw die appear on the surface of the hot-melt adhesive. These indentations appear regularly and continuously. In order to smooth these indentations, it is designed to coat the hot-melt adhesive for the second time before the extruder.
[0038] However, the first layer of aluminum sleeve coated with hot melt adhesive had already solidified and cooled when it arrived at the extruder. During the second coating, the hot hot melt adhesive and the solidified cold hot melt adhesive were not completely fused.
[0039] For this purpose, a cable aluminum sheath hot melt adhesive preheating device is designed before the second part of the hot melt adhesive coating device, which is used to preheat the cable composite aluminum sheath before the second coating of the hot melt adhesive, and heat the aluminum sheath coated with the hot melt adhesive for the first time, so that the hot melt adhesive on the surface of the aluminum sheath is in a state of being about to be hot-melted. When the composite aluminum sheath with the hot melt adhesive on the surface in a hot-melt state enters the second part of the hot melt adhesive coating device, the temperatures of the two parts of the hot melt adhesive are close, the two layers of coated hot melt adhesive are firmly fused together, and then quickly enter the extruder, and then double-layer co-extruded outer sheath and conductive layer.
[0040] like Figure 3 As shown, the designed cable aluminum sleeve hot melt adhesive preheating device includes a bracket and four thermoplastic air guns, the bracket is arranged on the base, and the thermoplastic air gun is arranged on the bracket. The hot air from the air outlet of each thermoplastic air gun is blown to the surface of the composite smooth aluminum sleeve. The composite smooth aluminum sleeve passes through the point where the hot air converges, and the four thermoplastic air guns blow hot air to preheat the composite smooth aluminum sleeve at the same time, so as to prevent the hot air of one thermoplastic air gun from failing to preheat the surface of the aluminum sleeve evenly. The four thermoplastic air guns are arranged on the bracket at equal intervals along the bracket, and the hot air from each thermoplastic air gun blows to the cable passing through the center of the circular bracket. The circular bracket can withstand large external forces without deformation, thereby ensuring the working quality of the preheating device. The four thermoplastic air guns are respectively arranged at the midpoints of the four sides of the bracket, and the air outlet direction of each thermoplastic air gun is perpendicular to the side of the bracket where the thermoplastic air gun is located, and the hot air of each thermoplastic air gun is blown to the surface of the composite smooth aluminum sleeve. After trial production, the temperature is controlled at about 100°C, and the best time is when the hot air blows to the hot melt adhesive close to the hot melt state. The square bracket can also ensure that the aluminum sheath of the composite cable passing through it is heated evenly. At the same time, the square bracket is easy to process and has low production cost. The base includes a telescopic rod, and the bracket is set on the telescopic rod of the base. The telescopic rod adjusts the height of the bracket. The height of the base can be adjusted to change the position of the hot air convergence point, which can meet the needs of the outer diameter circumference of cables of different production specifications.
[0041] Embodiment 2
[0042] A composite smooth aluminum sheath high voltage cable hot melt adhesive coating process, using a composite smooth aluminum sheath high voltage cable hot melt adhesive coating device in Example 1 for coating,
[0043] The designed new process flow of coating hot melt adhesive: cable core wrapped with buffer layer→→welding aluminum sheath→→drawing aluminum sheath (coating hot melt adhesive for the first time at the same time)→→preheating of composite aluminum sheath→→coating hot melt adhesive for the second time→double-layer co-extrusion of outer sheath conductive layer→→water tank cooling→→winding up the finished product.
[0044] This new process is to release the cable core wrapped with buffer layer from the pay-off frame, and after aluminum sleeve welding, enter the aluminum sleeve drawing process and apply the hot melt adhesive for the first time. These two steps are carried out simultaneously, and then the composite aluminum sleeve enters the hot melt adhesive preheating device, which is used to preheat the cable aluminum sleeve before the second hot melt adhesive coating, and heat the aluminum sleeve coated with hot melt adhesive for the first time, so that the hot melt adhesive on the surface of the aluminum sleeve is in a state of about to be hot-melted. When the composite aluminum sleeve with hot melt adhesive on the surface in a hot-melt state enters the second part of the hot melt adhesive coating device, the temperature of the two parts of the hot melt adhesive is close, and the two layers of hot melt adhesive are fused together, and then quickly enter the extruder, and then the outer sheath and the conductive layer are double-layer co-extruded. Using the excellent adhesion of hot melt adhesive, the outer sheath, conductive layer and aluminum sleeve are firmly bonded together to form a whole, and then cooled in a water tank, so that the hot melt adhesive layer coated on the aluminum sleeve and the outer sheath are cooled together. After cooling and solidification, the cable passes through the water tank and is pulled by the traction machine and rolled into the take-up drum. At this time, when the cable is bent and reeled in, the outer sheath has the characteristics of large elastic modulus and large bending shrinkage, so the outer sheath will not bend or wrinkled, ensuring the appearance quality of the cable.
[0045] The above is only a specific embodiment of the present invention, but the protection scope of the present invention is not limited thereto. Those skilled in the art should understand that the present invention includes but is not limited to the contents described in the above specific embodiments. Any modification that does not deviate from the functional and structural principles of the present invention will be included in the scope of the claims.
Claims
1. A hot melt adhesive coating device for a composite smooth aluminum sheathed high voltage cable, comprising a argon arc welding production line and an extruder, wherein the argon arc welding production line comprises a welding gun part and a traction part, characterized in that: Also includes: The first hot melt adhesive coating device is arranged between the welding gun part and the pulling part, and comprises a hot melt adhesive groove, an adhesive blocking die, a drawing die, and an electric heating temperature control component. The adhesive blocking die and the drawing die are arranged on two opposite side walls of the hot melt adhesive groove. The hot melt adhesive groove is filled with hot melt adhesive particles, which are heated by the electric heating temperature control component to turn the hot melt adhesive particles into liquid and completely immerse the aluminum sleeve. The aluminum sleeve enters the first hot melt adhesive coating device to perform a drawing process and is coated with hot melt adhesive for the first time at the same time; The second hot melt adhesive coating device is arranged at the front side of the extruder inlet, and includes a hot melt adhesive groove, a glue blocking mold, a coating mold, and an electric heating temperature control component. The glue blocking mold and the coating mold are arranged on two opposite side walls of the hot melt adhesive groove. The hot melt adhesive groove is filled with hot melt adhesive particles. The hot melt adhesive particles are heated by the electric heating temperature control component to become liquid and completely immerse the aluminum sleeve. The aluminum sleeve enters the second hot melt adhesive coating device for a second coating of hot melt adhesive.
2. The hot melt adhesive coating device for composite smooth aluminum sheathed high voltage cable according to claim 1 is characterized in that: A hot melt adhesive preheating device is provided before the second hot melt adhesive coating device, which is used to preheat the hot melt adhesive on the surface of the cable composite aluminum sheath before the second hot melt adhesive coating, so that the hot melt adhesive on the surface of the composite aluminum sheath is in a state of being about to be hot-melted.
3. The hot melt adhesive coating device for composite smooth aluminum sheathed high voltage cable according to claim 2 is characterized in that: The hot melt adhesive preheating device comprises an annular bracket and thermoplastic air guns uniformly distributed along the circumference of the annular bracket.
4. The hot melt adhesive coating device for composite smooth aluminum sheathed high voltage cable according to claim 3 is characterized in that: The hot melt adhesive preheating device also includes a base, the base is connected to a telescopic rod, the annular bracket is connected to the telescopic rod, and the height of the annular bracket is adjusted by the telescopic rod.
5. A hot melt adhesive coating device for a composite smooth aluminum sheathed high voltage cable according to claim 3 or 4, characterized in that: The annular bracket is square, and four thermoplastic air guns are respectively installed at the midpoints of the four sides of the annular bracket.
6. The hot melt adhesive coating device for composite smooth aluminum sheathed high voltage cable according to claim 1 is characterized in that: The hot melt adhesive groove is rectangular, and the adhesive blocking mold and the drawing mold or the coating mold are arranged on the side walls on both sides of the width of the hot melt adhesive groove.
7. A method for coating a composite smooth aluminum sheathed high-voltage cable with hot melt adhesive, using a composite smooth aluminum sheathed high-voltage cable hot melt adhesive coating device as claimed in any one of claims 1 to 6 for coating, characterized in that: After the aluminum sheath is welded on the argon arc welding production line, the composite aluminum sheath enters the first hot melt adhesive coating device for the drawing process and the first coating of hot melt adhesive is carried out at the same time, and then the composite aluminum sheath enters the hot melt adhesive preheating device for preheating the cable aluminum sheath, heating the aluminum sheath coated with hot melt adhesive for the first time, so that the hot melt adhesive on the surface of the aluminum sheath is in a state of about to be hot-melted. When the composite aluminum sheath with the hot melt adhesive on the surface in a hot-melt state enters the second hot melt adhesive coating device, the temperatures of the two parts of the hot melt adhesive are close, and the two layers of coated hot melt adhesive are fused with each other, and then enter the extruder for double-layer co-extrusion of the outer sheath and the conductive layer.
8. The method for hot melt adhesive coating of a composite smooth aluminum sheathed high voltage cable according to claim 7, characterized in that: The thickness of the hot melt adhesive coated by the second hot melt adhesive coating device is 0.1 to 0.3 mm.
9. The method for hot melt adhesive coating of a composite smooth aluminum sheathed high voltage cable according to claim 7, characterized in that: The temperature difference between the two parts of the hot melt adhesive is controlled at ±1°C.
10. A method for coating hot melt adhesive on a composite smooth aluminum sheathed high voltage cable according to claim 7, characterized in that: The temperature of the hot air blown out by the thermoplastic air gun in the hot melt adhesive preheating device is controlled at 100+2℃.