End wall thickness measurement method and system based on spiral movement of steel pipe
By using a combined system of laser displacement combined probe and spiral traveling drive device in steel pipe inspection, the problems of low accuracy and low efficiency of traditional wall thickness detection are solved, and high-precision and fast wall thickness measurement is achieved, which is suitable for high temperature and high speed. environment.
Patent Information
- Application Number
- CN201911416969.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2019-12-31
- Publication Date
- 2024-10-18
- Estimated Expiration
- 2039-12-31
AI Technical Summary
Existing steel pipe wall thickness detection methods have problems such as low detection accuracy, low efficiency and poor environmental adaptability. Especially under high temperature and high speed detection conditions, traditional methods are difficult to achieve high precision and rapid measurement.
A laser displacement combined probe system based on the spiral travel of steel pipes is used, including single-point and 2D line laser displacement sensors. Through the non-contact measurement principle, combined with the steel pipe spiral travel drive device and travel following device, the laser displacement sensor is used to measure the end wall of the steel pipe. Thickness, the actual wall thickness is calculated.
It achieves high-precision wall thickness detection, with dynamic thickness measurement accuracy reaching ±0.1mm. It is suitable for high temperature environments, has fast detection speed, is simple and portable, and is suitable for steel pipes of various diameters and lengths.
Smart Images

Figure CN110906874B_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the field of steel pipe end wall thickness detection, and in particular to a method for measuring the wall thickness of a steel pipe end by using a combined probe with a single-point and line laser displacement sensors when the steel pipe is spirally moving, and a corresponding measuring system. Background Art
[0002] Due to the particularity of the manufacturing process (hot rolling), the wall thickness of seamless steel pipes is prone to unevenness in the circumferential direction of the steel pipes. According to national standards, steel pipes must undergo 100% quality inspection before leaving the factory. Since seamless steel pipes are currently priced by length instead of weight, precise control of the wall thickness of steel pipes within the lower deviation range can also improve the economic benefits of steel pipe manufacturers to a certain extent. In addition, the evaluation of the wall thickness of steel pipes can also monitor the working conditions of the rolling mill. For example, when the rolling mill is eccentric, the wall thickness of the processed steel pipe will be uneven. In summary, the wall thickness detection of steel pipe ends has very important social benefits and economic value.
[0003] The traditional method of measuring the wall thickness of steel pipes is mainly to use tools such as calipers for manual inspection. This type of mechanical manual measurement has many disadvantages, such as high labor intensity, large manual errors, low detection efficiency, and difficulty in measuring internal dimensions. At present, the commonly used methods for automatic thickness measurement of steel pipes are electromagnetic method, ultrasonic method and ray method. The electromagnetic method mainly relies on the principle that the change in the wall thickness of the workpiece causes the change in magnetic flux to complete the measurement of the wall thickness of the steel pipe. This method based on relative measurement requires first giving a reference thickness value, and then comparing the measured value with the reference value to obtain an estimated thickness. Therefore, the measurement error is large, and generally only a wall thickness of <12mm can be detected. In comparison, the ultrasonic pulse reflection method can directly measure the wall thickness value, which is usually achieved by using a single straight probe to send and receive or two oblique probes to send and receive. Therefore, the ultrasonic method is the most widely used wall thickness measurement method at present, but the conventional ultrasonic method requires coupling agent and is a contact measurement with slow detection speed, so it is not suitable for high temperature and high speed detection, and the result of ultrasonic thickness measurement is greatly affected by the roughness of the workpiece surface; and for small diameter steel pipes, due to the large curvature, the accuracy of thickness measurement using ultrasonic method is not high. The wall thickness measurement method based on the ray method is too expensive and has too high requirements on the environment. Therefore, it is of great significance to develop a steel pipe wall thickness measurement system with fast detection speed, high detection accuracy and strong environmental adaptability. Summary of the invention
[0004] The purpose of the present invention is to overcome the shortcomings of the prior art and provide a device for measuring the wall thickness of a steel pipe end based on spiral movement, and a corresponding measuring method; based on the principle of non-contact measurement, the present invention solves the problems of low detection accuracy, low efficiency and high cost of purchased equipment in the existing wall thickness detection method. The technical solution adopted by the present invention is:
[0005] The embodiment of the present invention provides a terminal wall thickness measurement system based on the spiral movement of a steel pipe, comprising a laser displacement combined probe, a steel pipe spiral movement driving device, and a steel pipe movement following device;
[0006] The steel pipe spiral travel driving device is used to carry and drive the steel pipe to be tested to spirally travel;
[0007] The laser displacement combined probe is installed on the steel pipe travel following device, and includes a single-point laser displacement sensor and a 2D line laser displacement sensor;
[0008] The single-point laser displacement sensor and the 2D line laser displacement sensor are installed on the same straight line and configured at one end of the steel pipe to be measured; the single-point laser displacement sensor is located on the upper left of the 2D line laser displacement sensor, and the same straight line is inclined at an angle α to the vertical direction;
[0009] The steel pipe following device is used to drive the laser displacement combined measuring head to follow the steel pipe to be measured during measurement.
[0010] Furthermore, the steel pipe advancing and following device comprises an upper wedge block, a lower wedge block, an upper fixed plate, a lower fixed plate, and a linear slide;
[0011] The linear slide is installed on the frame; the lower fixed plate is installed on the linear slide, and the upper fixed plate is fixed on the side of the lower fixed plate away from the steel pipe spiral travel drive device; the single-point laser displacement sensor is installed on the upper fixed plate through an upper wedge block, and the 2D line laser displacement sensor is installed on the lower fixed plate through a lower wedge block, and the straight line where the two laser displacement sensors are installed concentrically is inclined at an angle α to the vertical direction.
[0012] More preferably, a workpiece hole is opened on the upper fixing plate, so that the steel pipe to be tested can move forward after the testing is completed.
[0013] Furthermore, a photoelectric sensor is also provided on the frame or the linear slide.
[0014] Furthermore, the steel pipe spiral advancement driving device adopts a roller driving device, and there is a skew angle between the rollers in the roller driving device and the axial direction of the steel pipe to be measured.
[0015] The embodiment of the present invention further provides a method for measuring the wall thickness of an end of a steel pipe based on spiral movement, comprising:
[0016] When the steel pipe to be tested spirally moves to the detection area at the set speed, the photoelectric sensor is triggered, and the PLC controls the laser displacement combination probe to start measuring the wall thickness of the end of the steel pipe to be tested; at the same time, the steel pipe moving following device drives the laser displacement combination probe to do a following movement of at least one pitch;
[0017] The distance to the inner wall of the steel pipe to be measured by the single-point laser displacement sensor is t1;
[0018] The Z-axis distance data of the central pixel point of the 2D line laser displacement sensor is t2, and the minimum Z-axis distance data of the 2D line laser displacement sensor is t3; the Z-axis direction of the 2D line laser displacement sensor is the direction of the 2D line laser displacement sensor toward the single-point laser displacement sensor;
[0019] The distance between the single-point laser displacement sensor and the 2D line laser displacement sensor is T;
[0020] When the steel pipe to be tested is stationary, its theoretical wall thickness d is calculated using formula (2);
[0021] d=(T-t1-t2)cosα (2)
[0022] The Z-axis data offset h of the center pixel of the 2D line laser displacement sensor; the horizontal offset X of the swing;
[0023] h=(t2-t3)cosα (3)
[0024] R1=X1+h (4)
[0025] (R1) 2 =X 2 +(X1) 2 (5)
[0026] X2=X1-d (6)
[0027] (R2) 2 =(X2) 2 +X 2 (7)
[0028] X1 and X2 are intermediate parameters. The outer radius R1 and X1 of the steel pipe to be tested are calculated by combining formulas (4) and (5). The inner radius R2 and X2 of the steel pipe to be tested are calculated by combining formulas (6) and (7).
[0029] t=R1-R2 (8)
[0030] Finally, the actual wall thickness t of the steel pipe to be tested is calculated by formula (8).
[0031] The advantages of the present invention are:
[0032] 1) The non-contact measuring mechanism and measuring method can be applied to the end wall thickness detection of high-temperature steel pipes, and have strong environmental adaptability.
[0033] 2) Fast detection speed, high precision, dynamic thickness measurement accuracy reaches ±0.1mm.
[0034] 3) Compared with the traditional wall thickness measurement method, no coupling agent is required and the device is simple and portable.
[0035] 4) It can measure a variety of steel pipes with different diameters and lengths, with great flexibility. BRIEF DESCRIPTION OF THE DRAWINGS
[0036] Figure 1 Schematic diagram of the structure of the measurement system according to an embodiment of the present invention.
[0037] Figure 2 Schematic diagram of the static measurement principle of an embodiment of the present invention.
[0038] Figure 3 Schematic diagram of the dynamic measurement principle of an embodiment of the present invention. DETAILED DESCRIPTION
[0039] The present invention will be further described below in conjunction with specific drawings and embodiments.
[0040] The embodiment of the present invention provides a terminal wall thickness measurement system based on the spiral movement of a steel pipe, comprising a laser displacement combined probe, a steel pipe spiral movement driving device, and a steel pipe movement following device;
[0041] The steel pipe spiral travel driving device is used to carry and drive the steel pipe 8 to be tested to travel spirally;
[0042] The laser displacement combined probe is installed on the steel pipe travel following device, and includes a single-point laser displacement sensor 1 and a 2D line laser displacement sensor 2;
[0043] The single-point laser displacement sensor 1 and the 2D line laser displacement sensor 2 are installed on the same straight line and configured at one end of the steel pipe 8 to be measured; the single-point laser displacement sensor 1 is located at the upper left of the 2D line laser displacement sensor 2, and the same straight line is inclined at an angle α to the vertical direction; the smaller the inclination angle, the higher the measurement accuracy, but if the angle is too small, the laser line will not fall on the inner wall of the steel pipe wall thickness measurement part. The specific installation angle α should take into account the outer diameter D of the steel pipe to be measured with the smallest diameter and the axial measurement range L of its end head;
[0044]
[0045] The laser line emitted by the single-point laser displacement sensor 1 is a laser point when it reaches the inner wall of the steel pipe to be measured;
[0046] The laser line emitted by the 2D line laser displacement sensor 2 is an arc when it reaches the outer wall of the steel pipe to be measured;
[0047] The measurement system in the embodiment of the present invention is suitable for steel pipes with a diameter of 60 to 180 mm, so the range selected by the single-point laser displacement sensor 1 is 200 mm, and the range selected by the 2D line laser displacement sensor 2 is 20 mm;
[0048] The steel pipe following device is used to drive the laser displacement combined probe to follow the steel pipe to be measured during measurement;
[0049] In some embodiments, the steel pipe spiral advancing driving device may adopt a roller driving device 9, and the rollers in the roller driving device 9 are axially inclined at a certain angle to the steel pipe 8 to be tested, so that the steel pipe 8 to be tested can be driven to move forward in a spiral manner;
[0050] In some embodiments, the steel pipe travel following device includes an upper wedge block 3, a lower wedge block 4, an upper fixing plate 5, a lower fixing plate 6, and a linear slide 7;
[0051] The linear slide 7 is mounted on the frame 10; the lower fixed plate 6 is mounted on the linear slide 7, and the upper fixed plate 5 is fixed on the side of the lower fixed plate 6 away from the steel pipe spiral travel drive device; the single-point laser displacement sensor 1 is mounted on the upper fixed plate 5 through the upper wedge block 3, and the 2D line laser displacement sensor 2 is mounted on the lower fixed plate 6 through the lower wedge block 4, and the straight line where the two laser displacement sensors are mounted in the center is inclined at an angle α to the vertical direction;
[0052] A photoelectric sensor may also be provided on the frame 10 or the linear slide 7 to detect whether the steel pipe 8 to be tested has moved to the detection position;
[0053] Preferably, a workpiece hole 501 is opened on the upper fixing plate 5, so that the steel pipe 8 to be tested can move forward after the test is completed, pass through the workpiece hole 501, and then be transported by other transport mechanisms;
[0054] The embodiment of the present invention further provides a method for measuring the wall thickness of an end of a steel pipe based on spiral movement, comprising:
[0055] When the steel pipe 8 to be tested spirally moves to the detection area at a set speed (for example, 2.5 m / s), the photoelectric sensor is triggered, and the PLC controls the laser displacement combined probe to start measuring the wall thickness of the end of the steel pipe 8 to be tested; at the same time, the steel pipe moving following device drives the laser displacement combined probe to perform a following movement of at least one pitch;
[0056] The distance to the inner wall of the steel pipe 8 to be measured measured by the single-point laser displacement sensor 1 is t1;
[0057] The Z-axis distance data of the central pixel point of the 2D line laser displacement sensor 2 is t2, and the minimum Z-axis distance data of the 2D line laser displacement sensor 2 is t3 (caused by the vibration of the steel pipe); the Z-axis direction of the 2D line laser displacement sensor 2 is the direction of the 2D line laser displacement sensor 2 toward the single-point laser displacement sensor 1;
[0058] The distance between the single-point laser displacement sensor 1 and the 2D line laser displacement sensor 2 is T;
[0059] When the steel pipe to be tested is stationary, its theoretical wall thickness d can be calculated using formula (2);
[0060] d=(T-t1-t2)cosα (2)
[0061] Since the steel pipe 8 to be tested will jump up and down and swing left and right when it moves in a spiral, the theoretical wall thickness d calculated directly using formula (2) will be larger than the actual wall thickness value;
[0062] The Z-axis data offset h of the center pixel of the 2D line laser displacement sensor 2; the horizontal offset X of the swing; Figure 3 As shown,
[0063] h=(t2-t3)cosα (3)
[0064] R1=X1+h (4)
[0065] (R1) 2 =X 2 +(X1) 2 (5)
[0066] X2=X1-d (6)
[0067] (R2) 2 =(X2) 2 +X 2 (7)
[0068] X1 and X2 are intermediate parameters. Combining formulas (4) and (5) can calculate the outer radius R1 and X1 of the steel pipe to be tested. Combining formulas (6) and (7) can calculate the inner radius R2 and X2 of the steel pipe to be tested.
[0069] t=R1-R2 (8)
[0070] Finally, the actual wall thickness t of the steel pipe to be tested is calculated by formula (8).
[0071] Since the steel pipe to be tested moves in a spiral, as the steel pipe to be tested rotates, full circumferential coverage detection of the steel pipe end can be achieved, and this method effectively overcomes the measurement error caused by the up and down bouncing and left and right swinging of the steel pipe under high-speed movement.
[0072] After the measurement is completed, the steel pipe 8 to be measured passes through the workpiece hole 501 of the upper fixing plate 5 and is then transferred away by other conveying mechanisms.
[0073] Finally, it should be noted that the above specific implementation methods are only used to illustrate the technical solution of the present invention rather than to limit it. Although the present invention has been described in detail with reference to examples, those skilled in the art should understand that the technical solution of the present invention can be modified or replaced by equivalents without departing from the spirit and scope of the technical solution of the present invention, which should be included in the scope of the claims of the present invention.
Claims
1. A system for measuring the end wall thickness of a steel pipe based on spiral movement, characterized in that: It includes a laser displacement combined measuring head, a steel pipe spiral travel driving device, and a steel pipe travel following device; The steel pipe spiral advancement driving device is used to carry and drive the steel pipe (8) to be tested to spirally advance; The laser displacement combined measuring head is installed on the steel pipe travel following device, and comprises a single-point laser displacement sensor (1) and a 2D line laser displacement sensor (2); The single-point laser displacement sensor (1) and the 2D line laser displacement sensor (2) are installed on the same straight line and are arranged at one end of the steel pipe (8) to be measured; the single-point laser displacement sensor (1) is located on the upper left of the 2D line laser displacement sensor (2), and the same straight line is inclined at an angle α to the vertical direction; The steel pipe following device is used to drive the laser displacement combined probe to follow the steel pipe to be measured during measurement; The steel pipe advancing and following device comprises an upper wedge block (3), a lower wedge block (4), an upper fixing plate (5), a lower fixing plate (6), and a linear slide (7); The linear slide (7) is mounted on a frame (10); a lower fixed plate (6) is mounted on the linear slide (7); an upper fixed plate (5) is fixed on a side of the lower fixed plate (6) away from the steel pipe spiral travel drive device; a single-point laser displacement sensor (1) is mounted on the upper fixed plate (5) via an upper wedge block (3); a 2D line laser displacement sensor (2) is mounted on the lower fixed plate (6) via a lower wedge block (4); and the straight line on which the two laser displacement sensors are mounted in a concentric manner forms an inclination angle α with the vertical direction.
2. The end wall thickness measurement system based on spiral movement of steel pipe according to claim 1 is characterized in that: A workpiece hole (501) is formed on the upper fixing plate (5) for the steel pipe (8) to be tested to move forward after the test is completed.
3. The end wall thickness measurement system based on spiral movement of steel pipe according to claim 1, characterized in that: A photoelectric sensor is also provided on the frame (10) or the linear slide (7).
4. The end wall thickness measurement system based on spiral movement of steel pipe according to any one of claims 1 to 3, characterized in that: The steel pipe spiral advancing driving device adopts a roller driving device (9), and there is an axial deviation angle between the rollers in the roller driving device (9) and the steel pipe (8) to be measured.
5. A method for measuring the wall thickness of an end of a steel pipe based on spiral movement, applicable to a system for measuring the wall thickness of an end of a steel pipe based on spiral movement as claimed in any one of claims 1 to 4, characterized in that: include: When the steel pipe to be tested spirally moves to the detection area at the set speed, the PLC controls the laser displacement combined probe to start measuring the wall thickness of the end of the steel pipe to be tested; at the same time, the steel pipe moving following device drives the laser displacement combined probe to do a following movement of at least one pitch; The distance to the inner wall of the steel pipe to be measured by the single-point laser displacement sensor is t1; The Z-axis distance data of the central pixel point of the 2D line laser displacement sensor is t2, and the minimum Z-axis distance data of the 2D line laser displacement sensor is t3; the Z-axis direction of the 2D line laser displacement sensor is the direction of the 2D line laser displacement sensor toward the single-point laser displacement sensor; The distance between the single-point laser displacement sensor and the 2D line laser displacement sensor is T; When the steel pipe to be tested is stationary, its theoretical wall thickness d is calculated using formula (2); d=(T-t1-t2)cosα (2) The Z-axis data offset h of the center pixel of the 2D line laser displacement sensor; the horizontal offset X of the swing; h=(t2-t3)cosα (3) R1=X1+h (4) (R1) 2 =X 2 +(X1) 2 (5) X2=X1-d (6) (R2) 2 =(X2) 2 +X 2 (7) X1 and X2 are intermediate parameters. The outer radius R1 and X1 of the steel pipe to be tested are calculated by combining formulas (4) and (5). The inner radius R2 and X2 of the steel pipe to be tested are calculated by combining formulas (6) and (7). t=R1-R2 (8) Finally, the actual wall thickness t of the steel pipe to be tested is calculated by formula (8).
Citation Information
Patent Citations
End wall thickness measuring system based on steel pipe spiral advancing
CN211121076U