An improved fiber braided winding pultruded pipe injection mold
By introducing a tapered injection section, overflow hole, PLC controller and constant temperature cavity into the fiber braided winding pultrusion pipe injection mold, the problem of excess resin inflow is solved and the automatic pressure control and injection effect of the injection mold are realized. improvement.
Patent Information
- Application Number
- CN202010588028.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2020-06-24
- Publication Date
- 2024-10-22
- Estimated Expiration
- 2040-06-24
AI Technical Summary
In the existing fiber braided winding pultruded pipe glue injection mold, excess resin cannot flow into the overflow section in time, resulting in poor glue injection effect or failure of the guide pillar.
An improved injection mold is designed, including a tapered injection section and an overflow hole. It combines a PLC controller, a pressure sensor and a solenoid valve to realize automatic control of the internal pressure of the injection mold cavity and set it in the mold. Constant temperature chamber to ensure the glue injection effect.
The design of the tapered injection section and overflow hole ensures that excess resin flows out smoothly and avoids injection failures; the cooperation of the PLC controller and the pressure sensor keeps the injection pressure within the normal range, improving injection efficiency and quality; constant temperature The cavity ensures the stability of the glue injection effect.
Smart Images

Figure CN111572065B_ABST
Abstract
Description
Technical Field
[0001] The invention relates to a glue injection mould, in particular to an improved fiber braided winding pultruded pipeline glue injection mould. Background Art
[0002] The utility model patent with authorization announcement number CN 209666321U is a glue injection mold for fiber braided pultruded pipes applied for by the applicant, comprising a mold body, the mold body having a glue injection mold cavity along its axis, the glue injection mold cavity comprising an inlet section, an overflow section, a glue injection section and an outlet section, the inlet section and the overflow section are both conical necking shapes, the inlet section and the overflow section are connected by a circular through hole section 1, an overflow hole is provided at the bottom of the large mouth end of the overflow section, the glue injection section is also conical necking shape, the glue injection section and the overflow section are connected by a circular through hole section 2, a glue injection hole is provided at the top of the large mouth end of the glue injection section, the outlet section is a circular through hole shape, the inner diameter of the circular through hole section 2 is equal to the inner diameter of the circular through hole section 1, but smaller than the inner diameter of the outlet section.
[0003] The above injection mold can prevent the resin from leaking and dripping from the injection mold, thus greatly saving resin raw materials. When the injection mold cavity is injected with glue, most of the resin flows along one side of the injection section, and a small part flows along the overflow section. The excess resin in the injection section flows in the opposite direction along the overflow section under the action of the tapered necking of the injection section. However, since the inner diameter of the circular through hole section 2 connecting the injection section and the overflow section is smaller than the front end of the injection section, it is easy to cause the excess resin to fail to flow into the overflow section in time, resulting in poor injection effect of the guide column or failure. To this end, we propose an improved fiber braided winding pultrusion pipe injection mold. Summary of the invention
[0004] The present invention provides an improved fiber braided winding pultruded pipe glue injection mold to solve the shortcomings that excess resin in the glue injection mold cannot flow into the overflow section in time, the guide column glue injection effect is poor or malfunction occurs, and the like.
[0005] The present invention adopts the following technical solution:
[0006] An improved fiber braided winding pultruded pipe injection mold, comprising a mold body, wherein the mold body has an injection mold cavity along its axis, the injection mold cavity comprises an inlet section, an injection section and an outlet section, the injection section forms a conical necking shape, a glue injection hole is provided at the large mouth end of the injection section, the large mouth end of the injection section is connected to the inlet section through a conical section, the front end of the conical section is a small mouth end, and the rear end is a large mouth end, the small mouth end of the injection section is connected to the outlet section, and an overflow hole is provided at the middle and rear ends of the injection section near its small mouth end.
[0007] Furthermore, the glue injection hole is connected to a glue injection device, and the glue injection device includes a glue injection tank, a glue injection pump and a glue injection tube. The glue injection tank is connected to the glue injection hole through the glue injection tube, and the glue injection pump is installed on the glue injection tube.
[0008] Furthermore, a pressure sensor is installed at the overflow hole, and the overflow hole is connected to a reflux pipe through a solenoid valve switch. The pressure sensor is respectively controlled and connected to the solenoid valve switch, and the reflux pipe is connected to the glue injection tank body.
[0009] Furthermore, the glue injection mold also includes a PLC controller, and the PLC controller is respectively connected to the glue injection pump, the pressure sensor and the solenoid valve switch through signal control.
[0010] Furthermore, the front end of the inlet section forms a conical expansion shape, and the rest of the section is a circular through hole shape. The outlet section is also a circular through hole shape, and the inner diameter of the outlet section is larger than the inner diameter of the circular through hole of the inlet section.
[0011] Furthermore, the length of the glue injection section is at least 450 mm.
[0012] Furthermore, a constant temperature cavity is provided in the mold body, and the constant temperature cavity is coated on the outside of the injection mold cavity.
[0013] Furthermore, the mold body consists of an upper template and a lower template, the upper template and the lower template are connected by fasteners, a glue injection groove is respectively opened at the lower part of the upper template and the upper part of the lower template, and the two glue injection grooves constitute the glue injection mold cavity.
[0014] From the above description of the structure of the present invention, it can be seen that compared with the prior art, the present invention has the following advantages:
[0015] 1. The injection mold of the invention has a tapered section between the inlet section and the injection section. The tapered section can limit the resin from flowing out to one end of the inlet section, and the overflow hole is arranged at the rear end of the injection section close to its small mouth end, so that excess resin liquid can flow along its flow direction and the forward direction of the core mold and flow out from the overflow hole, thereby preventing the occurrence of injection failure and ensuring the smooth progress of injection.
[0016] 2. The glue injection mold of the invention also includes a PLC controller, and is connected to the pressure sensor, the solenoid valve switch and the glue injection pump control, wherein the pressure sensor is arranged at the overflow hole, and is used to sense the pressure inside the glue injection mold cavity. The pressure sensor transmits the pressure sensing signal to the PLC controller. When the pressure is too high, the PLC controller controls the solenoid valve switch to open, discharges the excess resin inside, and reduces the pressure to within the normal glue injection pressure range; and when the pressure is too low, the PLC controller controls the glue injection pump to increase the injection amount, and increases the pressure inside the glue injection mold cavity to within the normal glue injection pressure range. Therefore, the glue injection mold of the present invention can realize the automatic control of the pressure inside the glue injection mold cavity, so that it is maintained within the normal glue injection pressure range, ensures the smooth progress of glue injection, and improves the glue injection efficiency and quality.
[0017] 3. The glue injection mold of the invention is provided with a constant temperature cavity to keep the inside of the glue injection cavity warm so that it is kept constant at about 15-20°C to ensure the glue injection effect. BRIEF DESCRIPTION OF THE DRAWINGS
[0018] Figure 1 It is the right side view of the present invention.
[0019] Figure 2 for Figure 1 Cross-sectional view along the AA direction.
[0020] Figure 3 It is the installation schematic diagram of the present invention. DETAILED DESCRIPTION
[0021] The specific implementation of the present invention is described below with reference to the accompanying drawings. In order to fully understand the present invention, many details are described below, but for those skilled in the art, the present invention can be implemented without these details. For well-known components, methods and processes, they are not described in detail below.
[0022] An improved fiber braided winding pultruded pipe injection mold, referring to Figure 1 and Figure 2 , including a mold body, the mold body is composed of an upper mold plate 10 and a lower mold plate 20, the upper mold plate 10 and the lower mold plate 20 are connected by fasteners, the lower part of the upper mold plate 10 and the upper part of the lower mold plate 20 are respectively provided with a glue injection groove 100, and the two glue injection grooves 100 are sealed and connected to form a glue injection mold cavity. A constant temperature cavity 200 is provided in the mold body, and the constant temperature cavity 200 is coated on the outside of the glue injection mold cavity to keep the inside of the glue injection mold cavity warm to keep it constant at about 15-20°C to ensure its glue injection effect.
[0023] Reference Figure 2The injection mold cavity includes an inlet section 31, an injection section 33 and an outlet section 35. The injection section 33 is formed into a tapered neck shape, and the length of the injection section 33 is at least 450 mm. A glue injection hole 331 is provided at the large end of the injection section 33. The large end of the injection section 33 is connected to the inlet section 31 through a tapered section 32. The front end of the tapered section 32 is a small end, and the rear end is a large end. The small end of the injection section 33 is connected to the outlet section 35. An overflow hole 332 is provided at the middle and rear end of the injection section 33 near its small end.
[0024] Reference Figure 2 The front end of the inlet section 31 forms a conical expansion shape, so that the core mold with the braided winding fiber can enter the injection mold cavity, and the rest of the part is a circular through hole. The end of the inlet section 31 is connected with the small end of the conical section, and the large end of the conical section 32 is connected with the large end of the injection section 33. The outlet section 35 is also a circular through hole, and the inner diameter of the outlet section 35 is slightly larger than the inner diameter of the circular through hole of the inlet section 31.
[0025] Reference Figure 3 The above-mentioned glue injection hole 331 is connected to a glue injection device, which includes a glue injection tank body 41, a glue injection pump 42 and a glue injection tube 43. The glue injection tank body 41 is connected to the glue injection hole 331 through the glue injection tube 43, and the glue injection pump 42 is installed on the glue injection tube 43.
[0026] Reference Figure 3 A pressure sensor 51 is installed at the overflow hole 332 , and the overflow hole 51 is connected to a reflux pipe 53 through a solenoid valve switch 52 . The pressure sensor 51 is respectively controlled and connected to the solenoid valve switch 52 , and the reflux pipe 53 is connected to the injection tank body 41 .
[0027] The glue injection mold of the present invention further includes a PLC controller 60, which is respectively connected to the glue injection pump 42, the pressure sensor 51 and the solenoid valve switch 52 through signal control. When the pressure is too high, the PLC controller 60 sends an opening signal to the solenoid valve switch 52, and the solenoid valve switch 52 opens after receiving the signal, discharges the excess resin inside, and reduces the pressure to within the normal glue injection pressure range; when the pressure is too low, the PLC controller 60 sends a signal to increase the glue injection amount to the glue injection pump 42, and the glue injection pump 42 increases the glue injection amount after receiving the signal, so that the pressure inside the glue injection mold cavity increases to within the normal glue injection pressure range, thereby realizing automatic control of the pressure inside the glue injection mold cavity.
[0028] The above is only a specific implementation of the present invention, but the design concept of the present invention is not limited thereto. Any non-substantial changes to the present invention using this concept shall be deemed as an infringement of the protection scope of the present invention.
Claims
1. An improved fiber braided winding pultruded pipe injection mold, comprising a mold body, the mold body is provided with an injection mold cavity along its axis, the injection mold cavity comprises an inlet section, an injection section and an outlet section, the injection section forms a conical necking shape, and a large end of the injection section is provided with an injection hole, characterized in that: The large mouth end of the injection section is connected to the inlet section through a tapered section, the front end of the tapered section is the small mouth end, and the rear end is the large mouth end, the small mouth end of the injection section is connected to the outlet section, and an overflow hole is provided at the middle and rear ends of the injection section near the small mouth end; the front end of the inlet section forms a tapered expansion shape, and the rest of the part is a circular through hole shape, the outlet section is also a circular through hole shape, and the inner diameter of the outlet section is larger than the inner diameter of the circular through hole of the inlet section; the injection hole is connected to a glue injection device, and the glue injection device includes a glue injection tank The invention relates to a body, a glue injection pump and a glue injection tube, wherein the glue injection tank body is connected to the glue injection hole through the glue injection tube, and the glue injection pump is installed on the glue injection tube; a pressure sensor is installed at the overflow hole, and the overflow hole is connected to a return pipe through a solenoid valve switch, the pressure sensor is respectively connected to the solenoid valve switch control, and the return pipe is connected to the glue injection tank body; and a PLC controller is also included, and the PLC controller is respectively connected to the glue injection pump, the pressure sensor and the solenoid valve switch through signal control.
2. An improved fiber braided winding pultruded pipe glue injection mold as claimed in claim 1, characterized in that: The length of the glue injection section is at least 450 mm.
3. An improved fiber braided winding pultruded pipe glue injection mold according to claim 1, characterized in that: A constant temperature cavity is arranged in the mold body, and the constant temperature cavity is covered on the outside of the injection mold cavity.
4. The improved fiber braiding winding pultrusion pipe injection mold according to claim 1, characterized in that: The mold body consists of an upper mold plate and a lower mold plate, the upper mold plate and the lower mold plate are connected by fasteners, a glue injection groove is respectively provided at the lower part of the upper mold plate and the upper part of the lower mold plate, and the two glue injection grooves constitute the glue injection mold cavity.