A reinforced chip exposed flip chip spherical array structure

By adding a sticky substance to the exposed flip-chip spherical array structure to protect the side walls of the chip and fixing a metal ring at the circuit board frame, the problem of balancing chip heat dissipation performance and warpage in the existing technology is solved, achieving efficient heat dissipation and preventing warpage. The effect of music.

CN111599770BActive Publication Date: 2024-10-11SILICONWARE TECH SUZHOU
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202010440250.2
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2020-05-22
Publication Date
2024-10-11
Estimated Expiration
2040-05-22

AI Technical Summary

Technical Problem

The existing chip-exposed structure has good heat dissipation performance but poor side protection and is easy to warp; the heat sink fixed structure has strong protection ability but poor heat dissipation performance, making it difficult to balance both.

Method used

Design a reinforced chip-exposed flip-chip spherical array structure. By adding a sticky substance around the chip to protect the side walls, and fixing a metal ring at the circuit board frame, it ensures that the chip can dissipate heat and is not prone to warping when exposed.

Benefits of technology

It is possible to enhance the protection ability of the chip sidewall without affecting the heat dissipation performance, reduce material warpage, and avoid chip damage at high temperatures.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN111599770B_ABST
    Figure CN111599770B_ABST
Patent Text Reader

Abstract

The present invention discloses a reinforced chip exposed flip-chip spherical array structure, which includes a chip, a circuit board, a metal connector, a first adhesive material, a second adhesive material, a third adhesive material, a fourth adhesive material, and a metal ring. The chip has two upper and lower surfaces. The upper surface of the chip is an exposed surface for contacting a heat sink. The lower surface of the chip is provided with at least one layer of circuit board. The chip and each layer of the circuit board are fixedly connected by the first adhesive material. The chip and each layer of the circuit board are interconnected by signals through metal connectors. A circle of second adhesive material is fixed around the first adhesive material. A certain gap is provided between the second adhesive material and the chip. The gap is filled by the third adhesive material. The four sides of the chip, the first adhesive material and the second adhesive material are fixedly connected by the third adhesive material. This technical solution can solve the problem that the two structures in the prior art have heat dissipation and product warping that cannot complement each other.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to a reinforced chip exposed flip-chip spherical array structure, which can be used in the technical field of semiconductor packaging. Background Art

[0002] There are two main types of existing product structures: one is the exposed chip structure, and the other is the fixed heat sink structure. The main purpose of both is to achieve heat dissipation performance and prevent material warping. The exposed chip structure has good heat dissipation performance, but poor side protection for the chip and large product warping. The fixed heat sink structure has good chip protection and good product warping control, but poor heat dissipation performance.

[0003] The exposed chip structure is directly exposed to the air through the upper surface and four sides of the chip, and the self-generated heat of the chip is directly dissipated without passing through the medium. It has good heat dissipation performance, but the side wall of the chip is not protected by solid materials and is easy to break and damage. Resin circuit boards are prone to deformation and warping at high temperatures without metal materials to fix them, which affects performance.

[0004] The surface of the chip in the heat sink fixed structure is connected to the metal sheet through an adhesive material. The heat of the chip is dissipated through the adhesive material and the metal sheet. The heat dissipation performance through the multi-layer medium is poor, but the chip and the resin circuit board are protected by the metal sheet. The chip is not easy to be damaged and is not easy to deform under high temperature conditions. Summary of the invention

[0005] The purpose of the present invention is to solve the above problems existing in the prior art and to provide a reinforced chip exposed flip chip ball array structure.

[0006] The object of the present invention is achieved by the following technical scheme: a reinforced chip exposed flip-chip spherical array structure, comprising a chip, a circuit board, a metal connector (3), a first adhesive substance, a second adhesive substance, a third adhesive substance, a fourth adhesive substance, a metal ring, and a solder ball. The chip has an upper and lower surface. The upper surface of the chip is an exposed surface for contacting with external substances. The lower surface of the chip is provided with at least one layer of circuit board. The chip and each layer of the circuit board are fixedly connected by the first adhesive substance. The chip and each layer of the circuit board are interconnected by signals through the metal connector. A circle of second adhesive substance is fixed around the first adhesive substance. A certain gap is provided between the second adhesive substance and the chip. The gap is filled with a third adhesive substance. The four sides of the chip, the first adhesive substance and the second adhesive substance are fixedly connected by the third adhesive substance. A circle of metal ring is provided around the outermost side of the circuit board. The metal ring is fixedly connected to the circuit board by the fourth adhesive substance. A solder ball is provided below the circuit board. The chip and the external signal are interconnected by the metal ball.

[0007] Preferably, the thickness of the chip is 100-800 um.

[0008] Preferably, the circuit board is a single-layer or multi-layer resin circuit board.

[0009] Preferably, the metal connecting piece is a columnar or spherical structure.

[0010] Preferably, the metal connecting piece is a metal bump or a metal ball.

[0011] Preferably, the metal bump is a tin bump, a copper bump, a gold bump, or a tin ball.

[0012] Preferably, the metal ball is a tin bump, a copper bump, a gold bump or a tin ball.

[0013] Preferably, the metal ring is made of copper or aluminum, and the surface is plated with nickel or chromium.

[0014] Preferably, the first adhesive material, the second adhesive material, the third adhesive material and the fourth adhesive material are all conductive or non-conductive adhesive materials.

[0015] Preferably, at least six solder balls are arranged in the gap below the circuit board.

[0016] The advantages of the technical solution of the present invention are mainly reflected in: based on the traditional design, this technical solution adds sticky material around the chip to protect the side walls of the chip from damage, so that the chip can ensure heat dissipation performance when exposed, while being protected from damage by collision in downstream processes. At the same time, a metal ring is fixed at the frame of the circuit board to reduce the warping of the entire material, thereby solving the problem of heat dissipation and warping that the existing technology cannot take into account at the same time. BRIEF DESCRIPTION OF THE DRAWINGS

[0017] Figure 1 It is a schematic diagram of a reinforced chip exposed flip-chip ball array structure of the present invention.

[0018] Figure 2 It is a schematic diagram of a reinforced chip exposed flip-chip ball array structure of the present invention.

[0019] Figure 3 The cross-sectional structure diagram of a reinforced chip exposed flip-chip spherical array structure of the present invention.

[0020] Reference numerals in the figure: 1---chip, 2---circuit board, 3---metal connecting piece, 4---first adhesive material, 5---second adhesive material, 6---third adhesive material, 7---metal ring, 8---fourth adhesive material, 9---tin ball. DETAILED DESCRIPTION

[0021] The purpose, advantages and features of the present invention will be illustrated and explained by the non-limiting description of the following preferred embodiments. These embodiments are only typical examples of the application of the technical solution of the present invention, and any technical solution formed by equivalent replacement or equivalent transformation falls within the scope of protection claimed by the present invention.

[0022] The present invention discloses a reinforced chip exposed flip chip spherical array structure, such as Figure 1 , Figure 2 and Figure 3 As shown, the enhanced chip exposed flip-chip ball array structure includes a chip 1, a circuit board 2, a metal connector 3, a first adhesive material 4, a second adhesive material 5, a third adhesive material 6, and a fourth adhesive material 8. The chip has two upper and lower surfaces, the upper surface of the chip is an exposed surface for contacting with external substances, and at least one layer of circuit board 2 is arranged on the lower surface of the chip. The chip and each layer of the circuit board are fixedly connected through the first adhesive material 4, and the chip and each layer of the circuit board are interconnected by signals through the metal connector 3.

[0023] The metal connector is a columnar or spherical structure. In the present technical solution, the metal connector can be a metal bump or a metal ball. Figure 1 As shown, when the metal connector is a metal bump, the metal bump is a tin bump, a copper bump, a gold bump, or a tin ball. Figure 2 As shown, when the metal connecting member is a metal ball, the metal ball is a tin bump or a copper bump or a gold bump or a tin ball. The metal ring is made of copper or aluminum, and the surface is plated with nickel or chromium.

[0024] A circle of second adhesive material 5 is fixed around the first adhesive material 4, and a certain gap is set between the second adhesive material 5 and the chip, and the gap is filled by the third adhesive material 6. The four sides of the chip, the first adhesive material 4 and the second adhesive material 5 are fixedly connected by the third adhesive material 6, so as to strengthen the protection of the four sides of the chip, so that the chip has only one side as an exposed surface for contacting the heat sink, that is, there is no plastic package wrapped above the chip, and the heat energy is quickly conducted to the outside of the package through the exposed surface of the chip, and there is no need to use a plastic package material with high heat dissipation performance.

[0025] A metal ring 7 is arranged around the outermost side of the circuit board, and the metal ring 7 is fixedly connected to the circuit board through a fourth adhesive material 8 to enhance the overall anti-deformation capability of the material. The thickness of the chip is 100-800um.

[0026] The first adhesive material 4 , the second adhesive material 5 , the third adhesive material 6 , and the fourth adhesive material 8 are all conductive or non-conductive adhesive materials.

[0027] The circuit board is a single-layer or multi-layer resin circuit board, and the gap below the circuit board is provided with multiple rows and columns of solder balls. In the present technical solution, the gap below the circuit board is provided with more than 2 rows and 2 columns of solder balls 9, and the chip signal is interconnected with the outside world through the solder balls below the resin circuit board.

[0028] Based on the traditional design, this technical solution adds sticky material around the chip to protect the side walls of the chip from damage, so that the chip can maintain heat dissipation performance when exposed, while protecting it from collision damage in downstream processes. At the same time, a metal ring is fixed at the frame of the circuit board to reduce the warping of the entire material, solving the problem of heat dissipation and warping that cannot be solved by existing technologies.

[0029] There are many implementation methods of the present invention, and all technical solutions formed by equivalent transformation or equivalent transformation fall within the protection scope of the present invention.

Claims

1. A reinforced chip exposed flip chip ball array structure, Features: The invention comprises a chip (1), a circuit board (2), a metal connecting piece (3), a first adhesive substance (4), a second adhesive substance (5), a third adhesive substance (6), a fourth adhesive substance (8), a metal ring (7), and a solder ball (9). The chip has an upper and lower surface. The upper surface of the chip is an exposed surface for contacting with external substances. The lower surface of the chip is provided with at least one layer of circuit board (2). The chip and each layer of the circuit board are fixedly connected via a first adhesive material (4). The chip and each layer of the circuit board are interconnected by signals via a metal connector (3). A circle of second adhesive material (5) is fixed around the first adhesive material (4), a certain gap is provided between the second adhesive material (5) and the chip, and the gap is filled by the third adhesive material (6), and the periphery of the chip, the first adhesive material (4) and the second adhesive material (5) are all fixedly connected by the third adhesive material (6). A metal ring (7) is arranged around the outermost side of the circuit board, the metal ring (7) is fixedly connected to the circuit board via a fourth adhesive material (8), a solder ball (9) is arranged below the circuit board, and the chip is interconnected with external signals via the metal ball; the circuit board is a single-layer or multi-layer resin circuit board; at least six solder balls (9) are arranged in the gap below the circuit board, and the chip signal is interconnected with the outside world via the solder balls below the resin circuit board; the first adhesive material (4), the second adhesive material (5), the third adhesive material (6), and the fourth adhesive material (8) are all conductive or non-conductive adhesive materials.

2. The enhanced chip exposed flip chip ball array structure according to claim 1, Features: The thickness of the chip is 100-800um.

3. The enhanced chip exposed flip chip ball array structure according to claim 1, Features: The metal connecting piece (3) is a columnar or spherical structure.

4. The enhanced chip exposed flip chip ball array structure according to claim 3, Features: The metal connecting piece (3) is a metal bump or a metal ball.

5. The enhanced chip exposed flip chip ball array structure according to claim 4, Features: The metal bumps are tin bumps, copper bumps, gold bumps or tin balls.

6. The enhanced chip exposed flip chip ball array structure according to claim 4, Features: The metal ball is a tin bump, a copper bump, a gold bump or a tin ball.

7. The enhanced chip exposed flip chip ball array structure according to claim 1, Features: The metal ring is made of copper or aluminum, and the surface is plated with nickel or chromium.