Aircraft wing parts

By using a composite metal matrix and a hollow ceramic sphere structure on the trailing edge of the wing, it provides structural strength and thermal insulation performance, solves the high-temperature impact of jet engine exhaust on the wing, extends the service life of the wing, and reduces costs. .

CN111688904BActive Publication Date: 2024-10-29AIRBUS DEFENCE AND SPACE(GB)
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
CN202010169972.9
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2020-03-12
Publication Date
2024-10-29
Estimated Expiration
2040-03-12

AI Technical Summary

Technical Problem

The high-temperature and high-pressure gases discharged by jet engines cause the ultimate tensile strength to decrease at the trailing edge of the wing, affecting the structural integrity and service life. Existing protection measures such as epoxy resin composites and thermal insulation slurries have limitations or high costs. .

Method used

Composite materials are used, including a metal matrix containing reinforcements and parts of hollow cermet spheres, which serve as insulating embedded layers to provide structural strength and thermal insulation properties. Wing components are manufactured through casting methods, using materials such as alumina to increase tensile strength. and thermal insulation effect.

Benefits of technology

It effectively improves the structural integrity and service life of the wing trailing edge, reduces the adverse effects of high temperature on materials, and avoids the problems of high cost and insufficient performance of thermal insulation materials in the existing technology.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN111688904B_ABST
    Figure CN111688904B_ABST
Patent Text Reader

Abstract

The present invention relates to an aircraft wing component, a wing assembly including such an aircraft wing component, and a method of manufacturing such a component and assembly. The trailing edge structure of an aircraft wing is subjected to high temperature exhaust from the aircraft's engine during use. Such elevated temperatures can adversely affect the ultimate tensile strength of the trailing edge. The aircraft wing component comprises a composite material having: a first portion (14), the first portion (14) comprising a metal matrix (16) containing a reinforcing material (17); and a second portion (15), the second portion (15) comprising a metal matrix (18) containing a plurality of hollow metal-ceramic spheres (19), the second portion being adjacent to a surface (20) of the composite material. Providing two portions, one of which comprises the reinforcing material and the other comprises the hollow spheres, means that the component has both structural strength and thermal insulation properties at the location where they are most needed. The portion of the composite material comprising the hollow metal-ceramic spheres serves as an inlay layer for thermal insulation.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to a component part of an aircraft wing. The invention also relates to a wing assembly comprising such a component part, and to methods of manufacturing such a component and assembly. Background Art

[0002] Advances in aircraft engine technology have resulted in jet engines that are more efficient and more powerful with high bypass ratios. Such engines tend to be larger in size than conventional jet engines and are more tightly integrated with the structural members of the adjacent wing assembly.

[0003] A problem that may be encountered in the development of such aircraft engines is that the proximity of the engine to the aircraft wing means that, in use, the trailing edge of the wing is more exposed to the hot, high-pressure gases exhausted by the engine. The exhaust of such an engine can reach temperatures of approximately 1600°C. Wing structures are typically made of aluminum and aluminum alloys; high temperatures have an adverse effect on the ultimate tensile strength (UTS) of this material.

[0004] Figure 1a and Figure 1b is a graph showing the effect of a high temperature air flow applied to the surface of a material of thickness 'd' made of a homogeneous aluminium alloy. The surface of the material is at d=0. Figure 1a The temperature distribution within a cross section of the material is shown. Due to the homogeneity of the material, the temperature of the material is highest at its surface and decreases approximately uniformly through the thickness of the material. Figure 1b The changes in UTS of the materials are shown. Figure 1b The broken line in represents the ultimate tensile strength of the material at room temperature. Throughout the thickness of the material, the UTS of the material is less than the UTS that the material would have at room temperature. This is most evident at the surface of the material exposed to high temperatures, where a significant drop in UTS can be seen. It will be appreciated that this effect may adversely affect the structural integrity of the trailing edge of the wing assembly and may limit the useful life of the assembly.

[0005] Various proposals have been made to protect the trailing edge wing structure from the adverse effects of high temperature emissions. In one proposal, the trailing edge structure comprises an epoxy resin composite material capable of withstanding elevated temperatures. Even so, this proposal can only protect the wing at temperatures that are at most well below the temperatures experienced by the trailing edge in use.

[0006] In another proposal, a thermal insulation slurry is applied to the trailing edge of the wing. However, such a slurry layer is unsightly and requires regular monitoring and maintenance. If applied incorrectly, the slurry may alter the aerodynamic performance of the wing.

[0007] Another suggestion is to use metals or alloys that work better at high temperatures, such as titanium or so-called superalloys, to make the trailing edge of the wing. However, such materials are generally expensive to produce and process. Summary of the invention

[0008] The present invention provides an aircraft wing component, the component comprising a composite material, a first portion of the composite material comprising a first metal matrix comprising a reinforcement material, and a second portion of the composite material comprising a second metal matrix comprising a plurality of hollow cermet spheres, the second portion being adjacent to a surface of the composite material. Providing two portions, one comprising the reinforcement material and the other comprising the hollow spheres, means that the component has both structural strength and thermal insulation properties where they are most needed. The portion of the composite material comprising the hollow cermet spheres acts as an insulated embedding layer at the surface of the composite material.

[0009] Preferably, the spheres have substantially the same diameter. This makes the temperature response of the second portion of the composite material at or near the surface of the material uniform. Alternatively, to provide better packing of the spheres within the metal matrix, the spheres may have a plurality of diameters within a predetermined range.

[0010] Preferably, the second portion containing the spheres has a thickness of less than 50% of the material, or even less than 25% of the material.By providing the reinforcement material over a majority of the thickness of the composite material, a material having a higher tensile strength is formed.

[0011] The spheres may be alumina which is cheap and lightweight.

[0012] Advantageously, the reinforcement material comprises a plurality of fibres which increase the tensile strength of the composite material.Alternatively, or additionally, the reinforcement material comprises particles.

[0013] The reinforcing material may also include alumina, or be entirely alumina.

[0014] Preferably, the metal matrix of the first portion is of the same material as the metal matrix of the second portion.The or each metal matrix may be aluminium.

[0015] The present invention also provides a method for manufacturing the aircraft wing component of the present invention, the method comprising the steps of: laying out the spheres and the reinforcing material in a mold; introducing liquid metal into the mold; and cooling the mold.

[0016] Preferably, the step of laying includes vibrating the mould to distribute the cermet spheres.

[0017] The invention also provides such a component, the component forming at least a portion of a trailing edge of an aircraft wing assembly.The component may form part of a control surface for an aircraft.

[0018] A wing assembly for an aircraft may include a wing body with an engine, wherein a portion of a downstream region of the engine, such as a trailing edge, includes a component of the present invention. BRIEF DESCRIPTION OF THE DRAWINGS

[0019] The present invention will now be described by way of example with reference to the accompanying drawings, in which:

[0020] Figure 1a is a graph showing a temperature profile through a cross section of a typical conventional aluminum alloy material when exposed to high temperature air;

[0021] Figure 1b It shows that when exposed to high temperature air Figure 1a The UTS curve of the alloy;

[0022] Figure 2a is a plan view of an aircraft incorporating a composite material constructed in accordance with the present invention;

[0023] Figure 2b is from Figure 2a A perspective view of a portion of a wing of an aircraft viewed from below;

[0024] Figure 3 is formed Figure 2a and Figure 2b a cross-sectional view of a portion of material of a portion of a wing;

[0025] Figure 4a is shown when exposed to high temperature air through Figure 3 A graph of the temperature profile of a cross section of a material;

[0026] Figure 4b It shows that when exposed to high temperature air Figure 3 A graph of the UTS of the material;

[0027] Figure 5 It is used to manufacture Figure 3 Flow chart of typical process of the material;

[0028] Figure 6a is a cross-sectional view of a material constructed in accordance with an alternative embodiment of the present invention; and

[0029] Figure 6b is a cross-sectional view of a material constructed in accordance with another alternative embodiment of the present invention. DETAILED DESCRIPTION

[0030] Reference Figure 2a and Figure 2b, a passenger aircraft is shown and is generally indicated by reference numeral 1. The aircraft 1 comprises a fuselage 2 for holding passengers and cargo, a right (starboard) wing 3 and a left (port) wing 4. A plurality of engines housed in nacelles 5, 6, 7, 8 are provided on the wings 3, 4. The engines are arranged to inhale large quantities of air in use, which is heated and compressed, mixed with jet fuel and burned. The air subsequently discharged from the exhaust nozzles of the engines produces thrust which causes the movement of the aircraft. The exhausted air, or effluent, is very hot and can reach 1600°C at its center. The portion of the aircraft wing immediately downstream of the exhaust nozzle, in particular the portion located on the underside of the wing, must be able to withstand such elevated temperatures.

[0031] Figure 2b A portion of the underside of a wing 3 is shown. In this figure is shown the exhaust pipe 9 of an engine housed in a nacelle 8. Large arrows 10 indicate the direction of the hot effluent from the exhaust nozzle. The area bounded by the dashed line 11 is subjected to the greatest exposure to the high temperature air flow. According to the invention, at least a portion of the trailing edges 12, 13 of the wings 3, 4 is formed by Figure 3 The composite material shown in cross section is made.

[0032] In order to effectively function as the trailing edge of a wing, the material must provide structural strength and be able to handle the high temperature effluent from the nozzle of an engine. To this end, two portions or regions 14, 15 of a metal matrix composite (MMC) material are provided. The first region 14 comprises a major portion of the material thickness and comprises a metal matrix 16 having a reinforcing material embedded within the metal matrix 16. In this embodiment, the reinforcing material comprises multiple layers of alumina filaments 17. This region 14 of MMC material provides the necessary structural strength required for the trailing edge of an aircraft wing so as to maintain the aerodynamic profile of the wing while being able to withstand the forces to which the wing is subjected during flight.

[0033] According to the present invention, the second region 15 comprises a metal matrix 18 containing a plurality of hollow cermet spheres 19 embedded within the metal matrix 18. In this embodiment, the hollow spheres 19 have a substantially constant diameter and are made of aluminum oxide. The region 15 of the composite material containing the cermet spheres is arranged at the surface 20 of the material so that the region 15 is more directly exposed to the hot engine exhaust. In both the first and second regions 14, 15, the metal matrix is ​​aluminum which is both lightweight and relatively inexpensive to produce. The region 15 acts as a heat shield to insulate the structural members of the trailing edge from the adverse effects of the high temperature exhaust.

[0034] Figure 4a and Figure 4bis a graph showing the effect of a high temperature air flow applied to the surface 20 of a composite material according to the invention.The surface 20 of the material is at approximately d=0. Figure 4a The temperature distribution in a cross section of the material is shown. Since region 15 acts as an insulating embedding layer separating region 14 from the hot air, the temperature of the material is highest at its surface and decreases in a hyperbolic manner through the thickness of the material. Figure 4b The change in UTS of the material is shown. The UTS of the material is lower in area 15, but much higher than hitherto achievable in area 14. The embedded thermally insulating area 15 helps to protect the main portion 14 of the composite material from the adverse effects of heating so that the trailing edge of the wing assembly maintains its structural integrity, thereby increasing the service life of the trailing edge of the wing assembly.

[0035] Figure 3 The material can be manufactured by casting, for example. Figure 5 The steps of the casting method are schematically shown in FIG.

[0036] In one embodiment of the casting method according to the present invention, the first step includes "laying" the hollow metal ceramic sphere and the reinforcement material. First, the sphere is placed in the mold (step 21). The hollow sphere can be arranged inside the mold, such as by shaking, so that the sphere can be filled with the best available tight packing density. Once the sphere is filled in the mold, the reinforcement material is added to the mold (step 22). This can be done by simply laying the fiber in the mold, or by winding the fiber around one of the more supporting structures that can be formed in the casting mold itself.

[0037] The next step 23 in the manufacturing process is to introduce the metal matrix material. One method of introducing the metal matrix material can be accomplished by pouring liquid metal into the mold. In this embodiment, the mold that combines the spheres and the reinforcement material is first preheated. Preferably, in order to prevent the matrix from prematurely solidifying before the mold is completely filled, the preheating temperature is approximately equal to the casting temperature of the liquid metal that forms the matrix.

[0038] The liquid metal forming the matrix is ​​cast into the mold in a manner that the gaps around the hollow sphere and the reinforcement are filled while avoiding interference with the sphere and reinforcement in the mold. In some embodiments, it may be useful to use a screen, a nail or other similar device for maintaining the arrangement of the sphere and reinforcement in the mold. Except for gravity casting, the mold can be subjected to a pressure difference during the casting process. For example, the mold can be pressurized or maintained under a vacuum.

[0039] Once the liquid metal forming the matrix has been satisfactorily cast into the mold, the liquid metal is solidified (step 24) to form a solid metal matrix around the hollow spheres and the reinforcing material. This solidification is usually performed by cooling the mold, which can be performed by atmospheric cooling or by more controlled cooling methods.

[0040] Figure 6a and Figure 6b An alternative composite material constructed in accordance with the present invention is shown. Figure 6a In the embodiment, the first region 25 comprises a metal matrix 26 which contains reinforcing elements in the form of a plurality of layers of fibers 27 which are shorter in length than the first region 25. Figure 3 The fibers in the embodiment of the present invention are short. Shorter fibers are generally less brittle than long fibers. The second region 28 includes a metal matrix 29 with embedded hollow cermet spheres 30, which in this embodiment have various diameters within a range of predetermined values. Such selection of spheres allows for a more compact arrangement than an arrangement where the spheres are all of one diameter.

[0041] exist Figure 6b In an embodiment of the invention, the first region 31 comprises a metal matrix 32 containing reinforcing elements in the form of a granular material 33 which can be considered to be the limit of the short fiber length. The advantage of using particle reinforcement is that the first region 31 of the resulting composite material will be isotropic, having the same mechanical properties in all directions. In this embodiment, the second region 34 comprises a metal matrix 35 containing spheres of two different diameters 36, 37; the spheres of the larger diameter 36 are arranged in the layer closest to the surface of the material, and the spheres of the smaller diameter are arranged between the first layer of spheres 36 and the reinforcing particle region 31. This arrangement provides a transition between the insulating part of the composite material and the reinforced part of the composite material.

[0042] Of course, any combination of reinforcements and spheres may be embedded in a metal matrix to form a wing component constructed in accordance with the present invention. The composite material may be tailored to have different regions depending on the desired physical properties of the material. For example, areas that require structural strength but are not exposed to extreme temperatures will include more reinforcements in the matrix, while areas exposed to the highest temperatures will contain more metal-ceramic spheres. The portion of the composite material that includes the material containing the spheres has been shown in the accompanying drawings as forming a relatively small portion of the overall thickness of the composite material, but this can of course be changed and customized depending on the desired properties of the resulting composite material. The spheres may comprise up to 50% of the corresponding portion in terms of weight of the composite material. Similarly, the reinforcements may comprise up to 50% of the corresponding portion in terms of weight of the composite material.

[0043] Other modifications may be made without departing from the scope of the invention. For example, the reinforcing element may be selected from any one or combination of cables, fibers, tapes, filaments, and particles. The reinforcing element may include, for example, aluminum oxide (alumina), silicon dioxide, boron, electroplated carbon, or any other high-strength fiber or particle.

[0044] The spheres may have any diameter in the range of micrometers to millimeters. The spheres may all have approximately the same diameter or a selection of multiple diameters. The spheres may be made of one material, such as aluminum oxide or carbon dioxide, or of multiple different materials of the same composition. The spheres may be coated to make them more easily integrated with the metal substrate.

[0045] The matrix material is a metal material such as aluminum, titanium, or any other suitable material. Preferably, the matrix material is relatively lightweight, low cost, and easy to process. Depending on the desired properties of the final product, the metal matrix can be the same throughout the material, or different materials can be used in different areas.

[0046] The composite material may be formed by other suitable processes known to those skilled in the art, such as powder metallurgy, extrusion casting or diffusion bonding.

[0047] The wing component of the present invention may comprise in whole or in part the trailing edge of the wing itself and / or may comprise the underside of the wing downstream of the engine. The wing component may comprise a flap, aileron or other control surface of an aircraft that will be exposed to high temperature airflow during use.

[0048] The present invention may be used in other wing structures that require structural integrity, for example, due to proximity to heat generating components or due to aerodynamic friction, and are at high temperatures. The present invention may be used to provide protection for extreme conditions of cryogenic temperatures. Other variations and applications will be apparent to those skilled in the art.

Claims

1. An aircraft wing component comprising a composite material, a first portion of the composite material comprising a first metal matrix comprising a reinforcing material and a second portion of the composite material comprising a second metal matrix comprising a plurality of hollow cermet spheres, the second portion being adjacent to a surface of the composite material in a thickness direction of the composite material, such that the first portion is spaced apart from the surface of the composite material in the thickness direction by the second portion.

2. The component according to claim 1, wherein The spheres have substantially the same diameter.

3. The component according to claim 1, wherein The sphere has a plurality of diameters within a predetermined range.

4. A component according to claim 1, 2 or 3, wherein: The second portion has a thickness that is less than 50% of the composite material.

5. A component according to claim 1, 2 or 3, wherein: The second portion has a thickness that is less than 25% of the composite material.

6. A component according to claim 1, 2 or 3, wherein: The reinforcement material includes at least one of: a plurality of fibers; and particles.

7. A component according to claim 1, 2 or 3, wherein: At least one of the reinforcing material and the spheres includes alumina.

8. A component according to claim 1, 2 or 3, wherein: The first metal substrate has the same material as the second metal substrate.

9. A component according to claim 1, 2 or 3, wherein: The metal matrix of at least one of the first portion and the second portion includes aluminum.

10. A component as claimed in claim 1, 2 or 3 comprising at least a portion of the trailing edge of a wing.

11. A component according to claim 1, 2 or 3 comprising an aircraft control surface.

12. A method of manufacturing a component according to claim 1, 2 or 3, the method comprising the steps of: Laying the spheres and reinforcement material in the mold; introducing liquid metal into the mold; and solidifying the metal.

13. The method according to claim 12, wherein: The step of laying out the spheres and reinforcement material in the mould includes vibrating the mould to distribute the spheres.

14. A wing assembly comprising: Wing body; engine; And a component according to any one of claims 1 to 3, arranged downstream of the engine.

15. An aircraft incorporating a wing assembly according to claim 14.

Citation Information

Patent Citations

  • Structural panel insert having encapsulated filler materials

    US20160375648A1