An online identification device and method for metal substrate exposure rate when removing thermal barrier coating by abrasive water jet
Through negative pressure tube reflow and current detection technology, the accuracy of metal matrix exposure rate detection when abrasive water jet removes thermal barrier coating is solved, and the accuracy of online identification of metal matrix exposure rate is achieved, ensuring the stability of electric spark processing sex.
Patent Information
- Application Number
- CN202011342295.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2020-11-26
- Publication Date
- 2024-11-15
- Estimated Expiration
- 2040-11-26
AI Technical Summary
When removing thermal barrier coating by abrasive water jets, how to judge the exposure rate of metal substrates online is a difficult problem. The existing methods are prone to leakage of power due to working fluid leakage, affecting detection accuracy.
Use negative pressure tube to force reflow of working fluid to prevent the working fluid from flowing onto the metal substrate. Use the weak conductivity of the working fluid to apply DC voltage between the workpiece and the nozzle. Data is collected through the current recorder to automatically identify the metal bareness rate to ensure detection. accuracy.
It effectively prevents the bypass current of the working fluid, improves the accuracy of identification of the bareness rate of the metal matrix, ensures the consistent removal rate of the thermal barrier coating at each hole, and promotes the stability of subsequent electric spark perforation processing.
Smart Images

Figure CN112276802B_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to an online detection technology for the bare metal substrate rate when the thermal barrier coating on the surface of a metal component is removed, and in particular to a technology capable of online identifying the bare metal substrate rate when the thermal barrier coating on the surface of a metal component is eroded, and specifically to an online identification device and method for the bare metal substrate rate when the thermal barrier coating is removed by an abrasive water jet. Background Art
[0002] Coating thermal barrier coatings on aircraft engine turbine blades can ensure that they can withstand operating temperatures higher than the limiting temperature of their own metal substrates, further improving the thrust-to-weight ratio of turbine gas engines. Since thermal barrier coatings are non-conductive, it is difficult to perform electrospark machining of air film holes on turbine blades with thermal barrier coatings. In order to perform electrospark drilling on metal components with thermal barrier coatings, it is necessary to partially remove the thermal barrier coating and expose the metal substrate to facilitate electrospark machining. Abrasive water jet is a current method for removing thermal barrier coatings, which has the advantages of good machining quality, low cost, and no negative impact on the environment. However, when using abrasive water jets to remove thermal barrier coatings, how to judge the erosion removal rate of the thermal barrier coating (i.e., the exposure rate of the metal substrate) online is a difficult problem. Although the removal thickness of the thermal barrier coating can be controlled by experiments and then controlling the processing time of the abrasive water jet, the coating thickness of the thermal barrier coating at various locations on the turbine blade is generally uneven, and it is difficult to ensure that the exposure rate of the metal substrate at each hole position after abrasive water jet machining is consistent, which in turn affects the success rate of subsequent electrospark machining. Therefore, it is necessary to perform online identification of the metal exposure rate during the erosion process of the thermal barrier coating to determine the exposure of the metal substrate. Previous studies have shown that the weak conductivity of the working fluid can be used to apply a certain DC voltage between the workpiece and the nozzle, and the exposure of the metal can be identified based on the change in current. However, since the working fluid beam flows around after being sprayed onto the workpiece, it is easy to flow to the metal substrate that is not coated with the thermal barrier coating, causing interference with the bypass current in the circuit, making this method unable to achieve the expected effect. Therefore, the present invention proposes to use a negative pressure tube to force the reflux of the working fluid to ensure that the working fluid does not flow out, thereby avoiding the generation of bypass current in the current detection circuit and increasing the accuracy of identifying the exposure rate of the metal substrate. In addition, according to the results of previous studies, the machinability of EDM holes is closely related to the exposure rate of the metal substrate, but it does not require the metal substrate to be completely exposed. For example, in the document "Electromachining and Mold, Issue 4, 2020, "Experimental Study on EDM Hole Making after Erosion of Thermal Barrier Coating", authors Gao Changshui, Xie Tianhai, Zhao Kai, and Liu Zhuang", EDM air film holes can be machined when the exposed area of the metal substrate reaches 20%, which further highlights the importance of online identification of the erosion removal rate of thermal barrier coatings. Summary of the invention
[0003] The purpose of the present invention is to solve the problem that the existing exposure rate detection is easily affected by leakage of the spray liquid, thereby affecting the detection accuracy. A method for online determination of the exposure rate of the metal substrate when removing the thermal barrier coating with an abrasive water jet is invented, and a corresponding device is provided. The device uses the negative pressure of air to suck the working fluid sprayed onto the surface of the workpiece, preventing the working fluid from flowing to the metal substrate of the workpiece, thereby eliminating the bypass current generated by the outward flow of the working fluid. At the same time, the weak conductivity of the working fluid is used to load a DC voltage between the workpiece substrate and the nozzle, and the current recorder collects the current data to automatically identify the metal exposure state, and finally realizes the online identification of the metal exposure rate.
[0004] One of the technical solutions of the present invention is:
[0005] An online identification device for the exposure rate of a metal substrate when removing a thermal barrier coating by an abrasive water jet, characterized in that it comprises an abrasive working liquid tank 1, an infusion pump 2, an infusion pipeline 4, a jet nozzle 7, a nozzle 8, a workbench 12, a working liquid reflux device and a weak current detection device; a workpiece 11 is installed on the workbench 12, the workpiece 11 is composed of a thermal barrier coating 11.1 and a metal substrate 11.2, the jet nozzle 7 is connected to the infusion pump 2 through the infusion pipeline 4, and the infusion pump 2 is connected to the working liquid tank 1 The working fluid in the working fluid tank 1 is pumped into the jet nozzle 7, and the nozzle 8 is installed on the jet nozzle 7; the working fluid reflux device comprises a jet protection sleeve 9.1, a sealing block 9.2, a negative pressure pipe 9.3 with a liquid extraction port 9.4 and an air inlet channel 9.5 on the side, a reflux pipeline 9.7, a working fluid recovery tank 9.8 and an air pump 9.9, the upper end of the negative pressure pipe 9.3 is connected to the jet protection pipe 9.1 through the sealing block 9.2, the jet protection pipe 9.1 is sleeved on the jet nozzle 7, and the negative pressure pipe 9.3 is connected to the jet protection pipe 9.1 through the sealing block 9.2, and the jet protection pipe 9.1 is sleeved on the jet nozzle 7. The lower end cover of the tube 9.3 is mounted on the thermal barrier coating 11.1. An air inlet channel 9.5 is provided on the end surface of the negative pressure tube 9.3 in contact with the thermal barrier coating 11.1. A liquid extraction port 9.4 is provided in the middle of the lower end of the negative pressure tube 9.3. The liquid extraction port 9.4 is connected to a working liquid recovery tank 9.8. An air pump 9.9 is connected to the working liquid recovery tank 9.8. When the air pump 9.9 is working, negative pressure of air is generated in the negative pressure tube 9.3. Air flow 9.6 flows into the air inlet channel 9.5 at the lower end of the negative pressure tube 9.3 and is connected to the working liquid recovery tank 9.8. The liquid reflux flows from the liquid extraction port 9.4 along the reflux pipeline 9.7 into the working liquid recovery box 9.8; the weak current detection device includes a DC power supply 10.1, a current recorder 10.2, a cable conductor 10.3 and a computer 10.4, the positive and negative poles of the DC power supply 10.1 are respectively connected to the metal substrate 11.2 and the jet nozzle 7, the current recorder 10.2 is connected in series to the loop, and the collected current data is transmitted to the computer 10.4 through the cable conductor 10.3.
[0006] An overflow valve 3, a pulsation damper 5 and a pressure gauge 6 are installed on the liquid delivery pipeline 4 connecting the jet nozzle 7 and the working liquid tank 1.
[0007] The jet nozzle 7 is made of a metal material that is wear-resistant and acid- and alkali-resistant; the working fluid is a mixed liquid of tap water with weak conductivity and solid abrasive.
[0008] The sampling frequency of the current recorder 10.2 is not less than 10 Hz, and the current recorder can detect microampere level current.
[0009] The lower end of the negative pressure tube 9.3 is in an inverted frustum-shaped structure that is smaller at the bottom and larger at the top.
[0010] The lower end of the jet protection sleeve 9.1 is connected to a tubular protection sleeve to facilitate the working fluid sprayed from the nozzle 8 to smoothly reach the thermal barrier coating 11.1.
[0011] The second technical solution of the present invention is:
[0012] An online identification method for the bare rate of a metal substrate when a thermal barrier coating is removed by erosion, characterized by comprising the following steps:
[0013] The first step is to clamp the workpiece on the insulating fixture, adjust the relative distance between the nozzle and the surface to be processed (i.e., the target distance); add the jet working fluid mixed with abrasive and tap water into the working fluid tank;
[0014] The second step is to detect the conductivity of the working fluid. According to the set parameters such as metal substrate exposure rate, DC voltage, working fluid conductivity, nozzle diameter, etc., the corresponding stop current value I is calculated when the metal substrate exposure rate reaches the set value through the electrochemical anodic dissolution principle formula. s :
[0015]
[0016] In the formula, is the exposure rate, d is the relative distance between the nozzle and the workpiece surface to be processed, U is the DC voltage applied between the jet nozzle and the metal substrate, D is the nozzle diameter, κ is the working fluid conductivity; π is the pi constant;
[0017] The third step is to connect the cathode of the DC power supply in the current detection device to the jet nozzle, connect the anode of the DC power supply to the metal substrate of the workpiece, and apply a certain DC voltage between the jet nozzle and the metal substrate of the workpiece;
[0018] The fourth step is to connect the DC power supply between the jet nozzle and the metal substrate of the workpiece, start the infusion pump and the air pump, and use the jet working fluid in the form of an abrasive water jet through the jet nozzle to erode and remove the thermal barrier coating on the surface of the workpiece. The negative pressure suction function of the working fluid reflux device is used to force the ejected working fluid to flow back to the working fluid collection box, thereby preventing the working fluid from flowing out of the negative pressure pipe and causing bypass current; use the current recorder to detect the current size in the loop, and synchronize the collected current data to the computer;
[0019] The fifth step is that as the abrasive water jet machining continues to remove the thermal barrier coating, the metal substrate of the eroded area begins to be exposed. The exposed metal part produces an electrochemical reaction under the action of the external electric field and the weak conductivity working fluid. A weak current flows through the circuit. According to the principle of current change during electrochemical reaction, as the exposed metal area increases, the current value in the circuit also increases. The weak current in the machining process is read online by a computer. When the current in the circuit reaches the stop current value I s , and maintain a current value not less than the stop current value for a certain period of time, it is judged that the set erosion exposure rate has been reached; at this time, the DC power supply is turned off, the infusion pump and the air pump are turned off, and the processing is ended.
[0020] The beneficial effects of the present invention are:
[0021] The present invention can effectively prevent the jet working fluid from flowing to various places on the workbench after being sprayed, avoid the influence of bypass current on current detection, and ensure the accuracy of identifying the metal exposure rate. It can ensure that the removal rate of the thermal barrier coating at each hole is consistent, which is conducive to the stable progress of subsequent electrospark perforation processing. BRIEF DESCRIPTION OF THE DRAWINGS
[0022] Figure 1 It is a schematic diagram of the online identification device of the metal substrate exposure rate when the thermal barrier coating is removed by erosion according to the present invention.
[0023] Figure 1 In: 1. working fluid tank, 2. infusion pump, 3. overflow valve, 4. infusion pipeline, 5. pulsation damper, 6. pressure gauge, 7. jet nozzle, 7.1. abrasive working fluid, 8. nozzle, 9.1. jet protection tube, 9.2. sealing block, 9.3. negative pressure tube, 9.4. liquid extraction port, 9.5. air inlet channel, 9.6. air flow, 9.7. return pipeline, 9.8. working fluid recovery tank, 9.9. air pump, 10.1. DC power supply, 10.2. current recorder, 10.3. cable conductor, 10.4. computer, 11. workpiece, 11.1. thermal barrier coating, 11.2. metal substrate, 12. workbench. DETAILED DESCRIPTION
[0024] The present invention will be further described below in conjunction with the accompanying drawings and specific examples.
[0025] Embodiment 1.
[0026] like Figure 1 shown.
[0027] An online identification device for the exposure rate of a metal substrate when removing a thermal barrier coating by an abrasive water jet, characterized in that it comprises an abrasive working liquid tank 1, an infusion pump 2, an infusion pipeline 4, a jet nozzle 7, a nozzle 8, a workbench 12, a working liquid reflux device and a weak current detection device; a workpiece 11 is installed on the workbench 12, the workpiece 11 is composed of a thermal barrier coating 11.1 and a metal substrate 11.2, the jet nozzle 7 is connected to the infusion pump 2 through the infusion pipeline 4, the infusion pump 2 is connected to the working liquid tank 1 and pumps the working liquid of the working liquid tank 1 into the jet nozzle 7, and an overflow valve 3, a pulsation damper 5 and a pressure gauge 6 are installed on the infusion pipeline 4 connecting the jet nozzle 7 and the working liquid tank 1. The nozzle 8 is installed on the jet nozzle 7, and the jet nozzle 7 is made of a wear-resistant, acid- and alkali-resistant metal material; the working liquid is a mixed liquid of tap water and solid abrasive with weak conductivity. The working fluid reflux device comprises a jet protection sleeve 9.1, a sealing block 9.2, a negative pressure pipe 9.3 with a liquid extraction port 9.4 and an air inlet channel 9.5 on the side, a reflux pipeline 9.7, a working fluid recovery tank 9.8 and an air pump 9.9. The lower end of the negative pressure pipe 9.3 is an inverted frustum structure with a small bottom and a large top. The lower end of the jet protection sleeve 9.1 is connected to a tubular protection sleeve to facilitate the working fluid sprayed from the nozzle 8 to smoothly reach the thermal barrier coating 11.1. The upper end of the negative pressure pipe 9.3 is connected to the jet protection pipe 9.1 through a sealing block 9.2. The jet protection pipe 9.1 is sleeved on the jet nozzle 7. The lower end cover of the negative pressure pipe 9.3 is mounted on the thermal barrier coating 11.1. An air inlet channel 9.5 is provided on the end surface of the negative pressure pipe 9.3 in contact with the thermal barrier coating 11.1. A liquid extraction port 9.4 is provided in the middle of the lower end of the negative pressure pipe 9.3. The liquid extraction port 9.4 is connected to the working liquid recovery tank 9.8. The air pump 9.9 is connected to the working liquid recovery tank 9.8. When the air pump 9.9 is working, air negative pressure will be generated in the negative pressure pipe 9.3. The air flow 9. 6 flows into the air inlet channel 9.5 at the lower end of the negative pressure tube 9.3, and flows into the working fluid recovery box 9.8 along the return pipe 9.7 from the liquid extraction port 9.4 with the working fluid reflux; the weak current detection device comprises a DC power supply 10.1, a current recorder 10.2, a cable 10.3 and a computer 10.4, the positive and negative electrodes of the DC power supply 10.1 are respectively connected to the metal substrate 11.2 and the jet nozzle 7, the current recorder 10.2 is connected in series to the loop, and the collected current data is transmitted to the computer 10.4 through the cable 10.3. The sampling frequency of the current recorder 10.2 is not less than 10Hz, and the current recorder can detect microampere level current.
[0028] The working principle of this embodiment is: start the infusion pump 2 and the air pump machine 9.9, turn on the direct current 10.1, and start the abrasive water jet erosion to remove the thermal barrier coating on the surface of the workpiece. When the jet working fluid hits and erodes the thermal barrier coating 11.1, the processed working fluid is sucked away in time by a coaxial gas-liquid two-phase fluid suction and recovery device based on the working fluid to avoid bypass current interference. In the previous experiments, it was found that when the metal substrate of the eroded part has not been exposed by erosion, no current passes through the circuit; when the metal substrate 11.2 begins to be exposed, the exposed metal part will produce an electrochemical reaction, and current will be conducted in the circuit. According to the principle of current change during electrochemical reaction, as the metal exposure rate increases, the current value in the circuit also increases. The current recorder 10.2 completes at least ten current samplings per second and transmits them synchronously to the computer 10.4. The computer is used to read the weak current in the processing process online. When it is detected that the current in the circuit reaches the stop current value I generated by the metal substrate exposure rate being the set value s时 , and maintain for 5 seconds not less than the stop current value I s , that is, it automatically determines that the set metal matrix exposure rate has been reached. At the same time, an alarm mechanism is added to the metal exposure rate online identification software system. When it is detected that the metal is just beginning to be exposed, the alarm sounds once. When the metal exposure rate reaches the set value, the alarm sounds twice, indicating that the exposed metal part can be processed by electric spark machining. At this time, the DC power supply 10.1 is turned off, the infusion pump 2 and the air pump machine 9.9 are turned off, and the machining is ended.
[0029] Embodiment 2.
[0030] like Figure 1 shown.
[0031] An online identification method for the bare rate of a metal substrate when a thermal barrier coating is removed by erosion, comprising the following steps:
[0032] 1. Clamp the workpiece on the insulating fixture, adjust the relative distance (target distance) between the nozzle and the workpiece surface to be processed to 10mm; add the jet working fluid mixed with abrasive and tap water into the working fluid tank, and the abrasive content in the working fluid reaches 1% by mass, and it needs to be stirred continuously to keep the mixture uniform, and detect the conductivity value of the abrasive working fluid 350μS / cm; using a nozzle with a diameter of 0.6mm;
[0033] 2. Connect the cathode of the DC power supply in the current detection device to the jet nozzle, connect the anode of the DC power supply to the metal substrate of the workpiece, and apply a DC voltage of 100V between the jet nozzle and the metal substrate of the workpiece; According to the results of previous studies, the machinability of EDM drilling does not require the metal substrate to be completely exposed, and EDM drilling can be performed when the exposed area of the metal substrate reaches 20%. Here, the expected value of the metal substrate exposure rate is set to 0.2.
[0034] 3. According to the principle of electrochemical anodic dissolution, calculate when the metal matrix exposure rate reaches the condition for EDM gas film hole, that is, the metal exposure rate Stop current at 20% , where: is the exposure rate, is the conductivity of the abrasive working fluid, U is the DC voltage applied between the jet nozzle and the metal substrate of the workpiece, D is the nozzle diameter, d is the relative distance between the nozzle and the surface to be processed of the workpiece (target distance), is the circumference constant; in this example, =0.2, U=100V, D=0.6mm, =350 , d = 10mm, calculated s =19.8 A.
[0035] 4. Start the infusion pump 2 and the air pump 9.9, turn on the DC current 10.1, and start the abrasive water jet erosion to remove the thermal barrier coating on the workpiece surface. When the jet working fluid impacts and erodes the thermal barrier coating 11.1, the processed working fluid is sucked away in time by the coaxial gas-liquid two-phase fluid suction recovery device based on the working fluid to avoid bypass current interference. In the previous experiments, it was found that when the metal substrate 11.2 began to be exposed, the exposed part of the metal would produce an electrochemical reaction, and a weak current would be conducted in the circuit. According to the principle of current change during electrochemical reaction, as the exposed area of the metal increases, the current value in the circuit also increases.
[0036] 5. The current recorder 10.2 completes at least ten current samplings per second and transmits them synchronously to the computer 10.4. The computer is used to read the weak current during the processing online. When the current in the circuit reaches 19.8 A, that is, the stopping current value generated when the metal substrate exposure rate is 20%, and it is maintained for 5 seconds and is not less than 19.8 A, that is, it is automatically determined that the set metal matrix exposure rate has been reached. At this time, the DC power supply 10.1 is turned off, the infusion pump 2 and the air pump machine 9.9 are turned off, and the processing is ended.
[0037] The present invention does not involve parts that are the same as the prior art or can be implemented by using the prior art.
Claims
1. An online identification device for the exposure rate of metal substrate when removing thermal barrier coating by abrasive water jet, characterized in that It comprises an abrasive working fluid tank (1), an infusion pump (2), an infusion pipeline (4), a jet nozzle (7), a nozzle (8), a workbench (12), a working fluid reflux device and a weak current detection device; a workpiece (11) is mounted on the workbench (12), the workpiece (11) is composed of a thermal barrier coating (11.1) and a metal substrate (11.2), the jet nozzle (7) is connected to the infusion pump (2) via the infusion pipeline (4), the infusion pump (2) is connected to the working fluid tank (1) and pumps the working fluid in the working fluid tank (1) into the jet nozzle (7), and the nozzle (8) is mounted on the jet nozzle (7); The working fluid reflux device comprises a jet protection sleeve (9.1), a sealing block (9.2), a negative pressure pipe (9.3) with a liquid extraction port (9.4) and an air inlet channel (9.5) on the side, a reflux pipeline (9.7), a working fluid recovery tank (9.8) and an air pump (9.9), the upper end of the negative pressure pipe (9.3) is connected to the jet protection pipe (9.1) through the sealing block (9.2), the jet protection pipe (9.1) is sleeved on the jet nozzle (7), the lower end cover of the negative pressure pipe (9.3) is mounted on the thermal barrier coating (11.1), and the negative pressure pipe (9.3) is in contact with the thermal barrier coating (11.1). An air inlet channel (9.5) is provided on the end surface, a liquid extraction port (9.4) is provided in the middle of the lower end of the negative pressure tube (9.3), the liquid extraction port (9.4) is connected to a working liquid recovery tank (9.8), an air pump (9.9) is connected to the working liquid recovery tank (9.8), and when the air pump (9.9) is working, negative air pressure is generated in the negative pressure tube (9.3), and an air flow (9.6) flows in from the air inlet channel (9.5) at the lower end of the negative pressure tube (9.3), and flows back from the liquid extraction port (9.4) along the reflux pipeline (9.7) into the working liquid recovery tank (9.8); the weak current detection device includes a DC power supply (10.1), a current recorder (10.2), a cable conductor (10.3) and a computer (10.4), the positive and negative electrodes of the DC power supply (10.1) are respectively connected to the metal substrate (11.2) and the jet nozzle (7), the current recorder (10.2) is connected in series to the loop, and the collected current data is transmitted to the computer (10.4) through the cable conductor (10.3); the sampling frequency of the current recorder (10.2) is not less than 10Hz, and the current recorder can detect microampere-level current; the lower end of the negative pressure tube (9.3) is an inverted cone-shaped structure with a small bottom and a large top.
2. The online identification device according to claim 1 is characterized in that the An overflow valve (3), a pulsation damper (5) and a pressure gauge (6) are installed on the jet nozzle (7) and the liquid delivery pipeline (4) of the working liquid tank (1).
3. The online identification device according to claim 1, characterized in that The jet nozzle (7) is made of a metal material that is wear-resistant and acid- and alkali-resistant; the working fluid is a mixed liquid of tap water with weak conductivity and solid abrasive.
4. The online identification device according to claim 1, characterized in that The lower end of the jet protective sleeve (9.1) is connected to a tubular protective sleeve to facilitate the working fluid sprayed from the nozzle (8) to smoothly reach the thermal barrier coating (11.1).
5. An online identification method based on the online identification device for the bare metal substrate when removing thermal barrier coating by abrasive water jet according to claim 1, characterized in that The following steps are involved: The first step is to clamp the workpiece on the insulating fixture and adjust the relative distance between the nozzle and the surface to be processed of the workpiece; add the jet working fluid mixed with abrasive and tap water into the working fluid tank; The second step is to detect the conductivity of the working fluid. According to the set parameters such as metal substrate exposure rate, DC voltage, working fluid conductivity, nozzle diameter, etc., the corresponding stop current value I is calculated when the metal substrate exposure rate reaches the set value through the electrochemical anodic dissolution principle formula. s : ; In the formula, is the exposure rate, d is the relative distance between the nozzle and the workpiece surface to be processed, U is the DC voltage applied between the jet nozzle and the metal substrate, D is the nozzle diameter, κ is the working fluid conductivity; π is the pi constant; The third step is to connect the cathode of the DC power supply in the current detection device to the jet nozzle, connect the anode of the DC power supply to the metal substrate of the workpiece, and apply a certain DC voltage between the jet nozzle and the metal substrate of the workpiece; The fourth step is to connect the DC power supply between the jet nozzle and the metal substrate of the workpiece, start the infusion pump and the air pump, and use the jet working fluid in the form of an abrasive water jet through the jet nozzle to erode and remove the thermal barrier coating on the surface of the workpiece. The negative pressure suction function of the working fluid reflux device is used to force the ejected working fluid to flow back to the working fluid collection box, thereby preventing the working fluid from flowing out of the negative pressure pipe and causing bypass current. Use a current recorder to detect the current in the loop and synchronize the collected current data to the computer; Step 5: As the abrasive water jet machining continues to remove the thermal barrier coating, the metal substrate of the eroded area begins to be exposed. The exposed metal part produces an electrochemical reaction under the action of the external electric field and the weak conductivity working fluid. A weak current flows through the circuit. According to the principle of current change during electrochemical reaction, as the exposed metal area increases, the current value in the circuit also increases. The weak current in the processing process is read online by a computer. When the current in the circuit reaches the stop current value I s , and maintain a current value not less than the stop current value for a certain period of time, it is judged that the set erosion exposure rate has been reached; at this time, the DC power supply is turned off, the infusion pump and the air pump are turned off, and the processing is ended.
Citation Information
Patent Citations
Method and apparatus for processing transparent conductive glass surface by dry ice particle spraying technique
CN101011814A
Wafer and polishing device and method, piezoelectric vibrating piece, method and apparatus for fabricating piezoelectric vibrating piece
CN101510767A
Device for removing thermal barrier coating on surface of metal component through abrasive water jet
CN209021903U
On-line identification device for metal matrix bareness rate during removal of thermal barrier coating by abrasive water jet
CN213673631U
Shot-peening device
JP2009006402A