By using multiple optical resonator structures and light-transmitting layers with different refractive indexes in the self-luminous element, the problem of balancing the resonator structure and the film thickness of the functional layer is solved, and a light-emitting element with efficient light extraction and long life is achieved.
Patent Information
- Application Number
- CN202011051643.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2020-09-29
- Publication Date
- 2024-10-29
- Estimated Expiration
- 2040-09-29
AI Technical Summary
In self-luminous elements, when extracting light through a resonator structure, it is difficult to simultaneously optimize the desired range of the peak wavelength of light and the film thickness of the functional layer, leading to problems of low luminous efficiency and color deviation.
First and second light-transmitting layers with different refractive indexes are used to form multiple optical resonator structures to adjust the peak wavelength of light, and the film thickness of the functional layer is optimized by combining these resonator structures to achieve efficient optical Extraction and longevity.
By adjusting the peak wavelength of the optical resonator structure and the film thickness of the functional layer, the peak wavelength of light in the light-emitting element is accurately extracted, the luminous efficiency is improved, the color deviation is reduced, and the life of the element is extended.
Smart Images

Figure CN112582561B_ABST
Abstract
Description
Technical Field
[0001] The present disclosure relates to a light-emitting element utilizing an electroluminescence phenomenon or a quantum dot effect, a self-luminous panel using the light-emitting element, and a method for manufacturing the same. Background Art
[0002] In recent years, display devices using self-luminous elements such as organic EL elements that utilize the electroluminescence phenomenon of organic materials and QLEDs that utilize the quantum dot effect have become increasingly popular.
[0003] The self-luminous element has a structure in which a functional layer is sandwiched between an anode and a cathode, and the functional layer includes at least a light-emitting layer. As functional layers other than the light-emitting layer, for example, there are functional layers (electron injection layer, electron transport layer, etc.) arranged between the light-emitting layer and the cathode for supplying electrons to the light-emitting layer, and functional layers (hole transport layer, hole injection layer) arranged between the light-emitting layer and the anode for supplying holes (holes) to the light-emitting layer.
[0004] In the self-luminous element, from the viewpoint of reducing power consumption or extending the life, it is also desired to improve the efficiency of extracting light from the light-emitting element of each color. In order to improve the light extraction efficiency, for example, as shown in Patent Document 1, it is also known to use a resonator structure in the organic EL element of each color as the self-luminous element.
[0005] Prior art literature
[0006] Patent Literature
[0007] Patent Document 1: International Publication No. 2012 / 020452 Summary of the invention
[0008] Technical problem to be solved by the invention
[0009] However, when light is extracted through a resonator structure, in a self-luminous element, the optical distance between the interface on the anode light-emitting layer side and the interface on the cathode light-emitting layer side needs to be designed corresponding to the peak wavelength of the extracted light. Therefore, if the resonator is designed so that the peak wavelength of the extracted light is within the desired range, the film thickness of the functional layer cannot be properly designed, and the efficiency of the light-emitting element cannot be achieved. On the other hand, if the film thickness of the functional layer is designed with the goal of improving the efficiency of the light-emitting element, the peak wavelength of the extracted light based on the resonator structure will deviate from the desired range, and color correction needs to be performed using a color filter or the like. In addition, the intensity of the light of the desired wavelength may not be sufficiently increased.
[0010] The present disclosure is made in view of the above problems, and aims to improve the light extraction efficiency based on the optical resonator structure and optimize the film thickness of the functional layer, thereby achieving high efficiency and long life of the light emitting element that outputs with a desired wavelength as the peak wavelength.
[0011] Solutions for solving technical problems
[0012] A light-emitting element, characterized in that it comprises: a light-reflective first electrode; a light-emitting layer arranged above the first electrode; a light-semi-transmissive second electrode arranged above the light-emitting layer; a first light-transmitting layer arranged to be in contact with the second electrode; and a second light-transmitting layer arranged to be in contact with the first light-transmitting layer, wherein a first optical resonator structure having a first wavelength as a peak wavelength is formed between a surface of the first electrode on the light-emitting layer side and a surface of the second electrode on the light-emitting layer side, wherein the first wavelength is a wavelength longer than a peak wavelength of light emitted from the light-emitting layer, and a second optical resonator structure having a second wavelength as a peak wavelength is formed between the surface of the first electrode on the light-emitting layer side and an interface between the first light-transmitting layer and the second light-transmitting layer, wherein the second wavelength is a wavelength shorter than the first wavelength, and a difference between the refractive index of the second light-transmitting layer and the refractive index of the first light-transmitting layer is greater than 0.3.
[0013] A light-emitting element, characterized in that it comprises: a light-reflective first electrode; a light-emitting layer arranged above the first electrode; a light-semi-transmissive second electrode arranged above the light-emitting layer; a first light-transmitting layer arranged to be in contact with the second electrode; and a second light-transmitting layer arranged to be in contact with the first light-transmitting layer, wherein a first optical resonator structure having a first wavelength as a peak wavelength is formed between a surface of the first electrode on the light-emitting layer side and a surface of the second electrode on the light-emitting layer side, wherein the first wavelength is a wavelength longer than a peak wavelength of light emitted from the light-emitting layer, and a second optical resonator structure having a second wavelength as a peak wavelength is formed between the surface of the first electrode on the light-emitting layer side and an interface between the first light-transmitting layer and the second light-transmitting layer, wherein the second wavelength is a wavelength shorter than the first wavelength, the first light-transmitting layer contains IZO or NbO, and the second light-transmitting layer contains silicon oxynitride.
[0014] A self-luminous panel is characterized in that a plurality of the above-mentioned light-emitting elements are formed on a substrate.
[0015] A self-luminous panel, characterized in that it comprises: a substrate, at least a portion of which is light-transmissive; a second light-transmissive layer, arranged above the light-transmissive portion of the substrate; a first light-transmissive layer, arranged to be in contact with the second light-transmissive layer; a light-semi-transmissive second electrode, arranged above the first light-transmissive layer; a light-emitting layer, arranged above the second electrode; and a light-reflective first electrode, arranged above the light-emitting layer, a first optical resonator structure having a first wavelength as a peak wavelength is formed between a surface of the first electrode on the light-emitting layer side and a surface of the second electrode on the light-emitting layer side, wherein the first wavelength is a wavelength longer than a peak wavelength of light emitted from the light-emitting layer, and a second optical resonator structure having a second wavelength as a peak wavelength is formed between a surface of the first electrode on the light-emitting layer side and an interface between the first light-transmissive layer and the second light-transmissive layer, wherein the second wavelength is a wavelength shorter than the first wavelength, and a difference between the refractive index of the second light-transmissive layer and the refractive index of the first light-transmissive layer is greater than 0.3.
[0016] A self-luminous panel, characterized in that it comprises: a substrate, at least a portion of which is light-transmissive; a second light-transmissive layer, arranged above the light-transmissive portion of the substrate; a first light-transmissive layer, arranged to be in contact with the second light-transmissive layer; a second light-semi-transmissive electrode, arranged above the first light-transmissive layer; a light-emitting layer, arranged above the second electrode; and a light-reflective first electrode, arranged above the light-emitting layer, a first optical resonator structure having a first wavelength as a peak wavelength is formed between a surface of the first electrode on the light-emitting layer side and a surface of the second electrode on the light-emitting layer side, wherein the first wavelength is a wavelength longer than a peak wavelength of light emitted from the light-emitting layer, a second optical resonator structure having a second wavelength as a peak wavelength is formed between a surface of the first electrode on the light-emitting layer side and an interface between the first light-transmissive layer and the second light-transmissive layer, wherein the second wavelength is a wavelength shorter than the first wavelength, the first light-transmissive layer contains IZO or NbO, and the second light-transmissive layer contains silicon oxynitride.
[0017] A method for manufacturing a self-luminous panel, characterized in that a light-reflective first electrode is formed on a substrate, a light-emitting layer is formed above the first electrode, a light-semi-transmissive second electrode is formed above the light-emitting layer, a first light-transmitting layer is formed in contact with the second electrode, and a second light-transmitting layer is formed in contact with the first light-transmitting layer, and a refractive index difference of 0.3 or more from that of the first light-transmitting layer is formed. In the formation of the second electrode, a first optical resonator structure having a first wavelength as a peak wavelength is formed between a surface of the first electrode on the light-emitting layer side and a surface of the second electrode on the light-emitting layer side, wherein the first wavelength is a wavelength longer than a peak wavelength of light emitted from the light-emitting layer. In the formation of the second light-transmitting layer, a second optical resonator structure having a second wavelength as a peak wavelength is formed between a surface of the first electrode on the light-emitting layer side and an interface between the first light-transmitting layer and the second light-transmitting layer, wherein the second wavelength is a wavelength shorter than the first wavelength, and the difference between the refractive index of the second light-transmitting layer and the refractive index of the first light-transmitting layer is 0.3 or more.
[0018] A method for manufacturing a self-luminous panel, characterized in that a light-reflective first electrode is formed on a substrate, a light-emitting layer is formed above the first electrode, a light-semi-transmissive second electrode is formed above the light-emitting layer, a first light-transmitting layer is formed in contact with the second electrode, and a second light-transmitting layer is formed in contact with the first light-transmitting layer, which has a refractive index difference of 0.3 or more from that of the first light-transmitting layer. In the formation of the second electrode, a first optical resonator structure having a first wavelength as a peak wavelength is formed between a surface of the first electrode on the light-emitting layer side and a surface of the second electrode on the light-emitting layer side, wherein the first wavelength is a wavelength longer than a peak wavelength of light emitted from the light-emitting layer. In the formation of the second light-transmitting layer, a second optical resonator structure having a second wavelength as a peak wavelength is formed between a surface of the first electrode on the light-emitting layer side and an interface between the first light-transmitting layer and the second light-transmitting layer, wherein the second wavelength is a wavelength shorter than the first wavelength. The first light-transmitting layer contains IZO or NbO, and the second light-transmitting layer contains silicon oxynitride.
[0019] A method for manufacturing a self-luminous panel, characterized in that a second light-transmitting layer is formed on a substrate, a first light-transmitting layer is formed in contact with the second light-transmitting layer, a second light-semi-transmitting electrode is formed in contact with the first light-transmitting layer, a light-emitting layer is formed above the second electrode, and a light-reflecting first electrode is formed above the light-emitting layer. In the formation of the second electrode, a first optical resonator structure having a first wavelength as a peak wavelength is formed between a surface of the first electrode on the light-emitting layer side and a surface of the second electrode on the light-emitting layer side, wherein the first wavelength is a wavelength longer than a peak wavelength of light emitted from the light-emitting layer. In the formation of the second light-transmitting layer, a second optical resonator structure having a second wavelength as a peak wavelength is formed between a surface of the first electrode on the light-emitting layer side and an interface between the first light-transmitting layer and the second light-transmitting layer, wherein the second wavelength is a wavelength shorter than the first wavelength, and a difference between the refractive index of the second light-transmitting layer and the refractive index of the first light-transmitting layer is greater than 0.3.
[0020] A method for manufacturing a self-luminous panel, characterized in that a second light-transmitting layer is formed on a substrate, a first light-transmitting layer is formed in contact with the second light-transmitting layer, a second light-semi-transmitting electrode is formed in contact with the first light-transmitting layer, a light-emitting layer is formed above the second electrode, and a light-reflecting first electrode is formed above the light-emitting layer. In the formation of the second electrode, a first optical resonator structure having a first wavelength as a peak wavelength is formed between a surface of the first electrode on the light-emitting layer side and a surface of the second electrode on the light-emitting layer side, wherein the first wavelength is a wavelength longer than a peak wavelength of light emitted from the light-emitting layer. In the formation of the second light-transmitting layer, a second optical resonator structure having a second wavelength as a peak wavelength is formed between a surface of the first electrode on the light-emitting layer side and an interface between the first light-transmitting layer and the second light-transmitting layer, wherein the second wavelength is a wavelength shorter than the first wavelength. The first light-transmitting layer contains IZO or NbO, and the second light-transmitting layer contains silicon oxynitride.
[0021] Effects of the Invention
[0022] According to the light emitting element of the above-described embodiment, by optimizing the film thickness of the light emitting layer and the functional layer existing between the first electrode and the second electrode, even if the peak wavelength of the first optical resonator structure formed between the first electrode and the second electrode is a wavelength longer than the desired wavelength, by setting the peak wavelength of the second optical resonator structure to a wavelength shorter than the first wavelength, the peak wavelength of the light extracted from the light emitting element can be set to the desired wavelength. Therefore, the film thickness of the functional layer can be optimized, and light with the desired wavelength as the peak wavelength can be extracted from the light emitting element by the combination of the two resonator structures, so that the light emitting element that outputs light with the desired wavelength as the peak wavelength can be improved in efficiency and its life can be extended. BRIEF DESCRIPTION OF THE DRAWINGS
[0023] Figure 1 It is a cross-sectional view schematically showing the structure of the organic EL element 1 according to the embodiment.
[0024] Figure 2 It is a schematic cross-sectional view for explaining interference of light in an optical resonator structure formed by the organic EL element 1 .
[0025] Figure 3 is a graph showing an emission spectrum of the first optical resonator structure and an emission spectrum of the organic EL element in a comparative example, Figure 3 (a) relates to Comparative Example 1, Figure 3 (b) relates to Comparative Example 2 in which the thickness of the functional layer is larger than that of Comparative Example 1.
[0026] Figure 4 (a) is a graph showing an emission spectrum of the first optical resonator structure and an emission spectrum of the organic EL element in the embodiment, Figure 4 (b) is a graph showing the influence of the difference in refractive index between the first optical adjustment layer and the second optical adjustment layer on the emission spectrum of the organic EL element.
[0027] Figure 5 This is a flowchart showing a process of manufacturing a self-luminous panel including an organic EL element according to an embodiment.
[0028] Figure 6 is a partial cross-sectional view schematically showing a part of a manufacturing process of a self-luminous panel according to an embodiment, and Figure 6 (a) shows a state where a TFT layer is formed on a substrate. Figure 6 (b) shows a state where an interlayer insulating layer is formed on the substrate. Figure 6 (c) shows a state where a pixel electrode material is formed on the interlayer insulating layer. Figure 6 (d) shows a state where a pixel electrode is formed. Figure 6(e) shows a state where a partition wall material layer is formed on the interlayer insulating layer and the pixel electrode.
[0029] Figure 7 is a partial cross-sectional view schematically showing a part of a manufacturing process of a self-luminous panel according to an embodiment, and Figure 7 (a) shows a state where a partition wall is formed, Figure 7 (b) shows a state where a hole injection layer is formed on the pixel electrode. Figure 7 (c) shows a state where a hole transport layer is formed on the hole injection layer. Figure 7 (d) shows a state where a light-emitting layer is formed on the hole injection layer.
[0030] Figure 8 is a partial cross-sectional view schematically showing a part of a manufacturing process of a self-luminous panel according to an embodiment, and Figure 8 (a) shows a state where an intermediate layer is formed on the light-emitting layer and the partition wall. Figure 8 (b) shows a state where an electron injection and transport layer is formed on the intermediate layer. Figure 8 (c) shows a state where a counter electrode is formed on the electron injection and transport layer. Figure 8 (d) shows a state where the first optical adjustment layer is formed on the counter electrode.
[0031] Fig. 9 is a partial cross-sectional view schematically showing a part of a manufacturing process of a self-luminous panel according to an embodiment, and Fig. 9 (a) shows a state where a second optical adjustment layer is formed on the first optical adjustment layer. Fig. 9 (d) shows a state where a third optical adjustment layer is formed on the second optical adjustment layer.
[0032] Fig.10 (a) is a schematic cross-sectional view of a light emitting element of Modification Example 1, Fig.10 (b) is a schematic cross-sectional view of a self-luminous panel having a light-emitting element according to variation example 2.
[0033] Fig.11 This is a block diagram showing the configuration of a display device according to an embodiment.
[0034] Description of Reference Numerals
[0035] 1…light-emitting element (organic EL element); 11…substrate; 12…interlayer insulating layer; 13…pixel electrode; 14…partition wall; 14a…opening; 15…hole injection layer; 16…hole transport layer; 17…light-emitting layer; 18…intermediate layer; 19…electron injection and transport layer; 20…counter electrode; 21…optical adjustment layer; 100…self-luminous panel (organic EL display panel); 200…drive control unit; 210 to 240…drive circuit; 250…control circuit. DETAILED DESCRIPTION
[0036] 《The process leading to one method of the present disclosure》
[0037] As a method for improving the light extraction efficiency of a light emitting element, an optical resonator structure is known. Specifically, Figure 2 As shown in the schematic cross-sectional view of (b), for example, the optical distance is adjusted so that the light through the path C1 directly released from the luminescent center and the light through the path C2 reflected and released from the luminescent center in the order of the light semi-transmissive electrode and the light reflective electrode reinforce each other. At this time, the optical path length difference between path C2 and path C1 depends on the sum of the optical path length of L0 (the value obtained by integrating the refractive index with the path length) and the optical path length of L1. At this time, the condition for mutual reinforcement of light depends on the relationship between the optical path length difference and the wavelength. The shorter the wavelength of the released light, the more it is necessary to shorten the optical path length of L0+L1. On the other hand, there is an optimal film thickness in the light-emitting layer or the functional layer other than the light-emitting layer (hole injection layer, hole transport layer, electron injection layer, electron transport layer). When the film thickness of the functional layer such as the light-emitting layer or the hole transport layer is insufficient, it is sometimes impossible to fully perform the function and the luminous efficiency is reduced. In particular, in elements with short emission wavelengths such as blue light-emitting elements, if the resonator structure is optimized, the film thickness of the functional layer will be insufficient and the luminous efficiency cannot be sufficiently improved. On the other hand, in a design in which the film thickness of the functional layer is sufficient, the optical path length of L0+L1 in the resonator structure becomes longer relative to the desired extraction wavelength. Therefore, there is a problem that the peak wavelength of the extracted light shifts to the long wavelength side and causes color deviation.
[0038] The inventors have studied optimization of both the resonator structure and the thickness of the functional layer, and have arrived at the present disclosure inspired by combining a plurality of resonators having different peak wavelengths.
[0039] "Open Way"
[0040] A light-emitting element according to one embodiment of the present disclosure is characterized in that it comprises: a light-reflective first electrode; a light-emitting layer arranged above the first electrode; a light-semi-transmissive second electrode arranged above the light-emitting layer; a first light-transmitting layer arranged to be in contact with the second electrode; and a second light-transmitting layer arranged to be in contact with the first light-transmitting layer, wherein a first optical resonator structure having a first wavelength as a peak wavelength is formed between a surface of the first electrode on the light-emitting layer side and a surface of the second electrode on the light-emitting layer side, wherein the first wavelength is a wavelength longer than a peak wavelength of light emitted from the light-emitting layer, and a second optical resonator structure having a second wavelength as a peak wavelength is formed between the surface of the first electrode on the light-emitting layer side and an interface between the first light-transmitting layer and the second light-transmitting layer, wherein the second wavelength is a wavelength shorter than the first wavelength, and a difference between a refractive index of the second light-transmitting layer and a refractive index of the first light-transmitting layer is greater than 0.3.
[0041] According to the light emitting element of the above-mentioned aspect, by optimizing the film thickness of the light emitting layer and the functional layer existing between the first electrode and the second electrode, even if the peak wavelength of the first optical resonator structure formed between the first electrode and the second electrode is a wavelength longer than the desired wavelength, by setting the peak wavelength of the second optical resonator structure to a wavelength shorter than the first wavelength, the peak wavelength of the light extracted from the light emitting element can be set to the desired wavelength. Therefore, the film thickness of the functional layer can be optimized, and light with the desired wavelength as the peak wavelength can be extracted from the light emitting element by the combination of the two resonator structures, so that the light emitting element that outputs with the desired wavelength as the peak wavelength can be improved in efficiency and a longer life can be achieved.
[0042] Furthermore, in the light emitting element of the above embodiment, the following may be adopted.
[0043] When the first wavelength is λ1, the optical distance from the surface of the first electrode on the light-emitting layer side to the light-emitting center is L0, and the optical distance from the light-emitting center to the surface of the second electrode on the light-emitting layer side is L1, it can be set as follows:
[0044]
[0045] in, is a phase change of light when reflected by the surface of the first electrode on the light-emitting layer side, is a phase change of light when reflected by the surface of the second electrode on the light emitting layer side, and m1 is an arbitrary natural number.
[0046] Thus, light having the first wavelength as a peak wavelength can be extracted through the first optical resonator structure.
[0047] In addition, when the second wavelength is λ2, the optical distance from the surface of the first electrode on the light-emitting layer side to the light-emitting center is L0, and the optical distance from the light-emitting center to the surface of the second optical adjustment layer on the light-emitting layer side is L2, it can be set as follows:
[0048]
[0049] in, is a phase change of light when reflected by the surface of the first electrode on the light-emitting layer side, is a phase change of light when reflected by the surface of the second optical adjustment layer on the light emitting layer side, and m2 is an arbitrary natural number.
[0050] Thus, light having the second wavelength as a peak wavelength can be extracted through the second optical resonator structure.
[0051] Furthermore, a difference between a peak wavelength of light emitted from the light emitting layer and a peak wavelength of light extracted outside the light emitting element obtained by combining light emitted from the first optical resonator structure and light emitted from the second optical resonator structure may be 15 nm or less.
[0052] Thus, the peak wavelength of light extracted from the light-emitting element can be brought close to the peak wavelength of light inside the light-emitting layer, and thus the light-emitting efficiency of the light-emitting element can be further improved.
[0053] In addition, it is also possible to further include a third light-transmitting layer, which is configured to be in contact with the second light-transmitting layer and includes one or more layers, and a third optical resonator structure is formed between the surface of the first electrode on the light-emitting layer side and the surface of any layer included in the third light-transmitting layer on the light-emitting layer side, and the optical distance between the surface of the second electrode on the light-emitting layer side and the upper surface of the third light-transmitting layer is less than 1 μm.
[0054] This makes it possible to design the peak wavelength of light extracted from the light emitting element via the third resonator structure in more detail.
[0055] Furthermore, the third optical resonator structure may be configured so as to weaken a peak wavelength of the first optical resonator structure.
[0056] This can reduce the azimuth dependency of the light intensity due to the first optical resonator structure, and thus reduce the variation in the intensity or peak wavelength of light extracted from the light emitting element depending on the viewing angle.
[0057] Furthermore, the third optical resonator structure may have a third wavelength between the first wavelength and the second wavelength as a peak wavelength.
[0058] Thus, even through the third optical resonator structure, light having a third wavelength near a desired peak wavelength as a peak wavelength can be extracted, and thus the light extraction efficiency of the light emitting element can be further improved.
[0059] In addition, a light-emitting element according to one embodiment of the present disclosure may include: a light-reflective first electrode; a light-emitting layer arranged above the first electrode; a light-semi-transmissive second electrode arranged above the light-emitting layer; a first light-transmitting layer arranged to be in contact with the second electrode; and a second light-transmitting layer arranged to be in contact with the first light-transmitting layer, wherein a first optical resonator structure having a first wavelength as a peak wavelength is formed between a surface of the first electrode on the light-emitting layer side and a surface of the second electrode on the light-emitting layer side, wherein the first wavelength is a wavelength longer than a peak wavelength of light emitted from the light-emitting layer, and a second optical resonator structure having a second wavelength as a peak wavelength is formed between the surface of the first electrode on the light-emitting layer side and an interface between the first light-transmitting layer and the second light-transmitting layer, wherein the second wavelength is a wavelength shorter than the first wavelength, the first light-transmitting layer contains IZO or NbO, and the second light-transmitting layer contains silicon oxynitride.
[0060] In the light-emitting element of the above-described method, since the film thickness of the light-emitting layer and the functional layer existing between the first electrode and the second electrode is optimized, even if the peak wavelength of the first optical resonator structure formed between the first electrode and the second electrode is a wavelength longer than the desired wavelength, by setting the peak wavelength of the second optical resonator structure to a wavelength shorter than the first wavelength, i.e., the second wavelength, the peak wavelength of the light extracted from the light-emitting element can be set to the desired wavelength. Therefore, the film thickness of the functional layer can be optimized, and light with the desired wavelength as the peak wavelength can be extracted from the light-emitting element by the combination of the two resonator structures, so that the light-emitting element that outputs light with the desired wavelength as the peak wavelength can be made more efficient and have a longer life.
[0061] Furthermore, the self-luminous panel according to one aspect of the present disclosure may be a self-luminous panel in which a plurality of light-emitting elements according to one aspect of the present disclosure are formed on a substrate.
[0062] Thus, a top emission type self-luminous panel including the light emitting element according to one embodiment of the present disclosure can be realized.
[0063] In addition, a self-luminous panel of one embodiment of the present disclosure may include: a substrate, at least a portion of which is light-transmissive; a second light-transmissive layer, arranged above the light-transmissive portion of the substrate; a first light-transmissive layer, arranged to be in contact with the second light-transmissive layer; a light-semi-transmissive second electrode, arranged above the first light-transmissive layer; a light-emitting layer, arranged above the second electrode; and a light-reflective first electrode, arranged above the light-emitting layer, a first optical resonator structure having a first wavelength as a peak wavelength is formed between a surface of the first electrode on the light-emitting layer side and a surface of the second electrode on the light-emitting layer side, wherein the first wavelength is a wavelength longer than a peak wavelength of light emitted from the light-emitting layer, and a second optical resonator structure having a second wavelength as a peak wavelength is formed between a surface of the first electrode on the light-emitting layer side and an interface between the first light-transmissive layer and the second light-transmissive layer, wherein the second wavelength is a wavelength shorter than the first wavelength, and a difference between the refractive index of the second light-transmissive layer and the refractive index of the first light-transmissive layer is greater than 0.3.
[0064] Thus, a bottom emission type self-luminous panel including the light emitting element according to one embodiment of the present disclosure can be realized.
[0065] In addition, a self-luminous panel of one embodiment of the present disclosure may include: a substrate, at least a portion of which is light-transmissive; a second light-transmissive layer, arranged above the light-transmissive portion of the substrate; a first light-transmissive layer, arranged to be in contact with the second light-transmissive layer; a light-semi-transmissive second electrode, arranged above the first light-transmissive layer; a light-emitting layer, arranged above the second electrode; and a light-reflective first electrode, arranged above the light-emitting layer, a first optical resonator structure having a first wavelength as a peak wavelength is formed between a surface of the first electrode on the light-emitting layer side and a surface of the second electrode on the light-emitting layer side, wherein the first wavelength is a wavelength longer than a peak wavelength of light emitted from the light-emitting layer, and a second optical resonator structure having a second wavelength as a peak wavelength is formed between a surface of the first electrode on the light-emitting layer side and an interface between the first light-transmissive layer and the second light-transmissive layer, wherein the second wavelength is a wavelength shorter than the first wavelength, the first light-transmissive layer contains IZO or NbO, and the second light-transmissive layer contains silicon oxynitride.
[0066] Thus, a bottom emission type self-luminous panel including the light emitting element according to one embodiment of the present disclosure can be realized.
[0067] In addition, a method for manufacturing a self-luminous panel according to one embodiment of the present disclosure is characterized in that a light-reflective first electrode is formed on a substrate, a light-emitting layer is formed above the first electrode, a light-semi-transmissive second electrode is formed for the light-emitting layer, a first light-transmitting layer is formed in contact with the second electrode, and a second light-transmitting layer is formed in contact with the first light-transmitting layer, and a refractive index difference of 0.3 or more from that of the first light-transmitting layer is formed. In the formation of the second electrode, a first optical resonator structure having a first wavelength as a peak wavelength is formed between a surface of the first electrode on the light-emitting layer side and a surface of the second electrode on the light-emitting layer side, wherein the first wavelength is a wavelength longer than a peak wavelength of light emitted from the light-emitting layer. In the formation of the second light-transmitting layer, a second optical resonator structure having a second wavelength as a peak wavelength is formed between a surface of the first electrode on the light-emitting layer side and an interface between the first light-transmitting layer and the second light-transmitting layer, wherein the second wavelength is a wavelength shorter than the first wavelength, and the difference between the refractive index of the second light-transmitting layer and the refractive index of the first light-transmitting layer is 0.3 or more.
[0068] In addition, in a method for manufacturing a self-luminous panel according to one embodiment of the present disclosure, a light-reflective first electrode is formed on a substrate, a light-emitting layer is formed above the first electrode, a light-semi-transmissive second electrode is formed for the light-emitting layer, a first light-transmitting layer is formed in contact with the second electrode, and a second light-transmitting layer having a refractive index difference of 0.3 or more from that of the first light-transmitting layer is formed in contact with the first light-transmitting layer. In the formation of the second electrode, a first optical resonator structure having a first wavelength as a peak wavelength is formed between a surface of the first electrode on the light-emitting layer side and a surface of the second electrode on the light-emitting layer side, wherein the first wavelength is a wavelength longer than a peak wavelength of light emitted from the light-emitting layer. In the formation of the second light-transmitting layer, a second optical resonator structure having a second wavelength as a peak wavelength is formed between a surface of the first electrode on the light-emitting layer side and an interface between the first light-transmitting layer and the second light-transmitting layer, wherein the second wavelength is a wavelength shorter than the first wavelength. The first light-transmitting layer contains IZO or NbO, and the second light-transmitting layer contains silicon oxynitride.
[0069] In addition, a method for manufacturing a self-luminous panel according to one embodiment of the present disclosure is characterized in that a second light-transmitting layer is formed on a substrate, a first light-transmitting layer is formed in contact with the second light-transmitting layer, a second light-transmitting electrode is formed in contact with the first light-transmitting layer, a light-emitting layer is formed above the second electrode, and a light-reflective first electrode is formed above the light-emitting layer. In the formation of the second electrode, a first optical resonator structure having a first wavelength as a peak wavelength is formed between a surface of the first electrode on the light-emitting layer side and a surface of the second electrode on the light-emitting layer side, wherein the first wavelength is a wavelength longer than a peak wavelength of light emitted from the light-emitting layer. In the formation of the second light-transmitting layer, a second optical resonator structure having a second wavelength as a peak wavelength is formed between a surface of the first electrode on the light-emitting layer side and an interface between the first light-transmitting layer and the second light-transmitting layer, wherein the second wavelength is a wavelength shorter than the first wavelength, and a difference between a refractive index of the second light-transmitting layer and a refractive index of the first light-transmitting layer is greater than 0.3.
[0070] In addition, in a method for manufacturing a self-luminous panel according to one embodiment of the present invention, a second light-transmitting layer is formed on a substrate, a first light-transmitting layer is formed in contact with the second light-transmitting layer, a second light-transmitting electrode is formed in contact with the first light-transmitting layer, a light-emitting layer is formed above the second electrode, and a light-reflective first electrode is formed above the light-emitting layer. In the formation of the second electrode, a first optical resonator structure having a first wavelength as a peak wavelength is formed between a surface of the first electrode on the light-emitting layer side and a surface of the second electrode on the light-emitting layer side, wherein the first wavelength is a wavelength longer than a peak wavelength of light emitted from the light-emitting layer. In the formation of the second light-transmitting layer, a second optical resonator structure having a second wavelength as a peak wavelength is formed between a surface of the first electrode on the light-emitting layer side and an interface between the first light-transmitting layer and the second light-transmitting layer, wherein the second wavelength is a wavelength shorter than the first wavelength. The first light-transmitting layer contains IZO or NbO, and the second light-transmitting layer contains silicon oxynitride.
[0071] Implementation Method
[0072] The following is a description of an embodiment of a self-luminous panel having a light-emitting element disclosed in the present invention. In addition, the following description is an example for illustrating the structure and function / effect of one embodiment of the present invention, and is not limited to the following embodiment except for the essential part of the present invention. In addition, the up and down in this specification and claims including the following description are relative positional relationships based on the light emission direction, and may not necessarily be consistent with the absolute (vertical) up and down positional relationship.
[0073] 1. Composition of organic EL elements
[0074] Figure 1 The organic EL display panel 100 (see Fig.11 ). The organic EL display panel 100 has a plurality of pixels composed of organic EL elements 1(R), 1(G), and 1(B) that emit light of three colors (red, green, and blue). That is, the organic EL elements 1(R), 1(G), and 1(B) each constitute a sub-pixel, and a collection of a plurality of sub-pixels with different luminous colors constitutes a pixel. Figure 1 , a cross section of one pixel is shown.
[0075] In the organic EL display panel 100, each organic EL element 1 is oriented toward the front ( Figure 1 The so-called top emission type that emits light (above the paper surface in the figure).
[0076] The organic EL element 1 (R), the organic EL element 1 (G), and the organic EL element 1 (B) have substantially the same configuration, and therefore, when not distinguished, they are described as the organic EL element 1 .
[0077] like Figure 1 As shown, the organic EL element 1 includes a substrate 11, an interlayer insulating layer 12, a pixel electrode 13, a partition wall 14, a hole injection layer 15, a hole transport layer 16, a light emitting layer 17, an intermediate layer 18, an electron injection and transport layer 19, an opposing electrode 20, and an optical adjustment layer 21. The optical adjustment layer 21 includes a first optical adjustment layer 211, a second optical adjustment layer 212, and a third optical adjustment layer 213 from the opposing electrode 20 side. The pixel electrode 13 and the opposing electrode 20 correspond to the first electrode and the second electrode of the present disclosure, respectively. In addition, the first optical adjustment layer 211 and the second optical adjustment layer 212 correspond to the first light-transmitting layer and the second light-transmitting layer of the present disclosure, respectively.
[0078] In addition, the substrate 11, the interlayer insulating layer 12, the intermediate layer 18, the electron injection and transport layer 19, the counter electrode 20, the first optical adjustment layer 211, the second optical adjustment layer 212 and the third optical adjustment layer 213 are not formed for each pixel, but are formed in common on the multiple organic EL elements 1 possessed by the organic EL display panel 100.
[0079] <Substrate>
[0080] The substrate 11 includes a TFT (Thin Film Transistor) layer 112 and a base material 111 as an insulating material. A driving circuit is formed in each sub-pixel in the TFT layer 112. The base material 111 can be, for example, a glass substrate, a quartz substrate, a plastic substrate, etc. As a plastic material, any resin of a thermoplastic resin or a thermosetting resin can be used. For example, polyimide (PI), polyetherimide (PEI), polysulfone (PSu), polycarbonate (PC), polyethylene terephthalate (PET), polyethylene naphthalate (PEN), polybutylene terephthalate, various thermoplastic elastomers such as styrene, polyolefin, and polyurethane, epoxy resins, unsaturated polyesters, silicone resins, polyurethanes, etc., or copolymers, blends, polymer alloys, etc. mainly based on them can be cited. A laminated body obtained by selecting and stacking one or more of them in a manner that is durable to the process temperature can be used.
[0081] <Interlayer insulation layer>
[0082] The interlayer insulating layer 12 is formed on the substrate 11. The interlayer insulating layer 12 includes a resin material for flattening the step on the upper surface of the TFT layer 112. As the resin material, for example, a positive photosensitive material can be cited. In addition, as such a photosensitive material, acrylic resin, polyimide resin, siloxane resin, phenolic resin, etc. can be cited. In addition, although Figure 1 Although not shown in the cross-sectional view of FIG. 1 , a contact hole is formed in the interlayer insulating layer 12 for each sub-pixel.
[0083] <Pixel electrode>
[0084] The pixel electrode 13 is formed on the interlayer insulating layer 12. The pixel electrode 13 is provided for each pixel and is electrically connected to the TFT layer 112 through a contact hole provided in the interlayer insulating layer 12.
[0085] In this embodiment, the pixel electrode 13 functions as a light-reflective anode.
[0086] Specific examples of metal materials with light reflectivity include Ag (silver), Al (aluminum), aluminum alloys, Mo (molybdenum), APC (an alloy of silver, palladium and copper), ARA (an alloy of silver, rubidium and gold), MoCr (an alloy of molybdenum and chromium), MoW (an alloy of molybdenum and tungsten), NiCr (an alloy of nickel and chromium), etc.
[0087] The pixel electrode 13 is formed of a single metal layer, but may also have a stacked structure in which a layer including a metal oxide such as ITO (indium tin oxide) or IZO (indium zinc oxide) is stacked on the metal layer.
[0088] <Partition wall>
[0089] The partition wall 14 is formed on the pixel electrode 13 while exposing a portion of the upper surface of the pixel electrode 13 and covering the surrounding area. The area (hereinafter referred to as the "opening") not covered by the partition wall 14 on the upper surface of the pixel electrode 13 corresponds to the sub-pixel. That is, the partition wall 14 has an opening 14a provided for each sub-pixel.
[0090] In this embodiment, the partition wall 14 is formed on the interlayer insulating layer 12 in a portion where the pixel electrode 13 is not formed. That is, in a portion where the pixel electrode 13 is not formed, the bottom surface of the partition wall 14 is in contact with the upper surface of the interlayer insulating layer 12.
[0091] The partition wall 14 includes, for example, an insulating organic material (e.g., acrylic resin, polyimide resin, Novolac resin, phenolic resin, etc.). The partition wall 14 functions as a structure for preventing the applied ink from overflowing when the light-emitting layer 17 is formed by a coating method, and functions as a structure for mounting a vapor deposition mask when the light-emitting layer 17 is formed by a vapor deposition method. In the present embodiment, the partition wall 14 includes a resin material, and as the material of the partition wall 14, acrylic resin, polyimide resin, siloxane resin, and phenolic resin can be cited. In the present embodiment, a phenolic resin is used.
[0092] <Hole injection layer>
[0093] The hole injection layer 15 is provided on the pixel electrode 13 to promote injection of holes (pores) from the pixel electrode 13 to the light emitting layer 17. Specific examples of the material of the hole injection layer 15 include conductive polymer materials such as PEDOT / PSS (a mixture of polythiophene and polystyrene sulfonic acid).
[0094] In addition, the hole injection layer 15 may be formed of an oxide of a transition metal. Specific examples of transition metals include Ag (silver), Mo (molybdenum), Cr (chromium), V (vanadium), W (tungsten), Ni (nickel), Ir (iridium), etc. Transition metals have multiple oxidation numbers and can therefore take multiple energy levels, resulting in easier hole injection, which helps reduce the driving voltage. In this case, it is preferred that the hole injection layer 15 has a large work function.
[0095] Alternatively, the hole injection layer 15 may have a laminated structure in which a conductive polymer material is laminated on a transition metal oxide.
[0096] <Hole transport layer>
[0097] The hole transport layer 16 has the function of transporting the holes injected from the hole injection layer 15 to the light-emitting layer 17. The hole transport layer 16 efficiently transports the holes from the hole injection layer 15 to the light-emitting layer 17, and is therefore formed of an organic material with high hole mobility. The hole transport layer 16 is formed by applying and drying an organic material solution. As the organic material forming the hole transport layer 16, a polymer compound such as polyfluorene or a derivative thereof, or polyarylamine or a derivative thereof can be used.
[0098] In addition, the hole transport layer 16 can also be formed using triazole derivatives, oxadiazole derivatives, imidazole derivatives, polyarylalkyl derivatives, pyrazoline derivatives and pyrazolone derivatives, phenylenediamine derivatives, aromatic amine derivatives, amino-substituted chalcone derivatives, oxazole derivatives, styryl anthracene derivatives, fluorenone derivatives, hydrazone derivatives, stilbene derivatives, porphyrin compounds, aromatic tertiary amine compounds and styrylamine compounds, butadiene compounds, polystyrene derivatives, hydrazone derivatives, triphenylmethane derivatives, and tetraphenylbenzene derivatives. It can also be that porphyrin compounds, aromatic tertiary amine compounds, and styrylamine compounds are particularly preferably used. In this case, the hole transport layer 16 is formed by vacuum evaporation. In addition, the material and manufacturing method of the hole transport layer 16 are not limited to the above content, and any material having a hole transport function can be used, and it can also be formed by any manufacturing method that can be used for the manufacture of the hole transport layer 16.
[0099] <Luminous layer>
[0100] The light emitting layer 17 is formed in the opening 14a. The light emitting layer 17 has a function of emitting light of each color of R, G, and B by recombination of holes and electrons. As the material of the light emitting layer 17, a known material can be used.
[0101] When the light-emitting element 1 is an organic EL element, as the organic light-emitting material contained in the light-emitting layer 17, for example, hydroxyquinoline compounds, perylene compounds, coumarin compounds, azacoumarin compounds, oxazole compounds, oxadiazole compounds, perinone compounds, pyrrolopyrrole compounds, naphthalene compounds, anthracene compounds, fluorene compounds, fluoranthene compounds, tetracene compounds, pyrene compounds, coronene compounds, quinolone compounds and azaquinolone compounds, pyrazoline derivatives and pyrazolone derivatives, rhodamine compounds, Compounds, phenanthrene compounds, cyclopentadiene compounds, stilbene compounds, diphenylquinone compounds, styryl compounds, butadiene compounds, dicyanomethylenepyran compounds, dicyanomethylenethiopyran compounds, fluorescein compounds, pyrylium compounds, thiopyrylium compounds, selenopyrylium compounds, telluropyrylium compounds, aromatic canrenone (Aldadiene) compounds, oligophenylene compounds, thioxanthene compounds, cyanine compounds, acridine compounds, metal complexes of 8-hydroxyquinoline compounds, metal complexes of 2-bipyridine compounds, complexes of Schiff salts and group III metals, hydroxyquinoline metal complexes, rare earth complexes and other fluorescent substances. In addition, known phosphorescent substances such as metal complexes that emit phosphorescence such as tris (2-phenylpyridine) iridium can be used. In addition, the light-emitting layer 17 can also be formed using polymer compounds such as polyfluorene or its derivatives, polyphenyl or its derivatives, or polyarylamine or its derivatives, or a mixture of the low molecular weight compound and the polymer compound. Furthermore, the light-emitting element 1 may be a quantum dot light-emitting element (QLED; Quantum-dot Light Emitting Diode), and as the material of the light-emitting layer 17 , a material having a quantum dot effect may be used.
[0102] <Middle layer>
[0103] The intermediate layer 18 is formed on the light-emitting layer 17 and includes a fluoride or a quinoline complex of a metal material having electron injection properties. As the metal material, it can be selected from alkali metals or alkaline earth metals. Specifically, the alkali metal is Li (lithium), Na (sodium), K (potassium), Rb (rubidium), Cs (cesium), Fr (francium). In addition, specifically, the alkaline earth metal is Ca (calcium), Sr (strontium), Ba (barium), Ra (radium). In this embodiment, NaF (sodium fluoride) is included.
[0104] <Electron injection and transport layer>
[0105] The electron injection transport layer 19 is formed on the intermediate layer 18, and is formed by doping a metal material that improves the electron injection property in an organic material having electron transport properties. Among them, doping refers to dispersing the metal atoms or metal ions of the metal material roughly evenly into the organic material, specifically, it refers to forming a single phase containing organic materials and trace amounts of metal materials. In addition, it is preferred that there is no phase other than it, especially a phase that only includes metal materials such as a metal sheet or a metal film, or a phase with metal materials as the main component. In addition, in a single phase containing organic materials and trace amounts of metal materials, the concentration of metal atoms or metal ions is preferably uniform, and the metal atoms or metal ions are preferably not condensed. As a metal material, it is preferably selected from rare earth metals, and Yb (ytterbium) is more preferred. In this embodiment, Yb is selected. In addition, the doping amount of the metal material in the electron injection transport layer 19 is preferably 3 to 60wt%. In this embodiment, it is 20wt%.
[0106] Examples of the organic material having an electron transporting property include π-electron low-molecular organic materials such as oxadiazole derivatives (OXD), triazole derivatives (TAZ), and phenanthroline derivatives (BCP, Bphen).
[0107] <Countering Electrode>
[0108] The counter electrode 20 is made of a light-semi-transmissive conductive material, and is formed on the electron injection and transport layer 19. In the present embodiment, the counter electrode 20 functions as a cathode.
[0109] The light reflection surface of the interface between the counter electrode 20 and the electron injection transport layer 19 and the light reflection surface of the interface between the pixel electrode 13 and the hole injection layer 15 form a pair to form a resonator structure. Therefore, when the light emitted from the light emitting layer 17 is incident from the electron injection transport layer 19 to the counter electrode 20, part of it needs to be reflected by the electron injection transport layer 19. Therefore, it is preferred that the refractive index is different between the counter electrode 20 and the electron injection transport layer 19. Therefore, the counter electrode 20 is preferably a metal thin film. In order to ensure light semi-transmittance, the film thickness of the metal layer is about 1nm to 50nm.
[0110] As the material of the counter electrode 20, for example, Ag, a silver alloy with Ag as the main component, Al, and an Al alloy with Al as the main component can be cited. As the Ag alloy, magnesium-silver alloy (MgAg) and indium-silver alloy can be cited. Ag basically has a low resistivity, and the Ag alloy is preferred in terms of excellent heat resistance and corrosion resistance and the ability to maintain good conductivity for a long time. As the Al alloy, magnesium-aluminum alloy (MgAl) and lithium-aluminum alloy (LiAl) can be cited. As other alloys, lithium-magnesium alloy and lithium-indium alloy can be cited. In the present embodiment, the counter electrode 20 is a thin film of Ag.
[0111] <First optical adjustment layer>
[0112] The first optical adjustment layer 211 includes a light-transmitting material and is formed on the counter electrode 20 .
[0113] The light reflection surface of the interface between the first optical adjustment layer 211 and the second optical adjustment layer 212 and the light reflection surface of the interface between the pixel electrode 13 and the hole injection layer 15 form a pair to form a resonator structure. Therefore, when the light emitted from the light emitting layer 17 is incident from the first optical adjustment layer 211 to the second optical adjustment layer 212, a part of it needs to be reflected toward the first optical adjustment layer 211. Therefore, it is preferable that the refractive index is different between the first optical adjustment layer 211 and the second optical adjustment layer 212. For example, the material of the optical adjustment layer 211 and the material of the second optical adjustment layer 212 can be selected so that the difference in refractive index is greater than 0.3.
[0114] As the material of the first optical adjustment layer 211, for example, ITO, IZO, zinc oxide (ZnO), niobium oxide (NbO), titanium oxide (TiO), a mixed material of niobium oxide and titanium oxide, gallium oxide (GaO), molybdenum oxide (MoO), tantalum oxide (TaO), a mixed material of titanium oxide and zinc oxide, a mixed material of zinc oxide, gallium oxide and silicon oxide (SiO), a mixed material of tin oxide (SnO) and silicon oxide, etc. can be cited. In particular, niobium oxide has a high refractive index and is therefore more preferred. In the present embodiment, the first optical adjustment layer 21 includes niobium oxide. In addition, the first optical adjustment layer 211 is located on the opposite side of the pixel electrode 13 with respect to the counter electrode 20, so it is not necessary to have conductivity, but it is preferred in that the sheet resistance of the counter electrode 20 can be reduced when it has conductivity.
[0115] <Second optical adjustment layer>
[0116] The second optical adjustment layer 212 includes a light-transmitting material and is formed on the first optical adjustment layer 211 .
[0117] The light reflection surface of the interface between the first optical adjustment layer 211 and the second optical adjustment layer 212 and the light reflection surface of the interface between the pixel electrode 13 and the hole injection layer 15 form a pair to form a resonator structure. Therefore, when the light emitted from the light emitting layer 17 is incident from the first optical adjustment layer 211 to the second optical adjustment layer 212, part of it needs to be reflected toward the first optical adjustment layer 211. Therefore, it is preferable that the refractive index is different between the first optical adjustment layer 211 and the second optical adjustment layer 212. For example, the material of the optical adjustment layer 211 and the material of the second optical adjustment layer 212 can be selected so that the difference in refractive index is greater than 0.3.
[0118] As the material of the second optical adjustment layer 212, for example, silicon oxynitride (SiON), silicon nitride (SiN), etc. can be cited. In addition, the second optical adjustment layer 212 can also be a resin material such as acrylic resin, silicone resin, etc. For example, when the material of the first optical adjustment layer 211 is IZO or niobium oxide, silicon oxynitride can be used as the material of the second optical adjustment layer 212. In this embodiment, the second optical adjustment layer 212 includes silicon oxynitride. In addition, the combination of the first optical adjustment layer 211 and the second optical adjustment layer 212 is not limited to the above content, but preferably has a different refractive index.
[0119] <Third optical adjustment layer>
[0120] The third optical adjustment layer 213 includes a light-transmitting material and is formed on the second optical adjustment layer 212 .
[0121] The third optical adjustment layer 213 functions as a sealing layer for protecting the second optical adjustment layer 212. In addition, the interface between the second optical adjustment layer 212 and the third optical adjustment layer 213 and the light reflecting surface of the interface between the pixel electrode 13 and the hole injection layer 15 may form a resonator structure in pairs. As the material of the third optical adjustment layer 213, for example, silicon oxynitride (SiON), silicon nitride (SiN), etc. may be cited. In addition, the third optical adjustment layer 212 may also be a resin material such as acrylic resin, silicone resin, etc. In this embodiment, the third optical adjustment layer 213 includes silicon nitride.
[0122] <Other>
[0123] In addition, although not Figure 1 , a color filter or an upper substrate may be bonded via a sealing resin on the third optical adjustment layer 213. By bonding the upper substrate, the hole transport layer 16, the light emitting layer 17, the intermediate layer 18, and the electron injection transport layer 19 can be protected from moisture, air, and the like.
[0124] 2. Optical resonator structure
[0125] (2.1) Details of the optical resonator structure
[0126] Figure 2 1 is a diagram for explaining interference of light in the optical resonator structure of the organic EL element 1 of the present embodiment. The first optical resonator structure is formed between the surface of the pixel electrode 13 on the hole injection layer 15 side and the surface of the counter electrode 20 on the electron injection transport layer 19 side. In addition, the second optical resonator structure is formed between the surface of the pixel electrode 13 on the hole injection layer 15 side and the surface of the second optical adjustment layer 212 on the first optical adjustment layer 211 side. The light emitting layer 17 exists inside the first optical resonator structure and inside the second optical resonator structure.
[0127] exist Figure 2 1 and 2 show the main paths of light emitted from the light emitting layer 17. Path C1 is a path in which light emitted from the light emitting layer 17 to the counter electrode 20 side passes through the counter electrode 20 without being reflected. Path C2 is a path in which light emitted from the light emitting layer 17 to the counter electrode 20 side is reflected by the surface of the counter electrode 20 on the electron injection and transport layer 19 side, and further reflected by the surface of the pixel electrode 13 on the hole injection layer 15 side, and passes through the light emitting layer 17 and the counter electrode 20. Path C3 is a path in which light emitted from the light emitting layer 17 to the counter electrode 20 side passes through the counter electrode 20 and is reflected by the surface of the second optical adjustment layer 212 on the first optical adjustment layer 211 side, and further reflected by the surface of the pixel electrode 13 on the hole injection layer 15 side, and passes through the light emitting layer 17, the counter electrode 20, and the second optical adjustment layer 212. In the first optical resonator structure, interference occurs between light emitted through path C1 and light emitted through path C2. In the second optical resonator structure, interference occurs between the light emitted through the path C1 and the light emitted through the path C3 . Furthermore, the light emitted by the first optical resonator structure and the light emitted by the second optical resonator structure are further combined to become the light emitted from the light emitting element 1 .
[0128] The difference in optical distance between path C1 and path C2 corresponds to Figure 2 The optical film thickness L is the sum of the optical film thickness L0 and the optical film thickness L1. 1t The optical film thickness refers to the value obtained by integrating the refractive index of the film with the film thickness. More specifically, the optical film thickness L 1t is the sum of the refractive index of the hole injection layer 15×the thickness of the hole injection layer 15, the refractive index of the hole transport layer 16×the thickness of the hole transport layer 16, the refractive index of the light emitting layer 17×the thickness of the light emitting layer 17, the refractive index of the intermediate layer 18×the thickness of the intermediate layer 18, and the refractive index of the electron injection transport layer 19×the thickness of the electron injection transport layer 19. Similarly, the difference in optical distance between the path C1 and the path C3 corresponds to the value of Figure 2 The optical film thickness L is the sum of the optical film thickness L0 and the optical film thickness L2. 2t .
[0129] In the first optical resonator structure, the optical film thickness L is set to 1t , so that the light emitted through the path C1 and the light emitted through the path C2 reinforce each other. In addition, in the second optical resonator structure, the optical film thickness L is set 2t, so that the light emitted through the path C1 and the light emitted through the path C3 reinforce each other. At this time, when the peak wavelength (wavelength in vacuum, the same in this specification and claims) of the emitted light from the counter electrode 20 obtained by the first optical resonator structure is set to λ1, the following relationship holds between λ1 and the optical distance.
[0130]
[0131] in, is the phase change of light when it is reflected by the surface of the pixel electrode 13 on the hole injection layer 15 side. It is a phase change of light when it is reflected by the surface of the counter electrode 20 on the electron injection and transport layer 19 side. In addition, m1 is an arbitrary natural number.
[0132] Similarly, when the peak wavelength of the outgoing light from the second optical adjustment layer 212 obtained by the second optical resonator structure is λ2, the following relationship holds between λ2 and the optical distance.
[0133]
[0134] in, It is a phase change of light when it is reflected by the surface of the second optical adjustment layer 212 on the first optical adjustment layer 211 side. In addition, m2 is an arbitrary natural number.
[0135] In the light emitting element 1 of the present embodiment, the peak wavelength λ1 of the first optical resonator structure and the peak wavelength λ2 of the second optical resonator structure, and the peak wavelength λ s , and the peak wavelength λ of the light emitted in the light-emitting layer 17 have the following relationship.
[0136] λ2<λ s <λ1…(Formula 3)
[0137] By satisfying Formula 3, even if the peak wavelength λ1 of the first optical resonator structure is larger than the peak wavelength λ of the light extracted from the light emitting element 1 s Even if the wavelength is longer, light having a desired wavelength as a peak wavelength can be extracted from the light emitting element 1.
[0138] In addition, in the light emitting element 1 of this embodiment, it is preferable that the following relationship exists.
[0139] λ-15[nm]<λ s <λ+15[nm]…(Formula 4)
[0140] λ s -20[nm]<λ1…(Formula 5)
[0141] λ2<λs +20[nm]…(Formula 6)
[0142] By satisfying Formula 4, most of the light extracted from the light-emitting layer can be set as light extracted from the light-emitting element 1, so it is possible to improve the light-emitting efficiency of the light-emitting element 1. In addition, by satisfying Formulas 5 and 6, the light extracted from the light-emitting layer by the first optical resonator structure and the second optical resonator structure can be efficiently extracted, which is effective for improving the light-emitting efficiency of the light-emitting element 1 and improving the light extraction efficiency.
[0143] (2.2) Effect of optical resonator structure
[0144] Figure 4 (a) Figure 3 Each of the schematic diagrams shows the effects of the optical resonator structure of the present embodiment or the comparative example.
[0145] As Comparative Example 1, Figure 3 (a) is a schematic diagram showing the emission spectrum of the conventional structure with λ1=λ2, where spectrum 311 shows the spectrum of light output from the first optical resonator structure, and spectrum 312 shows the spectrum of light output from the light emitting element. In contrast, as Comparative Example 2, Figure 3 (b) is a schematic diagram showing the emission spectrum of a light-emitting element in which the hole transport layer 16 or the light-emitting layer 17 is thickened relative to Comparative Example 1, where spectrum 321 shows the spectrum of light output from the first optical resonator structure, and spectrum 322 shows the spectrum of light output from the light-emitting element. In Comparative Example 2, the thickness of the light-emitting layer 17 is 8 nm greater than that of Comparative Example 1. As a result, the optical film thickness L0 and the optical film thickness L1 are increased, and therefore, λ1 and λ2 both become long wavelengths relative to Comparative Example 1. More specifically, in Comparative Example 1, λ s is approximately 450 nm, while in Comparative Example 2 s Therefore, if the desired wavelength to be extracted from the light emitting element is 450 nm, in order to avoid making the optical film thickness L 1t To achieve thicker hole transport layer 16 or light emitting layer 17 in a modified manner, it is necessary to reduce the thickness of electron injection transport layer 19 , which makes it difficult to optimize the thickness of each functional layer and extract light of a desired wavelength through an optical resonator structure.
[0146] In contrast, a schematic diagram showing the emission spectrum of this embodiment is shown in FIG. Figure 4Spectrum 331 is the spectrum of light output from the first optical resonator structure, spectrum 332 is the spectrum of light output from the second optical resonator structure, and spectrum 333 is the spectrum of light output from the light emitting element. In the present embodiment, as in Comparative Example 2, the hole transport layer 16 or the light emitting layer 17 is thickened, and the peak wavelength λ1 of the first optical resonator structure defined by the optical film thickness L0 and the optical film thickness L1 is on the longer wavelength side than in Comparative Example 1, as in Comparative Example 2. However, in the present embodiment, the optical film thickness L2 is designed so that the peak wavelength λ2 of the second optical resonator structure satisfies the above-mentioned relationship, that is, relative to the peak wavelength λ of the light extracted from the light emitting element 1. s Satisfying λ2<λ s Thus, the spectrum 333 of the light output from the light emitting element satisfies λ2<λ s <λ1, therefore, even in a state where λ1 is longer than the desired wavelength to be extracted from the light emitting element, light of a desired wavelength can be extracted.
[0147] also, Figure 4 (b) is a schematic diagram showing the relationship between the refractive index difference between the first optical adjustment layer 211 and the second optical adjustment layer 212 and the spectrum of light output from the light emitting element. In addition, spectrum 341 is the spectrum of light output from the first optical resonator structure. Spectra 351 to 366 are the spectrums of light output from the light emitting element, corresponding to the refractive index differences of 0.13, 0.30, 0.46, 0.63, and 0.79 between the first optical adjustment layer 221 and the second optical adjustment layer 222, respectively. Figure 4 As shown in (b), the greater the difference in refractive index between the first optical adjustment layer 211 and the second optical adjustment layer 212, the more the peak wavelength of the light output from the light emitting element shifts toward the shorter wavelength side. The reason for this is that the greater the difference in refractive index between the first optical adjustment layer 211 and the second optical adjustment layer 212, the greater the light reflectivity at the interface between the first optical adjustment layer 211 and the second optical adjustment layer 212, and thus it can be considered that the light output based on the second optical resonator structure becomes larger. Figure 4 As shown in (b), the larger the difference in refractive index between the first optical adjustment layer 211 and the second optical adjustment layer 212, the more preferably. The difference in refractive index between the first optical adjustment layer 211 and the second optical adjustment layer 212 is preferably 0.30 or more, for example.
[0148] 3. Summary
[0149] As described above, according to the light-emitting element of the embodiment, the peak wavelengths of light extracted by the first optical resonator structure formed between the pixel electrode and the counter electrode and the second optical resonator structure formed between the pixel electrode and the second optical adjustment layer are different. Therefore, the peak wavelength of the first optical resonator structure is designed to be longer than the peak wavelength of light to be extracted from the light-emitting element, and the peak wavelength of the second optical resonator structure is designed to be shorter than the peak wavelength of light to be extracted from the light-emitting element, so that the peak wavelength of light extracted from the light-emitting element can be increased without increasing the film thickness of the functional layer to achieve a wavelength longer than the desired wavelength. Therefore, the improvement of luminous efficiency due to the optimization of the film thickness of the functional layer or the improvement of efficiency and long life of the light-emitting element due to the reduction of the driving voltage can be achieved, and the light extraction efficiency from the light-emitting element at the desired wavelength can be improved.
[0150] 4. Method for manufacturing light-emitting element
[0151] A method for manufacturing a self-luminous panel including a light-emitting element will be described using the drawings. Figure 5 1 is a flowchart showing a manufacturing process of a self-luminous panel including light-emitting elements. Figure 6 (a)~(e), Figure 7 (a)~(d), Figure 8 (a)~(d), Fig. 9 (a) to (b) are schematic cross-sectional views showing states of each process in the manufacture of a self-luminous panel.
[0152] (1) First, Figure 6 As shown in (a) of FIG. 1 , the TFT layer 112 is formed on the base material 111 to form the substrate 11 (step S10 ). The TFT layer 112 can be formed by a known TFT manufacturing method.
[0153] (2) Formation of interlayer insulating layer 12
[0154] Then, if Figure 6 As shown in (b), the interlayer insulating layer 12 is formed on the substrate 11 (step S20). The interlayer insulating layer 12 can be formed by stacking using, for example, a plasma CVD method, a sputtering method, or the like.
[0155] Next, a contact hole is formed by dry etching at a portion on the source electrode of the TFT layer in the interlayer insulating layer 12. The contact hole is formed so that the surface of the source electrode is exposed at the bottom thereof.
[0156] Next, a connection electrode layer is formed along the inner wall of the contact hole. A portion of the upper portion of the connection electrode layer is disposed on the interlayer insulating layer 12. The connection electrode layer can be formed by, for example, sputtering, and after forming a metal film, patterning is performed using photolithography and wet etching.
[0157] (3) Formation of pixel electrode 13
[0158] Then, if Figure 6 As shown in (c), a pixel electrode material layer 130 is formed on the interlayer insulating layer 12. The pixel electrode material layer 130 can be formed by, for example, vacuum deposition or sputtering.
[0159] Then, if Figure 6 As shown in (d), the pixel electrode material layer 130 is patterned by etching to form a plurality of pixel electrodes 13 divided for each sub-pixel (step S30).
[0160] (4) Formation of partition wall 14
[0161] Then, if Figure 6 As shown in (e), a partition wall layer resin as a material of the partition wall 14 is applied to the pixel electrode 13 and the interlayer insulating layer 12 to form a partition wall material layer 140. The partition wall material layer 140 is formed by uniformly applying a solution in which a phenolic resin as a partition wall layer resin is dissolved in a solvent (for example, a mixed solvent of ethyl lactate and GBL) to the pixel electrode 13 and the interlayer insulating layer 12 using a spin coating method or the like. Then, the partition wall 14 ( Figure 7 (a)), the partition wall 14 is fired (step S40). Thus, the opening 14a which will become the formation region of the light emitting layer 17 is defined. The partition wall 14 is fired at a temperature of 150° C. to 210° C. for 60 minutes, for example.
[0162] In addition, in the process of forming the partition wall 14, the surface of the partition wall 14 may be treated with a predetermined alkaline solution, water, an organic solvent, etc., or subjected to plasma treatment. This is done to adjust the contact angle of the partition wall 14 with respect to the ink (solution) applied to the opening 14a or to impart hydrophobicity to the surface.
[0163] (5) Formation of the hole injection layer 15
[0164] Then, if Figure 7 As shown in (b), ink containing the constituent material of the hole injection layer 15 is ejected from the nozzle 401 of the inkjet head 410 to the opening 14a defined by the partition wall 14, applied to the pixel electrode 13 in the opening 14a, and fired (dried) to form the hole injection layer 15 (step S50).
[0165] In addition, the film formation of the hole injection layer 15 is not limited to the coating method, and can also be formed by evaporation or other methods. Alternatively, in the case where the hole injection layer 15 is also formed by evaporation or sputtering, after the formation of the pixel electrode material layer 130 in step 30, a hole injection material layer including the material of the hole injection layer 15 is formed on the pixel electrode material layer 130, and the pixel electrode material layer 130 and the hole injection material layer are patterned by the same patterning process to form a stacked structure of the pixel electrode 13 and the hole injection layer 15.
[0166] (6) Formation of the hole transport layer 16
[0167] Then, if Figure 7 As shown in (c), ink containing the constituent materials of the hole transport layer 16 is ejected from the nozzle 402 of the inkjet head 420 to the opening 14a specified by the partition wall 14, applied to the hole injection layer 15 in the opening 14a, and fired (dried) to form the hole transport layer 16 (step S60).
[0168] In addition, the film formation of the hole transport layer 16 is not limited to the coating method, and can also be formed by evaporation, etc. Furthermore, when the pixel electrode 13, the hole injection layer 15, and the hole transport layer 16 are all formed by evaporation or sputtering, as described above, each layer is patterned by the same patterning process.
[0169] (7) Formation of Light Emitting Layer 17
[0170] Then, if Figure 7 As shown in (d), ink containing constituent materials of the light-emitting layer 17 is ejected from nozzle 403R of inkjet head 430R, nozzle 403G of inkjet head 430G, and nozzle 403B of inkjet head 430B, respectively, applied to the hole transport layer 16 in the opening 14a, and fired (dried) to form the light-emitting layer 17 (step S70).
[0171] (8) Formation of Intermediate Layer 18
[0172] Then, if Figure 8 As shown in (a), the intermediate layer 18 is formed on the light emitting layer 17 and the partition wall 14 (step S80). The intermediate layer 18 is formed by, for example, forming NaF, which is an alkali metal fluoride, in common in each sub-pixel by vacuum deposition.
[0173] (9) Formation of the Electron Injection and Transport Layer 19
[0174] Then, if Figure 8As shown in (b), the electron injection transport layer 19 is formed on the intermediate layer 18 (step S90). The electron injection transport layer 19 is formed by, for example, forming a film of an electron transporting organic material and ytterbium as a doping metal in each sub-pixel by co-evaporation.
[0175] (10) Formation of Counter Electrode 20
[0176] Then, if Figure 8 As shown in (c), the counter electrode 20 is formed on the electron injection transport layer 19 (step S100). The counter electrode 20 is formed by forming a film of a metal material such as Ag or Al by sputtering or vacuum deposition, for example.
[0177] (11) Formation of the First Optical Adjustment Layer 211
[0178] Then, if Figure 8 As shown in (d) of FIG. 1 , the first optical adjustment layer 211 is formed (step S110 ). The first optical adjustment layer 211 is formed by depositing NbO by sputtering, for example.
[0179] (12) Formation of the Second Optical Adjustment Layer 212
[0180] Then, if Fig. 9 As shown in (a) of FIG. 1 , the second optical adjustment layer 212 is formed (step S120 ). The second optical adjustment layer 212 can be formed by, for example, sputtering or CVD using SiON.
[0181] (13) Formation of the Third Optical Adjustment Layer 213
[0182] Then, if Fig. 9 As shown in (b), the third optical adjustment layer 213 is formed (step S130). The third optical adjustment layer 213 can be formed by, for example, sputtering or CVD using SiN.
[0183] Furthermore, a layer having a sealing function may be further formed on the third optical adjustment layer 213 , or a color filter or an upper substrate may be placed and bonded.
[0184] 5. Overall structure of the display device
[0185] Fig.10 1 is a schematic block diagram showing the structure of a display device 1000 having a self-luminous panel 100. Fig.10 As shown, the display device 1000 includes a self-luminous panel 100 and a drive control unit 200 connected thereto. The drive control unit 200 includes four drive circuits 210 to 240 and a control circuit 250 .
[0186] In addition, in the actual display device 1000 , the arrangement of the drive control unit 200 with respect to the self-luminous panel 100 is not limited to this.
[0187] 《Variant 1》
[0188] In the organic EL element 1 as the self-luminous element of the embodiment, the resonator structures are two: the first optical resonator structure and the second optical resonator structure. However, if the self-luminous element has the first optical resonator structure and the second optical resonator structure, it may have other resonator structures.
[0189] This modification example is characterized in that a third resonator structure or a fourth resonator structure is further provided.
[0190] 1. Composition
[0191] Fig.10 (a) is a schematic cross-sectional view of the self-luminous element of this variant. The self-luminous element of this variant is different from the embodiment in that the optical adjustment layer 21 includes a first optical adjustment layer 211, a second optical adjustment layer 212, ..., and an nth optical adjustment layer 21-n (n is an integer greater than 4).
[0192] <Optical Adjustment Layer>
[0193] The optical adjustment layer 21 including four or more layers includes a light-transmitting material and is formed on the counter electrode 20 .
[0194] Each layer constituting the optical adjustment layer 21 includes a light-transmitting material, and at least the materials and refractive indexes of the adjacent layers are different. In addition, non-adjacent layers may also be composed of the same material. For example, the first optical adjustment layer 211, the third optical adjustment layer 213, the fifth optical adjustment layer, ..., are respectively composed of silicon oxynitride, and the second optical adjustment layer 212, the fourth optical adjustment layer 214, the sixth optical adjustment layer, ..., are respectively composed of silicon nitride. Among the layers constituting the optical adjustment layer 21, the light reflection surface of the interface between the first optical adjustment layer 211 and the second optical adjustment layer 212 and the light reflection surface of the interface between the pixel electrode 13 and the hole injection layer 15 form a pair to form a second optical resonator structure. Therefore, similar to the embodiment, it is preferred that the refractive index between the first optical adjustment layer 211 and the second optical adjustment layer 212 is different. For example, it is preferred that the difference in refractive index between the first optical adjustment layer 211 and the second optical adjustment layer 212 is 0.3 or more.
[0195] In addition, at least one of the interfaces of the second optical adjustment layer 212 and the third optical adjustment layer 213, the interface of the third optical adjustment layer 213 and the fourth optical adjustment layer 214, ..., the interface of the (n-1)th optical adjustment layer 21-(n-1) and the nth optical adjustment layer 21-n, and the light reflecting surface of the interface of the pixel electrode 13 and the hole injection layer 15 form a third resonator structure in a pair. Therefore, it is preferred that the refractive indexes of the two layers forming the interface of the third resonator structure are different. In addition, it is preferred that the distance from the interface of the (n-1)th optical adjustment layer 21-(n-1) and the nth optical adjustment layer 21-n, which is one of the reflecting surfaces of the third resonator structure, to the surface of the counter electrode 20 on the light emitting layer 17 side, which is one of the reflecting surfaces of the first optical resonator structure, is 1 μm or less.
[0196] Furthermore, the number of interfaces forming the resonator structure is not limited to one, but may be multiple.
[0197] 2. The first method of optical resonator structure
[0198] In this variant, the first optical resonator structure and the second optical resonator structure are the same as those in the embodiment. In addition, in this variant, a third resonator structure is provided. When the interface between the (k-1)th optical adjustment layer and the kth optical adjustment layer (k is an integer greater than 3 and less than n) and the light reflection surface of the interface between the pixel electrode 13 and the hole injection layer 15 are paired to form the third resonator structure, if the peak wavelength of the emitted light obtained by the third resonator structure is set to λ3, and the optical distance from the interface between the (k-1)th optical adjustment layer and the kth optical adjustment layer to the luminescence center is set to L k , the optical distance between the two interfaces of the third resonator structure is set to L kt (=L0+L k ), then the following relationship holds.
[0199]
[0200] in, is a phase change of light when reflected from the interface between the (k-1)th optical adjustment layer and the kth optical adjustment layer, and m3 is an arbitrary natural number.
[0201] Furthermore, it is preferable that λ3 satisfies the following relationship.
[0202] λ2<λ3<λ1…(Formula 8)
[0203] The above configuration allows light to be extracted so that the intensity of light of a desired wavelength is increased even with the third resonator structure, which is effective in improving the light emission efficiency and light extraction efficiency of the light emitting element 1 .
[0204] Furthermore, in addition to the third resonator structure, a fourth resonator structure and a fifth resonator structure may be further provided.
[0205] 3. Second method of optical resonator structure
[0206] In the first mode of the optical resonator structure, light is extracted by the third resonator structure so that the intensity of light of a desired wavelength is increased, but the third resonator structure may be configured as follows instead of this mode. That is, the third resonator structure is configured such that the interface between the (k-1)th optical adjustment layer and the kth optical adjustment layer (k is an integer greater than 3 and less than n) and the light reflecting surface of the interface between the pixel electrode 13 and the hole injection layer 15 are paired so as to satisfy the following relationship for a certain wavelength λ4.
[0207]
[0208] in, is a phase change of light when reflected from the interface between the (k-1)th optical adjustment layer and the kth optical adjustment layer, and m4 is an arbitrary natural number.
[0209] Furthermore, it is preferable that λ4 satisfies the following relationship.
[0210] λ2<λ4<λ1…(Formula 10)
[0211] Through the above configuration, in the third resonator structure, the light of wavelength λ4 is weakened relative to the path C1 or the first optical resonator structure. The optical resonator structure improves the light extraction efficiency. On the other hand, the optical distance has a field of view angle correlation, so there is an effect of enhancing the directivity, thereby also having the effect of narrowing the field of view angle. According to the above configuration, the narrowing of the field of view angle caused by the first optical resonator structure can be weakened by the third resonator structure, so it is effective for expanding the field of view angle of the light emitting element 1.
[0212] Furthermore, in addition to the third resonator structure, a fourth resonator structure and a fifth resonator structure may be further provided.
[0213] 《Variant 2》
[0214] The self-luminous panel including the light-emitting element of the embodiment is a top-emitting panel in which the pixel electrode is a light-reflective electrode and the counter electrode is a light-semi-transmissive electrode. However, the self-luminous panel may also be a bottom-emitting panel.
[0215] This modification example is characterized in that it is a bottom emission type panel in which the counter electrode is a light reflective electrode and the pixel electrode is a light reflective electrode.
[0216] 1. Composition
[0217] Fig.10(b) is a schematic cross-sectional view of the self-luminous panel of this variant. The self-luminous panel of this variant is different from the embodiment in that a light-emitting element 1 is provided on the substrate 11 in the order of a third optical adjustment layer 223, a second optical adjustment layer 222, a first optical adjustment layer 221, a light-semi-transmissive pixel electrode 131, ..., a light-emitting layer 17, ..., and a light-reflective counter electrode 201. In addition, when the light emission direction is set to the upper side, that is, when the light-reflective electrode is set to the lower side and the light-semi-transmissive electrode or the optical adjustment layer is set to the upper side in the light-emitting element, this variant can also be said to be a structure in which there is no substrate on the lower side of the light-emitting element that emits light upward and there is a substrate on the upper side.
[0218] Other Modifications of Implementation Methods
[0219] (1) In the above-mentioned embodiments and variations, the hole injection layer 15, the hole transport layer 16, the intermediate layer 18, and the electron injection transport layer 19 of the organic EL element 1 as a light-emitting element do not necessarily have the configuration of the above-mentioned embodiments. It is also possible not to have any one or more functional layers, or to have other functional layers. For example, it is also possible not to have the intermediate layer 18, or to have an electron transport layer instead of the intermediate layer 18 or between the intermediate layer 18 and the light-emitting layer 17.
[0220] The method of manufacturing each functional layer is merely an example. For example, the light emitting layer 17 may be formed by vapor deposition, or one or more layers of the optical adjustment layer may be formed by spin coating, coating, or the like.
[0221] (2) In the above-mentioned embodiments and variations, the self-luminous panel is provided with three types of light-emitting elements that emit light in R, G, and B, respectively, but the types of light-emitting elements may be two or more than four. The types of light-emitting elements refer to the changes in the elements that constitute the light-emitting elements. When the thickness of the light-emitting layer or the functional layer is different even for the same light-emitting color, the light-emitting elements may be considered to be of different types. In addition, the configuration of the light-emitting elements is not limited to the configuration of RGBRGB..., and may be the configuration of RGBBGRRGB..., or an auxiliary electrode layer or other non-luminous area may be provided between the light-emitting elements.
[0222] In the embodiment, the intermediate layer 18 , the electron injection transport layer 19 , the counter electrode 20 , and the optical adjustment layer are formed as common films, but the film thickness may be changed for each light emitting element.
[0223] (3) In the above-mentioned embodiments and variations, the light-emitting element is arranged in the self-luminous panel so that the substrate side is the anode, but the light-emitting element may be arranged so that the substrate side is the cathode. In this case, the optical adjustment layer is arranged in contact with the light-transmitting electrode regardless of the polarity of the electrode of the light-emitting element.
[0224] (4) The organic EL display panel and the organic EL display device disclosed in the present invention are described above based on the embodiments and variations, but the present invention is not limited to the above-mentioned embodiments and variations. The present invention also includes the methods obtained by implementing various modifications that can be thought of by those skilled in the art to the above-mentioned embodiments and variations, and the methods of realizing the embodiments and variations by arbitrarily combining the constituent elements and functions in the embodiments and variations without departing from the gist of the present invention.
[0225] Industrial Applicability
[0226] The present invention is useful for manufacturing a light-emitting element having a light-resonator structure, in which light extraction efficiency is significantly improved and power consumption is reduced.
Claims
1. A light emitting element, characterized in that: have: a light reflective first electrode; A light-emitting layer is disposed above the first electrode; A light-semi-transmissive second electrode, disposed above the light-emitting layer; A first light-transmitting layer is configured to contact the second electrode; as well as A second light-transmitting layer is configured to contact the first light-transmitting layer. A first optical resonator structure having a first wavelength as a peak wavelength is formed between a surface of the first electrode on the light emitting layer side and a surface of the second electrode on the light emitting layer side, wherein the first wavelength is a wavelength longer than a peak wavelength of light emitted from the light emitting layer, A second optical resonator structure having a second wavelength as a peak wavelength is formed between the surface of the first electrode on the light emitting layer side and the interface between the first light transmitting layer and the second light transmitting layer, wherein the second wavelength is a wavelength shorter than the first wavelength, The difference between the refractive index of the second light-transmitting layer and the refractive index of the first light-transmitting layer is greater than 0.3, When the first wavelength is λ1, the optical distance from the surface of the first electrode on the light-emitting layer side to the light-emitting center is L0, and the optical distance from the light-emitting center to the surface of the second electrode on the light-emitting layer side is L1, the following equation holds: When the second wavelength is λ2, the optical distance from the surface of the first electrode on the light-emitting layer side to the light-emitting center is L0, and the optical distance from the light-emitting center to the surface of the second optical adjustment layer on the light-emitting layer side is L2, the following equation holds: Furthermore, the peak wavelength of light extracted to the outside of the light emitting element, which is obtained by combining the light emitted from the first optical resonator structure and the light emitted from the second optical resonator structure, is set to λ s , when the peak wavelength of the light emitted in the light-emitting layer is set to λ, the following relationship is achieved: λ2<λ s <λ1, λ-15[nm]<λ s <λ+15[nm], l s -20[nm]<λ1, λ2<λ s +20[nm], in, is a phase change of light when reflected by the surface of the first electrode on the light-emitting layer side, is the phase change of light when it is reflected by the surface of the second electrode on the light-emitting layer side, m1 is an arbitrary natural number, is a phase change of light when reflected by the surface of the second optical adjustment layer on the light emitting layer side, and m2 is an arbitrary natural number.
2. The light emitting element according to claim 1, characterized in that A difference between a peak wavelength of light extracted to the outside of the light emitting element obtained by combining light emitted from the first optical resonator structure and light emitted from the second optical resonator structure and a peak wavelength of light emitted from the light emitting layer is 15 nm or less.
3. The light emitting element according to claim 1 or 2, characterized in that: The light emitting element further includes a third light-transmitting layer, the third light-transmitting layer being arranged in contact with the second light-transmitting layer and including one or more layers. A third optical resonator structure is formed between a surface of the first electrode on the light emitting layer side and a surface of any layer included in the third light-transmitting layer on the light emitting layer side. An optical distance between a surface of the second electrode on the light emitting layer side and an upper surface of the third light-transmitting layer is 1 μm or less.
4. The light emitting element according to claim 3, characterized in that The third optical resonator structure is configured to attenuate the peak wavelength of the first optical resonator structure.
5. The light emitting element according to claim 3, characterized in that The third optical resonator structure has a third wavelength between the first wavelength and the second wavelength as a peak wavelength.
6. A light emitting element, characterized in that: have: a light reflective first electrode; A light-emitting layer is disposed above the first electrode; A light-semi-transmissive second electrode, disposed above the light-emitting layer; A first light-transmitting layer is configured to contact the second electrode; as well as A second light-transmitting layer is configured to contact the first light-transmitting layer. A first optical resonator structure having a first wavelength as a peak wavelength is formed between a surface of the first electrode on the light emitting layer side and a surface of the second electrode on the light emitting layer side, wherein the first wavelength is a wavelength longer than a peak wavelength of light emitted from the light emitting layer, A second optical resonator structure having a second wavelength as a peak wavelength is formed between the surface of the first electrode on the light emitting layer side and the interface between the first light transmitting layer and the second light transmitting layer, wherein the second wavelength is a wavelength shorter than the first wavelength, The first light-transmitting layer comprises IZO or NbO, The second light-transmitting layer comprises silicon oxynitride, When the first wavelength is λ1, the optical distance from the surface of the first electrode on the light-emitting layer side to the light-emitting center is L0, and the optical distance from the light-emitting center to the surface of the second electrode on the light-emitting layer side is L1, the following equation holds: When the second wavelength is λ2, the optical distance from the surface of the first electrode on the light-emitting layer side to the light-emitting center is L0, and the optical distance from the light-emitting center to the surface of the second optical adjustment layer on the light-emitting layer side is L2, the following equation holds: Furthermore, the peak wavelength of light extracted to the outside of the light emitting element, which is obtained by combining the light emitted from the first optical resonator structure and the light emitted from the second optical resonator structure, is set to λ s , when the peak wavelength of the light emitted in the light-emitting layer is set to λ, the following relationship is achieved: λ2<λ s <λ1, λ-15[nm]<λ s <λ+15[nm], l s -20[nm]<λ1, λ2<λ s +20[nm], in, is a phase change of light when reflected by the surface of the first electrode on the light-emitting layer side, is the phase change of light when it is reflected by the surface of the second electrode on the light-emitting layer side, m1 is an arbitrary natural number, is a phase change of light when reflected by the surface of the second optical adjustment layer on the light emitting layer side, and m2 is an arbitrary natural number.
7. A self-luminous panel, characterized in that: A plurality of light-emitting elements according to any one of claims 1 to 6 are formed on a substrate.
8. A self-luminous panel, characterized in that: have: A substrate, at least a portion of which is light-transmissive; A second light-transmitting layer is disposed above the light-transmitting portion of the substrate; a first light-transmitting layer, configured to contact the second light-transmitting layer; A second light-semi-transmissive electrode, disposed above the first light-transmissive layer; A light-emitting layer is disposed above the second electrode; as well as A light-reflective first electrode is disposed above the light-emitting layer. A first optical resonator structure having a first wavelength as a peak wavelength is formed between a surface of the first electrode on the light emitting layer side and a surface of the second electrode on the light emitting layer side, wherein the first wavelength is a wavelength longer than a peak wavelength of light emitted from the light emitting layer, A second optical resonator structure having a second wavelength as a peak wavelength is formed between the surface of the first electrode on the light emitting layer side and the interface between the first light transmitting layer and the second light transmitting layer, wherein the second wavelength is a wavelength shorter than the first wavelength, The difference between the refractive index of the second light-transmitting layer and the refractive index of the first light-transmitting layer is greater than 0.3, When the first wavelength is λ1, the optical distance from the surface of the first electrode on the light-emitting layer side to the light-emitting center is L0, and the optical distance from the light-emitting center to the surface of the second electrode on the light-emitting layer side is L1, the following equation holds: When the second wavelength is λ2, the optical distance from the surface of the first electrode on the light-emitting layer side to the light-emitting center is L0, and the optical distance from the light-emitting center to the surface of the second optical adjustment layer on the light-emitting layer side is L2, the following equation holds: Furthermore, when the peak wavelength of light extracted to the outside of the light emitting element by combining the light emitted from the first optical resonator structure and the light emitted from the second optical resonator structure is λ s , when the peak wavelength of the light emitted in the light-emitting layer is set to λ, the following relationship is achieved: λ2<λ s <λ1, λ-15[nm]<λ s <λ+15[nm], l s -20[nm]<λ1, λ2<λ s +20[nm], in, is a phase change of light when reflected by the surface of the first electrode on the light-emitting layer side, is the phase change of light when it is reflected by the surface of the second electrode on the light-emitting layer side, m1 is an arbitrary natural number, is a phase change of light when reflected by the surface of the second optical adjustment layer on the light emitting layer side, and m2 is an arbitrary natural number.
9. A self-luminous panel, characterized in that: have: A substrate, at least a portion of which is light-transmissive; A second light-transmitting layer is disposed above the light-transmitting portion of the substrate; a first light-transmitting layer, configured to contact the second light-transmitting layer; A second light-semi-transmissive electrode, disposed above the first light-transmissive layer; A light-emitting layer is disposed above the second electrode; as well as A light-reflective first electrode is disposed above the light-emitting layer. A first optical resonator structure having a first wavelength as a peak wavelength is formed between a surface of the first electrode on the light emitting layer side and a surface of the second electrode on the light emitting layer side, wherein the first wavelength is a wavelength longer than a peak wavelength of light emitted from the light emitting layer, A second optical resonator structure having a second wavelength as a peak wavelength is formed between a surface of the first electrode on the light emitting layer side and an interface between the first light transmitting layer and the second light transmitting layer, wherein the second wavelength is a wavelength shorter than the first wavelength, and the first light transmitting layer includes IZO or NbO, The second light-transmitting layer comprises silicon oxynitride, When the first wavelength is λ1, the optical distance from the surface of the first electrode on the light-emitting layer side to the light-emitting center is L0, and the optical distance from the light-emitting center to the surface of the second electrode on the light-emitting layer side is L1, the following equation holds: When the second wavelength is λ2, the optical distance from the surface of the first electrode on the light-emitting layer side to the light-emitting center is L0, and the optical distance from the light-emitting center to the surface of the second optical adjustment layer on the light-emitting layer side is L2, the following equation holds: Furthermore, when the peak wavelength of light extracted to the outside of the light emitting element by combining the light emitted from the first optical resonator structure and the light emitted from the second optical resonator structure is λ s , when the peak wavelength of the light emitted in the light-emitting layer is set to λ, the following relationship is achieved: λ2<λ s <λ1, λ-15[nm]<λ s <λ+15[nm], l s -20[nm]<λ1, λ2<λ s +20[nm], in, is a phase change of light when reflected by the surface of the first electrode on the light-emitting layer side, is the phase change of light when it is reflected by the surface of the second electrode on the light-emitting layer side, m1 is an arbitrary natural number, is a phase change of light when reflected by the surface of the second optical adjustment layer on the light emitting layer side, and m2 is an arbitrary natural number.
10. A method for manufacturing a self-luminous panel, characterized in that: forming a light-reflective first electrode on the substrate, forming a light-emitting layer on the first electrode, A second light-transmissive electrode is formed above the light-emitting layer, contacting with the second electrode and forming a first light-transmitting layer, A second light-transmitting layer is formed on the first light-transmitting layer and is in contact with the first light-transmitting layer and has a refractive index different from that of the first light-transmitting layer by 0.3 or more. In forming the second electrode, a first optical resonator structure having a first wavelength as a peak wavelength is formed between a surface of the first electrode on the light emitting layer side and a surface of the second electrode on the light emitting layer side, wherein the first wavelength is a wavelength longer than a peak wavelength of light emitted from the light emitting layer, In forming the second light-transmitting layer, a second optical resonator structure having a second wavelength as a peak wavelength is formed between a surface of the first electrode on the light-emitting layer side and an interface between the first light-transmitting layer and the second light-transmitting layer, wherein the second wavelength is a wavelength shorter than the first wavelength. The difference between the refractive index of the second light-transmitting layer and the refractive index of the first light-transmitting layer is greater than 0.3, When the first wavelength is λ1, the optical distance from the surface of the first electrode on the light-emitting layer side to the light-emitting center is L0, and the optical distance from the light-emitting center to the surface of the second electrode on the light-emitting layer side is L1, the following equation holds: When the second wavelength is λ2, the optical distance from the surface of the first electrode on the light-emitting layer side to the light-emitting center is L0, and the optical distance from the light-emitting center to the surface of the second optical adjustment layer on the light-emitting layer side is L2, the following equation holds: Furthermore, when the peak wavelength of light extracted to the outside of the light emitting element by combining the light emitted from the first optical resonator structure and the light emitted from the second optical resonator structure is λ s , when the peak wavelength of the light emitted in the light-emitting layer is set to λ, the following relationship is achieved: λ2<λ s <λ1, λ-15[nm]<λ s <λ+15[nm], l s -20[nm]<λ1, λ2<λ s +20[nm], in, is a phase change of light when reflected by the surface of the first electrode on the light-emitting layer side, is the phase change of light when it is reflected by the surface of the second electrode on the light-emitting layer side, m1 is an arbitrary natural number, is a phase change of light when reflected by the surface of the second optical adjustment layer on the light emitting layer side, and m2 is an arbitrary natural number.
11. A method for manufacturing a self-luminous panel, characterized in that: forming a light-reflective first electrode on the substrate, forming a light-emitting layer on the first electrode, A second light-transmissive electrode is formed above the light-emitting layer, contacting with the second electrode and forming a first light-transmitting layer, A second light-transmitting layer is formed on the first light-transmitting layer and is in contact with the first light-transmitting layer and has a refractive index different from that of the first light-transmitting layer by 0.3 or more. In forming the second electrode, a first optical resonator structure having a first wavelength as a peak wavelength is formed between a surface of the first electrode on the light emitting layer side and a surface of the second electrode on the light emitting layer side, wherein the first wavelength is a wavelength longer than a peak wavelength of light emitted from the light emitting layer, In forming the second light-transmitting layer, a second optical resonator structure having a second wavelength as a peak wavelength is formed between a surface of the first electrode on the light-emitting layer side and an interface between the first light-transmitting layer and the second light-transmitting layer, wherein the second wavelength is a wavelength shorter than the first wavelength. The first light-transmitting layer comprises IZO or NbO, The second light-transmitting layer comprises silicon oxynitride, When the first wavelength is λ1, the optical distance from the surface of the first electrode on the light-emitting layer side to the light-emitting center is L0, and the optical distance from the light-emitting center to the surface of the second electrode on the light-emitting layer side is L1, the following equation holds: When the second wavelength is λ2, the optical distance from the surface of the first electrode on the light-emitting layer side to the light-emitting center is L0, and the optical distance from the light-emitting center to the surface of the second optical adjustment layer on the light-emitting layer side is L2, the following equation holds: Furthermore, when the peak wavelength of light extracted to the outside of the light emitting element by combining the light emitted from the first optical resonator structure and the light emitted from the second optical resonator structure is λ s , when the peak wavelength of the light emitted in the light-emitting layer is set to λ, the following relationship is achieved: λ2<λ s <λ1, λ-15[nm]<λ s <λ+15[nm], l s -20[nm]<λ1, λ2<λ s +20[nm], in, is a phase change of light when reflected by the surface of the first electrode on the light-emitting layer side, is the phase change of light when it is reflected by the surface of the second electrode on the light-emitting layer side, m1 is an arbitrary natural number, is a phase change of light when reflected by the surface of the second optical adjustment layer on the light emitting layer side, and m2 is an arbitrary natural number.
12. A method for manufacturing a self-luminous panel, characterized in that: forming a second light-transmitting layer on the substrate, contacting with the second light-transmitting layer and forming a first light-transmitting layer, a second electrode which is in contact with the first light-transmitting layer and is light-semi-transmissive, forming a light-emitting layer on the second electrode, forming a light-reflective first electrode on the light-emitting layer, In forming the second electrode, a first optical resonator structure having a first wavelength as a peak wavelength is formed between a surface of the first electrode on the light emitting layer side and a surface of the second electrode on the light emitting layer side, wherein the first wavelength is a wavelength longer than a peak wavelength of light emitted from the light emitting layer, In forming the second light-transmitting layer, a second optical resonator structure having a second wavelength as a peak wavelength is formed between a surface of the first electrode on the light-emitting layer side and an interface between the first light-transmitting layer and the second light-transmitting layer, wherein the second wavelength is a wavelength shorter than the first wavelength. The difference between the refractive index of the second light-transmitting layer and the refractive index of the first light-transmitting layer is greater than 0.3, When the first wavelength is λ1, the optical distance from the surface of the first electrode on the light-emitting layer side to the light-emitting center is L0, and the optical distance from the light-emitting center to the surface of the second electrode on the light-emitting layer side is L1, the following equation holds: When the second wavelength is λ2, the optical distance from the surface of the first electrode on the light-emitting layer side to the light-emitting center is L0, and the optical distance from the light-emitting center to the surface of the second optical adjustment layer on the light-emitting layer side is L2, the following equation holds: Furthermore, when the peak wavelength of light extracted to the outside of the light emitting element by combining the light emitted from the first optical resonator structure and the light emitted from the second optical resonator structure is λ s , when the peak wavelength of the light emitted in the light-emitting layer is set to λ, the following relationship is achieved: λ2<λ s <λ1, λ-15[nm]<λ s <λ+15[nm], l s -20[nm]<λ1, λ2<λ s +20[nm], in, is a phase change of light when reflected by the surface of the first electrode on the light-emitting layer side, is the phase change of light when it is reflected by the surface of the second electrode on the light-emitting layer side, m1 is an arbitrary natural number, is a phase change of light when reflected by the surface of the second optical adjustment layer on the light emitting layer side, and m2 is an arbitrary natural number.
13. A method for manufacturing a self-luminous panel, characterized in that: forming a second light-transmitting layer on the substrate, contacting with the second light-transmitting layer and forming a first light-transmitting layer, a second electrode which is in contact with the first light-transmitting layer and is light-semi-transmissive, forming a light-emitting layer on the second electrode, forming a light-reflective first electrode on the light-emitting layer, In forming the second electrode, a first optical resonator structure having a first wavelength as a peak wavelength is formed between a surface of the first electrode on the light emitting layer side and a surface of the second electrode on the light emitting layer side, wherein the first wavelength is a wavelength longer than a peak wavelength of light emitted from the light emitting layer, In forming the second light-transmitting layer, a second optical resonator structure having a second wavelength as a peak wavelength is formed between a surface of the first electrode on the light-emitting layer side and an interface between the first light-transmitting layer and the second light-transmitting layer, wherein the second wavelength is a wavelength shorter than the first wavelength. The first light-transmitting layer comprises IZO or NbO, The second light-transmitting layer comprises silicon oxynitride, When the first wavelength is λ1, the optical distance from the surface of the first electrode on the light-emitting layer side to the light-emitting center is L0, and the optical distance from the light-emitting center to the surface of the second electrode on the light-emitting layer side is L1, the following equation holds: When the second wavelength is λ2, the optical distance from the surface of the first electrode on the light-emitting layer side to the light-emitting center is L0, and the optical distance from the light-emitting center to the surface of the second optical adjustment layer on the light-emitting layer side is L2, the following equation holds: Furthermore, when the peak wavelength of light extracted to the outside of the light emitting element by combining the light emitted from the first optical resonator structure and the light emitted from the second optical resonator structure is λ s , when the peak wavelength of the light emitted in the light-emitting layer is set to λ, the following relationship is achieved: λ2<λ s <λ1, λ-15[nm]<λ s <λ+15[nm], l s -20[nm]<λ1, λ2<λ s +20[nm], in, is a phase change of light when reflected by the surface of the first electrode on the light-emitting layer side, is the phase change of light when it is reflected by the surface of the second electrode on the light-emitting layer side, m1 is an arbitrary natural number, is a phase change of light when reflected by the surface of the second optical adjustment layer on the light emitting layer side, and m2 is an arbitrary natural number.
Citation Information
Patent Citations
Organic light emitting element, organic light emitting device, organic display panel, organic display device, and method for manufacturing organic light emitting element
WO2012020452A1
Organic electroluminescent display device
JP2011076799A
Organic electroluminescent device
JP2011210678A