Stator, movement, watch, method for manufacturing movement, and method for manufacturing stator

By coating the stator main plate with chromium to form a non-magnetic area, the problem of contact between the stator and the gear train was solved, enabling stator assembly without the need for manual removal of slag, simplifying the manufacturing process and reducing costs.

CN112636489BActive Publication Date: 2024-11-05SEIKO CORP
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202011015598.3
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Priority Date
2019-09-24
Filing Date
2020-09-24
Publication Date
2024-11-05
Estimated Expiration
2040-09-24

AI Technical Summary

Technical Problem

In the stator of a simulated electronic clock, the slag generated by laser irradiation causes the stator to come into contact with the gear train, requiring manual removal of the slag, which increases cost and complexity.

Method used

Chromium is coated onto the main plate of the stator and a non-magnetic area is formed by laser irradiation. Combined with the shearing process of fixed and movable molds, a narrow width section and a non-magnetic area are formed to avoid the generation of slag.

Benefits of technology

This enables stator assembly without the need to remove slag, simplifying the manufacturing process, reducing costs, and improving assembly efficiency.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN112636489B_ABST
    Figure CN112636489B_ABST
Patent Text Reader

Abstract

[Subject] The object of the present invention is to provide a stator that can be assembled without removing scum. [Solution] The stator comprises: a magnetic plate having a surface, i.e., a main plate surface, that is, a main plate surface that is opposite to the main plate when assembled to the main plate of the movement, a rotor receiving hole formed in a portion of the magnetic plate; and a non-magnetic region that is formed by applying chromium to the main plate surface around the rotor receiving hole and irradiating the chromium with a laser from the main plate surface side to demagnetize it.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] Embodiments of the present invention relate to a stator, a movement, a timepiece, a method for manufacturing a movement, and a method for manufacturing a stator. Background Art

[0002] In the past, in analog electronic watches, stepper motors were used as power sources for rotating and driving the hour hand, minute hand, and other hands. In such stepper motors provided in analog electronic watches, an integrated stator having a rotor receiving hole in which a rotor is provided is used. In the integrated stator, narrow width portions having a width narrower than other portions are provided at two locations around the rotor receiving hole at intervals of 180 degrees. By providing the narrow width portions, the integrated stator becomes easy to saturate the magnetic flux.

[0003] The following technology is known: a Cr diffusion region is formed in a part of the magnetic circuit around the rotor receiving hole provided in the stator, and the magnetic permeability of the region is reduced to form a non-magnetic region. The non-magnetic region can be formed by arranging a Cr material for melting and diffusion in the stator, and irradiating the Cr material with a laser to melt and diffuse the Cr material into the inside of the magnetic circuit. (For example, refer to Patent Document 1).

[0004] [Previous Technical Literature]

[0005] [Patent Literature]

[0006] [Patent Document 1] Japanese Patent Application Publication No. 2019-68724. Summary of the invention

[0007] [Problems to be solved by the invention]

[0008] However, according to the conventional technology described in Patent Document 1, protrusions (scum) are generated on the laser irradiation surface. The stator becomes thicker due to the scum, and thus there is a problem that the scum of the stator contacts the gear train provided on the upper side of the stator.

[0009] In order to prevent the stator from contacting the gear train, it is conceivable to remove the scum, but the removal of the scum requires labor and cost.

[0010] Embodiments of the present invention have been made in view of such circumstances, and an object of the present invention is to provide a stator, a movement, a timepiece, a method for manufacturing a movement, and a method for manufacturing a stator that can be assembled without removing scum.

[0011]

Solutions to Solve the Problem

[0012] A stator according to one embodiment of the present invention comprises: a magnetic plate having a surface, namely a main plate surface, which is opposite to the main plate when mounted on the main plate of a movement, and a rotor receiving hole is formed in a portion thereof; and a non-magnetic area in which chromium is applied to the main plate surface around the rotor receiving hole and the chromium is demagnetized by irradiating a laser from the main plate surface side.

[0013] The stator according to one embodiment of the present invention may include a portion that is sheared by connecting a fixed mold to the main plate surface and connecting a movable mold to the back surface of the main plate surface.

[0014] A movement according to one aspect of the present invention includes: the above-mentioned stator; and the main plate having a concave cutout at a position facing the nonmagnetic region of the stator.

[0015] In addition, a movement involved in one embodiment of the present invention comprises: the above-mentioned stator; and a stator holding component, which has a retreat portion thinner than other portions at a position opposite to the nonmagnetic region of the stator, and the stator holding component is connected to the main board surface to hold the stator.

[0016] A timepiece according to one aspect of the present invention includes any one of the above-mentioned movements.

[0017] A method for manufacturing a movement according to one aspect of the present invention includes the step of arranging the main plate surface of any of the stators so as to face the main plate.

[0018] A method for manufacturing a stator according to one embodiment of the present invention is a method for manufacturing a stator as follows: chromium is applied to one surface of a magnetic plate around a rotor receiving hole, and a laser is irradiated on the chromium from the one surface side, thereby forming a non-magnetic region on the magnetic plate. In this manufacturing method, the one surface is a main board surface facing a main board of a movement.

[0019] [Effects of the Invention]

[0020] According to the embodiments of the present invention, it is possible to provide a stator, a movement, a timepiece, a method for manufacturing a movement, and a method for manufacturing a stator that can be assembled without removing scum. BRIEF DESCRIPTION OF THE DRAWINGS

[0021] Figure 1 This is a block diagram showing a timepiece using the stepping motor and timepiece movement according to the present embodiment.

[0022] Figure 2 It is a perspective view showing a schematic configuration example of a stepping motor according to the present embodiment.

[0023] Figure 3 It is a schematic front view of the stator involved in this embodiment.

[0024] Figure 4 It is a schematic front view of the stepping motor involved in this embodiment.

[0025] Figure 5 This is a diagram showing an example of a method for manufacturing a stator according to the present embodiment.

[0026] Figure 6 It is a plan view showing a hoop material of the stator according to the present embodiment before punching.

[0027] Figure 7 This is a diagram showing an example of a photograph of a cross section of a hoop material after chromium applied to a hoop material of permalloy is melted and diffused by laser to increase the chromium content to 15 wt % or more in the present embodiment.

[0028] Figure 8 This is a diagram showing an example of a photograph of a cross section of a hoop material after chromium applied to a hoop material of permalloy is melted and diffused by laser to make the weight ratio of chromium 15 weight % or more in the present embodiment.

[0029] Fig. 9 This is a diagram showing an example of a photograph of a cross section of a hoop material after chromium applied to a hoop material of permalloy is melted and diffused by laser to make the weight ratio of chromium 15 weight % or more in the present embodiment.

[0030] Fig. 10A It is a diagram showing a fusion zone according to this embodiment.

[0031] Fig. 10B This is a graph showing the results of line analysis of the fusion zone according to the present embodiment.

[0032] Fig.11 It is the state diagram of the Fe-Ni-Cr ternary alloy.

[0033] Fig. 12A It is a perspective view showing a stator according to the present embodiment.

[0034] Fig. 12B It is along Fig. 12A Cross-sectional view of the stator along line AA.

[0035] Fig.13 This is a plan view of an example of the internal structure of the mechanism module according to the present embodiment as viewed from the front side.

[0036] Fig.14 This is a cross-sectional view showing an example of the internal structure of the mechanism module according to the present embodiment when viewed from the side.

[0037] Fig.15AThe stator is shown screwed to the main board. Fig. 12B The corresponding cross-sectional view.

[0038] Fig. 15B The stator is shown screwed to the main board. Fig. 12B The corresponding cross-sectional view.

[0039] Fig. 15C The stator is shown screwed to the main board. Fig. 12B The corresponding cross-sectional view.

[0040] Fig.15D The stator is shown screwed to the main board. Fig. 12B The corresponding cross-sectional view. DETAILED DESCRIPTION

[0041] Hereinafter, embodiments of the present invention will be described with reference to the accompanying drawings. In the drawings used in the following description, the scale of each component is appropriately changed so that the size of each component can be recognized.

[0042] Figure 1 1 is a block diagram showing a timepiece 1 using a stepping motor and a timepiece movement according to the present embodiment. In the present embodiment, an analog electronic timepiece is illustrated and described as an example of a timepiece.

[0043] like Figure 1 As shown, the timepiece 1 includes a battery 2 , an oscillation circuit 3 , a frequency division circuit 4 , a control circuit 5 , a pulse drive circuit 6 , a stepping motor 7 , and an analog timepiece unit 8 .

[0044] In addition, the analog watch section 8 includes a train wheel 11, an hour hand 12, a minute hand 13, a second hand 14, a calendar display section 15, a watch case 81, and a watch movement 82 (hereinafter referred to as movement 82). In addition, in the present embodiment, when one of the hour hand 12, the minute hand 13, the second hand 14, and the calendar display section 15 is not particularly specified, it is referred to as a pointer 16.

[0045] The oscillation circuit 3, the frequency division circuit 4, the control circuit 5, the pulse drive circuit 6, the stepping motor 7 and the gear train 11 are components of the movement 82. The module including the stepping motor 7 and the gear train 11 is also referred to as a mechanism module 83.

[0046] Generally speaking, the mechanical body of a clock, which is composed of devices such as the time reference of the clock 1, is called a movement. An electronic movement is sometimes called a module. In the completed state of the clock, for example, a dial and hands are installed on the movement, and the movement is accommodated in the clock case 81.

[0047] The battery 2 is, for example, a lithium battery or a so-called button battery. Alternatively, the battery 2 may be a solar cell or a storage battery that stores electric power generated by a solar cell. The battery 2 supplies electric power to the control circuit 5 .

[0048] The oscillation circuit 3 is a passive element used to oscillate at a predetermined frequency by mechanical resonance of quartz using, for example, the piezoelectric phenomenon of quartz. Here, the predetermined frequency is, for example, 32 [kHz].

[0049] The frequency dividing circuit 4 divides the signal of a predetermined frequency outputted from the oscillation circuit 3 into a desired frequency, and outputs the divided signal to the control circuit 5 .

[0050] The control circuit 5 uses the divided signal output by the frequency dividing circuit 4 to perform timing, and generates a driving pulse based on the timing result. In addition, when the pointer 16 is moved in the forward direction, the control circuit 5 generates a forward driving pulse. When the pointer 16 is moved in the reverse direction, the control circuit 5 generates a reverse driving pulse. The control circuit 5 outputs the generated driving pulse to the pulse driving circuit 6.

[0051] The pulse drive circuit 6 generates a drive pulse for each pointer according to the drive instruction outputted from the control circuit 5. The pulse drive circuit 6 outputs the generated drive pulse to the stepping motor 7.

[0052] The stepping motor 7 moves the hands 16 (hour hand 12, minute hand 13, second hand 14, calendar display unit 15) according to the driving pulse output by the pulse driving circuit 6. Figure 1 In the illustrated example, for example, one stepping motor 7 is provided for the hour hand 12, minute hand 13, second hand 14, and calendar display 15. Alternatively, one stepping motor 7 may be provided for each of the hour hand 12, minute hand 13, second hand 14, and calendar display 15.

[0053] The hour hand 12 , the minute hand 13 , the second hand 14 , and the calendar display unit 15 are each moved by a stepping motor 7 .

[0054] The pulse drive circuit 6 drives the stepping motor 7, whereby the hour hand 12 rotates once in 12 hours. The pulse drive circuit 6 drives the stepping motor 7, whereby the minute hand 13 rotates once in 60 minutes. The pulse drive circuit 6 drives the stepping motor 7, whereby the second hand 14 rotates once in 60 seconds. The calendar display unit 15 is, for example, a pointer that displays the date, and the pulse drive circuit 6 drives the stepping motor 7, whereby the display of the calendar display unit 15 rotates in a manner that advances one day in 24 hours.

[0055] Next, a schematic configuration example of the stepping motor 7 according to the present embodiment will be described.

[0056] Figure 21 is a perspective view showing a schematic configuration example of the stepping motor 7 according to the present embodiment. Figure 2 As shown, the stepping motor 7 includes a stator 201 , a rotor 202 , a core 208 , a coil 209 , and a screw 220 .

[0057] The stator 201 is formed with a rotor accommodation hole 203 , a screw hole 218 a , and a screw hole 218 b .

[0058] The rotor 202 is rotatably disposed in the rotor receiving hole 203 .

[0059] The coil 209 is wound around the magnetic core 208 .

[0060] When the stepping motor 7 is used in an analog electronic timepiece, the stator 201 and the core 208 are fixed to the main plate 51 of the movement 82 by screws 220 and joined to each other.

[0061] Here, use Figure 3 The stator 201 will be described.

[0062] Figure 3 2 is a front view schematic diagram of the stator 201 according to the present embodiment. Figure 3 In the embodiment, the long side direction of the stator 201 is taken as the y-axis direction, and the short side direction is taken as the x-axis direction. Figure 3 As shown, cutouts 204 and 205 are formed in the rotor receiving hole 203. In addition, in the stator 201, narrow width portions 210 and 211 are formed around the rotor receiving hole 203. The stator 201 is formed of, for example, a magnetic plate material of Fe-Ni (iron-nickel). In addition, the narrow width portions 210 and 211 are non-magnetic regions. That is, the stator 201 is a magnetic plate material having the rotor receiving hole 203 formed in a portion. Here, a magnetic plate material does not include a case where two divided plates are joined.

[0063] In the case where the stepping motor 7 is used in a timepiece, an example of each dimension of the stator 201 will be described.

[0064] The diameter of the rotor receiving hole 203 is about 1.5-2 mm. The width of the narrowest part of the narrow width parts 210 and 211 is about 0.1 mm-0.2 mm. The thickness of the stator 201 is about 0.5 mm±0.1 mm. The length in the long side direction is about 10 mm.

[0065] Next, use Figure 4 The stepping motor 7 according to the present embodiment will be described in detail.

[0066] Figure 4 It is a schematic front view of the stepping motor 7 according to the present embodiment.

[0067] Figure 4 The stepping motor 7 shown in the figure includes a rotor accommodating hole 203 , a stator 201 , a rotor 202 , a core 208 , a coil 209 , and narrow width portions 210 , 211 .

[0068] A magnetic path R is provided around the rotor receiving hole 203 of the stator 201 . The rotor 202 is a two-pole rotor rotatably disposed in the rotor receiving hole 203 . The core 208 is joined to the stator 201 . The coil 209 is wound around the core 208 .

[0069] The notches 204 and 205 are provided in the rotor receiving hole 203 to ensure a stable stop position of the rotor 202, and the narrow width portions 210 and 211 are provided in portions that do not interfere with the notches 204 and 205. The coil 209 has a first terminal OUT1 and a second terminal OUT2.

[0070] The rotor receiving hole 203 is a through hole formed in the stator 201 in a circular shape. The cutouts (inner recesses) 204 and 205 are each half-moon-shaped, and a plurality of (inner recesses) are formed in the opposite portions of the rotor receiving hole 203. Figure 4 These notches 204 and 205 are configured as positioning portions for determining a stable stop position of the rotor 202. For example, the notch (inner notch) 204 serves to reduce the potential energy of the rotor 202 when the rotor 202 is disposed at a predetermined position, thereby stabilizing the position of the rotor 202.

[0071] The rotor 202 is magnetized into two poles (S pole and N pole). Figure 4 In other words, when the coil 209 is not excited, the rotor 202 stably stops (rests) at a position (angle θ0 position) where the magnetic pole axis A of the rotor 202 is orthogonal to the line segment connecting the notches 204 and 205.

[0072] In a portion of the magnetic circuit R provided around the rotor receiving hole 203 (in Figure 4 In the example of the stator 201, two locations are formed with narrow width portions 210 and 211 as non-magnetic areas. Here, regarding the narrow width portions 210 and 211 of the stator 201, the cross-sectional width in the direction perpendicular to the magnetic circuit is referred to as the cross-sectional width t, and the width in the direction along the magnetic circuit is referred to as the gap width w. The narrow width portions 210 and 211 are formed in the area defined by the cross-sectional width t and the gap width w.

[0073] In the following description, regarding the stator 201, the outer periphery of the narrow width portion 211 is defined as point a1, the inside of the narrow width portion 211 is defined as point b1, and a portion located near the narrow width portion 211 and between the outer periphery and the inner periphery of the magnetic circuit R is defined as point c.

[0074] Next, refer to Figure 4 Next, the operation of the stepping motor 7 according to the present embodiment will be described.

[0075] First, if the pulse drive circuit 6 ( Figure 1 ) A driving pulse signal such as the first terminal OUT1 side becomes positive and the second terminal OUT2 side becomes negative is supplied to the terminals OUT1 and OUT2 of the coil 209, and the current i flows along Figure 4 Flows in the direction of the arrow, generating magnetic flux in the stator 201 along the direction of the dotted arrow.

[0076] In this embodiment, narrow width portions 210 and 211 are formed as non-magnetic regions, and the magnetic resistance of the regions is increased. Therefore, in this embodiment, it is not necessary to magnetically saturate the regions corresponding to the conventional "narrow width portions", and leakage flux can be easily ensured. After ensuring the leakage flux, the rotor 202 is moved along the magnetic poles generated by the stator 201 through the interaction with the magnetic poles of the rotor 202. Figure 4 The magnetic pole rotates 180 degrees in the direction of the arrow and stops stably (rests) at a position where the magnetic pole axis faces an angle θ1.

[0077] In addition, by rotating the stepping motor 7, the rotation direction (in Figure 4 In the embodiment of the present invention, the counterclockwise direction is taken as the positive direction, and the opposite direction (clockwise direction) is taken as the negative direction. Here, when the stepping motor 7 is applied to an analog electronic clock, the normal action means the needle movement.

[0078] Next, from the pulse drive circuit 6 ( Figure 1 ) For example, when a driving pulse of opposite polarity is supplied to the terminals OUT1 and OUT2 of the coil 209, such that the first terminal OUT1 side becomes negative and the second terminal OUT2 side becomes positive, the current flows along Figure 4 Flows in the opposite direction of the arrow, generating a magnetic flux in the stator 201 in the direction opposite to the direction of the dotted arrow.

[0079] Subsequently, due to the interaction between the magnetic poles generated in the stator 201 and the magnetic poles of the rotor 202, the rotor 202 rotates 180 degrees in the same direction (positive direction) as described above, and stably stops (rests) at a position where the magnetic pole axis faces the angle θ0.

[0080] Thereafter, by alternately supplying signals of different polarities (alternating signals) to the coil 209, the above-described operation can be repeated to cause the rotor 202 to continuously rotate 180 degrees at a time in the direction of the arrow.

[0081] Since the narrow width portions 210 and 211 as non-magnetic regions are formed in a part of the magnetic path around the rotor accommodation hole 203 , the magnetic flux consumed in this region can be significantly reduced, and the leakage magnetic flux for driving the rotor 202 can be efficiently ensured.

[0082] In addition, by forming the narrow width portions 210 and 211 as non-magnetic regions at the "narrow width portions", it is possible to suppress the consumption of magnetic flux emitted from the rotor 202 itself in the regions. As a result, the loss of magnetic potential can be suppressed, and the holding force for magnetically stopping (stationary) / holding the rotor 202 can be increased.

[0083] In addition, after the rotor 202 is rotated by saturating the portion that was previously the "narrow width portion" with the magnetic flux on the OUT1 side (negative pole), in order to rotate the rotor 202 with the magnetic flux on the OUT2 side (positive pole), it is necessary to eliminate the residual magnetic flux generated when the rotor 202 is rotated by saturating the magnetic flux on the OUT1 side (negative pole). However, according to the present embodiment, the residual magnetic flux in this area is greatly reduced, so the time required to eliminate the residual magnetic flux is not required, and the time until the rotation of the rotor 202 is completed can be shortened. Therefore, according to the present embodiment, the stability of the operation can be maintained when the needle is moved at high speed, and the drive frequency can be increased. In addition, the drive pulse for driving the stepping motor 7 will be described later.

[0084] <Description of Manufacturing Method>

[0085] Next, use Figure 5 An example of a method for manufacturing the stator 201 will be described.

[0086] Figure 5 This is a diagram showing an example of a method for manufacturing the stator 201 according to the present embodiment.

[0087] (First manufacturing process: first punching (guide hole production))

[0088] In the first manufacturing process, the manufacturing system 300 is provided with a punching device 302. In addition, reference numeral 301 shows a state where a hoop material 310 before punching is wound. Reference numeral 303 shows a state where a hoop material after punching is wound. Reference numeral 310 shows a top view of the hoop material after punching. Figure 5 In the embodiment, the long side direction of the hoop material is the x-axis direction, and the short side direction is the y-axis direction. In addition, the width of the short side direction of the hoop material is, for example, 16.5 mm.

[0089] The punching device 302 forms positioning guide holes 312 and 313 on the upper and lower sides of the magnetic material (such as No. 38 Permalloy) in the state of the hoop material. After punching, the manufacturing system 300 winds the punched hoop material as shown by reference numeral 303.

[0090] (Second manufacturing process: Non-magnetic area production)

[0091] In the second manufacturing process, the manufacturing system 300 includes: a paste coating device 322 that applies chromium (Cr) in a paste form; a drying device 323; a laser irradiation device 324; and a cleaning device 325. In addition, reference numeral 321 shows a state where the punched hoop material is wound in the first manufacturing process. Reference numeral 326 shows a state where the hoop material 310 after the non-magnetic region is formed is wound.

[0092] The paste coating device 322 applies chromium paste to the desired position in the y-axis direction of the hoop material (coating process). The paste coating device 322 mixes chromium with an adhesive to form a paste and distributes it. That is, the paste coating device 322 is a dispenser. In addition, the desired position in the y-axis direction is the production Figure 3 The non-magnetic region of the stator 201 shown is the region of the narrow width portions 210 and 211. In addition, the paste coating device 322 applies chromium paste to a desired position based on the positions of the guide holes 312 and 313. In addition, as an example, the coating thickness of chromium is 150-200 [micrometers].

[0093] Next, the drying device 323 dries the chromium applied in the paste form.

[0094] Next, the laser irradiation device 324 irradiates the laser to the area (labeled 331) coated with chromium in a paste state (laser processing step). In addition, the laser is preferably a fiber laser with a deeper discharge depth. As a result, the applied chromium melts in the base material (permalloy material). Then, the chromium inside the coated chromium and the permalloy material diffuses and melts to form an area with a chromium weight ratio of more than 15% by weight. In addition, by laser irradiation, the temperature of the area coated with chromium in a paste state becomes above the melting point of the permalloy material and Cr (more than 1900 degrees). In addition, the caliber of the incident side of the laser is about 0.3-0.5mm. In addition, the laser irradiation device 324 irradiates the laser along the x-axis direction, for example at intervals of 25 [micrometers]. As a result, the heat applied to the base material (hoop material) due to laser irradiation can be reduced.

[0095] Next, the cleaning device 325 uses a solvent to clean and remove the unnecessary parts in the applied chromium. Reference numeral 310A is a top view showing the hoop material after being irradiated with laser and cleaned. In the hoop material shown in reference numeral 310A, reference numeral 331 shows a non-magnetic region. The width of the non-magnetic region 331 in the y-axis direction is about 0.3-0.5mm. In this way, through the second manufacturing process, the linear non-magnetic region 331 along the x-axis direction is formed at a predetermined position in the y-axis direction for the hoop material. In addition, as an example, the time spent on cleaning is 5 minutes.

[0096] After cleaning, the manufacturing system 300 winds the hoop material after forming the nonmagnetic region as shown at 326 .

[0097] (Third manufacturing process second stamping (finishing))

[0098] In the third manufacturing process, the manufacturing system 300 includes a punching device 342 as a finishing device. In addition, reference numeral 341 shows a state where the hoop material after the second manufacturing process is wound. Reference numeral 343 shows a state where the punched hoop material is wound.

[0099] like Figure 6 As shown, the punching device 342 adjusts the position of the hoop material 310A based on the positions of the guide holes 312 and 313 and performs punching so that the portions where the chromium weight ratio is 15 weight % or more become the narrow width portions 210 and 211 of the stator 201 . Figure 6 2 is a plan view showing a hoop material 310A before stamping of the stator 201 according to the present embodiment. The stator 201' is a stator before the fourth manufacturing step. Figure 6 In the figure, reference numeral 201' indicates a position where the stamping of the stator 201' is performed. In addition, the punching is a process in which the hoop material 310A is punched to punch out a part of the non-magnetic region 331 and to form a shape surrounding the rotor 202 for the stepping motor 7. That is, the stator 201' including the rotor receiving hole 203 is formed through the third manufacturing process.

[0100] Thus, the outer shape of the stator 201 ′ is completed in which the chromium weight ratio is different between the narrow width portions 210 and 211 and other portions.

[0101] (Fourth Manufacturing Process: Magnetic Annealing)

[0102] In the fourth manufacturing process, the manufacturing system 300 includes an annealing furnace 351 .

[0103] The annealing furnace 351 performs high temperature annealing (annealing) on ​​the stator 201 ′, thereby removing and relaxing the residual stress caused by the press working in the third manufacturing process.

[0104] The manufacturing system 300 is manufactured through the first to fourth manufacturing steps described above. Figure 3 The stator 201 is shown.

[0105] According to the stator 201 manufactured by the above manufacturing process, thermal deformation due to laser irradiation when forming the non-magnetic region can be reduced.

[0106] <Description of Photograph Example of Cross Section of Hoop Material after Laser Irradiation>

[0107] Then, in Figure 7-Figure 9 , , shows an example of a photograph of a cross section of a hoop material after the following process is performed: chromium applied to one surface of a hoop material made of permalloy is irradiated with laser to melt and diffuse the chromium by laser so that the weight ratio of chromium becomes 15 weight % or more. Figure 7-Figure 9 Each of the figures is a photographic example showing a cross section of a hoop material after the following process is performed: In the present embodiment, chromium applied to a hoop material made of permalloy is melt-diffused by laser so that the weight ratio of chromium becomes 15 weight % or more.

[0108] exist Figure 7-Figure 9 In the embodiment, the vertical direction (z-axis direction) is the thickness direction of the hoop material. In addition, the laser is irradiated from the surface (upper surface) coated with chromium. In addition, the thickness of the hoop material is, for example, 0.5 mm ± 0.1 mm. In addition, Figure 7-Figure 9 In the figure, reference numeral 401 denotes a molten portion melted by laser irradiation.

[0109] The scum P10 is a protrusion generated by laser irradiation.

[0110] Figure 7 An example is shown in which the molten portion 401 penetrates from the upper surface to the lower surface. Figure 8 An example is shown in which the molten portion 401 reaches the lower surface. Fig. 9 An example is shown in which the molten portion 401 does not reach the lower surface.

[0111] Figure 7 The label L1, Figure 8 The label L11, Fig. 9 The reference numerals L21 in FIG. 4 respectively indicate the width of the molten portion 401 observed from the laser irradiation side. Figure 7 The label L2, Figure 8 The label L12, Fig. 9 The reference numerals L22 respectively indicate the width of the molten portion at the center position in the thickness direction of the hoop material.

[0112] like Figure 7-Figure 9As shown, when the melting part 401 is formed in the hoop material by the manufacturing method of the present embodiment, the widths L1, L11, and L21 of the melting part 401 on the laser incident side are wider than the width of the melting part 401 except for the surface of the hoop material. In addition, as moving from one surface side (upper side) of the hoop material, which is a magnetic sheet material, toward the other surface side (lower side) in the thickness direction, the width of the melting part 401 becomes narrower and the cross-sectional area of the melting part 401 becomes smaller.

[0113] In addition, in any of the Figure 7-Figure 9 shown examples, the weight ratio of chromium in the melting part 401 is formed to be 15 wt% or more, and the melting part 401 becomes a non-magnetic region.

[0114] <Explanation of the EDS line analysis result>

[0115] Next, the result of the EDS line analysis of the melting part manufactured by the manufacturing method of the present embodiment will be described.

[0116] First, the outline of the EDS (Energy Dispersive X-ray Spectroscopy) line analysis will be described.

[0117] When X-rays are incident on an element, charges proportional to the energy of the X-rays are generated. An analysis device for performing EDS line analysis accumulates this charge on, for example, the gate electrode of a field-effect transistor and converts it into a current proportional to the amount of charge. Then, the analysis device pulse-converts the current change of each X-ray, and further measures it with a multi-channel analyzer as the number of pulses for each wave height (X-ray count). Moreover, the analysis device obtains the energy value (keV) of the X-ray on the horizontal axis and the count of the X-ray on the vertical axis, and makes the measurement result into a spectrum (for example, refer to Reference 1).

[0118] Reference 1:

[0119] “ (Basics of EDS Analysis)", Yamazaki, ブルカー・エイエックスエス (Co., Ltd.), 2014, https: / / www.bruker.com / fileadmin / user_upl oad / 8-PDF-Docs / X-rayDiffraction_ElementalAnalysis / Microanalysis_EBSD / Webinars / Br uker_Japanese_Webinar_2014-11-25_EDS_Feature_Analysis.pdf#search=%27%EF%BC%A5%EF %BC%A4%EF%BC%B3%E3%83%A9%E3%82%A4%E3%83%B3%E5%88%86%E6%9E%90%27 (Internet search 2017.9.10).

[0120] The analysis apparatus and analysis conditions are described.

[0121] The observation portion of the narrow width portions 210 and 211 was subjected to cross-sectional polishing (CP) processing using IB-09020CP (trade name) manufactured by JEOL Ltd. The acceleration voltage was 7 kV.

[0122] As a scanning electron microscope, a field emission scanning electron microscope (FE-SEM) (trade name: JSM-7800F, manufactured by JEOL Ltd.) was used.

[0123] After the sample was subjected to resin embedding and grinding using IB-09020CP manufactured by JEOL Ltd., the sample was subjected to ion milling.

[0124] The sample used for the measurement was a cross-section processed by ion milling {Ar (argon) ions, accelerated at 7 kV}.

[0125] The measurement environment is a vacuum degree of 10 -4 Up to 10 -5 Pa in a vacuum.

[0126] The EDS line analysis was performed using NORAN SYSTEM 7 (trade name) Ver3 manufactured by Thermo Fisher Scientific under the condition of a voltage of 15 kV.

[0127] Next, an example of the result of EDS line analysis of the molten portion is shown.

[0128] Fig. 10A and Fig. 10B FIG. 2 is a diagram showing an example of the result of EDS line analysis of the molten portion according to the present embodiment. Fig. 10AIn FIG. 1 , the figure indicated by reference numeral g1 is a figure showing the molten portion subjected to EDS line analysis. Figure 3 The long side direction of the stator 201 is shown. Fig. 10A The figure indicated by reference numeral g1 is the result of photographing the melted part at a magnification of 120 times using a reflection microscope. Fig. 10B The figure indicated by reference numeral g2 is a graph showing the results of line analysis. The horizontal axis is position [micrometer], and the vertical axis is weight %. Fig. 10B In the figure, the reference numeral g21 indicates the change in the weight % of Cr (chromium) relative to the distance, the reference numeral g22 indicates the change in the weight % of Fe (iron) relative to the distance, and the reference numeral g23 indicates the change in the weight % of Ni (nickel) relative to the distance. In addition, the area surrounded by the dotted line g24 is the area where the mass of chromium changes.

[0129] exist Fig. 10B The molten area is about 140 [micrometers]-400 [micrometers]. In this area, the weight ratio of chromium is about 20wt%-28wt%. The weight ratio of chromium in this area is more than 15wt%, so this area is paramagnetic at room temperature. Figure 4 Point b1 is this region. In addition, paramagnetism is a magnetism in which there is no magnetization when there is no external magnetic field, but magnetization occurs in the direction of the magnetic field if a magnetic field is applied. In addition, the state of paramagnetism at room temperature refers to a non-magnetic state. In addition, the weight ratio of iron in this region is about 41-51wt%, and the weight ratio of nickel is about 30-38wt%.

[0130] Here, in the case of Permalloy 38, which is an Fe-Ni-Cr alloy containing 54 wt% of iron, 38 wt% of nickel, and 8 wt% of chromium, it is ferromagnetic at room temperature. In addition, ferromagnetism refers to the magnetism of a substance having a magnetic moment.

[0131] exist Fig. 10B The area with a chromium weight ratio of about 8 wt% is from the outer end to about 140 [micrometers] and after 400 [micrometers]. The chromium weight ratio in these areas is about 7-8 wt%, which is equivalent to the weight ratio of the chromium component of Permalloy No. 38, so these areas are ferromagnetic areas. Figure 4 Point a1 and point c are these areas.

[0132] As described above, the stator 201 manufactured by the manufacturing process of this embodiment has a paramagnetic region with a chromium weight ratio of 15wt% or more, a ferromagnetic region with a chromium weight ratio of 7-8wt%, and a region with a significantly changed chromium weight ratio ( Fig. 10B Thus, the stator 201 manufactured by the manufacturing process of this embodiment has a non-magnetic region ( Figure 4In addition, in the stator 201, the difference between the weight ratio Xwt% of chromium in the molten portion and the weight ratio Ywt% of chromium in other regions is 6wt% or more (XY≥6), and the weight ratio of chromium in the molten portion is greater than the weight ratio of chromium in the base material.

[0133] In addition, if Fig. 10B As shown, the weight ratio of chromium in the non-magnetic molten region is 6 wt % to 18 wt % greater than 8 wt % of the weight ratio of chromium in the magnetic plate material except the non-magnetic molten region.

[0134] In addition, regarding the stepping motor 7 involved in this embodiment, the stator 201 is made of Fe-Ni alloy, but it is preferably made of Fe-Ni alloy with high magnetic permeability. For example, the above-mentioned No. 38 Permalloy can be exemplified. Fig.11 In the state diagram of Fe-38%Ni-8%Cr, the Curie temperature is 500K or more (point X), and when the weight ratio of Cr is 15wt% or more, the Curie temperature becomes 300K. That is, when the weight ratio of Cr is 15wt% or more, it becomes an austenite phase (point X') at room temperature. Fig.11 It is a state diagram of the ternary alloy of Fe-Ni-Cr. That is, near the room temperature at which the stepping motor 7 needs to be driven, when the weight ratio of Cr is 15wt% or more, the non-magnetic state of the stator 201 can be ensured. In addition, Fig.11 It is a reference to the state diagram on page 188 of Ternary alloys Between Fe, Co or Ni and Ti, V, Cr or Mn (Landolt-Bornstein new Series III / 32A).

[0135] <Cross-sectional shape of stator 201>

[0136] Fig. 12A and Fig. 12B It is a diagram for explaining a protrusion generated in the stator according to the present embodiment.

[0137] Fig. 12A 2 is a perspective view showing a stator 201 according to the present embodiment. Fig. 12A , the long side direction of the stator 201 is taken as the y-axis direction, the short side direction is taken as the x-axis direction, and the thickness direction is taken as the z-axis direction.

[0138] The stator 201 has a train wheel surface 201a, which is a surface facing the train wheel 11 when the stator 201 is installed in the movement. In addition, the stator 201 has a main plate surface 201b, which is a surface facing the main plate 51 when the stator 201 is installed in the main plate 51 of the movement. In the stator 201, the train wheel surface 201a is the back side of the main plate surface 201b.

[0139] Furthermore, in order to prevent the train wheel face 201a and the main plate face 201b from being installed inversely during assembly, the stator 201 is preferably left-right asymmetrical.

[0140] The narrow width portion 210 and the narrow width portion 211 include processing positions coated with chromium and irradiated with laser in the above-mentioned second manufacturing process. The main plate surface 201b is a surface coated with chromium and irradiated with laser in the second manufacturing process. That is, the narrow width portion 210 and the narrow width portion 211 include non-magnetic areas that are demagnetized by irradiating laser from the main plate surface 201b side.

[0141] In the third manufacturing process described above, the rotor receiving hole 203 of the stator 201 is formed by punching using the punching device 342. In the punching device 342, a fixed die (hereinafter also referred to as a concave die) is connected to the main plate surface 201b side of the stator 201. In addition, in the punching device 342, a movable die (hereinafter also referred to as a convex die) is connected to the gear train surface 201a side of the stator 201.

[0142] That is, a concave die is arranged on the main plate surface 201b side, a convex die is arranged on the gear train surface 201a side, and shearing is performed using the concave die and convex die arranged in this way to form the rotor accommodation hole 203. In this example, the outer shape, the screw hole 218a and the screw hole 218b are also formed by shearing in the same manner as the rotor accommodation hole 203.

[0143] Fig. 12B It is along Fig. 12A A cross-sectional view of the stator 201 along line AA. Fig. 12B , the short side direction of the stator 201 is taken as the x-axis direction, and the thickness direction is taken as the z-axis.

[0144] The narrow width portion 210 and the narrow width portion 211 are provided around the rotor accommodation hole 203 .

[0145] In the second manufacturing process described above, chromium is applied and laser irradiation is performed to form a Cr diffusion region A1 in the narrow portion 210. As the Cr diffusion region A1 is formed, scum P1 is formed on the main plate surface 201b side of the narrow portion 210. For the same reason, scum P2 is formed on the main plate surface 201b side of the narrow portion 211.

[0146] Cr diffusion area A1, Cr diffusion area A2, scum P1 and scum P2 are Figure 7-Figure 9 The molten portion 401 in the embodiment of the present invention.

[0147] Burrs P3 are generated on the main plate surface 201b side of the narrow portion 210. The burrs P3 are generated when the rotor housing hole 203 is punched out in the third manufacturing step. Burrs P6 are generated on the main plate surface 201b side of the narrow portion 211 for the same reason.

[0148] In addition, burrs P5 are generated on the main plate surface 201b side of the narrow portion 210. The burrs P5 are generated when the outer shape is punched out. For the same reason, burrs P4 are generated on the main plate surface 201b side of the narrow portion 211.

[0149] <Organization Module 83>

[0150] Fig.13 This is a plan view of an example of the internal structure of the mechanism module according to the present embodiment as viewed from the front side. Fig.14 This is a cross-sectional view showing an example of the internal structure of the mechanism module according to the present embodiment when viewed from the side.

[0151] like Fig.13 As shown in FIG. 8 , the mechanism module 83 includes an hour hand drive mechanism 91, a minute hand drive mechanism 92, and a second hand drive mechanism 93. Fig.14 As shown, the mechanism module 83 includes: a main plate 51 and a wheel train bridge 52; an hour wheel pressing member 53, which is arranged on the back side of the main plate 51 and fixed to the main plate 51; and a second bridge 54, which is arranged between the main plate 51 and the wheel train bridge 52. The main plate 51 and the wheel train bridge 52 support the hour hand driving mechanism 91, the minute hand driving mechanism 92 and the second hand driving mechanism 93.

[0152] In this example, the first motor 40A included in the hour hand drive mechanism 91 is described to illustrate the relationship between the stator 201 and the main plate 51. The second motor 40B included in the minute hand drive mechanism 92 and the third motor 40C included in the second hand drive mechanism 93 are the same as the first motor 40A.

[0153] In addition, the first motor 40A is an example of the stepping motor 7, the rotor 45 is an example of the rotor 202, the stator 44 is an example of the stator 201, the rotor hole 44a is an example of the rotor accommodating hole 203, the magnetic core 42 is an example of the magnetic core 208, the coil wire 43 is an example of the coil 209, and the screw 48 is an example of the screw 220.

[0154] like Fig.13 As shown, the main plate 51 constitutes a substrate of the mechanism module 83. The main plate 51 is formed of, for example, a resin material in a plate shape having an axial direction as a thickness direction.

[0155] The hour hand drive mechanism 91 rotates the hour hand 12 and includes a first rotating shaft 85 on which the hour hand 12 is mounted, a first motor 40A that drives the first rotating shaft 85 , and an hour hand train wheel 30A that decelerates the rotational driving force of the first motor 40A and transmits it to the first rotating shaft 85 .

[0156] The first motor 40A is a stepping motor in which the rotor 45 rotates 180° in one step. The first motor 40A is provided at a position that does not overlap with the rotation axis O. The first motor 40A includes: a coil block 41 including a magnetic core 42 and a coil conductor 43 wound around the magnetic core 42; a stator 44 disposed so as to contact both end portions of the magnetic core 42 of the coil block 41; and a rotor 45 disposed in a rotor hole 44a of the stator 44.

[0157] The coil block 41 includes a magnetic core 42 , a coil conductor 43 , and a coil lead substrate 46 fixed to one end of the magnetic core 42 .

[0158] The magnetic core 42 extends in a direction orthogonal to the axial direction and the radial direction. The magnetic core 42 is fixed to the main board 51 at its two ends by screws 48. The coil lead substrate 46 is a printed substrate. The coil lead substrate 46 is arranged on the front side of one end of the magnetic core 42 and is fastened together with the magnetic core 42 by screws 48. When viewed from the axial direction, the coil lead substrate 46 extends from a fixed portion relative to one end of the magnetic core 42 toward the central portion of the main board 51. A pair of wirings 47 are formed on the surface of the coil lead substrate 46. At one end 47a on the magnetic core 42 side of each wiring 47, the end of the coil conductor 43 is welded respectively.

[0159] A relay substrate 24 is arranged on the front side of the coil lead substrate 46. The relay substrate 24 is a component having a thickness in the axial direction. The relay substrate 24 has a pair of relay wirings 24a extending from the front surface to the back surface. The pair of relay wirings 24a contact the pair of wirings 47 of the first motor 40A on the back surface of the relay substrate 24, and contact the terminals of the circuit block 23 on the surface of the relay substrate 24. Thus, the relay substrate 24 electrically connects the pair of wirings 47 of the coil lead substrate 46 to the circuit block 23.

[0160] The stator 44 is arranged radially inward of the core 42 . The stator 44 is fastened to the main plate 51 together with the core 42 by a pair of screws 48 .

[0161] The rotor 45 is arranged radially inward of the magnetic core 42. The rotor 45 is rotatably supported by the main plate 51 and the train wheel bridge 52 (see Figure 4 ).

[0162] like Fig.13 and Fig.14As shown, the hour hand train wheel 30A has a first hour hand intermediate wheel 31, a second hour hand intermediate wheel 32, and an hour wheel 33. The first hour hand intermediate wheel 31 has a first hour hand intermediate gear 31a and a first hour hand intermediate pinion 31b, and is rotatably supported by the main plate 51 and the train wheel bridge 52. The first hour hand intermediate gear 31a meshes with the pinion 45a of the rotor 45 of the first motor 40A. The second hour hand intermediate wheel 32 has a second hour hand intermediate gear 32a and a second hour hand intermediate pinion 32b, and is rotatably supported by the main plate 51 and the train wheel bridge 52. The second hour hand intermediate gear 32a meshes with the first hour hand intermediate pinion 31b of the first hour hand intermediate wheel 31.

[0163] The hour wheel 33 is rotatably inserted into the center tube 55 on the back side of the main board 51. The center tube 55 is held by the main board 51. The center tube 55 extends coaxially with the rotation axis O and protrudes from the main board 51 to the back side. That is, the hour wheel 33 is arranged coaxially with the rotation axis O. The hour wheel 33 has an hour wheel gear 33a, and the hour wheel gear 33a is meshed with the second hour hand intermediate pinion 32b of the second hour hand intermediate wheel 32. The hour wheel 33 is pressed from the back side by the hour wheel pressing member 53. The hour wheel 33 is pushed toward the main board 51 side by the first needle seat 56 arranged between the hour wheel pressing member 53 and the hour wheel gear 33a. The end of the back side of the hour wheel 33 protrudes from the hour wheel pressing member 53 to the back side. That is, the hour wheel 33 is the first rotating shaft 85. The hour hand 12 is installed at the end of the back side of the hour wheel 33.

[0164] <Retreat portion of main board 51>

[0165] As described above, the stator 201 (stator 44 ) is screwed to the main board 51 by means of the screws 220 (screws 48 ).

[0166] That is, in the present embodiment, the stator 201 is provided so that the main plate surface 201 b of the stator 201 faces the main plate 51 .

[0167] Here, Figures 15A-15D Each of them is a cross-sectional view showing an example of a retreat portion included in the main plate 51 according to the present embodiment. Figures 15A-15D The figures show the stator 201 screwed to the main board 51 and Fig. 12B The corresponding cross-sectional view.

[0168] As described above, in the stator 201, scum P10 (hereinafter referred to as scum P10 when scum P1 and scum P2 are not distinguished) and burrs P20 (hereinafter referred to as burrs when burrs P2, burrs P3, burrs P4 and burrs P5 are not distinguished) are provided to protrude from the main plate surface 201b.

[0169] Fig.15AThe main plate 51 a is shown as an example in which the main plate 51 a has the escape portions E1 and E2 at positions corresponding to the narrow width portion 210 and the narrow width portion 211 , respectively. The main plate 51 a is one example of the main plate 51 .

[0170] The main plate surface 201b of the narrow portion 210 and the narrow portion 211 faces the main plate 51a. Since the narrow portion 210 and the narrow portion 211 have dross P10 and burr P20, the main plate 51a has the escape portions E1 and E2 for avoiding contact between the main plate 51a and the dross P10 and burr P20.

[0171] In this example, the escape portion E1 is a concave cutout for preventing the scum P1, burrs P3 and P5 of the narrow width portion 210 from contacting the main plate 51a. Similarly, the escape portion E2 is a concave cutout for preventing the scum P2, burrs P4 and P6 of the narrow width portion 211 from contacting the main plate 51a.

[0172] exist Fig.15A In the example shown, the length of the narrow width portion 210 in the short side direction (x-axis direction) is defined as width W1. In addition, the length of the retreat portion E1 in the same direction is defined as width W2. In this example, width W1 is smaller than width W2. The narrow width portion 211 has the same configuration.

[0173] In addition, Fig.15A In the illustrated example, the main plate 51 has a bank b1 which is not a cutout portion between the escape portion E1 and the escape portion E2 .

[0174] Fig. 15B An example is shown in which the main board 51 b has a common escape portion E3 at positions corresponding to the narrow width portion 210 and the narrow width portion 211. The main board 51 b is an example of the main board 51.

[0175] In this example, the main board 51b has a common escape portion E3, which is used to prevent the scum P1 of the narrow width portion 210 from contacting the main board 51b, and an escape portion used to prevent the scum P2 of the narrow width portion 211 from contacting the main board 51b. The escape portion E3 is a concave cutout used to prevent the scum P10 and burr P20 of the narrow width portion 210 and the narrow width portion 211 from contacting the main board 51b.

[0176] Fig. 15C An example of the escape portion E4 included in the main plate is shown in the case where the burr P20 is not generated in the narrow width portion 210 and the narrow width portion 211 or the burr P20 is small enough to be ignored. The main plate 51 c is an example of the main plate 51 .

[0177] In this example, the narrow width portion 210 has scum P1. The escape portion E4 of the main plate 51c is a concave cutout for preventing the scum P1 from contacting the main plate 51c. In addition, the narrow width portion 211 has scum P2. The escape portion E5 of the main plate 51c is a concave cutout for preventing the scum P2 from contacting the main plate 51c.

[0178] Since the narrow width portions 210 and 211 do not have the burrs P20 or the burrs P20 are so small as to be ignored, the escape portions E4 and E5 only need to have a size that can prevent the scum P10 from contacting the main plate 51 c.

[0179] exist Fig. 15C In the example shown, the length of the narrow width portion 210 in the short side direction (x-axis direction) is defined as width W1. In addition, the length of the retreat portion E4 in the same direction is defined as width W3. In this example, width W1 is greater than width W3. The narrow width portion 211 has the same configuration.

[0180] By configuring in this way, the main plate 51c can reduce the size of the cutout. Therefore, the main plate 51c can suppress a decrease in strength due to the cutout.

[0181] Fig.15D The example in which the escape portions E6 and E7 included in the main plate 51d are through holes penetrating the main plate 51d is shown. The main plate 51d is an example of the main plate 51.

[0182] In this example, the escape portion E6 for preventing the scum P1 of the narrow portion 210 from contacting the main plate 51d is a through hole. Similarly, the escape portion E7 for preventing the scum P2 of the narrow portion 211 from contacting the main plate 51d is a through hole.

[0183] With such a configuration, the main plate 51d can prevent the scum P10 from coming into contact with the main plate 51d even when the scum P10 is large in size.

[0184] exist Figures 15A-15D In each of the examples shown, the thickness of the main board 51 at the portion where the stator 201 engages with the main board 51 is 0.6 mm to 0.8 mm. Fig.15A The depth of the setbacks E1 and E2 shown, Fig. 15B The depth of the setback E3 shown and Fig. 15C The depths of the recessed portions E4 and E5 shown are respectively about 0.1 mm.

[0185] However, in Figures 15A-15DIn each of the examples shown, the size of the escape portions E1 to E7 is not limited, and the escape portions E1 to E7 may be sized to prevent the scum P10 from contacting the main plates 51 a to 51 d .

[0186] In addition, the stator 201 is described as being screwed to the main plate 51, but the present invention is not limited to this example. The stator 201 and the main plate 51 may be fixed by a method other than screwing.

[0187] In addition, the object holding the stator 201 is not limited to the main plate 51. A configuration in which another member such as a stator holding member is arranged between the stator 201 and the main plate 51 may be adopted.

[0188] For example, the stator holding member has a concave escape portion at a position facing the nonmagnetic region, and is connected to a part of the main plate surface 201b to hold the stator 201. The thickness of the escape portion is thinner than other portions.

[0189] The main plate 51 , the holding member, or the like may be any member as long as it can arrange the stator 201 so as to face the narrow width portion 210 and the narrow width portion 211 .

[0190] <Summary of Effects of Implementation Methods>

[0191] As described above, in this embodiment, dross P10 is generated on the main plate surface 201b of the stator 201. The main plate surface 201b is the back surface of the train wheel surface 201a. Therefore, in this embodiment, the dross P10 does not contact the train wheel 11.

[0192] In the stator 201 according to the above embodiment, the surface where the scum P10 and the surface where the burr P20 are generated are the same surface. Therefore, since neither the scum P10 nor the burr P20 exists on the train wheel surface 201 a , the scum P10 and the burr P20 do not contact the train wheel 11 .

[0193] Furthermore, according to the above-described embodiment, the main plate 51 included in the movement 82 includes the escape portions E1 to E7 , so that the main plate 51 does not come into contact with the scum P10 and the burr P20 .

[0194] Therefore, according to the embodiment of the present application, even if the main plate 51 is not subjected to treatments such as scum removal and burr removal, the manufacturability and assemblability are not hindered when the movement 82 is manufactured.

[0195] According to the above-described embodiment, the timepiece 1 includes the movement 82. That is, the main plate 51 included in the timepiece 1 includes the escape portions E1 to E7. Therefore, the main plate 51 does not come into contact with the scum P10 and the burr P20.

[0196] Therefore, according to the embodiment of the present application, even if the main plate 51 is not subjected to treatments such as scum removal and burr removal, the manufacturability and assemblability are not impaired when the timepiece 1 is manufactured.

[0197] Furthermore, the manufacturing method of the above embodiment includes a step of placing the main plate surface 201b of the stator 201 opposite to the main plate 51. In this embodiment, the main plate surface 201b is the surface where the scum P10 and the burr P20 are generated, so the scum P10 and the burr P20 do not contact the gear train 11.

[0198] Although the embodiments of the present invention have been described above with reference to the drawings, the specific configuration is not limited to the above-described embodiments. The present invention also includes configurations that implement design changes within the scope of the present invention.

[0199]

Number Description

[0200] 1...clock, 7...stepping motor, 201...stator, 201a...gear train surface, 201b...main board surface, 202...rotor, 203...rotor accommodating hole, 204...cut-out portion, 205...cut-out portion, 208...magnetic core, 209...coil, 210...narrow width portion, 211...narrow width portion, 218a...screw hole, 218b...screw hole, 220...screw, 401...melting portion, 51...main board.

Claims

1. A movement comprising a stator and a stator holding member for holding the stator, The stator comprises: A magnetic plate having a main plate surface that faces the main plate when mounted on the main plate of the movement, and a rotor receiving hole is formed in a portion of the magnetic plate; and Chromium is applied to the main plate surface around the rotor housing hole and a non-magnetic region is demagnetized by irradiating the chromium with laser light from the main plate surface side. The stator holding component, The stator has a retreat portion thinner than other portions at a position facing the nonmagnetic region of the stator, and the stator holding member is connected to a portion of the main plate surface to hold the stator. The escape portion has a space in which the stator and the stator holding member do not contact each other.

2. The movement according to claim 1, in, The fixed mold is connected to the main plate surface side and the movable mold is connected to the back side of the main plate surface and a portion is formed by shearing.

3. A timepiece comprising the movement according to claim 2. 4 . A method for manufacturing a movement, comprising a setting step of setting the main plate surface of the stator provided in the movement according to claim 1 or claim 2 so as to face a main plate.