Method for making a CFET device

By using dual-on-insulator semiconductor substrates and heat treatment technology in CFET devices, the problem of improving the density and current performance of CFET devices is solved, high-precision control of channel and electrical insulation layer thickness is achieved, and the height/width problem in traditional technologies is overcome. Ratio limit.

CN112640090BActive Publication Date: 2024-10-15SOITEC SA
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN201980057027.5
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Priority Date
2018-09-03
Filing Date
2019-09-03
Publication Date
2024-10-15
Estimated Expiration
2039-09-03

AI Technical Summary

Technical Problem

It is difficult to increase the transistor density per unit area while maintaining acceptable electrical performance of existing CFET devices, and there are technical limitations in the height/width ratio of fin manufacturing, which affects the amount of current.

Method used

A dual-on-insulator semiconductor substrate is used, including a carrier substrate, two single-crystal semiconductor layers, and two electrical insulating layers. The first single-crystal semiconductor layer is smoothed to less than 0.1nm RMS roughness through heat treatment, and is formed on the dual SOI substrate. Trench to manufacture CFET devices, achieving high-precision control of channel height and electrical insulation layer thickness.

Benefits of technology

It improves the density and current performance per unit area of ​​CFET devices, ensures high-precision control of channel height and electrical insulation layer thickness, and avoids the problem of difficult height control in traditional horizontal etching.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN112640090B_ABST
    Figure CN112640090B_ABST
Patent Text Reader

Abstract

The present invention relates to a method for manufacturing a CFET device, characterized in that the method comprises the following steps: forming a double semiconductor-on-insulator substrate, which comprises, from the base to its surface, in sequence: a carrier substrate (1), a first electrical insulating layer (2a), a first single crystal semiconductor layer (2b), a second electrical insulating layer (3a) and a second single crystal semiconductor layer (3b); forming a groove from the surface of the substrate to the first electrical insulating layer (2a) to form at least one fin (F); in each fin (F), forming a channel of a first transistor in the first semiconductor layer (2b), and forming a channel of a second transistor of the opposite type to the first transistor in the second semiconductor layer (3b), the step of forming the double semiconductor-on-insulator type substrate comprises: a first step and a second step of transferring the layer and a heat treatment at a temperature, the temperature being high enough to smooth the first single crystal semiconductor layer to a roughness of less than 0.1nm RMS.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to a method for manufacturing a CFET device. Background Art

[0002] A CFET device (CFET is an abbreviation for "complementary field-effect transistor") can be defined as a structure that includes complementary fin field-effect transistors (FinFETs). In other words, a CFET device is a three-dimensional electronic device that includes stacking two different types of FinFET transistors together, such as stacking an n-type transistor (so-called nFET) on a p-type transistor (so-called pFET).

[0003] Such stacking allows reducing the footprint of the device and thus increasing the density of transistors per unit area.

[0004] Traditionally, CFET devices are made of a bulk monocrystalline silicon substrate integrated with a buried sacrificial layer. The sacrificial layer may be, for example, a silicon germanium (SiGe) layer, wherein etching allows vertical trenches that define the various fins of the transistor. Selective etching of the sacrificial layer allows vertical physical separation of the two n-type and p-type FinFET transistors.

[0005] The active regions intended to form the source and drain regions of the complementary FinFET transistor may be n-doped and p-doped, for example by selective implantation in the thickness of the structure thus formed.

[0006] Furthermore, the channel can be n-doped or p-doped, depending on the type of target application. This doping can also be performed by selective implantation in the thickness of the structure.

[0007] The reduction in the width of the fin must be accompanied by an increase in the height of the active area, particularly the channel, in order to allow an increase in the amount of current that can pass.

[0008] However, there are technological limitations in the fabrication of fins, particularly in terms of height / width ratio, that push the transistor density per unit area that can be achieved while maintaining acceptable electrical performance towards a threshold. Summary of the invention

[0009] It is an object of the present invention to improve the design and fabrication of CFET devices.

[0010] To this end, the present invention provides a method for manufacturing a CFET device, characterized in that the method comprises the following steps:

[0011] - forming a double semiconductor-on-insulator substrate, the double semiconductor-on-insulator substrate comprising, from its base to its surface, in order: a carrier substrate, a first electrical insulating layer, a first single crystal semiconductor layer, a second electrical insulating layer, and a second single crystal semiconductor layer;

[0012] - forming a trench from said surface of said substrate to said first electrically insulating layer so as to form at least one fin;

[0013] - in each fin, forming a channel of a first transistor in the first semiconductor layer, and forming a channel of a second transistor of opposite type to the first transistor in the second semiconductor layer;

[0014] The steps of forming the double semiconductor-on-insulator substrate include:

[0015] a first layer transfer step to transfer the first electrically insulating layer and the first single-crystalline semiconductor layer to the carrier substrate to form a first semiconductor-on-insulator substrate, the first layer transfer step comprising a thermal treatment at a sufficiently high temperature to smooth the first single-crystalline semiconductor layer to a roughness of less than 0.1 nm RMS;

[0016] - a second layer transfer step after the heat treatment to transfer the second electrically insulating layer and the second single crystalline semiconductor layer to the first single crystalline semiconductor layer of the first semiconductor-on-insulator substrate.

[0017] Advantageous but optional features of this method can be implemented individually or in combination where technically appropriate:

[0018] - the trench is formed by etching, the first electrically insulating layer forming a stop layer for the etching;

[0019] - the thickness of the first single crystal semiconductor layer and the second single crystal semiconductor layer is between 25 nm and 40 nm;

[0020] - the thickness of the second electrically insulating layer is between 10 nm and 30 nm;

[0021] - the smoothing heat treatment of the first single-crystalline semiconductor layer is performed at a temperature between 1000° C. and 1200° C. for a time between 10 minutes and 120 minutes;

[0022] The method further comprises performing a heat treatment at a temperature between 1100° C. and 1250° C. for a time shorter than one minute, the heat treatment being used to finish the second single-crystalline semiconductor layer.

[0023] The CFET device thus formed comprises a carrier substrate and at least one fin extending from the carrier substrate, in which two stacked field effect transistors of opposite types are arranged, the device being characterized in that each fin, starting from the carrier substrate, comprises:

[0024] - a first electrically insulating layer;

[0025] - a first single crystal semiconductor layer, the first single crystal semiconductor layer forming a channel of a first transistor;

[0026] - a second electrically insulating layer;

[0027] - a second single crystal semiconductor layer, which forms a channel of a second transistor.

[0028] “Stacked” means that the transistors are stacked in a direction perpendicular to the main surface of the carrier substrate.

[0029] With regard to the first semiconductor layer and the second semiconductor layer, the following embodiments are conceivable, optionally in combination when technically relevant:

[0030] - the first semiconductor layer and the second semiconductor layer are made of opposite types of silicon doping;

[0031] - the first semiconductor layer and the second semiconductor layer are made of silicon having different crystal orientations;

[0032] - the first semiconductor layer and the second semiconductor layer are made of different materials;

[0033] - the semiconductor layer forming the channel of the n-type transistor is made of strained silicon;

[0034] - The semiconductor layer forming the channel of the p-type transistor is made of silicon germanium.

[0035] With regard to the first electrically insulating layer and the second electrically insulating layer, the following embodiments are conceivable, optionally in combination when technically relevant:

[0036] - the first electrically insulating layer and / or the second electrically insulating layer is made of silicon oxide (SiO2);

[0037] - the first electrically insulating layer and the second electrically insulating layer are made of different materials;

[0038] - the first electrically insulating layer is made of a material with a high dielectric constant ("high-k" material);

[0039] - The second electrically insulating layer is made of a material with a low dielectric constant ("low-k" material).

[0040] According to one implementation form, the carrier substrate comprises at least one additional layer selected from the following layers:

[0041] - Charge trapping layer;

[0042] - epitaxial semiconductor layer;

[0043] - A COP-free CZ silicon layer, ie a layer without COP-type crystal defects.

[0044] In certain embodiments, the fabrication of a CFET device may include the following steps:

[0045] - forming a double semiconductor-on-insulator substrate, the double semiconductor-on-insulator substrate comprising, in order from its base to its surface: a carrier substrate comprising a functional layer (such as a polycrystalline silicon layer, a so-called COP-free single-crystalline silicon layer or an epitaxial semiconductor layer, which may optionally be doped); a first electrically insulating layer, a first single-crystalline semiconductor layer; a second electrically insulating layer and a second single-crystalline semiconductor layer;

[0046] - forming a trench from said surface of said substrate to said first electrically insulating layer to form at least one fin;

[0047] - in each fin, a channel of a first transistor is formed in the first semiconductor layer, and a channel of a second transistor of opposite type to the first transistor is formed in the second semiconductor layer,

[0048] The steps of forming the double semiconductor-on-insulator substrate include:

[0049] - a first layer transfer step in order to transfer the first electrically insulating layer and the first single-crystalline semiconductor layer to the carrier substrate, thereby forming a first semiconductor-on-insulator substrate from a first donor substrate, the first donor substrate comprising a layer suitable for being etched selectively with respect to the first single-crystalline semiconductor layer (the layer can advantageously be produced by epitaxy) and a weakened zone (can advantageously be formed by implanting atomic species) located in the first donor substrate at a depth strictly greater than the thickness of the two layers;

[0050] - a second layer transfer step after selectively etching a layer adapted to be selectively etched relative to the first single crystalline semiconductor layer, so as to transfer the second electrically insulating layer and the second single crystalline semiconductor layer to the first single crystalline semiconductor layer on the first semiconductor-on-insulator substrate.

[0051] Particularly advantageously, the method allows obtaining a roughness of the first single-crystalline semiconductor layer of less than 0.1 nm RMS without using a thermal budget that is susceptible to damaging the functional layer. BRIEF DESCRIPTION OF THE DRAWINGS

[0052] Other features and advantages of the present invention will be apparent from the following detailed description with reference to the accompanying drawings, in which:

[0053] - Figure 1 is a schematic cross-sectional view of a CFET device according to one embodiment;

[0054] - Figure 2 is a schematic cross-sectional view of a CFET device according to another embodiment, wherein the carrier substrate includes a functional layer;

[0055] - FIG. 3A to FIG. 3F Various fabrication steps of a double semiconductor-on-insulator substrate suitable for forming a CFET device are schematically illustrated.

[0056] To aid clarity of the drawings, the various drawings are not necessarily drawn to scale.

[0057] In the drawings, the same reference numbers are used to represent the same elements or elements that perform the same function. DETAILED DESCRIPTION

[0058] The present invention proposes to use a semiconductor-on-insulator substrate to replace the above-mentioned bulk silicon substrate to form a CFET device, wherein the semiconductor-on-insulator substrate includes a carrier substrate, two single crystal semiconductor layers and two electrical insulation layers, wherein the two electrical insulation layers respectively separate the two semiconductor layers on the one hand, and separate the carrier substrate and the semiconductor layer closest to the carrier substrate on the other hand.

[0059] Compared with a traditional SOI substrate (SOI is the abbreviation of silicon-on-insulator) which includes a single crystal semiconductor layer and an electrical insulating layer between a carrier substrate and a semiconductor layer, this semiconductor-on-insulator substrate is called "double SOI" due to the presence of two pairs of semiconductor layers and electrical insulating layers.

[0060] The carrier substrate may be made of a semiconductor (eg silicon) or of another material, depending on whether the carrier substrate has to perform only a mechanical carrier function or an electrical function within the device.

[0061] Such a double SOI substrate can be manufactured by two consecutive transfers of a single-crystalline semiconductor layer to a carrier substrate. This is particularly possible using SmartCut TM The method comprises the following steps:

[0062] - providing a carrier substrate,

[0063] - providing a first single-crystalline semiconductor donor substrate,

[0064] - forming a weakened zone in said donor substrate so as to define a first thin surface layer therein (said weakened zone possibly being formed by implanting atomic species at a defined depth in the donor substrate),

[0065] - bonding the first donor substrate to the carrier substrate with the first electrically insulating layer at the bonding interface,

[0066] - separation of the first donor substrate along the weakened zone, resulting in the transfer of the first thin layer to the carrier substrate (obtaining SOI),

[0067] - performing a finishing treatment on the first transferred layer in order to repair or remove defects related to the separation step and to give said layer the desired final roughness and thickness characteristics,

[0068] - providing a second single crystalline semiconductor donor substrate, which may be the same as or different from the first single crystalline semiconductor donor substrate,

[0069] - forming a weakened area in said second donor substrate to define a second thin surface layer therein,

[0070] - bonding a second donor substrate to the preformed SOI, with the second electrically insulating layer at the bonding interface between the transferred first semiconductor layer and the second donor substrate,

[0071] - separation of the second donor substrate along the weakened zone, resulting in the transfer of the second thin layer to the carrier substrate (obtaining a double SOI),

[0072] - A finishing treatment is performed on the second transferred layer in order to repair or remove defects related to the separation step and to give said layer the desired final roughness and thickness characteristics.

[0073] The following will refer to FIG. 3A to FIG. 3F Describe the implementation details of this method.

[0074] Each of the single-crystalline semiconductor layers is intended to form an active region (source, drain and channel) of a corresponding FinFET transistor, the two transistors being of opposite types. For example, the active region of a pFET transistor is formed in the first single-crystalline semiconductor layer closest to the carrier substrate, while the active region of an nFET transistor is formed in the second single-crystalline semiconductor layer farthest from the carrier substrate. Conversely, according to another example, the active region of an nFET transistor may be formed in the first single-crystalline semiconductor layer, and the active region of a pFET transistor may be formed in the second single-crystalline semiconductor layer.

[0075] In a manner known per se, dry etching is performed on the double SOI substrate to form trenches allowing parallel fins to be defined.

[0076] In this paper, the "width" of the fin (in Figure 1The “height” (denoted by L in FIG. 1 ) refers to the dimension of the fin in a direction parallel to the main surface of the carrier substrate, which defines the width of the channel, while the “height” (denoted by L in FIG. 1 ) refers to the dimension of the fin in a direction parallel to the main surface of the carrier substrate, which defines the width of the channel. Figure 1 The dimension L (denoted by H in the figure) refers to the dimension of the fin in a direction perpendicular to the main surface of the carrier substrate (i.e., in the thickness direction of the double SOI substrate). The length of the channel extends in a direction perpendicular to the dimensions L and H and is defined by the distance between the source and drain distributed in this direction.

[0077] With respect to known CFET devices, the use of a dual SOI substrate has many advantages.

[0078] On the one hand, the height of the n-channel and p-channel (in Figure 1 Indicated as h T1 and h T2 ) is equal to the thickness of the semiconductor layer from which they are formed; therefore, due to the quality of the layer transfer process, this height can be controlled very accurately, which ensures a high precision and a high degree of uniformity in the thickness of the transferred semiconductor layer and the electrically insulating layer. The thickness of the transferred semiconductor layer after the finishing step may, for example, be between 4nm and 100nm, wherein the thickness can be controlled to a maximum of + / -0.5nm with respect to the target. The thickness of the produced electrically insulating layer may, for example, be between 10nm and 200nm (in particular the limit of 200nm applies to the first electrically insulating layer, the second electrically insulating layer being advantageously thinner), wherein the thickness can be controlled to a maximum of + / -1nm with respect to the target. The control of the variability of the thickness of the transferred / produced layer is adjusted by its influence on the variability of the transistor, which is well known to those skilled in the art. In prior art CFET devices, the height of the channel is defined by horizontal etching that is not well controlled.

[0079] Furthermore, the n-channel and the p-channel are separated by a layer which not only forms a physical boundary but also electrically insulates the channels. Likewise, the channel of the transistor closest to the carrier substrate is physically and electrically insulated from the carrier substrate.

[0080] Furthermore, the first electrically insulating layer advantageously forms an etch stop layer during the formation of the trenches.

[0081] Furthermore, the method for producing a double SOI substrate allows the materials of the single-crystalline semiconductor layer and the electrically insulating layer to be varied in order to adapt them to the properties sought.

[0082] Thus, in one embodiment, both single-crystalline semiconductor layers are made of silicon, but have different doping types. Preferably, the two layers are weakly doped, ie, the dopant concentration is less than or equal to 10 e 15 at / cm 3 .

[0083] In another embodiment, or in combination with the preceding embodiment, the single-crystalline semiconductor layers are both made of silicon, but have different crystal orientations. This allows the mobility of the carriers of each of the two FinFET transistors to be optimized: in particular, the crystal orientation of the active region that obtains the best carrier mobility for the n-type transistor is different from the crystal orientation that obtains the best carrier mobility for the p-type transistor.

[0084] In another embodiment, the single crystalline semiconductor layer is made of a different material.

[0085] For example, for nFET transistors, silicon can be advantageously replaced by strained silicon. For pFET transistors, silicon can be advantageously replaced by silicon germanium. These alternative materials allow increasing the charge-carrier mobility in the channel of the corresponding transistor.

[0086] The selection of the material of the individual semiconductor layers requires only the use of a suitable donor substrate during the fabrication of the double SOI substrate.

[0087] Furthermore, the n-doping or p-doping can be carried out before the individual semiconductor layers are transferred to the carrier substrate, which avoids subsequent implantation of dopants which could damage the device.

[0088] In one embodiment, the two electrically insulating layers are made of the same material, for example silicon oxide (SiO2). The oxide layer is usually obtained by thermal oxidation of a silicon substrate.

[0089] Alternatively, the two electrically insulating layers are made of different materials.

[0090] Therefore, according to one embodiment, the first electrically insulating layer may be made of a so-called "high-k" material, i.e. a material with a high dielectric constant, such as, but not limited to, hafnium oxide or zirconium oxide (in particular HfO2, HfON, HfSiO, HfSiON, ZrO2, HfZrO2 or HfZrO). With respect to silicon oxide, such a material may perform a better etch stop function due to a higher selectivity with respect to the material of the first single-crystalline semiconductor layer.

[0091] According to one embodiment, the second electrically insulating layer can be made of a so-called "low-k" material, i.e. a material with a low dielectric constant, such as, but not limited to, carbon-doped silicon oxide and / or fluorine-doped silicon oxide (in particular SiOC, SiOF, SiOCF, SiOCH), but also a porous oxide or an organic material (for example, polytetrafluoroethylene (PTFE), polyimide, parylene). With respect to the silicon oxide layer, and for given electrical insulating properties, the layer of this material is thinner (the ratio between the thicknesses of the layers of these two materials corresponds to the ratio between their dielectric permittivities). This configuration is particularly advantageous, as mentioned above, since the increase in density while maintaining acceptable transistor electrical properties is limited by the height / width ratio of the fins and the required spacing between the fins. Therefore, for a given height of the fins, the thickness of the second electrically insulating layer (in Figure 1 The reduction of the active area (denoted by e in the figure) is beneficial, and in particular is beneficial for the active area that may have a larger height (h T1 、h T2 ) channel, and therefore has better performance in terms of current. For example, the 20 nm SiO2 layer separating two channels of height 30 nm can be replaced by a 10 nm carbon-doped porous SiO2 layer; the height gain of the two channels is therefore 10 nm in total, i.e., the height of each channel is increased by almost 20%.

[0092] Depending on the characteristics of the device and the performance sought, a person skilled in the art may freely combine the various material choices described above with respect to the electrically insulating layer and the single-crystalline semiconductor layer.

[0093] Another advantage of the double SOI substrate is that the carrier substrate itself can be functionalized. In other words, the carrier substrate not only performs the mechanical carrier function of the transistor, but can include one or more layers that play a specific role in the operation of the device, or include one or more electronic components that allow the device to perform multiple functions in a system-on-chip device. This functionalization of the carrier substrate can be achieved during the manufacture of the double SOI substrate or in particular before the manufacture of the double SOI substrate by selecting the carrier substrate.

[0094] For example, the carrier substrate may include a layer for trapping charges, which layer may take the form of a polysilicon layer. Such a layer is particularly useful for the operation of radiofrequency devices, which can therefore be combined with CFET devices, allowing the integration of components intended for logic and computing and radiofrequency (RF) components required to manage connectivity into the same chip. Such a layer, containing many electron traps, limits self-bias and crosstalk between transistors via the substrate (caused by the strong electromagnetic radiation of radiofrequency transistors). This layer allows reducing this interference by trapping charges. In this precise case, double SOI is needed, since an electrically insulating layer must be placed between the trapping substrate layer and the useful layer.

[0095] According to another example, which can be optionally combined with the previous example, the carrier substrate can include a layer with a specific quality, for example, a silicon layer without defects called COP (crystal originated pits). The layer can be a CZ (Czochralski) layer or an epitaxial semiconductor layer of the qualified COP-free type in the literature (see page 27 of the work Silicon-on-Insulator Technology and Devices XI, Electrochemical Society Proceedings, Volume 2003-05), which can be optionally doped.

[0096] Such a layer allows in particular the integration of e-DRAM (embedded dynamic random access memory). Embedded DRAM memory allows a significant reduction in the latency between local memory and system memory (by a factor of about 3) by (partially) integrating the system memory directly into the chip instead of into a separate module. For this reason, embedded DRAM memory also replaces part of the static memory (so-called SRAM). The manufacture of embedded DRAM memory next to the logic circuits consists in burying the capacitors that produce the memory effect in the substrate. The layer in which the capacitors are manufactured must be doped.

[0097] Figure 1 is a schematic cross-sectional view of a CFET device according to one embodiment of the present invention.

[0098] The device comprises a carrier substrate 1. The carrier substrate may be made of bulk silicon or any other material capable of serving as a mechanical carrier for the device.

[0099] The carrier substrate 1 is covered by a first electrically insulating layer 2a. Advantageously, said layer 2a serves as an etch stop layer during the formation of the fins F and therefore extends over substantially the entire surface of the carrier substrate 1. However, it is not excluded that the layer 2a has partially or completely removed the material of the layer 2a from between the two fins. The layer 2a may be made of silicon oxide or another electrically insulating material, in particular chosen according to its selectivity with respect to etching. Thus, the layer 2a may advantageously be a high-k dielectric.

[0100] The fin F includes a single-crystalline semiconductor layer 2b on the first electrically insulating layer 2a, forming a channel of the first transistor. The height h of the channel is T1 is equal to the thickness of layer 2b. Layer 2b is, for example, p-doped, and preferably weakly p-doped. Layer 2b may be made of silicon or another semiconductor which may in particular be chosen to maximize the charge-carrier mobility in said layer. Thus, if the transistor is of p-type, layer 2b may advantageously be made of silicon germanium.

[0101] The fin comprises a second electrically insulating layer 3a on the first semiconductor layer 2b. The layer 3a may be made of silicon oxide or another electrically insulating material, which is in particular chosen to have a low dielectric constant, thereby allowing the thickness of the layer 3a to be minimized and, in exchange, the height of the channels of the two transistors to be maximized. Thus, the layer 3a may advantageously be a low-k dielectric, for example, carbon-doped porous SiO2.

[0102] Finally, the fin comprises, on the second electrically insulating layer 3a, a second single-crystalline semiconductor layer 3b forming a channel of the first transistor. The height h of the channel is T2 is equal to the thickness of layer 3b. Layer 3b is for example n-doped, and preferably weakly n-doped. Layer 3b may be made of silicon or another semiconductor which may in particular be chosen so as to maximize the charge-carrier mobility in said layer. Thus, if the transistor is of n-type, layer 3b may advantageously be made of strained silicon.

[0103] Figure 2 is a schematic cross-sectional view of a CFET device according to one embodiment of the present invention.

[0104] Relative to Figure 1 , Figure 2 The CFET device further comprises a functional layer contained in a carrier substrate. Thus, the carrier substrate 1 comprises a base substrate 1a, for example made of bulk silicon or any other material capable of serving as a mechanical carrier for the device, and a functional layer 1b arranged between the base substrate 1a and the first electrically insulating layer 2a.

[0105] The functional layer 1b may in particular be:

[0106] - a polysilicon layer, which performs a charge trapping function, in particular in radio frequency devices;

[0107] - so-called COP-free single-crystal silicon layers, i.e. layers without or with a very low density of cavities in the crystal lattice;

[0108] - an epitaxial semiconductor layer, which may optionally be doped (eg carbon-doped Si, phosphorus-doped Si, boron-doped Si or even SiGe).

[0109] For the sake of simplicity of the drawing, a single fin F is shown, but it goes without saying that a CFET device in principle comprises a large number of fins extending parallel to each other from a carrier substrate.

[0110] FIG. 3A to FIG. 3F The various steps of a method for manufacturing a double SOI substrate suitable for producing the above-mentioned CFET devices are schematically illustrated.

[0111] Via SmartCut TM The type of double-layer transfer to fabricate this dual SOI substrate must meet certain technical constraints specific to CFET device production.

[0112] In particular, the etching of the trenches in the double SOI substrate that allow the definition of the various fins must be carried out in a single step in order to ensure the alignment of the devices and their spacing. In practice, this etching can be carried out to a depth of no more than 90 nm (for example, a thickness between 60 nm and 90 nm).

[0113] Furthermore, in order to maximize the amount of current while trying to maximize the thickness of the n-channel and p-channel, the thickness of the single crystal semiconductor layers 2b and 3b must typically be about 25nm to 40nm, with the thickness of the electrically insulating layer 3a in between the layers (for its part) being between 10nm and 30nm.

[0114] Therefore, the thinness of these layers requires the layer transfer process to meet specific constraints in order to ensure that the defects are compatible with the expected performance of the CFET device.

[0115] In particular, the thin thickness of the electrically insulating layer 3a requires that the surface of the layer to which it must be bonded (i.e., the first single crystal semiconductor layer 2b) has a roughness of less than 0.1 nm RMS (RMS is the abbreviation for root mean square) and a density of defects of size 50 nm that is as low as possible.

[0116] Furthermore, the variation in thickness of the individual single-crystalline semiconductor layers intended to form an n-channel or p-channel must be extremely small, about ±1.5 nm relative to the target thickness. Such small variability cannot be achieved by means of chemical mechanical polishing (CMP) processes such as those commonly used to polish semiconductor surfaces, especially in SmartCut. TM used as acceptor substrate in the method.

[0117] In order to solve these difficulties, it has been proposed to implement in the first layer transfer step a method conventionally used for forming FDSOI substrates (FDSOI is an abbreviation for fully depleted SOI) which includes a high-temperature thermal treatment which smoothes the surface of the transferred layer to achieve the desired roughness. This roughness is equivalent to that obtained with chemical mechanical polishing, but allows the desired variability in the thickness of the transferred layer.

[0118] The reader is particularly referred to the article by W. Schwarzenbach et al. (ECS Trans. 53, p. 39 (2013)) for a graph of the power spectral density (PSD) as a function of the spatial frequency of the defect for an area of ​​30 μm x 30 μm.

[0119] However, relative to the known method for forming a planar FDSOI substrate, in this option, removing the step-by-step cleaning process usually included in the method for manufacturing the FDSOI substrate may be advantageous, and it has been described in the reference of W. Schwarzenbach et al. (IEEE ICICDT proceeding, 2011) that, assuming that the thickness variability required for the CFET device is higher than the variability sought in the planar FDSOI substrate (about ±0.5 nm relative to the target thickness), the step-by-step cleaning process seems to be redundant. Removing this cleaning step allows the cost of the manufacturing method to be minimized while retaining the required quality of the first semiconductor layer 2b.

[0120] Regarding the second layer transfer step, it may be performed under the same conditions as the first step, or a method for forming a PDSOI substrate may be employed as it is (PDSOI is an abbreviation of partially-depleted SOI).

[0121] According to a first option, the applicant has demonstrated, using the physical method described in the article by O. Kononchuck et al. (Solid State Phenomena, vol 131-133, pp 113-118, 2008), that a long-range smoothing heat treatment does not lead to oxide dissolution of the electrically insulating layer 2a.

[0122] FIG. 3A to FIG. 3C The first layer transfer step is schematically illustrated.

[0123] Reference Figure 3A , a first single crystalline semiconductor donor substrate 20 is provided, in which a weakened zone 21 is formed, the weakened zone 21 being intended to define therein a first thin surface layer of a layer 2b intended to form a CFET device.

[0124] As is known per se, the weakened zone may be formed by implanting atomic species such as hydrogen and / or helium at a defined depth in the donor substrate 20 .

[0125] Advantageously, the donor substrate 20 may have been previously covered with an electrically insulating layer intended to form at least some of the layers 2a of the CFET device.

[0126] Reference Figure 3B , the first donor substrate 20 is bonded to the carrier substrate 1 with the first electrical insulating layer 2a at the bonding interface. Figure 3B It is not illustrated in the figure, but the carrier substrate may be covered with an electrically insulating layer intended to form at least some of the layers 2a of the CFET device in combination with an electrically insulating layer optionally present at the surface of the first donor substrate 20 .

[0127] Reference Figure 3C , the first donor substrate 20 is separated along the weakened area 21, thereby transferring the layer 2b to the carrier substrate.

[0128] As described above, a treatment for finishing the transferred layer 2b is carried out on the first SOI substrate thus formed, in order to repair or remove the defects associated with the separation step and to give said layer the desired final roughness and thickness characteristics. Such a treatment comprises in particular a heat treatment at a high temperature, typically between 1000° C. and 1200° C., and for a relatively long time, typically between 10 and 120 minutes. This heat treatment has the effect of smoothing the surface until a roughness of less than 0.1 nm RMS is achieved.

[0129] Figures 3D to 3F The second layer transfer step is schematically illustrated.

[0130] Reference Figure 3D, a second single crystal semiconductor donor substrate 30 is provided, in which a weakened zone 31 is formed, intended to define therein a first thin surface layer of layer 3b intended to form a CFET device. Although the second donor substrate has been labeled with a different reference numeral than the first donor substrate 20, this may be a problem of the same substrate, which has been processed after separation in order to remove implantation-related defects. However, advantageously, the materials of the first and second donor substrates (e.g. in terms of composition, crystal orientation, doping and / or strain) are different and are selected according to the properties of the channel they are intended to form.

[0131] As is known per se, the weakened zone may be formed by implanting atomic species such as hydrogen and / or helium at a defined depth in the donor substrate 30 .

[0132] Advantageously, the donor substrate 30 may have been previously covered with an electrically insulating layer intended to form at least some of the layers 3a of the CFET device.

[0133] Reference Figure 3E , the first donor substrate 30 is bonded to the SOI substrate obtained at the end of the first layer transfer step, with the first electrically insulating layer 3a at the bonding interface.

[0134] Reference Figure 3F , the second donor substrate 30 is separated along the weakened area 31, thereby transferring the layer 2b to the SOI substrate.

[0135] As described above, according to one embodiment (type of method for manufacturing FDSOI substrates), a treatment of finishing the transferred layer 3b is carried out on the double SOI substrate thus formed, in order to repair or remove defects related to the separation step and to give the layer the desired final roughness and thickness characteristics. Such a treatment notably comprises a heat treatment at a high temperature, typically between 1000° C. and 1200° C., and for a relatively long time, typically between 10 and 120 minutes. This heat treatment has the effect of smoothing the surface until a roughness of less than 0.1 nm RMS is achieved.

[0136] According to another embodiment (type of method for manufacturing a PDSOI substrate), a treatment of finishing the transferred layer 3b is carried out on the double SOI substrate thus formed, in order to repair or remove defects related to the separation step and to give the layer the desired final roughness and thickness characteristics. Such treatments include in particular heat treatments at high temperatures, generally between 1100° C. and 1250° C., and for relatively short periods of time, generally less than one minute. These heat treatments have the effect of smoothing the surface until a roughness of less than 0.5 nm RMS is achieved.

[0137] Next, trenches are formed in the double SOI substrate by etching grooves down to the first electrically insulating layer 2a to define one or more fins, such as Figure 1 During this etching, layer 2a advantageously acts as an etch stop layer.

[0138] In some implementations, such as Figure 2 As shown, it may be advantageous to include a functional layer 1 b in the carrier substrate 1 .

[0139] In this case, the thermal budget achieved in the dual SOI substrate fabrication may be critical. Specifically, if the functional layer 1b includes polysilicon, applying a high temperature heat treatment to smooth the semiconductor layer 2b may result in recrystallization of the polysilicon of layer 1b, causing it to lose all or part of its charge trapping properties. In another example, if the functional layer 1b is doped, applying a high temperature heat treatment to smooth the semiconductor layer 2b may result in diffusion of dopants within the SOI substrate, thereby preventing the integration of e-DRAM memory.

[0140] In this case, it is advantageous to form layer 2b using a layer transfer process which allows very low roughness and very low defects to be obtained with a limited thermal budget. Such a process can be achieved under the following conditions: the donor substrate 20 will preferably carry two layers of material, one layer serving as a carrier for the selective etching process and the second layer forming layer 2b. The two layers can advantageously be produced by epitaxy. The weakened zone can be formed by implanting atomic substances such as hydrogen and / or helium at a defined depth strictly greater than the thickness of the above two layers. Advantageously, the donor substrate 20 can be previously covered with an electrically insulating layer intended to form at least some of the layers 2a of the CFET device.

[0141] Reference Figure 3B , the first donor substrate 20 is bonded to the carrier substrate 1 with the first electrical insulating layer 2a at the bonding interface. Figure 3B It is not illustrated in the figure, but the carrier substrate may be covered with an electrically insulating layer intended to form at least some of the layers 2a of the CFET device in combination with an electrically insulating layer optionally present at the surface of the first donor substrate 20 .

[0142] Reference Figure 3C , the first donor substrate 20 is separated along the weakened area 21, thereby transferring the layer 2b to the carrier substrate.

[0143] A finishing treatment is then carried out on the first SOI substrate thus formed, comprising a selective etching which stops on each of the two layers previously produced. Such a finishing treatment does not include any treatment at a temperature higher than 500° C. It allows to achieve a surface with a roughness of less than 0.1 nm RMS at its ends.

[0144] With regard to the layer 3b transferred in the second layer transfer step, the same constraints regarding the thermal budget apply (however, as described above), the PDSOI method is sufficient to obtain the required quality of the layer 3b using a thermal treatment that does not degrade the properties of the functional layer 1b.

[0145] In the case where layer 2b is a silicon germanium layer (especially in the case where this layer is intended to form the channel of a p-type transistor), it may be advantageous to form said SiGe layer by epitaxy on an SOI substrate. In particular, a 30nm epitaxial SiGe layer with a thickness variability of about 3% allows the variability criteria of CFET devices to be met. Such a silicon germanium on insulator (SiGeOI) substrate produced by epitaxy on an SOI substrate can be used as an acceptor substrate in a second layer transfer step. This second layer transfer step can advantageously be designed to transfer the strained silicon layer 3b (intended to form the channel of an n-type transistor) to the SiGeOI substrate.

[0146] According to one embodiment, the second donor substrate may comprise a SiGe seed layer and an epitaxial Si layer formed on the seed layer, the SiGe imposing its lattice parameter during the growth of the silicon, thereby generating strain in said silicon. Next, in a manner known per se, a weakened zone intended to define the layer to be transferred 3 b is formed in the silicon germanium layer, and the second donor substrate is then bonded to the SiGeOI substrate via an electrically insulating layer 3 a. The electrically insulating layer may in particular have been formed on the strained silicon before the implantation intended to form the weakened zone.

[0147] According to one embodiment, the second donor substrate can be made of unstrained silicon. In a manner known per se, a weakened zone is formed in the silicon intended to define the layer to be transferred 3b, and the second donor substrate is then bonded to the SiGeOI substrate through the electrically insulating layer 3a. The electrically insulating layer may have been formed on the second donor substrate, in particular, before the implantation intended to form the weakened zone. The formation of the grooves intended to separate the fins also has the effect of transferring at least some of the strain of the SiGe layer 2b (which usually has a progressive strain due to its epitaxial formation on the SOI substrate) to the silicon layer 3b. In the CFET device thus obtained, the SiGe layer 2b is then relaxed, while the silicon layer 3b is strained.

[0148] References

[0149] W.Schwarzenbach et al,Atomic Scale Thickness Control of SOI Wafers for Fully Depleted Applications,ECS Trans.53,p.39(2013)

[0150] W.Schwarzenbach et al,Excellent Silicon Thickness Uniformity Ultra-Thin SOI for controlling Vt variation of FDSOI,IEEE ICICDT proceeding,2011

[0151] O.Kononchuck et al,Internal Dissolution of Buried Oxide in SOIWafers,Solid State Phenomena,vol 131-133,pp 113-118,2008

Claims

1. A method for manufacturing a CFET device, characterized in that: The method comprises the following steps: - forming a double semiconductor-on-insulator substrate, the double semiconductor-on-insulator substrate comprising, from its base to its surface, in order: a carrier substrate (1), a first electrical insulating layer (2a), a first single crystal semiconductor layer (2b), a second electrical insulating layer (3a) with a thickness between 10 nm and 30 nm, and a second single crystal semiconductor layer (3b); - forming a trench from the surface of the substrate to the first electrically insulating layer (2a) to form at least one fin (F), - in each fin (F), a channel of a first transistor is formed in the first single crystal semiconductor layer (2b), and a channel of a second transistor of a type opposite to that of the first transistor is formed in the second single crystal semiconductor layer (3b), The steps of forming the double semiconductor-on-insulator substrate include: - a first layer transfer step, the first layer transfer step comprising: implanting atomic substances into a first donor substrate (20) to form a weakened zone (21), bonding the first donor substrate (20) to the carrier substrate (1), wherein the first electrically insulating layer (2a) is at the bonding interface between the first donor substrate (20) and the carrier substrate (1), and separating the first donor substrate (20) along the weakened zone (21) so as to transfer the first electrically insulating layer (2a) and the first single crystal semiconductor layer (2b) to the carrier substrate (1), thereby forming a first semiconductor-on-insulator substrate, the first layer transfer step further comprising performing a heat treatment at a sufficiently high temperature to smooth the first single crystal semiconductor layer to a roughness of less than 0.1 nmRMS, - a second layer transfer step after the heat treatment to transfer the second electrically insulating layer (3a) and the second single-crystalline semiconductor layer (3b) to the first single-crystalline semiconductor layer on the first semiconductor-on-insulator substrate.

2. The method according to claim 1, wherein: The trench is formed by etching, and the first electrical insulating layer (2a) forms a stop layer for the etching.

3. The method according to claim 1 or 2, wherein: The thickness of the first single crystal semiconductor layer (2b) and the second single crystal semiconductor layer (3b) is between 25 nm and 40 nm.

4. The method according to claim 1 or 2, wherein: The first single crystal semiconductor layer (2b) and the second single crystal semiconductor layer (3b) are made of opposite types of silicon doping.

5. The method according to claim 1 or 2, wherein: The first single crystal semiconductor layer (2b) and the second single crystal semiconductor layer (3b) are made of silicon having different crystal orientations.

6. The method according to claim 1 or 2, wherein: The first single crystal semiconductor layer (2b) and the second single crystal semiconductor layer (3b) are made of different materials.

7. The method according to claim 1 or 2, wherein: The semiconductor layer forming the channel of the n-type transistor is made of strained silicon.

8. The method according to claim 1 or 2, wherein: The semiconductor layer forming the channel of the p-type transistor is made of silicon germanium.

9. The method according to claim 1 or 2, wherein: The first electrically insulating layer (2a) and / or the second electrically insulating layer (3a) are made of silicon oxide (SiO2).

10. The method according to claim 1 or 2, wherein: The first electrically insulating layer (2a) and the second electrically insulating layer (3a) are made of different materials.

11. The method according to claim 1 or 2, wherein: The first electrical insulating layer (2a) is made of a high-k material.

12. The method according to claim 1 or 2, wherein: The second electrical insulating layer (3a) is made of a low-k material.

13. The method according to claim 1 or 2, wherein: The method comprises growing a semiconductor layer on the carrier substrate (1) by epitaxy.

14. The method according to claim 1 or 2, wherein: The carrier substrate (1) comprises at least one COP-free CZ silicon layer.

15. The method according to claim 1 or 2, wherein: The smoothing heat treatment of the first single crystal semiconductor layer (2b) is performed at a temperature between 1000°C and 1200°C for a time between 10 minutes and 120 minutes.

16. The method according to claim 1 or 2, further comprising performing a heat treatment at a temperature between 1100°C and 1250°C for a time shorter than one minute, the heat treatment being used to finish the second single crystal semiconductor layer (3b).