Temperature Sensor
By designing a specific cross-sectional structure of the solder leg in the temperature sensor, the maximum length in the width direction of the solder leg is the maximum width of the solder leg A, and the boundary width B ≤ A, which solves the problem of heat dissipation in the solder leg and improves the response of temperature measurement. performance and precision, achieving higher durability.
Patent Information
- Application Number
- CN201980069796.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2019-10-14
- Publication Date
- 2024-10-29
- Estimated Expiration
- 2039-10-14
AI Technical Summary
In existing temperature sensors, the design of the solder legs causes heat dissipation from the electrode wires to the joints, affecting the accuracy and responsiveness of temperature measurement.
Design a temperature sensor whose soldering leg has a specific cross-section in the direction orthogonal to the sensor axis. The maximum length in the width direction of the soldering leg is the maximum width of the soldering leg A. The boundary width B ≤ A. The width of the soldering leg is The shape reduces the root area of the solder leg and suppresses heat dissipation.
It effectively suppresses the heat dissipation of the welding leg, improves the responsiveness and accuracy of temperature measurement, and improves the durability of the temperature sensor.
Smart Images

Figure CN112912703B_ABST
Abstract
Description
[0001] Cross-reference to related applications
[0002] This application is based on Japanese application No. 2018-198079 filed on October 22, 2018, and the contents thereof are cited herein. Technical Field
[0003] The present disclosure relates to temperature sensors. Background Art
[0004] Patent document 1 discloses a temperature sensor for measuring the temperature of exhaust gas of an engine. The temperature sensor described in patent document 1 is disclosed as comprising: a temperature sensor element such as a thermistor for detecting the temperature of the exhaust gas; a pair of electrode wires extending from the temperature sensor element; and a terminal metal fitting for relaying the pair of electrode wires and a pair of lead wires for external output.
[0005] In the temperature sensor described in Patent Document 1, the electrode wire and the terminal metal fitting overlap in a direction perpendicular to the sensor axis and are connected to each other by brazing. Figure 4 As can be seen from the figures, a weld leg portion formed when the electrode wire and the terminal metal fitting are brazed is arranged on the side surface of the electrode wire.
[0006] Prior art literature
[0007] Patent Literature
[0008] Patent Document 1: Japanese Patent Application Publication No. 2011-127938 Summary of the invention
[0009] In the temperature sensor described in Patent Document 1, the weld leg has an end extension shape that becomes wider toward the terminal metal fitting side in the overlapping direction of the electrode wire and the terminal metal fitting. Therefore, the contact area between the weld leg and the terminal metal fitting is large, and the heat of the temperature sensor element is easily dissipated from the electrode wire to the terminal through the weld leg.
[0010] The present disclosure intends to provide a temperature sensor capable of suppressing heat dissipation from an element electrode line to a joint via a solder fillet.
[0011] One aspect of the present disclosure is a temperature sensor comprising:
[0012] Thermistors for detecting temperature;
[0013] a pair of element electrode wires connected to the thermal element; and
[0014] A pair of connectors respectively connected to a pair of element electrode wires,
[0015] The element electrode line has an overlapping line portion, and the overlapping line portion is connected to the connector so as to overlap with the connector in an overlapping direction orthogonal to the sensor axial direction.
[0016] A solder leg portion is disposed on the side of the overlapped line portion, the solder leg portion having a pair of solder leg pieces formed in a manner rising from a main surface, that is, a specific main surface, on the overlapped line portion side of the joint,
[0017] When a direction orthogonal to both the sensor axial direction and the overlapping direction is set as a width direction, and in a cross section passing through the weld leg portion and orthogonal to the sensor axial direction, a maximum length of the weld leg portion in the width direction is set as a weld leg maximum width A, and a length of a pair of boundary portions between a pair of weld leg pieces and the specific main surface in the width direction is set as a boundary width B,
[0018] As a cross section orthogonal to the sensor axial direction passing through the weld foot portion, at least a portion in the sensor axial direction has a specific cross section satisfying B≤A.
[0019] The temperature sensor of the above-described method has a specific cross-section that satisfies B≤A as a cross-section passing through the solder leg and orthogonal to the sensor axial direction, at least in a portion of the sensor axial direction. Therefore, the area of the root portion of the solder leg that is orthogonal to the overlapping direction can be reduced. As a result, heat dissipation from the element electrode line to the joint via the solder leg can be suppressed.
[0020] As described above, according to the above aspect, it is possible to provide a temperature sensor capable of suppressing heat dissipation from the element electrode wire to the joint via the fillet portion. BRIEF DESCRIPTION OF THE DRAWINGS
[0021] The above-mentioned and other objects, features and advantages of the present disclosure will become more apparent through the following detailed description with reference to the accompanying drawings.
[0022] Figure 1 is a front view showing a portion of the temperature sensor in Embodiment 1 cut away.
[0023] Figure 2 is an enlarged front view of the periphery of the solder leg portion of the temperature sensor in the first embodiment,
[0024] Figure 3 FIG. 1 is an enlarged side view of the periphery of the solder leg portion of the temperature sensor in Embodiment 1.
[0025] Figure 4 yes Figure 2 The cross-sectional view along the IV-IV line,
[0026] Figure 5 is an enlarged cross-sectional view of the periphery of the solder fillet of the temperature sensor for explaining the thickness of the solder fillet in the first embodiment.
[0027] Figure 6 is a graph used to show the comparison method and is similar to Figure 4 The cross-sectional diagram corresponding to the cross-section of
[0028] Figure 7 This is a graph showing the relationship between B / C and 63% response time in Experimental Example 3. DETAILED DESCRIPTION
[0029] (Implementation Method 1)
[0030] use Figure 1 to Figure 5 , an implementation method of the temperature sensor is described.
[0031] The temperature sensor 1 of this embodiment is as follows Figure 1 As shown, the thermosensitive element 2 for detecting temperature, a pair of element electrode wires 3 connected to the thermosensitive element 2 , and a pair of connectors 4 respectively connected to the pair of element electrode wires 3 are provided.
[0032] like Figure 1 to Figure 4 As shown, the element electrode wire 3 has an overlapping wire portion 31. The overlapping wire portion 31 is connected to the connector 4 so as to overlap with the connector 4 in the overlapping direction Z that is orthogonal to the sensor axial direction X. In addition, the sensor axial direction X is the direction in which the central axis of the temperature sensor 1 extends. In addition, the direction orthogonal to both the sensor axial direction X and the overlapping direction Z is referred to as the width direction Y.
[0033] like Figure 4 As shown, the solder fillet portion 5 is arranged on the side surfaces 311 on both sides of the overlap line portion 31 in the width direction Y. The solder fillet portion 5 has a pair of solder fillet pieces 51 formed to rise from the main surface on the overlap line portion 31 side of the joint 4, that is, the specific main surface 411.
[0034] Here, in the cross section of the temperature sensor 1 passing through the weld leg portion 5 and orthogonal to the sensor axial direction X, the maximum length of the weld leg portion 5 in the width direction Y is defined as the weld leg maximum width A, and the length in the width direction Y between the pair of weld leg pieces 51 and the pair of boundary portions 6 of the specific main surface 411 is defined as the boundary width B. At this time, as the cross section of the temperature sensor 1 passing through the weld leg portion 5 and orthogonal to the sensor axial direction X, at least a portion of the sensor axial direction X has a specific cross section satisfying B≤A. Figure 4 is an example of a specific section.
[0035] Hereinafter, this embodiment will be described in detail.
[0036] Hereinafter, the sensor axial direction X is sometimes referred to as the X direction, the overlapping direction Z is referred to as the Z direction, and the width direction Y is referred to as the Y direction. In addition, in the X direction, the side where the thermosensitive element 2 is arranged relative to the joint 4 is referred to as the X1 side, and the opposite side is referred to as the X2 side. In addition, in the Z direction, the side where the overlapping line portion 31 of the element electrode line 3 is arranged in the joint 4 is referred to as the Z1 side, and the opposite side is referred to as the Z2 side.
[0037] The temperature sensor 1 of this embodiment is installed in a hydrogen tank used in a fuel cell vehicle (so-called FCV), for example. The temperature sensor 1 detects the temperature inside the hydrogen tank when the hydrogen tank is filled with hydrogen. The filling speed of hydrogen into the hydrogen tank is controlled based on the detection result of the temperature inside the hydrogen tank by the temperature sensor 1. In the hydrogen tank, impact and pressure are generated due to the filling of hydrogen, so the temperature sensor 1 is designed to have a strength that can withstand the impact and pressure.
[0038] like Figure 1 As shown, the temperature sensor 1 includes a housing 7 for holding a pair of connectors 4. The housing 7 can be made of resin. For example, the housing 7 can be made of a resin containing 33 wt% glass fiber in a polyamide resin (PA66 resin). By making the housing 7 of resin, it is possible to achieve light weight and low cost. In addition, the housing 7 can also be made of a conductor such as metal as long as the insulation with the connector 4 is ensured.
[0039] The housing 7 can be formed by insert molding in which a pair of joints 4 are arranged in a mold. The housing 7 makes the ends of the pair of joints 4 on the X1 side, that is, the joint protrusions 41, protrude, and holds the pair of joints 4. The housing 7 has a pair of surrounding parts 71 that surround the root parts of the joint protrusions 41 in the pair of joints 4. The surrounding parts 71 have a shape that protrudes from the X1 side end of the housing 7 to the X1 side and decreases in diameter toward the X1 side.
[0040] The pair of terminals 4 are spaced apart from each other and are formed to be long in the X direction. The pair of terminals 4 are electrically connected to an external device on the X2 side and are electrically connected to the element electrode line 3 on the X1 side.
[0041] The joint 4 can be made of stainless steel. For example, the joint 4 can be made of SUS304. The melting point of the joint 4 can be set to be 200° C. or more lower than the melting point of the element electrode wire 3 .
[0042] The pair of joint protrusions 41 protrude from the housing 7 toward the X1 side. The pair of joint protrusions 41 are formed parallel to each other. The pair of joint protrusions 41 are arranged with a gap in the Y direction.
[0043] like Figure 1 to Figure 3 As shown in FIG. 1 , each joint protrusion 41 has a thickness in the Z direction and is formed into a plate shape that is long in the X direction. Figure 2 , Figure 3As shown, corners 412 on both sides of the Y direction of the X1 side end portion of each joint protrusion 41 are chamfered into a tapered shape that becomes more inward of the joint protrusion 41 in the Y direction as it goes toward the X1 side.
[0044] like Figure 2 , Figure 3 As shown, the overlapping line portions 31 of a pair of element electrode lines 3 are overlapped and joined on the main surface on the Z1 side of the pair of joint protrusions 41, that is, the specific main surface 411. The main surface on the Z1 side of the joint protrusion 41 is a surface of the joint protrusion 41 formed on the Z1 side except the surface of the solder leg portion 5, and is a surface adjacent to the surface of the solder leg portion 5.
[0045] The element electrode wire 3 is made of a platinum alloy. The platinum alloy may be based on Pt and contain 20 wt% Ir. Figure 4 As shown in FIG. 1 , the element electrode wire 3 is formed in a circular line shape with a circular cross section. Alternatively, the element electrode wire 3 may be formed in other shapes such as a line shape with a quadrangular cross section.
[0046] like Figure 1 As shown, the X2-side end of the element electrode wire 3 is an overlapped wire portion 31 that overlaps the X2-side end of the tab protrusion 41 in the Z direction. The overlapped wire portion 31 and the tab protrusion 41 are joined by resistance welding.
[0047] like Figure 2 to Figure 4 As shown in FIG. 1 , a plane portion 312 orthogonal to the Z direction is formed on the Z1 side of the overlapped line portion 31. The plane portion 312 is formed by pressing the overlapped line portion 31 with an electrode for resistance welding when the overlapped line portion 31 and the joint protrusion 41 are resistance welded. The plane portion 312 is formed from a portion of the overlapped line portion 31 that is slightly closer to the X2 side than the X1 side edge to the X2 side edge. Figure 1 The plane portion is omitted in the illustration.
[0048] like Figure 4 As shown, the end portion on the Z2 side of the overlapping line portion 31 is buried in the joint 4 in a manner arranged closer to the Z2 side than the pair of boundary portions 6. That is, the position of the end portion on the Z2 side of the overlapping line portion 31 is located closer to the Z2 side than the specific main surface 411. In addition, in the present embodiment, the overlapping line portion 31 is buried in the joint 4 in the entire X direction of the overlapping line portion 31, but it is sufficient as long as at least a part of the region in the X direction of the overlapping line portion 31 is buried in the joint 4.
[0049] like Figure 2 , Figure 4 As shown in FIG. 1 , a solder leg portion 5 composed of a pair of solder leg pieces 51 is formed on both sides of the overlap line portion 31 in the Y direction. The pair of solder leg pieces 51 are formed into substantially the same shape by a manufacturing method described later. The solder leg portion 5 contains the material constituting the joint 4 (i.e., SUS304). Figure 3In FIG. 1 , for convenience, the fillet portion 5 is hatched. The fillet portion 5 is formed in the entire region in the X direction where the overlap line portion 31 is formed.
[0050] like Figure 2 As shown in FIG. 1 , the surface of the solder fillet portion 5 is formed so as to bulge toward the side away from the overlap line portion 31 in the Y direction as it moves toward the center in the X direction. Figure 4 As shown, in a specific cross section, the surface of each solder fillet 51 is formed into an arc shape that bulges toward the side opposite to the overlapping line portion 31 side in the Y direction. In the specific cross section, the approximately central portion in the Z direction of the surface of each solder fillet 51 protrudes most toward the side opposite to the overlapping line portion 31 side in the Y direction, and the end portion on the Z2 side shrinks toward the overlapping line portion 31 side in the Y direction.
[0051] As mentioned above, Figure 4 As shown, as a cross section of the temperature sensor 1 passing through the solder leg portion 5 and perpendicular to the X direction, at least a portion in the X direction has a specific cross section in which the maximum width A of the solder leg and the boundary width B satisfy B ≤ A. The cross section of the temperature sensor 1 passing through the solder leg portion 5 and perpendicular to the X direction exists at countless positions in the X direction, but at least one of the cross sections at the countless positions is a specific cross section.
[0052] At least in a certain section located in a part of the X direction, the boundary width B is smaller than the maximum width A of the weld leg. That is, at least in a certain section located in a part of the X direction, the boundary width B and the maximum width A of the weld leg satisfy the relationship of A>B. Moreover, in a certain section located in the center of the weld leg portion 5 in the X direction, the maximum width A of the weld leg and the boundary width B satisfy A / B≥1.05.
[0053] In addition, if Figure 4 As shown, the solder foot portion 5 includes a pair of solder foot pieces 51, but the maximum width A of the solder foot means the length in the Y direction from the end of the solder foot piece 51 on one side of the Y direction in the solder foot portion 5 to the end of the solder foot piece 51 on the other side of the Y direction in the solder foot portion 5.
[0054] like Figure 5 As shown, at least one of the pair of fillet pieces 51 has a portion having a thickness greater than a thickness T1 of the end portion on the specific main surface 411 side (ie, Z2 side) in at least a specific cross section located in a portion in the X direction.
[0055] Here, the thickness of the fillet 51 on a specific cross section is the length of the fillet 51 in the normal direction of the side surface 311 of the overlap line portion 31. Figure 5In the figure, the thickness of the end portion of the solder fillet 51 on the Z2 side on a specific cross section is indicated by a double-headed arrow T1, and the maximum thickness of the solder fillet 51 is indicated by a double-headed arrow T2. The arrow T1 is formed along the normal direction of the side surface 311 of the overlap line portion 31 in a manner passing through the boundary portion 6. In the present embodiment, each of the pair of solder fillets 51 has a portion having a thickness greater than the thickness of the end portion on the specific main surface 411 side in at least a specific cross section located in a portion of the X direction.
[0056] like Figure 4 As shown, in the cross section of the temperature sensor 1 passing through the solder leg 5 and perpendicular to the X direction, the diameter of the overlapped line portion 31 is set to the electrode wire diameter C. At this time, in a specific cross section located at the center of the solder leg 5 in the X direction, the boundary width B and the electrode wire diameter C satisfy B / C≤6.
[0057] Here, in this embodiment, the overlap line portion 31 has the flat portion 312, so the diameter of the overlap line portion 31 on a specific cross section is not a perfect circle. In this case, the diameter of the overlap line portion 31 on a specific cross section means the diameter of the overlap line portion 31 in the Y direction.
[0058] like Figure 4 As shown, at least in a specific cross section located in a portion of the X direction, the solder leg portion 5 of at least one of the pair of solder leg pieces 51 is formed to the Z1 side from the center 31c in the Z direction of the overlap line portion 31. In the present embodiment, in the specific cross section, each of the pair of solder leg pieces 51 is formed to the Z1 side from the center 31c in the Z direction of the overlap line portion 31.
[0059] like Figure 4 As shown, in the cross section of the temperature sensor 1 passing through the solder leg portion 5 and orthogonal to the X direction, the length of the solder leg portion 5 in the Z direction is set as the solder leg height D. In addition, in the cross section of the temperature sensor 1 passing through the solder leg portion 5 and orthogonal to the X direction, the shortest length in the Z direction between the position of the end portion of the overlap line portion 31 on the Z2 side in the Z direction and the pair of boundary portions 6 is set as the embedding height E. At this time, in a specific cross section located at the center of the solder leg portion 5 in the X direction, the solder leg height D of at least one of the pair of solder leg pieces 51 and the embedding height E satisfy D / E≥2.
[0060] In addition, in the cross-section of the temperature sensor 1 passing through the solder leg portion 5 and being orthogonal to the X direction, when the lengths in the Z direction of a pair of solder leg pieces 51 constituting the solder leg portion 5 are different from each other, the height D of a pair of solder legs means the length in the Z direction of the solder leg piece 51 on the side with the longer length in the Z direction.
[0061] like Figure 1As shown, the ends of the pair of element electrode wires 3 on the X1 side are respectively connected to the thermistor 2. The thermistor 2 is fixed in a state of being clamped by the pair of element electrode wires 3 from both sides in the Y direction. The thermistor 2 is bonded to each of the pair of element electrode wires 3. The thermistor 2 is composed of, for example, a thermistor. In addition, it is not limited to this, and the thermistor 2 may also be composed of a thermocouple or a temperature measuring resistor composed of platinum or the like.
[0062] like Figure 1 As shown, a pair of element electrode wires 3 penetrate the flat plate 11. The flat plate 11 is formed by forming a ceramic material with forsterite as a base material into a cylindrical shape. Although not shown in the figure, the flat plate 11 has a pair of insertion holes formed through in the X direction. The pair of element electrode wires 3 are inserted into the pair of insertion holes.
[0063] like Figure 1 As shown, a glass seal 12 is formed from the flat plate 11 to the X1 side. The glass seal 12 is formed in a substantially hemispherical shape so as to bulge from the X1 side end of the flat plate 11 to the X1 side. The glass seal 12 buries the thermosensitive element 2 inside. The glass seal 12 is made of an insulating glass material. The glass seal 12 can be made of, for example, borosilicate glass to which boron oxide is added.
[0064] like Figure 1 As shown, a cover 13 covering the thermistor 2 is mounted on the housing 7. The cover 13 is joined to the housing 7 over the entire circumference of the X2 side end. The cover 13 can be made of resin. For example, the cover 13 can be made of a resin containing 33 wt% glass fiber in a polyamide resin (PA66 resin) like the housing 7. A plurality of through holes 131 are formed in the wall of the cover 13. When the temperature sensor 1 is used, the gas (hydrogen in this embodiment) of the temperature measurement object of the temperature sensor 1 is introduced into the vicinity of the thermistor 2 in the cover 13 through the through holes 131.
[0065] Next, an example of a method of resistance welding the overlap wire portion 31 and the joint protruding portion 41 will be described.
[0066] First, the overlapping line portion 31 of the element electrode line 3 is arranged on the surface on the Z1 side of the joint protrusion 41. In this state, the solder fillet 5 is not formed on the surface on the Z1 side of the joint protrusion 41, and the surface on the Z1 side of the joint protrusion 41 is formed into a plane orthogonal to the Z direction.
[0067] Next, a pair of electrodes for resistance welding are arranged on both sides of the overlapping wire portion 31 and the joint protrusion 41 in the Z direction. Then, the overlapping wire portion 31 and the joint protrusion 41 are clamped by the pair of electrodes and pressurized, and a current is passed between the pair of electrodes to perform a melting process to melt the contact portion of the joint protrusion 41 with the overlapping wire portion 31 and its surroundings.
[0068] In the melting process, the contact portion of the overlapping wire portion 31 in the joint protrusion 41 melts, and under the pressure of the pair of electrodes, the overlapping wire portion 31 is slightly embedded in the joint protrusion 41. In addition, at the same time, the molten portion of the joint protrusion 41 rises toward the Z1 side along the side surface 311 of the overlapping wire portion 31, and becomes the shape of the weld leg portion 5. Next, the conduction between the pair of electrodes is stopped, and the molten portion of the joint protrusion 41 is solidified, thereby forming the weld leg portion 5.
[0069] Here, in the melting process, if the temperature of the melting portion of the joint protrusion 41 becomes excessively high, the fluidity (wettability) of the melting portion becomes high, so that the melting portion is difficult to climb up the side surface 311 of the overlap line portion 31. Therefore, the melting portion does not become the shape of the weld leg portion 5 of this embodiment, but becomes Figure 6 As shown, the fillet portion 9 has a terminal expansion shape in which the width in the Y direction becomes wider toward the Z2 side.
[0070] Therefore, in the melting process, in order to prevent the temperature of the melting part of the joint protrusion 41 from being excessively high and the fluidity (wettability) of the melting part from being increased, the current flowing between the pair of electrodes is set to be low. As a result, the melting part easily rises on the side surface 311 of the overlap line portion 31, and the shape of the weld leg portion 5 of this embodiment can be formed.
[0071] Furthermore, even if the molten portion is temporarily formed into the shape of the weld leg portion 5 of the present embodiment, if the melting process time (i.e., the time for the current to flow between the pair of electrodes) is too long, the shape of the molten portion will collapse from the shape of the weld leg portion 5 of the present embodiment and become Figure 6 The aforementioned terminal extension shape of the weld leg 9 is shown. Therefore, the time of the melting process is set to a short time so that the shape of the molten portion formed into the shape of the weld leg 5 of this embodiment does not collapse. As described above, the overlap line portion 31 and the joint protrusion 41 are resistance welded.
[0072] Next, the effects of this embodiment will be described.
[0073] The temperature sensor 1 of this embodiment has a specific cross section that satisfies B≤A at least in a portion of the X direction as a cross section passing through the solder leg 5 and perpendicular to the X direction. Therefore, the area perpendicular to the Z direction of the root portion of the solder leg 5 can be reduced. As a result, heat dissipation from the element electrode wire 3 to the joint 4 via the solder leg 5 can be suppressed. As a result, the responsiveness of temperature measurement in the temperature sensor 1 and the accuracy of temperature measurement can be improved.
[0074] In addition, in a specific cross section located in the center of the weld leg portion 5 in the X direction, the weld leg maximum width A and the boundary width B satisfy A / B ≥ 1.05. As a result, the overlap line portion 31 is unlikely to peel off from the weld leg portion 5, and a temperature sensor 1 with high durability can be obtained. In addition, the above-mentioned numerical values are confirmed by the experimental examples described later.
[0075] In addition, in a specific cross section located at the center of the solder leg portion 5 in the X direction, the boundary width B and the electrode wire diameter C satisfy B / C ≤ 6. Therefore, it is possible to suppress heat dissipation from the element electrode wire 3 to the joint 4 via the solder leg portion 5, and it is possible to achieve an improvement in the responsiveness of temperature measurement in the temperature sensor 1 and an improvement in the accuracy of temperature measurement. In addition, the above-mentioned numerical values are verified by the experimental examples described later.
[0076] In addition, at least in a specific cross section located in a part of the X direction, the solder fillet 51 of at least one of the pair of solder fillets 51 is formed to the Z1 side from the center 31c in the Z direction of the overlapping line portion 31 of the element electrode line 3. That is, the side surface 311 of the overlapping line portion 31 is covered by the solder fillet 5 in a large range. Therefore, the overlapping line portion 31 is difficult to peel off from the solder fillet 5.
[0077] In addition, the end portion of the overlap line portion 31 on the Z2 side is embedded in the joint 4 so as to be arranged on the Z2 side relative to the boundary portion 6. Moreover, in a specific cross section located at the center of the weld leg portion 5 in the X direction, the weld leg height D and the embedding height E of at least one of the pair of weld leg pieces 51 satisfy D / E≥2. As a result, the overlap line portion 31 is unlikely to peel off from the weld leg portion 5, and a temperature sensor 1 with high durability can be obtained. In addition, the above-mentioned numerical values are verified by the experimental examples described later.
[0078] In addition, at least one of the pair of solder fillets 51 has a portion having a thickness greater than the thickness of the end portion on the Z2 side in at least a certain cross section located in a portion of the X direction. In other words, at least the thickness of the end portion on the Z2 side of at least one of the pair of solder fillets 51 does not constitute the maximum thickness of the solder fillet 51 in a certain cross section located in a portion of the X direction. Therefore, the area of the root portion of the solder fillet 5 orthogonal to the Z direction can be further reduced. As a result, it is easier to suppress heat dissipation from the element electrode line 3 to the joint 4 via the solder fillet 5. As a result, it is possible to achieve an improvement in the responsiveness of temperature measurement in the temperature sensor 1 and an improvement in the accuracy of temperature measurement.
[0079] As described above, according to this aspect, it is possible to provide a temperature sensor capable of suppressing heat dissipation from the element electrode wire to the joint via the fillet portion.
[0080] In addition, among the reference numerals used below, those that are the same as those used in the previously described embodiments indicate the same components as those in the previously described embodiments unless otherwise indicated.
[0081] (Experimental Example 1)
[0082] In this example, an experimental example of evaluating the bonding strength between the element electrode wire 3 and the joint 4 is performed on a plurality of samples in which the ratio of the maximum width A of the fillet to the boundary width B, i.e., A / B, in a central cross section described later is variously changed. The central cross section is a cross section of the temperature sensor 1 that passes through the center of the fillet in the X direction and is orthogonal to the X direction.
[0083] In this example, four samples, samples 1 to 4, were prepared, which had the same basic structure as the temperature sensor 1 of the first embodiment and had different ratios A / B in the central cross section. In the central cross section, the ratio A / B of sample 1 was 0.8, the ratio A / B of sample 2 was 1.0, the ratio A / B of sample 3 was 1.05, and the ratio A / B of sample 4 was 1.2. The ratio A / B in the central cross section of each of samples 1 to 4 was adjusted by changing the pressure applied by a pair of electrodes to the overlapping wire portion 31 and the joint protrusion 41 and the current value flowing between the pair of electrodes in the aforementioned melting process when manufacturing the temperature sensor 1.
[0084] The element electrode wire 3 of each sample is the same as that of the first embodiment, and is composed of a platinum alloy with Pt as the base material and containing 20wt% Ir. The diameter of the element electrode wire 3 of each sample is set to 0.25mm. In addition, the connector 4 of each sample is the same as that of the first embodiment, and is composed of SUS304. The thickness of the connector 4 of each sample is set to 0.6mm as the dimension in the Z direction, and the width is set to 1.5mm as the dimension in the Y direction.
[0085] Next, the test conditions of this example are described.
[0086] In this example, the vibration stress acting on the temperature sensor 1 due to the impact when filling the hydrogen tank with hydrogen is simulated, and the vibration frequency is swept in the frequency band near the primary resonance frequency at an acceleration of 20G to vibrate each sample in the Z direction. The number of vibrations is set to the number of times the temperature sensor 1 vibrates when the vehicle equipped with the temperature sensor 1 repeatedly fills the hydrogen tank with hydrogen for 15 years. In addition, the primary resonance frequency is the primary resonance frequency of the thermistor 2 measured by the laser Doppler vibrometer.
[0087] Next, a method for evaluating the bonding strength between the element electrode wire 3 and the tab 4 will be described.
[0088] In this example, after the test, the sample in which no disconnection occurred between the element electrode line 3 and the joint 4 was evaluated as "OK", and the sample in which disconnection occurred between the element electrode line 3 and the joint 4 was evaluated as "NO".
[0089] Table 1 shows the results.
[0090] [Table 1]
[0091] (Table 1)
[0092]
[0093] According to Table 1, samples 1 and 2 whose ratio A / B on the central section was less than 1 were evaluated as unacceptable. That is, for samples 1 and 2 whose ratio A / B on the central section was less than 1, it was found that a disconnection occurred between the element electrode line 3 and the connector 4. In both samples 1 and 2, after the test, a disconnection was confirmed at the joint between the overlapping line portion 31 of the element electrode line 3 and the connector 4.
[0094] On the other hand, regarding the samples 3 and 4 whose ratio A / B on the central section is 1.05 or more, it can be seen that the evaluation is acceptable. That is, it can be seen that in the specific section located in the center of the weld leg portion 5 in the X direction, the weld leg maximum width A and the boundary width B satisfy A / B ≥ 1.05, so that the overlap line portion 31 is difficult to peel off from the weld leg portion 5, and a temperature sensor 1 with high durability can be obtained.
[0095] (Experimental Example 2)
[0096] This example is an experimental example in which the bonding strength between the element electrode wire 3 and the tab 4 is evaluated for a plurality of samples in which the ratio of the fillet height D to the embedding height E in the central cross section is variously changed, namely, D / E.
[0097] In this example, four samples, samples 5 to 8, were prepared, which had the same basic structure as the temperature sensor 1 of the first embodiment and had different ratios D / E in the central cross section. In the central cross section, the ratio D / E of sample 5 was 1.2, the ratio D / E of sample 6 was 1.8, the ratio D / E of sample 7 was 2.0, and the ratio D / E of sample 8 was 3.0. The ratio D / E of the central cross section in each of samples 1 to 4 was adjusted by changing the pressure applied by the pair of electrodes to the overlapping wire portion 31 and the joint protrusion 41 and the current value flowing between the pair of electrodes in the aforementioned melting process when manufacturing the temperature sensor 1.
[0098] For each sample, the ratio of the maximum width A of the weld leg in the central section to the boundary width B, i.e., A / B, satisfies A / B ≥ 1. Specifically, the A / B of each sample in the central section is set to 1.2. The materials and shapes of the element electrode wire 3 and the connector 4 of each sample are the same as those shown in Experimental Example 1. In addition, the test conditions and the evaluation method of the bonding strength between the element electrode wire 3 and the connector 4 are the same as those in Experimental Example 1.
[0099] Table 2 shows the results.
[0100] (Table 2)
[0101] (Table 2)
[0102]
[0103] According to Table 2, samples 5 and 6, whose ratio D / E on the central section was less than 1.8, were evaluated as unacceptable. That is, for samples 5 and 6, whose ratio D / E on the central section was less than 1.8, it was found that a disconnection occurred between the element electrode line 3 and the connector 4. In both samples 5 and 6, after the test, a disconnection was confirmed at the joint between the overlapping line portion 31 of the element electrode line 3 and the connector 4.
[0104] On the other hand, regarding the samples 7 and 8 whose ratio D / E on the central section is 2.0 or more, it can be seen that the evaluation is acceptable. Therefore, it can be seen that in the specific section located in the center of the weld leg 5 in the X direction, the weld leg height D and the embedding height E satisfy D / E ≥ 2, so that the overlapping line portion 31 is difficult to peel off from the weld leg 5, and a temperature sensor 1 with high durability can be obtained. It is believed that this is because, in the section of the temperature sensor 1 passing through the weld leg 5 and orthogonal to the X direction, the larger the ratio D / E, the more the weld leg 5 is in a state of enclosing the overlapping line portion 31 of the element electrode line 3, and the durability against vibration in the Z direction is improved.
[0105] (Experimental Example 3)
[0106] This example is an experimental example in which the responsiveness of temperature measurement in the temperature sensor 1 was evaluated with respect to a plurality of samples in which the ratio of the boundary width B to the electrode wire diameter C in the central cross section was variously changed, that is, B / C.
[0107] In this example, seven samples were prepared, each having the same basic structure as the temperature sensor 1 of the first embodiment and having different ratios B / C on the central cross section. The B / C ratio of each sample on the central cross section is given by Figure 7 The ratio B / C of the central cross section in the seven samples was adjusted by changing the pressure applied by the pair of electrodes to the overlapped wire portion 31 and the joint protruding portion 41 and the current value flowing between the pair of electrodes in the aforementioned melting step when manufacturing the temperature sensor 1 .
[0108] In the central section of each sample, the ratio of the maximum width A of the solder leg to the boundary width B, i.e., A / B, satisfies A / B ≥ 1.05. Specifically, the A / B of each sample in the central section is set to 1.2. The material and shape of the element electrode line 3 and the connector 4 of each sample are set to be the same as those shown in Experimental Example 1.
[0109] Next, the test conditions of this example are described.
[0110] In this example, the responsiveness of the temperature measurement of the temperature sensor 1 was evaluated by measuring the 63% response time for each sample. Specifically, first, the temperature around the thermistor 2 of each sample was set to 25°C. Then, from this state, the peripheral part of the thermistor 2 of each sample was placed in a gas flow path with a gas temperature of 100° and a flow rate of 10 m / sec, and the 63% response time of each sample was measured. In this example, the 63% change when the temperature change from 25°C to 100°C is set to 100% is (100°C-25°C)×0.63=47.25°C. Therefore, the 63% response time means the time from the temperature of 25°C at the start of the test to 72.25°C obtained by adding 47.25°C to each sample. It can be said that the shorter the 63% response time of the sample, the higher the responsiveness of the temperature measurement in the temperature sensor 1. Figure 7 The vertical axis shows the 63% response time.
[0111] The results are shown in Figure 7 middle.
[0112] according to Figure 7 It can be seen that the 63% response time is shorter in the sample satisfying B / C≤6 in the central section than in the sample satisfying B / C>6 in the central section. Therefore, it can be seen that in the specific section located in the center of the solder leg 5 in the X direction, the boundary width B and the electrode wire diameter C satisfy B / C≤6, so that the responsiveness of the temperature measurement in the temperature sensor 1 becomes higher. It is believed that this is because, in the section of the temperature sensor 1 passing through the solder leg 5 and orthogonal to the X direction, the smaller the boundary width B is relative to the electrode wire diameter C, the smaller the area of the root part of the solder leg 5 orthogonal to the Z direction is, and the heat dissipation from the element electrode wire 3 to the joint 4 through the solder leg 5 can be suppressed.
[0113] In addition, it should be understood that although the present disclosure is described based on the embodiments, the present disclosure is not limited to the embodiments and configurations. The present disclosure also includes various modifications and modifications within the equivalent range. In addition, various combinations and modes, and further other combinations and modes including only one element, more than one element, or less than one element among them are also included in the scope and thought of the present disclosure.
[0114] For example, the joint may also be coated with a coating on the surface. In this case, the coating is also referred to as the joint. The coating may be nickel-plated or the like. In this case, the weld leg is mainly formed by melting the coating and contains the metal constituting the coating. In addition, the weld leg can also ensure strength by solidifying the material of the joint other than the coating with the material of the coating.
Claims
1. A temperature sensor, It is characterized in that have: Thermistor, used to detect temperature; a pair of element electrode wires connected to the thermal element; as well as A pair of connectors are respectively connected to a pair of element electrode wires, The element electrode line has an overlapping line portion, and the overlapping line portion is connected to the connector so as to overlap with the connector in an overlapping direction orthogonal to the sensor axial direction. A solder leg portion is disposed on the side of the overlapped line portion, the solder leg portion having a pair of solder leg pieces formed in a manner rising from a main surface, that is, a specific main surface, on the overlapped line portion side of the joint, When a direction orthogonal to the sensor axial direction and the overlapping direction is set as a width direction, and on a cross section passing through the weld leg portion and orthogonal to the sensor axial direction, a maximum length of the weld leg portion in the width direction is set as a weld leg maximum width A, and a length in the width direction between a pair of boundary portions of the pair of weld leg pieces and the specific main surface is set as a boundary width B, As a cross section passing through the weld leg portion and being orthogonal to the sensor axial direction, at least a portion in the sensor axial direction has a specific cross section satisfying B<A.
2. The temperature sensor according to claim 1, It is characterized in that The section passing through the center of the weld foot portion in the axial direction of the sensor and orthogonal to the axial direction of the sensor is the specific section. In the specific section located at the center of the weld foot portion in the axial direction of the sensor, the maximum width A of the weld foot and the boundary width B satisfy A / B≥1.
05.
3. The temperature sensor according to claim 2, It is characterized in that The section passing through the center of the weld foot portion in the axial direction of the sensor and perpendicular to the axial direction of the sensor is the specific section. On the section passing through the weld foot portion and perpendicular to the axial direction of the sensor, when the diameter of the overlapping line portion is set to the electrode wire diameter C, on the specific section located at the center of the weld foot portion in the axial direction of the sensor, the boundary width B and the electrode wire diameter C satisfy B / C≤6.
4. The temperature sensor according to any one of claims 1 to 3, It is characterized in that At least in the specific cross-section located in a portion of the sensor axial direction, the solder fillet of at least one of the pair of solder fillets is formed to a side farther away from the joint in the overlapping direction than the center of the overlapping direction in the overlapping line portion of the element electrode line.
5. The temperature sensor according to any one of claims 1 to 3, It is characterized in that The section passing through the center of the weld leg portion in the axial direction of the sensor and being orthogonal to the axial direction of the sensor is the specific section. When the joint side relative to the overlapping line portion in the overlapping direction is set as the buried side, the end of the buried side of the overlapping line portion is buried in the joint in a manner that is arranged closer to the buried side than a pair of the boundary portions. On the section passing through the weld leg portion and being orthogonal to the axial direction of the sensor, the length of the weld leg portion in the overlapping direction is set as the weld leg height D, and the position of the end of the buried side of the overlapping line portion and the shortest length in the overlapping direction between a pair of the boundary portions is set as the buried height E. On the specific section located at the center of the weld leg portion in the axial direction of the sensor, the weld leg height D and the buried height E of at least one of the pair of weld leg pieces satisfy D / E≥2.
6. The temperature sensor according to any one of claims 1 to 3, It is characterized in that At least in the specific cross section that is located at a portion in the axial direction of the sensor, at least one of the pair of the solder fillet pieces has a portion having a thickness greater than a thickness of an end portion on the specific main surface side.
Citation Information
Patent Citations
Temperature sensor
JP2011127938A
System and method for directing content to user of social networking engine
JP2018198079A
Temperature sensor