Etch support cleaning using clean substrates with controlled geometry and composition
Solving the problem of nanostructure surface adhesion in lithography devices by using clean substrates with controlled surface coatings to remove contaminants using localized contact and relative motion, enabling in-situ cleaning and avoiding downtime .
Patent Information
- Application Number
- CN201980073815.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Priority Date
- 2019-10-09
- Filing Date
- 2019-10-31
- Publication Date
- 2024-10-11
- Estimated Expiration
- 2039-10-31
AI Technical Summary
In lithography equipment, material transfer on the surface of nanostructures causes adhesion problems, causing the mask to stick and be difficult to unload. The existing technology requires shutdown for wet cleaning and cannot be cleaned in situ.
Using a cleaning substrate with a controlled surface coating, contaminants are removed through local contact and relative motion, and the geometry and material selection of the coating are used to promote the stripping of contaminants and achieve in-situ cleaning.
It achieves rapid and effective removal of contaminants without stopping the operation of the equipment, avoids downtime, and is suitable for cleaning various shapes and surfaces.
Smart Images

Figure CN112955822B_ABST
Abstract
Description
[0001] CROSS-REFERENCE TO RELATED APPLICATIONS
[0002] This application claims priority to (1) U.S. Provisional Patent Application No. 62 / 757,837, filed on November 9, 2018, and (2) U.S. Provisional Patent Application No. 62 / 912,971, filed on October 9, 2019, the entire contents of which are incorporated herein by reference. Technical Field
[0003] The present disclosure relates to cleaning of equipment used to maintain wafers, reticles, masks, etc. in a lithographic apparatus. Background Art
[0004] The lithographic apparatus applies the desired pattern to a substrate such as a wafer of semiconductor material. A patterning device, such as a mask or reticle, can be used to generate the circuit pattern to be formed on a single layer of the wafer. Transfer of the pattern is usually accomplished by imaging onto a layer of radiation-sensitive material (resist) disposed on the substrate. Typically, a single substrate will contain adjacent target portions that are patterned in succession.
[0005] The lithographic apparatus includes a support structure (e.g., a wafer stage) having a working surface configured to hold a wafer using, for example, mechanical, vacuum, electrostatic or other clamping techniques. The support structure includes a spur configured to support a corresponding portion of the wafer. Each spur facing the surface of the wafer includes the formation of patterned bumps, and the patterned bumps have nanometer-scale dimensions. These bumps are referred to herein as nano bumps. The nano bumps define a reduced contact surface area between the wafer and the spurs. The reduced contact surface area mitigates the adhesion effect between the wafer and the spurs, and modifies the friction force during the clamping process.
[0006] The wafer table and its integral burls are usually made of Si:SiC composite ceramic material. The wafer table surface may include about 10,000 burls, each with a diameter of about hundreds of microns and a height of about 100 microns. The burls usually cover about 1% of the surface area of the wafer table.
[0007] When in use, the nanobump working surface may adhere or "stick" to the substrate even when there are nanostructures to avoid such adhesion. One mechanism that promotes adhesion is the material transfer between the working surface (fixture surface) and the previous substrate. This material contamination is left on the working surface in various forms, which are collectively referred to as particles in this article. For example, when the working surface is a mask fixture and the substrate is a mask, the mask fixture may strip chrome from the patterned surface of the mask, resulting in damage to the mask. Because the displaced metal accumulates on the fixture surface, the mask may stick and cannot be unloaded.
[0008] Accumulated contamination can be removed by removing (removing) the work surface from its operating environment and "wet cleaning" the work surface using chemicals to dissolve the contamination. However, it is desirable to avoid these steps and the attendant downtime and to be able to clean the work surface in situ. Summary of the invention
[0009] A simplified summary of one or more embodiments is given below in order to provide a basic understanding of the embodiments. This summary is not an exhaustive overview of all contemplated embodiments and is not intended to identify key or important elements of all embodiments, nor is it intended to limit the scope of any or all embodiments. Its sole purpose is to present some concepts of one or more embodiments in a simplified form as a prelude to a more detailed description presented later.
[0010] According to one aspect of the embodiment, tooling is used to clean the working surface in situ in a controlled manner. The tooling takes the form of a dedicated cleaning substrate having a controlled surface with a partial coating to remove transferred material (metal contamination) from a textured (nano-bump) working surface. The same mechanism that causes contamination (material transfer due to locally higher contact forces) is used in a controlled manner to clean the surface.
[0011] According to another aspect of the embodiment, the cleaning substrate is configured so that there is a limited contact area between the cleaning substrate and the working surface. This allows the use of a cleaning substrate that may stick. Coating thickness and geometry (e.g., the angle of the protrusion caused by the coating geometry) can be selected to promote stripping action, rather than orthogonal pulling. The geometry of the surface to be cleaned (e.g., the high local contact load on the nano-bump peak) can be used to force contaminants to pass through the surface coating, thereby exposing bulk materials that may be beneficial to cleaning, otherwise the bulk materials will not be able to be used, such as, for example, materials (such as copper or gold) that are usually prohibited, materials (such as aluminum and chromium) that produce surface oxides, or non-vacuum compatible materials (such as zinc and cadmium). By limiting the coated area and using different coating materials, the coating can be used to remove contamination.
[0012] The use of a cleaning substrate can result in a faster process that can be performed as a maintenance action (tooling / preventive maintenance) without having to move the work surface out of its operating environment. The geometry of the cleaning surface on the cleaning substrate can be adapted to various shapes and surfaces of the work surface, such as a cleaning wafer with concentric rings.
[0013] Other features and advantages of the present invention and the structure and operation of various embodiments of the present invention will be described in detail below with reference to the accompanying drawings. Note that the present invention is not limited to the specific embodiments described herein. Such embodiments are presented herein for illustrative purposes only. Based on the teachings contained herein, other embodiments will be apparent to those skilled in the relevant art. BRIEF DESCRIPTION OF THE DRAWINGS
[0014] The accompanying drawings, which are incorporated in and constitute a part of this specification, illustrate the present invention and, together with the description, further serve to explain the principles of the invention and enable those skilled in the relevant art to make and use the invention.
[0015] Figure 1 A lithographic apparatus according to an embodiment of the present invention is shown.
[0016] Figure 2 is a not-to-scale drawing of a burl having a top portion with nanoscale topography.
[0017] Figure 3A , 3B 3C is a not-to-scale illustration of the use of a cleaning substrate for removing particles of contaminants from a working surface according to one aspect of an embodiment.
[0018] Figure 4 is a not-to-scale illustration of a process for removing contaminants from a work surface according to one aspect of an embodiment.
[0019] Figure 5 is a not-to-scale illustration of a process for removing contaminants from a work surface according to one aspect of an embodiment.
[0020] Fig. 6A , 6B 6C are diagrams illustrating the operating principle according to one aspect of the embodiment.
[0021] Figure 7 is a flow chart illustrating a process for removing contaminants from a work surface according to one aspect of an embodiment.
[0022] Figure 8 is a flow chart illustrating a process for removing contaminants from a work surface according to one aspect of an embodiment.
[0023] Fig. 9 is a not-to-scale illustration of a cleaning substrate for removing particles of contaminants from a working surface according to one aspect of an embodiment.
[0024] Fig.10 is a not-to-scale illustration of a cleaning substrate for removing particles of contaminants from a working surface according to one aspect of an embodiment.
[0025] Fig.11 is a not-to-scale illustration of a cleaning substrate for removing particles of contaminants from a working surface according to one aspect of an embodiment.
[0026] The features and advantages of the present invention will become more apparent from the following detailed description in conjunction with the accompanying drawings, in which similar reference numerals always identify corresponding elements. In the accompanying drawings, similar reference numerals generally represent identical, functionally similar and / or structurally similar elements. DETAILED DESCRIPTION
[0027] This specification discloses one or more embodiments that incorporate features of the present invention. The disclosed embodiment(s) merely illustrate the present invention. The scope of the present invention is not limited to the disclosed embodiment(s). The present invention is defined by the appended claims.
[0028] The embodiment(s) described in this specification and references to "one embodiment", "embodiment", "example embodiment", etc. in this specification indicate that the embodiment(s) described may include a particular feature, structure, or characteristic, but each embodiment may not necessarily include the particular feature, structure, or characteristic. Moreover, such phrases do not necessarily refer to the same implementation. In addition, when a particular feature, structure, or characteristic is described in conjunction with an embodiment, it can be considered that it is within the cognition of those skilled in the art to implement such feature, structure, or characteristic in conjunction with other embodiments, whether or not explicitly described.
[0029] In the following description and in the claims, the terms "upper", "lower", "top", "bottom", "vertical", "horizontal" and similar terms may be used. These terms are intended only to show relative orientations, not any orientation with respect to gravity. Similarly, terms such as left, right, front, back, etc. are intended only to give relative orientations.
[0030] Before describing the embodiments in further detail, it is helpful to provide an example environment in which embodiments of the invention may be implemented.
[0031] Reference Figure 1 , lithography system 100 includes an illumination system 105. Illumination system 105 includes a light source that generates a pulsed light beam 110 and directs it to a lithography exposure device or scanner 115. Scanner 115 includes a patterning device 116, such as a mask or reticle on a support structure 117. Patterning device 116 carries a pattern that is transferred to beam 110 to create a patterned beam 119 that patterns microelectronic features on a wafer 120. Wafer 120 is placed on a wafer stage 125, which is constructed to hold wafer 120 and is connected to a positioner that is configured to accurately position wafer 120 according to certain parameters.
[0032] The lithography system 100 may use a beam 110 having a wavelength in the deep ultraviolet (DUV) range (e.g., having a wavelength of 248 nanometers (nm) or 193 nm). The size of the microelectronic features patterned on the wafer 120 depends on the wavelength of the beam 110, with lower wavelengths describing smaller minimum feature sizes. Alternatively, the lithography system 100 may use a beam 110 having a wavelength in the extreme ultraviolet (EUV) portion of the spectrum, for example, electromagnetic radiation (sometimes also referred to as soft X-rays) having a wavelength of about 50 nm or less, and including light having a wavelength of about 13.5 nm. The term "light" is used here and elsewhere in the text even though it is understood that the radiation described using this term may not be in the visible portion of the spectrum. The method of generating EUV light includes converting a target material from a liquid state to a plasma state. The target material preferably includes at least one element, such as xenon, lithium, or tin, and has one or more emission lines in the EUV range. In one such method, generally referred to as laser produced plasma ("LPP"), the desired plasma may be produced by irradiating a target material having the desired line-emitting element with a laser beam.
[0033] The scanner 115 includes an optical arrangement having, for example, one or more focusing lenses and an objective lens arrangement. The patterning device 116 can be moved in one or more directions, such as along the optical axis of the light beam 110 or in a plane perpendicular to the optical axis. The objective lens arrangement includes a projection lens and enables image transfer from the patterning device 116 to the photoresist on the wafer 120 to occur. The illumination system 105 adjusts the angular range at which the light beam 110 impinges on the mask. The illumination system 105 also homogenizes (makes uniform) the intensity distribution of the light beam 110 on the mask.
[0034] Among other features, the scanner 115 may include an etch controller 130, air conditioning, and power supplies for various electrical components. The etch controller 130 controls how layers are printed on the wafer 120. The etch controller 130 includes a memory that stores information such as a process recipe. The process program or recipe determines the exposure length on the wafer 120, the mask used, and other factors that affect the exposure. During etching, multiple pulses of the beam 110 illuminate the same area of the wafer 120 to constitute an exposure dose.
[0035] The lithography system 100 also preferably includes a control system 135. Typically, the control system 135 includes one or more of digital electronic circuitry, computer hardware, firmware, and software. The control system 135 also includes memory, which may be read-only memory and / or random access memory. Storage devices suitable for tangibly embodying computer program instructions and data include all forms of non-volatile memory, including, for example, semiconductor memory devices (such as EPROM, EEPROM, and flash memory devices); magnetic disks (such as internal hard disks and removable disks); magneto-optical disks; and CD-ROM disks.
[0036] The support structure 117 holds the patterning device 116 in a manner that depends on the orientation of the patterning device, the design of the lithographic apparatus, and other conditions, such as, for example, whether the patterning device is held in a vacuum environment. The support structure 117 can use mechanical, vacuum, electrostatic, or other clamping techniques to hold the patterning device. The support structure 117 can be, for example, a frame or table, which can be fixed or movable as needed. The support structure 117 can ensure that the patterning device 116 is in a desired position, for example, relative to the projection system.
[0037] The term "patterning device" should be broadly interpreted as referring to any device that can be used to impart a pattern in a cross-section of a radiation beam so as to create a pattern in a target portion of a substrate. The pattern imparted to the radiation beam may correspond to a specific functional layer in a device created in the target portion such as an integrated circuit.
[0038] The patterning device can be transmissive or reflective. As depicted here, the patterning device 116 is transmissive (e.g., using a transmissive mask). Examples of patterning devices include masks, programmable mirror arrays, and programmable LCD panels. Masks are well known in photolithography and include mask types such as binary, alternating phase shift, and attenuated phase shift, as well as various hybrid mask types. An example of a programmable mirror array uses a matrix arrangement of small mirrors, each of which can be individually tilted to reflect an incident radiation beam in different directions. The tilted mirrors impart a pattern in the radiation beam reflected by the mirror matrix.
[0039] The projection system, like the illumination system, may include various types of optical components, such as refractive, reflective, magnetic, electromagnetic, electrostatic or other types of optical components, or any combination thereof, as appropriate for the exposure radiation used or other factors such as the use of a vacuum. It may be desirable to use a vacuum for EUV radiation, since gases may absorb too much radiation. A vacuum environment may therefore be provided to the entire beam path with the aid of vacuum walls and a vacuum pump.
[0040] As mentioned, the wafer stage may be provided with an ordered or disordered (random) array of burls, and the top surface of each burl (i.e., the surface intended to come into contact with the wafer) may be provided with a nanoscale structured topography, i.e., structures having a feature size of about one nanometer or tens of nanometers. Figure 2 is shown in . Figure 2 The top surface of the wafer table WT is shown with a burl 300. The top surface of the burl 300 has a nanometer scale topography 310. The nanometer scale topography is shown as an array of hemispherical bumps, but it is to be understood that other shapes (such as pillars) can also be used. These are all referred to herein as nano bumps.
[0041] like Figure 3A As shown, substrate 300 has a working surface in the form of a nano-bump surface, i.e., a surface provided with an array of nano-bumps. Clean substrate 320 is laterally aligned with substrate 300. At least a portion of the surface of clean substrate 320 facing the working surface is provided with coating 330. Coating 330 may be made of a material such as aluminum, which forms a surface layer 340 of aluminum oxide. Figure 3A Also visible in the image is a particle 350 of contamination. The particle 350 may be made of, for example, chromium, which has adhered to the nanobump surface after transfer from, for example, a mask. The size of the particle 350 is typically about five microns or less.
[0042] In operation, Figure 3B As shown, clean substrate 320 is pressed against the nanobump surface of substrate 300. Alternatively and equivalently, the nanobump surface of substrate 300 is pressed against clean substrate 320. The surfaces may be pressed together with sufficient force to cause particle 350 to penetrate surface layer 340 and come into contact with coating 330. Due to the mechanical action of particle 350 penetrating surface layer 340 and the choice of material for coating 330, particle 350 is dislodged from the nanobump surface and transferred to coating 330 when substrate 300 and clean substrate 320 are moved away from each other, as shown in FIG. Figure 3C shown.
[0043] The above proposes a possible mechanism (a surface layer that mechanically captures particles) by which a surface with a specified geometry and composition can be used to remove contaminants. However, it is not necessary for the contaminants to "penetrate" the surface layer. For example, the bulk material (e.g., aluminum) below the surface layer can be relatively ductile, allowing the surface layer (e.g., alumina) to bend and conform to the contaminant to trap it. Therefore, the surface layer can be adherent in terms of bond energy, and the bulk material below the surface layer can allow the surface layer to bend around the particle, thereby increasing the surface area of contact, the effects of which work alone or together to promote the removal of contaminants.
[0044] The above description is primarily directed to the removal of contaminants in the form of particles, but contaminants may also take other physical forms. For example, contaminants may be in the form of a monolayer (contaminants before they accumulate enough to be considered particles) or stains / residues. Particles may be products of use or excess residues from a manufacturing process. The teachings of the present disclosure may be applied to facilitate the removal of all of these types of contaminants.
[0045] In the example shown, coating 330 covers only a portion of substrate 320. If coating 330 covers the entire facing area with the nanobump surface, it is possible that coating 330 will not be fully released. Therefore, for some applications, it is desirable to divide the area of the nanobump surface into sub-areas and successively use a series of cleaning substrates 320 with complementary patterned coatings to clean the nanobump surface. This is particularly useful in Figure 4 4 is shown in FIG. 4 , where a working surface 400 having an array of nano bumps is subdivided into a plurality of regions, such as region 410 and region 420. To clean the surface 400 in region 410, a cleaning substrate 430 having a coating 440 is used. Cleaning substrate 430 is shown in the figure as being smaller than the surface of target 400, but it is understood that surface 400 and cleaning substrate 430 may have substantially the same lateral dimensions. To clean area 420, a cleaning substrate 450 having a coating 460 is used, the coating 460 being in a region corresponding to region 420. Additional cleaning substrates may be used to clean additional regions.
[0046] As mentioned, this process can be performed in situ, for example, in a DUV tool, the process can be used to remove chrome from a reticle platform. Alternatively, the process can be performed to perform initial testing on a part.
[0047] Regarding the selection of the material of coating 330, in the case of some applications, for the material that is desired to be pulled away from the working surface, it is desired that the material for coating 330 has a higher bond dissociation energy than the working surface. The bond dissociation energy (enthalpy change) of the bond AB broken by the reaction AB→A+B is defined as the standard state enthalpy change of the reaction at a specific temperature. This means that, chemically, the particles will tend to adhere to the material of the coating in preference to the working surface. It is also desired that the material of the coating exhibits a low yield strength so that the particles can penetrate the coating, and the yield strength is the stress that produces a specific amount of plastic deformation. It is also desired that, for some applications, the material of the coating has a high Hamaker constant, which is a material constant that measures the relative strength of the van der Waals attraction between two surfaces (here, the surface of the particle and the surface of the coating 330 passing through layer 340).
[0048] As described above, in addition to aluminum, candidate materials for the coating include Ti, TiN, Si, SiN, Cr, CrN, CrO, CrNO, AlN, SiO, Ta, TaB, TaN, BO, BN, Cu, Au, and Ag. The thickness of the coating may preferably be in the range of about 0.1 nm to about 1000 nm, and more preferably in the range of about 20 nm to about 500 nm.
[0049] Figure 5 Another arrangement is shown where the working surface 500 is divided into sub-areas 510 and 520. To clean area 510, a cleaning substrate 530 having a coating 540 is brought opposite to and pressed against the working surface 500. To clean area 520, a cleaning substrate 550 having a coating 560 is brought opposite to and pressed against the working surface 500.
[0050] According to one aspect of an embodiment, the geometry of the coating is selected to amplify the local pressing force provided by the fixture or chuck. Typically, the size of the force that a fixture or chuck can generate is limited. For example, in EUV applications where an electrostatic chuck may be used, the size of the force that can be generated is limited by the dielectric breakdown of the insulator used to manufacture the chuck. On the DUV side, where a vacuum chuck may be used, the size of the force that can be generated is limited by the pressure difference between atmospheric pressure and vacuum. However, the local geometry of the coating can be used to create a higher local clamping force than is normally the case.
[0051] Fig. 6A , 6B 6C are diagrams illustrating these principles. Fig. 6A , 6B 6C illustrate an example in the case of an EUV source using an electrostatic chuck. The chuck 600 includes four electrodes 610 and a knobbed surface 620. The clean mask 630 has a conductive coating 640, which is necessary to achieve electrostatic clamping. The clean mask 630 also has a coating 650. Fig. 6A In the embodiment, the clamp 600 and the clean mask 630 are positioned facing each other. The electrostatic clamp is then energized so that the clean mask 630 is pressed against the knobbed surface 620, as shown in FIG. Figure 6B As described above, the total force applied by the clamp 600 is limited by the dielectric strength of the material used to make the clamp 600. However, the geometry and location of the coating 650 causes the right burl of the burled surface 620 to experience a higher localized compressive force during clamping. Moreover, the lateral extent of the coating 650 is geometrically limited to promote the peeling action of the coating relative to the burl. When the clamping force is removed, the coating 650 begins to peel from a well-defined location, such as Figure 6C shown.
[0052] Figure 7 1 is a flow chart showing a process of cleaning a work surface using a clean substrate as described above. In step S10, the clean substrate is loaded onto a platform. For example, this may be a mask platform or a wafer platform. In step S20, the clean substrate is moved to a position adjacent to the work surface. In step S30, the clean substrate is pressed against the work surface. In step S40, the clean substrate is withdrawn from contact with the work surface. In step S50, the clean substrate is moved to an unloading position. In step S60, the clean substrate is unloaded.
[0053] Figure 8 The process of cleaning a work surface using multiple cleaning substrates (coatings or other cleaning material layers, such as polyester-based wipes, etc.) is shown. In step S100, a first cleaning substrate of a cleaning substrate is pressed against the work surface. In step 110, the first cleaning substrate is pulled away from the work surface. In step S120, the next cleaning substrate is pressed against the work surface. The next cleaning substrate has a coating in a different position compared to the position of the coating on the first cleaning substrate to clean different areas of the work surface. In step S130, the next cleaning substrate is pulled away from the work surface. In step S140, it is determined whether all areas of the work surface desired to be cleaned have been cleaned. If not, the process returns to step S120. If yes, the process ends.
[0054] As mentioned above, due to the higher expected peel force during reticle blowing, material transfer to support structures such as reticle clamps leads to reticle adhesion problems and subsequent film failure. The use of nanostructured surfaces exacerbates these challenges. This may be due, at least in part, to the localized increase in contact pressure caused by the use of nanostructured surfaces.
[0055] Therefore, it is important to clean the fixture regularly to prevent problems associated with material transfer from becoming worse (e.g., by causing cracks in the film on the reticle fixture). For example, it is known to use a chrome etchant to remove chrome that has been transferred from the reticle to the nanostructured surface of the fixture (e.g., the nanostructured surface of the film placed on the fixture). This is a manual service action that can incur hours of downtime for the user. The foregoing describes at least one in-situ technique for removing chrome.
[0056] According to another aspect of the embodiment, another system and method for in-situ transfer material removal is described. As in the above example, the transferred material is chromium that was previously relocated from the mask to the mask fixture, but it is understood that the transferred material can be or include other materials. The system and method involve the use of a special tooling mask having a coating made of a relatively soft material (e.g., aluminum) with a Mohs hardness in the range of about 2.5 to 3. Although aluminum is used as an example in the following description, it is understood that another similar soft material can also be used for the coating.
[0057] The tooling reticle can be deployed in situ in a dry mode without the use of solvents or in a wet mode where a solvent such as isopropyl alcohol (IPA) can be used. In either mode, relative lateral motion is induced between the tooling reticle and the reticle fixture so that the tooling reticle is scrubbed on the surface of the reticle fixture to remove chromium transferred to the fixture. The soft coating helps capture chromium contamination while the relative motion displaces the chromium contamination and moves it away from the reticle fixture surface, for example, away from nano-bumps on the surface of a nanostructured reticle fixture. For in situ applications, the tooling reticle can be held fixed by the reticle handling handle clamp while the reticle stage clamp is scrubbed against the tooling reticle.
[0058] Typically, the lateral shape and size of the tooling reticle can be selected to be approximately the same as the lateral shape and size of the reticle holder surface. However, for some applications, it may be advantageous to use a tooling reticle with a different lateral size and shape. For example, the tooling reticle can be shorter than the facing surface of the fixture in the translation direction to allow a greater degree or range of relative translation, i.e., scrubbing.
[0059] According to another embodiment, two tooling reticles can be used to sequentially remove transferred material from the fixture. The first tooling reticle is used to displace material that has been transferred to the surface of the reticle fixture and capture some of the displaced material. The second tooling reticle is used to sweep away particles of the transferred material that were displaced but not captured by the first tooling reticle. These reticles can optionally be provided with a container for a cleaning fluid (such as IPA) to be able to operate in wet mode. The second reticle can be at least partially covered with a piece of material soaked with a cleaning solution (e.g., a clean room wipe) attached to the second reticle, which will be used to capture any loose displaced particles and slide them off the fixture.
[0060] Therefore, if Fig. 9As shown, a mask stage fixture 700 is supported by a mask stage 710. The surface of the mask fixture 700 facing the mask has nanostructures in the form of nano bumps in the example shown, the size of which is exaggerated in the figure for clarity. As discussed above, this surface may be contaminated with material (such as chromium) from the mask, to which the mask stage fixture has previously been used to fix the mask. In order to remove the transferred material, a tooling mask 720 is held in place by a mask handling handle 730. The tooling mask 720 includes a substrate 740 made of, for example, fused silica. The substrate 740 is provided with a coating 750, which is made of, for example, a soft material (such as aluminum). The vertical arrow on the left side of the figure indicates the clamping force to which the mask fixture is subjected due to the vacuum being drawn from the area where the fixture is located. In order to ensure that scrubbing can still be performed under this clamping force, the amount of vacuum drawn is lower than the vacuum amount when a normal mask is clamped. The fixture is compliant in nature, so the vacuum forces the fixture to contact the reticle and conform to its geometry. The horizontal arrows on the right side of the figure indicate that the reticle stage 710 is moved laterally while the tooling reticle 720 remains fixed to induce relative motion between the two, so that the tooling reticle 740 effectively scrubs the upper surface of the fixture 700. The reticle can also be made of a low stiffness material (such as plastic) so as to also conform to the geometry of the fixture assembly, which may have a pre-existing rotational tilt about the translation axis.
[0061] like Fig.10 As shown in the figure, in which similar reference numerals refer to similar structures, instead of providing a solid substrate of fused silica to the tooling mask 720, the substrate 760 can be provided with a cutout defining a container 770. The container 770 can contain a cleaning solution such as isopropyl alcohol. As shown, the container 770 can be in fluid communication with the facing surface of the coating 750 through a series of channels 800. The cleaning solution can be delivered through the channels 800 by means of capillary action. Alternatively, the cleaning solution can be delivered by operating one or more valves 810 ( Fig.11 ) to deliver cleaning fluid. Valve 810 can be actuated in various ways (including mechanical, pneumatic and electrical actuation). Fig.10 Also shown is a tooling mask cover 790. In operation, the tooling mask 720 is held in place while the mask platform 710 is moved laterally to cause a relative translational scrubbing motion. The relative translational motion may be unidirectional or bidirectional. At the same time, a cleaning fluid is dispensed from the container 770.
[0062] The embodiments may be further described using the following terms:
[0063] 1. In a system for generating radiation for use in lithography, the apparatus comprising:
[0064] a clamping structure including a working surface; and
[0065] A cleaning substrate for removing contaminants from a work surface, the cleaning substrate comprising:
[0066] a base having a side surface; and
[0067] A coating on at least a portion of the side surface.
[0068] 2. A device according to claim 1, wherein the coating comprises a surface layer and a bulk material.
[0069] 3. The apparatus of clause 1 or clause 2, wherein the working surface comprises a reticle stage and cleaning the substrate comprises cleaning the reticle.
[0070] 4. The apparatus of clause 1 or clause 2, wherein the working surface comprises a wafer stage and cleaning the substrate comprises cleaning the wafer.
[0071] 5. A cleaning substrate for removing particles of contaminants comprising a first material from a working surface comprising a second material, the cleaning substrate comprising:
[0072] a base having a side surface; and
[0073] A coating on at least a portion of the side surface, the coating comprising a third material, wherein a bond dissociation energy of a bond between the first material and the second material is less than a bond dissociation energy of a bond between the second material and the third material.
[0074] 6. The clean substrate of clause 5, wherein the working surface comprises a reticle stage and the clean substrate comprises a clean reticle.
[0075] 7. The cleaning substrate of clause 5, wherein the working surface comprises a wafer stage and the cleaning substrate comprises a cleaning wafer.
[0076] 8. The clean substrate of clause 5, wherein the first material comprises silicon.
[0077] 9. The clean substrate of clause 8, wherein the second material comprises chromium.
[0078] 10. The cleaning substrate of clause 9, wherein the third material comprises aluminum.
[0079] 11. The cleaning substrate of clause 5, wherein the third material has a low yield strength.
[0080] 12. The clean substrate of clause 5, wherein the third material has a high Hamaker constant.
[0081] 13. A method for removing contaminants from a working surface of a clamping structure in a lithography tool, the method comprising the steps of:
[0082] pressing a cleaning substrate against the work surface, the cleaning substrate comprising a base having a side surface and a coating on at least a portion of the side surface; and
[0083] The cleaning substrate is moved away from the work surface to remove contaminants from the work surface.
[0084] 14. The method of clause 13, wherein the working surface comprises a reticle stage, and cleaning the substrate comprises cleaning the reticle.
[0085] 15. The method of clause 13, wherein the work surface comprises a wafer stage and cleaning the substrate comprises cleaning the wafer.
[0086] 16. The method of clause 13, wherein the moving step is performed in a manner that causes a peeling action between the coating and the working surface.
[0087] 17. A method of removing particles of contaminants comprising a first material from a working surface comprising a second material, the method comprising the steps of:
[0088] pressing a cleaning substrate against the working surface, the cleaning substrate comprising a base having a side surface and a coating on at least a portion of the side surface, the coating comprising a third material, wherein a bond dissociation energy of a bond between the first material and the second material is less than a bond dissociation energy of a bond between the second material and the third material, such that contaminants are transferred from the working surface to the coating; and
[0089] The cleaning substrate is moved away from the work surface to remove contaminants from the work surface.
[0090] 18. The method of clause 17, wherein the working surface comprises a reticle stage, and cleaning the substrate comprises cleaning the reticle.
[0091] 19. The method of clause 17, wherein the work surface comprises a wafer stage and cleaning the substrate comprises cleaning the wafer.
[0092] 20. The method of clause 17, wherein the first material comprises silicon.
[0093] 21. The method of clause 20, wherein the second material comprises chromium.
[0094] 22. The method of clause 21, wherein the third material comprises aluminum.
[0095] 23. The method of clause 17, wherein the third material has a low yield strength.
[0096] 24. The method of clause 17, wherein the third material has a high Hamaker constant.
[0097] 25. A method of removing particles of contaminants according to clause 13 or 17, wherein the steps are repeated a plurality of times to remove the contaminants from substantially the entire working surface.
[0098] 26. The method according to clause 13 or 17, wherein the working surface is located in a vacuum chamber, and wherein the method further comprises the steps of:
[0099] Prior to the pressing step, the step of moving the cleaning substrate into position adjacent to the work surface; and
[0100] After the moving step, a step of repositioning the clean substrate to a position where the clean substrate can be unloaded.
[0101] 27. A method for removing contaminants from a work surface, the method comprising the steps of:
[0102] (a) pressing a first clean substrate against a first portion of the working surface, the clean substrate comprising a base having a side surface and a first coating on at least a portion of the side surface, the clean substrate having a lateral size and shape corresponding to the size and shape of the first portion, so that contaminants are transferred from the first portion to the first coating;
[0103] (b) moving the first clean substrate away from the working surface to remove contaminants from a first portion of the working surface;
[0104] (c) pressing a second clean substrate against a second portion of the working surface, the second clean substrate comprising a base having a side surface and a second coating on at least a portion of the side surface, the second clean substrate having a lateral size and shape corresponding to a size and shape of the second portion such that contaminants are transferred from the second portion to the second coating; and
[0105] (d) moving the second clean substrate away from the working surface to remove contaminants from a second portion of the working surface.
[0106] 28. A method of removing particles of contaminants comprising a first material from a working surface comprising a second material, the method comprising the steps of:
[0107] (a) pressing a first clean substrate against a first portion of the working surface, the clean substrate comprising a base having a side surface and a first coating on at least a portion of the side surface, the clean substrate having a lateral size and shape corresponding to the size and shape of the first portion, the first coating comprising a third material, wherein a bond dissociation energy of a bond between the first material and the second material is less than a bond dissociation energy of a bond between the second material and the third material, such that contaminants are transferred from the first portion to the first coating;
[0108] (b) moving the first clean substrate away from the working surface to remove contaminants from a first portion of the working surface;
[0109] (a) pressing a second clean substrate against a second portion of the working surface, the second clean substrate comprising a base having a side surface and a second coating on at least a portion of the side surface, the second clean substrate having a lateral size and shape corresponding to the size and shape of the second portion, the second coating comprising a third material, wherein a bond dissociation energy of a bond between the first material and the second material is less than a bond dissociation energy of a bond between the second material and the third material, such that contaminants are transferred from the second portion to the second coating; and
[0110] (d) moving the second clean substrate away from the working surface to remove contaminants from a second portion of the working surface.
[0111] 29. A method of removing particles of contaminants according to clause 28, wherein steps (a) to (d) are repeated a plurality of times to remove the contaminants from substantially the entire working surface.
[0112] 30. In a system for generating radiation for use in lithography, the apparatus comprising:
[0113] a clamping structure including a working surface; and
[0114] A cleaning substrate for removing contaminants from a working surface includes a base having a side surface and a coating on at least a portion of the side surface, the coating including a metal having a Mohs hardness of less than 5.
[0115] 31. The apparatus of clause 30, wherein the working surface comprises a reticle stage, and cleaning the substrate comprises cleaning the reticle.
[0116] 32. The apparatus of clause 30, wherein the working surface comprises a wafer stage and cleaning the substrate comprises cleaning the wafer.
[0117] 33. In a system for generating radiation for use in lithography, the apparatus comprising:
[0118] a clamping structure including a working surface; and
[0119] A cleaning substrate for removing contaminants from a work surface, the cleaning substrate comprising:
[0120] A base having a surface,
[0121] a coating on at least a portion of the surface, the coating comprising a metal having a Mohs hardness of less than 5,
[0122] a container within the cleaning substrate adapted to hold a cleaning fluid, and
[0123] A plurality of channels are arranged to place the container in fluid communication with the exterior of the coating.
[0124] 34. A cleaning substrate for removing contaminants from a work surface, the cleaning substrate comprising:
[0125] A base having a surface,
[0126] a coating on at least a portion of the surface, the coating comprising a metal having a Mohs hardness of less than 5;
[0127] a container within the cleaning substrate adapted to hold a cleaning fluid; and
[0128] A plurality of channels are arranged to place the container in fluid communication with the exterior of the coating.
[0129] 35. The clean substrate of clause 34, wherein the working surface comprises a reticle platform and the clean substrate comprises a clean reticle.
[0130] 36. The cleaning substrate of clause 34, wherein the working surface comprises a wafer stage and the cleaning substrate comprises a cleaning wafer.
[0131] 37. A method of removing contaminants from a working surface of a clamping structure in a lithography tool, the method comprising the steps of:
[0132] pressing a cleaning substrate against a work surface, the cleaning substrate comprising a base having a side surface and a coating on at least a portion of the side surface;
[0133] causing relative translational motion between the cleaning substrate and the work surface; and
[0134] Remove the clean substrate from the work surface.
[0135] 38. The method of clause 37, wherein the working surface comprises a reticle stage, and cleaning the substrate comprises cleaning the reticle.
[0136] 39. The method of clause 37, wherein the work surface comprises a wafer stage and cleaning the substrate comprises cleaning the wafer.
[0137] 40. The method of clause 37, further comprising, after the pressing step, the step of introducing a cleaning fluid between the cleaning substrate and the working surface.
[0138] 41. A method of removing contaminants from a working surface of a clamping structure in a lithography tool, the method comprising the steps of:
[0139] providing a piece of flexible material having a wet chemical etchant adsorbed therein;
[0140] attaching the piece of flexible material to a clean reticle;
[0141] pressing the clean reticle with the attached piece of flexible material against the work surface; and
[0142] The clean reticle with the attached piece of flexible material is removed from the work surface.
[0143] 42. The method according to clause 41, further comprising the following steps after the moving step:
[0144] removing the flexible material from the cleaned reticle;
[0145] providing a second piece of flexible material having a rinse agent absorbed therein;
[0146] attaching the second piece of flexible material to the clean reticle; and
[0147] The clean reticle is pressed against the work surface with the second piece of flexible material attached.
[0148] 43. The method of clause 42, further comprising, after the pressing step, the step of causing relative motion between the cleaning reticle and the working surface.
[0149] 44. The method of clause 41, wherein the flexible material comprises a polyester material.
[0150] 45. The method according to clause 43, wherein the rinse agent comprises isopropyl alcohol.
[0151] 46. The method according to clause 43, wherein the rinse agent comprises deionized water.
[0152] 47. A method for removing particles of contaminants from a work surface, the method comprising the steps of:
[0153] pressing a cleaning substrate against a work surface, the cleaning substrate comprising a base having a side surface and a coating on at least a portion of the side surface;
[0154] causing relative translational motion between the cleaning substrate and the work surface; and
[0155] Remove the clean substrate from the work surface.
[0156] 48. The method of clause 47, wherein the working surface comprises a reticle stage, and cleaning the substrate comprises cleaning the reticle.
[0157] 49. The method of clause 47, wherein the work surface comprises a wafer stage and cleaning the substrate comprises cleaning the wafer.
[0158] 50. The method of clause 47, further comprising, after the pressing step, the step of introducing a cleaning fluid between the cleaning substrate and the working surface.
[0159] 51. The method of clause 47, wherein the steps are repeated a plurality of times to remove the contaminant from substantially the entire working surface.
[0160] 52. The method of clause 47, wherein the working surface is located in a vacuum chamber, and wherein the method further comprises the steps of:
[0161] Prior to the pressing step, the step of moving the cleaning substrate into position adjacent to the work surface; and
[0162] After the moving step, a step of repositioning the clean substrate to a position where the clean substrate can be unloaded.
[0163] 53. A method for removing contaminants from a work surface, the method comprising the steps of:
[0164] (a) pressing a first clean substrate against a first portion of the working surface, the clean substrate comprising a base having a side surface and a first coating on at least a portion of the side surface, the clean substrate having a lateral size and shape corresponding to the size and shape of the first portion, so that contaminants are transferred from the first portion to the first coating;
[0165] (b) causing relative translational motion between the cleaning substrate and the working surface;
[0166] (c) moving the first clean substrate away from the working surface to remove contaminants from a first portion of the working surface;
[0167] (d) pressing a second clean substrate against a second portion of the working surface, the second clean substrate comprising a base having a side surface and a second coating on at least a portion of the side surface, the second clean substrate having a lateral size and shape corresponding to the size and shape of the second portion, such that contaminants are transferred from the second portion to the second coating;
[0168] (e) causing relative translational motion between the cleaning substrate and the work surface; and
[0169] (f) moving the second clean substrate away from the working surface to remove contaminants from a second portion of the working surface.
[0170] Although specific reference may be made herein to the use of lithographic apparatus in the manufacture of ICs, it should be understood that the lithographic apparatus described herein may have other applications, such as the manufacture of integrated optical systems, magnetic domain memories, flat panel displays, liquid crystal displays (LCDs), guidance and detection patterns of thin film heads, etc. It will be appreciated by those skilled in the art that in the case of such alternative applications, any use of the term "wafer" herein may be considered synonymous with the more general term "substrate" or "target portion", respectively. The substrate referred to herein may be processed before or after exposure, for example in a track (a tool that typically applies a resist layer to a substrate and develops the exposed resist), a metrology tool, and / or an inspection tool. Where applicable, the disclosure herein may be applied to such and other substrate processing tools. In addition, a substrate may be processed more than once, for example, to create a multi-layer IC, so the term "substrate" used herein may also refer to a substrate that already contains multiple processed layers.
[0171] Although specific embodiments of the present invention have been described above, it will be appreciated that the present invention may be practiced in a manner other than that described. The above description is intended to be illustrative rather than restrictive. Therefore, it will be apparent to those skilled in the art that modifications may be made to the described invention without departing from the scope of the claims set forth below.
[0172] It is to be understood that the "Detailed Description" section, rather than the "Summary" and "Abstract" sections, is intended to be used to interpret the claims. The Summary and Abstract sections may set forth one or more but not all exemplary embodiments of the present invention as contemplated by the inventors, and thus, are not intended to limit the present invention and the appended claims in any way.
[0173] The present invention has been described above by means of functional building blocks that illustrate the implementation of specified functions and their relationships. For ease of description, the boundaries of these functional building blocks have been arbitrarily defined in this article. Other boundaries can be defined as long as the specified functions and their relationships are properly performed.
[0174] The foregoing description of specific embodiments will reveal the general nature of the invention so fully that others can easily modify and / or adapt to various applications such as the specific embodiments without undue experimentation by applying knowledge within the art without departing from the general concept of the invention. Therefore, based on the teachings and guidance set forth herein, such adaptations and modifications are intended to fall within the meaning and range of equivalents of the disclosed embodiments. It is to be understood that the terms or terminology herein are for purposes of description and not limitation, so that the terms or terminology of this specification will be interpreted by the skilled person based on the teachings and guidance.
[0175] Thus, the breadth and scope of the present invention should not be limited by any of the above-described exemplary embodiments, but should be defined only in accordance with the following claims and their equivalents.
Claims
1. A device for removing pollutants, comprising: a clamping structure including a working surface; as well as A cleaning substrate for removing the contaminants from the working surface, the cleaning substrate comprising: a base having a lateral surface; as well as a coating for removing said contaminants only on parts of said lateral surfaces, The coating forms raised corners and the remainder of the lateral surface is uncoated.
2. The device of claim 1, wherein the coating comprises a surface layer and a bulk material.
3. The apparatus of claim 1 or claim 2, wherein the working surface comprises a reticle stage and the clean substrate comprises a clean reticle.
4. The apparatus of claim 1 or claim 2, wherein the working surface comprises a wafer stage and the cleaning substrate comprises a cleaning wafer.
5. A cleaning substrate for removing particles of contaminants comprising a first material from a working surface comprising a second material, the cleaning substrate comprising: a base having a lateral surface; as well as A coating for removing particles of the contaminant on only a portion of the lateral surface, the coating comprising a third material and a raised corner, wherein a bond dissociation energy of a bond between the first material and the second material is less than a bond dissociation energy of a bond between the second material and the third material, and the remainder of the lateral surface is uncoated.
6. The clean substrate of claim 5, wherein the working surface comprises a reticle stage and the clean substrate comprises a clean reticle.
7. The cleaning substrate of claim 5, wherein the working surface comprises a wafer stage and the cleaning substrate comprises a cleaning wafer.
8. The cleaning substrate of claim 5, wherein the first material comprises silicon.
9. The cleaning substrate of claim 8, wherein the second material comprises chromium.
10. The cleaning substrate of claim 9, wherein the third material comprises aluminum.
11. The cleaning substrate of claim 5, wherein the third material has a low yield strength.
12. The cleaning substrate of claim 5, wherein the third material has a high Hamaker constant.
13. A method for removing pollutants, the method comprising the following steps: pressing a clean substrate against a working surface of a clamping structure in a lithography tool, the clean substrate comprising a base having a lateral surface, and a coating for removing the contaminants on only a portion of the lateral surface, wherein the coating forms a raised corner and a remainder of the lateral surface is uncoated; and The cleaning substrate is moved away from the working surface to remove the contaminants from the working surface.
14. The method of claim 13, further comprising using a reticle stage having the working surface, and a clean reticle as the clean substrate.
15. The method of claim 13, further comprising using a wafer stage having the working surface, and a cleaning wafer as the cleaning substrate.
16. The method of claim 13, wherein the moving step is performed in a manner that causes a peeling action between the coating and the working surface.
17. A method of removing particles of contaminants comprising a first material from a working surface comprising a second material, the method comprising the steps of: pressing a cleaning substrate against the working surface, the cleaning substrate comprising a base having a lateral surface, and a coating for removing particles of the contaminant on only a portion of the lateral surface, the coating comprising a third material and raised corners, wherein a bond dissociation energy of a bond between the first material and the second material is less than a bond dissociation energy of a bond between the second material and the third material, such that the contaminant is transferred from the working surface to the coating, and a remaining portion of the lateral surface is uncoated; and The cleaning substrate is moved away from the working surface to remove the contaminants from the working surface.
18. The method of claim 17, wherein the working surface comprises a reticle stage and the clean substrate comprises a clean reticle.
19. The method of claim 17, wherein the working surface comprises a wafer stage and the cleaning substrate comprises a cleaning wafer.
20. The method of claim 17, wherein the first material comprises silicon. The method of claim 20 , wherein the second material comprises chromium.
22. The method of claim 21, wherein the third material comprises aluminum.
23. The method of claim 17, wherein the third material has a low yield strength.
24. The method of claim 17, wherein the third material has a high Hamaker constant.
25. The method of claim 13 or 17, wherein the steps are repeated a plurality of times to remove the contaminants from substantially the entire working surface.
26. The method of claim 13 or 17, wherein the working surface is located in a vacuum chamber, and wherein the method further comprises the steps of: Prior to the pressing step, a step of moving the cleaning substrate to a position adjacent to the working surface; as well as After the moving step, a step of repositioning the clean substrate to a position where the clean substrate can be unloaded.
27. A method for removing contaminants from a work surface, the method comprising the steps of: (a) pressing a first cleaning substrate against a first portion of the working surface, the first cleaning substrate comprising a base having a lateral surface, and a first coating for removing the contaminants on only a portion of the lateral surface, the first coating comprising raised corners, the first cleaning substrate having a lateral size and shape corresponding to the size and shape of the first portion, so that the contaminants are transferred from the first portion to the first coating; (b) moving the first clean substrate away from the working surface to remove the contaminants from the first portion of the working surface; (c) pressing a second clean substrate against a second portion of the working surface, the second clean substrate comprising a base having a lateral surface, and a second coating on only a portion of the lateral surface, the second clean substrate having a lateral size and shape corresponding to the size and shape of the second portion, such that the contaminants are transferred from the second portion to the second coating, wherein the lateral surface of the first clean substrate and the corresponding remaining portions of the lateral surface of the second clean substrate are uncoated; and (d) moving the second clean substrate away from the working surface to remove the contaminants from the second portion of the working surface.
28. A method of removing particles of contaminants comprising a first material from a working surface comprising a second material, the method comprising the steps of: (a) pressing a first clean substrate against a first portion of the working surface, the first clean substrate comprising a base having a lateral surface, and a first coating for removing the contaminant on only a portion of the lateral surface, the first coating comprising raised corners, the first clean substrate having a lateral size and shape corresponding to the size and shape of the first portion, the first coating comprising a third material, wherein a bond dissociation energy of a bond between the first material and the second material is less than a bond dissociation energy of a bond between the second material and the third material, so that the contaminant is transferred from the first portion to the first coating; (b) moving the first clean substrate away from the working surface to remove the contaminants from the first portion of the working surface; (c) pressing a second clean substrate against a second portion of the working surface, the second clean substrate comprising a base having a lateral surface, and a second coating on only a portion of the lateral surface, the second coating comprising raised corners, the second clean substrate having a lateral size and shape corresponding to the size and shape of the second portion, the second coating comprising a third material, wherein a bond dissociation energy of a bond between the first material and the second material is less than a bond dissociation energy of a bond between the second material and the third material, such that the contaminant is transferred from the second portion to the second coating, wherein respective remaining portions of the lateral surface of the first clean substrate and the lateral surface of the second clean substrate are uncoated; and (d) moving the second clean substrate away from the working surface to remove the contaminants from the second portion of the working surface.
29. The method of removing particles of contaminants according to claim 28, wherein said steps (a) to (d) are repeated a plurality of times to remove said contaminants from substantially the entire working surface.