Measurement method and device
By detecting radiation asymmetry and using a double-layer grating structure, the focal length problem of interlayer relative alignment measurement in 3D-NAND equipment is solved, and the measurement accuracy and throughput of the lithography process are improved.
Patent Information
- Application Number
- CN201980061872.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Priority Date
- 2018-09-19
- Filing Date
- 2019-09-19
- Publication Date
- 2024-11-08
- Estimated Expiration
- 2039-09-19
AI Technical Summary
During the manufacturing process of 3D-NAND equipment, when using existing image-based overprinting tools to measure relative alignment between layers, the image is inaccurate due to focal length problems, resulting in increased measurement time and reduced throughput.
By irradiating the target with radiation and detecting scattered radiation asymmetry, the integration of the signal is calculated to determine the parameters of interest, using a single image acquisition method, combined with symmetric and asymmetric irradiation techniques, a double-layer grating structure is used to improve measurement accuracy.
Accurate measurement of interlayer instrument is achieved, at least twice the measurement throughput and improve the efficiency of the manufacturing process.
Smart Images

Figure CN113168103B_ABST
Abstract
Description
[0001] CROSS-REFERENCE TO RELATED APPLICATIONS
[0002] This application claims priority to U.S. Application No. 62 / 733,490, filed on September 19, 2019, the entire contents of which are incorporated herein by reference. Background Art
[0003] Integrated circuits are usually manufactured by means of a manufacturing process in which layers are formed on top of each other on a substrate by means of several process steps. One of the process steps is photolithography, which can use electromagnetic radiation in the deep ultraviolet (DUV) spectral range or the extreme ultraviolet (EUV) spectral range. The substrate is usually a silicon wafer. The smallest dimensions in the manufactured structures are in the nanometer range.
[0004] During the manufacturing process, it is necessary to inspect the manufactured structure and / or measure the properties of the manufactured structure. Suitable inspection and metrology devices are known in the art. One type of metrology device known is a scatterometer, for example a dark field scatterometer.
[0005] Patent application publication US2016 / 0161864A1, patent application publication US2010 / 0328655A1, and patent application publication US2006 / 0066855A1 discuss embodiments of lithography apparatus and embodiments of scatterometers. The cited documents are incorporated herein by reference in their entirety.
[0006] In certain types of integrated circuits, such as 3D-NAND memory devices, a staircase profile has been made. The staircase needs to make contact with a single memory plane in the 3D-NAND device. This staircase is made by repeatedly removing a thin layer of resist, followed by an etching step to form a new double layer. The process is repeated N times, where N is the number of double layers. For many double layers, the initial resist pattern needs to be very thick, on the order of 10 μm. In addition, the lithography process used to make this resist pattern is designed to make sidewall angles of about 70 to 80 degrees, because it makes the best staircase profile.
[0007] exist Figure 1 The middle figure shows such a device. Figure 1 A cross section of an actual device is shown. In this example, the growth and processing directions of the layers (i.e. the way in which the layers are formed on top of each other) are from Figure 1 100. The bottom of the device, starting from element 106 and moving towards the surface of the device, in this example, the last layer depicted is the resist layer 102. Element 103 describes the continuity of the double layer. Element 102 is a thick layer of resist, for example with a thickness of 10 microns. Element 100 describes a typical opening, for example in the form of a V-groove, which is made with consideration for processing such a device. Figure 1 The V-shape shown in is only an example. The angle characterizing the opening is 101, which is, for example, 20 degrees.
[0008] During the manufacture of 3D-NAND devices, it is important to accurately know the relative alignment between opening 100 in layer 102 and structures in layer 106 (where layer 106 is a base layer). Such a measurement is referred to as overlay between opening 100 and structures in layer 106 (e.g., structures such as line 105). As described in the previously cited U.S. patent applications, overlay can be accurately measured using metrology tools. Overlay can be measured using an image-based overlay (IBO) tool or using a diffraction-based overlay (DBO) tool, the operation of which is well known and fully described in the prior art.
[0009] Due to the large distance between the two layers of interest (e.g. 20 microns), the problem with measuring overlay using an IBO tool is an out-of-focus image, i.e. if layer 102 is well within the focus of the impinging illuminating radiation, the structures in layer 106 are outside the focus of the impinging illuminating radiation, resulting in a poor quality image and therefore inaccurate overlay calculation. The solution is to measure the device twice, each time with the radiation beam focused first on the top layer and then on the bottom layer. This approach helps improve the measured overlay, but it results in an increase in the time used for metrology measurements, resulting in a reduction in throughput in the overall metrology and manufacturing process. Summary of the invention
[0010] The object of the present invention is to provide a method for measuring parameters of a lithography process such as overlay, comprising a single image acquisition. The measured image is not limited to the image plane, which is a known element of a metrology device that has been well described in the prior art, but can also be formed if the imaging sensor is placed in the pupil plane of the metrology device, which is also known and well described in the prior art. Using a single image acquisition suitable for allowing accurate overlay measurement, the throughput of the metrology is improved by at least a factor of two.
[0011] According to the present invention, a method for measuring a parameter of a manufacturing process is disclosed, the method comprising irradiating a target with radiation, detecting scattered radiation from the target, and determining a parameter of interest based on an asymmetry of the detected radiation. In addition, according to the method, the asymmetry is calculated as an integral of the measured signal.
[0012] According to the present invention, a method for measuring manufacturing process parameters is also disclosed, the method comprising irradiating a target using radiation from a radiation source of an optical instrument, wherein the target is made using a manufacturing process, wherein the radiation has symmetry about an axis (e.g., an optical axis of the optical instrument).
[0013] According to the present invention, a target suitable for measurement is also disclosed, the target comprising a first structure in a first layer, a second structure in a second layer, wherein the second structure comprises at least two gratings formed by photolithography, and wherein the first structure comprises at least a first lithographically formed opening. In addition, according to the target, the opening of the first structure is a V-groove. In addition, according to the target, the grating of the second structure is 2 longitudinal bars or gratings. In addition, according to the present invention, a target for measurement is disclosed, the target comprising a V-groove structure. BRIEF DESCRIPTION OF THE DRAWINGS
[0014] 2a) to 2f) illustrate a method of measuring parameters of a lithography process (such as overlay) using a metrology tool (eg, an IBO tool or a DBO tool). Figure 1 Schematic diagram of the described device. Figures 2d) to 2f) illustrate the measurement signal, which in an example is obtained by irradiating the Figure 1 structure and detecting scattered radiation from the target.
[0015] The structure illustrated in FIG2a) does not include the structure in layer 106. The scattered radiation detected on the image sensor is shown in FIG2d). With the addition of line 105 (two-element grating) as shown in FIG2b), the scattered signal changes to the form shown in FIG2e). For example, Figure 1 As shown in element 104, the distance between the gratings 105 is 5 microns. Figures 2d) to 2f) in Figure 2 are not proportions of the actual measured intensities, but rather schematic diagrams illustrating the expected behavior of the measured signal and the signal. The signal in Figure 2e) shows additional satellite peaks, which are caused by the additional line 105. In addition, if there is a misalignment between layer 102 and layer 106, and therefore in the presence of overlay, as shown in element 200 in Figure 2c), the measured signal plotted in Figure 2f) may show an enhanced satellite peak and a weakened satellite peak. The enhancement or weakening of the peak depends on the direction in which the overlay occurs. In addition, the magnitude of the enhancement is proportional to the amount of overlay that exists between the two layers. It is now recognized that the signal plotted in Figure 2e) is an example of a measured signal when there is no overlay between the layers of interest. DETAILED DESCRIPTION
[0016] In an embodiment, the maximum width of the opening 100 close to the layer 102 is 5 microns. In an embodiment, the distance between the two elements 105 (in Figure 1 Element 104) is also 5 microns.
[0017] In an embodiment, as illustrated in FIG2f, the overlay is proportional to the measured asymmetry. In order to obtain a value for the overlay, as expressed in nanometers, it is necessary to determine a proportionality factor between the measured asymmetry and the overlay. This proportionality factor, also referred to as K, can be eliminated by using a known procedure from DBO metrology, where two targets are used, where a known offset d is applied between the top and bottom gratings. One target has a positive offset d, and the other target has a negative offset -d. Any other method described in the art may also be used to determine or mitigate the presence of the proportionality factor K.
[0018] In an embodiment, the asymmetry of the measured signal may be determined by measuring the total area between the curve and the horizontal axis. In an embodiment, the asymmetry may be determined by measuring the integral of the measured signal about the horizontal axis. In an embodiment, the asymmetry may be measured by first determining the position of each satellite peak and using the difference between the values of the signals measured at these positions (i.e. where the satellite peaks are identified) as the measured asymmetry.
[0019] In an embodiment, the illuminating radiation is symmetric, e.g. the average angle of incidence is 0. If an asymmetric illumination can be used, two measurements are made of the same target from two directions (from opposite sides) with symmetric angles. In such an asymmetric (oblique) illumination, the measured signal is asymmetric even if there is no overlay. By adding the two measurement signals, the asymmetry due to the oblique illumination can be removed.
[0020] In one embodiment, the method is further extended by measuring two targets: a first target does not include element 105, so that the signal is mainly caused by the opening in layer 102, and a second target includes a target as shown in FIG2 c). Furthermore, if the method is further extended, wherein the target of FIG2 c) is measured with radiation of different wavelengths or polarization degrees. With such a measurement, possible effects of asymmetric illumination profiles or asymmetric shapes of the openings in layer 102 are mitigated.
[0021] It should be noted that Figure 1 The embodiment of FIG. 2 is an example. Those skilled in the art may imagine modifications having the same functionality, and these modifications are within the scope and spirit of the present invention.
Claims
1. A method for measuring parameters of a manufacturing process, include: irradiating a target with radiation, the target comprising: photolithographically formed openings; and At least two gratings formed by photolithography, wherein the gratings and the openings are located in different layers; determining a measurement signal by detecting scattered radiation from the target; In response to the measurement signal having an asymmetry, it is determined that the opening is misaligned with the grating.
2. The method of claim 1, wherein the asymmetry is calculated as the integral of the measured signal.
3. A method for measuring parameters of a manufacturing process, include: A target is illuminated with radiation from a radiation source of an optical instrument, the target comprising: photolithographically formed openings; and at least two gratings formed by photolithography, wherein the gratings and the openings are located in different layers, wherein said target is fabricated using said fabrication process; determining a measurement signal based on the scattered radiation from the target; and In response to determining that the measurement signal has asymmetry, determining the parameter as the presence of overlay in the manufacturing process, Wherein the radiation has symmetry about an axis, the axis being the optical axis of the optical instrument.
4. A target suitable for measurement, include: a first structure in a first layer; a second structure in the second layer; wherein the second structure comprises at least two gratings formed by photolithography; as well as The first structure at least includes an opening formed by a first photolithography, The first structure receives radiation to generate scattered radiation, and when the scattered radiation has an asymmetry, it is determined that the openings of the first structure are not aligned with the gratings of the second structure.
5. The target of claim 4, wherein the opening of the first structure is a V-shaped groove.
6. The target according to claim 4, wherein the grating of the second structure is 2 longitudinal bars.