Anode assembly and related manufacturing method

By forming reduced thickness areas and cavity of carbonaceous anode in the anode assembly to absorb the expansion force of the metal block, the problem of breaking the anode assembly under high temperature conditions is solved, and a lower cost and complex manufacturing method is achieved, reducing the The risk of anode rupture.

CN113195792BActive Publication Date: 2024-11-12RIOTINTO ALCAN INT LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN201980083098.2
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Priority Date
2018-12-20
Filing Date
2019-12-12
Publication Date
2024-11-12
Estimated Expiration
2039-12-12

AI Technical Summary

Technical Problem

The problem of the expansion of existing anode assemblies under high temperature conditions leads to anode rupture, existing solutions are costly and complex, and require manual placement of refractory fibers to absorb expansion forces, increasing manufacturing and recycling cost time.

Method used

In the manufacturing method of anode assembly, a reduced thickness region and cavity is formed inside the carbonaceous anode to absorb the longitudinal expansion force of the metal block, reduce the risk of anode rupture, and pass the sealing region between the sealing material and the metal block and the anode Form a conductive connection.

Benefits of technology

The risk of breakage of anode assembly under high temperature conditions is reduced, and it is lower in cost and complexity compared with the prior art, improves manufacturing efficiency, and reduces recycling costs and time.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN113195792B_ABST
    Figure CN113195792B_ABST
Patent Text Reader

Abstract

The invention relates to a method (100) for manufacturing an anode assembly (10) designed for a cell for producing aluminum by electrolysis, the anode assembly (10) comprising: an anode rod (1); a metal block (2) fixed to one of the ends (11) of the anode rod (1), the metal block (2) being able to expand in a longitudinal direction under the action of heat; a carbonaceous anode (3), the carbonaceous anode (3) comprising a recess (30) and a sealing area (41) in which the metal block (2) is accommodated for sealing the metal block (2) The carbon anode (3) is sealed, and the sealing area is filled with a sealing material extending between the metal block (2) and the carbon anode (3), characterized in that the method (100) includes a step (102) of forming at least a first cavity (42) inside the carbon anode (3), and the at least first cavity (42) together with the recess (30) forms a first reduced thickness area (43) inside the carbon anode (3), and the first reduced thickness area (43) can be deformed or broken under the expansion effect of the metal block (2) in the longitudinal direction.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to an anode assembly for a cell designed to produce aluminium by electrolysis, and to a method for producing such an anode assembly.

[0002] The invention is particularly suitable for electrolytic cells with prebaked anodes. Background Art

[0003] Aluminium is mainly produced by electrolysis of aluminium oxide dissolved in a cryolite bath. The electrolytic cell that allows this operation consists of a steel box and is lined with a refractory insulating product.

[0004] The cathode formed by a carbonaceous block is placed in the box. It is covered by an anode or a plurality of carbonaceous anodes or carbonaceous anode blocks inserted into a cryolite bath. This (or these) carbonaceous anodes are gradually oxidized by the oxygen produced by the decomposition of the alumina.

[0005] The current flows from the anode to the cathode through a cryolite bath which is maintained in a liquid state by the Joule effect.

[0006] The usual operating temperature of the cell is between 930°C and 980°C, the produced aluminium is liquid and is deposited by gravity on the cathodes. Periodically, the produced aluminium or part of it is extracted by a pouring ladle and transferred to a casting furnace. Once the anodes are exhausted, they are replaced with new ones.

[0007] To allow processing and its powering, each anode is usually associated with a structure to form an anode assembly. This structure generally consists of the following parts:

[0008] - an anode rod made of a material with high electrical conductivity, such as aluminum or copper, and

[0009] - Connection means made of a material resistant to the elevated temperatures encountered when the anode is in use, such as steel.

[0010] The connection means generally comprise a multipode formed as an integral crossbar, located at the base of a rod associated with a plurality of advantageously cylindrical blocks, the axes of which are parallel to the rod.

[0011] The block is partially introduced into a recess formed on the upper surface of the anode and the gap existing between the block and the recess is filled by pouring molten metal (usually cast iron). The metal cylinder thus manufactured ensures good mechanical fastening and good electrical connection between the rod and the anode.

[0012] However, it has been found in the prior art that the presence of the blocks causes an ohmic drop in the anode connection, as well as heat losses through the anode assembly.

[0013] Thus, document WO 2012 / 100340 proposes an anode assembly in which the assembly consisting of crossbars and blocks is replaced by a longitudinal connecting rod. During sealing, the connecting rod is introduced into a longitudinal recess formed on the upper surface of the anode. Molten cast iron is then deposited on the periphery of the connecting rod to fill the space between the connecting rod and the recess.

[0014] This solution makes it possible to improve the current distribution inside the anode, reduce the ohmic drop at the contact between carbon and cast iron and limit heat losses, as already taught in document FR 1,326,481, which proposes a solution identical to that of WO 2012 / 100340.

[0015] However, if the anode assemblies of the prior art preferably comprise cylindrical blocks, it is mainly to limit the risk of anode degradation due to the expansion experienced by the connection means during the introduction of the anode into a cryolite bath at a temperature between 930°C and 980°C.

[0016] In fact, unlike the expansion of a cylindrical block, which results in radial thermal expansion forces being exerted on the anode, the thermal expansion of a metal rod results in lateral and longitudinal forces being exerted on the anode, which may crack the anode.

[0017] No solution to this cracking problem is proposed in FR 1,326,481 or WO 2012 / 100340.

[0018] In the document WO 2015 / 110906, a solution to this rupture problem is proposed. The solution consists in providing at least one space without sealing material at one of the longitudinal ends of the connecting rod, the space being advantageously lined with a compressible filling material, such as refractory fibers. Therefore, during the expansion of the connecting rod, the refractory fibers absorb the force applied longitudinally by the connecting rod, thereby preventing the anode from rupturing under the action of the force. However, the disadvantage of this solution is that the refractory fibers need to be placed manually before the sealing material is poured. Therefore, this increases the cost and manufacturing time. In addition, once electrolysis is carried out, the refractory fibers must be removed from the anode assembly so that the carbon can be recovered. This operation also increases the cost and recovery time.

[0019] One object of the present invention is to propose a manufacturing method that is less expensive and less complex than the method proposed in document WO 2015 / 110906. This manufacturing method for forming an anode assembly has a lower risk of anode cracking under the effect of thermal expansion of the connecting rod.

[0020] Another object of the present invention is to provide an anode assembly obtainable by said manufacturing method. Summary of the invention

[0021] To this end, the present invention provides a method for manufacturing an anode assembly, wherein the anode assembly is used for a cell for producing aluminum by electrolysis, the anode assembly comprising: an anode rod; a metal block, wherein the metal block is fixed to one of the ends of the anode rod, and the metal block can expand in a longitudinal direction under the action of heat; a carbonaceous anode, wherein the carbonaceous anode comprises a recess and a sealing area, wherein the metal block is accommodated in the recess for sealing the metal block at the carbonaceous anode, and the sealing area is filled with a sealing material extending between the metal block and the carbonaceous anode, and is characterized in that the method comprises the step of forming at least a first cavity inside the carbonaceous anode, wherein the at least first cavity together with the recess forms a first reduced thickness area inside the carbonaceous anode, and the first reduced thickness area can be deformed or broken under the action of expansion in the longitudinal direction of the metal block.

[0022] Thus configured, the manufacturing method according to the invention makes it possible to form an anode assembly which presents a reduced risk of rupture of the carbonaceous anode under the effect of the expansion of the metal block.

[0023] In fact, part of the force applied to the anode during expansion of the metal block in its longitudinal direction is absorbed by the region of reduced thickness and the cavity.

[0024] Advantageously, the method of the present invention may further include the step of forming at least a second cavity inside the carbonaceous anode, wherein the at least second cavity together with the recess forms a second reduced thickness region inside the carbonaceous anode, and the second reduced thickness region is capable of deforming or breaking under the action of expansion in the longitudinal direction of the metal block.

[0025] In an alternative embodiment, the metal block has a substantially parallelepiped shape, in particular defined by four longitudinal surfaces, which are connected by two lateral surfaces, the at least first reduced thickness region and the corresponding at least second reduced thickness region being placed parallel to one of the lateral surfaces and separated from the lateral surface by the sealing area.

[0026] In case the anode assembly comprises two regions of reduced thickness, each region of reduced thickness will advantageously extend to a respective longitudinal end of the metal block. The regions of reduced thickness will then be distributed on both sides of the anode rod, which will allow on the one hand a better distribution of the intensity of the forces during expansion and on the other hand a better balancing of the mass of the anode assembly.

[0027] In a variant of the embodiment, the step of forming the at least first cavity and, respectively, the at least second cavity may comprise the following steps: placing an insert in a mould for forming the carbonaceous anode so as to define at least one protrusion inside the mould, the protrusion being designed to form the at least first cavity and, respectively, the at least second cavity.

[0028] In another variant of embodiment, the step of forming the at least first cavity, respectively the at least second cavity, may comprise the step of machining the carbonaceous anode.

[0029] The present invention also relates to an anode assembly of a cell for producing aluminum by electrolysis, the anode assembly comprising: an anode rod; a metal block, the metal block being fixed to one of the ends of the anode rod, the metal block being capable of expanding in a longitudinal direction under the action of heat; a carbonaceous anode, the carbonaceous anode comprising a recess and a sealing area, the metal block being accommodated in the recess for sealing the metal block at the carbonaceous anode, the sealing area being filled with a sealing material extending between the metal block and the carbonaceous anode, characterized in that the carbonaceous anode comprises at least a first cavity, the at least first cavity together with the recess forming a first reduced thickness area inside the carbonaceous anode, the first reduced thickness area being capable of deforming or breaking under the action of expansion in the longitudinal direction of the metal block.

[0030] Preferred but non-limiting aspects of the anode assembly are as follows:

[0031] - the carbonaceous anode comprises at least a second cavity, the at least second cavity forming with the recess a second reduced thickness region inside the carbonaceous anode, the second reduced thickness region being capable of being deformed or broken under the effect of expansion in the longitudinal direction of the metal block;

[0032] - said metal block has a substantially parallelepiped shape, in particular defined by four longitudinal surfaces connected by two transverse surfaces, said at least first area of ​​reduced thickness and respectively said at least second area of ​​reduced thickness being placed parallel to one of said transverse surfaces and separated therefrom by said sealing area;

[0033] The first cavity and the corresponding second cavity protrude laterally and vertically from the longitudinal projection of the lateral inner side wall of the recess, preferably by less than 5 cm;

[0034] - said first region of reduced thickness and respectively said at least second region of reduced thickness have a substantially flat contour and are oriented perpendicularly to said longitudinal direction;

[0035] - said first region of reduced thickness and respectively said at least second region of reduced thickness have a three-part profile, i.e. a central part surrounded by two end parts, said central part being substantially flat and oriented perpendicularly to said longitudinal direction and said end parts being oriented obliquely with respect to said central part;

[0036] - said first area of ​​reduced thickness and respectively said at least second area of ​​reduced thickness have a two-part profile, i.e. a first part and a second part connected to each other at an attachment area, each of said first part and second part having a biconvex profile, and wherein said first area of ​​reduced thickness and respectively said at least second area of ​​reduced thickness have a smaller thickness at said attachment area;

[0037] - the first region of reduced thickness and the respective at least second region of reduced thickness have a two-part profile, i.e. a first part and a second part connected to each other at an attachment region, each of the first part and the second part having a flat profile, and wherein the first region of reduced thickness and the respective at least second region of reduced thickness have a smaller thickness at the attachment region;

[0038] -The first reduced thickness area and the corresponding at least second reduced thickness area have a two-part profile, i.e., a first part and a second part connected to each other at an attachment area, each of the first part and the second part having a flat biconvex profile, and wherein the first reduced thickness area and the corresponding at least second reduced thickness area have a smaller thickness at the attachment area. BRIEF DESCRIPTION OF THE DRAWINGS

[0039] Other advantages and features of the anode assembly and its associated method of manufacture will emerge from the following description of several alternative embodiments given by way of non-limiting examples, in which:

[0040] [ Figure 1 ] Figure 1 is a perspective view of an anode assembly according to a first variant of an embodiment of the invention,

[0041] [ Figure 2 ] Figure 2 is integrated into the metal block Figure 1 A perspective view of the metal block of the anode assembly prior to being attached to the anode rod is shown in FIG.

[0042] [ Figure 3 ] Figure 3 It is used to manufacture Figure 1 A perspective view of a carbonaceous anode of an anode assembly is shown in FIG.

[0043] [ Figure 4 ] Figure 4 is a top view of an anode assembly according to a second variant of an embodiment of the present invention,

[0044] [ Figure 5 ] Figure 5 is along Figure 4 A cross-sectional view of CC' of the anode assembly represented in,

[0045] [Figure 6] Figures 6a to 6e are partial views of several variations of embodiments of the present invention,

[0046] [ Figure 7 ] Figure 7 is a block diagram of a method for manufacturing an anode assembly according to the present invention. DETAILED DESCRIPTION

[0047] An embodiment of a method for manufacturing an anode assembly and an embodiment of an anode assembly obtained from the process will now be described.In the different figures, equivalent elements have the same numerical references.

[0048] In the remainder of the text, the terms "side surface", "lower surface", "upper surface", "side wall" and "bottom" will be used with reference to the anode rod extending along the AA' axis.

[0049] The reader will understand that, in the context of the present invention:

[0050] - "lower surface" or "upper surface" means a surface extending in a plane perpendicular to the axis AA', the upper surface of a given piece being closer to the anode rod than the lower surface,

[0051] - "surface / side wall" means the surface / wall extending in a plane parallel to the A-A' axis of the anode rod,

[0052] - "surface / longitudinal wall" means a surface / wall extending parallel to the longitudinal axis of a longitudinal object (e.g. a recess or a metal block),

[0053] - "surface / transverse wall" means a surface / wall extending perpendicularly to the longitudinal axis of a longitudinal object,

[0054] - "longitudinal direction" or "longitudinally" means a direction parallel to the longitudinal axis of a longitudinal object (such as a recess or a metal block),

[0055] - By "outer wall" or "inner wall" of a cavity is meant the wall which is furthest or nearest to the AA' axis, respectively.

[0056] Figure 1 An embodiment of an anode assembly according to the present invention is illustrated. Figures 1 to 3 The anode assembly 10 includes an anode rod 1, a metal block 2 and a carbonaceous anode 3.

[0057] The anode rod 1 is made of an electrically conductive material. It extends along an axis A-A'. The anode rod is of a type conventionally known to a person skilled in the art and will not be described in more detail below.

[0058] The metal block 2 forms the connection means. The metal block 2 is made of a conductive material that can withstand the high use temperature of the anode assembly. For example, the metal block is made of steel.

[0059] The dimensions of the metal block 2 may be as follows:

[0060] - length L between 80 cm and 200 cm,

[0061] - The width I and the height h are between 5 cm and 50 cm.

[0062] In all cases, the length L is at least twice the width I of the metal block 2 .

[0063] The metal block 2 is integral with the anode rod 1 at one of its ends 11 and extends along a longitudinal axis BB' perpendicular to the axis A-A'. The metal block 2 comprises an upper surface 23 in contact with the anode rod 1, a lower surface 24 opposite to the upper surface 23, two longitudinal side surfaces 22 and two transverse side surfaces 21. The metal block 2 is, for example, a rod, may have a rectangular parallelepiped shape, and may include teeth on its side surfaces 21, 22 and / or its lower surface 24, in particular having a rounded shape.

[0064] The anode 3 is an anode block made of a prebaked carbon material, the composition and general form of which are known to those skilled in the art and will not be described in more detail later. The upper surface of the anode 3 has a recess 30 in which the metal block 2 is accommodated.

[0065] Advantageously, the recess 30 may have a shape complementary to that of the metal block 2 . In this case, the recess 30 has a longitudinal inner side wall 32 , a transverse inner side wall 31 and a bottom 34 .

[0066] The width I′ of the recess or groove is greater than the width I of the metal block 2 to allow insertion of the metal block 2 .

[0067] The anode assembly further comprises a sealing area filled with a sealing material 41. The sealing area extends between the longitudinal inner wall 32 of the recess 30 and the longitudinal side surface 22 of the metal block 2.

[0068] In the context of the present invention, the term "sealing material" is intended to mean a material allowing a rigid and electrically conductive connection to be formed between the anode and the metal block, the connection usually being provided by a cast metal (such as cast iron) or an electrically conductive glue between the metal block and the anode.

[0069] like Figure 1 As shown, the sealing material 41 covers all side surfaces 21, 22 of the metal block 2. The forces exerted longitudinally by the metal block 2 during its expansion will therefore be transferred integrally to the anode 3 via the sealing areas 41 adjacent to the lateral side surfaces 21 of the metal block 2.

[0070] In fact, we must remember, as a guide, that a steel metal block with a length equal to 1 meter can undergo a longitudinal expansion of up to 2 centimeters at 1000° C. Such a longitudinal expansion could potentially cause a very significant degradation of the anode 3 (rupture, explosion, etc.).

[0071] In order to avoid such degradation of the anode 3 under the effect of said longitudinal forces, the anode 3 is advantageously provided with a pair of cavities 42 placed on either side of the recess 30 along the longitudinal axis BB', each cavity 42 being located in the vicinity of a sealing area 41 adjacent to one of the lateral side surfaces 21 of the metal block 2. So placed, each cavity 42 forms, together with the recess 30, a reduced thickness area 43 in the anode 3, said reduced thickness area 43 being located between said sealing area 41 and said cavity 42. In particular, this reduced thickness area 43 will be configured to be able to deform or break under the effect of the forces exerted longitudinally by the metal block 2.

[0072] The thickness of the minimum thickness zone 43 is advantageously less than 5 cm and preferably between 0.5 cm and 3 cm to be able to deform or break without expanding the rupture in the rest of the anode. The cavity 42 will advantageously have a thickness greater than 0.5 cm and preferably greater than 1 cm to be able to absorb the deformation of the thickness of the reduced thickness zone 43 caused by the expansion of the metal block 2.

[0073] Thus, during expansion of the metal block 2, the forces exerted longitudinally by the metal block 2 will advantageously be transmitted first to the reduced thickness region 43, which will cause deformation or fracture of said reduced thickness region 43. Since the rest of the anode 3, in particular the part of the anode 3 between one of the side edges 33 of the anode 3 and the outer wall of the cavity 42 closest to this side edge, is not directly subjected to all the forces exerted longitudinally by the metal block, the risk of degradation is greatly reduced.

[0074] refer to Figure 4 and Figure 5 , another embodiment of the anode assembly is illustrated in a top view and a cross-sectional view along CC', respectively.

[0075] In this variant embodiment, the anode 3 has only one cavity 42 which, together with the recess 30, defines a single area of ​​reduced thickness 43. However, this area of ​​reduced thickness 43 will be sufficient to limit the risk of damaging the entire anode 3.

[0076] Regardless of the embodiment, the anode 3 includes at least one cavity 42 spaced apart from the recess 30, so that a reduced thickness region 43 of the anode 3 is formed between the at least one cavity 42 and the recess 30. Therefore, the anode 3 includes at least one reduced thickness region 43. The reduced thickness region 43 is a structure of the anode 3 that can be deformed or broken, for example, in the longitudinal direction, under the expansion effect of the metal block.

[0077] from Figure 4 and Figure 5 As can be seen in FIG. 4 , the cavity 42 extends laterally and vertically beyond the longitudinal projection of the inner transverse side wall 31. This configuration allows the breakage in the cavity 42 to recede, extending from the transverse inner side wall in a generally longitudinal direction, slightly away from the CC' axis. The overrun is advantageously less than 5 cm and preferably less than 3 cm to avoid weakening the anode 3 and disturbing the distribution of the current over the entire lower surface of the anode 3.

[0078] The shape of the reduced thickness region 43, the cavity 42 and the recess 30 may vary depending on various parameters, such as, in particular, the constituent material, size and / or shape of the anode 3 and / or the metal block 2. In particular, in certain embodiments, the shape of the minimum thickness region 43 may include at least one fracture interface of the anode 3, which is configured such that the reduced thickness region 43 can be fractured at the at least one fracture interface, for example, under the effect of a given stress generated by the expansion of the metal block. Such a fracture interface may adjoin a concave surface of the recess 30 or cavity 42. The concave surface may be curved, that is to say defining a curve (as Figure 6a The curve of this concavity can be configured to a greater or lesser extent so that the effect of the stress concentration in the minimum thickness area 43 can be of greater or lesser importance. The concavity can also be angular, i.e., the angle between the two parts defining the concavity (as in Figure 6b The angle of this concavity can be configured to a greater or lesser extent so that the effect of stress concentration in the minimum thickness region 43 can be of greater or lesser importance.

[0079] refer to Figures 6a to 6e , several advantageous embodiments of anodes 3 that can be used in the anode assembly of the present invention are shown.

[0080] exist Figure 6a In the embodiment shown, the reduced thickness region 43 has a substantially flat profile and is oriented perpendicularly towards the BB' axis of the metal block 2. The lateral inner side walls 31 of the recess 30 adjacent to the reduced thickness region 43 and the corresponding inner and outer walls of the cavity 42 in this case have a straight profile and are perpendicular to the BB' axis.

[0081] exist Figure 6bIn the embodiment shown, the area of ​​reduced thickness 43 has a profile in two parts, a first part 434 and a second part 435, connected to each other at the attachment area 430. Each of the parts 434, 435 has a biconvex profile, and the area of ​​reduced thickness 43 has a smaller thickness at the attachment area 430. The transverse inner side wall 31 of the recess 30 adjacent to the area of ​​reduced thickness 43 has in this case a curved profile complementary to the profile of the area of ​​reduced thickness 43, and the inner wall of the corresponding cavity 42 also has a curved profile complementary to the profile of the area of ​​reduced thickness 43.

[0082] exist Figure 6c In the embodiment shown, the area of ​​reduced thickness 43 has a two-part profile, namely a first part 436 and a second part 437 connected to each other at the attachment area 430. Each of the parts 436, 437 has a substantially flat profile, and the area of ​​reduced thickness 43 has a smaller thickness at the attachment area 430. The transverse inner side walls 31 of the recess 30 and the corresponding inner walls of the cavity 42 adjacent to the area of ​​reduced thickness 43 are in this case substantially straight in profile and perpendicular to the BB' axis, except for their respective areas aligned with the attachment area 430, whereby the profile is substantially triangular.

[0083] exist Figure 6d In the embodiment shown, the area of ​​reduced thickness 43 has a three-part profile, i.e. a central portion 431 surrounded by two end portions 432 and 433. The central portion 431 is substantially flat and oriented perpendicularly to the BB' axis, and the end portions 432 and 433 are oriented obliquely relative to the central portion 431. The transverse inner sidewalls 31 of the recess 30 adjacent to the area of ​​reduced thickness 43 have in this case a straight profile perpendicular to the BB' axis, and the corresponding inner and outer walls of the cavity 42 have a profile substantially complementary to the profile of the area of ​​reduced thickness 43.

[0084] exist Figure 6e In the embodiment shown, the area of ​​reduced thickness 43 has a two-part profile, namely a first part 438 and a second part 439 connected to each other at the attachment area 430. Each of the parts 438, 439 has a flat biconvex profile, and the area of ​​reduced thickness 43 has a smaller thickness at the attachment area 430. The lateral inner side wall 31 of the recess 30 adjacent to the area of ​​reduced thickness 43 has a curved profile in this case, complementary to the profile of the area of ​​reduced thickness 43, and the inner wall of the corresponding cavity 42 also has a curved profile, complementary to the profile of the area of ​​reduced thickness 43. Therefore, the cavity 42 has a gull-wing profile in this case.

[0085] Now refer to Figure 7 An embodiment of a method of manufacturing an anode assembly according to the present invention is described.

[0086] The manufacturing method 100 may be applied to form an anode assembly 10 whose anode 3 has a single reduced thickness region 43 adjacent one of the lateral inner sidewalls 31 of the recess 30 .

[0087] As a variant, the manufacturing method 100 can also be applied to form an anode assembly 10 whose anode 3 has two reduced thickness regions 43 placed on either side of the recess 30 , each region of reduced thickness 43 being adjacent to one of the lateral inner side walls 31 of the recess 30 .

[0088] In a first step 101 of the manufacturing method 100 , a metal block 2 fixed to an anode rod 1 is provided.

[0089] In a second step 102, a carbonaceous anode 3 is formed provided with a recess 30 and at least one cavity 42. In a first variant of the method, before the step of molding the carbonaceous anode 3, the second step 102 may comprise the step of placing an insert in the mold intended to form the carbonaceous anode 3 so as to define at least one protrusion inside the mold, the protrusion being intended for forming the at least one cavity 42.

[0090] In a second variant of the method, the second step 102 may comprise a step of moulding the carbonaceous anode 3 , followed by a step of machining the carbonaceous anode 3 to form said at least one cavity 42 .

[0091] In the third step 103 , the metal block 2 is introduced into the recess 30 , and the gap separating the metal block 2 from the anode 3 is filled with a sealing material to form a sealing area 41 .

[0092] Thus, by a method easily adaptable to industry, an anode assembly 10 according to the invention is obtained. Thus formed, this anode assembly 10 makes it possible to limit the risks of cracking and / or bursting of the anode 3 when it is introduced into a cryolite bath.

Claims

1. A method (100) for manufacturing an anode assembly (10) designed as a cell for producing aluminum by electrolysis, the anode assembly (10) comprising: An anode rod (1); a metal block (2), the metal block being fixed to one of the ends (11) of the anode rod (1), the metal block (2) being capable of expanding in a longitudinal direction under the action of heat; a carbonaceous anode (3), the carbonaceous anode (3) comprising a recess (30) and a sealing area (41), the metal block (2) being accommodated in the recess for sealing the metal block (2) at the carbonaceous anode (3), the sealing area being filled with a sealing material extending between the metal block (2) and the carbonaceous anode (3), characterized in that the method (100) comprises forming at least a first cavity (42) inside the carbonaceous anode (3) ), the at least first cavity (42) together with the recess (30) forms a first reduced thickness region (43) inside the carbonaceous anode (3), the first reduced thickness region (43) being adjacent to the lateral inner side wall (31) of the recess (30) and being capable of deforming or breaking under the expansion of the metal block (2) in the longitudinal direction, wherein the shape of the first reduced thickness region (43) includes at least one fracture interface, and the at least one fracture interface is configured so that the first reduced thickness region (43) can break at the at least one fracture interface under the action of a given stress generated by the expansion of the metal block.

2. The manufacturing method (100) according to claim 1 further includes a step (102) of forming at least a second cavity inside the carbonaceous anode (3), wherein the at least second cavity together with the recess (30) forms a second reduced thickness region inside the carbonaceous anode (3), and the second reduced thickness region is capable of being deformed or broken under the expansion action of the metal block (2) in the longitudinal direction.

3. A manufacturing method (100) according to any one of claims 1 or 2, wherein the metal block (2) has a substantially parallelepiped shape, in particular defined by four longitudinal surfaces (22-24), the longitudinal surfaces being connected by two transverse surfaces (21), and the at least first reduced thickness area (43) being arranged parallel to one of the transverse surfaces (21) and separated from the transverse surface by the sealing area (41).

4. The manufacturing method (100) according to any one of claims 1 or 2, wherein the step (102) of forming the at least first cavity (42) may include the following steps: An insert is placed in a mold for forming the carbonaceous anode (3) so as to define at least one protrusion inside the mold, the protrusion being designed to form the at least first cavity (42).

5. The manufacturing method (100) according to any one of claims 1 or 2, wherein the step (102) of forming the at least first cavity (42) comprises the step of machining the carbonaceous anode (3).

6. The manufacturing method (100) according to any one of claims 1 or 2, wherein the at least first cavity (42) is formed to protrude laterally and vertically from the longitudinal projection of the lateral inner wall (31) of the recess (30), and the protrusion amount is less than 5 cm.

7. An anode assembly (10) designed for a cell for producing aluminium by electrolysis, said anode assembly (10) comprising: An anode rod (1); a metal block (2), the metal block being fixed to one of the ends (11) of the anode rod (1), the metal block (2) being capable of expanding in a longitudinal direction under the action of heat; a carbonaceous anode (3), the carbonaceous anode (3) comprising a recess (30) and a sealing area (41), the metal block (2) being accommodated in the recess for sealing the metal block (2) at the carbonaceous anode (3), the sealing area being filled with a sealing material extending between the metal block (2) and the carbonaceous anode (3), characterized in that the carbonaceous anode (3) comprises at least a first cavity (42), the The at least first cavity (42) together with the recess (30) forms a first reduced thickness region (43) inside the carbonaceous anode (3), the first reduced thickness region (43) being adjacent to the lateral inner wall (31) of the recess (30) and being capable of deforming or breaking under the action of expansion in the longitudinal direction of the metal block (2), wherein the shape of the first reduced thickness region (43) includes at least one fracture interface, and the at least one fracture interface is configured so that the first reduced thickness region (43) can break at the at least one fracture interface under the action of a given stress generated by the expansion of the metal block.

8. The anode assembly (10) according to claim 7, wherein the carbonaceous anode (3) comprises at least a second cavity, wherein the at least second cavity and the recess (30) form a second reduced thickness region inside the carbonaceous anode (3), and the second reduced thickness region is capable of being deformed or broken under the expansion action of the metal block (2) in the longitudinal direction.

9. Anode assembly (10) according to any one of claims 7 or 8, wherein the metal block (2) has a substantially parallelepiped shape, in particular defined by four longitudinal surfaces (22-24), the longitudinal surfaces being connected by two transverse surfaces (21), and the at least first reduced thickness area (43) being arranged parallel to one of the transverse surfaces (21) and separated from the transverse surface by the sealing area (41).

10. The anode assembly (10) according to claim 7 or 8, wherein the first region of reduced thickness (43) has a substantially flat profile and is oriented perpendicular to the longitudinal direction.

11. An anode assembly (10) according to claim 7 or 8, wherein the first reduced thickness region (43) has a three-part profile, i.e., a central portion (431) is surrounded by two end portions (432, 433), the central portion (431) being substantially flat and oriented perpendicular to the longitudinal direction and the end portions (432, 433) being oriented obliquely relative to the central portion (431).

12. An anode assembly (10) according to claim 7 or 8, wherein the first reduced thickness region (43) has a two-part profile, namely, a first part and a second part connected to each other at an attachment area (430), each of the first part and the second part having a double convex profile, and wherein the first reduced thickness region (43) has a smaller thickness at the attachment area (430).

13. An anode assembly (10) according to claim 7 or 8, wherein the first reduced thickness region (43) has a two-part profile, i.e., a first part and a second part are connected to each other at an attachment region (430), each of the first part and the second part has a substantially flat profile, and wherein the first reduced thickness region and the corresponding second reduced thickness region have a smaller thickness at the attachment region (430).

14. An anode assembly (10) according to claim 7 or 8, wherein the first reduced thickness region (43) and the corresponding second reduced thickness region have a two-part profile, i.e., a first part and a second part connected to each other at an attachment region (430), each of the first part and the second part having a double convex profile, and wherein the first reduced thickness region and the corresponding second reduced thickness region have a smaller thickness at the attachment region (430).

15. Anode assembly (10) according to claim 7 or 8, wherein the at least first cavity (42) protrudes laterally and vertically from the longitudinal projection of the transverse inner side wall (31) of the recess (30) by less than 5 cm.