Photosensitive conductor paste, laminated electronic component and method for producing the same

By using high melting point quartz powder and conductor powder with appropriate particle size in the photosensitive conductor paste, the problem of voids generated during heat treatment is solved and the density of stacked electronic components is improved. and mechanical properties.

CN113534632BActive Publication Date: 2024-12-03TDK CORP
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202110371585.8
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Priority Date
2020-04-16
Filing Date
2021-04-07
Publication Date
2024-12-03
Estimated Expiration
2041-04-07

AI Technical Summary

Technical Problem

During the heat treatment process, the existing photosensitive conductor paste has a gap between the conductor pattern and the body pattern due to the softening of the glass powder, which affects the quality of the stacked electronic components.

Method used

The photosensitive conductor paste containing quartz powder is used. The melting point of the quartz powder is higher than the heat treatment temperature to avoid melting. The particle size of the conductor powder is larger than that of the quartz powder. The conductor and body pattern are formed by photolithography to ensure that the conductor layer is during heat treatment. It is close to the shrinkage rate and shrinkage action of the body layer, inhibiting the generation of voids.

Benefits of technology

The gap between the conductor layer and the body layer is effectively suppressed, the density and accuracy of the laminated electronic components are improved, and its mechanical properties are enhanced.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN113534632B_ABST
    Figure CN113534632B_ABST
Patent Text Reader

Abstract

The present invention provides a photosensitive conductor paste, which includes a photosensitive organic component, a conductor powder and a quartz powder, wherein the quartz powder does not melt or is extremely difficult to melt during a heat treatment process, so that the conductor layer and the element layer can fully function in a manner that makes the shrinkage rate and shrinkage behavior of the two close during the heat treatment process, thereby being able to suppress the generation of voids when used in the manufacture of stacked coil components.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This application claims priority based on Japanese Patent Application No. 2020-73424 filed on April 16, 2020, the entire contents of which are incorporated herein by reference.

[0002] The present disclosure relates to a photosensitive conductor paste, a laminated electronic component, and a method for manufacturing the same. Background Art

[0003] Conventionally, there is known a technique for forming a conductor pattern of a laminated electronic component by a photolithography method using a photosensitive conductor paste. Japanese Patent Application Laid-Open No. 2001-264965 discloses a photosensitive conductor paste to which glass frit is added as an inorganic additive. Summary of the invention

[0004] The inventors have repeatedly studied inorganic additives added to photosensitive conductor pastes and have obtained the following knowledge: by adding inorganic additives, the difference in shrinkage rate and shrinkage behavior between the element body and the conductor pattern of the laminated electronic component can be adjusted. However, in the photosensitive conductor paste to which glass powder is added as an inorganic additive, the glass softens during the heat treatment in the manufacturing process, and as a result, voids may be generated between the element body and the conductor pattern.

[0005] According to the present disclosure, a photosensitive conductor paste, a laminated electronic component and a method for manufacturing the same in which generation of voids is suppressed are provided.

[0006] A photosensitive conductor paste according to one aspect of the present disclosure includes a photosensitive organic component, a conductor powder, and a quartz powder.

[0007] Since the melting point of quartz is higher than the heat treatment temperature when manufacturing a laminated electronic component, the quartz powder is less likely to melt in the photosensitive conductor paste, and the generation of voids can be suppressed when used in the manufacture of a laminated electronic component.

[0008] In the photosensitive conductor paste according to another aspect, the median particle size of the quartz powder is 0.4 to 5.0 μm.

[0009] In the photosensitive conductor paste according to another aspect, the median particle size of the conductor powder is equal to or larger than the median particle size of the quartz powder.

[0010] In the photosensitive conductor paste according to another aspect, the conductor powder is silver powder.

[0011] A laminated electronic component according to one aspect of the present disclosure has a laminated structure including a plurality of element layers having defect portions with rectangular cross sections and a plurality of conductor layers filling the defect portions of the plurality of element layers, wherein the conductor layers are formed of conductors enclosing quartz powder.

[0012] In the above-mentioned laminated electronic component, the conductor layer contains quartz powder, so that melting during heat treatment during manufacturing is suppressed, and the generation of voids between the element layer and the conductor layer is suppressed.

[0013] In the laminated electronic component according to another aspect, the plurality of conductor layers constitute a coil.

[0014] In the laminated electronic component according to another aspect, the element layer is made of a material containing a glass component.

[0015] A method for manufacturing a stacked electronic component according to one aspect of the present disclosure includes: a process of forming a stacked body, wherein the stacked body includes a plurality of element patterns that are stacked and each have a defect portion with a rectangular cross-section, and a plurality of conductor patterns that fill the defect portions of each of the plurality of element patterns; and a process of heat-treating the stacked body so that the element pattern becomes an element layer and the conductor pattern becomes a conductor layer, wherein the conductor pattern is formed by photolithography using a photosensitive conductor paste containing a photosensitive organic component, conductor powder and quartz powder.

[0016] In the above-mentioned method for manufacturing a laminated electronic component, since the quartz powder added to the photosensitive conductor paste is difficult to melt in the heat treatment step, the generation of voids between the element layer and the conductor layer is suppressed. BRIEF DESCRIPTION OF THE DRAWINGS

[0017] Figure 1 This is an electron microscope photograph of the photosensitive conductor paste according to the first embodiment after heat treatment.

[0018] Figure 2 This is a perspective view of a laminated coil component manufactured by the method for manufacturing the laminated coil component according to the first embodiment.

[0019] Figure 3 yes Figure 1 An exploded perspective view of the laminated coil component shown.

[0020] Figure 4 This is a flowchart showing the method for manufacturing the laminated coil component according to the first embodiment.

[0021] Figure 5 A to 5G are cross-sectional views conceptually showing the method for manufacturing the laminated coil component according to the first embodiment.

[0022] Figure 6 6A and 6B are cross-sectional views conceptually showing the method for manufacturing the laminated coil component according to the first embodiment.

[0023] Figure 7 This is an electron microscope photograph of a photosensitive conductor paste to which glass frit is added after heat treatment.

[0024] Figure 8 This is a flowchart showing a method for manufacturing a laminated coil component according to the second embodiment.

[0025] Fig. 9 A to 9E are cross-sectional views conceptually showing the method for manufacturing the laminated coil component according to the second embodiment. DETAILED DESCRIPTION

[0026] Hereinafter, embodiments of the present disclosure will be described in detail with reference to the accompanying drawings. In the description, the same elements or elements having the same functions are denoted by the same reference numerals, and repeated descriptions are omitted.

[0027] [First embodiment]

[0028] (Photosensitive conductor paste)

[0029] The photosensitive conductor paste according to the first embodiment includes conductor powder as a conductive component in a photosensitive organic component and quartz powder as an inorganic additive component. More specifically, the photosensitive conductor paste has conductor powder and quartz powder dispersed in the photosensitive organic component. The photosensitive conductor paste does not include glass as an inorganic additive component.

[0030] The photosensitive organic component of the photosensitive conductor paste includes an organic binder and an organic solvent, and may further include, for example, a photopolymerizable monomer or a photopolymerization initiator, etc. The photosensitive organic component may be either negative or positive.

[0031] The conductor powder is, for example, a metal powder such as silver powder or alloy powder. In the present embodiment, the conductor powder is silver powder. In the present embodiment, the silver powder has a median particle size (d50 particle size) of 0.5 to 5.0 μm (2.5 μm as an example).

[0032] Quartz powder is a fine powder (silica sand) composed of quartz, obtained by, for example, crushing. In the present embodiment, the quartz powder has a median particle size (d50 particle size) of 0.4 to 5.0 μm. In the present embodiment, the median particle size of the silver powder is greater than the median particle size of the quartz powder. The quartz powder may also have a d95 particle size of 1.0 to 7.0 μm. The quartz powder may also have a maximum particle size of 2.0 to 10 μm. As an example, the median particle size of the quartz powder is 1.0 μm, the d95 particle size is 2.0 μm, and the maximum particle size is 5.0 μm. In the case where the quartz powder is too fine, when the photosensitive conductor paste is dried and filmed, the thickness (reaction film thickness) of the photopolymerization reaction caused by light reaching the quartz powder is deteriorated, and therefore, a certain degree of large particle size is required for the quartz powder. The quartz powder is added at a ratio of about 0.5 to 2.5 wt% relative to the silver powder. By adjusting the addition ratio of quartz powder, the shrinkage rate of the photosensitive conductor paste during heat treatment can be adjusted. For example, by increasing the addition ratio of quartz powder, the shrinkage rate (final shrinkage rate) can be reduced, and the difference in shrinkage rate between the conductor layer and the body layer in the laminated electronic component described later can be reduced. In addition, by adjusting the addition ratio of quartz powder, the behavior of the body layer from the beginning of shrinkage to the end of shrinkage (shrinkage behavior) can be made close to the shrinkage behavior of the conductor layer. By making the shrinkage rate and shrinkage behavior between the conductor layer and the body layer close, the voids generated near the interface between the conductor layer and the body layer due to the difference in shrinkage rate and shrinkage behavior can be suppressed.

[0033] like Figure 1 As shown, the quartz powder has a shape with multiple corners (or sharp parts), for example, a polygonal cross section. As for the quartz powder, if it is heat-treated at a temperature lower than the melting point of quartz (about 1600 to 1700°C), it will not melt and maintain its shape. When the quartz powder is not melted, the quartz powder will not agglomerate with each other and will remain dispersed even after heat treatment.

[0034] Furthermore, since the quartz powder has sufficient light transmittance (UV transmittance), the quartz powder does not hinder the exposure during the exposure in the photolithography method with respect to the photosensitive conductor paste.

[0035] (Laminated coil components)

[0036] Reference Figure 2 and Figure 3 A laminated coil component according to a first embodiment will be described. Figure 2 This is a perspective view of a laminated coil component manufactured by the method for manufacturing the laminated coil component according to the first embodiment. Figure 3 yes Figure 2 An exploded perspective view of the laminated coil component shown.

[0037] like Figure 2 and Figure 3As shown, the laminated coil component 1 according to the first embodiment includes: an element body 2 ; mounting conductors 3 , 4 ; a plurality of coil conductors 5 c , 5 d , 5 e , 5 f ; and connection conductors 6 , 7 .

[0038] The element body 2 is in the shape of a rectangular parallelepiped. The rectangular parallelepiped shape includes the shape of a rectangular parallelepiped with chamfered corners and ridges, and the shape of a rectangular parallelepiped with rounded corners and ridges. The element body 2 has end faces 2a, 2b and side faces 2c, 2d, 2e, 2f. The end faces 2a, 2b are opposite to each other. The side faces 2c, 2d are opposite to each other. The side faces 2e, 2f are opposite to each other. Hereinafter, the relative direction of the end faces 2a, 2b is set as direction D1, the relative direction of the side faces 2c, 2d is set as direction D2, and the relative direction of the side faces 2e, 2f is set as direction D3. Direction D1, direction D2, and direction D3 are substantially orthogonal to each other.

[0039] The end faces 2a and 2b extend in the direction D2 so as to connect the side faces 2c and 2d. The end faces 2a and 2b also extend in the direction D3 so as to connect the side faces 2e and 2f. The side faces 2c and 2d extend in the direction D1 so as to connect the end faces 2a and 2b. The side faces 2c and 2d also extend in the direction D3 so as to connect the side faces 2e and 2f. The side faces 2e and 2f extend in the direction D2 so as to connect the side faces 2c and 2d. The side faces 2e and 2f also extend in the direction D1 so as to connect the end faces 2a and 2b.

[0040] The side surface 2c is a mounting surface, for example, a surface facing other electronic devices (eg, circuit substrates or electronic components) when the laminated coil component 1 is mounted on other electronic devices (eg, circuit substrates or electronic components) not shown. The end surfaces 2a and 2b are surfaces continuous from the mounting surface (ie, the side surface 2c).

[0041] The length of the element body 2 in the direction D1 is longer than the length of the element body 2 in the direction D2 and the length of the element body 2 in the direction D3. The length of the element body 2 in the direction D2 and the length of the element body 2 in the direction D3 are equal to each other. That is, in the present embodiment, the end faces 2a and 2b are square, and the side faces 2c, 2d, 2e, and 2f are rectangular. The length of the element body 2 in the direction D1 may be equal to the length of the element body 2 in the direction D2 and the length of the element body 2 in the direction D3, or may be shorter than these lengths. The length of the element body 2 in the direction D2 and the length of the element body 2 in the direction D3 may also be different from each other.

[0042] In addition, in this embodiment, “equivalent” may also be defined as values ​​that include a slight difference or manufacturing error within a predetermined range. For example, if multiple values ​​are within a range of ±5% of the average value of the multiple values, the multiple values ​​are defined as being equal.

[0043] The element body 2 is provided with recessed portions 21, 22, 23, and 24. The recessed portions 21 and 22 are provided integrally, and correspond to the mounting conductor 3. The recessed portions 23 and 24 are provided integrally, and correspond to the mounting conductor 4.

[0044] The recess 21 is provided on the side of the end face 2a of the side face 2c and is recessed toward the side face 2d. The recess 22 is provided on the side of the side face 2c of the end face 2a and is recessed toward the end face 2b. The recess 23 is provided on the side of the end face 2b of the side face 2c and is recessed toward the side face 2d. The recess 24 is provided on the side of the side face 2c of the end face 2b and is recessed toward the end face 2a. The recesses 21, 22, 23, and 24 have, for example, the same shape. The recesses 21, 22, 23, and 24 are provided separately from the side faces 2d, 2e, and 2f. The recess 21 and the recess 23 are provided separately from each other in the direction D1.

[0045] The element body 2 is formed by stacking a plurality of element body layers 12a to 12f in the direction D3. The specific stacking structure will be described later. In the actual element body 2, the plurality of element body layers 12a to 12f are integrated to such an extent that the boundaries between the layers cannot be identified. The element body layers 12a to 12f are, for example, composed of a magnetic material (Ni-Cu-Zn ferrite material, Ni-Cu-Zn-Mn ferrite material, or Ni-Cu ferrite material, etc.). The magnetic material constituting the element body layers 12a to 12f may also include Fe alloys, etc. The element body layers 12a to 12f may also include glass materials, or may be composed of non-magnetic materials (glass ceramic materials, dielectric materials, etc.).

[0046] The mounting conductor 3 is arranged in the recesses 21 and 22. The mounting conductor 4 is arranged in the recesses 23 and 24. The mounting conductors 3 and 4 are separated from each other in the direction D1. The mounting conductors 3 and 4 are, for example, of the same shape. The mounting conductors 3 and 4 are, for example, L-shaped in cross section. It can also be said that the mounting conductors 3 and 4 are, for example, L-shaped when viewed from the direction D3. A plating layer may be formed on the outer surface of the mounting conductors 3 and 4 by electroplating or electroless plating. The plating layer includes, for example, Cu, Ni, Sn, Au, etc.

[0047] The mounting conductor 3 is formed by stacking a plurality of mounting conductor layers 13 in an L-shape when viewed from the direction D3 in the direction D3. In the actual mounting conductor 3, the plurality of mounting conductor layers 13 are integrated to such an extent that the boundaries between the layers cannot be identified. The mounting conductor 3 has integrally formed conductor portions 31 and 32. The conductor portions 31 and 32 are in a substantially rectangular plate shape. The conductor portions 31 and 32 are, for example, in the same shape. The conductor portion 31 is disposed in the recess 21. The conductor portion 32 is disposed in the recess 22.

[0048] The mounting conductor 4 is formed by stacking a plurality of mounting conductor layers 14 in an L-shape when viewed from the direction D3 in the direction D3. In the actual mounting conductor 4, the plurality of mounting conductor layers 14 are integrated to such an extent that the boundaries between the layers cannot be identified. The mounting conductor 4 has integrally formed conductor portions 41 and 42. The conductor portions 41 and 42 are in a substantially rectangular plate shape. The conductor portions 41 and 42 are, for example, in the same shape. The conductor portion 41 is disposed in the recess 23. The conductor portion 42 is disposed in the recess 24.

[0049] The plurality of coil conductors 5c, 5d, 5e, 5f are connected to each other to form a coil 10 in the element body 2. The coil conductors 5c, 5d, 5e, 5f are arranged so that at least a portion overlaps with each other when viewed from the direction D3. The coil conductors 5c, 5d, 5e, 5f are arranged separately from the end faces 2a, 2b and the side faces 2c, 2d, 2e, 2f.

[0050] The coil conductor 5c constitutes one end of the coil 10. One end of the coil conductor 5c and the connecting conductor 6 are adjacent to each other in the direction D1 and are connected to each other. The other end of the coil conductor 5c and one end of the coil conductor 5d are adjacent to each other in the direction D3 and are connected to each other. The other end of the coil conductor 5d and one end of the coil conductor 5e are adjacent to each other in the direction D3 and are connected to each other. The other end of the coil conductor 5e and one end of the coil conductor 5f are adjacent to each other in the direction D3 and are connected to each other. The other end of the coil conductor 5f and the connecting conductor 7 are adjacent to each other in the direction D1 and are connected to each other.

[0051] The coil conductors 5c, 5d, 5e, 5f are formed by stacking a plurality of coil conductor layers 15c, 15d, 15e, 15f in the direction D3. That is, the plurality of coil conductor layers 15c, 15d, 15e, 15f are arranged so as to overlap each other when viewed from the direction D3. The coil conductors 5c, 5d, 5e, 5f may also be formed by a single coil conductor layer 15c, 15d, 15e, 15f. In addition, Figure 3 Only one coil conductor layer 15c, 15d, 15e, 15f is shown in the figure. In the actual coil conductors 5c, 5d, 5e, 5f, a plurality of coil conductor layers 15c, 15d, 15e, 15f are integrated to such an extent that the boundaries between the layers cannot be recognized.

[0052] The connection conductor 6 extends along the direction D1 and is connected to the coil conductor 5c and the conductor portion 42 of the coil 10. The connection conductor 7 extends along the direction D1 and is connected to the coil conductor 5f and the conductor portion 32. The connection conductors 6 and 7 are formed by stacking a plurality of connection conductor layers 16 and 17 in the direction D3. Figure 3In the figure, only one connection conductor layer 16, 17 is shown. In actual connection conductors 6, 7, a plurality of connection conductor layers 16, 17 are integrated to such an extent that the boundaries between the layers cannot be recognized.

[0053] The above-mentioned mounting conductor layers 13, 14, coil conductor layers 15c, 15d, 15e, 15f, and connecting conductor layers 16, 17 are composed of conductors containing silver and quartz powder. These layers can also be composed of the same material or different materials. These layers have a rectangular cross-section. In addition, the "rectangular cross-section" of the present embodiment refers to a portion extending in a specified direction, in which the shape of the cross-section when cut along a surface perpendicular to the direction is rectangular. In addition, the "rectangle" of the present embodiment is not limited to a shape (rectangle or square) surrounded by four straight lines and all four corners are right angles. If it presents a roughly rectangular outline, the relative straight lines may not be parallel, part or all of the straight lines may be bent, the corners may not be right angles, or the corners may be rounded.

[0054] The laminated coil component 1 includes a plurality of layers La, Lb, Lc, Ld, Le, and Lf. The laminated coil component 1 is formed by, for example, stacking two layers La, one layer Lb, three layers Lc, three layers Ld, three layers Le, three layers Lf, one layer Lb, and two layers La in sequence from the side 2f. In addition, Figure 3 In the figure, three layers Lc, three layers Ld, three layers Le, and three layers Lf are each shown one by one, and the other two are omitted.

[0055] The layer La is composed of the element layer 12a.

[0056] The layer Lb is formed by combining the element layer 12b and the mounting conductor layers 13 and 14. The element layer 12b is provided with a shape corresponding to the shape of the mounting conductor layers 13 and 14 and filling the missing portion Rb of the mounting conductor layers 13 and 14. The element layer 12b and the mounting conductor layers 13 and 14 are in a complementary relationship as a whole.

[0057] The layer Lc is formed by combining the element layer 12c and the mounting conductor layers 13, 14 and the coil conductor layer 15c. The element layer 12c is provided with a shape corresponding to the shapes of the mounting conductor layers 13, 14 and the coil conductor layer 15c, and a missing portion Rc that fills the mounting conductor layers 13, 14, the coil conductor layer 15c and the connecting conductor layer 16. The element layer 12c and the mounting conductor layers 13, 14, the coil conductor layer 15c and the connecting conductor layer 16 have a complementary relationship as a whole.

[0058] The layer Ld is formed by combining the element layer 12d and the mounting conductor layers 13, 14 and the coil conductor layer 15d. The element layer 12d is provided with a shape corresponding to the shape of the mounting conductor layers 13, 14 and the coil conductor layer 15d, and a missing portion Rd is filled in the mounting conductor layers 13, 14 and the coil conductor layer 15d. The element layer 12d and the mounting conductor layers 13, 14 and the coil conductor layer 15d are in a complementary relationship as a whole.

[0059] The layer Le is formed by combining the element layer 12e and the mounting conductor layers 13, 14 and the coil conductor layer 15e. The element layer 12e is provided with a shape corresponding to the shape of the mounting conductor layers 13, 14 and the coil conductor layer 15e, and a missing portion Re is filled in the mounting conductor layers 13, 14 and the coil conductor layer 15e. The element layer 12e and the mounting conductor layers 13, 14 and the coil conductor layer 15e are in a complementary relationship as a whole.

[0060] The layer Lf is formed by combining the element layer 12f with the mounting conductor layers 13, 14, the coil conductor layer 15f, and the connection conductor layer 17. The element layer 12f is provided with a shape corresponding to the shapes of the mounting conductor layers 13, 14, the coil conductor layer 15f, and the connection conductor layer 17, and a missing portion Rf is filled in the mounting conductor layers 13, 14, the coil conductor layer 15f, and the connection conductor layer 17. The element layer 12f and the mounting conductor layers 13, 14, the coil conductor layer 15f, and the connection conductor layer 17 are in a complementary relationship as a whole.

[0061] The defective portions Rb, Rc, Rd, Re, and Rf are integrated to form the above-mentioned recessed portions 21, 22, 23, and 24. The width of the defective portions Rb, Rc, Rd, Re, and Rf (hereinafter, the width of the defective portions) is set to be substantially wider than the width of the mounting conductor layers 13 and 14, the coil conductor layers 15c, 15d, 15e, and 15f, and the connection conductor layers 16 and 17 (hereinafter, the width of the conductor portion). In order to improve the adhesion of the element layers 12b, 12c, 12d, 12e, and 12f, the mounting conductor layers 13 and 14, the coil conductor layers 15c, 15d, 15e, and 15f, and the connection conductor layers 16 and 17, the width of the defective portions may be set to be narrower than the width of the conductor portion. The value of the width of the defective portion minus the width of the conductor portion may be, for example, greater than -3 μm and less than 10 μm, or greater than 0 μm and less than 10 μm.

[0062] (Method for manufacturing laminated coil component)

[0063] Reference Figure 4 , Figure 5 A~5G, Figure 6A and 6B illustrate a method for manufacturing the laminated coil component 1 according to the embodiment. Figure 4 This is a flowchart showing the method for manufacturing the laminated coil component according to the first embodiment. Figure 5 A~5G, Figure 6 6A and 6B are cross-sectional views conceptually showing the method for manufacturing the laminated coil component according to the first embodiment. Figure 5 A~5G, Figure 6 The cross-sectional views of A and 6B are conceptual views and may not necessarily correspond to the actual cross-sectional views of the laminated coil component 1. Figure 1 To.

[0064] First, if Figure 5 As shown in FIG. 1A, a body forming layer 21 is formed on a substrate 20 (step S1). The substrate 20 is, for example, a PET film. The body forming layer 21 is formed, for example, by applying a body paste containing a photosensitive organic component to which the constituent materials of the above-mentioned body layers 12a to 12f are added on the substrate 20. The photosensitive organic component contained in the body paste may be either a negative type or a positive type, and a known component may be used.

[0065] Then, if Figure 5 As shown in FIG. 2B , the element forming layer 21 is exposed and developed by photolithography using, for example, a Cr mask, and an element pattern 22 is formed on the substrate 20 from which a shape corresponding to the shape of the conductor pattern 32 described later is removed (step S2). The element pattern 22 is a layer that becomes the element layers 12b to 12f after the heat treatment. That is, in step S2, an element pattern 22 is formed in which defect portions 23 that become defect portions Rc, Rd, Re, and Rf are provided. In addition, the "photolithography" of this embodiment is any method that is used as long as a layer of a processing object containing a photosensitive organic component is exposed and developed to form a desired pattern, and there is no limitation on the type of mask, etc.

[0066] On the other hand, Figure 5 As shown in FIG. 3C, a conductor forming layer 31 is formed on a substrate 30 (step S3). The substrate 30 is, for example, a PET film. The conductor forming layer 31 is formed by applying the above-mentioned photosensitive conductor paste on the substrate 30. Figure 5 As shown in FIG. 2 , for example, the conductor forming layer 31 is exposed and developed by photolithography using a Cr mask to form a conductor pattern 32 on the substrate 30 (step S4). The conductor pattern 32 is a layer that becomes the mounting conductor layers 13 and 14, the coil conductor layers 15c, 15d, 15e, 15f, and the connection conductor layers 16 and 17 after heat treatment.

[0067] Then, if Figure 5As shown in step E, the element body forming layer 21 formed in the above step S1 is transferred from the substrate 20 to the support 40 (step S5). By repeating step S5 multiple times, a plurality of element body forming layers 21 can be stacked on the support 40. In this embodiment, by repeating step S5 twice, two layers of element body forming layers 21 are stacked on the support 40. These element body forming layers 21 are layers that become layers La after heat treatment.

[0068] Next, the conductor pattern 32 and the element pattern 22 are repeatedly transferred onto the support 40 to stack the conductor pattern 32 and the element pattern 22 in the direction D3. Figure 5 As shown in FIG. 5 , the conductor pattern 32 formed in the above step S4 is transferred from the substrate 30 to the element forming layer 21 transferred in the above step S5 (step S6). Figure 5 As shown in FIG. 1 , the element body pattern 22 formed in the above step S2 is transferred from the substrate 20 to the element body forming layer 21 transferred in the above step S5 (step S7). The conductor pattern 32 transferred to the element body forming layer 21 in the above step S6 is filled in the defective portion 23 of the element body pattern 22, and the element body pattern 22 and the conductor pattern 32 become the same layer.

[0069] In addition, if Figure 6 As shown in A, the above-mentioned steps S6 and S7 are repeatedly performed to stack the element pattern 22 and the conductor pattern 32 in a state of being combined with each other (step S8). Thus, the layers Lb, Lc, Ld, Le, and Lf are stacked after heat treatment. In addition, in the above-mentioned step S8, it is not necessarily necessary to repeat the above-mentioned steps S6 and S7 one by one. For example, the above-mentioned step S6 may be repeated more than the above-mentioned step S7. Thus, for example, the conductor pattern 32 corresponding only to the mounting conductor layers 13 and 14 may be additionally transferred relative to the element pattern 22. Next, as Figure 6 As shown in FIG. 1B, the element body forming layer 21 formed in the above step S1 is transferred from the substrate 20 to the layer stacked in the above step S8 (step S9). By repeating step S9 multiple times, multiple element body forming layers 21 can be stacked on the layer. In this embodiment, by repeating the process twice, two layers of element body forming layers 21 are stacked on the layer from the substrate 20. These element body forming layers 21 are layers that become layers La after heat treatment.

[0070] Through the above, the laminated body 50 constituting the laminated coil component 1 after heat treatment is formed on the support body 40. In addition, for example, a layer or a colored layer with a cutting mark or a mark indicating the directionality of the chip (laminated coil component 1) can be further laminated as needed to form the laminated body 50.

[0071] Next, the obtained laminated body 50 is cut into a predetermined size (step S10 ).

[0072] Then, the cut laminate 50 is subjected to a binder removal process and then to a heat treatment (step S11). The heat treatment temperature is, for example, about 850 to 900°C. Thus, the laminated coil component 1 is obtained. The mounting conductors 3 and 4 may be subjected to electroplating or electroless plating as required.

[0073] After the heat treatment step S11, the photosensitive conductor paste becomes a conductor pattern composed of silver containing quartz powder. It is not necessary that all the quartz powder is present inside the conductor pattern, and a part of the quartz powder may be partially exposed from the surface of the conductor pattern. Figure 1 As shown in the electron microscope photograph of , since the heat treatment temperature in the heat treatment step S11 is lower than the melting point of quartz, the quartz powder in the photosensitive conductor paste does not melt and can maintain its shape. In addition, not only does the quartz powder not fuse with each other, but also the dispersed state of the quartz powder in the photosensitive conductor paste can be maintained even after the heat treatment step S11.

[0074] On the other hand, when the photosensitive conductor paste contains glass powder as an inorganic additive, since the softening point of glass (e.g., about 800° C.) is lower than the melting point of quartz, there is a risk that the heat treatment temperature in the heat treatment step S11 will be higher than the softening point of glass. Figure 7 As shown in FIG. 1 , the glass powder in the photosensitive conductor paste softens. Figure 7 In the figure, the black area around the glass is a phase (heterogeneous phase) in which the glass component is solid-dissolved in the conductive component. The glass powder does not maintain its shape after the heat treatment process, but becomes spherical. In addition, as a result of the softening of the glass powder, the glass powders also aggregate with each other, and the dispersion state of the glass powder in the photosensitive conductor paste is not maintained. In addition, when the photosensitive conductor paste contains quartz powder as an inorganic additive, the thickness of the heterogeneous phase at the interface with the conductive component is narrow, less than 10μm, and can also be less than 6μm.

[0075] Next, the mounting conductors 3 and 4 are subjected to electroplating or electroless plating as necessary to form a plating layer on the outer surfaces of the mounting conductors 3 and 4. In this way, the laminated coil component 1 is obtained.

[0076] As described above, in the photosensitive conductor paste involved in the present embodiment, melting of quartz powder does not occur or is extremely difficult to occur in the heat treatment step S11, and the heat treatment step S11 is fully exerted in a manner that makes the shrinkage rates and shrinkage behaviors of the conductor layer and the element layer close when they shrink. Therefore, the generation of voids can be suppressed when used for the manufacture of the stacked coil component 1.

[0077] In the present embodiment, the body pattern and the conductor pattern are both formed by photolithography, and therefore, the body pattern and the conductor pattern can be formed with higher precision than when they are formed by printing, for example.

[0078] [Second embodiment]

[0079] Reference Figure 8 and Fig. 9 A to 9E describe a method for manufacturing the laminated coil component 1 according to the second embodiment. Figure 8 This is a flowchart showing a method for manufacturing a laminated coil component according to the second embodiment. Fig. 9 A to 9E are cross-sectional views conceptually showing the method for manufacturing the laminated coil component according to the second embodiment. Fig. 9 The cross-sectional views A to 9E are conceptual views and do not necessarily correspond to the actual cross-sectional views of the laminated coil component 1 . Figure 1 The laminated coil component 1 manufactured by the manufacturing method according to the second embodiment and the laminated coil component 1 manufactured by the manufacturing method according to the first embodiment have the same structure.

[0080] In the manufacturing method according to the second embodiment, first, Fig. 9 As shown in FIG. 1A, a body forming layer 21 is formed on a support 40 (step S21). The body forming layer 21 is formed by, for example, applying a body paste to the surface of the support 40. In the present embodiment, step S21 is performed twice to stack two layers of the body forming layer 21. These body forming layers 21 are layers that become layers La after heat treatment.

[0081] Then, if Fig. 9 As shown in step B, a conductor forming layer 31 is formed on the element forming layer 21 (step S22). The conductor forming layer 31 is formed by applying the above-mentioned photosensitive conductor paste on the element forming layer 21. Fig. 9 As shown in FIG. 3 , for example, the conductor forming layer 31 is exposed and developed by photolithography using a Cr mask to form a conductor pattern 32 on the element forming layer 21 (step S23). The conductor pattern 32 is a layer that becomes the mounting conductor layers 13 and 14, the coil conductor layers 15c, 15d, 15e, 15f, and the connection conductor layers 16 and 17 after heat treatment.

[0082] Then, if Fig. 9 As shown in FIG. 2D , a new element formation layer 21 is formed on the element formation layer 21 so as to cover the conductor pattern 32 provided on the element formation layer 21 (step S24 ). The newly formed element formation layer 21 is formed so as to fill the periphery of the conductor pattern 32 .

[0083] Then, if Fig. 9As shown in E, the newly formed element formation layer 21 is patterned by photolithography using a Cr mask, for example (step S25). The conductor pattern 32 formed in the above step S23 is filled in the defective portion 23 of the element pattern 22, and the element pattern 22 and the conductor pattern 32 are formed in the same layer.

[0084] Then, the above-mentioned steps S22, S23 and steps S24, S25 are repeatedly performed. Figure 6 As shown in the structure of A, the element pattern 22 and the conductor pattern 32 are stacked in a state of being combined with each other. (Step S26) In the above step S26, steps S22, S23 and steps S24, S25 do not necessarily need to be repeated one by one. For example, the above steps S22, S23 may be repeated more than the above steps S24, S25. Thus, for example, the conductor pattern 32 corresponding only to the mounting conductor layers 13, 14 may be additionally transferred to the element pattern 22. Next, since it is set Figure 6 B, so a new element body forming layer 21 is formed on the layer stacked in the above step S26. (Step S27) By repeating step S27 multiple times, multiple element body forming layers 21 can be stacked on the layer. In this embodiment, by repeating it twice, two layers of element body forming layers 21 are stacked on the layer from the substrate 20. These element body forming layers 21 are layers that become layers La after heat treatment.

[0085] Through the above, the laminated body 50 constituting the laminated coil component 1 after heat treatment is formed on the support body 40. Next, as in the first embodiment, the obtained laminated body 50 is cut into a predetermined size (step S28), and then, after the cut laminated body 50 is subjected to a binder removal process, a heat treatment is performed (step S29). Thus, the laminated coil component 1 is obtained.

[0086] As described above, in the second embodiment, as in the first embodiment, a photosensitive conductor paste is used. Therefore, melting of the quartz powder does not occur or is extremely difficult to occur in the heat treatment step S29. The heat treatment step S29 is fully utilized in a manner that makes the shrinkage rates and shrinkage behaviors of the conductor layer and the element layer close when they shrink. Therefore, the generation of voids can be suppressed when used for the manufacture of the stacked coil component 1.

[0087] The present disclosure is not limited to the above-described embodiments, and various modifications are possible.

[0088] The body pattern and the conductor pattern may be formed by printing, for example, instead of photolithography. The body pattern and the conductor pattern do not necessarily need to be formed on different substrates, and may be formed on a common substrate if the body pattern and the conductor pattern are separated from each other.

[0089] In the above-mentioned first embodiment and second embodiment, the stacked coil component 1 is described as an example of a stacked electronic component, but the present disclosure is not limited to this and can also be applied to the manufacturing method of other electronic components such as stacked ceramic capacitors, stacked resistors, stacked piezoelectric actuators, stacked thermistors, or stacked composite components.

Claims

1. A photosensitive conductor paste, wherein: Contains photosensitive organic components, conductor powder and quartz powder. The photosensitive conductor paste does not contain glass, The median particle size of the quartz powder is 0.4 to 5.0 μm. The conductor powder is silver powder, and the addition ratio of the quartz powder to the silver powder is 0.5-2.5wt%.

2. The photosensitive conductor paste according to claim 1, wherein The median particle size of the conductor powder is greater than the median particle size of the quartz powder.

3. A laminated electronic component, wherein: A laminated structure including a plurality of element layers having defective portions with rectangular cross sections and a plurality of conductor layers filling the defective portions of the plurality of element layers. The conductor layer is composed of a conductor containing quartz powder. The conductor layer is formed by using a photosensitive conductor paste containing a photosensitive organic component, a conductor powder and the quartz powder. The photosensitive conductor paste does not contain glass, The median particle size of the quartz powder is 0.4 to 5.0 μm. The conductor powder is silver powder, and the addition ratio of the quartz powder to the silver powder is 0.5-2.5wt%.

4. The laminated electronic component according to claim 3, wherein: The plurality of conductor layers constitute a coil.

5. The laminated electronic component according to claim 3 or 4, wherein: The element layer is made of a material containing a glass component.

6. A method for manufacturing a laminated electronic component, wherein: Include: a step of forming a laminated body, the laminated body comprising a plurality of element patterns stacked and each having a defect portion having a rectangular cross section, and a plurality of conductor patterns filling the defect portions of each of the plurality of element patterns; as well as a step of heat-treating the laminate so that the element pattern becomes an element layer and the conductor pattern becomes a conductor layer, The conductor pattern is formed by photolithography using a photosensitive conductor paste containing a photosensitive organic component, a conductor powder and a quartz powder. The photosensitive conductor paste does not contain glass, The median particle size of the quartz powder is 0.4 to 5.0 μm. The conductor powder is silver powder, and the addition ratio of the quartz powder to the silver powder is 0.5-2.5wt%.