A fiber optic sensor for simultaneously monitoring steel bar stress and corrosion rate

Through the combination of long-period fiber grating and Fabry-Platinol cavity, the stress and corrosion rate of the steel bars are monitored, and the problems of insufficient monitoring complexity and sensitivity in the existing technology are solved, real-time, lossless steel bar state evaluation and structure are achieved Safety guarantee.

CN113804612BActive Publication Date: 2024-11-26DALIAN UNIV OF TECH
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202111057321.1
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2021-09-09
Publication Date
2024-11-26
Estimated Expiration
2041-09-09

AI Technical Summary

Technical Problem

The prior art is difficult to efficiently monitor the stress and corrosion rate of steel bars simultaneously. The steel bar stress gauge is complex in installation and limited range, while the corrosion monitoring method is inconvenient to operate and is not suitable for civil engineering structures.

Method used

Using a fiber sensor combined with a long-period fiber grating (LPFG) and a Fabry-Parole cavity, the corrosion degree and strain of the steel bar surface can be measured in real time by monitoring the changes in the refractive index and cavity length, thereby reflecting the corrosion and stress of the steel bar. state.

Benefits of technology

It realizes lossless and real-time monitoring of steel bar stress and corrosion rate, provides a basis for evaluation of steel bar performance status and structural safety, has high sensitivity and large-scale measurement capabilities, is small in size and strong anti-interference, and is suitable for monitoring of civil engineering structures.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN113804612B_ABST
    Figure CN113804612B_ABST
Patent Text Reader

Abstract

The invention belongs to the field of structural health monitoring technology or sensor technology, and discloses a fiber optic sensor for simultaneously monitoring steel bar stress and corrosion rate, including a transmission optical fiber, a capillary steel bar tube, a long-period fiber grating, a flexible waterproof sealing material, an external sleeve, a reflective mirror, a connecting key, a first clamp, and a second clamp. The sensor comprehensively utilizes the Fabry-Platinum cavity and the long-period fiber grating, and indirectly monitors the stress and corrosion rate of the steel bar by simultaneously monitoring the changes in the reflection spectrum signals of the Fabry-Platinum cavity and the long-period fiber grating under different steel bar corrosion rates and steel bar stress conditions. The sensor can realize long-term, non-destructive, and real-time simultaneous monitoring of the stress and corrosion rate of the steel bar, and has high measurement accuracy and a large range. It has the advantages of relatively simple manufacture, small size, high strength, and high sensitivity. The sensor has broad application prospects and is easy to promote.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to an optical fiber sensor for simultaneously monitoring steel bar stress and corrosion rate, and belongs to the technical field of structural health monitoring or sensor technology. Background Art

[0002] As one of the most widely used civil engineering materials in the world today, steel bars have many advantages such as high strength, high plasticity and toughness, and easy manufacturing. Their high tensile properties can well adapt to the high compressive properties of concrete, which is an important reason why reinforced concrete structures are widely used in civil construction.

[0003] However, due to the nature of the work of civil engineering structures during their service, they are very likely to be exposed to corrosive environments, such as marine environments such as docks, seaports, and cross-sea bridges. Even for civil engineering structures that only work in ordinary atmospheric environments, as the service time goes by, concrete cracks develop, and corrosive ions continue to enter and destroy the passivation film of the steel bars, it will also cause corrosion of the steel bars. Steel bar corrosion is one of the important factors in the durability failure of concrete structures. If the corrosion of steel bars in civil structures can be reasonably monitored, it will provide an important basis for the durability assessment of the structure, the prediction of the remaining life of the structure, and the reinforcement and maintenance of the structure.

[0004] Secondly, as one of the important stress-bearing parts in a component, the stress value of the steel bar can reflect the working state of the stress-bearing component. Generally speaking, if the stress value of the steel bar section at a certain place or even several places in a certain component in the structure is greater than the design value, it means that the structure is already in a stress state beyond the design. However, the working state of the component and whether there will be danger require reference to the accurate real-time stress of the steel bar for analysis. Therefore, if the stress value of the steel bar can be accurately monitored in real time, it can provide an important basis for the working state and safety assessment of the structure.

[0005] At present, the monitoring methods of steel bar corrosion are mainly divided into two categories: electrochemical methods and non-electrochemical methods. Electrochemical methods include: AC impedance method, linear polarization method, electrochemical noise method, etc. Non-electrochemical methods include: surface inspection method, weight loss method, ultrasonic method, etc. However, the above methods generally have the disadvantages of inconvenient operation, complicated monitoring process, and unsuitability for monitoring steel bar corrosion in civil engineering structures. The current monitoring method of steel bar stress is mainly to measure steel bar stress with the help of steel bar stress gauge, but it has the disadvantages of complex installation and limited range.

[0006] In recent years, fiber optic sensors have gradually been used to measure corrosion and stress of steel due to their advantages such as small size, light weight, resistance to electromagnetic interference, strong corrosion resistance, high monitoring accuracy and real-time continuous monitoring.

[0007] Therefore, the present invention creatively proposes an optical fiber sensor for simultaneously monitoring the stress and corrosion rate of steel bars, which is expected to provide a new idea and method for monitoring the stress and corrosion rate of steel bars in current civil engineering structures. Summary of the invention

[0008] In order to solve the above technical problems, the present invention proposes a fiber optic sensor for simultaneously monitoring the stress and corrosion rate of steel bars. The biggest feature of this sensor is that it uses a long period fiber grating (LPFG) in series with a Fabry-Platt cavity to simultaneously monitor the refractive index change of the medium around the LPFG and the change of the cavity length of the Fabry-Platt cavity, and indirectly measures the corrosion degree of the monitored steel bar surface and the steel bar strain, and can further accurately reflect the corrosion and stress state of the steel bar. At the same time, this fiber optic sensor is simple to make, and can simultaneously monitor the stress and corrosion rate of steel bars in a non-destructive and real-time manner, thereby providing a basis for reasonably evaluating the performance status of steel bars, ensuring the normal performance of the steel bar force, and further ensuring the safety of the structure.

[0009] The technical solution of the present invention:

[0010] An optical fiber sensor for simultaneously monitoring steel bar stress and corrosion rate, characterized in that the optical fiber sensor comprises a transmission optical fiber (1), a capillary steel bar tube (3), a long period optical fiber grating (4), a flexible waterproof sealing material (5), an external sleeve (6), a reflective mirror (8), a first clamp (11), a second clamp (13), and a connecting key (7)(9)(15);

[0011] One end of the transmission optical fiber (1) is connected to a spectrometer, and the other end serves as a first reflection surface (12) corresponding to a reflection mirror surface (8) whose end serves as a second reflection surface, thereby forming a Fabry-Platt cavity (14); a long-period fiber grating (4) is written on the transmission optical fiber (1), and the long-period fiber grating (4) is located in the capillary steel tube (3);

[0012] The capillary steel tube (3) is sleeved on the outside of the transmission optical fiber (1), and a cavity (2) of suitable size is provided between the two.

[0013] The outer sleeve (6) is sleeved on the outside of the capillary steel tube (3) and the reflective mirror surface (8);

[0014] The flexible waterproof sealing material (5) is sealed at the connection between the capillary steel tube (3) and the external sleeve (6);

[0015] The wall thickness of the capillary steel tube (3) can be adjusted according to the specific requirements for the sensitivity of steel corrosion monitoring and service life;

[0016] The inner diameter of the outer sleeve (6) is equal to the outer diameter of the capillary steel tube (3), that is, the two are tightly sheathed and connected together under the premise of not affecting the deformation of the sensor.

[0017] The connecting keys (7) (9) (15) can be completed by 3D printing, laser welding or epoxy adhesive bonding;

[0018] The optical fiber sensor for simultaneously monitoring the stress and corrosion rate of a steel bar is fixed on the steel bar to be tested (10) via a first clamp (11) and a second clamp (13);

[0019] The flexible waterproof sealing material (5) is not too rigid to cause deformation that affects the optical fiber sensor, while ensuring sealing and waterproofing;

[0020] The long-period fiber grating (4) etched on the transmission optical fiber (1) monitors the refractive index of the external medium and further monitors the corrosion rate;

[0021] The manufacturing methods of the long-period fiber grating (4) and the reflecting mirror (8) can be adjusted according to specific conditions.

[0022] Working principle of the present invention:

[0023] After the light is incident through the transmission optical fiber 1, it first passes through the long-period fiber grating 4, and then reaches the Fabry-Perot cavity 14, where it is continuously reflected and transmitted between the two end faces of the Fabry-Perot interferometer cavity 14, forming multi-beam light interference. When the steel bar 10 to be tested is deformed by external forces, the capillary steel tube 3 and the external sleeve 6 attached to its surface will cause the length of the Fabry-Perot cavity 14 to change. The change in the distance between the two measuring points on the steel bar 10 to be tested is equal to the change in the length of the Fabry-Perot cavity 14. The change in the cavity length will cause the shape of the spectrum obtained by the optical fiber demodulator to change. The free spectral range (FSR) in the spectrum diagram has the following relationship with the cavity length L:

[0024]

[0025] Where n is the refractive index of the medium, λ is the wavelength of light, and L is the cavity length. The refractive index of the medium is minimally affected by the change in cavity length and can be ignored. It can be further deduced that:

[0026]

[0027] The steel bar strain ε to be measured can be obtained by dividing the cavity length change ΔL of the Fabry-Platt interferometer cavity 14 by the distance between the two measuring points, as shown in the following formula. The smaller the distance between the two measuring points, the larger the strain monitoring range. Therefore, if the distance between the two measuring points is at the millimeter level, the range can reach tens of thousands of microstrains, or even hundreds of thousands of microstrains.

[0028]

[0029] Among them, ΔL is the change in the distance between the two measuring points, and L is the distance between the two measuring points.

[0030] After measuring the strain, the stress σ of the steel bar can be calculated using the following formula.

[0031] σ=Eε (4)

[0032] Where E is the elastic modulus of the steel bar being tested.

[0033] The LPFG grating is engraved on the optical fiber, forming a periodic refractive index modulation over a grating length of several centimeters. The grating couples the incident light from the propagating core mode to the co-propagating cladding mode, generating a series of attenuation bands of the transmission spectrum. The center (resonance) wavelength of the spectral attenuation band can be expressed in the following way.

[0034]

[0035] Where λ0 is the resonant wavelength, is the effective refractive index of the fiber core, is the effective refractive index of the cladding mode LP0m, which is related to the refractive index of the core n1, cladding n2, and surrounding medium n3, and Λ is the period of the grating. The ambient refractive index n3 reflects the overall optical properties of the surrounding medium environment, which depends on the type and concentration of different media. In the working situation of the present invention, the refractive index of the core n1 and cladding n2 remains unchanged.

[0036] Therefore, once external corrosion penetrates the capillary steel tube wall 3, due to the presence of corrosion products, the optical properties of the medium in the cavity 2 will change immediately, causing the resonant wavelength of the light signal received on the spectrometer to shift. By setting different capillary steel tube wall thicknesses, since the capillary steel tube material is exactly the same as the monitored steel bar, the corrosion rate of the steel bar can be inferred from the time when the resonant wavelength shifts. For example: if the capillary steel tube wall is set to 1mm, and after 500 days, the resonant wavelength in the spectrometer is found to shift, it can be concluded that the steel bar corrosion rate is 2μm / day.

[0037] The signal caused by the change of the Fabry-Platinum cavity length has a high spatial frequency characteristic, while the change of the LPFG feedback signal caused by the change of the refractive index of the external medium has a low spatial frequency characteristic. In layman's terms, during the monitoring process: the signal fed back by the Fabry-Platinum cavity is a rapidly changing stripe, as shown in Figure (a) of the spectrum diagram, while the signal fed back by the long-period fiber grating is a slowly changing envelope, and the place where the envelope suddenly drops is where the resonant wavelength is located, as shown in Figure (b) of the spectrum diagram. In summary, when the two are output at the same time and superimposed on a spectrum diagram, the shape is as shown in Figure (c) of the spectrum diagram, that is, the output is a superposition of the slowly changing envelope generated by the long-period fiber grating (LPFG) and the rapidly changing stripes generated by the Fabry-Platinum cavity. It is not difficult to find that filters can be used to separate them to obtain the change of the free spectral range representing the stress information of the monitored steel bar and the shift of the resonant wavelength representing the corrosion rate information of the monitored steel bar. Thereby achieving simultaneous monitoring of the stress and corrosion rate of the monitored steel bar.

[0038] Beneficial effects of the present invention:

[0039] (1) The present invention can achieve high sensitivity of corrosion and large-range measurement of stress by setting the wall thickness of the capillary steel bar tube and the distance between the clamps.

[0040] (2) The present invention combines the use of Fabry-Platt cavity and long-period fiber grating to achieve continuous real-time monitoring of steel bar stress and corrosion rate.

[0041] (3) The present invention has a very small size. After being embedded in a structure and clamped on the steel bar with a clamp, it will not affect the normal operation of the steel bar being tested, and non-destructive monitoring can be achieved.

[0042] (4) The present invention uses a demodulator to infer the stress and corrosion rate of the steel bar from the spectrum, has strong anti-interference ability, and the monitoring result is more accurate.

[0043] (5) The present invention is relatively simple to manufacture, easy to use, and reasonably priced, suitable for promotion, and has a high application prospect. BRIEF DESCRIPTION OF THE DRAWINGS

[0044] Figure 1 The figure is a schematic diagram of the structure of the optical fiber sensor used for simultaneously monitoring the stress and corrosion rate of steel bars according to the present invention.

[0045] Figure 2 A schematic diagram of a capillary steel bar tube portion of an optical fiber sensor for simultaneously monitoring steel bar stress and corrosion rate according to the present invention;

[0046] Figure 3 A schematic diagram of an outer casing of an optical fiber sensor for simultaneously monitoring steel bar stress and corrosion rate according to the present invention;

[0047] Figure 4 It is a schematic diagram of the sealing structure at the connection between the outer sleeve of the optical fiber sensor and the capillary steel bar tube for simultaneously monitoring the stress and corrosion rate of the steel bar of the present invention;

[0048] Figure 5 The figure is a schematic diagram of the spectrum principle of the optical fiber sensor used for simultaneously monitoring the stress and corrosion rate of steel bars according to the present invention.

[0049] In the figure: 1 input optical fiber; 2 inner hole of capillary steel tube; 3 capillary steel tube; 4 long period fiber grating; 5 flexible waterproof sealing material; 6 outer sleeve; 7 connection key; 8 reflection mirror; 9 connection key; 10 steel bar to be tested; 11 first fixture; 12 first reflection surface; 13 second fixture; 14 Fabry-Platt cavity; 15 connection key; DETAILED DESCRIPTION

[0050] In order to make the purpose, features and advantages of the present invention more intuitive and easy to understand, the technical solutions in the embodiments of the present invention are clearly and completely described below in combination with the drawings in the embodiments of the present invention. Obviously, the embodiments described below are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0051] As shown in the schematic diagram, an optical fiber sensor for simultaneously monitoring steel bar stress and corrosion rate includes a transmission optical fiber 1, a capillary steel bar tube 3, a long period fiber grating 4, a flexible waterproof sealing material 5, an external sleeve 6, a reflective mirror 8, a connecting key 7, a connecting key 9, a connecting key 15, a first clamp 11, and a second clamp 13;

[0052] One end of the transmission optical fiber 1 is connected to the spectrometer, and the other end is used as a first reflection surface 12 corresponding to the reflection mirror surface 8 whose end is used as a second reflection surface, forming a Fabry-Platt cavity 14; a long period fiber grating 4 is written on the transmission optical fiber 1, and the long period fiber grating 4 is located in the capillary steel tube 3;

[0053] The capillary steel tube 3 is sleeved on the outside of the transmission optical fiber 1, and there is a cavity 2 of suitable size between the two, which contains air;

[0054] The outer sleeve 6 is sleeved on the outside of the capillary steel tube 3 and the reflective mirror surface 8;

[0055] The reflective mirror surface 8 can be prepared by polishing or metal ion sputtering;

[0056] The flexible waterproof sealing material 5 is sealed at the connection between the capillary steel tube 3 and the external sleeve 6 .

[0057] The optical fiber sensor for simultaneously monitoring steel bar stress and corrosion rate is characterized in that the capillary steel bar tube 3 is made of the same material as the steel bar to be measured, and its wall thickness can be adjusted according to the specific requirements for the sensitivity of steel bar corrosion monitoring.

[0058] The optical fiber sensor for simultaneously monitoring steel bar stress and corrosion rate is characterized in that the inner diameter of the outer sleeve 6 is equal to the outer diameter of the capillary steel bar tube 3, that is, the two are tightly connected together without affecting the deformation of the sensor.

[0059] The optical fiber sensor for simultaneously monitoring steel bar stress and corrosion rate is characterized in that the connecting keys 7, 9, 15 can be completed by 3D printing, laser welding or epoxy adhesive bonding.

[0060] The optical fiber sensor for simultaneously monitoring the stress and corrosion rate of a steel bar is fixed on the steel bar 10 to be tested by means of a first clamp 11 and a second clamp 13 .

[0061] The flexible waterproof sealing material 5 is provided with the premise of ensuring sealing and waterproofing, and the rigidity thereof is not too large to cause deformation affecting the optical fiber sensor.

[0062] The long-period fiber grating 4 etched on the transmission optical fiber 1 monitors the refractive index of the external medium and further monitors the corrosion rate.

[0063] The manufacturing methods of the long-period fiber grating 4 and the reflective mirror 8 can be adjusted according to specific conditions.

[0064] Step 1: Take an ordinary optical fiber and make a long-period fiber grating at a suitable position as shown in the schematic diagram. The specific production method and specific grating period are adjusted according to actual conditions.

[0065] Step 2: Based on the schematic diagram, use the same steel material as the monitored steel bar to make a capillary steel bar tube of a certain thickness.

[0066] Step 3: Put the capillary steel tube made in step 2 on the optical fiber in step 1. Note that the long-period fiber grating is located inside the capillary steel tube, and there is a cavity of suitable size between the capillary steel tube and the optical fiber. The initial medium inside the cavity is air (it can also be adjusted according to the actual situation of the monitoring requirements). Note that in combination with the schematic diagram, the optical fiber should leave enough length to protrude from the capillary steel tube in preparation for the future production of the Fabry-Platinum cavity.

[0067] Step 4: Combined with the schematic diagram, use the connection key to seal the capillary steel tube and the optical fiber completed in the previous step. Then make a stainless steel clamp to fix it to the outer wall of the capillary steel tube, which can be fixed by welding or bonding.

[0068] Step 5: Make a stainless steel outer sleeve with an inner diameter equal to the outer diameter of the capillary steel tube after the optical fiber is installed in the previous step, and put the outer sleeve on the outside of the capillary steel tube. Note that the sleeve stiffness should be appropriate and should not affect the deformation of the sensor in the future. Make a stainless steel clamp to fix it to the outer wall of the sleeve, which can be fixed by welding or bonding.

[0069] Step 6: Combined with the schematic diagram, use waterproof sealing material to seal the connection between the outer sleeve and the capillary steel tube. Note that the sealing stiffness should be appropriate and should not affect the deformation of the sensor in the future.

[0070] Step 7: Measure the distance between the two fixtures. During production, the specific distance between the two fixtures can be adjusted according to the monitoring range requirements.

[0071] Step 8: Fix the two clamps of the sensor on the surface of the steel bar to be monitored. The fixing method can be welding, gluing, or opening holes of appropriate size on the surface of the steel bar to be monitored, and then inserting the clamps to fix them. However, it is necessary to ensure that the relative displacement of the clamps can accurately reflect the relative movement of the two points where the clamps are located on the monitored steel bar.

[0072] Step 9: Connect an external optical fiber demodulator to continuously monitor the spectral signal and the corrosion and stress state of the steel bars.

[0073] Step 10: You can select a steel bar, make and connect the sensor according to the above requirements, place the steel bar in an accelerated corrosion environment, connect the optical fiber to an external demodulator, continuously monitor the optical fiber signal, calculate the stress change and the relationship between the corrosion rate and the spectral signal, and complete the laboratory calibration.

[0074] Step 11: embed the calibrated sensor into the structure to be monitored and fix it on the steel bar to be monitored to monitor the steel bar corrosion rate and stress.

[0075] The above embodiments are only used to illustrate the technical solutions of the present invention, rather than to limit the same. Although the present invention has been described in detail with reference to the aforementioned embodiments, those skilled in the art should understand that the technical solutions described in the aforementioned embodiments may still be modified, or some of the technical features may be replaced by equivalents. However, these modifications or replacements do not deviate the essence of the corresponding technical solutions from the spirit and scope of the technical solutions of the embodiments of the present invention.

Claims

1. An optical fiber sensor for simultaneously monitoring steel bar stress and corrosion rate, characterized in that: The optical fiber sensor comprises a transmission optical fiber (1), a capillary steel tube (3), a long period optical fiber grating (4), a flexible waterproof sealing material (5), an external sleeve (6), a reflective mirror (8), a connecting key (7) (9) (15), a first clamp (11), and a second clamp (13); One end of the transmission optical fiber (1) is connected to a spectrometer, and the other end serves as a first reflection surface (12) corresponding to a reflection mirror surface (8) whose end serves as a second reflection surface, thereby forming a Fabry-Platt cavity (14); a long-period fiber grating (4) is written on the transmission optical fiber (1), and the long-period fiber grating (4) is located in the capillary steel tube (3); The capillary steel tube (3) is sleeved on the outside of the transmission optical fiber (1), and there is a cavity (2) of suitable size between the two, which contains air or other media; The capillary steel tube (3) is made of the same material as the steel bar to be tested, and its wall thickness can be adjusted according to the specific requirements for the sensitivity of steel bar corrosion monitoring; The outer sleeve (6) is sleeved on the outside of the capillary steel tube (3) and the reflective mirror surface (8); The inner diameter of the outer sleeve (6) is equal to the outer diameter of the capillary steel tube (3), that is, the two are tightly connected together without affecting the deformation of the sensor; The flexible waterproof sealing material (5) is sealed at the connection between the capillary steel tube (3) and the external sleeve (6).

2. The optical fiber sensor for simultaneously monitoring steel bar stress and corrosion rate according to claim 1, characterized in that: The connecting keys (7) (9) (15) can be completed by 3D printing, laser welding or epoxy adhesive bonding.

3. The optical fiber sensor for simultaneously monitoring steel bar stress and corrosion rate according to claim 1, characterized in that: The optical fiber sensor for simultaneously monitoring the strain and corrosion rate of a steel bar is fixed on the steel bar (10) to be tested via a first clamp (11) and a second clamp (13).

4. The optical fiber sensor for simultaneously monitoring steel bar stress and corrosion rate according to claim 1, characterized in that: The flexible waterproof sealing material (5) is not too rigid to cause deformation that affects the optical fiber sensor, while ensuring sealing and waterproofing.

5. The optical fiber sensor for simultaneously monitoring steel bar stress and corrosion rate according to claim 1, characterized in that: The long-period fiber grating (4) etched on the transmission optical fiber (1) monitors the refractive index of the external medium and further monitors the corrosion rate.

6. The optical fiber sensor for simultaneously monitoring steel bar stress and corrosion rate according to claim 1, characterized in that: The manufacturing methods of the long-period fiber grating (4) and the reflecting mirror (8) can be adjusted according to specific conditions.