Glass article manufacturing device and manufacturing method
By setting a cover and a flow reduction mechanism at the upper end of the cylindrical part of the state adjustment groove, the problems of volatiles falling into and cooling pipe damage are solved, the quality and yield of glass products are improved, and the solution is achieved with low cost and light weight. plan.
Patent Information
- Application Number
- CN202080039106.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Priority Date
- 2019-07-03
- Filing Date
- 2020-06-23
- Publication Date
- 2024-11-05
- Estimated Expiration
- 2040-06-23
AI Technical Summary
During the manufacturing process of glass articles, the opening of the state adjustment groove opens to cause volatiles to adhere and fall into molten glass, affecting product quality and yield, and the cooling tube is susceptible to damage.
Design a glass article manufacturing device, which provides a cover at the upper end of the cylindrical portion of the state adjustment groove to cover the opening, and improves durability by covering the set piece with a platinum or platinum alloy, and combines the flow reduction mechanism and gas flow path design to prevent Volatiles fall into and cooling tubes are damaged.
It effectively inhibits the fall of volatiles into foreign matter in molten glass, improves the quality and yield of glass products, and reduces the probability of cooling pipe damage, achieving a low-cost and lightweight solution.
Smart Images

Figure CN113874331B_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to a manufacturing device and a manufacturing method for a glass article, and more particularly to an improvement of a state adjustment tank provided in a transfer device for transferring molten glass from a melting furnace to a forming device. Background Art
[0002] As is well known, the manufacturing device of glass articles comprises a melting furnace for generating molten glass from glass raw materials, a forming device for forming the molten glass, and a transfer device for transferring the molten glass flowing out of the melting furnace to the forming device. The transfer device is equipped with, for example, a clarification tank, a stirring tank, a state adjustment tank, etc. in sequence from the upstream side.
[0003] The clarification tank removes bubbles from the molten glass flowing out of the melting furnace. The stirring tank stirs the molten glass with a stirrer to homogenize it. The state adjustment tank mainly adjusts the viscosity and flow rate of the molten glass just before supplying the molten glass to the forming device.
[0004] Since the flow of molten glass in the state adjustment tank is easily stagnant, it is possible to cause devitrification (crystallization) around the liquid surface of the molten glass. In response to this problem, Patent Document 1 discloses that devitrification is suppressed by lowering the liquid surface of the molten glass in the state adjustment tank.
[0005] Prior art literature
[0006] Patent Literature
[0007] Patent Document 1: Japanese Patent Application Publication No. 2017-14067 Summary of the invention
[0008] Problems to be solved by the invention
[0009] In addition, in the state adjustment tank disclosed in patent document 1, the opening at the upper end is open. The opening serves as an insertion port for a plunger that blocks the downward flow of molten glass. In addition, the gas in the state adjustment tank (mainly the steam obtained by gasification of molten glass) is released to the outside from the opening. However, in the past, the actual situation was that no attention was paid to the released gas, and it was left as it was. This is because most of the bubbles in the molten glass are removed in the clarification tank, so the generation of gas based on bubbles in the state adjustment tank is a trace amount.
[0010] As a result of intensive studies, the present inventors have found that when molten glass is formed by a forming apparatus, various adverse effects may be caused by gas released from the opening of a state adjustment tank.
[0011] If one example of this drawback is described, tin oxide and the like as a clarifier remain in the molten glass in the state adjustment tank. When the opening at the upper end of the state adjustment tank is opened, the remaining tin oxide and the like volatilize, which may cause volatiles to adhere to the inner surface near the opening. In addition, the temperature near the opening is lowered by the influence of the external air, so that the volatiles are easily liquefied or solidified and adhered, and it is also easy to produce the state of condensation of the volatiles after the attachment. These situations affect each other, and the volatiles attached to the inner surface near the opening fall into the molten glass as time passes and become foreign matter. As a result, the quality of the glass products as products is reduced or the product yield rate is deteriorated.
[0012] From the above viewpoints, an object of the present invention is to avoid the adverse effects that may be caused by opening the opening of the state adjustment tank provided in the transfer device.
[0013] Solutions to Solve Problems
[0014] The first aspect of the present invention made to solve the above-mentioned problems is a manufacturing device for glass articles, wherein a transfer device for transferring molten glass from a melting furnace to a forming device is equipped with a state adjustment tank for adjusting the state of the molten glass, and the manufacturing device for glass articles is characterized in that the state adjustment tank comprises: a cylindrical portion whose central axis is along the up-down direction and has an opening at the upper end; and a cover body, which covers the opening of the cylindrical portion.
[0015] According to the manufacturing device of the glass article, in particular, when the forming device is utilized to form the molten glass, the opening of the cylindrical part is covered by the cover. Therefore, it is possible to avoid the drawbacks that may be caused by the opening of the cylindrical part. Specifically, even if the tin oxide etc. remaining in the molten glass in the state adjustment tank volatilizes, the vicinity of the opening of the cylindrical part is always maintained at a high temperature, so it is possible to prevent the volatile matter from liquefying or solidifying and adhering to the inner surface near the opening. Therefore, it is possible to appropriately suppress the situation that the attached volatile matter falls into the molten glass and becomes a foreign body. In addition, since the heat dissipation from the opening is greatly reduced, it is also possible to obtain the effect of preventing the devitrification near the liquid level of the molten glass before it happens. The above result is that it is possible to achieve the improvement of the quality of the glass article as a product or the improvement of the product yield rate.
[0016] In this case, it is preferred that the cover body has: a refractory; and a covering member, which covers at least the lower surface of the refractory and is composed of platinum or a platinum alloy. Here, the "covering member" refers to a plate (thin plate) or a layer formed by spraying, etc. In addition, the "refractory" mentioned here refers to, for example, a refractory such as dense zircon, mullite, alumina, or zirconia.
[0017] In this way, the lower surface of the cover body, which is easily corroded, is covered by the covering member composed of platinum or a platinum alloy, so that corrosion of the cover body can be effectively suppressed and durability can be improved. In addition, when the entire cover body is formed of platinum or a platinum alloy, the cost is increased and the weight is increased. However, if the refractory is covered with a covering member composed of platinum or a platinum alloy, the cost can be reduced and the weight can be reduced.
[0018] In the above structure, the cylindrical portion may also have a flange at its upper end extending from the outer peripheral end of the cover body to the outer peripheral side, and the state adjustment groove may include: a cooling pipe, which is assembled on the upper side of the portion of the flange extending from the cover body; and a flow reduction mechanism, which reduces the flow of gas flowing out from the gap between the upper end of the cylindrical portion and the cover body and going to the cooling pipe.
[0019] In this way, for example, the state adjustment tank is electrically heated well. In detail, it is common practice that the state adjustment tank is electrically heated for the purpose of adjusting the temperature of the molten glass inside. In addition, it is also common practice that the electrode for electrically heating the state adjustment tank is assembled on the above-mentioned flange from the perspective of layout. Therefore, the flange is cooled by the cooling pipe, and with this, the electrode is protected from the influence of heat. In this case, the cooling pipe is assembled on the upper side of the flange. Therefore, when the gas (mainly the steam obtained by gasification of the molten glass) generated from the molten glass in the state adjustment tank flows out from the gap between the upper end of the cylindrical part and the cover body, the gas flows above the flange and may contact the cooling pipe. Since the gas is high temperature, the cooling pipe may be damaged or broken due to oxidation and corrosion. In addition, when the cooling pipe is broken, the cooling liquid leaking from the cooling pipe may fall into the state adjustment tank through the gap between the upper end of the cylindrical part and the cover body. In contrast, since a flow rate reducing mechanism is provided to reduce the flow rate of the gas to the cooling pipe, the gas is less likely to come into contact with the cooling pipe, and the probability of damage or breakage of the cooling pipe can be reduced.
[0020] In this case, the flow rate reducing mechanism may be a gas flow path provided in the cover body.
[0021] In this way, the gas flow path provided in the cover body allows the internal gas to flow out in priority to the gap between the upper end of the cylindrical portion and the cover body, thereby reducing the flow rate of the gas to the cooling pipe. Therefore, the cover body is effectively used to construct a flow reduction mechanism, realizing a cheap and compact flow reduction mechanism.
[0022] In this configuration, the inlet and outlet of the gas flow path may be formed at different positions in a plan view.
[0023] Here, the flow outlet of the gas flow path is affected by the external gas and the temperature is reduced, so volatiles such as tin oxide are easily attached to the inner peripheral surface of the flow outlet. Therefore, the attached volatiles may fall into the molten glass as time passes. In contrast, the flow outlet and the flow inlet are located at different positions when viewed from above, so there is no flow inlet in the path where the volatiles attached to the inner peripheral surface of the flow outlet fall downward vertically. Thus, it is possible to avoid the situation where the volatiles fall into the molten glass through the flow inlet.
[0024] In this configuration, the inlet and the outlet of the gas flow path may be formed so that the gas flows in different directions.
[0025] In this way, the gas flow directions at the inlet and the outlet are different, so even if the volatiles attached to the inner peripheral surface of the outlet fall, they are likely to stop in the middle of the gas flow path and are difficult to reach the inlet. Thus, it is also possible to avoid the situation where the volatiles pass through the inlet and fall into the molten glass.
[0026] Furthermore, the flow rate reducing mechanism may be a shielding wall disposed between an outer peripheral end of the cover body and the cooling pipe.
[0027] Thus, even if the gas generated from the molten glass flows out from the gap between the upper end of the cylindrical portion and the cover, the shielding wall prevents the gas from contacting the cooling pipe. As a result, the probability of damage or breakage of the cooling pipe can be reduced.
[0028] Furthermore, the cylindrical portion may have a flange at an upper end thereof, and the state adjusting tank may include a cooling pipe mounted on the flange, wherein the cooling pipe is mounted on a lower side of the flange.
[0029] Thus, even if the gas generated from the molten glass flows out from the gap between the upper end of the cylindrical portion and the cover, the gas flows above the flange and therefore does not contact the cooling pipe mounted on the lower side of the flange, thereby reliably avoiding damage or breakage of the cooling pipe.
[0030] The second aspect of the present invention made to solve the above-mentioned problems is a method for manufacturing glass articles, which includes a transfer process of transferring molten glass from a melting furnace to a forming device using a transfer device. In the transfer process, a state adjustment process of adjusting the state of the molten glass using a state adjustment groove equipped with the transfer device is performed. The method for manufacturing glass articles is characterized in that the state adjustment groove has: a cylindrical portion, whose central axis is along the up-down direction and has an opening at the upper end; and a cover body, which covers the opening of the cylindrical portion when the state adjustment process is performed.
[0031] According to this production method, similarly to the case of the production apparatus described above, it is possible to appropriately suppress the volatile matter from falling into the molten glass.
[0032] Effects of the Invention
[0033] According to the present invention, adverse effects that may be caused by opening the opening of the state adjustment tank provided in the transfer device are suppressed. BRIEF DESCRIPTION OF THE DRAWINGS
[0034] Figure 1 This is a schematic side view showing the overall structure of a glass product manufacturing apparatus according to an embodiment of the present invention.
[0035] Figure 2 It is a perspective view showing the upper structure of the state adjustment tank according to the first embodiment of the present invention.
[0036] Figure 3 is in accordance with Figure 2 The longitudinal section main view obtained by cutting along the AA line.
[0037] Figure 4 This is a perspective view showing an example of a cover body used in the first embodiment of the present invention.
[0038] Figure 5 This is a perspective view showing another example of using the cover body in the first embodiment of the present invention.
[0039] Figure 6 This is a longitudinal sectional front view for explaining the problems of the first embodiment of the present invention.
[0040] Figure 7 It is a longitudinal sectional front view showing the upper structure of the state adjusting tank according to the second embodiment of the present invention.
[0041] Figure 8 It is a perspective view showing the upper structure of a state adjusting tank according to a third embodiment of the present invention.
[0042] Fig. 9 is in accordance with Figure 8 The longitudinal section main view obtained by cutting along the BB line.
[0043] Fig.10 It is a longitudinal sectional front view showing the upper structure of a state adjusting tank according to a fourth embodiment of the present invention.
[0044] Fig.11 It is a longitudinal sectional front view showing the upper structure of the state adjusting tank according to the fifth embodiment of the present invention.
[0045] Fig.12 It is a perspective view showing the upper structure of a state adjusting tank according to a sixth embodiment of the present invention.
[0046] Fig.13 is in accordance with Fig.12 The longitudinal section main view obtained by cutting along the CC line.
[0047] Fig.14 It is a perspective view showing the upper structure of a state adjusting tank according to the seventh embodiment of the present invention.
[0048] Fig.15 is in accordance with Fig.14 The longitudinal section main view obtained by cutting along the DD line.
[0049] Fig.16 It is a perspective view showing the upper structure of a state adjusting tank according to an eighth embodiment of the present invention.
[0050] Fig.17 is in accordance with Fig.16 The longitudinal section main view obtained by cutting along the EE line.
[0051] Fig.18 It is a perspective view showing the upper structure of a state adjusting tank according to a ninth embodiment of the present invention.
[0052] Fig.19 is in accordance with Fig.18 The longitudinal section main view obtained by cutting along the FF line. DETAILED DESCRIPTION
[0053] Hereinafter, a manufacturing apparatus and a manufacturing method of a glass article according to an embodiment of the present invention will be described with reference to the drawings.
[0054] [Glass article manufacturing device]
[0055] Figure 1 The overall structure of the manufacturing device of the glass article of the present invention is illustrated. As shown in the figure, the manufacturing device 1 generally comprises: a melting furnace 2, which is provided at the upstream end and generates molten glass Gm from glass raw materials; a transfer device 3, which transfers the molten glass Gm flowing out of the melting furnace 2 toward the downstream side; and a forming device 4, which forms the molten glass Gm supplied from the transfer device 3 into a strip-shaped plate glass Gp.
[0056] The transfer device 3 includes a clarification tank 5, one or more (two in the example) stirring tanks 6, and a state adjustment tank 7 in order from the upstream side. The clarification tank 5 removes bubbles in the molten glass Gm flowing out of the melting furnace 2. The stirring tank 6 stirs and homogenizes the molten glass Gm using a stirrer 8. The state adjustment tank 7 mainly adjusts the viscosity of the molten glass Gm and the flow rate of the molten glass Gm supplied to the forming device 4 before the molten glass Gm is supplied to the forming device 4.
[0057] The melting furnace 2 is connected to the clarification tank 5 via the upstream connecting pipe 9. The clarification tank 5 is connected to the stirring tank 6 on the upstream side via the intermediate connecting pipe 10. The stirring tank 6 on the upstream side is connected to the stirring tank 6 on the downstream side via the downstream connecting pipe 11. The stirring tank 6 on the downstream side is connected to the state adjustment tank 7 via the cooling pipe 12. The state adjustment tank 7 is composed of a cylindrical portion 13 as a large diameter pipe, a reduced diameter portion 14 as a conical pipe, and a lower portion 15 as a small diameter pipe. The central axis of the cylindrical portion 13 is along the up-down direction and the cylindrical portion 13 has an opening 16 at the upper end. The reduced diameter portion 14 is connected to the lower end of the cylindrical portion 13 and the inner diameter gradually decreases as it moves downward. The lower portion 15 is connected to the lower end of the reduced diameter portion 14. The inlet 17 of the state adjustment tank 7 is provided on the side wall of the cylindrical portion 13 and is connected to the cooling pipe 12. The outlet 18 of the state adjustment tank 7 is the lower end opening of the lower portion 15.
[0058] The forming device 4 includes a forming body 19 that forms a plate glass Gp by flowing down the molten glass Gm by an overflow down-draw method, and a large-diameter introduction pipe 20 that introduces the molten glass Gm into the forming body 19. The lower portion 15 of the state adjustment tank 7 is inserted into the introduction pipe 20, and the lower end portion of the lower portion 15 is immersed in the molten glass Gm in the introduction pipe 20. With this structure, the molten glass Gm is supplied from the state adjustment tank 7 to the introduction pipe 20.
[0059] [Method for manufacturing glass articles]
[0060] The manufacturing method of the glass article of the present invention includes a melting step of heating glass raw materials by a melting furnace 2 to generate molten glass Gm, a transfer step of transferring the molten glass Gm from the melting furnace 2 to a forming device 4 by a transfer device 3, and a forming step of forming the molten glass Gm supplied from the transfer device 3 by the forming device 4. In the forming step, the glass article is formed by an overflow down-draw method. In the transfer step, a state adjustment process of adjusting the state of the molten glass Gm by a state adjustment tank 7 provided in the transfer device 3 is performed.
[0061] Hereinafter, first to ninth embodiments concerning the upper portion of the state adjustment tank 7 which is the main part of the present invention will be described.
[0062] [First embodiment]
[0063] Figure 2 1 is a perspective view showing the upper structure of the state adjustment tank 7 according to the first embodiment of the present invention. Figure 3 is in accordance with Figure 2A longitudinal sectional front view obtained by cutting along the AA line of the cylindrical portion 13. As shown in the above-mentioned figures, the opening 16 at the upper end of the cylindrical portion 13 is covered by the cover 21 during the execution of the transfer process and the forming process. If described in detail, the cylindrical portion 13 has a flange 22 at the upper end. The cover 21 is placed on the inner peripheral side portion 22a of the flange 22 in a state of covering the opening 16, and can be easily installed and removed. The cylindrical portion 13 is formed of platinum or a platinum alloy. The flange 22 is formed of platinum or a platinum alloy or other metals. Here, in the example shown in the figure, the opening area of the opening 16 of the cylindrical portion 13 is substantially the same size as the pipeline area of the cylindrical portion 13, but the former may be smaller than the latter or may be larger than the latter. In addition, the height of the liquid level GL of the molten glass Gm is preferably formed at the inlet 17 of the cylindrical portion 13 (refer to Figure 1 ) is located in the middle between the upper and lower ends (especially near the upper end).
[0064] The outer peripheral part 22b of the flange 22 extends from the outer peripheral end 21a of the cover body 21. A cooling pipe 23 is mounted on the upper side of the outer peripheral part 22b of the flange 22. Specifically, the cooling pipe 23 is fixed to the upper surface of the outer peripheral part 22b of the flange 22 in a manner that is approximately one circle along the circumferential direction. And, by circulating the cooling liquid in the cooling pipe 23, the flange 22, in particular, the outer peripheral part 22b is cooled. An electrode (not shown) for electrically heating the state adjustment tank 7 is mounted on the outer peripheral part 22b of the flange 22.
[0065] Figure 4 : is a three-dimensional diagram showing the structure of the cover body 21. As shown in the figure, the cover body 21 is composed of a plurality of (two in the example) refractory materials 24 and a thin plate 25 as a covering member that covers the refractory materials 24 and is made of platinum or a platinum alloy. The thin plate 25 includes a lower thin plate 25a that covers the lower surfaces of the two refractory materials 24, an outer peripheral thin plate 25b that covers the entire outer peripheral surface of the two refractory materials 24, and a partition thin plate 25c that is sandwiched between the two refractory materials 24. The above-mentioned thin plates 25a, 25b, and 25c are integrated. It should be noted that, as Figure 5 As shown, it can also be the following structure, that is, respectively utilize lower thin plate 25a, peripheral thin plate 25b and partition thin plate 25c to cover two refractory materials 24 separately, and make two partition thin plates 25c contact in a way that can be away from or join in a way that cannot be away from. In addition, thin plate 25 can cover the entire surface including the upper surface of refractory material 24, or it can only cover the lower surface of refractory material 24. It should be noted that the covering setting member is not limited to thin plate 25, and can be a layer composed of platinum or platinum alloy formed by spraying to refractory material 24. Here, refractory material 24 is, for example, a refractory material composed of dense zircon, mullite, alumina system, or zirconium oxide system (the "refractory material" described below is also the same).
[0066] According to the manufacturing device 1 of the glass article of the first embodiment, the following effects are achieved. When the molten glass Gm is formed by the forming device 4, the opening 16 of the cylindrical portion 13 in the state adjustment tank 7 is covered by the lid 21. Therefore, it is possible to avoid the disadvantages that may be caused by the opening 16 opening. Specifically, even if the tin oxide and the like remaining in the molten glass Gm in the state adjustment tank 7 volatilize, since the vicinity of the opening 16 of the cylindrical portion 13 is always maintained at a high temperature, it is also possible to prevent the volatile matter from liquefying or solidifying and adhering to the inner surface near the opening. Therefore, it is possible to appropriately suppress the situation where the attached volatile matter falls into the molten glass Gm and becomes a foreign body. In addition, since the heat dissipation from the opening 16 is greatly reduced, it is also possible to obtain the effect of preventing the devitrification near the liquid level GL of the molten glass Gm before it happens. The above result is that it is possible to achieve the improvement of the quality of the glass article (glass plate) as a product or the improvement of the product yield.
[0067] In addition, since the easily corroded portion, i.e., the lower surface of the cover 21, is covered by a thin plate (covering member) 25 made of platinum or a platinum alloy, corrosion of the cover 21 can be effectively suppressed, thereby improving durability. In this case, when the entire cover 21 is formed of platinum or a platinum alloy, the cost is increased and the weight is increased, but by covering the refractory 24 with a thin plate 25 made of platinum or a platinum alloy, low cost and light weight can be achieved.
[0068] It should be noted that, in the structure of the first embodiment described above, Figure 6 As exaggeratedly shown in FIG. 2 , the gas inside (mainly the vapor obtained by vaporizing the molten glass) may flow out through the gap 26 between the upper end of the cylindrical portion 13 and the cover 21. When the gas flows out through the gap 26 as shown by the arrow a, the gas flows toward the outer peripheral side above the outer peripheral portion 22b of the flange 22 and may contact the cooling pipe 23. Since the gas is at a high temperature, the cooling pipe 23 may be damaged or broken due to corrosion caused by oxidation. In addition, when the cooling pipe 23 is broken, the coolant leaking from the cooling pipe 23 may fall into the state adjustment tank 7 through the gap 26.
[0069] [Second embodiment]
[0070] A solution for avoiding such an inconvenience is the second embodiment of the present invention. Figure 72 is a longitudinal sectional front view showing the upper structure of the state adjustment tank 7 of the second embodiment of the present invention. As shown in the figure, a through hole 27 is formed in the central part of the cover 21 so that the internal gas flows out upward as shown by the arrow b. The inner peripheral surface of the through hole 27 is also covered by a covering member made of platinum or platinum alloy. The other structures are the same as those of the first embodiment described above, so the common components in the two embodiments are described in detail. Figure 7 In this way, the gas inside flows out from the through hole 27 in the upward direction indicated by the arrow b in preference to the gap 26, thereby obtaining the advantage that the gas is unlikely to come into contact with the cooling pipe 23. In addition, when a plunger is used to block the downward flow of the molten glass Gm, the through hole 27 can be effectively utilized as a hole through which the shaft of the plunger passes.
[0071] In the structure of the second embodiment described above, the outflow side (upper part) of the inner peripheral surface of the through hole 27 formed in the cover body 21 is affected by the external air and the temperature is lowered. Therefore, the outflow side of the inner peripheral surface of the through hole 27 becomes a state where volatiles such as tin oxide are easily liquefied or solidified and attached, and it is also easy to produce condensation of the volatiles after attachment. In addition, the volatiles attached to the outflow side of the inner peripheral surface of the through hole 27 may fall into the molten glass Gm as time passes and become foreign matter. It should be noted that the amount of volatiles attached in this case is small compared with the amount of volatiles attached to the inner surface near the opening when the opening of the state adjustment tank is opened in the past.
[0072] [Third Embodiment]
[0073] The third embodiment of the present invention avoids this inconvenience. Figure 8 1 is a perspective view showing the upper structure of the state adjustment tank 7 according to the third embodiment of the present invention. Fig. 9 is in accordance with Figure 8BB line cut. As shown in the above figures, the gas flow path 30 is provided in the cover body 21. If described in detail, the cover body 21 includes: a flat base wall portion 31, which covers the upper end of the cylindrical portion 13 and the upper surface of the inner peripheral side portion 22a of the flange 22; an annular or cylindrical side wall portion 32, which is provided on the base wall portion 31; and a flat top wall portion 33, which covers the upper side of the side wall portion 32. In addition, the gas flow path 30 is composed of an inlet 34, an internal space 35 communicating with the inlet, and an outlet 36 communicating with the internal space 35. The inlet 34 is a through hole formed in the central part of the base wall portion 31. The internal space 35 is a space surrounded by the side wall portion 32 and the top wall portion 33. The outlet 36 is a notch portion formed at the upper part of one position in the circumferential direction of the side wall portion 32. In this case, the positions of the inlet 34 and the outlet 36 when viewed from above are different. In addition, the central axis of the inlet 34 is along the vertical direction, whereas the central axis of the outlet 36 is along the horizontal direction. Therefore, the flow direction of the gas at the inlet 34 is generally in the upward direction along the vertical direction (the direction of the arrow c), whereas the flow direction of the gas at the outlet 36 is generally in the lateral direction along the horizontal direction (the direction of the arrow d).
[0074] Here, the base wall portion 31 is the same as that of the second embodiment described above (see Figure 7 ) has the same structure as the cover body 21 in the cooling tube 23. In addition, the side wall portion 32 and the top wall portion 33 are preferably formed only by refractory materials, but at least the parts of these refractory materials that are in contact with the gas may also be covered by a covering member of platinum or a platinum alloy. Here, when the opening area of the inlet 34 is set to M1 and the opening area of the opening portion 16 is set to M2, M1 / M2 preferably has a lower limit of 1 / 200 and an upper limit of 1 / 10, and more preferably has a lower limit of 1 / 100 and an upper limit of 1 / 20. In addition, the opening area of the outlet 36 is smaller than the opening area of the inlet 34. Furthermore, the height position of the outlet 36 is the same as the height position of the upper part of the cooling tube 23 or is higher than the height position of the upper part of the cooling tube 23. It should be noted that the outlet 36 is not limited to one circumferential position of the side wall portion 32, and may also be formed at multiple circumferential positions.
[0075] According to the manufacturing device 1 of the glass article of the third embodiment, the following effects are achieved. After the gas in the state adjustment tank 7 flows into the internal space 35 from the inlet 34 of the gas flow path 30 in priority to the above-mentioned gap 26, it flows out from the outlet 36 to the outside. In this case, since the inner peripheral surface of the outlet 36 is affected by the external gas and the temperature is reduced, the volatiles such as tin oxide contained in the gas are easily liquefied or solidified and attached to the inner peripheral surface. In addition, when the volatiles are attached to the inner peripheral surface of the outlet 36, the volatiles may fall with the passage of time. However, for the inlet 34 and the outlet 36, the position when viewed from above and the flow direction of the gas are different, so there is no inlet 34 in the path where the volatiles fall, and the volatiles are blocked by the bottom of the inner peripheral surface of the outlet 36 and the upper surface of the base wall portion 31. Therefore, the volatiles are prevented from falling into the molten glass Gm. It should be noted that the inner peripheral surface of the inlet 34 is not easily affected by the external gas, so it is maintained at a high temperature. Therefore, it is possible to prevent volatile substances such as tin oxide from being attached to the inner peripheral surface of the inlet 34 .
[0076] In addition, the height position of the outflow port 36 is the same as or higher than the height position of the upper end of the cooling pipe 23, so the gas flowing out of the outflow port 36 in the direction of the arrow d is unlikely to contact the cooling pipe 23. It should be noted that the gas flowing out of the outflow port 36 is at a higher temperature than the outside air, so the gas gradually moves upward immediately after flowing out. Therefore, the situation where the gas contacts the cooling pipe 23 can be more reliably avoided.
[0077] [Fourth Embodiment]
[0078] Fig.10 This is a longitudinal sectional front view showing the upper structure of the state adjustment tank 7 of the fourth embodiment of the present invention. As shown in the figure, the structure of the fourth embodiment is different from the structure of the third embodiment described above in that a receiving member 37 is provided on the base wall portion 31 of the cover body 21. The receiving member 37 has a hanging portion 37a extending downward from the lower portion of the base wall portion 31 and a receiving portion 37b extending laterally (horizontally) from the lower end of the hanging portion 37a. The receiving portion 37b is arranged in the upper space of the liquid surface GL of the molten glass Gm. The area of the receiving portion 37b (the area when viewed from above) is larger than the opening area of the inlet 34, and the inlet 34 falls within the upper surface area of the receiving portion 37b when viewed from above. The other structures are the same as those of the third embodiment described above, so regarding the components common to the two embodiments, the receiving portion 37b is described in detail below. Fig.10The same reference numerals are used in the figure, and the description thereof is omitted. According to the structure of the fourth embodiment, even if the volatiles attached to the inner peripheral surface of the inlet 34 fall or the volatiles fall from the internal space 35 through the inlet 34, the volatiles are received by the receiving portion 37b of the receiving member 37. Therefore, it is possible to further reliably suppress the volatiles from falling into the molten glass Gm and becoming platinum foreign matter, etc. The other effects are substantially the same as those of the third embodiment described above.
[0079] [Fifth Embodiment]
[0080] Fig.11 : is a longitudinal sectional front view showing the upper structure of the state adjustment tank 7 of the fifth embodiment of the present invention. As shown in the figure, the structure of the fifth embodiment is different from the structure of the third embodiment described above in that an inlet 34 is formed at a position offset from the central portion to one side of the base wall portion 31 of the cover body 21, and an outlet 36 is formed at a position offset from the central portion to the other side of the top wall portion 33. Therefore, the positions of the inlet 34 and the outlet 36 when viewed from above are different. In this case, the flow direction of the gas at the inlet 34 is the same as the flow direction of the gas at the outlet 36, and both are roughly in the upward direction along the plumb line (the direction of the arrow e and the direction of the arrow f). It should be noted that no notch is formed in the side wall portion 32. In addition, the internal space 35 of the gas flow path 30 is expanded in the transverse direction compared to the third embodiment described above. The other structures are the same as those of the second example described above, so regarding the components common to the two examples, Fig.14 31. The same reference numerals are used in the figure, and the description thereof is omitted. According to the structure of the fifth embodiment, the positions of the inlet 34 and the outlet 36 when viewed from above are different, so there is no inlet 34 in the path where the volatiles fall, and the volatiles are blocked by the upper surface of the base wall portion 31. Therefore, the volatiles are prevented from falling into the molten glass Gm. In addition, the gas flowing out of the outlet 36 goes to the upper direction (arrow f direction) just after flowing out, so it is reliably made difficult for the gas to contact with the cooling pipe 23.
[0081] [Sixth Embodiment]
[0082] Fig.12 1 is a perspective view showing the upper structure of the state adjustment tank 7 according to the sixth embodiment of the present invention. Fig.13 is in accordance with Fig.12A longitudinal sectional front view obtained by cutting along the CC line of the flange 22. In the structure of the sixth embodiment, the cover body 21 has an annular or cylindrical side wall portion 32 arranged on the inner peripheral side portion 22a of the flange 22, and a flat top wall portion 33 covering the upper part of the side wall portion 32. The gas flow path 30 is composed of an internal space 35 and an outflow port 36. The internal space 35 is a space surrounded by the side wall portion 32 and the top wall portion 33. The outflow port 36 is a notch portion formed at the upper part of a position in the circumferential direction of the side wall portion 32. According to the structure of the sixth embodiment, the gas in the state adjustment groove 7 has priority over the gap 26 between the upper end of the cylindrical portion 13 and the side wall portion 32, and flows out to the outside from the outflow port 36 through the internal space 35 of the gas flow path 30. In this case, even if the volatiles attached to the inner peripheral surface of the outflow port 36 fall, the volatiles are also blocked by the bottom of the inner peripheral surface of the outflow port 36, the upper surface of the inner peripheral side portion 22a of the flange 22, and the upper end surface of the cylindrical portion 13. Therefore, it is possible to prevent the volatiles from falling into the molten glass Gm. In this case, the space above the opening 16 (internal space 35) is surrounded by the side wall portion 32 and the top wall portion 33, so it is maintained at a high temperature. Therefore, the vicinity of the opening 16 becomes a state where volatiles such as tin oxide are difficult to adhere to and it is also difficult to produce condensation of the volatiles after attachment. Thus, it is avoided that the volatiles adhere to and condense near the opening 16, and it is possible to prevent the volatiles from falling from the vicinity of the opening 16 into the molten glass Gm. In addition, the flow direction of the gas at the outflow port 36 becomes horizontal as shown by the arrow g, so the flow resistance of the gas when passing through the gas flow path 30 becomes large. Thus, it is possible to avoid the situation where the flow rate of the gas through the gas flow path 30 is too much. The height of the outlet 36 is about the same as or higher than the height of the upper end of the cooling pipe 23. Therefore, the gas flowing out from the outlet 36 in the direction of arrow g is unlikely to come into contact with the cooling pipe 23.
[0083] [Seventh Embodiment]
[0084] Fig.14 1 is a perspective view showing the upper structure of the state adjustment tank 7 according to the seventh embodiment of the present invention. Fig.15 It shows that according to Fig.14 The structure of the seventh embodiment is similar to that of the first embodiment described above (see Figure 2 as well as Figure 3 ) is different in that a shielding wall 40 as a flow reduction mechanism is arranged between the outer peripheral end 21a of the cover body 21 and the cooling pipe 23. The shielding wall 40 is fixed to the upper surface of the flange 22 and is annular or cylindrical. The upper end of the shielding wall 40 is higher than the upper end of the cooling pipe 23. The other structures are the same as those of the first embodiment described above, so the common components in the two embodiments are described in Fig.14 as well as Fig.15 The same reference numerals are used in the figure, and their description is omitted. According to the seventh embodiment, even if the gas generated from the molten glass Gm in the state adjustment tank 7 flows out from the gap 26 between the upper end of the cylindrical portion 13 and the cover 21, the shielding wall 40 can be used to prevent the gas from contacting the cooling pipe 23. As a result, the probability of damage or breakage of the cooling pipe 23 can be reduced. The other effects are substantially the same as those of the first embodiment described above.
[0085] [Eighth Embodiment]
[0086] Fig.16 1 is a perspective view showing the upper structure of the state adjustment tank 7 according to the eighth embodiment of the present invention. Fig.17 is in accordance with Fig.16 The structure of the eighth embodiment is similar to that of the first embodiment described above (see Figure 2 as well as Figure 3 ) is different in that the cooling pipe 23 is mounted on the lower side of the outer peripheral portion 22b of the flange 22. The other structures are the same as those of the first embodiment described above, so the common components in the two embodiments are described in Fig.16 as well as Fig.17 , and the same reference numerals are used in the state adjustment tank 7, and their description is omitted. According to the eighth embodiment, even if the gas generated from the molten glass Gm in the state adjustment tank 7 flows out from the gap 26 between the upper end of the cylindrical portion 13 and the cover 21, the gas also flows on the upper side of the flange 22. In contrast, the cooling pipe 23 is assembled on the lower side of the flange 22, so the above-mentioned gas does not contact the cooling pipe 23. The other effects are substantially the same as those of the first embodiment described. It should be noted that, in the eighth embodiment, the flange 22 may not extend from the outer peripheral end of the cover 21 to the outer peripheral side.
[0087] [Ninth Embodiment]
[0088] Fig.18 1 is a perspective view showing the upper structure of the state adjustment tank 7 according to the ninth embodiment of the present invention. Fig.19 is in accordance with Fig.18 The structure of the ninth embodiment is similar to that of the first embodiment described above (see Figure 2 as well as Figure 3) The difference is that the cooling pipe 23 is mounted on the lower side of the outer peripheral part 22b of the flange 22, and a recessed portion 41 recessed toward the lower side is formed in the inner peripheral part 22a of the flange 22, and the cover body 21 is embedded in the recessed portion 41. According to the ninth embodiment, even if the gas flows out from the curved gap 26 between the upper end of the cylindrical portion 13 and the cover body 21 to the upper side of the flange 22, the gas does not contact the cooling pipe 23 mounted on the lower side of the flange 22. In addition, by bending the above-mentioned gap 26, the outflowing gas goes in the upward direction just after flowing out. Thereby, the gas is also prevented from contacting the cooling pipe 23. Therefore, in this embodiment, the cooling pipe 23 can also be mounted on the upper side of the flange 22.
[0089] It should be noted that, in the above embodiment, the cylindrical portion 13 provided on the upper portion of the state adjustment groove is set to be cylindrical in the example, but it can also be a square cylindrical shape of a quadrilateral or polygonal shape when viewed from above. In addition, the flange 22 formed on the upper end of the cylindrical portion 13 and the cover 21 covering the opening 16 of the cylindrical portion 13 are set to be circular in the example when viewed from above, but they can also be quadrilateral, polygonal, etc. when viewed from above.
[0090] Description of Reference Numerals
[0091] 1 Manufacturing equipment
[0092] 2 Melting furnace
[0093] 3 Transfer device
[0094] 4 Forming device
[0095] 5 Clarification tank
[0096] 6 Mixing tank
[0097] 7 Status Adjustment Slots
[0098] 13 cylindrical part
[0099] 16 Opening
[0100] 21 Cover
[0101] 21a Outer peripheral end of cover
[0102] 22 Flange
[0103] 22a Inner circumference of flange
[0104] 22b Outer peripheral portion of flange
[0105] 23 Cooling pipe
[0106] 24 Refractory
[0107] 25 Covering member (thin plate)
[0108] 26 Gap
[0109] 30 Gas flow path
[0110] 34 Inlet
[0111] 36 Outlet
[0112] 40 Blocking wall
[0113] 41 recess
[0114] Gm Molten glass.
Claims
1. A manufacturing device for glass articles, wherein a state adjustment tank for adjusting the state of the molten glass is provided in a transfer device for transferring molten glass from a melting furnace to a forming device, The manufacturing device of the glass article is characterized in that: The state adjustment tank comprises: a cylindrical portion whose central axis is along the vertical direction and has an opening at the upper end; and a cover body that covers the opening of the cylindrical portion. The cylindrical portion has a flange at its upper end extending from the outer peripheral end of the cover toward the outer peripheral side. The state adjustment tank includes: a cooling pipe mounted on the upper side of the portion of the flange extending from the cover body; and a flow reduction mechanism that reduces the flow of gas flowing out from the gap between the upper end of the cylindrical portion and the cover body and heading to the cooling pipe. The flow rate reducing mechanism is provided in the gas flow path of the cover body.
2. The manufacturing device for glass articles according to claim 1, wherein: The inlet and outlet of the gas flow path are formed at different positions in a plan view.
3. The manufacturing device for glass articles according to claim 2, wherein: The inlet and the outlet of the gas flow path are formed so that the flow direction of the gas is different from each other.
4. A manufacturing device for glass articles, wherein a state adjustment tank for adjusting the state of the molten glass is provided in a transfer device for transferring the molten glass from a melting furnace to a forming device, The manufacturing device of the glass article is characterized in that: The state adjustment tank comprises: a cylindrical portion whose central axis is along the vertical direction and has an opening at the upper end; and a cover body that covers the opening of the cylindrical portion. The cylindrical portion has a flange at its upper end extending from the outer peripheral end of the cover toward the outer peripheral side. The state adjustment tank includes: a cooling pipe mounted on the upper side of the portion of the flange extending from the cover body; and a flow reduction mechanism that reduces the flow of gas flowing out from the gap between the upper end of the cylindrical portion and the cover body and heading to the cooling pipe. The flow rate reducing mechanism is a shielding wall disposed between the outer peripheral end of the cover body and the cooling pipe.
5. The manufacturing device for a glass article according to any one of claims 1 to 4, wherein: The cover body includes: a refractory material; and a covering member that covers at least a lower surface of the refractory material and is made of platinum or a platinum alloy.
6. A method for manufacturing a glass article, comprising a transfer step of transferring molten glass from a melting furnace to a forming device using a transfer device, wherein in the transfer step, a state adjustment process of adjusting the state of the molten glass using a state adjustment tank provided in the transfer device is performed, The method for manufacturing the glass article is characterized in that: The state adjustment tank comprises: a cylindrical portion, the central axis of which is along the up-down direction and has an opening at the upper end; and a cover body, which covers the opening of the cylindrical portion when the state adjustment process is performed. The cylindrical portion has a flange at its upper end extending from the outer peripheral end of the cover toward the outer peripheral side. The state adjustment tank includes: a cooling pipe mounted on the upper side of the portion of the flange extending from the cover body; and a flow reduction mechanism that reduces the flow of gas flowing out from the gap between the upper end of the cylindrical portion and the cover body and heading to the cooling pipe. The flow rate reducing mechanism is provided in the gas flow path of the cover body.
7. A method for manufacturing a glass article, comprising a transfer step of transferring molten glass from a melting furnace to a forming device using a transfer device, wherein in the transfer step, a state adjustment process of adjusting the state of the molten glass using a state adjustment tank provided in the transfer device is performed, The method for manufacturing the glass article is characterized in that: The state adjustment tank comprises: a cylindrical portion, the central axis of which is along the up-down direction and has an opening at the upper end; and a cover body, which covers the opening of the cylindrical portion when the state adjustment process is performed. The cylindrical portion has a flange at its upper end extending from the outer peripheral end of the cover toward the outer peripheral side. The state adjustment tank includes: a cooling pipe mounted on the upper side of the portion of the flange extending from the cover body; and a flow reduction mechanism that reduces the flow of gas flowing out from the gap between the upper end of the cylindrical portion and the cover body and heading to the cooling pipe. The flow rate reducing mechanism is a shielding wall disposed between the outer peripheral end of the cover body and the cooling pipe.
Citation Information
Patent Citations
Molten Glass Supply Device
CN106186642A
Cooling unit, heat insulating structure, substrate processing apparatus and semiconductor device manufacturing method
CN109494172A
Water outlet device for smelting furnace and fused water heater
CN1490557A
Mold-press forming apparatus and method of manufacturing a formed product
CN1769224A
Refractory structure with electrode and glass manufacturing apparatus
JP2007076939A