Pyrolysis tar upgrading

By performing two heat treatments on the pyrolysis tar to separate and transform its solid part, the problem of solid matter in the pyrolysis tar affecting the hydrotreating efficiency is solved, the yield and compatibility of the tar are increased, and the process economy is improved.

CN113906118BActive Publication Date: 2024-10-11EXXONMOBIL CHEMICAL PATENTS INC
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202080040800.X
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Priority Date
2019-10-31
Filing Date
2020-05-15
Publication Date
2024-10-11
Estimated Expiration
2040-05-15

AI Technical Summary

Technical Problem

In the existing technology, there are a large amount of solid substances in the pyrolysis tar produced during the hydrocarbon pyrolysis process, which leads to low hydrotreating efficiency, reduced yield, and reactor clogging. In addition, conventional catalytic hydrotreating methods can lead to catalyst deactivation and abnormality. Sediment formation is required, which affects process economy.

Method used

By performing two heat treatments on the pyrolysis tar, the higher-density and lower-density parts are separated respectively, and the solids in the higher-density part are converted into liquids in the second heat treatment to reduce the gas phase products and increase the hydrotreated tar yield. efficiency and process economy.

Benefits of technology

It effectively reduces the formation of solid deposits during hydrotreating, increases tar yield and compatibility, improves process economy, and increases hydrotreating efficiency.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN113906118B_ABST
    Figure CN113906118B_ABST
Patent Text Reader

Abstract

The present application provides methods and apparatus for preparing liquid hydrocarbon products. In one embodiment, the method for preparing a liquid hydrocarbon product includes heat treating tar to produce a first tar composition and blending the tar composition with a utility fluid to form a tar-fluid mixture. The method includes separating the tar-fluid mixture to form a first lower density portion and a first higher density portion containing solids. The method further includes heat treating the first higher density portion to form a heat treated first higher density portion to convert at least a portion of the solids into a liquid.
Need to check novelty before this filing date? Find Prior Art

Description

Field of the Invention

[0001] This application claims priority to and the benefit of U.S. Provisional Application No. 62 / 857,442, filed on June 5, 2019, and European Patent Application No. 19206400.4, filed on October 31, 2019, which are incorporated herein by reference.

[0002] Embodiments generally relate to upgrading tar, such as by one or more thermal treatments. More particularly, embodiments relate to methods and apparatus for thermal soaking steam cracking tar solids. Background Art

[0003] Hydrocarbon pyrolysis processes, such as steam cracking, crack hydrocarbon feedstocks into a wide range of relatively high value molecules, including ethylene, propylene, butenes, steam cracked gas oil ("SCGO"), steam cracked naphtha ("SCN"), or any combination thereof. In addition to these useful products, hydrocarbon pyrolysis can also produce large amounts of relatively low value heavy products, such as pyrolysis tar. When pyrolysis is carried out by steam cracking, the pyrolysis tar is identified as steam cracked tar ("SCT"). The economic viability of refining and petrochemical processes depends in part on the ability to introduce as many products and residual fractions, such as SCT, into the value chain as possible. One use for the residual fractions and / or relatively low value products is to blend these fractions with other hydrocarbons, such as other feed streams or products.

[0004] However, SCT typically contains relatively high molecular weight molecules, conventionally referred to as tar heavies ("TH") and considerable amounts of sulfur. The presence of sulfur and TH makes SCT a less desirable blending material, such as for blending with fuel oil blend-feedstocks or different SCTs. Compatibility is typically determined by visual inspection of solid formation, as described, for example, in U.S. Pat. No. 5,871,634. In general, SCT has a high viscosity and poor compatibility with other heavy hydrocarbons, such as fuel oil, or is only compatible in small amounts. Likewise, SCT produced under specific conditions typically has poor compatibility with SCT produced under different conditions.

[0005] By catalytically hydrotreating SCT, viscosity and compatibility can be improved, and sulfur content can be reduced. However, catalytic hydrotreating of undiluted SCT results in significant catalyst deactivation and the formation of undesirable deposits (e.g., coke deposits or particles) on reactor internals. As the amount of these deposits increases, the yield of the desired upgraded pyrolysis tar (upgraded SCT) decreases and the yield of undesirable byproducts increases. The pressure drop of the hydrotreating reactor also increases, to the point where the reactor may not be operable.

[0006] It is conventional to hydrotreat SCT in the presence of a fluid, such as a solvent having a significant aromatic content, to reduce the formation of deposits. The hydrotreated product contains an upgraded SCT product that typically has a reduced viscosity, a reduced atmospheric boiling point range, and an increased hydrogen content compared to the SCT fed, resulting in improved compatibility with the fuel oil blend feedstock. In addition, hydrotreating SCT in the presence of a fluid produces fewer undesirable byproducts and the rate of increase in the pressure drop of the reactor is slower. Some forms of SCT processing are disclosed in U.S. Patent Nos. 2,382,260 and 5,158,668 and in U.S. Patent Application Publication No. US2008 / 0053869. PCT Patent Application Publication Nos. WO 2013 / 033590, WO 2018 / 111577, and WO2019.203981 disclose recycling a portion of the hydrotreated tar for use as a fluid.

[0007] The presence of solids within SCT presents a serious challenge to efficient SCT hydroprocessing. A significant amount of the solids in SCT is in the form of particulate matter, such as coke (e.g., pyrolysis coke), oligomeric and / or polymeric materials, inorganic solids (e.g., fines, metals, metal-containing compounds, ash, etc.), aggregates of one or more of these, and the like. Although removal of SCT particulate matter, such as by filtration, sedimentation, centrifugation, etc., results in SCT that can be more readily hydroprocessed, doing so will undesirably reduce the yield of the hydroprocessed SCT. Moreover, managing large inventories of removed particulate matter may negatively impact process economics.

[0008] As an example, coke fines, inorganic fines, and other solids may be present in the SCT. Coke fines or particles may be or include pyrolytic coke and / or polymerized coke. These fines or particles may be formed during polymerized conditions (e.g., ≥ 150°C) present in the primary fractionator after pyrolytic tar formation (upstream of the hydrotreater).

[0009]

[0006] Therefore, there is a need for improved tar conversion processes that involve less solids in the conversion of hydrocarbon feedstocks to tar. SUMMARY OF THE INVENTION

[0011] In certain embodiments, a method for upgrading tar, such as pyrolysis tar, is provided. Tar, such as tar containing pyrolysis tar such as steam cracker tar, is subjected to a first thermal treatment to produce a tar composition. A first higher density portion and a first lower density portion are separated from the tar composition. The first higher density portion is subjected to a second thermal treatment to produce a heat-treated first higher density portion. A second higher density portion and a second lower density portion are separated from the heat-treated first higher density portion. At least a portion of the second lower density portion can be recycled to one or more of the following: (i) tar, (ii) tar composition, and (iii) the first higher density portion. The second higher density portion can be directed away, such as for storage and / or further processing. It is observed that the amount of solids present in the heat-treated first higher density portion is less than the amount of solids present in the first higher density portion. Surprisingly, the second thermal treatment effectively converts the solids in the first higher density portion mainly into liquids in the heat-treated first higher density portion, and rarely into gaseous substances, if any conversion. This in turn results in improved process economics, greater efficiency, increased amounts of desirable liquid phase materials, and reduced amounts of less desirable solids compared to conventional tar processing. Returning at least a portion of the second lower density fraction (which contains liquids from the conversion of solids in the second thermal treatment) to the process increases the amount of tar available for hydroprocessing, thereby resulting in increased yield in the hydroprocessed tar.

[0012] In other embodiments, a method for upgrading steam cracker tar is provided. A steam cracker feed is steam cracked to form a steam cracker effluent containing steam cracker tar. A steam cracker tar composition is produced by at least (i) separating at least a portion of the steam cracker tar from the steam cracker effluent, and (ii) thermally treating at least a portion of the separated steam cracker tar in a first thermal treatment. A tar-fluid mixture is produced by adding a first utility fluid and / or a first separation fluid to the pyrolysis tar composition. A first separation is performed, wherein (i) a first lower density portion containing upgraded steam cracker tar and (ii) a first higher density portion are separated from the thermally treated steam cracker tar composition. At least a portion of the first lower density portion is directed away, for example for hydroprocessing. A diluent, typically containing a second utility fluid and / or a second separation fluid, is introduced into the first higher density portion to form a diluted first higher density portion. The diluted first higher density portion is subjected to a second thermal treatment to produce a thermally treated first higher density portion. The amount of solids in the heat treated first higher density fraction is less than the amount of solids present in the diluted first higher density fraction. In a second separation, the second lower density fraction and the second higher density fraction are separated from the heat treated first higher density fraction. At least a portion of the second lower density fraction is added to one or more of: (i) a steam cracker effluent, (ii) a steam cracker tar, (iii) a steam cracker tar composition; (iv) a tar-fluid mixture, (v) the first higher density fraction and (vi) the first lower density fraction.

[0013] In other embodiments, a process for steam cracking a steam cracker feed containing a heavy oil, such as a heavy oil containing residue, is provided. The steam cracker effluent includes steam cracker tar. The steam cracker includes a convection section and a radiant section. The radiant section includes at least one radiant coil having an inlet and an outlet. The steam cracker feed is preheated in the convection section. A stream of mainly gaseous phase and a stream of mainly non-gaseous phase are separated from at least a portion of the preheated steam cracker feed, wherein ≥50 wt% of the residue in the feed is transferred to the stream of non-gaseous phase. At least a portion of the stream of mainly gaseous phase is directed to the inlet of the radiant coil. Steam cracking is carried out in the radiant coil under steam cracking conditions in the presence of steam. Steam cracking conditions include a temperature ranging from about 760°C to about 1200°C at the outlet of the radiant coil, a steam cracking pressure ranging from about 1 bar (absolute pressure) to about 10 bar (absolute pressure) at the outlet of the radiant coil, and a steam cracking residence time in the radiant coil ranging from about 0.1 second to about 2 seconds. A steam cracker effluent containing steam cracker tar is directed away from the radiant section via the outlet of the radiant coil. At least a portion of the steam cracker tar is separated from the steam cracker effluent. In a first thermal treatment, at least a separated portion of the steam cracker tar is thermally treated to produce a steam cracker tar composition. A first utility fluid and / or a first separation fluid is added to the steam cracker tar composition, and / or a tar-fluid mixture is produced. At least two additional separations are performed. In the first of these separations, at least one centrifuge can be used to separate (i) a first lower density portion containing upgraded steam cracker tar and (ii) a first higher density portion from the tar-fluid mixture. At least a portion of the first lower density portion is directed away, for example, for hydroprocessing. A diluent containing a second utility fluid and / or a second separation fluid is introduced into the first higher density portion to form a diluted first higher density portion. The diluted first higher density portion is subjected to a second heat treatment to produce a heat treated first higher density portion. The amount of solids in the heat treated first higher density portion is less than the amount of solids present in the diluted first higher density portion. The second separation of these separations, which may also utilize at least one centrifuge, separates (i) a second lower density portion and (ii) a second higher density portion from the heat treated first higher density portion. At least a portion of the second lower density portion is added to one or more of the following: (i) a steam cracker effluent, (ii) a steam cracker tar, (iii) a steam cracker tar composition, (iv) a tar-fluid mixture, (v) the first higher density portion, and (vi) the first lower density portion.

[0014] Other aspects of the invention include comminuting the first higher density fraction (e.g., by grinding) prior to the second thermal treatment. Still other aspects of the invention include separating a stream of primarily gaseous phase and a stream of primarily non-gaseous phase from the preheated steam cracker feed in a separation section integrated with the convection section. The separated stream of primarily gaseous phase may be exposed to additional heating in the convection section prior to cracking in the radiant section.

[0015] Other aspects of the invention relate to systems and apparatus for carrying out any of the foregoing methods, to upgraded pyrolysis tars, to upgraded steam cracker tars, and to compositions containing one or more of these, to separated lower density and higher density fractions, and to the use of any of these or any portion thereof as feed for further processing, such as as feed for tar hydroprocessing.

[0016] These and other features, aspects and advantages of the method will become better understood from the following description, appended claims and accompanying drawings. BRIEF DESCRIPTION OF THE DRAWINGS

[0018] Figure 1 is a schematic diagram illustrating an apparatus for implementing certain aspects of the present disclosure.

[0019] Figure 2 is a graph illustrating solids loss (wt %) as a function of temperature employed in a heat treatment corresponding to a second heat treatment, according to an embodiment.

[0020] Detailed description

[0021] The present invention generally relates to separating pyrolysis tar from pyrolysis effluent, and upgrading at least the separated pyrolysis tar. More particularly, the present invention relates to separating at least a portion of the pyrolysis tar from the pyrolysis effluent, and exposing at least a portion of the separated pyrolysis tar to a first thermal treatment to produce a pyrolysis tar composition. A first lower density portion (upgraded pyrolysis tar) and a first higher density portion are separated from the pyrolysis tar composition. At least a portion of the first higher density portion is exposed to a second thermal treatment to produce a heat-treated first higher density portion having less solids (weight basis) than the first higher density portion. A second lower density portion and a second higher density portion are separated from the heat-treated first higher density portion. At least a portion of the second lower density portion can be recycled, for example, to the separated pyrolysis tar and / or the pyrolysis effluent. At least a portion of the second higher density portion can be directed away, for example, for storage and / or further processing. It has been found that upgrading pyrolysis tar in this manner will increase the amount of pyrolysis tar available for further upgrading, for example in one or more hydroprocessing stages, and improve the compatibility of the upgraded pyrolysis tar for blending with other hydrocarbon streams, and produce less particulates than conventional processes. The invention will now be more particularly described with respect to pyrolysis tar produced by steam cracking (steam cracker tar, or "SCT"). The invention is not limited to processing SCT, and this description is not meant to exclude the upgrading of pyrolysis tar produced by other forms of pyrolysis within the broader scope of the invention.

[0022] In certain aspects, the steam cracker effluent from the steam cracker furnace is cooled, for example, by indirect heat transfer in one or more transfer line exchangers. Alternatively or in addition, the steam cracker effluent and / or the cooled steam cracker effluent may be quenched (for example, by direct heat transfer). This may be done by combining the steam cracker effluent and / or the cooled steam cracker effluent with a quench oil. In at least one separation stage, the SCT is separated from the cooled and / or quenched steam cracker effluent. Certain methods of separating SCT from the steam cracker effluent and thermally treating the separated SCT are now described in more detail. The present invention is not limited to these aspects, and this description should not be construed to exclude other methods of separating and thermally treating SCT within the broader scope of the present invention.

[0023] In certain aspects, SCT is separated from the cooled and / or quenched steam cracker effluent in a separation vessel, such as a tar removal drum. The separated SCT accumulates at the bottom of the drum and is typically combined with (i) materials already present in the drum bottoms product, and (ii) optionally added flux (e.g., utility fluid) to form an SCT composition. The overhead stream removed from the tar removal drum is typically directed to at least one fractionator, such as a primary fractionator. The overhead stream typically comprises (i) ≥ 75 wt % of the remainder of the cooled and / or quenched steam cracker effluent after SCT separation, e.g., ≥ 90 wt %, such as ≥ 99 wt %; (ii) ≥ 50 wt % of any flux that may be present in the tar separation drum, e.g., ≥ 75 wt %, or ≥ 90 wt %; and (iii) ≥ 50 wt % of any quench oil (if used) directed to the tar separation drum along with the quenched steam cracker effluent, e.g., ≥ 75 wt %, such as ≥ 90 wt %. Due to the tar drum in the imperfect separator, (i) the tar drum overhead stream may contain unseparated SCT, typically ≤ 10 wt% of the total amount of SCT in the steam cracker effluent, and (ii) the tar drum drum bottoms product includes an SCT composition including the separated heat-treated SCT, ≥ 90 wt% of any flux remaining after the tar drum overhead is directed away, and ≥ 90 wt% of any quench oil remaining after the tar drum overhead is directed away. In these and some other aspects, the tar drum overhead is directed to a primary fractionator, typically for separation of a process gas stream from the tar drum overhead, the process gas stream comprising light olefins, and optionally one or more of: (i) a pyrolysis gasoline stream, (ii) a steam cracker gas oil stream, and (iii) a fractionator bottoms stream. The fractionator bottoms stream or a portion thereof can be used as a quench oil or quench oil component. In these and some other aspects, a specified SCT composition is produced by maintaining a drum bottoms product of a tar separation drum at a temperature within a specified temperature range for a residence time within a specified residence time range.

[0024] In other aspects, a tar removal drum is not used. In these and some other aspects, the cooled and / or quenched steam cracker effluent is directed directly from the cooling and / or quenching section of the effluent to one or more fractionators, such as a primary fractionator. Typically in these aspects, the primary fractionator serves to separate a process gas stream containing light olefins, and optionally one or more of: (i) a pyrolysis gasoline stream, (ii) a steam cracker gas oil stream, (iii) a quench oil stream, and (iv) a bottoms stream containing an SCT composition, which includes separated SCT. In these and some other aspects, a specified heat-treated SCT can be produced from the primary fractionator bottoms stream. For example, a bottoms pump cycle can be utilized, wherein the bottoms pump cycle has one or more sections for heating and / or cooling by indirect heat transfer to achieve a specified temperature range and a specified residence time range for heat treatment of the SCT composition.

[0025] In the aspect of containing primary fractionator, the fractionation conditions can be adjusted to reduce or substantially eliminate the formation of solids (e.g., polymers) in the bottom product of the primary fractionator and / or the quench oil stream. For example, the primary fractionator inlet temperature can be preselected in the range of 150°C to 300°C, such as 160°C to 210°C. In the conventional method of upgrading SCT, the solids produced in the first thermal treatment and / or primary fractionator are used as low-value streams, such as being directed away from a filter and / or a centrifuge. Surprisingly, it has been found that at least a portion of these solids can be converted in a prescribed second thermal treatment, and the conversion product is separated from the unconverted solids in the second SCT separation, recycled into the tar-fluid mixture, and then transferred to the first lower density portion in the first SCT separation. Doing so will increase the amount of substances in the first lower density portion of higher value, which in turn can be the feed amount for a beneficial process such as SATC.

[0026] Certain aspects of the invention include separating at least a first higher density portion and a first lower density portion from a SCT composition. The separation may be performed in one or more centrifuge stages (collectively referred to as the "first centrifuge"). Since SCT compositions typically exhibit relatively large viscosities within the specified processing temperature range, a stream containing a first utility fluid and / or a first separation fluid (these having a lower viscosity than the SCT) is typically added upstream of at least this separation. In these cases, the first higher density portion and the first lower density portion are separated from a tar-fluid mixture containing the SCT composition and the added utility fluid / separation fluid stream.

[0027] The first lower density portion is typically subjected to additional processing, such as in a solvent assisted tar conversion (SATC) process. For example, conventional SATC processes are described in PCT Patent Application Publication No. WO2018 / 111577 and U.S. Patent Application Serial Nos. 62 / 659183 and 62 / 750636, each of which is incorporated herein by reference.

[0028] In a conventional SATC, the first higher density portion in the SCT can be diverted from the process. Instead of doing so, certain aspects of the present invention also include further processing of this stream, such as one or more of the following: (1) comminuting (e.g., grinding) the first higher density portion, which achieves a solid size (e.g., particle size) reduction to produce a comminuted first higher density portion, (2) diluting the first higher density portion, such as before and / or after comminuting by adding one or more of the following: (a) a second utility fluid, (b) a second separation fluid, and (c) a recycle stream to produce a diluted first higher density portion, and (3) heat treating the comminuted and / or diluted first higher density portion in a second thermal treatment to produce a heat-treated first higher density portion. It has been found that diluting the first higher density portion prior to the second thermal treatment can reduce or significantly prevent asphaltene formation (oligomerization) reactions that might otherwise occur in the second thermal treatment. It has also been found that the amount of solids (weight basis, based on the weight of the first higher density portion) in the heat-treated first higher density portion is less than the amount of solids in the first higher density portion. This reduction in solids occurs regardless of whether comminution is performed prior to the second heat treatment.

[0029] For example, in one or more centrifuges (collectively referred to as "second centrifuges"), the second lower density fraction and the second higher density fraction are separated from the heat-treated first higher density fraction. The second higher density fraction can be transported away. At least a portion of the second lower density fraction can be returned to (e.g., recycled to) the process. For example, certain aspects of the present invention include adding at least a portion of the second lower density fraction to one or more of the following: (i) steam cracker effluent, for example as quench oil, (ii) SCT before and / or during the first thermal treatment, (iii) SCT composition, (iv) tar-fluid mixture before and / or during separation of the first higher density fraction and the first lower density fraction, (v) the first higher density fraction, and (vi) the first lower density fraction. Recycling at least a portion of the second lower density fraction to one or more of streams (i) to (vi) will result in a highly desirable increase in the amount (by weight) of the first lower density fraction separated from the heat-treated SCT.

[0030] In certain aspects, at least a portion of the second lower density portion is recycled and combined with the SCT composition. Typically, a first utility fluid is also added to the SCT composition. The combination of the SCT composition, the recycled portion of the second lower density portion, and the first utility fluid added if any (collectively referred to as the tar-fluid mixture form) is directed to a separation section for separation of the first lower density portion and the first higher density portion. Doing so will increase the weight ratio of the first lower density portion: the first higher density portion, and thus increase the amount of the first lower density portion available for further processing, such as in the SATC process. This, in turn, will increase the amount of hydrotreated tar required to be produced by the SATC compared to a conventional SCT conversion process that does not use a second thermal treatment or a second centrifugation.

[0031] Compared to conventional methods and apparatus for tar upgrading, the methods and apparatus of the present disclosure provide the ability to upgrade increased amounts of SCT using downstream hydroprocessing. Moreover, in aspects utilizing a tar cut drum upstream of the primary fractionator, the primary fractionator bottoms portion can be maintained at a sufficiently low temperature to reduce the amount of undesirable polymerization that might otherwise occur in the bottoms portion of a primary fractionator operating at a greater temperature, e.g., >160°C.

[0032] definition

[0033] "Hydrocarbon-containing feed" refers to a flowable composition, such as a liquid phase, high viscosity, and / or slurry composition, which (i) includes carbon bonded to hydrogen, and (ii) has a mass density greater than gasoline, typically ≥ 0.72 Kg / L, such as ≥ 0.8 Kg / L, such as ≥ 0.9 Kg / L, or ≥ 1.0 Kg / L, or ≥ 1.1 Kg / L. Such a composition may include one or more of crude oil, crude oil fractions, and compositions derived therefrom, which (i) has a kinematic viscosity at 50°C of ≤ 1.5×10 3 cSt, (ii) contains carbon bonded to hydrogen, and (iii) has a mass density ≥ 740 kg / m 3 The hydrocarbon feed typically has a final boiling point at atmospheric pressure ("atmospheric boiling point", or "normal boiling point") ≥ 430°F (220°C). Certain hydrocarbon feeds include components with atmospheric boiling points ≥ 290°C, such as hydrocarbon feeds containing ≥ 20% (by weight), such as ≥ 50%, such as ≥ 75%, or ≥ 90% components with atmospheric boiling points ≥ 290°C. When illuminated by sunlight, including luminance ≤ 7 cd / m 2Certain hydrocarbon feeds appear to have a black or dark brown color when illuminated by those of the invention, where brightness is measured according to CIECAM02 established by the Commission Internationale de l'éclairage. Non-limiting examples of such feeds include pyrolysis tar, SCT, vacuum fracturing residue, atmospheric fracturing residue, vacuum gas oil ("VGO"), atmospheric gas oil ("AGO"), heavy atmospheric gas oil ("HAGO"), steam cracking gas oil ("SCGO"), deasphalted oil ("DAO"), catalytic cycle oil ("CCO", including light catalytic cycle oil, "LCCO", and heavy catalytic cycle oil, "HCCO"), natural and synthetic feeds derived from tar sands or shale oil, coal.

[0034] The term "pyrolysis tar" refers to a mixture of (a) hydrocarbons having one or more aromatic components and optionally (b) non-aromatic and / or non-hydrocarbon molecules, the mixture being derived from the pyrolysis of hydrocarbons, and at least 70% of the mixture having a boiling point of ≥ about 550°F (290°C) at atmospheric pressure. Certain pyrolysis tars have an initial boiling point of ≥ 200°C. For certain pyrolysis tars, ≥ 90.0 wt% of the pyrolysis tar has a boiling point of ≥ 550°F (290°C) at atmospheric pressure. The pyrolysis tar may include, for example, ≥ 50.0 wt%, for example, ≥ 75.0 wt%, for example, ≥ 90.0 wt% of hydrocarbon molecules having (i) one or more aromatic components and (ii) a carbon number of ≥ about 15 (including mixtures and aggregates thereof), based on the weight of the pyrolysis tar. The pyrolysis tar generally has an average carbon content of ≤ 1.0×10 3 The metal contents in ppmw, based on the weight of the pyrolysis tar, are much lower than those found in crude oils (or crude oil components) of the same average viscosity.

[0035] "SCT" means pyrolysis tar obtained from steam cracking. Typically, SCT comprises (a) a mixture of hydrocarbons having one or more aromatic components and optionally (b) non-aromatic and / or non-hydrocarbon molecules, wherein 90% of the total boiling point of the mixture is ≥ 550°F (290°C) (e.g., ≥ 90.0 wt% of the SCT molecules have an atmospheric boiling point ≥ 550°F (290°C)). SCT may contain, based on the weight of SCT, > 50.0 wt% (e.g., > 75.0 wt%, such as > 90.0 wt%) hydrocarbon molecules having (i) one or more aromatic components and (ii) carbon number ≥ 15 (including mixtures and aggregates thereof). SCT generally has a carbon number ≤ 1.0×10 3 The metal content in ppmw is based on the weight of the SCT (e.g., the metal content is much lower than the metal content found in crude oil (or crude oil components) of the same average viscosity). Typically, the mass density of SCT is ≥1.0 Kg / L, e.g., ≥1.05 Kg / L, e.g., ≥1.1 Kg / L, or ≥1.15 Kg / L.

[0036] The present invention is not limited to pyrolysis tars, such as SCT, and this description should not be interpreted as excluding other tars or similar compositions from the broader scope of the present invention. For example, in certain aspects, the tar can be or include one or more tars, asphalts, resids, gums, resins, and the like, such as those obtained from petroleum processes such as crude oil processing, resid processing, deasphalting, processing atmospheric and / or vacuum tower bottoms, processing compositions derived from catalytic cracking (e.g., processing of major tower bottoms), compositions obtained from hydroprocessing (e.g., processing of asphalt obtained and / or derived from crude oil processing, resid processing, including hydroprocessing of resids, and the like), etc. Therefore, the term "tar" encompasses these compositions and pyrolysis tars such as SCT.

[0037] "Solvent-assisted tar conversion" or ("SATC") is a method of producing upgraded tars, such as SCT. The method includes hydroprocessing a tar stream in the presence of a utility fluid and is generally described in PCT Patent Application Publication No. WO 2018-111577. For example, SATC may include hydroprocessing one or more SCT streams, including those that have been previously pretreated in the presence of a utility fluid, to produce a hydroprocessed tar having a lower viscosity, improved blending characteristics, fewer heteroatom impurities, and less solids content (e.g., fewer particulates) than SCT.

[0038] "Tar heavies" ("TH") refers to hydrocarbon pyrolysis products typically included in pyrolysis tars, such as SCT. TH typically has an atmospheric boiling point > 565°C and contains > 5 wt% molecules with multiple aromatic nuclei based on the weight of the tar. TH is typically solid at 25°C and generally includes a SCT fraction that is insoluble in a 5:1 (vol:vol) ratio of n-pentane:SCT at 25°C. TH generally includes asphaltenes and other high molecular weight molecules.

[0039] Tar can contain various solid forms, wherein the term "solid" encompasses solid phase materials and materials such as semi-solids, quasi-solids, and the like having certain liquid-like characteristics and certain solid-like characteristics. The term "solid" also encompasses materials in particle form, which means solids in the form of granules. The term particle includes polymerized asphaltene particles, polymerized coke particles, pyrolytic coke particles, inorganic fines, other organic or inorganic particles, or any combination thereof. The particles present in tar typically have a specific gravity of about 1.04 to about 1.5. When a flowable material, such as tar or upgraded tar, is compared with another flowable material in terms of granular content (regardless of weight, volume or quantity), the comparison is performed under substantially the same conditions, such as substantially the same temperature, pressure, etc. When a sample of a flowable material is obtained from a process for comparison elsewhere, such as in a laboratory, the granular content comparison can be performed under (i) conditions simulating the process conditions and / or (ii) environmental conditions, such as a temperature of 25° C. and a pressure of 1 bar (absolute pressure).

[0040] Coke is a solid composition that can be found in certain tars, for example, pyrolytic tars such as SCT. "Pyrolytic coke" or "pyrolytic coke particles" refers to material produced by pyrolysis of organic molecules present in SCT and / or quench oil. Pyrolytic coke is in solid form, such as particle form. "Polymerized coke" or "polymerized coke particles" refers to material produced by oligomerization of olefin molecules that can be seeded with small fouling agent particles. Olefin molecules can be present in SCT and / or quench oil. Polymerized coke materials or particles typically have a specific gravity of about 1.04 to about 1.1, which is much less than the specific gravity of coke solids (non-polymerized materials) typically found in tars, which is about 1.2 to about 1.3.

[0041] "Solubility blend value (S)" and "insolubility value (I)" are described in U.S. Pat. No. 5,871,634 and are determined using n-heptane as the so-called "non-polar nonsolvent" and chlorobenzene as the solvent, which is incorporated herein by reference in its entirety. The S and I values ​​are determined at oil to test liquid mixture weight ratios ranging from 1 to 5. Various such values ​​are referred to herein, for example, "I TC " refers to the insolubility value of a pyrolysis tar composition, such as an SCT composition; "I TF " refers to the insolubility value of the tar-fluid mixture; "I LD " refers to the insolubility value of the first lower density fraction separated from the tar-fluid mixture; "I FHD " refers to the insolubility value of the first higher density portion, especially the liquid phase thereof; "S 流体 " refers to the solubility blending value of a fluid or, if appropriate, a fluid-rich stream. In conventional notation, these I and S values ​​are often defined as I N and S BN .

[0042] The terms "higher density portion" and "lower density portion" are relative terms, which means the mass density (ρ 2 ) is higher than the density of the lower density part (ρ 1 ), for example, 2 ≥1.01*ρ 1 , for example 2 ≥1.05*ρ 1 , or 2 ≥1.10*ρ 1 In some aspects, the higher density portion contains primarily solid components and the lower density portion contains primarily liquid components. The higher density component may also include liquid components separated from the lower density portion. Likewise, the lower density portion may contain solids (even in particulate form), such as those having a density similar to that of the liquid hydrocarbon components of the pyrolysis tar.

[0043] The term "portion" generally refers to one or more components derived from a mixture, such as a tar-fluid mixture.

[0044] Except for its use in terms of parts per million, the term "part" is used relative to a specified process stream and generally means that it is less than the entire specified stream that may be selected.

[0045] In this specification, the particle size in hydrocarbons can be characterized by laser diffraction. Note that the particle size distribution can vary between different equipment types when performing laser diffraction to characterize the particle size. The particle size distribution can be characterized using a Mastersizer from Malvern Instruments. Optionally, the particle size distribution of a sample can be determined according to a suitable ASTM method, such as ASTM D4464.

[0046] Pyrolysis and pyrolysis tar

[0047] Pyrolysis tar is a product or by-product of hydrocarbon pyrolysis, for example, steam cracking. Steam cracking is now described in more detail. The disclosure of the present invention is not limited to the use of pyrolysis tar produced by steam cracking, and this specification is not meant to exclude the use of pyrolysis tar formed by other pyrolysis processes within the broader scope of the disclosure of the present invention.

[0048] Steam Cracking

[0049] A steam cracking unit typically includes a furnace facility for producing a steam cracking effluent and a recovery facility for removing various products and by-products, such as light olefins and SCT, from the steam cracking effluent. The furnace facility typically includes a plurality of steam cracking furnaces. A steam cracking furnace typically includes two main sections: a convection section and a radiant section, the radiant section typically containing a fired heater. Flue gas from the fired heater is transferred from the radiant section to the convection section. The flue gas flows through the convection section and is then directed away, for example to one or more treatments for removal of combustion by-products such as NO x . A hydrocarbon-containing feed is introduced into a tubular coil (convection coil) located in a convection section for preheating. Steam is added to the preheated hydrocarbon-containing feed to produce a steam cracking feed (also called a steam cracker feed). Typically, the steam cracking feed is reintroduced into the convection section, for example via an additional convection coil, to produce a heated steam cracking feed. The combination of indirect heating by flue gases and direct heating by added steam in the convection section can result in vaporization, or additional vaporization, when the hydrocarbon feed is already at least partially in the gas phase, if the hydrocarbons are first introduced into the convection section. Optionally, at least a portion of any heated steam cracking feed that is not in the gas phase is separated and directed away. The heated steam cracking feed or the gas phase components separated therefrom can be transferred from the convection coil to one or more tubular radiant coils located in the radiant section. The indirect heating of the steam cracking feed in the radiant tubes results in cracking of at least a portion of the hydrocarbon components in the steam cracking feed. Steam cracking conditions within the radiant section may include, for example, one or more of the following: (i) a temperature range of 760°C to about 1200°C, such as about 760°C to about 880°C, (ii) a pressure range of 1 to 5 bar (absolute pressure), or (iii) a cracking residence time range of 0.10 to 2 seconds.

[0050] In certain aspects, the hydrocarbon-containing feed comprises crude oil or a crude oil fraction, such as those containing ≥1 wt% hydrocarbons having a normal boiling point ≥566°C (about 1050°F), based on the weight of the hydrocarbon-containing feed, e.g., ≥5 wt%, or ≥10 wt%. In these aspects, it is typically beneficial to utilize a steam cracking furnace that further comprises a vapor-liquid separation section, such as a vapor-liquid separation drum, which is heat integrated with (but typically located external to) the convection section of the steam cracking furnace.

[0051] When such a vapor-liquid separation section is used, a stream of mainly vapor phase and a stream of mainly non-vapor phase are separated from the steam cracking feed in the vapor-liquid separation section. For example, ≥50 wt% of the portion of crude oil (or crude oil fraction) having a normal boiling point ≥566°C can be transferred to the stream of non-vapor phase. The separated stream of mainly vapor phase is typically exposed to additional heating in the convection section before cracking. For the stream of mainly vapor phase, ≥70 wt%, such as ≥90 wt% of the stream is in the vapor phase. For the stream of mainly non-vapor phase, ≥70 wt%, such as ≥90 wt% of the stream is not in the vapor phase.

[0052] At least a portion of the stream of the main gas phase is directed to the inlet of at least one radiant coil located in the radiant section for cracking under steam cracking conditions. The radiant coil includes an inlet and an outlet, and the steam cracking conditions include one or more of the following: a temperature range of about 760°C to about 1200°C (e.g., about 880°C to about 1,200°C, such as about 1,000°C to about 1,200°C) at the outlet of the radiant coil; a steam cracking pressure range of about 1 bar (absolute pressure) to about 10 bar (absolute pressure) at the outlet of the radiant coil (e.g., about 1 bar (absolute pressure) to about 5 bar (absolute pressure), alternatively about 6 bar (absolute pressure) to about 10 bar (absolute pressure)); and / or a steam cracking residence time range of about 0.1 seconds to about 2 seconds in the radiant coil. The steam cracker effluent is directed from the radiant section for cooling and / or quenching. At least a portion of the SCT is separated from the cooled and / or quenched steam cracker effluent to produce an SCT composition.

[0053] Certain hydrocarbonaceous feeds will now be described in greater detail. The present invention is not limited to these hydrocarbonaceous feeds, and this specification should not be construed to exclude the steam cracking of other hydrocarbonaceous feeds within the broader scope of the present invention.

[0054] Although the hydrocarbon-containing feed may include one or more light hydrocarbons such as methane, ethane, propane, butane, etc., the SCT yield is greater when the hydrocarbon-containing feed includes a large amount of higher molecular weight hydrocarbons. For example, the hydrocarbon-containing feed may include ≥ 1.0 wt%, such as ≥ 10 wt%, such as ≥ 25.0 wt%, or ≥ 50.0 wt% (based on the weight of the hydrocarbon-containing feed) hydrocarbon compounds in the liquid phase and / or solid phase at 25° C. and 1 bar absolute pressure.

[0055] The hydrocarbon portion of the hydrocarbon-containing feed typically includes ≥10.0 wt%, for example, ≥50.0 wt%, for example ≥90.0 wt% (based on the weight of the hydrocarbon portion) of one or more of naphtha, gas oil, vacuum gas oil, waxy residue, atmospheric residue, residue mixture, crude oil and SCT. Certain hydrocarbon-containing feeds include ≥about 0.1 wt% asphaltenes. When the hydrocarbon-containing feed includes crude oil and / or one or more fractions thereof, the crude oil is optionally a desalted crude oil. Suitable crude oils include, for example, high-sulfur unprocessed crude oils, such as those rich in polycyclic aromatic hydrocarbons. Crude oil fractions can be produced by separating the atmospheric pressure tube furnace ("APS") bottom product from the crude oil and then subjecting the APS bottom product to a vacuum tube furnace ("VPS") treatment. Suitable crude oils include, for example, the hydrocarbon-containing feed may include ≥90.0 wt% of one or more crude oil fractions, such as those obtained from atmospheric pressure APS and / or VPS; waxy residue; atmospheric residue; naphtha contaminated with crude oil; various residue mixtures.

[0056] Steam cracking feed is typically produced by heating a hydrocarbonaceous feed in one or more convection coils and combining the heated hydrocarbonaceous feed with steam. The steam cracking feed typically comprises ≥ 10.0 wt% hydrocarbons, based on the weight of the steam cracking feed, e.g., ≥ 25.0 wt%, ≥ 50.0 wt%, e.g., ≥ 65 wt%. Typically, ≥ 90 wt% of the steam cracker feed is steam.

[0057] In certain aspects, SCT is separated from the cooled and / or quenched steam cracker effluent in one or more separation sections. Conventional separation equipment can be used to separate SCT and other products and by-products from the cooled and / or quenched steam cracking effluent, such as one or more flash drums, separation drums, fractionators, water quench towers, indirect condensers, etc. Suitable separation sections are described in U.S. Patent No. 8,083,931 and in PCT Patent Application Publication No. WO2018-111574, which are incorporated herein by reference in their entirety. SCT can be separated from the quenched effluent itself and / or from one or more streams (which have been separated from the cooled and / or quenched effluent). For example, SCT can be separated from the bottom product of a flash drum (e.g., the bottom product of one or more tar separation drums located downstream of a steam cracking furnace and upstream of a primary fractionator). Some SCT is a mixture of the bottom product of a primary fractionator and the bottom product of a tar separation drum.

[0058] Representative SCTs are now described in more detail. Embodiments are not limited to use with these SCTs, and this description is not meant to exclude other SCTs, or other treatments of pyrolysis tars, from the broader scope of the present disclosure.

[0059] Steam Cracker Tar ("SCT")

[0060] Typically, the cooled and / or quenched steam cracker effluent comprises steam, molecular hydrogen, hydrocarbons (saturated and unsaturated hydrocarbons), non-hydrocarbon compositions, and solids (typically hydrocarbon solids, such as TH, and non-hydrocarbon solids), including particulates. For example, the cooled and / or quenched steam cracker effluent may comprise ≥ 1.0 wt% C 2 unsaturates and ≥ 0.1 wt % TH, the weight percentages being based on the weight of the cooled and / or quenched steam cracker effluent. It is also typical for the cooled and / or quenched steam cracker effluent to include ≥ 0.5 wt % TH, such as ≥ 1.0 wt % TH. The SCT in the cooled and / or quenched steam cracker effluent typically includes ≥ 50.0 wt %, such as ≥ 75.0 wt %, such as ≥ 90.0 wt % of all TH in the cooled and / or quenched steam cracker effluent. The TH is typically in the form of aggregates comprising hydrogen and carbon and having an average size in at least one dimension ranging from 10.0 nm to 300.0 nm and an average number of carbon atoms of ≥ 50. Generally, TH comprises ≥50.0 wt%, e.g., ≥80.0 wt%, e.g., ≥90.0 wt% of aggregates having a C:H atomic ratio in the range of 1.0 to 1.8, a molecular weight in the range of 250 to 5000, and a melting point in the range of 100° C. to 700° C. SCT typically comprises ≥50.0 wt%, e.g., ≥75.0 wt%, e.g., ≥90.0 wt% of TH in the quench effluent, based on the total weight of TH in the quench effluent.

[0061] Representative SCTs typically have (i) a TH content ranging from 5.0 wt% to 40.0 wt%, based on the weight of the SCT, (ii) an API gravity (measured at a temperature of 15.8°C) of ≤8.5°API, e.g., ≤8.0°API, or ≤7.5°API; and (iii) a TH content ranging from 200 cSt to 1.0×10 7 cSt, e.g., 1×10 3 cSt to 1.0×10 7 The 50°C viscosity of the SCT may be, for example, >0.5 wt%, or >1 wt%, or more, such as in the range of 0.5 wt% to 7.0 wt%, based on the weight of the SCT. In aspects where the steam cracking feed does not contain significant amounts of sulfur, the SCT may include ≤0.5 wt% sulfur, such as ≤0.1 wt%, such as ≤0.05 wt% sulfur, based on the weight of the SCT.

[0062] The SCT may have, for example, (i) a TH content ranging from 5.0 wt% to 40.0 wt%, based on the weight of the SCT; (ii) a TH content of 1.01 g / cm at 15°C; 3Up to 1.19 g / cm 3 Density range, for example, range of 1.07 g / cm 3 Up to 1.18g / cm 3 and (iii) a viscosity at 50°C in the range of ≥200 cSt, e.g., ≥600 cSt, or in the range of 200 cSt to 1.0×10 7 cSt. For density range ≥1.10g / cm at 15℃ 3 , for example, ≥1.12 g / cm 3 , ≥1.14g / cm 3 , ≥1.16g / cm 3 , or ≥1.17g / cm 3 The prescribed hydroprocessing is particularly advantageous for SCT of ≥1.0×10 4 cSt, e.g. ≥1.0×10 5 cSt, or ≥1.0×10 6 cSt, or even ≥1.0×10 7 cSt 50°C kinematic viscosity. Optionally, the SCT has an I > 80 N and >70 wt% of the pyrolysis tar molecules have atmospheric boiling points ≥290°C. Typically, the insoluble content ("IC T ")≥0.5wt%, for example,≥1wt%, for example≥2wt%, or≥4wt%, or≥5wt%, or≥10wt%.

[0063] In at least one embodiment, SCT comprises a mixture of hydrocarbons having one or more aromatic components and optionally non-aromatic hydrocarbons and / or non-hydrocarbons, and at least 70% of the mixture has a boiling point greater than or equal to about 550°F (290°C) at atmospheric pressure. SCT typically comprises hydrocarbons having (i) one or more aromatic components and (ii) a carbon number greater than about 15 (including mixtures and aggregates thereof). SCT typically has a metal content less than or equal to 1000 ppmw, based on the weight of the pyrolysis tar, which is much less than the metal content found in crude oil (or crude oil components) of the same average viscosity. Optionally, SCT has a normal boiling point of ≥290°C and a viscosity at 15°C of ≥1×10 4 cSt, and density ≥1.1g / cm 3. The SCT may be a mixture comprising a first SCT and one or more additional pyrolysis tars, such as a combination of the first SCT and one or more additional SCTs. When the SCT is a mixture, typically at least 70 wt% of the mixture has a normal boiling point of at least 290°C and includes olefins that contribute to the reactivity of the tar under hydroprocessing conditions. When the mixture includes a first and a second pyrolysis tar (one or more of which are optionally SCTs), ≥ 90 wt% of the second pyrolysis tar optionally has a normal boiling point of ≥ 290°C.

[0064] It has been found that an increase in reactor fouling occurs during the hydroprocessing of a tar-fluid mixture containing SCT with an excess of olefins. In order to reduce the amount of reactor fouling, it is beneficial that the SCT has an olefin content of ≤10.0 wt% (based on the weight of the SCT), e.g., ≤5.0 wt%, such as ≤2.0 wt%. More specifically, it has been observed that less reactor fouling occurs during the hydroprocessing when the SCT has (i) ≤5.0 wt% vinyl aromatic content (based on the weight of the SCT), e.g., ≤3 wt%, such as ≤2.0 wt% and / or (ii) an amount of aggregates incorporated with vinyl aromatics ≤5.0 wt% (based on the weight of the SCT), e.g., ≤3 wt%, such as ≤2.0 wt%.

[0065] SCT Composition

[0066] The SCT composition typically includes ≥40 wt% SCT that has been separated from the steam cracker effluent, based on the weight of the SCT composition, for example, ≥60 wt%, such as ≥70 wt%, or more. The SCT composition may further include a composition formed during the thermal treatment of the SCT. In certain aspects, for example, in aspects where (i) quench oil is not used to quench the steam cracker effluent and (ii) no utility fluid is added to the tar separation drum, the SCT composition may include ≥90 wt% thermally treated SCT, for example, ≥95 wt%, or ≥99 wt%, or more. The SCT composition typically includes ≥90.0 wt% SCT that has been (i) separated from the cooled and / or quenched steam cracker effluent, and (ii) thermally treated. The SCT may further include SCT-derived materials that are recycled to the first thermal treatment or an upstream location thereof (e.g., a recycled portion of the second lower density portion). SCT compositions obtained from one or more specified SCT sources may contain ≥ 50.0 wt% SCT based on the weight of the stream, for example, ≥ 75.0 wt%, such as ≥ 90.0 wt%, or more. In aspects where ≥50 wt%, or ≥75 wt%, or ≥90 wt%, or more of the SCT in the SCT composition is SCT separated in a tar drum, the remainder of the SCT stream (e.g., that portion of the stream, if any, that is not SCT) by weight, greater than 90 wt%, typically includes one or more of the following: (i) any flux (e.g., utility fluid) that remains with the SCT after the tar drum overhead stream is directed away, in aspects where flux is added to the tar drum; (ii) any quench oil that may remain with the SCT after the tar drum overhead stream is directed away, in aspects where quench oil is introduced into the steam cracker effluent and / or the cooled steam cracker effluent; (iii) materials formed during or as a result of the first thermal treatment; and (iv) particulate matter.

[0067] Aspects in which the first thermal treatment comprises heat soaking in a tar separation drum are now described in more detail. The invention is not limited in these respects, and this description should not be interpreted as excluding (i) other forms of thermal treatment, such as thermal treatment of the SCT composition in a primary fractionator, or (ii) other forms of thermal treatment of pyrolysis tar.

[0068] SCT heat treatment by heat soaking

[0069] During the hot soaking process, at least the separated SCT is maintained at a hot soaking position, such as in the bottom product area of ​​the tar separation drum, or in one or more soaker containers adapted for this purpose and located outside the tar separation drum. Conventional equipment for hot soaking SCT can be used, but the present invention is not limited to this. A conventional equipment structure for hot soaking SCT is disclosed in PCT Patent Application Publication No. WO2018-111574, which discloses hot soaking SCT in the bottom product area of ​​the tar separation drum, and optionally in the presence of a utility fluid added as a flux. The flux can be used as an auxiliary agent in separation and hot soaking, such as a flux having substantially the same composition as the first utility fluid. Separation and hot soaking of SCT can be performed before, during and / or after the addition of the flux. Since aspects of the present invention include at least one additional heat treatment (second heat treatment) of a stream derived from the SCT composition, the heat treatment of the separated SCT is referred to as "first heat treatment" or "first heat soak".

[0070] Using, for example, the heat soaking structure disclosed in PCT Patent Application Publication No. WO 2018-111574, at least the separated SCTs can be independently heated and / or cooled to reach a desired heat soaking temperature (T HS1 ) and the required duration (t HS1 ). Temperature T HS1 Typically in the range of about 200°C, about 220°C, about 230°C, about 240°C, about 250°C, about 260°C, about 270°C, about 275°C, about 280°C, or about 290°C to about 295°C, about 300°C, about 310°C, about 320°C, about 325°C, about 330°C, about 340°C, about 350°C, about 360°C, about 375°C, about 400°C, about 450°C, about 500°C, or more. For example, T HS1The range may be about 200°C to about 500°C, about 230°C to about 500°C, about 250°C to about 500°C, about 280°C to about 500°C, about 290°C to about 500°C, about 300°C to about 500°C, about 320°C to about 500°C, about 350°C to about 500°C, about 250°C to about 450°C, about 280°C to about 450°C, about 290°C to about 450°C, about 300°C to about 450°C, about 320°C to about 450°C 0° C., about 350° C. to about 450° C., about 250° C. to about 400° C., about 280° C. to about 400° C., about 290° C. to about 400° C., about 300° C. to about 400° C., about 320° C. to about 400° C., about 350° C. to about 400° C., about 250° C. to about 350° C., about 280° C. to about 350° C., about 290° C. to about 350° C., about 300° C. to about 350° C., about 320° C. to about 350° C., or about 330° C. to about 350° C. Although it is not required to maintain the separated SCT at a substantially constant temperature (i.e., at T ) during the heat soaking process, the temperature of the separated SCT may be maintained at a substantially constant temperature (i.e., at T ). HS1 of the temperature within a specified range), but typically this is done.

[0071] Typically, the first heat soak is performed for a predetermined time t in the range of about 2 min, about 5 min, about 10 min, about 12 min, or about 15 min to about 20 min, about 25 min, about 30 min, about 45 min, about 60 min, about 90 min, about 2 hr, about 3 hr, about 5 hr, or longer. HS1 For example, t HS1 The range of t can be about 5 min to about 5 hr, about 5 min to about 3 hr, about 5 min to about 2 hr, about 5 min to about 1 hr, about 5 min to about 45 min, about 5 min to about 30 min, or about 5 min to about 20 min. In one or more examples, t HS1 The range of about 2 min, about 5 min, about 10 min, about 15 min, or about 20 min to about 30 min, about 45 min, about 60 min, about 90 min, about 2 hr, about 3 hr, or about 5 hr to dissolve and / or decompose at least a portion of the particles present in the separated SCT.

[0072] Although not wishing to be bound by any theory or model, it is believed that the first heat soak dissolves and / or decomposes the particles within the separated SCT, or otherwise reduces the particle content. It is also observed that while maintaining the separated SCT at temperature T HS1 Next scheduled time t HS1Thereafter, the SCT composition typically contains fewer particles than the separated SCT. In one or more embodiments, during and / or as a result of the first heat soak, about 25 wt%, about 30 wt%, about 35 wt%, or about 40 wt% to about 45 wt%, about 50 wt%, about 60 wt%, about 70 wt%, about 75 wt%, about 80 wt%, about 85 wt%, about 90 wt%, about 92 wt%, about 95 wt%, about 97 wt%, about 98 wt%, about 99 wt%, or more of the particles in the separated SCT are dissolved and / or decomposed. In some instances, at least 25 wt%, at least 30 wt%, at least 35 wt%, at least 40 wt%, at least 45 wt%, at least 50 wt%, at least 60 wt%, at least 70 wt%, at least 75 wt%, at least 80 wt% to about 85 wt%, about 90 wt%, about 92 wt%, about 95 wt%, about 97 wt%, about 98 wt%, about 99 wt%, or more of the particles within the separated SCT are dissolved and / or decomposed during and / or as a result of the first heat soak. For example, during and / or as a result of the first heat soak, about 25 wt % to about 99 wt %, about 30 wt % to about 99 wt %, about 35 wt % to about 99 wt %, about 40 wt % to about 99 wt %, about 45 wt % to about 99 wt %, about 50 wt % to about 99 wt %, about 60 wt % to about 99 wt %, about 70 wt % to about 99 wt %, about 75 wt % to about 99 wt %, about 25 wt % to about 95 wt %, about 30 wt % to about 95 wt %, about 35 wt % to about 95 wt %, about 40 wt % to about 95 wt %, about 45 wt % to about 95 wt %, about 50 wt % to about 95 wt %, about 60 wt % to about 95 wt %, about 7 ...5 %, about 25 wt % to about 90 wt %, about 30 wt % to about 90 wt %, about 35 wt % to about 90 wt %, about 40 wt % to about 90 wt %, about 45 wt % to about 90 wt %, about 50 wt % to about 90 wt %, about 60 wt % to about 90 wt %, about 70 wt % to about 90 wt %, about 75 wt % to about 90 wt %, about 25 wt % to about 80 wt %, about 30 wt % to about 80 wt %, about 35 wt % to about 80 wt %, about 40 wt % to about 80 wt %, about 45 wt % to about 80 wt %, about 50 wt % to about 80 wt %, about 60 wt % to about 80 wt %, about 70 wt % to about 80 wt %, or about 75 wt % to about 80 wt % of the particles within the separated SCT are dissolved and / or decomposed.

[0073] The SCT composition typically includes the separated SCT that is now heat treated, plus any added flux, minus that portion of the separated SCT that may be converted during or as a result of the first heat treatment, plus at least a portion of certain conversion products (e.g., solids, such as polymer particulates) that may be formed during or as a result of the first heat treatment. Other examples of the latter class include certain compositions (e.g., those having a normal boiling point range similar to that of SCT) that may result from decomposition during the first heat treatment of any solids present in the separated SCT. It has been discovered that certain solids, such as particulate solids, are formed by polymerization of the separated SCT during or as a result of the first heat treatment, such as in a tar cut drum and / or primary fractionator.

[0074] The SCT composition is further processed, including separating a first higher density portion and a first lower density portion in a first stage of SCT separation ("first SCT separation stage"). At least a portion of any solids formed during or as a result of the first thermal treatment typically resides in the first higher density portion.

[0075] Although the SCT composition may be the feed to the first SCT separation stage, it is typical to combine the SCT composition with a recycle portion of the second lower density portion upstream of the first SCT separation stage to form a tar-fluid mixture. Certain representative tar-fluid mixtures are now described in more detail. The present invention is not limited to these tar-fluid mixtures, and within the broader scope of the present invention, this description should not be interpreted as excluding other tar-fluid mixtures within the broader scope of the present invention.

[0076] Tar-fluid mixture

[0077] The tar-fluid mixture typically includes an SCT composition and a fluid. The fluid includes a recycle portion of the second lower density portion and typically further includes a first utility fluid and / or a first separation fluid. The amount of fluid in the tar-fluid mixture (e.g., by weight) typically ranges from 20 wt% to 60 wt%, for example, 30 wt% to 50 wt%. The amount of the recycle portion of the second lower density portion in the fluid is typically substantially equal to the amount of the recycle portion of the second lower density portion during or as a result of the second thermal treatment (e.g., using Figure 2) converted to a lower density material (typically particles), plus the weight of diluent (e.g., second utility fluid and / or second separation fluid) added to the first higher density fraction, the comminuted first higher density fraction, the diluted first higher density fraction, and / or the heat treated first higher density fraction. Typically, ≥50 wt% of the remainder of the fluid (e.g., that portion of the fluid that is not the recycled second lower density fraction) is the first utility fluid and / or first separation fluid, e.g., ≥75 wt%, such as ≥90 wt%, or ≥99 wt%. The first utility fluid (and / or first separation fluid) when used may be added to (i) the SCT composition (which may already contain at least some utility fluid as a flux) and / or (ii) a mixture of the SCT composition and the recycled portion of the second lower density fraction. In other words, the first utility fluid and / or first separation fluid may be added to the SCT composition before, during, and / or after the SCT composition is combined with the recycled portion of the second lower density fraction. The viscosity of the tar-fluid mixture is lower than that of the SCT composition.

[0078] The tar-fluid mixture typically contains ≥5 wt % of the SCT composition, e.g., ≥10 wt %, ≥20 wt %, ≥30 wt %, ≥40 wt %, ≥50 wt %, ≥60 wt %, ≥70 wt %, ≥80 wt %, or ≥90 wt % of the SCT composition, based on the total weight of the tar-fluid mixture (e.g., the combined weight of all components in the tar-fluid mixture). Additionally or alternatively, the tar-fluid mixture may include ≤10 wt % of the SCT composition, e.g., ≤20 wt %, ≤30 wt %, ≤40 wt %, ≤50 wt %, ≤60 wt %, ≤70 wt %, ≤80 wt %, ≤90 wt %, or ≤95 wt % of the SCT composition, based on the total weight of the tar-fluid mixture. Explicitly disclosed ranges include combinations of any of the above enumerated values, for example, about 5 wt % to about 95 wt %, about 5 wt % to about 90 wt %, about 5 wt % to about 80 wt %, about 5 wt % to about 70 wt %, about 5 wt % to about 60 wt %, about 5 wt % to about 50 wt %, about 5 wt % to about 40 wt %, about 5 wt % to about 30 wt %, about 5 wt % to about 20 wt %, or about 5 wt % to about 10 wt % of the SCT composition.

[0079] In addition to the SCT composition, the tar-fluid mixture typically further includes ≥5 wt % utility fluid, e.g., ≥10 wt %, ≥20 wt %, ≥30 wt %, ≥40 wt %, ≥50 wt %, ≥60 wt %, ≥70 wt %, ≥80 wt %, or ≥90 wt %, based on the total weight of the tar-fluid mixture (e.g., the combined weight of all components in the tar-fluid mixture). Additionally or alternatively, the tar-fluid mixture may include ≤10 wt % utility fluid, e.g., ≤20 wt %, ≤30 wt %, ≤40 wt %, ≤50 wt %, ≤60 wt %, ≤70 wt %, ≤80 wt %, ≤90 wt %, or ≤95 wt % utility fluid, based on the total weight of the tar-fluid mixture. Explicitly disclosed ranges include any combination of the above enumerated values, for example, about 5 wt % to about 95 wt %, about 5 wt % to about 90 wt %, about 5 wt % to about 80 wt %, about 5 wt % to about 70 wt %, about 5 wt % to about 60 wt %, about 5 wt % to about 50 wt %, about 5 wt % to about 40 wt %, about 5 wt % to about 30 wt %, about 5 wt % to about 20 wt %, or about 5 wt % to about 10 wt % of the utility fluid.

[0080] In certain aspects, the tar-fluid mixture includes (i) an SCT composition, (ii) a recycled portion of the second lower density portion, and (iii) any first utility fluid added to the SCT composition prior to the first SCT separation stage. For example, the tar-fluid mixture can contain about 15 wt%, about 20 wt%, about 25 wt%, 30 wt%, about 35 wt%, about 40 wt%, about 45 wt%, or about 50 wt% to about 55 wt%, about 60 wt%, about 65 wt%, about 70 wt%, about 75 wt%, about 80 wt%, about 85 wt%, or about 90 wt%, or more of the utility fluid, based on the combined weight of the tar-fluid mixture (e.g., the combined weight of all components in the tar-fluid mixture). Typically, the tar-fluid mixture contains about 15 wt % to about 90 wt %, about 20 wt % to about 90 wt %, about 20 wt % to about 80 wt %, about 20 wt % to about 70 wt %, about 20 wt % to about 60 wt %, about 20 wt % to about 50 wt %, about 20 wt % to about 50 wt %, about 20 wt % to about 40 wt %, about 20 wt % to about 30 wt %, about 25 wt % to about 90 wt %, about 30 wt % to about 85 wt %, about 30 wt % to about 80 wt %, about 35 wt % to about 80 wt %, about 40 wt % to about 80 wt %, about 40 wt % to about 75 wt %, about 40 wt % to about 70 wt %, about 40 wt % to about 65 wt %, about 40 wt % to about 60 wt %, about 40 wt % to about 55 wt %, about 40 wt % to about 50 % to about 80wt%, about 45wt% to about 75wt%, about 45wt% to about 70wt%, about 45wt% to about 65wt%, about 45wt% to about 60wt%, about 45wt% to about 55wt%, about 45wt% to about 50wt%, about 50wt% to about 80wt%, about 50wt% to about 75wt%, about 50wt% to about 70wt%, about 50wt% to about 65wt%, about 50wt% to about 60wt%, about 50wt% to about 55wt%, about 55wt% to about 80wt%, about 55wt% to about 75wt%, about 55wt% to about 70wt%, about 55wt% to about 65wt%, or about 55wt% to about 60wt% of the utility fluid, based on the total weight of the tar-fluid mixture.

[0081] The SCT composition, the utility fluid, and the recycle portion of the second lower density portion are combined under conditions that reduce or substantially prevent asphaltene precipitation. One skilled in the art will appreciate that by doing so, one can take advantage of blending information of these compositions, such as the insolubility value I TF And solubility blending value S TFThus, in some aspects, the S of the tar-fluid mixture is TF ≤150, such as ≤140, or ≤130, or ≤120, or ≤115, or ≥110, or ≥105, or ≥100, or ≥95, or ≥90. In some examples, the S of the tar-fluid mixture is TF is about 70, about 80, about 85, about 90, about 95, about 100, about 105, about 110, about 115, about 120, about 130, about 140, or about 150. For example, the S of the tar-fluid mixture TF The range is about 70 to about 150, about 70 to about 130, about 70 to about 125, about 70 to about 120, about 70 to about 115, about 70 to about 110, about 70 to about 105, about 70 to about 100, about 70 to about 95, about 70 to about 90, about 70 to about 85, about 80 to about 130, about 80 to about 125, about 80 to about 120, about 80 to about 115, about 80 to about 110, about 80 to about 105, about 8 ...80 to about 95 0 to about 95, about 80 to about 90, about 85 to about 130, about 85 to about 125, about 85 to about 120, about 85 to about 115, about 85 to about 110, about 85 to about 105, about 85 to about 100, about 85 to about 95, about 85 to about 90, about 90 to about 130, about 90 to about 125, about 90 to about 120, about 90 to about 115, about 90 to about 110, about 90 to about 105, about 90 to about 100, or about 90 to about 95.

[0082] Particularly in aspects where the tar-fluid mixture components are not subsequently hydrotreated, the fluid of the tar-fluid mixture may further include a first separation fluid, in this context "fluid" refers to the total amount of the first utility fluid in the tar-fluid mixture plus the total amount of the first separation fluid in the tar-fluid mixture. The separation fluid can be used as an auxiliary in separating the first higher density and lower density portions and in separating the second higher density and lower density portions. Although the separation fluid can have substantially the same composition as the utility fluid, it typically has a different composition. The tar-fluid mixture may optionally include a first separation fluid typically in an amount of ≤35 wt%, e.g., ≤30 wt%, ≤25 wt%, ≤20 wt%, ≤15 wt%, ≤10 wt%, ≤5 wt%, ≤2.5 wt%, or ≤1.5 wt%, based on the total weight of the fluid (e.g., utility fluid plus separation fluid) in the tar-fluid mixture. Additionally or alternatively, the separation fluid may be present in an amount of ≥ to 0 wt %, e.g., ≥ 1.5 wt %, ≥ 2.5 wt %, ≥ 5 wt %, ≥ 10 wt %, ≥ 15 wt %, ≥ 20 wt %, ≥ 25 wt %, or ≥ 30 wt %, based on the total weight of the fluid in the tar-fluid mixture. Explicitly disclosed ranges include combinations of any of the above enumerated values, e.g., 0 to about 35 wt %, 0 to about 30 wt %, 0 to about 25 wt %, 0 to about 20 wt %, 0 to about 15 wt %, 0 to about 10 wt %, 0 to about 5 wt %, 0 to about 2.5 wt %, 0 to about 1.5 wt % of the separation fluid, based on the total weight of the fluid in the tar-fluid mixture.

[0083] Thus, in some aspects, the fluid includes ≥50 wt % of the separation fluid, e.g., ≥60 wt %, ≥70 wt %, ≥80 wt %, ≥90 wt %, ≥95 wt %, ≥97.5 wt %, ≥99 wt %, or about 100 wt % of the separation fluid, based on the total weight of the tar-fluid mixture. Additionally or alternatively, the tar-fluid mixture may include ≤99 wt % of the separation fluid, e.g.,

[0084] ≤97.5 wt %, ≤95 wt %, ≤90 wt %, ≤80 wt %, ≤70 wt %, or ≤60 wt % of the separated fluid, based on the total weight of the tar-fluid mixture. Explicitly disclosed ranges include any combination of the above enumerated values, for example, about 50 wt % to about 100 wt %, about 60 wt % to about 100 wt %, about 70 wt % to about 100 wt %, about 80 wt % to about 100 wt %, about 90 wt % to about 100 wt %, about 95 wt % to about 100 wt %, about 97.5 wt % to about 100 wt %, or about 99 wt % to about 100 wt % of the separated fluid.

[0085] The dynamic viscosity of the tar-fluid mixture is typically less than that of the SCT composition. In some aspects, the dynamic viscosity of the tar-fluid mixture at a temperature of about 50°C to about 250°C, such as about 100°C, can be ≥0.5 cP, for example, ≥1 cP, ≥2.5 cP, ≥5 cP,

[0086] ≥7.5 cP. Additionally or alternatively, the dynamic viscosity of the tar-fluid mixture at a temperature of about 50°C to about 250°C, such as about 100°C, can be ≤10 cP, for example, ≤7.5 cP, ≤5 cP, ≤2.5 cP, ≤1 cP, ≤0.75 cP. The range includes any combination of the above enumerated values, for example, about 0.5 cP to about 10 cP, about 1 cP to about 10 cP, about 2.5 cP to about 10 cP, about 5 cP to about 10 cP, or about 7.5 cP to about 10 cP at a temperature of about 50°C to about 250°C, such as about 100°C.

[0087] Utility Fluid

[0088] The first and second utility fluids may be independently selected. Each may be selected from conventional utility fluids, such as those used as process aids for hydroprocessing tars such as SCT, but the invention is not limited thereto. Suitable utility fluids include those disclosed in U.S. Provisional Application No. 62 / 716754; U.S. Patent Nos. 9,090,836; 9,637,694; and 9,777,227; and 9,809,756 and in PCT Patent Application Publication No. WO 2018-111574, which are incorporated herein by reference in their entirety. Although not required, the first and second utility fluids may have substantially the same composition and may be referred to as "utility fluids".

[0089] The utility fluid typically includes ≥40 wt% of at least one aromatic or non-aromatic ring-containing compound, e.g., ≥45 wt%, ≥50 wt%, ≥55 wt%, or ≥60 wt%, based on the weight of the utility fluid. Particular utility fluids contain ≥40 wt%, ≥45 wt%, ≥50 wt%, ≥55 wt%, or ≥60 wt% of at least one polycyclic compound, based on the weight of the utility fluid. The compounds contain mostly carbon and hydrogen atoms, but may also contain various substituents and / or heteroatoms.

[0090] In certain aspects, the utility fluid contains aromatics, for example, ≥70wt% aromatics, based on the weight of the utility fluid, for example ≥80wt%, or ≥90wt%. Typically, the utility fluid contains ≤10wt% paraffins, based on the weight of the utility fluid. For example, the utility fluid may contain ≥95wt% aromatics, ≤5wt% paraffins. Optionally, the utility fluid has a final boiling point of ≤750°C (1,400°F), for example, ≤570°C (1,050°F), for example ≤430°C (806°F). Such utility fluids may contain ≥25wt% 1-ring and 2-ring aromatics (e.g., those aromatics having one or two rings and at least one aromatic nucleus), based on the weight of the utility fluid. Utility fluids with relatively low final boiling points may be used, for example, utility fluids with a final boiling point of ≤400°C (750°F). The utility fluid may have a 10% (weight basis) total boiling point of ≥120°C, for example, ≥140°C, for example, ≥150°C and / or a 90% total boiling point of ≤430°C, for example, ≤400°C. Suitable utility fluids include those having a true boiling point distribution range of typically 175°C (350°F) to about 400°C (750°F). The true boiling point distribution may be determined, for example, by conventional methods, such as the ASTM D7500 method, when the true boiling point distribution has a final boiling point outside the range covered by the ASTM method, the true boiling point distribution may be extended by extrapolation. In certain aspects, the mass density of the utility fluid is ≤0.91 g / mL, for example, ≤0.90 g / mL, for example ≤0.89 g / mL, or ≤0.88 g / mL, for example, in the range of 0.87 g / mL to 0.90 g / mL.

[0091] The utility fluid typically contains aromatics, e.g., ≥95.0 wt% aromatics, e.g., ≥99.0 wt%. For example, the utility fluid may contain ≥75 wt% of one or more of the following based on the weight of the utility fluid: benzene, ethylbenzene, trimethylbenzene, xylenes, toluene, naphthalene, alkylnaphthalenes (e.g., methylnaphthalenes), decalin or alkyldecalin (e.g., methyldecalin), e.g., ≥90 wt%, or ≥95 wt%, or ≥99.0 wt%, e.g., ≥99.9 wt%. For the utility fluid, it is generally desirable to be substantially free of molecules having olefinic functional groups, particularly in aspects employing hydroprocessing catalysts that have a tendency to form coke (e.g., pyrolysis and / or polymerized particles) in the presence of such molecules. In certain aspects, the utility fluid contains ≤10.0 wt% having C 1 -C 6 Cyclic compounds with alkenyl functional groups in side chains, based on the weight of the utility fluid.

[0092] In some examples, the utility fluid may include ≥ 90 wt% of monocyclic aromatic hydrocarbons, including those having one or more hydrocarbon substituents, such as 1 to 3 or 1 to 2 hydrocarbon substituents. Exemplary hydrocarbon substituents or hydrocarbon groups may be or include, but are not limited to, C 1 -C 6 Alkyl, wherein the hydrocarbon group may be branched or straight chain, and the hydrocarbon groups may be the same or different.

[0093] In some instances, the utility fluid can be substantially free of molecules having terminal unsaturation, such as vinyl aromatics. As used herein, the term "substantially free" means that the utility fluid includes less than or equal to 10 wt%, such as less than or equal to 5 wt%, or less than or equal to 1 wt% of terminal unsaturation, based on the weight of the utility fluid. The utility fluid can include ≥50 wt% molecules having at least one aromatic nucleus, such as ≥60 wt% or ≥70 wt%, based on the weight of the utility fluid. In some instances, the utility fluid can include ≥60 wt% molecules having at least one aromatic nucleus and less than or equal to 1 wt% of terminal unsaturation, such as vinyl aromatics, based on the weight of the utility fluid.

[0094] In aspects where hydroprocessing is envisioned, such as hydroprocessing of the first lower density fraction, the utility fluid typically contains sufficient molecules having one or more aromatic nuclei to act as a processing aid, such as to effectively increase the run length of the tar hydroprocessing process. For example, the utility fluid may contain ≥50.0 wt% molecules having at least one aromatic nucleus (e.g., ≥60.0 wt%, such as ≥70 wt%), based on the total weight of the utility fluid. In one aspect, the utility fluid contains (i) ≥60.0 wt% molecules having at least one aromatic nucleus and (ii) ≤1.0 wt% vinyl aromatics, the weight percentages being based on the weight of the utility fluid.

[0095] The utility fluid may be a utility fluid having a high solubility, as indicated by the solubility blending value ("S 流体 "). For example, a utility fluid may have S 流体 ≥90, e.g., ≥100, ≥110, ≥120, ≥150, ≥175, or ≥200. Additionally or alternatively, S 流体 It may be ≤ 200, for example, ≤ 175, ≤ 150, ≤ 125, ≤ 110, or ≤ 100. Explicitly disclosed ranges include any combination of the above enumerated values.

[0096] Additionally or alternatively, the utility fluid may be characterized in that the dynamic viscosity is typically less than the tar-fluid mixture. In particular aspects, the dynamic viscosity of the tar-fluid mixture at a temperature of about 50°C to about 250°C, such as about 100°C, can be ≥0.1 cP, for example, ≥0.5 cP, ≥1 cP, ≥2.5 cP, or ≥4 cP. Additionally or alternatively, the dynamic viscosity of the tar-fluid mixture at a temperature of about 50°C to about 250°C, such as about 100°C, can be ≤5 cP, for example, ≤4 cP, ≤2.5 cP, ≤1 cP, ≤0.5 cP, or ≤0.25 cP. The ranges explicitly disclosed include any combination of the above enumerated values. In some aspects, the dynamic viscosity of the utility fluid is adjusted so that when combined with the SCT composition to produce a tar-fluid mixture, solids greater than 25 μm in size settle out of the tar-fluid mixture to provide a solids-rich fraction (extract) and a solids-lean fraction (raffinate) as described herein, and more particularly the viscosity is adjusted to also enable an appropriate amount of solids removal and yield of the solids-lean fraction from the process.

[0097] Optional separation fluid

[0098] Each of the first and second separation fluids may be independently selected. Each may be selected from a hydrocarbon liquid having a mass density less than the mass density of the SCT composition, such as ≤1% of the feed, such as ≤5%, or ≤10%. Although not required, the first and second separation fluids may have substantially the same composition and may be referred to as "separation fluids". The separation fluid may be any hydrocarbon liquid, typically a non-polar hydrocarbon, or a mixture thereof. In some aspects, the separation fluid may be a paraffin or a mixture of paraffins. Particular paraffin fluids include C 5 -C 20 Hydrocarbons and mixtures thereof, especially C 5 -C 10 Hydrocarbons, such as hexane, heptane and octane. Such fluids can be particularly useful when subsequent hydroprocessing is not desired. In certain aspects, the mass density of the separation fluid is ≤0.91 g / mL, such as ≤0.90 g / mL, such as ≤0.89 g / mL, or ≤0.88 g / mL, such as, in the range of 0.87 to 0.90 g / mL.

[0099] When a different separation fluid (i.e., a separation fluid having a substantially different composition from the utility fluid) is used in the production of a tar-fluid mixture, the separation fluid may be present in the tar-fluid mixture in an amount of ≤35 wt%, e.g., ≤30 wt%, ≤25 wt%, ≤20 wt%, ≤15 wt%, ≤10 wt%, ≤5 wt%, ≤2.5 wt%, or ≤1.5 wt%, based on the total weight of the fluid in the tar-fluid mixture. Additionally or alternatively, the separation fluid may be present in an amount of ≥ to 0 wt%, e.g., ≥1.5 wt%, ≥2.5 wt%, ≥5 wt%, ≥10 wt%, ≥15 wt%, ≥20 wt%, ≥25 wt%, or ≥30 wt%, based on the total weight of the fluid in the tar-fluid mixture. Explicitly disclosed ranges include any combination of the above enumerated values. In these and other aspects, typically, the separation fluid (if used) and the SCT composition together comprise ≥50 wt% of the balance of the tar-fluid mixture (the balance being that portion of the tar-fluid mixture that is not the utility fluid + the recycled portion of the second lower density portion), e.g., ≥75 wt%, e.g., ≥90 wt%, or ≥95 wt%, or ≥99 wt%.

[0100] Tar-fluid mixtures may contain both effective and separated fluids. In particular, in aspects where the tar-fluid mixture components are not subjected to subsequent hydroprocessing, the tar-fluid mixture may include ≥30wt% of separated fluids. Therefore, in some aspects, the fluid of the tar-fluid mixture (i.e., any utility fluid present in the tar-fluid mixture plus any separated fluid present in the tar-fluid mixture) may contain ≥50wt% of separated fluids, for example, ≥60wt%, ≥70wt%, ≥80wt%, ≥90wt%, ≥95wt%, ≥97.5wt%, ≥99wt%, or 100wt% of separated fluids, based on the total weight of the tar-fluid mixture. Additionally or alternatively, the tar-fluid mixture may include ≤99wt% of separated fluids, for example, ≤97.5wt%, ≤95wt%, ≤90wt%, ≤80wt%, ≤70wt%, or ≤60wt% of separated fluids, based on the total weight of the tar-fluid mixture. The range explicitly disclosed includes any combination of the above enumerated values.

[0101] Aspects of the invention involving separation of a first higher density fraction and a first lower density fraction from a tar-fluid mixture in a first SCT separation stage are now described in more detail. The invention is not limited in these respects, and this description should not be interpreted as excluding other forms of separation.

[0102] First SCT separation - separation of the first higher density and first lower density fractions from the tar-fluid mixture

[0103] The first higher density and lower density parts can be separated from the tar-fluid mixture by any means suitable for achieving the specified separation, including one or more of precipitation, filtration and extraction. Conventional separation techniques can be used, but the embodiments are not limited to this. For example, the first lower density part can be separated from the tar-fluid mixture by decantation, filtration and / or boiling point separation (e.g., one or more distillation towers, splitters, flash drums, or any combination thereof). The first higher density part can be separated from the tar-fluid mixture in a similar manner, such as by removing the first higher density part as a bottom product part from the separation section. The first higher density part and the first lower density part can be separated from the tar-fluid mixture in any order, such as substantially simultaneously, by first separating the first higher density part and then separating the first higher density part from the first lower density part, or vice versa. In some aspects, the first lower density part and the first higher density part are separated by exposing the tar-fluid mixture to centrifugal force, such as by using one or more centrifuges in the separation section.

[0104] Induced centrifugal force

[0105] In some aspects, a tar-fluid mixture containing SCT, solids (e.g., pyrolytic coke, polymerized coke and / or inorganics), and a first utility fluid and / or a first separation fluid is provided to a centrifuge for exposing the tar-fluid mixture to centrifugal forces sufficient to form at least a higher density portion and a lower density portion. Optionally, the tar-fluid mixture undergoes one or more filtration stages, such as to remove solids having a size of ≥5000 μm, e.g., ≥3000 μm, e.g., ≥2000 μm, or ≥1000 μm. In certain aspects, the size range of the solids present in the tar-fluid mixture is less than 1 μm to 3000 μm, such as in the range of about 0.5 μm to 2000 μm. Typically, ≥75 wt% of the solids have a size of ≤2000 μm, e.g., ≥90 wt%, e.g., ≥95 wt%, or ≥99 wt%. Typically, ≥ 75 wt % of the solids are in the size range of 50 μm to 88 μm, e.g. ≥ 90 wt %, such as ≥ 95 wt %, or ≥ 99 wt %.

[0106] Typically, the tar-fluid mixture exhibits a substantially uniform circular motion within the centrifuge as a result of the applied centrifugal force. Depending on the choice of reference frame, the central force may be referred to as the centrifugal force (in the reference frame of the tar-fluid mixture) or the centripetal force (in the reference frame of the centrifuge). The process may be carried out in a batch, semi-batch or continuous manner.

[0107] The centrifuge can be configured to apply heat to the tar-fluid mixture, for example by heating the tar-fluid mixture to an elevated temperature. In some aspects, inducing centrifugal force further comprises heating the tar-fluid mixture to a temperature of about 20°C, about 25°C, about 30°C, about 40°C, about 50°C, about 55°C, or about 60°C to about 65°C, about 70°C, about 80°C, about 85°C, about 90°C, about 95°C, about 100°C, about 110°C, about 120°C, or greater. For example, while centrifuging, the tar-fluid mixture can be heated to a temperature of about 20°C to about 120°C, about 20°C to about 100°C, about 30°C to about 100°C, about 40°C to about 100°C, about 50°C to about 100°C, about 60°C to about 100°C, about 70°C to about 100°C, about 80°C to about 100°C, about 90°C to about 100°C, about 20°C to about 80°C, about 30°C to about 80°C, about 40°C to about 80°C, about 50°C to about 80°C, about 60°C to about 80°C, or about 70°C to about 80°C.

[0108] Centrifugal force can be applied for any amount of time. Typically, centrifugal force is applied for ≥1 minute, for example, ≥5 minutes, ≥10 minutes, ≥30 minutes, ≥60 minutes, or ≥120 minutes. Additionally or alternatively, centrifugal force can be applied for ≤120 minutes, ≤60 minutes, ≤30 minutes, ≤10 minutes, or ≤5 minutes. Clearly disclosed scope includes any combination of numerical values ​​enumerated above, for example, about 1 minute to about 120 minutes, about 5 minutes to about 120 minutes, about 10 minutes to about 120 minutes, about 30 minutes to about 120 minutes, or about 60 minutes to about 120 minutes. Centrifugal force can be applied at any size of force or speed. For example, by providing enough force at about 1,000rpm to about 10,000rpm, about 2,000rpm to about 7,500rpm, or about 3,000rpm to about 5,000rpm centrifuges operating.

[0109] Centrifuging the tar-fluid mixture typically results in separation of at least (i) an extract comprising, consisting essentially of, or consisting of a first, higher density portion of the tar-fluid mixture, and (ii) a raffinate comprising, consisting essentially of, or consisting of a first, lower density portion from the tar-fluid mixture. In other words, exposing the tar-fluid mixture to centrifugal forces results in removal of at least the higher density portion (the extract) from the tar-fluid mixture. When the process is operated continuously or semi-continuously, at least two streams are directed away from the centrifuge: one stream comprising the extract and another stream comprising the raffinate. Centrifuges with this capability are commercially available, but the invention is not limited thereto.

[0110] Typically centrifugation is sufficient to separate ≥80 wt%, ≥90 wt%, ≥95 wt%, ≥99 wt% of solids (including particles in the tar-fluid mixture) of size ≥2 μm, e.g., ≥10 μm, e.g., ≥20 μm, or ≥25 μm in the tar-fluid mixture into a first higher density portion (e.g., extract), wherein the wt% is based on the total weight of solids in the higher density and lower density portions. When subsequent hydroprocessing of the raffinate is envisioned, the higher density portion contains ≥95 wt%, especially ≥99 wt% of solids of size ≥2 μm, e.g., ≥10 μm, e.g., ≥20 μm, or ≥25 μm. In other aspects, such as when the first lower density portion (e.g., raffinate) is not subjected to hydroprocessing, filtration should be sufficient to separate at least 80 wt% of the solids into the first higher density portion.

[0111] Although the description focuses on separating the first higher density fraction and the first lower density fraction, other embodiments envision that the components in the first tar-fluid mixture can be separated and extracted more independently, such as very light components to the top of the mixture, a fraction containing primarily fluid, an upgraded tar fraction, tar heavies, or solids at the bottom of the centrifuge chamber. Each of these fractions or a combination thereof can be selectively removed from the mixture as one or more raffinates.

[0112] first lower density portion

[0113] The first lower density portion can be directed away for one or more of the following: storage, blending with other hydrocarbons, or further processing, such as for SATC. The first lower density portion generally has a desired insolubility value, such as an insolubility value less than the SCT composition and / or less than the higher density portion. Typically, the insolubility value (I FLD ) is ≥20, e.g., ≥30, ≥40, ≥50, ≥60, ≥70, ≥80, ≥90, ≥100, ≥110, ≥120, ≥130, ≥140, or ≥150. Additionally or alternatively, I FLDIt may be ≤150, for example, ≤140, ≤130, ≤120 ≤110, ≤100, ≤90, ≤80, ≤70, ≤60, ≤50, ≤40, or ≤30. Explicitly disclosed ranges include any combination of the above enumerated values, for example, about 20 to about 150, about 20 to about 140, about 20 to about 130, about 20 to about 120, about 20 to about 110, about 20 to about 100, about 20 to about 90, about 20 to about 80, about 20 to about 70, about 20 to about 60, about 20 to about 50, about 20 to about 40, or about 20 to about 30. Those skilled in the art will appreciate that hydrocarbon separation techniques are imperfect, and thus a small amount of solids may be present in the first lower density portion, for example, an amount of solids that is ≤0.1 times the amount of solids in the tar-fluid mixture, for example ≤0.01 times. In aspects where at least a portion of the first lower density fraction is hydroprocessed, such as by a SATC process, solids removal equipment (eg, one or more filters) is typically used between the separation stage and the hydroprocessing stage.

[0114] Insolubility value I of the first lower density fraction FLD Insolubility value I for SCT composition TC The ratio is ≤0.95, e.g., ≤0.90, ≤0.85, ≤0.80, ≤0.75, ≤0.70, ≤0.65, ≤0.60, ≤0.55, ≤0.50, ≤0.40, ≤0.30, ≤0.20, or ≤0.10. Additionally or alternatively, I FLD to I TC The ratio can be ≥0.10, for example, ≥0.20, ≥0.30, ≥0.40, ≥0.50, ≥0.55, ≥0.60, ≥0.65, ≥0.70, ≥0.75, ≥0.80, ≥0.85, or ≥0.90. The explicitly disclosed range includes any combination of the above enumerated values, for example, about 0.10 to 0.95, about 0.20 to 0.95, about 0.30 to 0.95, about 0.40 to 0.95, about 0.50 to 0.95, about 0.55 to 0.95, about 0.60 to 0.95, about 0.65 to 0.95, about 0.70 to 0.95, about 0.75 to 0.95, about 0.80 to 0.95, about 0.85 to 0.95, or about 0.90 to 0.95.

[0115] First higher density portion

[0116] The first higher density portion typically includes solids with a size of ≤5000 μm, e.g., ≤2000 μm, e.g., ≤1000 μm, and optionally contains liquids such as utility fluid and / or separation fluid brought from separation (e.g., from centrifugation). For example, the first higher density portion may contain solids with a size of ≤5000 μm (or ≤3000 μm, or ≤2000 μm) in an amount ranging from 1 wt% to 25 wt%, e.g., 5 wt% to 15 wt%, based on the weight of the first higher density portion. In certain aspects, the first higher density portion contains solids with a size ranging from ≤1 μm to 5000 μm, e.g., 0.1 μm to 3000 μm, e.g., in the range of about 0.5 μm to 2000 μm. Typically, ≥75 wt% of the solids have a size of ≤2000 μm, e.g., ≥90 wt%, e.g., ≥95 wt%, or ≥99 wt%. Typically, ≥ 75 wt % of the solids are in the size range of 50 μm to 88 μm, e.g. ≥ 90 wt %, such as ≥ 95 wt %, or ≥ 99 wt %.

[0117] The first higher density portion, particularly the liquid phase thereof, may have an insolubility value I FHD , ≥20, ≥40, ≥70, ≥90, ≥100, ≥110, ≥120, ≥130, ≥140, or ≥150. Additionally or alternatively, I FHD It can be ≤40, ≤70, ≤90, ≤100, ≤110, ≤120, ≤130, ≤140, or ≤150. Explicitly disclosed ranges include any combination of the above enumerated values, for example, about 20 to about 150, about 40 to about 150, about 70 to about 150, about 90 to about 150, about 100 to about 150, about 110 to about 150, about 120 to about 150, about 130 to about 150, or about 140 to about 150.

[0118] Additionally or alternatively, the first higher density portion may contain asphaltenes and / or tar heavies. In some aspects, the first higher density portion, particularly the liquid portion thereof, contains ≥50 wt% asphaltenes, e.g., ≥60 wt%, ≥75 wt%, based on the total weight of the first higher density portion. The first higher density portion may include ≤10 wt%, e.g., ≤7.5 wt%, ≤5 wt%, ≤2.5 wt%, ≤2 wt%, ≤1.5 wt%, or ≤1 wt% of the total asphaltenes content in the SCT composition. The first higher density portion may include ≥1 wt%, e.g., ≥1.5 wt%, ≥2 wt%, ≥2.5 wt%, ≥5 wt%, or ≥7.5 wt% of the total asphaltenes content in the SCT composition. Explicitly disclosed ranges include any combination of the above enumerated values, e.g., 1 wt% to 10 wt%, 1 wt% to 7.5 wt%, 1 wt% to 5 wt%, 1 wt% to 2.5 wt%, 1 wt% to 2 wt%, or 1 wt% to 1.5 wt% of the total asphaltenes content in the SCT composition. It may be preferred to remove smaller amounts of asphaltene content. For example, it was surprisingly discovered that separating even a small amount of asphaltenes into the higher density fraction had a surprising effect on the insolubility value of the first, lower density fraction. While not wishing to be bound by any theory or model, it is believed that the presence of relatively high density asphaltenes in the SCT composition has a much greater effect on the insolubility value than the lower density asphaltenes. Thus, a relatively large amount of problematic molecules may be separated, leaving behind the molecules of the first, lower density fraction that contribute to the overall yield of the process.

[0119] The advantages of the process can be obtained even when the first higher density portion contains a relatively small portion of the SCT composition. The first higher density portion may contain ≤10 wt%, e.g., ≤7.5 wt%, ≤5 wt%, ≤2.5 wt%, ≤2 wt%, ≤1.5 wt%, or ≤1 wt% of the total weight of the SCT composition. Explicitly disclosed ranges include combinations of any of the above enumerated values, e.g., 1 wt% to 10 wt%, 1 wt% to 7.5 wt%, 1 wt% to 5 wt%, 1 wt% to 2.5 wt%, 1 wt% to 2 wt%, or 1 wt% to 1.5 wt% of the total weight of the SCT composition. Removal of a relatively small weight portion can surprisingly be accompanied by a relatively large improvement in the insolubility value of the first lower density portion. The solids present in the extract optionally have a mass density of ≥1.05 g / mL, e.g., ≥1.10 g / mL, e.g., ≥1.2 g / mL, or ≥1.3 g / mL, or in the range of about 1.05 g / mL to 1.5 g / mL.

[0120] The first higher density portion typically includes ≥50 wt% of any SCT solids remaining after the first thermal treatment, e.g., ≥75 wt%, e.g., ≥90 wt%, or ≥99 wt%. The first higher density portion typically further includes ≥50 wt% of any solids in the SCT composition formed during or as a result of the first thermal treatment, e.g., ≥75 wt%, e.g., ≥90 wt%, or ≥99 wt%. The first higher density portion is treated in the second thermal treatment and the size of the solids present in the first higher density portion is optionally physically reduced (e.g., by comminution, e.g., grinding) in order to reduce the amount of solids. This treatment may be performed in the presence of a diluent.

[0121] Optional size reduction - physical methods

[0122] Optionally, a physical method (grinding, etc. - collectively referred to as pulverization) of solid, such as particle size reduction, is performed on the first higher density portion to form a pulverized higher density portion. Examples of physical methods of size reduction may include grinding, ball milling, ablation in an ablation drum, and / or other mechanical size reduction methods. Physical methods of size reduction can be contrasted with chemical methods of size reduction. For example, as described herein, at least a portion of sufficiently small solids (e.g., particles) in an SCT fraction (or other pyrolysis tar fraction) may be hydrotreated (e.g., under SATC conditions) to convert small solids into liquid products. During certain SATC methods, a combination of increased temperature, increased pressure, the presence of chemical reagents, and / or the presence of a catalyst is used to induce a chemical reaction. The chemical reaction results in a change in chemical composition, which can then result in size reduction. On the contrary, in some aspects, physical size reduction before and after size reduction can result in solids with roughly similar compositions (surface layers may be an exception).

[0123] After the first physical size reduction process is performed on the first higher density fraction, the weight of solids with a size greater than or equal to 25 μm in the comminuted higher density fraction may be further reduced in one or more additional stages. The weight of solids with a size greater than or equal to 25 μm in the effluent from these stages is less than or equal to 85%, or less than or equal to 75%, or less than or equal to 65%, or less than or equal to 50%, for example up to 10% or possibly still lower, relative to the weight of such solids in the first higher density fraction or the diluted first higher density fraction, as the case may be.

[0124] Suitable equipment for reducing the size of solids is commercially available, but the invention is not limited thereto. Grinding mills, ball mills, and ablators are suitable. More generally, any convenient method for reducing the size of solids, such as coke fines, may be used.

[0125] Since the first higher density portion is typically more depleted in the overall fluid (any first utility fluid + any first separation fluid) than the tar-fluid mixture, a diluted first higher density portion may be formed by introducing a second utility fluid and / or a second separation fluid into the first higher density portion. These diluents are optional and may be added to the first higher density portion, for example as a flux and / or as an adjuvant, during (i) the second heat treatment and / or (ii) the separation of the second higher density and second lower density portions. These diluents may be added before and / or after optional size reduction (e.g., optional grinding). For example, the second utility fluid may be added before and / or after optional grinding. The second utility fluid may be selected from the same composition specified for the first utility fluid, and typically the first and second utility fluids have substantially the same composition.

[0126] Dilute the first higher density portion

[0127] If desired, for example, as an aid to the processability of the first higher density portion, a diluent (typically which includes a second utility fluid and / or a second separation fluid) may be added to the first higher density portion to form a diluted first higher density portion. The diluent, if used, may be equivalent to 20 wt% to 60 wt% of the diluted first higher density portion, or 20 wt% to 50 wt%, or 30 wt% to 60 wt%. Even if the diluent is added to the first higher density portion before the size reduction process, additional diluent may be added after size reduction to further promote the heat soaking of the first higher density portion (or comminuted higher density portion) present in the diluted first higher density portion. Typically, the diluent includes ≥50 wt% of the utility fluid, based on the weight of the diluent, for example, ≥75 wt%, such as ≥90 wt%. Typically, the balance of the diluent of ≥90 wt% includes the separation fluid.

[0128] In certain aspects, the diluent is free of a second separation fluid. It has been found that treating the diluted first higher density fraction in a second heat treatment prior to separating the second higher density fraction and the second lower density fraction can obviate the need for a second separation fluid.

[0129] It has been found to be advantageous that the diluent includes a second utility fluid and that the second thermal treatment is performed under conditions different from those of the first thermal treatment. It has been found that doing so provides dissolution of at least a portion of polymer solids in the first higher density portion, such as those formed during and / or as a result of the first thermal treatment, and the deliberate depolymerization of these polymer solids. In addition, the second utility fluid dilutes the depolymerization products of the second thermal treatment, and it is observed that the depolymerization products reduce or eliminate the repolymerization of these products. The second utility fluid can be selected from a utility fluid containing a reactive composition such as SCGO. When this second utility fluid is present in the first higher density portion of the dilution during the second thermal treatment, a decrease in reactivity (e.g., a decrease in SCGO reactivity) is observed. This feature simulates the use of a higher value diluent, such as a utility fluid (e.g., middle distillate) recovered from the SATC process (and eliminates the need for it). In other words, the diluent can include SCGO, middle distillate, or a combination thereof.

[0130] In some aspects, the diluent may contain ≥65wt% of a utility fluid, for example, ≥75wt%, ≥80wt%, ≥85wt%, ≥90wt%, or ≥95wt% of a utility fluid, based on the gross weight of the diluent. Additionally or alternatively, the diluent may contain ≤100wt% of a utility fluid, for example, ≤95wt%, ≤90wt%, ≤85wt%, ≤80wt%, ≤75wt%, or ≤70wt% of a utility fluid, based on the gross weight of the diluent. Clearly disclosed ranges include any combination of the above enumerated numerical values, for example, about 65wt% to about 100wt%, about 75wt% to about 100wt%, about 80wt% to about 100wt%, about 85wt% to about 100wt%, about 90wt% to about 100wt%, or about 95wt% to about 100wt% of a utility fluid. In some aspects, the diluent is a utility fluid.

[0131] In the following description of the diluted first higher density portion and the second heat treatment, it should be understood that in aspects in which the optional comminution step is performed, the first higher density portion can be a comminuted first higher density portion. Typically, the diluted first higher density portion contains ≥5 wt % of the first higher density portion, e.g., ≥10 wt %, ≥20 wt %, ≥30 wt %, ≥40 wt %,

[0132] ≥50 wt%, ≥60 wt%, ≥70 wt%, ≥80 wt%, or ≥90 wt%, based on the total weight of the diluted first higher density portion. One skilled in the art will recognize that the amount of utility fluid in the diluted first higher density portion includes (i) any residual first utility fluid transferred from the tar-fluid mixture to the first higher density portion and (ii) the second utility fluid.

[0133] In addition to the first higher density portion, the diluted higher density portion typically contains ≥5 wt% of diluent, for example, ≥10 wt%, ≥20 wt%, ≥30 wt%, ≥40 wt%, ≥50 wt%,

[0134] ≥60 wt%, ≥70 wt%, ≥80 wt%, or ≥90 wt%, based on the total weight of the diluted higher density portion (e.g., the combined weight of the first higher density portion, any residual first utility fluid brought from the tar-fluid mixture, any first separation fluid brought from the tar-fluid mixture, any second utility fluid, and any second separation fluid). Additionally or alternatively, the diluted first higher density portion may include ≤10 wt% fluid, e.g., ≤20 wt%, ≤30 wt%, ≤40 wt%, ≤50 wt%, ≤60 wt%, ≤70 wt%, ≤80 wt%, ≤90 wt%, or ≤95 wt% of diluent, based on the total weight of the diluted first higher density portion. Explicitly disclosed ranges include any combination of the above enumerated values, for example, about 5 wt % to about 95 wt %, about 5 wt % to about 90 wt %, about 5 wt % to about 80 wt %, about 5 wt % to about 70 wt %, about 5 wt % to about 60 wt %, about 5 wt % to about 50 wt %, about 5 wt % to about 40 wt %, about 5 wt % to about 30 wt %, about 5 wt % to about 20 wt %, or about 5 wt % to about 10 wt % of the fluid.

[0135] In some aspects, the diluted first higher density portion has a Solubility Blending Value of less than 150, such as less than or equal to about 140, less than or equal to about 130, less than or equal to about 120, less than or equal to about 115, less than or equal to about 110, less than or equal to about 105, less than or equal to about 100, less than or equal to about 95, or less than or equal to about 90. In some examples, the diluted first higher density portion has a Solubility Blending Value of about 70, about 80, about 85, about 90, about 95, about 100, about 105, about 110, about 115, about 120, about 130, about 140, or about 150. For example, the solubility blend value of the diluted first higher density portion is about 70 to about 150, about 70 to about 130, about 70 to about 125, about 70 to about 120, about 70 to about 115, about 70 to about 110, about 70 to about 105, about 70 to about 100, about 70 to about 95, about 70 to about 90, about 70 to about 85, about 80 to about 130, about 80 to about 125, about 80 to about 120, about 80 to about 115, about 80 to about 110, about 80 to about 105, about 80 to about 100, about 70 to about 95, about 70 to about 90, about 70 to about 85, about 80 to about 130, about 80 to about 125, about 80 to about 120 0 to about 100, about 80 to about 95, about 80 to about 90, about 85 to about 130, about 85 to about 125, about 85 to about 120, about 85 to about 115, about 85 to about 110, about 85 to about 105, about 85 to about 100, about 85 to about 95, about 85 to about 90, about 90 to about 130, about 90 to about 125, about 90 to about 120, about 90 to about 115, about 90 to about 110, about 90 to about 105, about 90 to about 100, or about 90 to about 95.

[0136] The dynamic viscosity of the diluted first higher density portion can be less than the first higher density portion. In some aspects, the dynamic viscosity of the diluted first higher density portion can be ≥0.5 cP, for example, ≥1 cP, ≥2.5 cP, ≥5 cP, ≥7.5 cP at a temperature of about 50°C to about 250°C, for example, about 100°C. Additionally or alternatively, the dynamic viscosity of the tar-fluid mixture can be ≤10 cP, for example, ≤7.5 cP, ≤5 cP, ≤2.5 cP, ≤1 cP, ≤0.75 cP at a temperature of about 50°C to about 250°C, for example, about 100°C. Ranges may include any combination of the above enumerated values, for example, about 0.5 cP to about 10 cP, about 1 cP to about 10 cP, about 2.5 cP to about 10 cP, about 5 cP to about 10 cP, or about 7.5 cP to about 10 cP at a temperature of about 50°C to about 250°C, such as about 100°C.

[0137] The diluted first higher density portion is subjected to an additional heat treatment. Aspects in which the second heat treatment comprises a second heat soak are now described in more detail. The invention is not limited in these respects, and this description should not be interpreted as excluding forms of heat treatment that do not include a heat soak.

[0138] Second heat treatment

[0139] In other embodiments, the first higher density portion or the diluted first higher density portion (as the case may be) is subjected to a second heat treatment, for example, a second heat soak. The second heat treatment may be performed by heat soaking in at least one container or drum. The heat soaking may include pyrolysis, for example thermal pyrolysis.

[0140] Certain forms of solids are present in the SCT when the SCT is separated from the steam cracker effluent. Other forms of solids, such as certain particulates, are formed during and / or as a result of the first thermal treatment, for example by polymerization of the SCT separated in the tar drum and / or in the primary fractionator. It has been found that (i) the SCT composition can contain two solid forms, and (ii) when the first SCT separation is operated under specified conditions, ≥50 wt% of the solids in the SCT composition are transferred to the first higher density portion, for example, ≥75 wt%, such as ≥90 wt%, or ≥95 wt%, or ≥99 wt%. Surprisingly, it has been found that such solids can be converted during and / or as a result of the second thermal treatment to form conversion products (typically in the liquid phase) having a mass density in substantially the same range as the first lower density portion. The amount of material residing in the first lower density fraction can thus be increased by (i) transferring at least a portion of these conversion products of the second thermal treatment into the second lower density fraction and then recycling the second lower density fraction to (i) the first lower density fraction and / or (ii) at a location in the process upstream of separation of the first lower density fraction from the SCT composition. Typically, ≥50 wt% of the solids in the first higher density fraction are those produced during the first thermal treatment, e.g., ≥75 wt%, e.g., ≥90 wt%, or more. Figure 2 can be used to determine the amount of these solids converted in a given second thermal treatment. While not wishing to be bound by any theory or model, it is believed that the second thermal treatment at least partially converts (e.g., dissolves or decomposes) solids present in the diluted first higher density portion, particularly those solids produced during and / or as a result of the first thermal treatment (e.g., by polymerization). For a typical SCT, Figure 2represents the amount of solids that are converted from a greater mass density to a lower mass density (e.g., from a more dense solid phase and / or semi-solid phase to a less dense liquid phase) during or as a result of the second heat treatment as a function of the second heat treatment temperature for a time range of 30 minutes to 60 minutes. Those skilled in the art will appreciate that similar curves can be generated for other tars without undue experimentation. Conventional hot soaking equipment, such as one or more soaker drums, may be used for the second hot soak, but the invention is not limited thereto. The second hot soak may be performed at a desired temperature ("T HS2 ") and for the desired period of time ("t HS2 "), which is typically predetermined. HS2 Typically, the temperature is about 200°C, about 220°C, about 230°C, about 240°C, about 250°C, about 260°C, about 270°C, about 275°C, about 280°C, or about 290°C to about 295°C, about 300°C, about 310°C, about 320°C, about 325°C, about 330°C, about 340°C, about 350°C, about 360°C, about 375°C, about 400°C, about 450°C, about 500°C, or more. For example, T HS2 The range may be about 200°C to about 500°C, about 230°C to about 500°C, about 250°C to about 500°C, about 280°C to about 500°C, about 290°C to about 500°C, about 300°C to about 500°C, about 320°C to about 500°C, about 350°C to about 500°C, about 250°C to about 450°C, about 280°C to about 450°C, about 290°C to about 450°C, about 300°C to about 450°C, about 320°C to about 450°C 0° C., about 350° C. to about 450° C., about 250° C. to about 400° C., about 280° C. to about 400° C., about 290° C. to about 400° C., about 300° C. to about 400° C., about 320° C. to about 400° C., about 350° C. to about 400° C., about 250° C. to about 350° C., about 280° C. to about 350° C., about 290° C. to about 350° C., about 300° C. to about 350° C., about 320° C. to about 350° C., or about 330° C. to about 350° C. Although it is not required to maintain the diluted first higher density portion at a substantially constant temperature (i.e., at T ) during the second heat soak, the first higher density portion may be heated to a temperature of about 100° C. or about 150° C. HS2 The temperature is essentially constant within the specified range), but typically this is done. HS2 It can be about 2 min, about 5 min, about 10 min, about 12 min, or about 15 min to about 20 min, about 25 min, about 30 min, about 45 min, about 60 min, about 90 min, about 2 hr, about 3 hr, about 5 hr, or longer. For example, t HS2The range of t can be about 5 min to about 5 hr, about 5 min to about 3 hr, about 5 min to about 2 hr, about 5 min to about 1 hr, about 5 min to about 45 min, about 5 min to about 30 min, or about 5 min to about 20 min. In one or more embodiments, during or as a result of the second heat treatment, t HS2 The range is about 2 min, about 5 min, about 10 min, about 15 min, or about 20 min to about 30 min, about 45 min, about 60 min, about 90 min, about 2 hr, about 3 hr, or about 5 hr to convert (e.g., dissolve or decompose) the solids (e.g., polymer solids) within the first higher density portion or the diluted first higher density portion (as the case may be) into a less dense substance.

[0141] It is observed that before the second heat treatment, the second heat soak produces a heat-treated first higher density portion with less solids compared to the first higher density portion. In aspects where a diluent is used, the second heat soak produces a heat-treated diluted first higher density portion with less solids compared to the diluted first higher density portion. In one or more embodiments, during or as a result of the second heat treatment, about 25wt%, about 30wt%, about 35wt%, or about 40wt% to about 45wt%, about 50wt%, about 60wt%, about 70wt%, about 75wt%, about 80wt%, about 85wt%, about 90wt%, about 92wt%, about 95wt%, about 97wt%, about 98wt%, about 99wt%, or more solids (e.g., polymer solids formed by the first heat treatment) are converted (e.g., dissolved or decomposed) into (typically less dense) liquid substances in the first higher density portion or the diluted first higher density portion (as the case may be). In some instances, during or as a result of the second heat treatment, at least 25 wt%, at least 30 wt%, at least 35 wt%, at least 40 wt%, at least 45 wt%, at least 50 wt%, at least 60 wt%, at least 70 wt%, at least 75 wt%, at least 80 wt% to about 85 wt%, about 90 wt%, about 92 wt%, about 95 wt%, about 97 wt%, about 98 wt%, about 99 wt%, or more of the solids (e.g., particles) are converted within the first higher density portion or the diluted first higher density portion (as the case may be).For example, during or as a result of the second heat treatment, about 25 wt % to about 99 wt %, about 30 wt % to about 99 wt %, about 35 wt % to about 99 wt %, about 40 wt % to about 99 wt %, about 45 wt % to about 99 wt %, about 50 wt % to about 99 wt %, about 60 wt % to about 99 wt %, about 70 wt % to about 99 wt %, about 75 wt % to about 99 wt %, about 25 wt % to about 95 wt %, about 30 wt % to about 95 wt %, about 35 wt % to about 95 wt %, about 40 wt % to about 95 wt %, about 45 wt % to about 95 wt %, about 50 wt % to about 95 wt %, about 60 wt % to about 95 ...5 wt %, about 75 wt % to about 95 wt %, about 25 wt % to about 90 wt %, about 30 wt % to about 90 wt %, about 35 wt % to about 90 wt %, about 40 wt % to about 90 wt %, about 45 wt % to about 90 wt %, about 50 wt % to about 90 wt %, about 60 wt % to about 90 wt %, about 70 wt % to about 90 wt %, about 75 wt % to about 90 wt %, about 25 wt % to about 80 wt %, about 30 wt % to about 80 wt %, about 35 wt % to about 80 wt %, about 40 wt % to about 80 wt %, about 45 wt % to about 80 wt %, about 50 wt % to about 80 wt %, about 60 wt % to about 80 wt %, about 70 wt % to about 80 wt %, or about 75 wt % to about 80 wt % of the solids (e.g., polymer solids formed by the first thermal treatment, such as polymer pellets) are converted (e.g., dissolved or decomposed).

[0142] In certain aspects, the amount of solids (wt%) in the heat-treated first higher density portion ("A 2 ", based on the weight of the heat-treated first higher density portion) is less than the amount of solids (wt %) in the first higher density portion ("A 1 ", based on the weight of the first higher density portion), for example, A 2 ≤R*A 1 , wherein R is a real number <1, ​​for example, one of 0.9, 0.8, 0.7, 0.6, 0.5, 0.4, 0.3, 0.2, and 0.1. In other aspects, the solid amount (wt %) in the heat-treated first higher density portion ("A 2 ", based on the weight of the heat-treated first higher density portion) is less than the amount of solids (wt %) in the diluted first higher density portion ("A 1d ", based on the weight of the diluted first higher density portion), for example, A 2 ≤R*A 1dIt has been found that before the second heat treatment the relationship A is achieved 2 ≤R*A 1 and A 2 ≤R*A 1d It does not matter whether comminution is performed on the first higher density portion, although a smaller R value ("R c "). c It can be, for example, R*0.9, for example R*0.8, or R*0.7. With or without pulverization, for example, A 2 The range is 10% of A 1 Up to 40% A 1 , for example 15% of A 1 Up to 30% A 1 , or 20% of A 1 Up to 25% A 1 .

[0143] The solids converted in the second thermal treatment are typically converted predominantly to a liquid phase composition, eg, > 75 wt% of the solids converted products are in the liquid phase, eg, > 90 wt%, or > 95 wt%, or > 99 wt%.

[0144] It is observed that the second heat treatment, e.g., the second heat soak improves the properties of the first higher density portion contained within the diluted first higher density portion. Although at least a portion of the heat treated first higher density portion is typically further processed (e.g., separating and recycling the second lower density portion), the heat treated first higher density portion itself is a useful product, e.g., for use as a fuel oil. This is because the heat treated first higher density portion is less reactive and has a lower solids content than the first higher density portion.

[0145] Representative heat-treated first higher density parts are now described in more detail. The disclosure of the present invention is not limited to these, and this description is not meant to exclude other heat-treated first higher density parts within the broader scope of the disclosure of the present invention, such as those produced by the second heat treatment form without the second heat soak.

[0146] Heat treated first higher density portion

[0147] The final boiling point of the heat-treated first higher density portion is typically at least about 550°F+ (-288°C+). The boiling point and / or fractional weight distillation point can be determined, for example, by ASTM D2892. The final boiling point of the heat-treated first higher density portion can depend on the properties of the higher density portion, which in turn can depend on the composition of the steam cracking feed and the steam cracking conditions.

[0148] Compared to other heavy oil fractions, such as those typically processed in refineries or petrochemical plants, the portion of the heat-treated first higher density portion having a boiling point of ≥550°F (≥288°C+) at atmospheric pressure typically has a relatively low hydrogen content. For example, the portion of the heat-treated first higher density portion can have a hydrogen content of less than or equal to about 8.0 wt%, less than or equal to about 7.5 wt%, or less than or equal to about 7.0 wt%, or less than or equal to about 6.5 wt%, such as a range of about 5.5 wt% to about 8.0 wt%, or about 6.0 wt% to about 7.5 wt%.

[0149] The portion of the heat-treated first higher density portion having a boiling point of ≥550°F (≥288°C+) at atmospheric pressure is typically highly aromatic in nature. The paraffin content of this portion of the heat-treated first higher density portion can be less than or equal to about 2.0 wt%, or less than or equal to about 1.0 wt%, such as having essentially no paraffin content. The cycloparaffin content of this portion of the heat-treated first higher density portion can also be less than or equal to about 2.0 wt%, or less than or equal to about 1.0 wt%, such as having essentially no cycloparaffin content. In some aspects, the combined paraffin and cycloparaffin content of this portion of the heat-treated first higher density portion can be less than or equal to about 1.0 wt%.

[0150] The following aspect of the invention is now described in more detail, which aspect includes separating a second higher density portion and a second lower density portion from a heat treated first higher density portion. The invention is not limited in these aspects, and this specification should not be interpreted as excluding other forms of separation within the broader scope of the present disclosure. For simplicity, this separation is referred to as the "second SCT separation". Those skilled in the art will understand that this identifier is used because the heat treated first higher density portion is derived from SCT. The use of this identifier should not be interpreted as limiting the second separation to the separation of a stream from an SCT itself, such as an SCT that has not undergone a first heat treatment or a first SCT separation.

[0151] Second SCT separation - separation of the second higher density and second lower density fractions from the heat treated first higher density fraction

[0152] The second higher density and lower density portion can be separated from the heat-treated first higher density portion by any means to achieve the specified separation, including one or more of sedimentation, filtration and extraction. Conventional separation techniques can be used, but the embodiment is not limited thereto. For example, the second lower density portion can be separated from the heat-treated first higher density portion by decantation, filtration and / or boiling point separation (e.g., one or more distillation towers, splitters, flash drums, or any combination thereof). The second higher density portion can be separated from the heat-treated first higher density portion in a similar manner, such as by removing the second higher density portion as a bottom product portion from the separation section. The second higher density portion and the second lower density portion can be separated from the heat-treated first higher density portion in any order, such as substantially simultaneously, by first separating the second higher density portion and then separating the second higher density portion from the second lower density portion, or vice versa. In some aspects, the second higher density portion and the second lower density portion are separated by exposing the heat-treated first higher density portion to centrifugal force, such as by using one or more centrifuges in the separation section.

[0153] The second higher density portion and the second lower density portion may be separated from the heat treated first higher density portion by any means to form the second higher density portion and the second lower density portion. Aspects of separation using one or more centrifuges in the second SCT separation stage are now described in greater detail. Embodiments are not limited in these respects, and this description is not to be construed as excluding the use of additional and / or alternative separation techniques, such as those that do not involve exposing the heat treated first higher density portion to centrifugal forces.

[0154] Induced centrifugal force

[0155] In some aspects, the heat-treated first higher density portion containing the heat-treated SCT, any diluent, and any solids remaining after the second heat treatment is provided to a second centrifuge for exposure of the heat-treated first higher density portion to a centrifugal force sufficient to form at least a second higher density portion and a second lower density portion. Typically, as a result of the application of the centrifugal force, the heat-treated first higher density portion exhibits a substantially uniform circular motion within the centrifuge, the central force being referred to as a centrifugal force (within the reference frame of the heat-treated first higher density portion) or a centripetal force (within the reference frame of the centrifuge), depending on the choice of reference frame. The method can be performed in a batch, semi-batch, or continuous manner.

[0156] The centrifuge can be configured to apply heat to the heat-treated first higher density portion, for example, by heating the heat-treated first higher density portion to an elevated temperature. In some aspects, inducing centrifugal force further comprises heating the heat-treated first higher density portion to a temperature of about 20°C, about 25°C, about 30°C, about 40°C, about 50°C, about 55°C, or about 60°C to about 65°C, about 70°C, about 80°C, about 85°C, about 90°C, about 95°C, about 100°C, about 110°C, about 120°C, or greater. For example, while centrifuging, the heat-treated first higher density portion can be heated to a temperature of about 20°C to about 120°C, about 20°C to about 100°C, about 30°C to about 100°C, about 40°C to about 100°C, about 50°C to about 100°C, about 60°C to about 100°C, about 70°C to about 100°C, about 80°C to about 100°C, about 90°C to about 100°C, about 20°C to about 80°C, about 30°C to about 80°C, about 40°C to about 80°C, about 50°C to about 80°C, about 60°C to about 80°C, or about 70°C to about 80°C.

[0157] Centrifugal force can be applied for any amount of time. Typically, centrifugal force is applied for ≥1 minute, for example, ≥5 minutes, ≥10 minutes, ≥30 minutes, ≥60 minutes, or ≥120 minutes. Additionally or alternatively, centrifugal force can be applied for ≤120 minutes, ≤60 minutes, ≤30 minutes, ≤10 minutes, or ≤5 minutes. Clearly disclosed scope includes any combination of numerical values ​​enumerated above, for example, from about 1 minute to about 120 minutes, from about 5 minutes to about 120 minutes, from about 10 minutes to about 120 minutes, from about 30 minutes to about 120 minutes, or from about 60 minutes to about 120 minutes. Centrifugal force can be applied under any force or speed size. For example, by providing enough force at about 1,000rpm to about 10,000rpm, from about 2,000rpm to about 7,500rpm, or from about 3,000rpm to about 5,000rpm centrifuges operating.

[0158] Centrifuging the heat-treated first higher density portion typically results in separation of at least (i) an extract containing a second higher density portion of the heat-treated first higher density portion and (ii) a second raffinate or a second lower density portion from the heat-treated first higher density portion. In other words, exposing the heat-treated first higher density portion to centrifugal force results in removal of at least the second higher density portion (the second extract) from the heat-treated first higher density portion. When the process is operated continuously or semi-continuously, at least two streams may be directed away from the centrifuge: one stream containing the second extract and another stream containing the second raffinate. Centrifuges with this capability are commercially available.

[0159] Typically, centrifugation is sufficient to separate ≥80 wt%, ≥90 wt%, ≥95 wt%, ≥99 wt% of solids with a size of ≥2 μm, e.g., ≥10 μm, e.g., ≥20 μm, or ≥25 μm into a second higher density portion (e.g., a second extract), wherein the wt% is based on the total weight of solids in the second higher density and second lower density portions. In the case where subsequent hydroprocessing of the second raffinate is envisioned, the second higher density portion contains ≥95 wt%, especially ≥99 wt% of solids with a size of ≥2 μm, e.g., ≥10 μm, e.g., ≥20 μm, or ≥25 μm. In other aspects, filtering should be sufficient to separate at least 80 wt% of the solids into the higher density portion.

[0160] Although this description focuses on the second higher density portion and the second lower density portion, other embodiments envision that the components in the heat treated first higher density portion can be separated and extracted more independently, such as very light components separated to the top of the mixture, a portion containing mainly diluent, an upgraded tar portion, tar heavies, or solids at the bottom of the centrifuge chamber. One or more of these portions can be selectively removed from the mixture as one or more raffinates. Typically, at least a portion of the second lower density portion is recycled (directly or indirectly) to the first centrifuge. The second higher density portion can be transported away from the process, such as for storage and / or further processing, including additional centrifugation.

[0161] The second lower density portion

[0162] The second lower density fraction is typically removed from the separation stage as a second raffinate, a portion of which (e.g., ≥50 wt%, ≥75 wt%, ≥90 wt%) may be directed away for recycling, for example as a component of a tar-fluid mixture. In certain aspects, the second lower density fraction is recycled and combined with one or more of: (i) a steam cracker effluent, (ii) SCT, (iii) an SCT composition, (iv) a tar-fluid mixture prior to and / or during separation of the first higher density fraction and the first lower density fraction, (v) a first higher density fraction, and (vi) a first lower density fraction. In certain aspects, the second lower density fraction may be added to the SCT composition in an amount sufficient to form a portion or all of the fluid used to form the tar-fluid mixture. In aspects where the first, lower density portion is hydrotreated (e.g., SATC hydrotreated), recycling at least a portion of the second, lower density portion provides a greater yield of upgraded (e.g., hydrotreated) tar compared to conventional tar upgrading processes, provides material and cost savings for the tar upgrading process, and produces less solids that are directed away.

[0163] The second lower density portion generally has a desired insolubility value, such as an insolubility value less than one or more of: (i) SCT, (ii) SCT composition, (iii) tar-fluid mixture, (iii) the first higher density portion, and the second higher density portion. Typically, the insolubility value (I LD ) is ≥20, e.g., ≥30, ≥40, ≥50, ≥60, ≥70, ≥80, ≥90, ≥100, ≥110, ≥120, ≥130, ≥140, or ≥150. Additionally or alternatively, I LD It may be ≤150, for example, ≤140, ≤130, ≤120≤110, ≤100, ≤90, ≤80, ≤70, ≤60, ≤50, ≤40, or ≤30. Explicitly disclosed ranges include any combination of the above enumerated values, for example, about 20 to about 150, about 20 to about 140, about 20 to about 130, about 20 to about 120, about 20 to about 110, about 20 to about 100, about 20 to about 90, about 20 to about 80, about 20 to about 70, about 20 to about 60, about 20 to about 50, about 20 to about 40, or about 20 to about 30. It will be understood by those skilled in the art that hydrocarbon separation techniques are not perfect, and therefore a small amount of solids may be present in the second lower density portion, for example, an amount of solids that is ≤0.1 times the amount of solids in the heat treated first higher density portion, for example, ≤0.01 times. The insoluble value I of the second lower density portion LD Insolubility value I for tar-fluid mixture TF The ratio is ≤0.95, for example, ≤0.90, ≤0.85, ≤0.80, ≤0.75, ≤0.70, ≤0.65, ≤0.60, ≤0.55, ≤0.50,

[0164] ≤0.40, ≤0.30, ≤0.20, or ≤0.10. Additionally or alternatively, I LD to I TF The ratio can be ≥0.10, for example, ≥0.20, ≥0.30, ≥0.40, ≥0.50, ≥0.55, ≥0.60, ≥0.65, ≥0.70, ≥0.75, ≥0.80, ≥0.85, or ≥0.90. The explicitly disclosed range includes any combination of the above enumerated values, for example, about 0.10 to 0.95, about 0.20 to 0.95, about 0.30 to 0.95, about 0.40 to 0.95, about 0.50 to 0.95, about 0.55 to 0.95, about 0.60 to 0.95, about 0.65 to 0.95, about 0.70 to 0.95, about 0.75 to 0.95, about 0.80 to 0.95, about 0.85 to 0.95, or about 0.90 to 0.95.

[0165] Typically, at least a portion of the second lower density portion is in the liquid phase, e.g., ≥25 wt%, e.g., ≥50 wt%, or ≥75 wt%, or ≥90 wt%. Typically, ≥50 wt% of the solids converted (e.g., from granular form) during and / or as a result of the second thermal treatment reside in the second lower density portion, e.g., ≥75 wt%, e.g., ≥90 wt%, or ≥99 wt%. Typically, ≥50 wt% of the diluent in the diluted first higher density portion resides in the second lower density portion, e.g., ≥50 wt%, e.g., ≥75 wt%, or ≥90 wt%, or ≥99 wt%.

[0166] Example of construction for hot soaking of cracked tar solids

[0167] Figure 1 is a schematic diagram illustrating an apparatus for implementing certain aspects of the present invention. More generally, the apparatus may be used in conjunction with Figure 1 A similar configuration is used to heat soak the higher density portion of the pyrolysis tar composition.

[0168] exist Figure 1 In the embodiment of the present invention, the steam cracker effluent 102 containing SCT is introduced into a first thermal treatment stage 124, such as the bottoms stage of a tar drum. A stream of mainly gas phase is directed away from stage 124 via line 128 to a primary fractionator 126 for separation of at least a quench oil stream 160 and a process gas 170. An SCT composition containing thermally treated (e.g., heat soaked) SCT is directed away from stage 124 via line 105.

[0169] Recycle stream 104 and optional stream 103 (which contains an optional first utility fluid and / or an optional first separation fluid provided by a source (not shown)) are added to the SCT composition to produce a tar-fluid mixture. The tar-fluid mixture is introduced into a first SCT separation stage 120, which typically includes at least one centrifuge, such as a decanter centrifuge. A first higher density fraction (directed away via line 125) and a first lower density fraction (directed away via line 122) are separated from the tar-fluid mixture in stage 120. In continuous operation, the first higher density fraction directed via line 125 typically includes ≥50 wt% of the first higher density fraction available for further processing in hot soak vessel 116, e.g., ≥75 wt%, such as ≥90 wt%.

[0170] exist Figure 1In the illustrated configuration, at least a portion of the first lower density fraction is directed to optional stage 140 via line 122 for hydroprocessing, such as SATC hydroprocessing. The first higher density fraction may be transferred to one or more optional stages, such as at least one optional size reduction stage 130, to produce a pulverized first higher density fraction. The first higher density fraction is combined with a diluent (which includes a second utility fluid and / or a second separation fluid provided by one or more sources (not shown)) via lines 127 and / or 135, such as before and / or after pulverization. The diluted first higher density fraction is introduced into a second thermal treatment stage 116 (e.g., a second heat soak vessel) via line 114. The second thermal treatment stage 116 provides a thermally treated first higher density fraction, which is introduced into a second SCT separation stage 150, which typically contains at least one centrifuge, such as a decanter centrifuge, via line 118. Stage 150 provides a second higher density fraction that may be transported away via line 122, such as for storage, additional thermal processing, and / or additional separation. The second lower density fraction circulates via line 104 . Example

[0171] Examples of high temperature dissolution / decomposition in the second heat treatment

[0172] 0.5 g of solid obtained from a representative tar (in this case representative SCT) was mixed with approximately 50 mL of toluene in a bomb reactor. Toluene corresponds to the second utility fluid of line 127. The solid was heated to 100 psig at a temperature ranging from 250°C to 350°C (sand bath temperature). 2 The mixture was heat treated (hot soaked) for 30 min at 4 °C. The reactor was quickly quenched with cold water and filtered through a 1.5 μm filter. The reactor was washed with excess toluene to ensure complete solid recovery. The weight of the residual solids was measured after the heat treatment and the solid loss wt% was reported.

[0173] Figure 2 1 is a graph illustrating the solid loss (wt%) as a function of the temperature used in the process using toluene as a solvent. The experimental results show that at least 80% or more of the solids (relatively low value materials) can be upgraded to higher value liquid phase materials suitable for use as SATC feed. Therefore, key operating parameters include temperature, residence time and suitable solvent. It was observed that hot soaking at a temperature of 275°C-300°C for 30 minutes to 60 minutes is sufficient.

[0174] All documents described herein are incorporated by reference in all jurisdictions where such practice is permitted, including any priority documents and / or testing procedures, to the extent that they do not conflict with this article, provided, however, that any priority documents not mentioned in the initially submitted application or submission document are not incorporated by reference in this article. Although the form of the embodiment has been set forth and described, various modifications may be made without departing from the spirit and scope of the disclosure of the present invention. Therefore, it is not intended to limit the disclosure of the present invention. Likewise, the term "comprising" is considered to be synonymous with the terms "including" and "containing". Likewise, at any time when there is a composition, element or element group before the transitional wording "comprising", it is understood that we also consider the same composition or element group with the transitional wording "substantially consisting of", "consisting of", "selected from" or "is" before citing a composition, one or more elements, and vice versa.

[0175] Certain embodiments and features are described using a set of numerical upper limits and a set of numerical lower limits. It should be understood that, unless otherwise indicated, any combination of lower limits with any upper limits, any combination of two lower limits, and / or any combination of two upper limits are contemplated. Certain lower limits, upper limits, and ranges appear in one or more of the following claims.

Claims

1. A method for upgrading tar, the method comprising: thermally treating the tar in a first thermal treatment to produce a tar composition; separating a first lower density portion and a first higher density portion from at least a portion of the tar composition, wherein the first higher density portion comprises solids in an amount of A1 wt % based on the weight of the first higher density portion; directing away an upgraded pyrolyzed tar composition comprising at least a portion of the first lower density portion; heat treating at least a portion of the first higher density portion in a second heat treatment to form a heat-treated first higher density portion, the second heat treatment being performed by heat soaking to convert 50 wt % to 99 wt % of the solids in the first higher density portion into liquid in the heat-treated first higher density portion, wherein (i) the heat-treated first higher density portion comprises solids in an amount of A2 wt %, based on the weight of the heat-treated first higher density portion, and (ii) A2 <A1; separating a second lower density portion and a second higher density portion from at least a portion of the heat treated first higher density portion; and At least a portion of the second lower density fraction is added to one or more of: (i) the tar before and / or during the first heat treatment, (ii) the tar composition, (iii) the first higher density fraction, and (iv) the first lower density fraction.

2. The method of claim 1, further comprising adding a fluid to the tar composition, wherein > 90 wt% of the added fluid is transferred to the first lower density portion.

3. The method of claim 1 or 2, further comprising adding a diluent to the first higher density portion, and wherein > 90 wt% of the added diluent resides in the second lower density portion.

4. The method of claim 1, wherein the first thermal treatment comprises maintaining the tar at a temperature of ≤ 350°C for a time ranging from 10 minutes to 60 minutes.

5. The method of claim 1, wherein the first heat treatment comprises maintaining the tar at a temperature in the range of 150°C to 300°C for a time in the range of 15 minutes to 30 minutes.

6. The method of claim 1, wherein (i) the second heat treatment comprises maintaining the first higher density portion at a temperature in the range of 220°C to 500°C for a time in the range of 10 minutes to 100 minutes, and (ii) A2≤0.8*A1.

7. The method of claim 1, wherein the second heat treatment comprises maintaining the first higher density portion at a temperature in the range of 250°C to 400°C for a time in the range of 20 minutes to 90 minutes.

8. The method of claim 1, wherein A2 ranges from 10% of A1 to 40% of A1.

9. The process of claim 1, wherein the tar is a pyrolysis tar comprising steam cracker tar.

10. The process of claim 1, wherein the tar is a steam cracker tar produced by steam cracking a steam cracker feed comprising ≥ 10 wt% of material in a solid or liquid phase at 25°C and 1 bar absolute pressure, based on the weight of the steam cracker feed.

11. The method of claim 1, wherein: (i) the tar is a steam cracked tar produced by steam cracking a hydrocarbon feed comprising ≥ 1 wt% hydrocarbons having a normal boiling point ≥ 566°C, based on the weight of the steam cracker feed; (ii) a steam cracker comprising a convection section and a radiant section; (iii) preheating the hydrocarbon feed in a convection section and combining with steam to produce a steam cracker feed; (iv) separating a stream of a primarily gaseous phase and a stream of a primarily non-gaseous phase from at least a portion of the steam cracker feed, wherein ≥ 50 wt% of any hydrocarbons in the hydrocarbonaceous feed having a normal boiling point ≥ 566°C are transferred to the stream of the non-gaseous phase; (v) directing at least a portion of the stream of predominantly gaseous phase into an inlet of at least one radiant coil located in the radiant section for cracking under steam cracking conditions, wherein the radiant coil comprises the inlet and the outlet, and the steam cracking conditions comprise: The temperature at the outlet of the radiation coil ranges from 760°C to 1200°C. a steam cracking pressure in the range of 1 bara to 10 bara at the outlet of the radiant coils, and Steam cracking residence time in the radiant coils ranging from 0.1 seconds to 2 seconds; (vi) directing the steam cracker effluent away from the radiant section; and (vii) separating at least steam cracker tar from the steam cracker effluent.

12. The process of claim 11, wherein a stream of mainly gaseous phase and a stream of mainly non-gaseous phase are separated from the steam cracker feed in a separation section integrated with the convection section, and wherein the separated stream of mainly gaseous phase is exposed to additional heating in the convection section prior to cracking.

13. The method of claim 11, wherein the temperature at the outlet of the radiant coil ranges from 880°C to 1,200°C.

14. The process of claim 11, wherein the temperature at the outlet of the radiant coils ranges from 1,000°C to 1,200°C, and the steam cracking pressure ranges from 6 bara to 10 bara.

15. The process of claim 11, wherein the steam cracking temperature ranges from 760°C to 880°C, and the steam cracking pressure ranges from 1 bara to 5 bara.

16. The method of claim 3, further comprising grinding the first higher density portion before and / or after adding the diluent.

17. A method for upgrading steam cracker tar, the method comprising: steam cracking a hydrocarbon feed comprising heavy oil to form a steam cracker effluent comprising steam cracker tar; separating at least a portion of the steam cracker tar from the steam cracker effluent; thermally treating at least the separated steam cracker tar in a first thermal treatment to produce a steam cracker tar composition; adding a first utility fluid and / or a first separation fluid to a steam cracker tar composition to produce a tar-fluid mixture; separating (i) a first lower density fraction comprising upgraded steam cracker tar and (ii) a first higher density fraction from the tar-fluid mixture; directing away at least a portion of the first lower density portion; introducing a second utility fluid into the first higher density portion to form a diluted first higher density portion, wherein the diluted first higher density portion comprises solids in an amount of A1 wt % based on the weight of the first higher density portion; heat treating the diluted first higher density portion in a second heat treatment to form a heat-treated first higher density portion, the second heat treatment being performed by heat soaking to convert 50 wt % to 99 wt % of the solids in the first higher density portion into liquids in the heat-treated first higher density portion, wherein (i) the heat-treated first higher density portion comprises solids in an amount of A2 wt %, based on the weight of the heat-treated first higher density portion, and (ii) A2 ≤ 0.8*A1; separating at least a second lower density fraction and a second higher density fraction from the heat treated first higher density fraction in a second separation; and At least a portion of the second lower density fraction is added to one or more of: (i) a steam cracker effluent, (ii) a steam cracker tar before and / or during the first thermal treatment, (iii) a steam cracker tar composition, (iv) a tar-fluid mixture before and / or during separation of the first higher density fraction and the first lower density fraction, (v) the first higher density fraction, and (vi) the first lower density fraction.

18. The method of claim 17, wherein: (i) steam cracking of heavy oil at a temperature of 760° C. to 880° C., a pressure of 1 bar (absolute pressure) to 5 bar (absolute pressure) and a residence time of 0.1 second to 2 seconds; (ii) a first thermal treatment comprises maintaining the steam cracker tar at a temperature in the range of 150°C to 300°C for a time in the range of 15 minutes to 30 minutes; and (iii) The second heat treatment includes maintaining the diluted first higher density portion at a temperature in the range of 300° C. to 400° C. for a time in the range of 30 minutes to 60 minutes.

19. The method of claim 17 or 18, wherein the tar-fluid mixture comprises a steam cracker tar composition in an amount ranging from 40 wt% to 80 wt%, based on the weight of the tar-fluid mixture.

20. The method of claim 17, further comprising grinding the first higher density portion before and / or after introducing the second utility fluid.

21. The method of claim 17, further comprising (i) hydrotreating at least a portion of the first, lower density portion, and (ii) directing away at least a portion of the second, higher density portion.

22. The method of claim 17, wherein (i) the first and / or second heat treatment comprises heat soaking in at least one infuser drum, and / or (ii) the first and / or second separation comprises centrifugation and / or filtration.

23. A method for upgrading steam cracker tar, the method comprising: steam cracking a hydrocarbon feed containing heavy oil at a temperature of 760° C. to 880° C., a pressure of 1 bar (absolute) to 5 bar (absolute) and a residence time of 0.1 second to 2 seconds to form a steam cracker effluent containing steam cracker tar; separating at least a portion of the steam cracker tar from the steam cracker effluent; thermally treating at least the separated steam cracker tar in a first thermal treatment by maintaining the steam cracker tar at a temperature of 150° C. to 300° C. for a period of 15 minutes to 30 minutes to produce a steam cracker tar composition comprising polymer pellets formed during or as a result of the first thermal treatment; adding a first utility fluid and / or a first separation fluid to a steam cracker tar composition to produce a tar-fluid mixture; Separating from the tar-fluid mixture (i) a first lower density fraction comprising upgraded steam cracker tar and (ii) a first higher density fraction comprising polymer pellets, wherein the first higher density fraction comprises polymer pellets in an amount of A1 wt %, based on the weight of the first higher density fraction; directing away at least a portion of the first lower density portion; introducing a second utility fluid into the first higher density portion to form a diluted first higher density portion; heat treating the diluted first higher density portion by maintaining the diluted first higher density portion at a temperature in the range of 300° C. to 400° C. for a time in the range of 30 minutes to 60 minutes in a second heat treatment to form a heat-treated first higher density portion, the second heat treatment being performed by heat soaking to convert 50 wt % to 99 wt % of the solids in the first higher density portion into liquids in the heat-treated first higher density portion, wherein (i) the heat-treated first higher density portion comprises a conversion product having a lower density than the polymer particulates, (ii) the heat-treated first higher density portion comprises polymer particulates in an amount of A2 wt % based on the weight of the heat-treated first higher density portion, and (iii) A2≤0.8*A1; separating at least a second lower density fraction and a second higher density fraction from the heat treated first higher density fraction in a second separation, the second lower density fraction comprising a lower density conversion product; and At least a portion of the second lower density fraction is added to one or more of: (i) a steam cracker effluent, (ii) a steam cracker tar before and / or during the first thermal treatment, (iii) a steam cracker tar composition, (iv) a tar-fluid mixture before and / or during separation of the first higher density fraction and the first lower density fraction, (v) the first higher density fraction and (vi) the first lower density fraction.