A connection structure between a kiln nozzle brick and a kiln nozzle
By designing the connection structure between the kiln nozzle bricks and nozzles in float glass equipment, using high-speed airflow to mix with natural gas, reducing the temperature difference of the kiln bricks, solving the problem of easy damage to the kiln nozzle bricks, extending the service life and replacement cycle.
Patent Information
- Application Number
- CN202111276627.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2021-10-29
- Publication Date
- 2024-11-22
- Estimated Expiration
- 2041-10-29
AI Technical Summary
In the existing float glass equipment, the furnace nozzle bricks are easily damaged due to long-term high-speed combustion, resulting in local high-thermal stress, which leads to frequent replacement and long production quality cycle.
A connection structure between the kiln nozzle brick and the kiln nozzle is designed, including a natural gas input pipe, an intake pipe and an outlet pipe. The combustion head is connected through the flaring to form a heat insulation cavity, and air intake holes and valves are provided on the outlet pipe. , use a blower to drive the high-speed airflow to mix with natural gas to reduce the temperature difference of the kiln bricks.
It effectively extends the service life and replacement cycle of the kiln bricks, reduces the temperature at the kiln bricks close to the combustion head, reduces the temperature difference, and thus slows down the damage of the kiln bricks.
Smart Images

Figure HDA0003329630620000011 
Figure HDA0003329630620000021 
Figure HDA0003329630620000031
Abstract
Description
Technical Field
[0001] The invention belongs to the technical field of float glass equipment and relates to a connection structure between a kiln nozzle brick and a kiln nozzle. Background Art
[0002] The melting furnace is one of the three major thermal equipment in float glass production equipment. The melting process of the melting furnace mainly relies on the radiation heat transfer of the high-speed combustion spray gun to achieve the melting effect. Due to production needs, the spray gun is in a state of non-stop combustion. For a long time, as the age of the kiln increases, the burnout of the nozzle bricks has increased, affecting the flame state and the safety of the kiln structure. At present, the main way to extend the service life is to replace the nozzle bricks, but the replacement process is time-consuming and labor-intensive, and affects the production and quality cycle for a long time.
[0003] The main reason why the kiln bricks at the nozzle are easily damaged is that the local heating temperature of the kiln bricks at the nozzle is higher than that of other parts and other kiln bricks, which causes the thermal stress of the kiln bricks at the nozzle to be larger and easy to be damaged. Summary of the invention
[0004] The purpose of the present invention is to provide a kiln nozzle that can extend the service life of kiln nozzle bricks in view of the above-mentioned problems existing in the prior art. The technical problem to be solved by the present invention is how to extend the service life and maintenance cycle of kiln bricks.
[0005] The object of the present invention can be achieved through the following technical solutions: a connection structure of a kiln nozzle brick and a kiln nozzle, characterized in that it includes a natural gas input pipe, an air inlet pipe sleeved outside the natural gas input pipe, an air outlet pipe sleeved outside the air inlet pipe and a combustion head, the outlet of the natural gas input pipe is connected to the combustion head through a flare, the flare is a conical tubular structure with the large diameter end facing the combustion head, the natural gas input pipe is connected to the air outlet pipe through the flare, the air inlet pipe and the air outlet pipe are connected at the flare, an insulating cavity is formed between the air outlet pipe and the air inlet pipe, an air inlet hole is opened on the peripheral wall of the flare, a socket for allowing the air outlet pipe to be inserted is opened on the kiln wall, and the kiln brick is fixed on the air outlet pipe outside the insulating cavity.
[0006] Furthermore, a limiting ring is detachably connected to the air outlet pipe located on the inner side of the kiln wall, and a mounting seat is detachably connected to the burner head.
[0007] Furthermore, a valve is provided at the outlet end of the outlet pipe, and the outlet gas volume is controlled by controlling the valve opening, thereby controlling the air intake volume entering the combustion head through the air intake hole.
[0008] Furthermore, the limiting ring is a metal part, and the mounting seat is a ceramic part.
[0009] The blower drives high-speed airflow from the air inlet pipe into the expansion port. Since the air inlet hole on the expansion port is facing the flow direction of the air inlet flow, part of the air enters the combustion head and is mixed with natural gas. Most of the air in the air inlet pipe is turned back from the end of the air inlet pipe and enters the air outlet pipe. In addition to cooling the kiln wall and kiln bricks outside the air outlet pipe, this part of the gas also has the effect of reducing the temperature difference. This is because: the airflow begins to heat up rapidly at the end of the air inlet pipe, and can maintain a relatively low temperature before that. After turning back and entering the air outlet pipe, this part of the air is heated by the kiln wall and is still in a heated state, thereby making the temperature difference between the inside and outside of the kiln bricks outside the air outlet pipe relatively small, and the temperature of the kiln bricks near the combustion head, which is most prone to damage, is relatively low, which can effectively extend the service life and replacement cycle of the kiln bricks. BRIEF DESCRIPTION OF THE DRAWINGS
[0010] Figure 1 It is a schematic diagram of the three-dimensional structure of the kiln nozzle.
[0011] Figure 2 It is a schematic diagram of the cross-sectional structure of the kiln nozzle.
[0012] Figure 3 It is a structural diagram of the kiln nozzle when it is installed.
[0013] In the figure, 1. natural gas input pipe; 2. air inlet pipe; 3. air outlet pipe; 4. expansion port; 5. heat insulation cavity; 6. air inlet hole; 7. limit ring; 8. mounting seat; 9. valve; 10. kiln wall; 11. kiln brick; 12. combustion head. DETAILED DESCRIPTION
[0014] The following are specific embodiments of the present invention and the accompanying drawings to further describe the technical solution of the present invention, but the present invention is not limited to these embodiments.
[0015] like Figure 1 , Figure 2 and Figure 3 As shown, it includes a natural gas input pipe 1, an air inlet pipe 2 sleeved outside the natural gas input pipe 1, an air outlet pipe 3 sleeved outside the air inlet pipe 2 and a burner head 12. The outlet of the natural gas input pipe 1 is connected to the burner head 12 through a flare 4. The flare 4 is a conical tubular structure with the large diameter end facing the burner head 12. The natural gas input pipe 1 is connected to the air outlet pipe 3 through the flare 4. The air inlet pipe 2 and the air outlet pipe 3 are connected at the flare 4. An insulating cavity 5 is formed between the air outlet pipe 3 and the air inlet pipe 2. An air inlet hole 6 is opened on the peripheral wall of the flare 4. A plug hole allowing the air outlet pipe 3 to be inserted is opened on the kiln wall 10. The kiln brick 11 is fixed on the air outlet pipe 3 outside the insulating cavity 5.
[0016] A limiting ring 7 is detachably connected to the air outlet pipe 3 located at the inner side of the kiln wall 10, and a mounting seat 8 is detachably connected to the combustion head 12. The limiting ring 7 is a metal part, and the mounting seat 8 is a ceramic part.
[0017] A valve 9 is provided at the outlet end of the outlet pipe 3 , and the outlet gas volume is controlled by controlling the opening of the valve 9 , thereby controlling the air intake volume entering the combustion head 12 through the air intake hole 6 .
[0018] The blower drives a high-speed airflow from the air inlet pipe 2 into the expansion port 4. Since the air inlet hole 6 on the expansion port 4 is facing the flow direction of the air inlet airflow, part of the air enters the combustion head 12 and is mixed with the natural gas. Most of the air in the air inlet pipe 2 is turned back from the end of the air inlet pipe 2 and enters the air outlet pipe 3. In addition to cooling the kiln wall 10 and the kiln bricks 11 outside the air outlet pipe 3, this part of the gas also has the effect of reducing the temperature difference. This is because: the airflow begins to heat up rapidly at the end of the air inlet pipe 2, and can maintain a relatively low temperature before that. After turning back and entering the air outlet pipe 3, this part of the air is heated by the kiln wall 10 and is still in a heated state, thereby making the temperature difference between the inside and outside of the kiln bricks 11 located outside the air outlet pipe 3 relatively small, and the temperature of the part of the kiln bricks 11 close to the combustion head 12, which is most prone to damage, is relatively low, which can effectively extend the service life and replacement cycle of the kiln bricks 11.
[0019] The specific embodiments described herein are merely examples of the spirit of the present invention. Those skilled in the art may make various modifications or additions to the specific embodiments described or replace them in similar ways, but they will not deviate from the spirit of the present invention or exceed the scope defined by the appended claims.
Claims
1. A connection structure between a kiln nozzle brick and a kiln nozzle, characterized in that: The invention comprises a natural gas input pipe (1), an air inlet pipe (2) sleeved outside the natural gas input pipe (1), an air outlet pipe (3) sleeved outside the air inlet pipe (2), and a burner head (12); the outlet of the natural gas input pipe (1) is connected to the burner head (12) via a flared opening (4); the flared opening (4) is a conical tubular structure with the large diameter end facing the burner head (12); the natural gas input pipe (1) is connected to the air outlet pipe (3) via the flared opening (4); the air inlet pipe (2) and the air outlet pipe (3) are connected at the flared opening (4); a heat insulating cavity (5) is formed between the air outlet pipe (3) and the air inlet pipe (2); an air inlet hole (6) is provided on the peripheral wall of the flared opening (4); a plug hole for allowing the air outlet pipe (3) to be inserted is provided on the kiln wall (10); and a kiln brick (11) is fixed to the air outlet pipe (3) outside the heat insulating cavity (5).
2. The connection structure between a kiln nozzle brick and a kiln nozzle according to claim 1, characterized in that: A limiting ring (7) is detachably connected to the air outlet pipe (3) located on the inner side of the kiln wall (10), and a mounting seat (8) is detachably connected to the combustion head (12).
3. The connection structure between a kiln nozzle brick and a kiln nozzle according to claim 1 or 2, characterized in that: A valve (9) is provided at the outlet end of the outlet pipe (3), and the outlet gas volume is controlled by controlling the opening of the valve (9), thereby controlling the air intake volume entering the combustion head (12) through the air intake hole (6).
4. The connection structure between a kiln nozzle brick and a kiln nozzle according to claim 2, characterized in that: The limiting ring (7) is a metal part, and the mounting seat (8) is a ceramic part.